Chip packaging structure and chip packaging method
By using the barrier layers of windows and openings and the broken coating to fill the cavity in the chip package structure, the problem of low reliability of the chip package structure is solved, ensuring the normal operation and filling of the filter and non-filter chips.
Patent Information
- Application Number
- CN202411054559.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-11-21
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-08-01
AI Technical Summary
The reliability of the existing chip packaging structure is not high, especially due to the lack of effective plastic packaging material filling, the reliability of non-filter devices cannot be guaranteed.
Using a first barrier layer with a window and an opening, covering the filter and non-filter chips, and breaking the coating near the window of the second barrier layer to form a fracture to fill the window and cavity to ensure the operation of the filter chip and Improve the filling reliability of non-filter chips.
Through this method, the normal operation of the filter chip is ensured, and the filling reliability of non-filter devices is improved, and the reliability of the overall chip packaging structure is enhanced.
Smart Images

Figure CN118969787A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of chip packaging, and in particular to a chip packaging structure and a chip packaging method. Background Art
[0002] Surface acoustic wave filters use sound waves to transmit on the surface of the chip to achieve their functions. Therefore, for the packaging of surface acoustic wave filters, the surface of the interdigital transducer in the surface acoustic wave filter needs to not contact other substances, that is, a cavity needs to be formed on the chip surface, otherwise it will affect signal transmission. The chip packaging structure based on the surface acoustic wave filter can also include conventional components that can work without a cavity, such as antenna switches, low-noise amplifiers, capacitors, inductors, etc.
[0003] For example, traditional diversity reception (DRX) modules often use a coating method to isolate the outer plastic packaging material to ensure that the surface of the filter forms a cavity. However, other devices in the module cannot be well filled at the bottom due to the influence of the coating, which easily leads to a short circuit of the device. At the same time, the reliability of non-filter devices cannot be guaranteed because there is no plastic packaging material filling. How to improve the reliability of such chip packaging structures has become a problem that technicians in this field need to solve. Summary of the invention
[0004] The object of the present invention is to provide a chip packaging structure and a chip packaging method to solve the problem of low reliability of the chip packaging structure in the prior art.
[0005] In order to solve the above technical problems, the present invention provides a chip packaging structure, the chip packaging structure comprising:
[0006] A substrate, the substrate comprising a filter-carrying area, a non-filter-carrying area, and an aisle area surrounding the filter-carrying area and the non-filter-carrying area, a first solder pad and a second solder pad being formed on the substrate, the first solder pad being located in the filter-carrying area, and the second solder pad being located in the non-filter-carrying area;
[0007] A first barrier layer is formed on the substrate, the first barrier layer having a window and an opening penetrating in a thickness direction, the window exposing the substrate and the second pad in the non-filter carrying area and a portion of the substrate in the aisle area surrounding the non-filter carrying area, and the opening exposing the first pad;
[0008] a second barrier layer formed on the first barrier layer, wherein the second barrier layer is located at an edge of the first barrier layer close to the window;
[0009] A filter chip aligned with the filter bearing area, the filter chip comprising a first substrate, an IDT formed on the first substrate, and a first bump formed on the first substrate, the IDT facing the first barrier layer, the first bump and the first pad being electrically connected, and a first cavity being formed below the filter chip;
[0010] A non-filter chip aligned with the non-filter bearing area, the non-filter chip comprising a second substrate and a second bump formed on the second substrate, the second bump and the second pad are electrically connected, a second cavity is formed below the non-filter chip, and the window is connected to the second cavity;
[0011] a coating covering the filter chip, the non-filter chip, the first barrier layer and the second barrier layer, the coating sealing the first cavity and breaking the second barrier layer near the window to form a fracture; and,
[0012] A plastic sealing layer covers the surface of the coating, and the plastic sealing layer also passes through the fracture to fill the window and the second cavity.
[0013] Optionally, in the chip packaging structure, the thickness of the coating is H1, the particle size in the plastic encapsulation layer is H2, the projection of the non-filter chip on the substrate coincides with the non-filter bearing area, and the distance between at least one boundary of the window and the corresponding boundary of the non-filter bearing area is greater than or equal to H1+2H2.
[0014] Optionally, in the chip packaging structure, the projection of the non-filter chip on the substrate overlaps with the non-filter supporting area, and the distance between at least one boundary of the window and the corresponding boundary of the non-filter supporting area is greater than or equal to 10 μm.
[0015] Optionally, in the chip packaging structure, the second barrier layer is ring-shaped around the window.
[0016] Optionally, in the chip packaging structure, the second barrier layer is formed only on the first barrier layer aligned with the aisle region, and the width of the second barrier layer along the surface of the substrate is smaller than the width of the aisle region.
[0017] Optionally, in the chip packaging structure, the width of the second barrier layer along the surface of the substrate is greater than or equal to 50 μm.
[0018] Optionally, in the chip packaging structure, a boundary of the second barrier layer close to the window is flush with a boundary of the first barrier layer close to the window.
[0019] Optionally, in the chip packaging structure, a surface of the non-filter chip close to the substrate is lower than, equal to, or higher than a surface of the second barrier layer.
