Screen drum with axially variable wear-resistant coating thickness
By applying a thicker wear-resistant coating on the wedge-shaped screw of the pulp screen barrel, especially at the outflow end, the problem of uneven wear is solved, extending the service life of the screen barrel and improving efficiency.
Patent Information
- Application Number
- CN202480002084.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-01-23
- Filing Date
- 2024-01-19
- Publication Date
- 2024-11-15
AI Technical Summary
The existing pulp screen barrels wear unevenly during use, especially the surface of the wedge-shaped screw near the outflow end wears faster, resulting in premature wear and frequent replacement of the screening medium, which affects efficiency and life.
Using a cylindrical screening medium with inflow and outflow sides, a wear-resistant coating is applied to the axially extending wedge screw, which is thicker at the outflow end, and is applied evenly by spraying techniques to reduce wear and ensure groove width and Uniformity of screw profile.
It extends the service life of the screen barrel, reduces wear, improves screening efficiency, avoids unnecessary replacement, and maintains the performance and efficiency of the screen barrel.
Smart Images

Figure CN118974349A_ABST
Abstract
Description
[0001] This application claims priority to International Application No. PCT / IB2023 / 050553, filed on January 23, 2023. The entire disclosure of that application is incorporated herein by reference. Field of the Invention
[0002] The present application relates generally to screen cylinders for removing oversized solid contaminants from solid-liquid suspensions such as pulp, and particularly to screen cylinders having improved wear characteristics and methods of making and using the same. Technical Background
[0003] Papermaking involves the processing or production of pulp, which is a solid-liquid suspension of fibers (e.g., cellulose fibers or other fibers). Pulp typically contains various contaminants, such as wood chips, fiber bundles, metal flakes, hardened adhesives or other contaminants. This is especially true when paper is made from recycled paper as the source of pulp, because hardened adhesives, metal fragments and plastic particles may be easily present in such recycled pulp. If these contaminants are not removed, the quality of the paper may be reduced and / or the papermaking process may be disturbed.
[0004] To remove contaminants including oversized particles or fibers, pulp is typically screened. Screening can also be used to fractionate pulp into streams having different fiber size distributions. Pulp screening can be accomplished by introducing the pulp into a pulp screen where an acceptable portion of the pulp passes through openings, such as slots, in the screen. Oversized solid contaminants or other unacceptable portions of the pulp will not pass through the slots or openings in the screen and will be discharged from the outflow end of the screen via an outlet as rejects. Pulp screens can also be used to remove oversized and other solid contaminants from slurries and solid suspensions other than pulp.
[0005] Pulp screening can be done using a screen cylinder located in a pulp screen. The screen cylinder can screen various types of fibers, such as but not limited to cellulose fibers, cotton fibers, glass fibers or other fibers. The screen cylinder can be an inflow screen cylinder or an outflow screen cylinder, in which the acceptable portion of the solid suspension flows radially inward through the screen cylinder, and in which the acceptable portion of the solid suspension flows radially outward through the screen cylinder. The pulp screen may include a rotor or other device that is operable to accelerate the pulp suspension to produce desired flow conditions at the entrance of the holes in the screen cylinder, and to produce pressure pulsations that backwash the blockage from the screen cylinder holes. Each of these behaviors promotes acceptable pulp to pass through the screen slot while limiting contaminants and undesirable pulp from passing through the screen slot. Some screen cylinders utilize solid metal cylinders through which multiple holes or slots are drilled or milled. However, in order to increase the throughput of the pulp screening process, pulp screening generally preferably includes a screen cylinder with multiple longitudinally arranged wavy wedge screws, between which multiple narrow slots extending over most of the length of the screen cylinder are formed.
[0006] These wedge wire screen cylinders are typically made by arranging a plurality of wedge wire rods into a cylindrical shape. The slots formed between the wedge wire rods allow the desired pulp to pass therethrough while preventing the undesired pulp or other contaminants from also passing therethrough. Thus, the slot size of the screen cylinder is selected based on the pulp parameters and such desired results. However, pulp is abrasive, causing the screen cylinder and the rods forming the screen cylinder to wear after a period of use. Wear of the screen cylinder may affect the performance and / or efficiency of the screen cylinder.
[0007] The rods forming the slots in the screen cylinder are coated with wear-resistant coatings such as chromium to help minimize the wear of the rods and the screen cylinder. The chromium coating is applied by an electroplating process, in which the screen cylinder is in a bath of chromic acid and other chemical components. The screen cylinder acts as a cathode during the electroplating process, and chromium is therefore deposited on the wedge-shaped steel wire strip. However, due to the variability of various factors in the electroplating process, including the gap between the current, the acid bath temperature, the anode and the cathode (i.e., the screen cylinder) and the chemical strength of the acid bath, the chromium coating may be difficult to be constantly applied to the surface of the screw rod. In addition, the wear-resistant coating can be applied to the screw rod by known coating or spraying methods, such as but not limited to high-speed oxygen fuel (HVOF) spraying, plasma spraying, laser spraying, chemical vapor deposition (CVD), physical vapor deposition (PVD) and atomic layer deposition (ALD).
[0008] In any case, screen drums tend to wear unevenly, and most typically, the majority of the wear occurs at the outflow end of the drum. The outflow end of the drum, toward or near the reject outlet, may wear at a greater rate than the inflow end of the drum due to the higher concentration of rejects flowing at the outflow end of the drum. It is not uncommon for a drum to wear prematurely because the surface of the wedge-shaped screw rods near the outflow end have worn while the surface of the same rods near the inflow end has not yet worn. In such cases, it may be necessary to replace the screening media of the entire drum, even though only the end near its outflow end has worn.
[0009] Therefore, it is desirable to achieve a screen cylinder having a screening medium that resists wear at an increased rate toward the outflow end of the screen cylinder and at the surface of the wedge-shaped screw near the outflow end. In addition, it is desirable to utilize a wear-resistant coating that can be applied by spraying without negatively affecting certain characteristics of the screening medium, such as the uniformity of the slot width and the profile of the screw. Summary of the invention
[0010] Therefore, there is a continuing need for a screen cylinder having a wear-resistant coating, wherein the coating is preferentially applied to specific desired locations of the screw and / or portion of the screen cylinder, such as a thicker coating at or near the outflow end of the screen cylinder, without negatively affecting certain characteristics of the screening medium, such as the uniformity of the slot width and the profile of the screw. In addition, it is preferred that the use of any coating results in a substantially uniform thickness of the coating in a cross-section of the width of the screw in the direction of the inflow surface of the screw when viewed from the axial direction. Therefore, this uniformity will not significantly change the profile of the inflow surface along the screw when viewed from this direction.
