Power device and preparation method thereof

By using magnetic metal materials and conductors as conductive channel media in semiconductor power devices and controlling the movement of magnetic metal materials by using electric fields, the problem of poor consideration of breakdown voltage, on-resistance and switching speed of traditional devices is solved, and the problem of poor consideration of breakdown voltage, on-resistance and switching speed is improved. The stability of the device and its resistance to current and voltage shocks.

CN118969822AInactive Publication Date: 2024-11-15ASAHI SEMICON (SHANGHAI) CO LTD +1
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411442448.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-16
Publication Date
2024-11-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

While increasing the breakdown voltage, traditional semiconductor power devices are difficult to maintain low on-resistance and high switching speed, and have poor resistance to current and voltage shocks, resulting in insufficient stability and reliability.

Method used

Using magnetic metal materials and conductive bodies as conductive channels, by forming trenches on the substrate and installing magnetic metal materials therein, the movement of magnetic metal materials is controlled by using electric field changes to form or disconnect the current path, and the breakdown voltage is increased. and switching speed, and enhance resistance to current and voltage shocks.

Benefits of technology

Achieve higher breakdown voltage and lower on-resistance, improve switching speed and device stability and reliability, and can take into account the performance of breakdown voltage, on-resistance and switching speed.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118969822A_ABST
    Figure CN118969822A_ABST
Patent Text Reader

Abstract

The invention relates to a power device and a preparation method thereof, the power device comprises a substrate, a magnetic metal material, a plurality of conductors, an insulating layer, a control electrode, a first electrode and a second electrode, a plurality of grooves are formed in the substrate, the plurality of grooves extend from the surface of the substrate to the inside, and the part, with the grooves, of the substrate is divided into a plurality of insulators; the magnetic metal material is arranged in the plurality of grooves, and the thickness of the magnetic metal material is smaller than the depth of the grooves; the plurality of conductors are arranged on the plurality of insulators in a one-to-one correspondence manner; the insulating layer is positioned on the plurality of conductors and covers the plurality of grooves; the control electrode is arranged on the insulating layer and the projection is overlapped with the magnetic metal material; the first electrode and the second electrode are arranged on the insulating layer and distributed on the two sides of the control electrode, and the first electrode and the second electrode are arranged at intervals. The power device can effectively improve the withstand voltage, reduce the on-resistance and improve the switching speed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of semiconductor technology, and in particular relates to a power device and a preparation method thereof. Background Art

[0002] Power devices are a type of semiconductor device used to process and control the conversion and transmission of electrical energy. These devices are particularly suitable for high voltage, high current and high power applications. Power devices have two main functions: one is the switching function, which can perform fast switching operations in the circuit to achieve control of current or voltage; the other is the amplification function, which can amplify a small current signal into a large current signal, or amplify a small voltage signal into a large voltage signal. The main types of power devices include rectifiers, thyristors, power metal-oxide semiconductor field effect transistors (MOSFETs), insulated gate bipolar transistors (IGBTs), power operational amplifiers, etc. They play an important role in many application fields such as power systems, motors, power converters, electric vehicles, etc.

[0003] In the application field of power devices, switches are the most common and most popular power device applications. Traditional switching devices have three electrode structures: source, drain and gate, and the gate controls the current flow between the source and drain. Current power devices are usually made of semiconductor materials (such as silicon materials), and the flow of current is realized by carrier transmission in the semiconductor materials. Some key parameters of these devices, such as breakdown voltage, on-resistance and switching speed, are often contradictory due to the physical mechanism of semiconductor materials. While increasing the breakdown voltage of the device, it will also increase the on-resistance and reduce the switching speed. Even after various optimizations such as super junction, IGBT and other devices and optimized SiC new materials with balance curves such as withstand voltage and on-resistance, it is difficult to take into account the performance of withstand voltage, on-resistance and switching speed at the same time.

[0004] In addition, semiconductor devices are accompanied by a certain leakage current when in reverse cutoff, and there will also be leakage current under high temperature conditions. When encountering current and voltage shocks, such power devices are also prone to failure, which is a major defect for harsh operating environments and high-intensity work requirements.