[0020] Optionally, in the chip packaging structure, a material of the second barrier layer is the same as or different from a material of the first barrier layer.
[0021] Optionally, in the chip packaging structure, the first barrier layer and the second barrier layer are both made of solder resist layers.
[0022] Optionally, in the chip packaging structure, the number of the filter chips and the number of the non-filter chips are one or more respectively, and the number of the filter-carrying areas and the number of the non-filter-carrying areas are one or more respectively.
[0023] The present invention also provides a chip packaging method, the chip packaging method comprising:
[0024] Providing a substrate, the substrate comprising a filter-carrying area, a non-filter-carrying area, and an aisle area surrounding the filter-carrying area and the non-filter-carrying area, a first solder pad and a second solder pad being formed on the substrate, the first solder pad being located in the filter-carrying area, and the second solder pad being located in the non-filter-carrying area;
[0025] forming a first barrier layer on the substrate, wherein the first barrier layer has a window and an opening penetrating in a thickness direction, wherein the window exposes the substrate and the second pad in the non-filter carrying area and a portion of the substrate in the aisle area surrounding the non-filter carrying area, and the opening exposes the first pad;
[0026] forming a second barrier layer on the first barrier layer, wherein the second barrier layer is located at an edge of the first barrier layer close to the window;
[0027] A filter chip is connected to the filter bearing area, wherein the filter chip includes a first substrate, an interdigital transducer formed on the first substrate, and a first bump formed on the first substrate, the interdigital transducer faces the first barrier layer, the first bump is electrically connected to the first pad, and a first cavity is formed below the filter chip;
[0028] A non-filter chip is connected to the non-filter bearing area, wherein the non-filter chip includes a second substrate and a second bump formed on the second substrate, the second bump is electrically connected to the second pad, a second cavity is formed below the non-filter chip, and the window is connected to the second cavity;
[0029] forming a coating covering the filter chip, the non-filter chip, the first barrier layer and the second barrier layer, wherein the coating closes the first cavity and is broken at a position of the second barrier layer near the window to form a fracture; and,
[0030] A plastic sealing layer is formed to cover the surface of the coating, and the plastic sealing layer also passes through the fracture to fill the window and the second cavity.
[0031] Optionally, in the chip packaging method, the fracture is formed in the coating by using a laser process.
[0032] Optionally, in the chip packaging method, the plastic sealing layer is formed by using a low-pressure plastic sealing process, and the pressure of the low-pressure plastic sealing process is less than 4T.
[0033] In the chip packaging structure and chip packaging method provided by the present invention, the first barrier layer has a window, and the window exposes the substrate and the second solder pad of the non-filter bearing area and the substrate of the partial aisle area surrounding the non-filter bearing area. A second barrier layer is formed on the first barrier layer and the second barrier layer is located at the edge of the first barrier layer close to the window. Therefore, the coating can close the first cavity under the filter chip and easily break at the second barrier layer close to the window to form a fracture. The plastic sealing layer will fill the window and the second cavity through the fracture, that is, fill the space at the bottom of the non-filter chip, thereby ensuring the operation of the filter chip and solving the problem that the reliability of the non-filter device cannot be guaranteed due to the lack of plastic sealing material filling, thereby improving the reliability of the chip packaging structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 It is a schematic flow chart of a chip packaging method according to an embodiment of the present invention.
[0035] Figure 2 It is a schematic cross-sectional view of a device in which a first barrier layer and a second barrier layer are formed according to an embodiment of the present invention.
[0036] Figure 3 It is a schematic top view of a device in which a first barrier layer and a second barrier layer are formed according to an embodiment of the present invention.
[0037] Figure 4 It is a schematic cross-sectional view of a device connecting a filter chip and a non-filter chip according to an embodiment of the present invention.
[0038] Figure 5 It is a schematic cross-sectional view of a device with a coating formed thereon according to an embodiment of the present invention.
[0039] Figure 6 It is a cross-sectional schematic diagram of a chip packaging structure according to an embodiment of the present invention.
[0040] The reference numerals are described as follows:
[0041] 10-chip packaging structure; 100-substrate; 110-filter carrying area; 120-non-filter carrying area; 130-aisle area; 140-first solder pad; 150-second solder pad; 200-first barrier layer; 210-window; 220-opening; 300-second barrier layer; 400-filter chip; 410-first substrate; 420-interdigital transducer; 430-first bump; 440-first cavity; 500-non-filter chip; 510-second substrate; 520-second bump; 530-second cavity; 600-film; 610-fracture; 700-plastic layer.
[0042] H-distance; W-width. DETAILED DESCRIPTION
[0043] The chip packaging structure and chip packaging method proposed in the present invention are further described in detail below in conjunction with the accompanying drawings and specific embodiments. The advantages and features of the present invention will become clearer according to the following description. It should be noted that the accompanying drawings are all in a very simplified form and are not in precise proportions, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.