[0011] According to one or more aspects, the screen drum includes a cylindrical screening medium having an inflow side and an outflow side. The screening medium is formed by a plurality of axially extending and circumferentially spaced grooves, which are formed between axially extending wedge-shaped screws. The axially extending screw of the screening medium has an inflow surface facing the inflow side. The screen drum and the screening medium have an inflow end and an outflow end axially opposite to the inflow end. The axially extending screw includes a wear-resistant coating on the inflow surface of the screening medium. Compared with the wear-resistant coating on the screw toward the inflow end of the screening medium, the wear-resistant coating on the screw toward the outflow end of the screening medium is thicker. Compared with the coating on each rod located near the inflow end of the screening medium, the wear-resistant coating of each rod in the screen drum toward the outflow end of the screening medium is thicker. The wear-resistant coating forms a substantially uniform coating area between an area on the inflow surface of the rod near the first slot and an area on the inflow surface of the rod near the second slot. The substantially uniform coating region at multiple axial positions of the rod has a substantially uniform thickness along the inflow surface in a circumferential direction perpendicular to the axial direction, while the thickness of the substantially uniform coating region increases along the axial direction or along multiple axial positions of the rod. Preferably, the wear resistant coating is a sprayed wear resistant coating having a harder hardness than the substrate. The wear resistant coating is typically a high velocity oxygen fuel coating and is preferably formed of a uniform layer of a single coating, which may be formed of multiple sub-layers, each of which has a similar coating material, without using other coatings including, for example, chromium.
[0012] The screen drum may include a plurality of profiled wedge screw rods that are longitudinally aligned and connected to at least one support ring at the attachment end of the rod. The length of each rod generally extends the length of the screen drum. Each rod includes an inflow surface away from at least one support ring, a first slot surface extending from the inflow surface to the attachment end of the rod opposite to the inflow surface, and a second slot surface opposite to the first slot surface and extending from the first slot surface to the attachment end of the rod. The first slot surface of a rod and the second slot surface of another adjacent rod can define a slot. A spray nozzle can be used to apply a wear-resistant coating to the inflow surface of the rod by passing the spray nozzle along the length of the rod multiple times when the screen drum rotates or between the incremental rotations of the screen drum, thereby causing the wear-resistant coating to be sprayed onto the inflow surface of the rod during the nozzle passing in the spray channel of the spray nozzle. The wear-resistant coating forms a substantially uniform coating area between an area on the inflow surface of the rod near the first slot and an area on the inflow surface of the rod near the second slot. The substantially uniform coating area at multiple axial positions of the rod has a substantially uniform thickness along the inflow surface in a circumferential direction perpendicular to the axial direction, while the thickness of the substantially uniform coating area increases at multiple axial positions or along the rod along the axial direction. The wear-resistant coating is applied thicker on the rod toward the outflow end of the screening medium than on the rod toward the inflow end of the screening medium. In other words, the wear-resistant coating on each and all rods of the screen drum has a coating whose thickness increases toward the outflow end of the screen drum.
[0013] According to another aspect of the present disclosure, a method for manufacturing a screen drum is provided. The method includes forming a cylindrical screening medium having an inflow side and an outflow side when the screening medium has a plurality of circumferentially spaced axially extending grooves formed between axially extending rods, and the axially extending rods of the screening medium have an inflow surface facing the inflow portion. The screen drum and the screening medium include an inflow end and an outflow end axially opposite to the inflow end. The method also includes applying a wear-resistant coating on the inflow surface of the axially extending rod of the screening medium. The wear-resistant coating forms a substantially uniform coating area between an area on the inflow surface of the rod near the first slot and an area on the inflow surface of the rod near the second slot. The substantially uniform coating area has a substantially uniform thickness along the inflow surface in a circumferential direction perpendicular to the axial direction at multiple axial positions along the rod, and the substantially uniform coating area increases in thickness at multiple axial positions along the axial direction of the rod. The wear-resistant coating on each rod toward the outflow end of the screening medium is thicker than the wear-resistant coating on the rod toward the inflow end of the screening medium. The screen cylinder can be formed using a wedge screw rod providing a profiled rod, the profiled rod including an attachment end and an inflow surface facing a direction opposite to the attachment end. The wedge screw rod may also include a first groove surface extending from the inflow surface to the attachment end of the wedge screw rod and a second groove surface opposite to the first groove surface and extending from the inflow surface to the attachment end.
[0014] In some aspects of the screen drum, the thickness of the substantially uniform coating area varies along the inflow surface in a direction perpendicular to the axial direction by 20 percent or less of the average thickness, preferably 15 percent or less of the average thickness, preferably 10 percent or less of the average thickness, and / or more preferably 5 percent or less of the average thickness. The wear-resistant coating comprises a material having a hardness greater than that of the substrate of the rods. The axially extending grooves of the screen drum may have a groove width, which is defined by the minimum distance between adjacent rods at the area between the rods not coated with the wear-resistant coating, so that the groove width is not reduced by the wear-resistant coating. Moreover, the minimum distance between the coated areas of adjacent rods is preferably greater than or equal to the groove width defined by the minimum distance between adjacent rods at the area between the rods not coated with the wear-resistant coating. Furthermore, the groove width is preferably not reduced or covered by the wear-resistant coating.
[0015] The substantially uniform coating area at the inflow surface of the rod can start anywhere within 0 mm to 0.7 mm from the upper ridge, but in some embodiments should be as close to the upper ridge as possible, including at the upper ridge. The substantially uniform coating area can extend to anywhere within at least 0 mm to 0.7 mm from the transition region, but in some embodiments should be as close to the transition region as possible, including at the transition region. Therefore, it is preferred that the substantially uniform coating area is 0.7 mm or closer to the upper ridge (including at the upper ridge) and 0.7 mm or closer to the transition region (including at the transition region). The upper ridge area is the area between the first groove surface of the rod and the inflow surface of the rod, and the transition region is the area between the second groove surface of the rod and the inflow surface of the rod.
[0016] In various aspects of the screen drum and its manufacturing method, the wear-resistant coating thickness increases from the inflow end to the outflow end along the axial length of the rod. The wear-resistant coating thickness can gradually increase from the inflow end to the outflow end along the axial length of the rod. The wear-resistant coating thickness can gradually increase from the inflow end to the outflow end along the axial length of the rod at a linear rate or greater than a linear rate. The wear-resistant coating thickness can gradually increase from the inflow end to the outflow end along the axial length of the rod at a rate less than linear. The wear-resistant coating thickness can change in a step-like manner and gradually increase from the inflow end to the outflow end along the axial length of the rod in the outflow direction. The thickness of the wear-resistant coating can change in a waveform shape and gradually increase from the inflow end to the outflow direction along the axial length of the rod. The thickness of the wear-resistant coating can be increased from a nominal thickness of 30 microns or more to a nominal thickness of 300 microns or less. The thickness of the wear-resistant coating can be increased from a nominal thickness of 75 microns or more to a nominal thickness of 150 microns or less.
[0017] Preferably, the wear-resistant coating is sprayed onto the inflow surface of the axially extending rods of the screening medium using a nozzle. The nozzle moves axially along the injection channel in the screen drum, and the screen drum rotates to apply the wear-resistant coating to the inflow surface of each axially extending rod of the screening medium. When spraying the wear-resistant coating, the number of passes or the speed of the nozzle can be changed to change the thickness of the wear-resistant coating along each rod. Each spraying can deposit an additional layer of wear-resistant coating along each rod. By increasing the number of passes and / or duration toward the outflow end of the cylinder, the thickness of the entire coating on each rod toward the outflow end of the cylinder can be increased more than toward the inflow end.