[0005] Therefore, in traditional semiconductor devices, there is a defect that the breakdown voltage, on-resistance and switching speed cannot be optimized at the same time, and the resistance to current and voltage shocks is poor, and the stability and reliability of the device cannot be guaranteed. Summary of the invention

[0006] In order to solve the above problems existing in the prior art, the present invention provides a power device and a method for manufacturing the same. The technical problem to be solved by the present invention is achieved through the following technical solutions: An embodiment of the present invention provides a power device, including: a substrate, a magnetic metal material, a plurality of conductors, an insulating layer, a control electrode, a first electrode, and a second electrode, wherein: A plurality of grooves are formed in the substrate, and the plurality of grooves extend from the surface of the substrate to the inside, and separate the portion of the substrate having the grooves into a plurality of insulators; The magnetic metal material is disposed in the plurality of grooves, and the thickness of the magnetic metal material is smaller than the depth of the grooves; The plurality of conductors are arranged on the plurality of insulators in a one-to-one correspondence; The insulating layer is located on the plurality of conductors and covers the plurality of grooves; The control electrode is arranged on the insulating layer and its projection overlaps with the magnetic metal material; The first electrode and the second electrode are arranged on the insulating layer and distributed on both sides of the control electrode, and are spaced apart from the control electrode.

[0007] In one embodiment of the present invention, the thickness of the magnetic metal material is equal to the thickness of the conductor.

[0008] In one embodiment of the present invention, the depth of the groove is 8-10 μm.

[0009] In one embodiment of the present invention, the magnetic metal material includes one or more of magnetized aluminum metal, a single substance containing a magnetic metal, an oxide containing a magnetic metal, and an alloy containing a magnetic metal, wherein the magnetic metal includes one or more of iron, cobalt, nickel, and manganese.

[0010] In one embodiment of the present invention, the thickness of the magnetic metal material is 4-5 μm.

[0011] In one embodiment of the present invention, the material of the conductor includes one or more of metal aluminum and aluminum-copper alloy, and the thickness is 4-5 μm.

[0012] In one embodiment of the present invention, the insulating layer is made of silicon dioxide and has a thickness of 1-2 μm.

[0013] Another embodiment of the present invention provides a method for preparing a power device, comprising the steps of: Making a plurality of grooves extending from the surface of the substrate to the inside of the substrate in the substrate, and dividing the portion of the substrate having the grooves into a plurality of insulators; preparing a plurality of conductors on the plurality of insulators; Preparing a magnetic metal material inside the groove, wherein the thickness of the magnetic metal material is less than the depth of the groove; preparing an insulating layer on the plurality of conductors, and making the insulating layer cover the plurality of grooves; A control electrode, a first electrode and a second electrode are prepared on the surface of the insulating layer so that the projection of the control electrode overlaps with the magnetic metal material, and the first electrode and the second electrode are distributed on both sides of the control electrode and are spaced apart from the control electrode.

[0014] In one embodiment of the present invention, preparing a magnetic metal material inside the groove includes: The magnetic metal material is deposited inside the groove by using physical vapor deposition technology, chemical vapor deposition technology or electrochemical deposition technology.

[0015] In one embodiment of the present invention, preparing an insulating layer on the plurality of conductors and making the insulating layer cover the plurality of grooves comprises: depositing a first insulating material on the magnetic metal material in the groove; Depositing a second insulating material on the first insulating material and the plurality of conductors; A hole is opened in the second insulating material above the trench, and the first insulating material is removed by wet method to form the insulating layer.

[0016] Compared with the prior art, the present invention has the following beneficial effects: The power device of the present invention uses magnetic metal materials and conductors as conductive channel media, allowing the device to have a higher breakdown voltage and the impedance of the channel can be effectively reduced. Since the material can quickly respond to changes in the electric field, the switching speed can be increased. At the same time, since the magnetic metal material has a strong resistance to current and voltage shocks compared to silicon materials, the stability and reliability of the device are greatly improved, and the breakdown voltage, on-resistance and switching speed are taken into account. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 A schematic diagram of the structure of a power device provided by an embodiment of the present invention; Figure 2a-2i A schematic diagram of a process of a method for preparing a power device provided in an embodiment of the present invention. DETAILED DESCRIPTION

[0018] The present invention is further described in detail below with reference to specific embodiments, but the embodiments of the present invention are not limited thereto.

[0019] Embodiment 1 See also Figure 1 , Figure 1 A schematic diagram of the structure of a power device provided by an embodiment of the present invention.