[0044] The terms used in the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. Unless otherwise defined in the present application document, the technical terms or scientific terms used in the present invention should be the common meaning understood by people with ordinary skills in the field to which the present invention belongs. The words "first", "second" and similar words used in the present specification and claims do not indicate any order, quantity or importance, but are only used to distinguish different components. Similarly, words such as "one" or "one" do not indicate a quantitative limit, but indicate that there is at least one. "Multiple" or "several" means two or more. Unless otherwise specified, words such as "upper / upper layer" and / or "lower / lower layer" are only for convenience of explanation and are not limited to one position or one spatial orientation. Words such as "include" or "comprise" mean that the elements or structures appearing in front of "include" or "comprise" include the elements or structures listed after "include" or "comprise" and their equivalents, and do not exclude other elements or structures. Words such as "connect" or "connected" are not limited to physical or mechanical connections, and can include electrical connections, whether direct or indirect. The singular forms "a", "said" and "the" used in the present specification and the appended claims are also intended to include the plural forms, unless the context clearly indicates otherwise. It should also be understood that the term "and / or" used herein refers to and includes any or all possible combinations of one or more of the associated listed items.
[0045] The core idea of the present invention is to provide a chip packaging structure and a chip packaging method, wherein the first barrier layer has a window, the window exposes the substrate and the second solder pad of the non-filter bearing area and the substrate of the partial aisle area surrounding the non-filter bearing area, and a second barrier layer is formed on the first barrier layer and the second barrier layer is located at the edge of the first barrier layer close to the window, thereby the coating can close the first cavity under the filter chip and can be easily broken at the second barrier layer close to the window to form a fracture, and the plastic sealing layer will fill the window and the second cavity through the fracture, that is, fill the space at the bottom of the non-filter chip, thereby ensuring the operation of the filter chip and solving the problem that the reliability of the non-filter device cannot be guaranteed due to the lack of plastic sealing material filling, thereby improving the reliability of the chip packaging structure.
[0046] For details, please refer to Figure 1 , which is a schematic diagram of the process of the chip packaging method according to an embodiment of the present invention. Figure 1 As shown, in the embodiment of the present application, the chip packaging method specifically includes the following steps:
[0047] Step S10: providing a substrate, the substrate comprising a filter-bearing area, a non-filter-bearing area, and an aisle area surrounding the filter-bearing area and the non-filter-bearing area, a first solder pad and a second solder pad being formed on the substrate, the first solder pad being located in the filter-bearing area, and the second solder pad being located in the non-filter-bearing area;
[0048] Step S20: forming a first barrier layer on the substrate, wherein the first barrier layer has a window and an opening penetrating in a thickness direction, wherein the window exposes the substrate and the second pad in the non-filter bearing area and a portion of the substrate in the aisle area surrounding the non-filter bearing area, and the opening exposes the first pad;
[0049] Step S30: forming a second barrier layer on the first barrier layer, wherein the second barrier layer is located at an edge of the first barrier layer close to the window;
[0050] Step S40: connecting a filter chip on the filter bearing area, the filter chip comprising a first substrate, an IDT formed on the first substrate, and a first bump formed on the first substrate, the IDT facing the first barrier layer, the first bump and the first pad being electrically connected, and a first cavity being formed below the filter chip;
[0051] Step S50: connecting a non-filter chip on the non-filter bearing area, wherein the non-filter chip includes a second substrate and a second bump formed on the second substrate, the second bump is electrically connected to the second pad, a second cavity is formed below the non-filter chip, and the window is connected to the second cavity;
[0052] Step S60: forming a coating covering the filter chip, the non-filter chip, the first barrier layer and the second barrier layer, wherein the coating seals the first cavity and is broken near the window in the second barrier layer to form a fracture; and
[0053] Step S70: forming a plastic sealing layer covering the surface of the coating, wherein the plastic sealing layer also passes through the fracture and fills the window and the second cavity.
[0054] For further information, please refer to Figures 2 to 6 ,in, Figure 2 is a schematic cross-sectional view of a device having a first barrier layer and a second barrier layer formed thereon according to an embodiment of the present invention; Figure 3 is a schematic top view of a device in which a first barrier layer and a second barrier layer are formed according to an embodiment of the present invention; Figure 4 is a schematic cross-sectional view of a device in which a filter chip and a non-filter chip are connected according to an embodiment of the present invention; Figure 5 is a schematic cross-sectional view of a device with a coating formed thereon according to an embodiment of the present invention; Figure 6 It is a cross-sectional schematic diagram of a chip packaging structure according to an embodiment of the present invention.
[0055] like Figure 2 As shown, in an embodiment of the present application, a substrate 100 is first provided, and the material of the substrate 100 can be, for example, semiconductor, resin, ceramic or glass. Here, the substrate 100 includes a filter bearing area 110 for bearing a filter chip, a non-filter bearing area 120 for bearing a non-filter chip, and an aisle area 130 surrounding the filter bearing area 110 and the non-filter bearing area 120. In an embodiment of the present application, the filter bearing area 110 and the non-filter bearing area 120 are spaced by the aisle area 130, and further, the filter bearing area 110 is located in the aisle area 130 and the non-filter bearing area 120 is located in the aisle area 130. In this way, it can not only ensure the convenience of subsequent connection of the filter chip or the non-filter chip, but also improve the reliability of the connection, so that the plastic encapsulation layer formed subsequently can cover the surface of the filter chip and the non-filter chip, and improve the protection of the filter chip and the non-filter chip.