[0018] The method can spray the wear-resistant coating while the screen drum is rotating. The rotation speed of the screen drum can be changed according to the position of the nozzle. The thickness of the wear-resistant coating can be increased from a thickness of 30 microns or more to a thickness of 300 microns or less. The thickness of the wear-resistant coating can be increased from a thickness of 75 microns or more to a thickness of 150 microns or less.
[0019] The foregoing general description and the following detailed description describe various embodiments and provide an overview or framework for understanding the nature and character of the claimed subject matter. However, the invention is in no way limited to the specific embodiments disclosed. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The accompanying drawings are included in and constitute a part of this specification. The drawings illustrate various embodiments described herein, and together with the description serve to explain the principles and operation of aspects of the invention.
[0021] Figure 1 schematically depicts a front perspective view of a screen drum according to one or more embodiments shown and described herein;
[0022] Figure 2 Schematically illustrates a device according to one or more embodiments shown and described herein. Figure 1 A perspective view of a portion of a screen cylinder showing a plurality of profiled or wedge-shaped lead screws coupled to a support ring of the screen cylinder;
[0023] Figure 3 Schematically shows Figure 1 Cross-sectional view of five types of special-shaped screws of the middle screen cylinder, with wear-resistant coating on the inflow surface of the special-shaped screws;
[0024] Figures 4A-4D A schematic side view of a wedge screw having a wear-resistant coating whose thickness gradually increases toward the outlet end of a screen drum according to one or more embodiments of the present invention shown and described herein is shown, wherein the coating increases linearly, more than linearly, stepwise, and in a wave-like manner, respectively;
[0025] Figure 5shows a cross-sectional view of a screen drum having a mechanical arm with a nozzle at the end thereof to spray a wear resistant coating onto the inflow surface of the rod;
[0026] Figure 6 depicts a front perspective view of a screen drum on a rotatable platform and a robotic arm with a spray nozzle for applying a wear resistant coating; and
[0027] Figure 7 A schematic diagram depicting a technique for varying the thickness of a wear resistant coating applied to the inflow surface of bars on a screen cylinder by varying the path length of a nozzle.
[0028] Figure 8 An axial cross-sectional view of a wedge-shaped special-shaped screw according to another embodiment of the present invention is shown. DETAILED DESCRIPTION
[0029] Although the details of the screen cylinder described herein are derived from the embodiments of typical screen cylinders, the configuration and features of the screen cylinder can vary. For example, some screen cylinders can be coupled to a structural back plate on the outside of the screen cylinder to support the structure of the screen cylinder. This configuration is shown and described in U.S. Patent No. 5,200,072, authorized on April 6, 1993, the entire contents of which are incorporated herein by reference. The structural back plate can allow fewer support rings on the screen cylinder. In any case, the benefits and features of the invention described herein are achievable and usable in different types of screen cylinders, including but not limited to screen cylinders with or without a structural back plate.
[0030] Reference will now be made in detail to embodiments of a screen cylinder with a profiled wedge screw, examples of which are illustrated in the accompanying drawings. The same reference numerals will be used throughout the drawings to refer to the same or similar parts.
[0031] Reference Figure 1 , shows an embodiment of a screen cylinder 10 according to an embodiment of the present disclosure. The screen cylinder includes an inflow end 8 at an axial end thereof and an outflow end 6 at an opposite axial end thereof. Pulp or similar fiber suspension enters the cylinder at the inflow end 8, and a reject stream (including undesirable components) leaves the screen cylinder at the outflow end 6. Accepted or desired pulp radially passes through the screening medium and is collected for later use or further processing.
[0032] The screen drum 10 may include a plurality of profiled wedge-shaped screw rods 12 that are longitudinally aligned and coupled to at least one support ring 14 at the attachment ends of the plurality of profiled rods 12. The profiled rods form a grooved cylindrical wall 16. Figure 2 and Figure 3Each of the profiled rods 12 may include an inflow surface 32 facing away from the support ring 14, a first groove surface 33 extending from the inflow surface 32 to the attachment end 30 of the profiled rod 12, and a second groove surface 35 opposite to the first groove surface 33 and extending from the inflow surface 32 to the attachment end 30 of the profiled rod 12. The first groove surface 33 of one profiled rod and the second groove surface 35 of another adjacent profiled rod may define the groove 20 ( Figure 3 ). Each profiled rod may include a wear resistant coating as part of at least the inflow surface of the profiled rod 12. The wear resistant coating has a thickness that gradually increases toward the outflow end of the screen drum. The inflow surface 32 of the rod is located on the inflow side of the screening medium and the cylinder. The attachment end 30 of the rod is located on the outflow side of the screening medium and the screen drum.
[0033] During operation of the screen drum 10, an acceptable portion of the pulp or other solid suspension flows through the slots 20 in the slotted cylindrical wall 16 (see Figure 3 ). The wear resistant coating applied to the profiled rods 12 can reduce the wear of the profiled rods 12 caused by the abrasive solid components of the pulp. Reducing the wear on the rods and their inflow surfaces located near the outlet end of the screen drum can help maintain the performance and efficiency of the screen drum 10 over time because the inflow surfaces of the rods are located near the outlet end of the screen drum. The rate of wear at the outlet tends to accelerate, resulting in the need to replace the entire screen drum. Therefore, reducing the wear towards the outflow end of the screen drum 10 over time can increase the useful life of the screen drum.
[0034] Directional terms used herein, such as above, below, right, left, front, back, top, bottom, are designated only with reference to the drawings drawn and the coordinate axes provided with the drawings, and are not intended to imply an absolute orientation. Moreover, the thickness markings, including the thickness of the wear-resistant coating and the thickness markings of the nominal thickness of the webbing, are the expected thicknesses. And as explained herein, when the wear-resistant coating is referred to as being substantially uniform, the actual coating thickness may vary from the average thickness by up to 20%. For example, the average thickness of the coating is 100 microns, which may vary by up to 20% anywhere, and the thickness is substantially uniform. And, some areas of the inflow surface, particularly areas near the groove surface, may be uncoated.
[0035] As used herein, the singular forms "a," "an," and "the" include plural referents unless the context clearly dictates otherwise. Thus, for example, reference to "a" component includes aspects having two or more such components unless the context clearly dictates otherwise.
[0036] As used herein, the terms "longitudinal" or "axial" may refer to an orientation or direction that is generally parallel to the central axis of the screen drum.
[0037] As used herein, the term "radial" may refer to the direction from the screen drum ( Figure 1) in the direction of any radius extending outward from the central axis.
