Wafer adsorption method
By adjusting the pressure of the polishing head and polishing disk in the CMP process, the vacuum degree between the wafer and the polishing pad is reduced, and the problem of wafer adsorption is solved, achieving efficient wafer adsorption and equipment stability improvement.
Patent Information
- Application Number
- CN202411045484.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-19
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the existing CMP process, wafers are easily firmly adsorbed after polishing due to a local vacuum formed between the grooveless polishing pad, resulting in the polishing head being unable to absorb the wafer normally, which increases the cost of consumables and low adsorption efficiency. .
By controlling the pressure adjustment of the polishing head and polishing disk, especially the pressure of the retaining ring, internal support ring and pressure film, adjust the internal pressure of the polishing head, reduce the vacuum degree formed by the wafer surface and the polishing pad surface, and achieve smooth adsorption of the wafer .
It improves the success rate of wafer adsorption, ensures 100% adsorption success rate, enhances the stability and process efficiency of the equipment, and reduces costs.
Smart Images

Figure CN118983219A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of wafer adsorption, and in particular to a wafer adsorption method. Background Art
[0002] With the continuous development of the integrated circuit industry, the circuit line width has become smaller, the number of layers has increased, and Moore's Law has continued. The chemical mechanical planarization (CMP) process has become an important part of the entire chip process flow, especially in chip manufacturing. With the continuous upgrading of chip manufacturing technology, higher requirements are placed on the CMP process flow. In the processing and manufacturing of wafers, the CMP process will use some special grooveless soft polishing pads. This kind of soft pad can greatly improve the surface roughness of the wafer after CMP, improve wafer utilization, and provide a flatter processing surface for subsequent photolithography processes. However, it is precisely because of the grooveless soft pad that the wafer will be firmly adsorbed on the surface of the polishing pad after CMP and cannot be lifted by the polishing head. Such as Figure 1 As shown in the figure, the wafer is facing downward and the back side is facing upward before CMP polishing. Figure 1 As shown in (1a) in FIG. 1 , the back side of the wafer is polished on the polishing pad under pressure. Figure 1 As shown in (1b) in the figure, the problems that occur after polishing are as follows Figure 1 Therefore, in the conventional wafer adsorption method after the CMP process, a local vacuum may be generated between the lower surface of the wafer and the polishing pad, and the wafer may be firmly adsorbed on the surface of the polishing pad, resulting in the problem that the polishing head cannot normally absorb the wafer.
[0003] There are currently two common solutions to the vacuum problem. One is to increase the pressure of the internal support ring, increase the vacuum degree of the pressure membrane, and thus increase the adsorption force of the polishing head on the wafer. However, although the increased back pressure of the pressure membrane in this solution can lift the wafer, it will consume the life of the pressure membrane to a certain extent, increasing the cost of consumables. The second is to remove the vacuum formed between the front of the wafer and the polishing pad by moving the polishing head out of the polishing disk, and then adsorb the wafer; however, in this solution, it takes time to move the polishing head out, and when adsorbing the wafer again, it has to be moved back to the polishing disk. The time consumed will affect the wafer adsorption efficiency, and the success rate cannot reach 100%.
[0004] Therefore, a wafer adsorption method is needed to reduce the vacuum formed between the wafer surface and the grooveless polishing pad surface, increase the success rate of wafer adsorption, thereby effectively improving the stability of the equipment, and further improving the process efficiency and product yield. Summary of the invention
[0005] Therefore, the present invention provides a wafer adsorption method to solve the problem in the prior art that a local vacuum is generated between the lower surface of the wafer and the grooveless polishing pad, and the wafer is firmly adsorbed on the surface of the polishing pad, causing the polishing head to be unable to normally adsorb the wafer, thereby resulting in high consumables cost and low wafer adsorption efficiency for adsorbing the wafer.