[0056] Furthermore, the substrate 100 may include one or more filter-carrying areas 110 to be connected to one or more filter chips. Similarly, the substrate 100 may include one or more non-filter-carrying areas 120 to be connected to one or more non-filter chips.
[0057] Among them, the filter bearing area 110 is the same as the projection of the filter chip to be connected on the substrate 100; or it is larger than the projection of the filter chip to be connected on the substrate 100, that is, each boundary of the projection of the filter chip to be connected on the substrate 100 coincides with the corresponding boundary of the filter bearing area 110 or is located in the filter bearing area 110. Similarly, the non-filter bearing area 120 is the same as the projection of the non-filter chip to be connected on the substrate 100; or it is larger than the projection of the non-filter chip to be connected on the substrate 100, that is, each boundary of the projection of the non-filter chip to be connected on the substrate 100 coincides with the corresponding boundary of the non-filter bearing area 120 or is located in the non-filter bearing area 120. In the embodiment of the present application, the filter bearing area 110 is the same as the projection of the filter chip to be connected on the substrate 100, that is, the two coincide; the non-filter bearing area 120 is the same as the projection of the non-filter chip to be connected on the substrate 100, that is, the two coincide.
[0058] Please continue to refer to Figure 2 In the embodiment of the present application, a first solder pad 140 and a second solder pad 150 are formed on the substrate 100, wherein the first solder pad 140 is located in the filter bearing area 110, and the second solder pad 150 is located in the non-filter bearing area 120. Wherein, when the substrate 100 includes a plurality of filter bearing areas 110 or a plurality of non-filter bearing areas 120, each filter bearing area 110 is formed with the first solder pad 140, and each non-filter bearing area 120 is formed with the second solder pad 150. The material of the first solder pad 140 and the second solder pad 150 is metal, for example, the material of the first solder pad 140 and the second solder pad 150 is tin. Further, the number of the first solder pad 140 on each filter bearing area 110 can be multiple and can be arranged in a desired manner, and the number of the second solder pad 150 on each non-filter bearing area 120 can also be multiple and can be arranged in a desired manner, and the present application does not limit this.
[0059] Please refer to Figure 3In the embodiment of the present application, the shapes of the first pad 140 and the second pad 150 are both circular. In other embodiments of the present application, they may also be other shapes, such as square. Here, four first pads 140 are formed on the filter bearing area 110, and the four first pads 140 are arranged in a rectangular shape; four second pads 150 are formed on the non-filter bearing area 120, and the four second pads 150 are also arranged in a rectangular shape. In other embodiments of the present application, the first pad 140 and the second pad 150 may also be arranged in other forms, which is not limited in the present application.
[0060] Please continue to refer to Figure 2 Then, a first barrier layer 200 is formed on the substrate 100. The first barrier layer 200 has a window 210 and an opening 220 that penetrate in the thickness direction. The window 210 exposes the substrate 100 and the second pad 150 in the non-filter bearing area 120 and the substrate 100 in the passage area 130 surrounding the non-filter bearing area 120. The opening 220 exposes the first pad 140. That is, the window 210 is larger than the non-filter bearing area 120. In the embodiment of the present application, each boundary of the non-filter bearing area 120 is located within the window 210.
[0061] For further information, please refer to Figure 3 , one window 210 corresponds to one non-filter bearing area 120. Accordingly, when the substrate 100 includes a plurality of non-filter bearing areas 120, a plurality of windows 210 are formed in the first barrier layer 200, and the windows 210 correspond to the non-filter bearing areas 120 one by one. Preferably, the windows 210 expose all the second pads 150 on the corresponding non-filter bearing areas 120.
[0062] Preferably, the distance H between at least one boundary of the window 210 and the corresponding boundary of the non-filter bearing area 120 is greater than or equal to 10 μm. More preferably, the distance H between each boundary of the window 210 and the corresponding boundary of the non-filter bearing area 120 is greater than or equal to 10 μm. Figure 3 As shown, in the embodiment of the present application, the non-filter bearing area 120 and the window 210 are both rectangular. The distances between the corresponding boundaries of the window 210 and the non-filter bearing area 120 may be equal or unequal. In the embodiment of the present application, the distances between the corresponding boundaries of the window 210 and the non-filter bearing area 120 are equal.
[0063] In other embodiments of the present application, the distance H between at least one boundary of the window 210 and the corresponding boundary of the non-filter bearing area 120 can also be determined according to the coating and plastic encapsulation layer to be formed subsequently. Specifically, the thickness of the coating to be formed is H1, the particle size in the plastic encapsulation layer to be formed is H2, and the distance H between at least one boundary of the window 210 and the corresponding boundary of the non-filter bearing area 120 is greater than or equal to H1+2H2. There will be particle fillers in the plastic encapsulation layer, and the boundary size that allows the particles to pass through is retained here, which is conducive to the subsequent plastic encapsulation layer filling the space at the bottom of the non-filter chip.