[0038] As used herein, the terms "inflow" and "outflow" may refer to the relative position of features relative to the direction of flow of a solid suspension or slurry, such as inflow when entering a slot and outflow when leaving a slot. For the wedge screw of the present disclosure, the flow of the solid suspension generally flows from the inflow surface 32 of the profiled rod 12 to the outflow attachment end 30 of the profiled rod 12. Thus, for example, "inflow direction" or "towards the inflow direction" refers to a direction away from the inflow surface, radially opposite to the flow direction, or upstream in the flow direction. However, "outflow direction" or "towards the outflow direction" refers to a direction away from the inflow surface radially or downstream in the flow direction, which is opposite to the inflow direction. "Upstream" and "downstream" refer to the flow positions relative to each other as the flow of the solid suspension moves from upstream to downstream. For a screen cylinder, the inflow end refers to the end of the screen cylinder where the pulp enters, and the outflow end refers to the end of the screen cylinder where the waste pulp is discharged. In addition, the flow direction as described above refers to the overall movement of the flow averaged in space and time - taking into account the possible flow recirculation through the cylinder and transient flow reversals, such as slot backwash.
[0039] As used herein, the term "solid contaminants" or "oversized solid contaminants" may refer to solid objects, such as fiber bundles, metal pieces, dried adhesives, plastic plaques, or other contaminants, which are not intended and are not desired in the present invention. Solid suspensions or slurries and can be distinguished from solid components (e.g., fibers) intended to be present in solid suspensions.
[0040] Reference Figure 1 and Figure 2 , schematically shows a screen drum 10 including a plurality of wedge-shaped profiled bars 12. The screen drum 10 includes a plurality of support rings 14. The screen drum 10 includes a plurality of such bars 12, which are longitudinally aligned and coupled to at least one support ring 14 at the attachment end 30 of the bars 12. The screen drum 10 may also include an annular end flange at either axial end of the screen drum 10. Although not shown in the drawings herein, the screen drum typically includes a rotor therein to accelerate the suspension circumferentially and generate pressure pulsations that facilitate the flow of pulp through the slots of the screen drum 10. Details regarding the construction of the screen drum and its operation may be found in U.S. Patent Nos. 7,188,733, 7,856,718, and 5,200,072, the entire contents of each of which are incorporated herein by reference.
[0041] Each rod 12 may be longitudinally aligned with each of the other rods 12 around the centerline of the screen drum 10 and circumferentially spaced at a specific radial distance. The rods 12 may be arranged side by side along the inner circumference or outer circumference of the support ring 1 to form a slotted cylindrical wall 16. The slotted cylindrical wall 16 formed by a plurality of rods 12 may include a slot 20 defined between each pair of adjacent rods of the rods 12. The slot 20 may extend along the length of the screen drum 10 between the two annular end flanges.
[0042] By extending the slots 20 along the length of the screen cylinder 10, the screen cylinder 10 including the plurality of profiled bars 12 generally provides an increased open area through which an acceptable pulp or other solid suspension can flow. Figure 1 and Figure 2 The screen drum 10 is depicted as outwardly flowing, wherein the acceptable solid suspension flows radially outward through the slots 20 ( Figure 3 ). However, features of the present disclosure may also be used with an inward flow screen drum or any other type of pressure screen device utilizing a plurality of profiled bars. The screen drum 10 is operable to separate solid contaminants from a solid suspension.
[0043] Reference Figure 3 , shows a cross-sectional view of an embodiment of a profiled rod 12 mounted on a support ring 14 of a screen drum. Each rod 12 may have an attachment end 30 coupled to the support ring 14. Each rod 12 may have an inflow surface 32 that faces primarily away from at least one support ring 14. The inflow surfaces 32 of the plurality of rods 12 form a grooved cylindrical wall 16 ( Figure 1 ). Still refer to Figure 3 , each rod 12 may have a first groove surface 33 extending from the inflow surface 32 to the attachment end 30 of the profiled rod 12, which is opposite to the inflow surface 32. Each profiled rod 12 may have a second groove surface 35 on a side opposite to the first groove surface 33, and the second groove surface 35 extends from the inflow surface 32 to the attachment end 30 of the profiled rod 12. The first groove surface 33 and the second groove surface 35 face away from the inflow surface 32 and toward the support ring 14. The first groove surface 33 of one profiled rod 12 and the second groove surface 35 of another adjacent profiled rod 12 define one groove in the groove 20 of the screen drum 10. When two profiled rods 12 are adjacent, the first groove surface 33 of the first profiled rod and the second groove surface 35 of the second profiled rod define the groove 20, and no other profiled rod is arranged between the first profiled rod and the second profiled rod. The groove width is defined as the closest distance between the first groove surface 33 and the second groove surface 35 of the adjacent rods.
[0044] The first groove surface 33 may have a flat surface shape, and the second groove surface 35 may also have a flat surface shape. The first groove surface 33 may be fitted with the inflow surface 32 at an upper ridge 39, which protrudes radially away from the support ring 14, such as inwardly, and toward the adjacent rod located counterclockwise therefrom. The upper ridge 39 may include a bend or corner between the inflow surface 32 and the first groove surface 33. Downstream of the first groove surface 33, the rod side surface has a slight profile change between the upper ridge 39 and the attachment end 30. The second groove surface 35 may be fitted with the inflow surface 32 of the profiled rod 12 at a radially lower ridge or transition area 38 connected to the inflow surface 32. Downstream of the transition area 38 and the second groove surface 35 of the profiled rod 12, the connecting end 30 of the side surface rod may be connected to the connecting end 30 of the rod. As previously described, the flow of the solid suspension through the groove 20 generally flows from the inflow surface 32 of the profiled rod 12 to the attachment end 30. The transition region 38 connects the second groove surface 35 to the inflow-facing surface 32, with a corner or bend between the second groove surface 35 and the inflow-facing surface 32. However, the wedge screw may have a plurality of grooves other than the grooves of the second groove surface 35 and the inflow-facing surface 32. Figure 3 For example, the inflow surface 32, the first slot surface 33 and the second slot surface 35 may have any suitable shape for producing a screen cylinder for removing oversized solid contaminants from slurries and solid suspensions.
[0045] For a screen drum 10 used for screening pulp, the slots 20 may have a slot width greater than or equal to 80 microns (0.08 mm), such as from 0.08 mm to 1.5 mm. However, for applications in other industries, the spacing between the profiled bars 12 and the slot width may be larger or smaller, depending on the specific industry application. The slot width of the slot 20 should be consistent along the longitudinal length of the profiled bar 12.
[0046] Reference Figure 3 , the wear resistant coating 50 is located on and is a part of the inflow surface 32 of the rod 12 . Figure 3 A cross-sectional view of the rod in the axial direction is shown. Figure 3Only a portion of the rod at the same axial position is depicted, and for simplicity, the portion of the coating that increases in thickness toward the outlet end of the cylinder is not depicted. Wear may cause erosion of the inflow surface 32, which will destroy its fluid dynamic properties and reduce the flow through the screen cylinder. Because of the wear of the inflow surface, its profile or contour will change shape, the hydraulic performance of the screen will decrease, and the grooves may be more easily blocked. Profile wear generally increases in the axial direction. Therefore, when used to remove solid contaminants from a solid suspension of cellulose fibers or other solid components, the service life of a screen cylinder without a wear-resistant coating may be shortened. In some cases, the service life may be shortened to only a few months. In this embodiment, the wear-resistant coating 50 is applied to the entire length of the rod 12, but its thickness increases at, near and / or toward the outflow end 6 of the rod 12 and the screen cylinder 10. At a given axial position, and preferably at all axial positions, the thickness of the rod is substantially uniform in a direction perpendicular to the axial direction (such as Figure 3 1 ). In other embodiments, the wear resistant coating may not be applied to the area near the inflow end 8 of the rod 12. The wear resistant coating on the inflow surface thus prevents the surface from wearing prematurely. However, the coating is not applied to the groove surfaces 33, 35 of the rod in a manner that reduces the minimum width or "groove width" of the groove 20, which is defined as the minimum distance between the first groove surface 33 and the second groove surface 35, which is generally located between the point 34 and the transition area 38 of the first groove surface and the second groove surface, respectively.