[0006] The present invention provides a wafer adsorption method, which is used for adsorbing the wafer on the polishing pad after the CMP polishing machine finishes the grinding process;
[0007] The CMP polishing machine comprises:
[0008] Polishing discs;
[0009] A polishing pad, located on one side of the polishing disc;
[0010] A polishing head is away from the polishing disk and arranged opposite to the polishing pad; the polishing head comprises a retaining ring, an internal support ring, a pressure membrane, a pressure regulating device and an air inlet device; the internal support ring is located at the inner ring of the polishing head on the side facing the polishing pad; the retaining ring is located at the outer ring of the polishing head on the side facing the polishing pad, the retaining ring is concentrically arranged with the internal support ring and surrounds the internal support ring; the pressure membrane is located on the side of the internal support ring facing the wafer; the pressure regulating device is located on the side of the retaining ring facing away from the polishing pad; the air inlet device is located on the side of the pressure regulating device facing away from the retaining ring; the retaining ring, the internal support ring and the pressure membrane form a semi-enclosed area, the wafer is suitable for being arranged on the side of the polishing pad facing away from the polishing disk, and is located inside the semi-enclosed area;
[0011] The wafer adsorption method comprises:
[0012] Controlling the polishing head and the polishing plate to stop rotating, adjusting the pressure of the retaining ring to a first pressure, and releasing the pressure of the internal support ring and the pressure of the pressure membrane to 0 psi;
[0013] The pressure of the retaining ring and the pressure of the internal support ring are adjusted to a second pressure, the pressure of the pressure film is adjusted to a preset negative pressure, and the polishing head starts to absorb the wafer;
[0014] The pressure of the retaining ring is released and adjusted to the preset negative pressure, and the polishing head absorbs the wafer and lifts it up.
[0015] Optionally, before the step of controlling the polishing head and the polishing plate to stop rotating, the wafer adsorption method further includes:
[0016] Controlling the polishing head and the polishing disk to reduce the rotation speed so as to reduce the friction between the wafer and the polishing head and the polishing pad;
[0017] The pressure of the retaining ring is adjusted to a second pressure, and the pressure of the inner support ring and the pressure of the pressure membrane are released.
[0018] Optionally, after adjusting the pressure of the retaining ring and the pressure of the internal support ring to a second pressure, the wafer adsorption method further includes:
[0019] Detecting whether the wafer is in a balanced state.
[0020] Optionally, before the step of releasing the pressure of the retaining ring and adjusting the pressure to the preset negative pressure, the wafer adsorption method further includes:
[0021] The inner support ring is used to detect whether the pressure of the pressure film reaches a preset negative pressure, and to confirm whether the wafer is separated from the polishing pad.
[0022] Optionally, the pressure of the pressure membrane and the pressure of the retaining ring are adjusted to the preset negative pressure by a vacuum operation.
[0023] Optionally, the pressure of the retaining ring, the pressure of the internal support ring and the pressure of the pressure membrane are all adjusted by the pressure regulating device and the air intake device.
[0024] Optionally, the first pressure is less than the second pressure.
[0025] Optionally, the first pressure is 1.2psi to 1.8psi;
[0026] The second pressure is 2 psi to 3 psi;
[0027] The preset negative pressure is -7psi to -4.6psi.
[0028] Optionally, the first pressure is 1.5 psi;
[0029] The second pressure is 2 psi.
[0030] Optionally, the polishing pad is a non-groove soft pad.
[0031] The wafer adsorption method provided by the present invention controls the polishing head and the polishing disk to stop rotating, and adjusts the internal pressure of the polishing head by adjusting the pressures of the retaining ring, the internal support ring and the pressure film, thereby reducing the vacuum formed between the wafer surface and the polishing pad surface, thereby smoothly completing the action of the wafer being adsorbed from the polishing pad, and improving the success rate of the wafer being adsorbed. The method is particularly suitable for the situation where a non-grooved soft pad is used as a polishing pad and is easy to form a vacuum with the wafer, and can better avoid the problem that the wafer cannot be adsorbed. By using the wafer adsorption method provided by the present invention, the success rate of the wafer being adsorbed is as high as 100%, which can effectively improve the stability of the equipment, thereby improving the process efficiency and product yield. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0033] Figure 1 Schematic diagram of different states of a wafer during a CMP process in the prior art;
[0034] Figure 2 It is a schematic diagram of the wafer being unable to be adsorbed in the prior art;
[0035] Figure 3 A schematic structural diagram of a CMP polishing machine according to an embodiment of the present invention;
[0036] Figure 4 A schematic diagram of a process of a wafer adsorption method according to an embodiment of the present invention;
[0037] Figure 5 The figure is a schematic diagram of a specific process of a wafer adsorption method according to an embodiment of the present invention.