[0064] like Figure 2 and Figure 3 As shown, here, there are multiple openings 220, and one opening 220 correspondingly exposes one first pad 140. The opening 220 may expose part or all of the corresponding first pad 140. In the embodiment of the present application, each opening 220 exposes and only exposes part or all of the corresponding first pad 140.
[0065] In the embodiment of the present application, specifically, a first barrier material layer (not shown in the figure) may be formed first, and the first barrier material layer covers the entire upper surface of the substrate 100; then, a portion of the first barrier material layer may be removed by semiconductor processes such as etching and ashing to form the window 210 and the opening 220, thereby obtaining the first barrier layer 200. The material of the first barrier layer 200 is preferably a solder resist layer; in other embodiments of the present application, the material of the first barrier layer 200 may also be other materials, such as a dielectric material.
[0066] like Figure 2 As shown, then, a second barrier layer 300 is formed on the first barrier layer 200, and the second barrier layer 300 is located at the edge of the first barrier layer 200 close to the window 210. In the embodiment of the present application, the second barrier layer 300 is annular and surrounds the window 210. Here, the second barrier layer 300 is in a square ring shape. In other embodiments of the present application, the second barrier layer 300 may also be in other shapes, for example, the second barrier layer 300 is irregular in shape, and has a window, and the window is aligned with the window 210. The boundary of the second barrier layer 300 may be located on the first barrier layer 200 on the aisle area 130, or may extend to the surface of the first barrier layer 200 on the filter supporting area 110, and the present application does not limit this.
[0067] In the embodiment of the present application, the second barrier layer 300 is formed only on the first barrier layer 200 aligned with the aisle area 130, and the width of the second barrier layer 300 along the surface of the substrate 100 is smaller than the width of the aisle area 130 at the corresponding position. That is, the second barrier layer 300 is formed only on the first barrier layer 200 in part of the aisle area 130, and compared with the filter bearing area 110, the second barrier layer 300 is closer to the non-filter bearing area 120. The width W of the second barrier layer 300 along the surface of the substrate 100 is greater than or equal to 50 μm, thereby improving the adhesion between the second barrier layer 300 and the first barrier layer 200.
[0068] Please continue to refer to Figure 2 In the embodiment of the present application, the boundary of the second barrier layer 300 close to the window 210 is flush with the boundary of the first barrier layer 200 close to the window 210. Thus, the contact area between the second barrier layer 300 and the first barrier layer 200 is increased, and the adhesion between the two is improved.
[0069] In other embodiments of the present application, a boundary of the second barrier layer 300 close to the window 210 may be concave or convex relative to a boundary of the first barrier layer 200 close to the window 210 .
[0070] When the boundary of the second barrier layer 300 near the window 210 is concave relative to the boundary of the first barrier layer 200 near the window 210, the second barrier layer 300 exposes a portion of the first barrier layer 200 near the window 210. Preferably, the cross-sectional width of the portion of the second barrier layer 300 exposing the first barrier layer 200 near the window 210 is smaller than the cross-sectional width of the second barrier layer 300.
[0071] When the boundary of the second barrier layer 300 near the window 210 is convex relative to the boundary of the first barrier layer 200 near the window 210, the second barrier layer 300 includes a first portion (not shown in the figure) protruding from the first barrier layer 200 and a second portion (not shown in the figure) covering the first barrier layer 200, wherein the cross-sectional width of the first portion is smaller than the cross-sectional width of the second portion. Thus, the contact area between the second barrier layer 300 and the first barrier layer 200 can be ensured, and the adhesion between the two can be ensured. Furthermore, at this time, the distance between the projection of the boundary of the second barrier layer 300 near the window 210 on the substrate 100 and the corresponding boundary of the non-filter bearing area 120 is also greater than or equal to 10 μm; or, greater than or equal to H1+2H2, so that the subsequent plastic encapsulation layer can fill the space at the bottom of the non-filter chip.
[0072] In the embodiment of the present application, the material of the second barrier layer 300 is a solder resist layer, such as green oil. Preferably, the material of the first barrier layer 200 is also a solder resist layer, such as green oil, so that the adhesion between the second barrier layer 300 and the first barrier layer 200 can be further improved, thereby improving the quality and reliability of the formed chip packaging structure.
[0073] Preferably, the thickness of the second barrier layer 300 is the same as that of the first barrier layer 200, or the thickness of the second barrier layer 300 is thicker than that of the first barrier layer 200. Thus, when a coating is subsequently formed, the coating is more easily broken at the interface between the second barrier layer and the window.
[0074] Next, please refer to Figure 4 , a filter chip 400 is connected to the filter bearing area 110 and a non-filter chip 500 is connected to the non-filter bearing area 120. The connection of the filter chip 400 to the filter bearing area 110 can be performed at the same time as the connection of the non-filter chip 500 to the non-filter bearing area 120, or the connection of the filter chip 400 to the filter bearing area 110 can be performed before the connection of the non-filter chip 500 to the non-filter bearing area 120, or the connection of the filter chip 400 to the filter bearing area 110 can be performed after the connection of the non-filter chip 500 to the non-filter bearing area 120.