[0047] Each profiled rod 12 may be formed of a base metal 46 having a wear-resistant coating applied thereto. The base metal 46 may be a rigid metal having sufficient strength to withstand pressure pulses and other mechanical loads from the rotor without deformation or fracture. In some embodiments, the base metal 46 may be stainless steel, such as 304L stainless steel or 316L stainless steel. The hardness value of the base metal 46 without the wear-resistant coating 50 may have a hardness value less than that of the wear-resistant coating 50. For example, the base metal 46 may have a hardness less than 500 HV0.05.
[0048] refer to Figures 4A-4D , which shows some examples of axial profiles of wear-resistant coating gradients according to aspects of the present invention. Figures 4A-4D A shape consistent with the shape shown in FIG. 1 is applied to the base metal 46 of each profiled rod 12 in the screen cylinder. However, for illustration purposes, Figures 4A-4DAn exaggerated thickness of the coating 50 is shown. The wear-resistant coating 50 is sprayed onto the inflow surface 32 of the profiled bar. As previously mentioned, the vicinity of the inflow surface 32 and the outflow end of the screen drum may be the area that experiences the greatest wear. Therefore, the greatest effect of the wear-resistant coating 50 should occur at this location of the screen drum, i.e., at and toward or near the outflow end. The wear-resistant coating 50 may have a thickness profile sufficient to protect the outflow end of the screen drum from premature or excessive wear.
[0049] exist Figure 4A In the figure, a linear axial gradient of the wear-resistant coating 50 is shown. Here, the thickness of the coating increases at a linear rate toward the outflow end of the screen cylinder 6. The rate of increase in axial thickness can be based on the characteristics of the fiber suspension being screened, the parameters of the screen cylinder and the change to select the wear rate of the outflow end of the screen cylinder. For example, the thickness can increase from 0 microns at the inlet to 100 microns at the outlet, or from 50 microns at the inlet to 150 microns at the outlet. In another embodiment of the linear shape, there can be a constant coating thickness, such as a 50 micron thick portion, which starts from the inlet of the cylinder and extends one-third of the length of the cylinder, followed by a portion where the coating thickness increases linearly from 50 microns to 150 microns, followed by a portion of the last one-third of the length of the cylinder, which extends to the outlet, where the coating thickness is a constant 150 microns.
[0050] Moreover, in Figure 4B 50 is shown in the axial gradient of the wear-resistant coating 50 greater than linear growth. Here, the thickness of the coating increases toward the outflow end of the screen cylinder 6 at a rate exceeding linearity, such as a power rate or an exponential rate. The rate of increase of the thickness rate slope can be selected based on the characteristics of the fiber suspension being screened, the screen cylinder parameters, and the change of the wear rate toward the outflow end of the screen cylinder. For example, the thickness can be increased from 0 microns at the entrance to 10 microns at a third of the length of the entrance, then from 10 microns to 40 microns on the second third of the length of the cylinder, and finally the thickness on the last third of the length of the cylinder is from 40 microns to 100 microns. In another embodiment of the gradient shape, there can be a portion of constant coating thickness at the entrance of the cylinder, such as a thickness of 30 microns, which can extend a quarter of the length of the cylinder, followed by the next quarter of the length of the cylinder, its coating thickness increases from 30 microns to 40 microns, then on the next quarter of the length of the cylinder, the coating thickness increases from 40 microns to 70 microns, followed by the last quarter of the length of the cylinder, the coating thickness increases from 70 microns to 130 microns.
[0051] Moreover, in Figure 4C6 shows a step-wise increase in the axial gradient of the wear-resistant coating 50. Here, the thickness of the coating increases toward the outflow end of the screen drum 6 at a step-wise rate, shape and / or pattern. The frequency, distance and / or number of steps in the axial direction can be selected based on the characteristics of the coating, the fiber suspension being screened, the parameters of the screen drum, and the change in the wear rate toward the outflow end 6 of the screen drum 10. In addition, the height or thickness increase of each step can also be selected based on the characteristics of the fiber suspension, the parameters of the screen drum being screened, and the change in the wear rate at the outflow end of the screen drum. For example, in one embodiment, the thickness in the first step can be 50 microns thick, which will extend over the first quarter of the length of the drum starting from the inlet; then, the thickness of the second step will increase to 75 microns, which will extend to the next half of the length of the drum; finally, the thickness of the third step will increase to 125 microns, which will extend to the last quarter of the length of the drum.
[0052] exist Figure 5 D shows a waveform increase in the axial gradient of the wear-resistant coating 50. Here, the thickness of the coating increases relative to the screen drum 6 at a curve or waveform rate, shape and / or pattern. The length, frequency, shape, distance and / or number of the curve or waveform in the axial direction can be selected based on the following factors: the characteristics of the fiber suspension being screened, the parameters of the screen drum, and the change in the wear rate at the outflow end of the screen drum. In addition, the height or thickness increase of each curve or wave can also be selected based on the characteristics of the fiber suspension being screened, the parameters of the screen drum, and the change in the wear rate toward the outflow end of the screen drum. For example, in one possible embodiment, the initial coating thickness at the inlet end of the drum can be 30 microns, which will increase to 50 microns at the end of the first quarter of the drum length, and then increase to 80 microns at the end of the second quarter of the drum length. The thickness decreases to 40 microns during the second quarter of the drum length; then increase to 120 microns at the end of the third quarter of the drum length, and the thickness decreases to 70 microns during the third quarter of the drum length; then finally increase to 150 microns at the end of the drum, and the thickness decreases to 110 microns.
[0053] Additionally, the axial gradient pattern may include Figures 4A-4D For example, the axial gradient of the coating may include a combination of linear shapes with step, gradient, and wavy shapes, or any combination or arrangement of these shapes over different portions of the axial length of the rod. For example, Figure 4A The linear slope shown in can be generated with Figure 4C Some features of the ladder shown in , and Figure 4C The steps shown in can be generated without having a distinctly different axial face as each step increases.