[0020] The power device of this embodiment is a lateral structure device, including: a substrate 1, a magnetic metal material 2, a plurality of conductors 3, an insulating layer 4, a control electrode 5, a first electrode 6 and a second electrode 7. Among them, a plurality of grooves 11 are formed in the substrate 1, and the plurality of grooves 11 extend from the surface of the substrate 1 to the inside, and separate the portion of the substrate 1 with the grooves into a plurality of insulators 12; the magnetic metal material 2 is arranged in the plurality of grooves 11, and the thickness of the magnetic metal material 2 is less than the depth of the grooves 11; the plurality of conductors 3 are arranged on the plurality of insulators 12 in a one-to-one correspondence; the insulating layer 4 is located on the plurality of conductors 3 and covers the plurality of grooves 11; the control electrode 5 is arranged on the insulating layer 4 and its projection overlaps with the magnetic metal material 2; the first electrode 6 and the second electrode 7 are arranged on the insulating layer 4, and are distributed on both sides of the control electrode 5, and are arranged at intervals from the control electrode 5.

[0021] Specifically, a groove 11 is formed in the substrate 1, and the groove 11 separates the portion of the substrate 1 having the groove to form a plurality of insulators 12. The substrate 1, the insulator 12, the conductor 3, and the insulating layer 4 together close the groove 11 to form a cavity for accommodating the magnetic metal material 2, and the thickness of the magnetic metal material 2 is less than the depth of the groove 11. When no electric field is applied, the magnetic metal material 2 and the conductor 3 remain isolated, and the current path is disconnected at this time; when the electric field changes, the magnetic metal material 2 moves from the bottom of the groove 11 to the surface of the insulating layer 4 in the cavity, and reaches a state of contact with the conductor 3. At this time, the magnetic metal material 2 and the conductor 3 together serve as a conductive channel medium to form a current path.

[0022] Specifically, the magnetic metal material 2 in each groove 11 needs to be located below the control electrode 5, that is, the two ends of the control electrode 5 can only cover the magnetic metal material 2 in the end groove 11, or extend to the top of the end conductor 3 to fully cover the magnetic metal material 2 in multiple grooves. The first electrode 6 and the second electrode 7 are respectively arranged on both sides of the control electrode 5, not in contact with the control electrode 5, and are located above the end conductor 3.

[0023] This embodiment uses attraction and repulsion to control the switch of the device. When a voltage that attracts the magnetic metal material 2 is applied to the control electrode 5, the magnetic metal material 2 is attracted to the bottom of the insulating layer 4 by the voltage, and contacts the conductors 3 on both sides to form a current path. The potential difference between the first electrode 6 and the second electrode 7 can achieve the effect of current flow, thereby turning on the power device; when the voltage applied to the control electrode 5 is canceled or a negative voltage that repels the magnetic metal material 2 is applied to the control electrode 5 in the opposite direction, the magnetic metal material 2 falls back to the bottom of the groove, isolating from the conductor 3, the current path is disconnected, and the device is turned off.

[0024] In a specific embodiment, the thickness of the magnetic metal material 2 is equal to the thickness of the conductor 3. At this time, the conduction channel formed by the magnetic metal material 2 and the conductor 3 is in metal contact, so the conduction resistance is very small and the loss generated is correspondingly reduced.

[0025] In a specific embodiment, the substrate 1 is an N-type phosphorus-doped substrate with a resistivity of 0.001~0.004ohm. The depth of the groove 11 is 8~10μm. The magnetic metal material 2 includes one or more of magnetized aluminum metal, a single substance containing a magnetic metal, an oxide containing a magnetic metal, and an alloy containing a magnetic metal, wherein the magnetic metal includes one or more of iron, cobalt, nickel, and manganese. The thickness of the magnetic metal material 2 is 4~5μm. The material of the conductor 3 includes one or more of metal aluminum and aluminum-copper alloy, with a thickness of 4~5μm. The material of the insulating layer 4 includes silicon dioxide, with a thickness of 1~2μm. The material of the control electrode 5, the first electrode 6, and the second electrode 7 can be one or more of conductive polysilicon and metal Al material, with a thickness of 4~8μm.

[0026] For the lateral power device of this embodiment, when the device thickness is relatively thin, the withstand voltage of the device can be increased by increasing the length of the first electrode and the second electrode. That is, the power device of this embodiment can increase the withstand voltage without increasing the chip thickness, and can effectively ensure the control of the control pole over the magnetic metal material, ensure the stability and reliability of the device operation, and is conducive to the production of high-voltage devices.