[0075] Specifically, the filter chip 400 includes a first substrate 410, an IDT 420 formed on the first substrate 410, and a first bump 430 formed on the first substrate 410, wherein the first bump 430 and the IDT 420 are located on the same surface of the first substrate 410. The IDT 420 faces the first barrier layer 200, the first bump 430 is electrically connected to the first pad 140, and a first cavity 440 is formed below the filter chip 400. The first bump 430 is made of metal, for example, the first bump 430 may be a copper column, a gold ball, or a tin ball. The first bump 430 may be electrically connected to the first pad 140 by welding.
[0076] Preferably, the height of the first cavity 440 is less than or equal to 20 μm, that is, the distance between the IDT 420 and the first barrier layer 200 is greater than 0 and less than or equal to 20 μm. Thus, the cavity can be formed, the connection reliability between the filter chip 400 and the substrate 100 can be improved, and the formed chip packaging structure can be miniaturized.
[0077] The non-filter chip 500 includes a second substrate 510 and a second bump 520 formed on the second substrate 510, the second bump 520 is electrically connected to the second pad 150, a second cavity 530 is formed below the non-filter chip 500, and the window 210 is connected to the second cavity 530. In the embodiment of the present application, the window 210 covers the second cavity 530, that is, the projection of the second cavity 530 on the substrate 100 is located within the projection of the window 210 on the substrate 100.
[0078] The second bump 520 is made of metal, for example, the second bump 520 may be a copper column, a gold ball, or a solder ball. The second bump 520 may be electrically connected to the second pad 150 by welding. The non-filter chip 500 may be, for example, an antenna switch, a low noise amplifier, a capacitor, an inductor, or other conventional components that can work without a cavity, and the present application does not limit this.
[0079] The surface of the non-filter chip 500 close to the substrate 100 is lower than, equal to, or higher than the surface of the second barrier layer 300. Specifically, for example, the height of the second bump 520 can be adjusted to adjust the relationship between the lower surface of the non-filter chip 500 and the upper surface of the second barrier layer 300; or the height of the second pad 150, the thickness of the first barrier layer 200, the second barrier layer 300, etc. can also be adjusted.
[0080] Then, if Figure 5 As shown, a coating 600 covering the surface of the current device is formed. Specifically, the coating 600 covers the surfaces of the filter chip 400, the non-filter chip 500, the first barrier layer 200 and the second barrier layer 300, and the coating 600 closes the first cavity 440. The material of the coating 600 can be, for example, a PI-based or epoxy-based dry film material. Preferably, the thickness of the coating 600 is not less than the height of the first cavity 440. More preferably, the thickness of the coating 600 is the same as the height of the first cavity 440, so that the stability of the first cavity 440 can be ensured, and it can be easily broken at a position close to the window 210 to form a fracture.
[0081] Please refer to Figure 5 and Figure 6 In the embodiment of the present application, a fracture 610 is formed in the coating 600 , and the fracture 610 is located in the second barrier layer 300 near the window 210 .
[0082] In one embodiment of the present application, the fracture 610 can be formed by utilizing the deformation of the coating 600. Specifically, since the second barrier layer 300 is formed on the first barrier layer 200 and the second barrier layer 300 is located at the edge of the first barrier layer 200 close to the window 210, the deformation of the coating 600 at the second barrier layer 300 close to the window 210 will be further increased, and the coating 600 will become thinner, so that the coating 600 at this location will be easily broken to form a fracture.
[0083] In the embodiment of the present application, the fracture 610 is optionally formed in the cover film 600 by a laser process, and the fracture 610 is aligned with the spacing area between the second barrier layer 300 and the non-filter chip 500, that is, located at the second barrier layer 300 near the window 210. The fracture 610 can be formed quickly and accurately by the laser process. Furthermore, a plurality of fractures 610 can be formed around the non-filter chip 500 to facilitate the subsequent filling of the plastic encapsulation layer.
[0084] Please refer to Figure 6 Then, a plastic encapsulation layer 700 is formed to cover the surface of the coating 600. The plastic encapsulation layer 700 fills the window 210 and the second cavity 530 through the fracture 610, that is, fills the cavity between the non-filter chip 500 and the substrate 100, thereby solving the problem that the reliability of the non-filter device cannot be guaranteed due to the lack of plastic encapsulation material filling, and improving the reliability of the chip packaging structure.
[0085] Preferably, the plastic encapsulation layer 700 is formed by a low-pressure plastic encapsulation process, and the pressure of the low-pressure plastic encapsulation process is less than 4 T. Thus, the plastic encapsulation layer 700 can well fill the bottom of the non-filter chip 500 and well maintain the closed state of the first cavity 440, thereby improving the quality and reliability of the formed chip packaging structure 10.