[0054] For example, but not limited to, the wear-resistant coating 50 may have a thickness greater than or equal to 5 microns, greater than or equal to 10 microns, greater than or equal to 15 microns, or even greater than or equal to 20 microns. In an embodiment, the thickness of the wear-resistant coating 50 may be 5 microns to 300 microns, 5 microns to 250 microns, 5 microns to 200 microns, 5 microns to 100 microns, 5 microns to 50 microns, 5 microns to 5 microns, 10 microns to 300 microns, 10 microns to 100 microns, or 10 microns to 50 microns. In some embodiments, the wear-resistant coating 50 may have a thickness greater than 300 microns without departing from the scope of the present disclosure. For example, the thickness of the wear-resistant coating may gradually increase from about 5 microns to 300 microns.
[0055] The wear-resistant coating 50 may have a hardness sufficient to reduce wear of the wedge screw 12 during operation of the screen drum 10. The hardness of the wear-resistant coating 50 may be greater than the hardness of the base metal 46 of the wedge screw 12. For example, the wear-resistant coating 50 may have a hardness value greater than the hardness value of cold-rolled stainless steel, which is about 400 HV0.05. The wear-resistant coating 50 may have a hardness value between 500 HV0.05 and 1200 HV0.05. The hardness value may be determined by measurements performed according to a standard Vickers hardness test method.
[0056] Reference Figure 5 and Figure 6 , a system for applying a wear-resistant coating to a screen drum 10 is shown. In this system, a mechanical arm 52 includes a nozzle 54 at its end. The nozzle 54 is suitable for spraying the wear-resistant coating 50 on the inflow side of the screen drum and on the inflow surface 32 of the rod. The mechanical arm 52 is oriented to allow the nozzle 54 to travel axially inside the screen drum 10 along the entire inner axial length of the screen drum 10. In some embodiments, the nozzle 54 may not be able to travel along the entire inner axial length; in this case, the drum is coated along approximately half of its length and then turned 180 degrees to coat the other half. The nozzle 54 moves relative to the screen drum 10 at least in the axial direction and the radial direction. The nozzle sprays the wear-resistant coating in the form of, for example, an elongated cylindrical plume, typically about 7 mm in diameter. For example, a coating of about 10 microns thick is deposited each time. By changing the length, number and / or speed of the stroke along the axial length of the drum, the thickness of the wear-resistant coating 50 and its axial gradient or profile can be controlled. In one embodiment, when the nozzle 54 applies the coating 50, a rotating platform 56 can be used to rotate the screen drum 10.
[0057] refer to Figure 7, the technique for applying the wear-resistant coating 50 will now be described. Using this technique, the nozzle applies a 10 micron thick coating in each axial passage. During each axial pass, the screen drum 10 may or may not rotate about its central axis. Initially, the screen drum 10 is oriented so that the outlet end 6 is located at the top or beginning of each injection channel. The first series of axial strokes A occurs when the nozzle 54 travels the entire axial length of the screen drum 10. Then, the second series of axial strokes B occurs, but the length of each stroke in the second series of axial strokes is smaller than the length of each stroke in the first series of axial strokes. Then, the third series of axial strokes C occurs, but the length of each stroke in the third series of axial strokes is less than the length of each stroke in the second series of axial strokes. Then, the fourth series of D axial strokes occurs, but the length of each stroke in the fourth series of axial strokes is less than the length of each stroke in the third series of axial strokes. Then, the fifth series of E axial strokes occurs, but the length of each stroke in the fifth series of axial strokes is less than the length of each stroke in the fourth series of axial strokes. Then, the sixth series of F axial strokes occurs, but the length of each stroke in the sixth series of axial strokes is less than the length of each stroke in the fifth series of axial strokes. Each series of axial strokes may include one or more axial strokes, where one cycle is considered to be a continuous stroke in opposite directions, depending on the desired axial profile thickness. Each series of axial strokes may form a step or wave pattern if desired. In addition, an additional series of continuous shorter lengths may be sprayed to customize the axial gradient of the wear-resistant coating. The screen drum may rotate about its central axis during and / or between the axial strokes of the nozzle.
[0058] Moreover, by programming the rotational speed of the screen drum and / or the axial speed of the nozzle 54 when applying the nozzle coating, various different axial gradient profiles of increasing thickness can be achieved. Moreover, the axial movement speed of the nozzle and / or the rotational speed of the screen drum can be reduced toward the outlet end of the screen drum to achieve various different axial gradient profiles of increasing thickness toward the outlet end of the screen drum. The rotational speed of the screen drum and / or the stroke length or speed of the nozzle can be changed or adjusted in an infinite manner to achieve various axial gradient profiles of increasing thickness. For example, the rotational speed of the screen drum can be varied based on the axial position of the nozzle.
[0059] Preferably, forming the wear-resistant coating 50 may include applying the wear-resistant coating 50 only to the inflow surface 32 of the profiled rod 12. Applying the wear-resistant coating 50 may include any coating process discussed herein, and the wear-resistant coating 50 may be formed using any material discussed herein. In some embodiments, applying the wear-resistant coating to at least the inflow surface 32 may include a thermal spray process. In some embodiments, the thermal spray process may include a high velocity oxygen fuel (HVOF) process.
[0060] The rods 12 forming the screening media are preferably coated on the inflow face or surface 32 using high velocity flame spraying under the combustion of a liquid or gaseous fuel. The wear resistant coating is applied to the inflow side of the rod using a high velocity flame nozzle such as a high velocity oxygen flame (HVOF). This technique allows the coating to be integrally bonded to the rod surface. The coating is highly adhered to the rod surface and produces a dense grain structure thereon.
[0061] Wear-resistant coating 50 can be, for example, a hard metal coating containing tungsten carbide and / or chromium carbide. Basic elements such as Ti, V, Nb, Mo, Ta and Hf can also exist as carbides and can be used in wear-resistant coatings containing carbides. Carbides of cobalt, chromium and nickel can also be used for wear-resistant coatings. Screen cylinder rods can be coated with wear-resistant coatings by thermal spraying. The coating material is completely or partially offset into a molten or plastic state, and is finely distributed and sprayed onto the rod to be coated via nozzle 54 in the form of a particle mist through an airflow. After cooling, the particles are mechanically adhered to the surface of the rod to be coated to form a coating. Any material with a stable molten state, such as metal, ceramic or its alloy, can be used as a coating material. The thermal spraying method of wear-resistant coating materials includes flame spraying, arc spraying, plasma spraying, vacuum plasma spraying, high-speed flame spraying, explosion spraying and explosion spraying, etc. For example, high-speed flame spraying (HVOF, HVAF) can be used to form a hard metal coating, such as WC-Co (Cr) and Cr3C2-NiCr. Furthermore, the wear resistant coating may exhibit a hardness between 500 HV0.05 and 1200 HV0.05. The hardness value may be determined by measurements performed according to the standard Vickers hardness test method.
[0062] Using such a technique, a coating 50 having optimum hardness, wear resistance and fracture toughness can be obtained. Wear-resistant thermal sprayed hard metal coatings may contain other hard particles besides carbides, such as nitrides, oxides or borides.