[0027] The power device of this embodiment uses magnetic metal materials and conductors as conductive channel media, allowing the device to have a higher breakdown voltage, and the impedance of the channel can also be effectively reduced. Since the material can quickly respond to changes in the electric field, the switching speed can be increased. At the same time, since the magnetic metal material has a strong resistance to current and voltage shocks compared to silicon materials, it can effectively improve the device's tolerance to voltage and current, greatly improving the stability and reliability of the device. Therefore, the power device can effectively improve the withstand voltage, reduce the on-resistance, and increase the switching speed, achieving a balance between breakdown voltage, on-resistance, and switching speed.

[0028] Embodiment 2 Based on the first embodiment, this embodiment provides a method for preparing a power device.

[0029] See also Figure 2a-2i , Figure 2a-2i A schematic diagram of a process of manufacturing a power device provided in an embodiment of the present invention. The method of manufacturing a power device in this embodiment comprises the following steps: S1. A plurality of grooves 11 extending from the surface of the substrate 1 to the inside are made in the substrate 1, and the portion of the substrate 1 having the grooves is separated into a plurality of insulators 12, such as Figure 2a and Figure 2b shown.

[0030] Specifically, a plurality of grooves 11 with a depth of 8 to 10 μm and spaced apart are etched in the substrate 1 by photolithography, etching and other techniques for subsequent placement of magnetic metal materials. The plurality of grooves 11 separate a portion of the substrate 1 to form a plurality of insulators 12 .

[0031] S2, preparing a plurality of conductors 3 on a plurality of insulators 12, such as Figure 2c shown.

[0032] Specifically, metal aluminum or aluminum-copper alloy is deposited on the surface of a number of insulators 12 and in a number of grooves 11 by using deposition techniques such as physical vapor deposition, chemical vapor deposition, and electrochemical deposition; then, the metal aluminum or aluminum-copper alloy in the grooves 11 is etched away by using processes such as wet etching or dry etching (such as plasma etching) to obtain an electric conductor 3 located on the surface of the insulator 12, and the thickness of the electric conductor 3 is 4~5μm.

[0033] S3, preparing a magnetic metal material 2 inside the groove 11, wherein the thickness of the magnetic metal material 2 is less than the depth of the groove 11, such as Figure 2d shown.

[0034] Specifically, the magnetic metal material 2 is deposited as the conductive channel medium in the groove 11 by using deposition techniques such as physical vapor deposition, chemical vapor deposition, and electrochemical deposition, with a deposition thickness of 4 to 5 μm. It can be understood that the formed magnetic metal material 2 is an integral block structure.

[0035] The magnetic metal material 2 includes one or more of magnetized aluminum metal, a single substance containing magnetic metal, an oxide containing magnetic metal, and an alloy containing magnetic metal, wherein the magnetic metal includes one or more of iron, cobalt, nickel, and manganese. Exemplarily, magnetized aluminum metal is used as the magnetic metal material. Magnetized aluminum metal is compatible with existing wafer processing technology, has a simple preparation process, and is low in cost.

[0036] S4. Prepare an insulating layer 4 on the plurality of conductors 3 , and make the insulating layer 4 cover the plurality of grooves 11 .

[0037] Specifically, first, a first insulating material 10 is deposited on the magnetic metal material 2 in the groove 11, so that the first insulating material 10 fills the groove 11 and the surface of the first insulating material 10 is flush with the surface of the conductor 3; the first insulating material 10 can be SiN or an organic polyimide material, such as Figure 2e shown.

[0038] Then, a second insulating material is deposited on the first insulating material 10 and the conductor 3 as an insulating layer 4. The second insulating material may be silicon dioxide and may have a thickness of 1 to 2 μm. Figure 2f shown.

[0039] Finally, a hole 41 is opened in the second insulating material above the trench 11 by photolithography, dry etching and other processes. The width of the hole 41 is less than 0.1 μm and is located at the edge of the active area. Figure 2g As shown, the chemical liquid is passed through the hole 41 into the groove, and the first insulating material 10 is removed by wet method to form an insulating layer 4, which is used to isolate the surface electrode and protect the magnetic metal material 2. Figure 2h shown.

[0040] S5. Prepare a control electrode 5, a first electrode 6 and a second electrode 7 on the surface of the insulating layer 4 so that the projection of the control electrode 5 overlaps with the magnetic metal material 2, and the first electrode 6 and the second electrode 7 are distributed on both sides of the control electrode 5 and are spaced apart from the control electrode 5.