[0086] Please continue to refer to Figure 6Accordingly, the embodiment of the present application further provides a chip packaging structure 10, the chip packaging structure 10 comprising: a substrate 100, the substrate 100 comprising a filter bearing area 110, a non-filter bearing area 120 and an aisle area 130 surrounding the filter bearing area 110 and the non-filter bearing area 120, a first solder pad 140 and a second solder pad 150 formed on the substrate 100, the first solder pad 140 being located in the filter bearing area 110, and the second solder pad 150 being located in the non-filter bearing area 120; a first barrier layer 200 formed on the substrate 100, the first barrier layer 200 A window 210 and an opening 220 are provided which penetrate in the thickness direction, wherein the window 210 exposes the substrate 100 and the second pad 150 in the non-filter bearing area 120 and the substrate 100 in the passage area 130 which surrounds the non-filter bearing area 120, and the opening 220 exposes the first pad 140; a second barrier layer 300 is formed on the first barrier layer 200, and the second barrier layer 300 is located at an edge position of the first barrier layer 200 close to the window 210; a filter chip 400 is aligned with the filter bearing area 110, and the filter chip 400 includes The filter chip 400 includes a first substrate 410, an interdigital transducer 420 formed on the first substrate 410, and a first bump 430 formed on the first substrate 410, wherein the interdigital transducer 420 faces the first barrier layer 200, the first bump 430 is electrically connected to the first pad 140, and a first cavity 440 is formed below the filter chip 400; a non-filter chip 500 aligned with the non-filter bearing area 120, the non-filter chip 500 includes a second substrate 510 and a second bump 520 formed on the second substrate 510, the second bump 520 is electrically connected to the second pad 150 A second cavity 530 is formed under the non-filter chip 500, and the window 210 is connected to the second cavity 530; a coating 600 covers the surface of the filter chip 400, the non-filter chip 500, the first barrier layer 200 and the second barrier layer 300, the coating 600 closes the first cavity 440 and is broken near the window 210 in the second barrier layer 300 to form a fracture 610; and a plastic sealing layer 700 covers the surface of the coating 600, and the plastic sealing layer 700 also fills the window 210 and the second cavity 530 through the fracture 610.
[0087] Further, the projection of the non-filter chip 500 on the substrate 100 overlaps with the non-filter bearing area 120, and the distance H between the boundary of the window 210 and the boundary of the non-filter bearing area 120 is greater than or equal to 10 μm. Alternatively, the thickness of the coating 600 is H1, the particle size in the plastic encapsulation layer 700 is H2, and the distance between at least one boundary of the window 210 and the corresponding boundary of the non-filter bearing area 120 is greater than or equal to H1+2H2.
[0088] Preferably, the second barrier layer 300 is annular around the window 210. The second barrier layer 300 is formed only on the first barrier layer 200 aligned with the aisle area 130, and the width W of the second barrier layer 300 along the surface of the substrate 100 is smaller than the width at the corresponding position of the aisle area 130. The width W of the second barrier layer 300 along the surface of the substrate 100 is greater than or equal to 50 μm.
[0089] The boundary of the second barrier layer 300 near the window 210 is flush with the boundary of the first barrier layer 200 near the window 210. Alternatively, the boundary of the second barrier layer 300 near the window 210 is concave or convex relative to the boundary of the first barrier layer 200 near the window 210.
[0090] In summary, it can be seen that in the chip packaging structure and chip packaging method provided in the embodiments of the present application, the first barrier layer has a window, and the window exposes the substrate and the second solder pad of the non-filter bearing area and the substrate of the partial aisle area surrounding the non-filter bearing area. A second barrier layer is formed on the first barrier layer and the second barrier layer is located at the edge of the first barrier layer close to the window. As a result, the coating can close the first cavity under the filter chip and easily break at the second barrier layer close to the window to form a fracture. The plastic sealing layer will fill the window and the second cavity through the fracture, that is, fill the space at the bottom of the non-filter chip, thereby ensuring the operation of the filter chip, and solving the problem that the reliability of the non-filter device cannot be guaranteed due to the lack of plastic sealing material filling, thereby improving the reliability of the chip packaging structure.
[0091] In the present application, references to "one embodiment" or "some embodiments" mean that features, structures, or characteristics described in conjunction with the embodiment are included in at least one embodiment, at least some embodiments, of the present application. Therefore, the appearance of the phrases "in one embodiment" or "in some embodiments" in various places of the present application does not necessarily refer to the same or the same embodiments. In addition, in one or more embodiments, features, structures, or characteristics may be combined in any suitable combination and / or sub-combination.
[0092] Although some specific embodiments of the present application have been described in detail by way of example, it will be appreciated by those skilled in the art that the above examples are for illustration only and are not intended to limit the scope of the present application. The various embodiments of the present application may be combined in any manner without departing from the spirit and scope of the present application. It will also be appreciated by those skilled in the art that various modifications may be made to the embodiments without departing from the scope and spirit of the present application. The scope of the present application is defined by the appended claims.