[0063] The base material of the rod 12 is typically stainless steel, but may also be composed of other metals and alloys. Preferably, the wear-resistant coating 50 is applied to the inflow side surface 32 or the face of the rod at one or more predetermined angles relative to the inflow side surface 32 or the face of the rod to ensure the desired coating profile. The wear-resistant coating may be applied by one or more nozzles or a nozzle having a plurality of nozzles 54. The angle of the nozzle or nozzle may be set to 90 degrees relative to the flat inclined portion of the inflow surface. However, other spray angles may be used and / or, for example, the angle of the nozzle 54 may be varied during its subsequent spraying process.
[0064] The angle of inclination of the nozzle 54 or spray head relative to the flat inclined surface of the inflow surface is generally preferably about 90 degrees. Preferably, the nozzle or spray head makes multiple passes over the screen to obtain the desired coating profile. The nozzle or spray head makes multiple passes over the screening medium to obtain the desired coating profile.
[0065] Reference Figure 8 , showing the basic uniformity of thickness on the inflow surface of the rod. Similar to the cross-sectional view, this uniformity of thickness can be observed in the cross section of the rod perpendicular to the axial direction. However, Figure 8 Only a portion of the rod at the same axial position is depicted, and for simplicity, the portion of the coating that increases in thickness toward the outlet end of the cylinder is not depicted. Also, the coating area on the inflow surface of the rod at a particular axial position has an average thickness when viewed in the axial direction. However, the uniformity of the coating area at any or all axial positions may vary by up to 20% of the average thickness, and preferably up to 15%, preferably up to 10%, and most preferably up to 5%, including all amounts between 0 and 5%. Therefore, substantially uniform as used herein means that the coating area thickness varies by at most 20% of the average thickness, preferably at most 15%, at most 10%, and more preferably at most 5%, including all amounts between 0 and 5%. Moreover, the thickness may actually decrease slightly from the area near the transition region 38 to the area near the upper ridge 39, but still remain substantially uniform. At any given axial position of the rod 12, and preferably at all axial positions of the rod 12, the coating 50 is substantially uniform in the circumferential direction perpendicular to the axial direction (e.g., Figure 3 and Figure 8 Furthermore, the rods 12 may be coated in the axial direction along their entire length or a portion of their entire length.
[0066] Moreover, if Figure 8As can be seen in the figure, the substantially uniform coating area 50 may not extend the entire width of the inflow surface 32. In other words, the wear-resistant coating may have some non-uniformity at the edge of the inflow surface 32. Such non-uniformity may occur when the coating 50 is applied in individual strokes, wherein the thickness of the coating deposited in each stroke is about 10 microns thick, i.e., one sublayer at a time, wherein each sublayer may not be perfectly aligned with the previously applied sublayer. The sublayers together form a coating area having a total thickness of the final layer as described herein. The substantially uniform coating area begins at the inflow surface 32 of the rod adjacent to the upper ridge 39 and may be within a range of 0 to 0.7 mm from the upper ridge 39. Preferably, the substantially uniform coating area begins within a range of 0 to 0.5 mm from the upper ridge 39, and more preferably within a range of 0 to 0.2 mm from the upper ridge 39. However, it may also be most preferred that the substantially uniform coating area 50 begins at the upper ridge 39 itself, so that there is no area between the upper ridge 39 and the substantially uniform coating area. The substantially uniform coating area 50 then extends on the inflow surface 32 in a direction perpendicular to the axial direction, for example circumferentially relative to the screen drum, until it terminates at a position of the inflow surface 32 of the rod near the second slot, which is within 0 to 0.7 mm from the transition region 38. Preferably, the substantially uniform coating area starts within 0 to 0.5 mm from the transition region 38, and more preferably starts within 0 to 0.2 mm from the transition region 38. However, it may also be most preferred that the substantially uniform coating area starts at the transition region 38 itself, so that there is no area between the transition region 38 and the substantially uniform coating area. A typical wedge wire rod 12 for pulp screening has a width of about 3.2 mm at its inflow surface. The most common wedge wire rods have a width of between 2.6 and 3.6 mm. However, when used for pulp screening, some rods may be as narrow as 2.3 mm and some as wide as 5.0 mm at the inflow surface. In all possible widths at the inflow surface of the rod, including any width between 2.3-5.0 mm, a substantially uniform coating area can begin and end near the upper ridge 39 and transition area 38, as described above. By maintaining a nozzle (not shown) spraying the wear resistant coating at a constant angle relative to the flat surface on the inflow surface of the rod, the substantially uniform coating area can be most uniform at the flat portion of the inflow surface. For example, by maintaining the nozzle at a constant angle relative to the flat surface when applying the coating 50, Figure 8 The sloped flat surface of the coated area 50 shown may be the most uniform.
[0067] Furthermore, the axially extending groove has a groove width 20, which is defined by the minimum distance between adjacent rods at the area between the rods that is not coated with the wear-resistant coating. Preferably, the wear-resistant coating 50 is not applied to the groove surface, especially at the location of the groove, so that the groove width is not effectively reduced by the presence of any wear-resistant coating at the area. Moreover, it is preferred that the minimum distance between the areas of adjacent rods having any coating material thereon is greater than or equal to the minimum groove width 20, so that the effective groove width 20 between adjacent rods is not reduced by the application of the wear-resistant coating. In this regard, the application of the wear-resistant coating 50 (or any overspray thereof) on the first groove surface 33 or the second groove surface 35, especially upstream and slightly downstream of the groove width 20 at points 34 and 38, should be avoided.
[0068] As previously discussed herein, the screen cylinder 10 including the profiled rods 12 having the wear resistant coating 50 may be used to process a solid suspension of cellulose or other fibers in a pulp in the paper industry as described herein. However, the screen cylinder 10 may not be limited to use in the pulp and paper industry. For example, the screen cylinder 10 of the present invention having the coated profiled rods 12 may be used to screen a solid suspension and / or slurry to remove oversized solid contaminants in mining and drilling applications, food preparation and processing operations, water treatment processes, coating operations, or other industries.
[0069] Although various embodiments of the profiled rod 12 for the screen drum 10 and methods for making and using the profiled rod 12 have been described herein, it should be understood that it is contemplated that each of these embodiments and techniques may be used alone or in combination with one or more embodiments and techniques. It will be apparent to those skilled in the art that various modifications and variations may be made to the embodiments described herein without departing from the spirit and scope of the claimed subject matter. Therefore, this specification is intended to cover modifications and variations of the various embodiments described herein as long as such modifications and variations fall within the scope of the appended claims and their equivalents.
[0070] Unless otherwise expressly stated, any method presented herein is in no way intended to be construed as requiring that its steps be performed in a particular order, nor is it intended to require that any apparatus have a particular orientation. Thus, if a method claim does not actually recite the order in which its steps are to be followed, or if any apparatus claim does not actually recite the order or orientation of individual components, or if otherwise specifically stated in the claim or specification, then if steps are restricted to a particular order, or if a particular order or orientation of components of an apparatus is not recited, then no order or orientation is intended to be inferred in any way.