[0041] Specifically, an electrode material is deposited on the surface of the insulating layer 4. The electrode material may be conductive polysilicon or metal Al material with a thickness of 4 to 8 μm. The deposited electrode material may completely cover the hole 41. The control electrode 5, the first electrode 6 and the second electrode 7 are manufactured by photolithography, etching and other process technologies, so that the projection of the control electrode 5 overlaps with the magnetic metal material 2, and the first electrode 6 and the second electrode 7 are distributed on both sides of the control electrode 5 and are spaced apart from the control electrode 5, as shown in FIG. Figure 2i As shown. Thus, a power device is prepared.

[0042] In the description of the present invention, it should be understood that the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0043] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0044] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification.

[0045] Although the present application is described herein in conjunction with various embodiments, in the process of implementing the claimed application, those skilled in the art may understand and implement other variations of the disclosed embodiments by viewing the drawings, the disclosure, and the appended claims. In the claims, the word "comprising" does not exclude other components or steps, and "a" or "an" does not exclude a plurality of components. Certain measures are recorded in different dependent claims, but this does not mean that these measures cannot be combined to produce good results.

[0046] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the scope of protection of the present invention.

Claims

1. A power device, characterized in that: include: A substrate, a magnetic metal material, a plurality of conductors, an insulating layer, a control electrode, a first electrode and a second electrode, wherein: A plurality of grooves are formed in the substrate, and the plurality of grooves extend from the surface of the substrate to the inside, and separate the portion of the substrate having the grooves into a plurality of insulators; The magnetic metal material is disposed in the plurality of grooves, and the thickness of the magnetic metal material is smaller than the depth of the grooves; The plurality of conductors are arranged on the plurality of insulators in a one-to-one correspondence; The insulating layer is located on the plurality of conductors and covers the plurality of grooves; The control electrode is arranged on the insulating layer and its projection overlaps with the magnetic metal material; The first electrode and the second electrode are arranged on the insulating layer and distributed on both sides of the control electrode, and are spaced apart from the control electrode.

2. The power device according to claim 1, characterized in that: The thickness of the magnetic metal material is equal to the thickness of the electrical conductor.

3. The power device according to claim 1, characterized in that: The depth of the groove is 8-10 μm.

4. The power device according to claim 1, characterized in that: The magnetic metal material includes one or more of magnetized aluminum metal, a single substance containing a magnetic metal, an oxide containing a magnetic metal, and an alloy containing a magnetic metal, wherein the magnetic metal includes one or more of iron, cobalt, nickel, and manganese.

5. The power device according to claim 1, characterized in that: The thickness of the magnetic metal material is 4-5 μm.

6. The power device according to claim 1, characterized in that: The material of the conductor includes one or more of metal aluminum and aluminum-copper alloy, and the thickness is 4-5 μm.

7. The power device according to claim 1, characterized in that: The insulating layer is made of silicon dioxide and has a thickness of 1-2 μm.

8. A method for preparing a power device, characterized in that: Includes steps: Making a plurality of grooves extending from the surface of the substrate to the inside of the substrate in the substrate, and dividing the portion of the substrate having the grooves into a plurality of insulators; preparing a plurality of conductors on the plurality of insulators; Preparing a magnetic metal material inside the groove, wherein the thickness of the magnetic metal material is less than the depth of the groove; preparing an insulating layer on the plurality of conductors, and making the insulating layer cover the plurality of grooves; A control electrode, a first electrode and a second electrode are prepared on the surface of the insulating layer so that the projection of the control electrode overlaps with the magnetic metal material, and the first electrode and the second electrode are distributed on both sides of the control electrode and are spaced apart from the control electrode.

9. The method for preparing a power device according to claim 8, characterized in that: The magnetic metal material is prepared inside the groove, comprising: The magnetic metal material is deposited inside the groove by using physical vapor deposition technology, chemical vapor deposition technology or electrochemical deposition technology.

10. The method for preparing a power device according to claim 8, characterized in that: Preparing an insulating layer on the plurality of conductors so that the insulating layer covers the plurality of grooves, comprising: depositing a first insulating material on the magnetic metal material in the groove; Depositing a second insulating material on the first insulating material and the plurality of conductors; A hole is opened in the second insulating material above the trench, and the first insulating material is removed by wet method to form the insulating layer.

Citation Information

Patent Citations

  • High-speed, high-durability and low-fluctuation FeFET and preparation method thereof

    CN114361257A

  • Power device, manufacturing method and using method thereof

    CN118401090A

  • Film actuator based mems device and method