[0038] Description of reference numerals:
[0039] 1-polishing disc; 2-polishing pad; 3-polishing head; 31-retaining ring; 32-inner support ring; 33-pressure membrane; 34-air inlet device; 35-pressure regulating device; 4-wafer. DETAILED DESCRIPTION
[0040] During the wafer polishing process, under the environment of the selected polishing pad, polishing liquid, and polishing pad regulator, the downward pressure on the back of the wafer is controlled by applying different pressures to the retaining ring, the internal support ring, and the pressure film, and the wafer is pressed on the rotating polishing pad. The polishing liquid flows between the wafer and the polishing pad, and is evenly distributed on the polishing pad under the sweeping of the restorer and the centrifugal force. Under the action of the internal pressure of the polishing head, the lower surface of the wafer will be in close contact with the polishing pad. When the polishing pad is a non-grooved soft pad, since there are no grooves on the surface of the polishing pad and the polishing liquid soaks and covers the surface of the polishing pad, the air between the lower surface of the wafer and the contact polishing pad is completely squeezed out under the action of the polishing liquid, and a vacuum is formed between the wafer surface and the polishing pad. Therefore, the wafer will be firmly attached to the polishing pad after completing the polishing process. At this time, the internal support ring and the pressure film pressure inside the polishing head will also form a certain vacuum to absorb the wafer and make it leave the surface of the polishing pad, but because the upward adsorption force formed by the polishing head is not large enough, it cannot offset the force of atmospheric pressure on the wafer surface. Therefore, the wafer cannot be successfully adsorbed by the polishing head, and the following will occur: Figure 2 As shown in the phenomenon, the wafer separates from the polishing head and rotates with the polishing pad or even slides off the polishing pad. At this time, the equipment will also give a fault alarm.
[0041] In order to solve the problem in the prior art that a local vacuum is generated between the lower surface of the wafer and the grooveless polishing pad, the wafer is firmly adsorbed on the surface of the polishing pad, so that the polishing head cannot normally absorb the wafer, which leads to high consumables cost and low wafer adsorption efficiency in order to absorb the wafer, the present invention provides a wafer adsorption method, which is used for adsorbing the wafer on the polishing pad after the CMP polishing machine finishes the grinding process; the CMP polishing machine comprises: a polishing disk; a polishing pad, which is located on one side of the polishing disk; a polishing head, which is away from the polishing disk and arranged opposite to the polishing pad; the polishing head comprises a retaining ring, an internal support ring, a pressure membrane, a pressure regulating device and an air intake device; the internal support ring is located on the inner ring of the polishing head on the side facing the polishing pad; the retaining ring is located on the outer ring of the polishing head on the side facing the polishing pad, the retaining ring is concentrically arranged with the internal support ring and surrounds the internal support ring; the pressure membrane is located at the inner ring of the polishing head on the side facing the polishing pad The inner support ring faces the side of the wafer; the pressure regulating device is located on the side of the retaining ring facing away from the polishing pad; the air inlet device is located on the side of the pressure regulating device facing away from the retaining ring; the retaining ring, the inner support ring and the pressure membrane form a semi-enclosed area, and the wafer is suitable for being arranged on the side of the polishing pad facing away from the polishing disk, and is located inside the semi-enclosed area; it is characterized in that the wafer adsorption method includes: controlling the polishing head and the polishing disk to stop rotating, adjusting the pressure of the retaining ring to a first pressure, releasing the pressure of the inner support ring and the pressure of the pressure membrane to 0psi; adjusting the pressure of the retaining ring and the pressure of the inner support ring to a second pressure, adjusting the pressure of the pressure membrane to a preset negative pressure, and the polishing head starts to adsorb the wafer; releasing the pressure of the retaining ring and adjusting it to the preset negative pressure, and the polishing head adsorbs the wafer and lifts it.
[0042] The technical solution of the present invention will be clearly and completely described below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. In the description of the present invention, it should be noted that the terms "first", "second" and "third" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.