Claims
1. A screen drum comprising: a screening medium having an inflow side and an outflow side, the screening medium being cylindrical and having a plurality of circumferentially spaced axially extending slots formed between axially extending bars, the axially extending bars of the screening medium having an inflow surface facing the inflow side, wherein the inflow surface extends lengthwise in the axial direction and widthwise in the circumferential direction relative to the screening medium; The screening medium has an inflow end and an outflow end axially opposite to the inflow end, and the axially extending rod extends from the inflow end to the outflow end; wherein the axially extending rods include a sprayed wear-resistant coating on the inflow surface of the screening medium, the wear-resistant coating forming a substantially uniform coating region between an area on the inflow surface of the rods near a first slot and an area on the inflow surface of the rods near a second slot, and wherein (i) the substantially uniform coating region at multiple axial positions is substantially uniform in thickness along the inflow surface in an axial normal direction, and (ii) the substantially uniform coating region at multiple axial positions increases in thickness in an axial direction, such that the wear-resistant coating on the rods at the outflow end of the screening medium is thicker than the wear-resistant coating on the rods at the inflow end of the screening medium.
2. A screen drum as claimed in claim 1, wherein the thickness variation of the substantially uniform coating area along the inflow surface in the axial normal direction is 20 percent or less of the average thickness, preferably 15 percent or less of the average thickness, preferably 10 percent or less of the average thickness, and / or more preferably 5 percent or less of the average thickness.
3. The screen cylinder of claims 1-2, wherein the wear resistant coating of the substantially uniform coated area comprises a material having a hardness greater than a hardness of a matrix material of the rods.
4. The screen drum according to claims 1-3, wherein the groove width of the axially extending grooves is determined by the minimum distance between adjacent rods, which distance is located at the area between the rods where the wear-resistant coating is not applied, so that the groove width is not reduced by the wear-resistant coating in said area.
5. A screen cylinder according to claims 1-4, wherein the minimum distance between coated areas of adjacent rods is greater than or equal to the groove width defined by the minimum distance between adjacent rods in areas not coated with wear-resistant coating between the rods, so that the groove width is not reduced by the wear-resistant coating in said areas.
6. A screen cylinder as described in claims 1-5, wherein the substantially uniform coating area starts from the inflow surface of the rod near the first groove, and its position is in the range of 0 to 0.7 mm, preferably in the range of 0 to 0.5 mm, and more preferably in the range of 0 to 0.2 mm, and the area between the first groove surface of the rod and the inflow surface of the rod is the upper ridge, and the upper ridge extends to the position of the inflow surface of the rod near the second groove, which is in the range of 0 to 0.7 mm, preferably in the range of 0 to 0.5 mm, and more preferably in the range of 0 to 0.2 mm in the transition area, and the transition area is the area between the second groove surface of the rod and the inflow surface of the rod.
7. The screen cylinder according to claims 1-6, wherein the thickness of the wear-resistant coating gradually increases along the axial length of the rod from the inflow end to the outflow end.
8. The screen cylinder according to claims 1-7, wherein the wear-resistant coating thickness gradually increases linearly from a portion of the rod along the axial length of the rod from the inflow end to the outflow end.
9. The screen cylinder according to claims 1-7, wherein the wear-resistant coating gradually increases in an axial direction along the axial length of the rod from a portion of the rod from the inflow end to the outflow end in a step-like manner.
10. The screen cylinder according to claims 1-5, wherein the thickness increases in a wave shape in the axial direction, from a portion of the rod toward the inflow end, and increases in a wave shape in the outflow direction along the axial length of the rod.
11. A screen cylinder according to claims 1-9, wherein the thickness of the substantially uniform coated area increases in the axial direction from 30 microns or more to 300 microns or less, preferably from 75 microns or more to 150 microns or less.
12. A method for manufacturing a screen drum, comprising: forming a screening medium having an inflow side and an outflow side, the screening medium being cylindrical and having a plurality of circumferentially spaced axially extending slots formed between axially extending rods, the axially extending rods of the screening medium having an inflow surface facing the inflow side, wherein the inflow surface extends lengthwise in the axial direction and widthwise in the circumferential direction relative to the screening medium; The sieving medium comprises an inflow end and an outflow end axially opposite to the inflow end; as well as A wear-resistant coating is sprayed on the inflow surface of the axially extending rod of the screening medium, the wear-resistant coating forms a substantially uniform coating area between an area on the inflow surface of the rod near the first groove and an area on the inflow surface of the rod near the second groove, and wherein (i) the substantially uniform coating area at multiple axial positions has a substantially uniform thickness along the inflow surface in the axial normal direction, and (ii) the substantially uniform coating area at multiple axial positions increases in thickness along the axial direction, so that the wear-resistant coating on the rod at the outflow end of the screening medium is thicker than the wear-resistant coating on the rod at the inflow end of the screening medium.
13. The method of claim 12, wherein applying the wear-resistant coating comprises: spraying the wear resistant coating onto the inflow surface of the axially extending rods of the screening medium using a nozzle; Move the nozzle axially along the screen drum to spray the wear-resistant coating on the inflow surface of the axially extending rod of the screening medium; as well as When spraying the wear-resistant coating, the number, length and / or speed of the nozzle strokes are changed to change the thickness of the wear-resistant coating.
14. A method according to claims 11-12, wherein the variation in the substantially uniform thickness along the inflow surface in the axial normal direction is twenty percent or less of the average thickness, preferably fifteen percent or less of the average thickness, preferably ten percent or less of the average thickness, and / or more preferably five percent or less of the average thickness.
15. The method according to claims 11-13, wherein the groove width of the axially extending groove is determined by the minimum distance between adjacent bars not coated with the wear resistant coating, so that the groove width is not reduced by the wear resistant coating in the area.
16. The method according to claims 11-14, wherein the minimum distance between coated areas of adjacent rods is greater than or equal to the groove width defined by the minimum distance between adjacent rods in areas of the wear-resistant coating not coated between the rods, so that the groove width is not reduced by the wear-resistant coating in the areas.
17. The method of claims 11-15, wherein the wear resistant coating comprises a material having a hardness greater than the hardness of the matrix of the rod.
18. A method according to claims 11-17, wherein a substantially uniform coating area starts from the inflow surface of the rod near the first groove, and its position is in the range of 0 to 0.7 mm, preferably in the range of 0 to 0.5 mm, and more preferably in the range of 0 to 0.2 mm, and the area between the first groove surface of the rod and the inflow surface of the rod is the upper ridge, and the upper ridge extends to the position of the inflow surface of the rod near the second groove, which is in the range of 0 to 0.7 mm, preferably in the range of 0 to 0.5 mm, and more preferably in the range of 0 to 0.2 mm in the transition area, and the transition area is the area between the second groove surface of the rod and the inflow surface of the rod.
19. The method of claims 13-18, wherein the thickness of the substantially uniform coated region gradually increases along the axial length of the rod from the inflow end to the outflow end.
20. The method of claims 13-19, wherein the thickness of the substantially uniform coated region increases in the axial direction from 30 microns or more to 300 microns or less, or in the axial direction from 75 microns or more to 150 microns or less.
21. The method of claims 11-20, wherein the screen drum is rotated while the wear resistant coating is sprayed.
22. The method according to claims 11-21, wherein the rotation speed of the screen drum is varied depending on the position of the nozzles.