Claims
1. A chip packaging structure, characterized in that: The chip packaging structure comprises: A substrate, the substrate comprising a filter-carrying area, a non-filter-carrying area, and an aisle area surrounding the filter-carrying area and the non-filter-carrying area, a first solder pad and a second solder pad being formed on the substrate, the first solder pad being located in the filter-carrying area, and the second solder pad being located in the non-filter-carrying area; A first barrier layer is formed on the substrate, the first barrier layer having a window and an opening penetrating in a thickness direction, the window exposing the substrate and the second pad in the non-filter carrying area and a portion of the substrate in the aisle area surrounding the non-filter carrying area, and the opening exposing the first pad; a second barrier layer formed on the first barrier layer, wherein the second barrier layer is located at an edge of the first barrier layer close to the window; A filter chip aligned with the filter bearing area, the filter chip comprising a first substrate, an IDT formed on the first substrate, and a first bump formed on the first substrate, the IDT facing the first barrier layer, the first bump and the first pad being electrically connected, and a first cavity being formed below the filter chip; A non-filter chip aligned with the non-filter bearing area, the non-filter chip comprising a second substrate and a second bump formed on the second substrate, the second bump and the second pad are electrically connected, a second cavity is formed below the non-filter chip, and the window is connected to the second cavity; a coating covering the filter chip, the non-filter chip, the first barrier layer and the second barrier layer, the coating sealing the first cavity and breaking the second barrier layer near the window to form a fracture; and, A plastic sealing layer covers the surface of the coating, and the plastic sealing layer also passes through the fracture to fill the window and the second cavity.
2. The chip packaging structure according to claim 1, characterized in that: The thickness of the coating is H1, the particle size in the plastic encapsulation layer is H2, the projection of the non-filter chip on the substrate coincides with the non-filter bearing area, and the distance between at least one boundary of the window and the corresponding boundary of the non-filter bearing area is greater than or equal to H1+2H2.
3. The chip packaging structure according to claim 1, characterized in that: The projection of the non-filter chip on the substrate overlaps with the non-filter bearing area, and the distance between at least one boundary of the window and the corresponding boundary of the non-filter bearing area is greater than or equal to 10 μm.
4. The chip packaging structure according to claim 1, characterized in that: The second barrier layer is annularly arranged around the window.
5. The chip packaging structure according to claim 1, characterized in that: The second barrier layer is formed only on the first barrier layer aligned with the aisle region, and a width of the second barrier layer along the surface of the substrate is smaller than a width of the aisle region.
6. The chip packaging structure according to claim 1, characterized in that: The width of the second barrier layer along the surface of the substrate is greater than or equal to 50 μm.
7. The chip packaging structure according to claim 1, characterized in that: A boundary of the second barrier layer close to the window is flush with a boundary of the first barrier layer close to the window.
8. The chip packaging structure according to any one of claims 1 to 7, characterized in that: The surface of the non-filter chip close to the substrate is lower than, equal to, or higher than the surface of the second barrier layer.
9. The chip packaging structure according to any one of claims 1 to 7, characterized in that: The material of the second barrier layer is the same as or different from that of the first barrier layer.
10. The chip packaging structure according to any one of claims 1 to 7, characterized in that: The first barrier layer and the second barrier layer are both made of solder resist.
11. The chip packaging structure according to any one of claims 1 to 7, characterized in that: The number of the filter chips and the number of the non-filter chips are one or more respectively, and the number of the filter bearing area and the number of the non-filter bearing area are one or more respectively.
12. A chip packaging method, characterized in that: The chip packaging method comprises: Providing a substrate, the substrate comprising a filter-carrying area, a non-filter-carrying area, and an aisle area surrounding the filter-carrying area and the non-filter-carrying area, a first solder pad and a second solder pad being formed on the substrate, the first solder pad being located in the filter-carrying area, and the second solder pad being located in the non-filter-carrying area; forming a first barrier layer on the substrate, wherein the first barrier layer has a window and an opening penetrating in a thickness direction, wherein the window exposes the substrate and the second pad in the non-filter carrying area and a portion of the substrate in the aisle area surrounding the non-filter carrying area, and the opening exposes the first pad; forming a second barrier layer on the first barrier layer, wherein the second barrier layer is located at an edge of the first barrier layer close to the window; A filter chip is connected to the filter bearing area, wherein the filter chip includes a first substrate, an interdigital transducer formed on the first substrate, and a first bump formed on the first substrate, the interdigital transducer faces the first barrier layer, the first bump is electrically connected to the first pad, and a first cavity is formed below the filter chip; A non-filter chip is connected to the non-filter bearing area, wherein the non-filter chip includes a second substrate and a second bump formed on the second substrate, the second bump is electrically connected to the second pad, a second cavity is formed below the non-filter chip, and the window is connected to the second cavity; forming a coating covering the filter chip, the non-filter chip, the first barrier layer and the second barrier layer, wherein the coating closes the first cavity and is broken at a position of the second barrier layer near the window to form a fracture; and, A plastic sealing layer is formed to cover the surface of the coating, and the plastic sealing layer also passes through the fracture to fill the window and the second cavity.
13. The chip packaging method according to claim 12, characterized in that: The fracture is formed in the coating by using a laser process.
14. The chip packaging method according to claim 12, characterized in that: The plastic sealing layer is formed by using a low-pressure plastic sealing process, and the pressure of the low-pressure plastic sealing process is less than 4T.
Citation Information
Patent Citations
Module chip packaging structure and circuit board
CN113794461A
Chip packaging structure and packaging method
CN114530445A
Cavity filter system-level packaging module, electronic product and preparation method
CN116799456A
Chip packaging structure
CN217544617U
Chip packaging structure
CN221551882U