[0043] Example 1
[0044] This embodiment provides a wafer adsorption method for adsorbing a wafer 4 on a polishing pad after a CMP polishing machine finishes a grinding process;
[0045] like Figure 3 As shown, the CMP polishing machine comprises:
[0046] Polishing disc 1;
[0047] A polishing pad 2, located on one side of the polishing plate 1;
[0048] The polishing head 3 is away from the polishing disc 1 and is arranged opposite to the polishing pad 2; the polishing head 3 includes a retaining ring 31, an internal support ring 32, a pressure membrane 33, a pressure regulating device 34 and an air inlet device 35; the internal support ring 32 is located at the inner ring of the polishing head 3 facing the polishing pad 2; the retaining ring 31 is located at the outer ring of the polishing head 3 facing the polishing pad 2, the retaining ring 31 is concentrically arranged with the internal support ring 32 and surrounds the internal support ring 32; the pressure membrane 33 is located at the side of the internal support ring 32 facing the wafer 4; the pressure regulating device 34 is located at the side of the retaining ring 31 facing away from the polishing pad 2; The air inlet device 35 is located on the side of the pressure regulating device 34 facing away from the retaining ring 31; the retaining ring 31, the internal support ring 32 and the pressure membrane 33 form a semi-enclosed area, and the wafer 4 is suitable for being arranged on the side of the polishing pad 2 facing away from the polishing disk 1, and is located inside the semi-enclosed area; the retaining ring 31 is used to support the polishing head 3, the internal support ring 32 is used to fix the wafer 4, the pressure membrane 33 is used to adsorb the wafer 4, the air inlet device 35 is used to perform a vacuum operation, and the pressure regulating device 34 is used to change the pressure of the retaining ring 31, the internal support ring 32 and the pressure membrane 33 in combination with the air inlet device 35.
[0049] like Figure 4 As shown, the wafer adsorption method includes:
[0050] S101, controlling the polishing head and the polishing plate to stop rotating, adjusting the pressure of the retaining ring to a first pressure, and releasing the pressure of the internal support ring and the pressure of the pressure membrane to 0 psi.
[0051] During specific implementation, the friction force of the polishing head on the polishing pad is 0, and the wafer remains in a state of being free from force.
[0052] S102, adjusting the pressure of the retaining ring and the pressure of the internal support ring to a second pressure, adjusting the pressure of the pressure membrane to a preset negative pressure, and the polishing head starts to absorb the wafer.
[0053] In specific implementation, the pressure of the retaining ring is adjusted to the second pressure, and the pressure of the internal support ring is adjusted to the second pressure to maintain pressure without air leakage, and the pressure membrane begins to evacuate to negative pressure, so that the polishing head is ready to break the vacuum of the wafer and the polishing pad. The pressure range of the pressure membrane is controlled at a preset negative pressure, and the polishing head begins to suck the wafer.
[0054] S103, releasing the pressure of the retaining ring and adjusting it to the preset negative pressure, and the polishing head adsorbs the wafer and lifts it up.
[0055] During specific implementation, the pressure of the retaining ring is released and adjusted to the preset negative pressure, the internal support ring maintains pressure at the second pressure, and it is detected that the pressure of the pressure membrane and the pressure of the retaining ring both reach the preset negative pressure, thereby breaking the vacuum between the wafer and the polishing pad, so that the polishing head absorbs the wafer and lifts it up.
[0056] The wafer adsorption method provided by the present invention controls the polishing head and the polishing disk to stop rotating, and adjusts the internal pressure of the polishing head by adjusting the pressures of the retaining ring, the internal support ring and the pressure film, thereby reducing the vacuum formed between the wafer surface and the polishing pad surface, thereby smoothly completing the action of the wafer being adsorbed from the polishing pad, and improving the success rate of wafer adsorption. The method is particularly suitable for the situation where a non-grooved soft pad is used as a polishing pad and is easy to form a vacuum with the wafer, and can better avoid the problem that the wafer cannot be adsorbed. By using the wafer adsorption method provided by the present invention, the success rate of wafer adsorption is as high as 100%, thereby effectively improving the stability of the equipment, thereby improving the process efficiency and product yield.
[0057] Furthermore, in some embodiments, before the step of controlling the polishing head and the polishing disk to stop rotating, the wafer adsorption method also includes: controlling the polishing head and the polishing disk to reduce the rotation speed to reduce the friction between the wafer and the polishing head and the polishing pad; adjusting the pressure of the retaining ring to the second pressure, and releasing the pressure of the internal support ring and the pressure of the pressure membrane.
[0058] Specifically, by controlling the polishing head and the polishing disk to reduce their rotation speed, the friction between the polishing head and the wafer inside the polishing head and the polishing pad can be slowly reduced; at the same time, the pressure of the retaining ring is adjusted to the second pressure, and the pressure of the internal support ring and the pressure membrane are released.
[0059] Further, in some embodiments, after adjusting the pressure of the retaining ring and the pressure of the internal support ring to a second pressure, the wafer adsorption method further includes: detecting whether the wafer is in a balanced state.
[0060] In a specific implementation, when the pressure of the internal support ring is adjusted to the second pressure, that is, the pressure of the internal support ring is increased from 0 psi to the second pressure, by detecting signal feedback, it is determined whether the wafer is in a balanced state and whether the wafer is flying.
[0061] Furthermore, in some embodiments, before the step of releasing the pressure of the retaining ring and adjusting it to the preset negative pressure, the wafer adsorption method also includes: using the internal support ring to detect whether the pressure of the pressure membrane reaches the preset negative pressure, and confirming whether the wafer is separated from the polishing pad.
[0062] During specific implementation, a pressure test is performed through an internal support ring to determine whether there is leakage. If there is leakage, it means that the vacuum between the wafer and the polishing pad has not been broken.
[0063] Furthermore, in some embodiments, the pressure of the pressure membrane and the pressure of the retaining ring are adjusted to the preset negative pressure by a vacuum operation.
[0064] During specific implementation, a vacuum operation is performed through an air intake device to reduce the pressure of the pressure membrane and the pressure of the retaining ring, and the pressures are adjusted to the negative pressure.
[0065] Furthermore, in some embodiments, the pressure of the retaining ring, the pressure of the internal support ring and the pressure of the pressure membrane are all adjusted by a pressure regulating device and an air intake device.
[0066] Further, in some embodiments, the first pressure is less than the second pressure.
[0067] Specifically, the first pressure is smaller than the second pressure, and can accurately monitor whether the wafer is on the polishing head. The first pressure monitors the wafer with a small pressure, and the second pressure tests whether the wafer is firmly adsorbed on the polishing head with a larger pressure.
[0068] Further, in some embodiments, the first pressure is 1.2 psi to 1.8 psi, such as 1.2 psi, 1.5 psi, 1.6 psi, 1.8 psi, etc.;
[0069] The second pressure is 2psi to 3psi, such as 2psi, 2.4psi, 2.6psi, 3psi, etc.;
[0070] The preset negative pressure is -7psi to -4.6psi, for example, -7psi, -6.5psi, -5psi, -4.6psi, etc.
[0071] Specifically, the preset negative pressure is in the range of -7psi to -4.6psi, which can make it easier to adsorb the wafer. If it is less than this range, the wafer may not be adsorbed. If it is greater than this range, it will cause cracks in the wafer or even break the wafer.
[0072] Furthermore, in some embodiments, the first pressure is 1.5 psi; the second pressure is 2 psi.
[0073] Furthermore, in some embodiments, the polishing pad is a non-grooved soft pad. Since the non-grooved soft pad is more likely to form a local vacuum with the wafer, the wafer is firmly adsorbed. Therefore, the method is particularly suitable for the situation where the non-grooved soft pad is easily used as a polishing pad to form a vacuum with the wafer, which can better avoid the problem that the wafer cannot be adsorbed. By using the wafer adsorption method provided by the present invention, the wafer adsorption success rate is as high as 100%, which can effectively improve the stability of the equipment, thereby improving the process efficiency and product yield.
[0074] Example 2
[0075] refer to Figure 5 This embodiment provides a specific process of a wafer adsorption method, including steps S201-S207, which is used to absorb the wafer on the polishing pad after the CMP polishing machine finishes the grinding process.
[0076] S201, first reduce the rotation speed of the polishing head and the polishing disc, while keeping the pressure of the ring at 2 psi, release the pressure of the internal support ring and the pressure membrane, and set this step to be completed within 2 seconds.
[0077] S202, stop the rotation speed of the polishing head and the polishing disc, while keeping the pressure of the ring at 1.5 psi, release the pressure of the internal support ring and the pressure of the pressure membrane to 0 psi, and complete it within 2 seconds.
[0078] S203, the rotation speed of the polishing head and the polishing disc remains stopped, the pressure of the holding ring is maintained at 2psi, the pressure of the internal support ring is maintained at 2psi, and the pressure of the pressure membrane is maintained at 0psi, which is completed within 1s.
[0079] S204, the rotation speed of the polishing head and the polishing disk remains stopped, the holding ring maintains a pressure of 2psi, the internal support ring is pressurized at 2psi, the pressure membrane is evacuated to negative pressure, preparations are made to break the vacuum between the wafer and the polishing pad, and the wafer suction work is started, which is completed within 3 seconds.
[0080] S205, the rotation speed of the polishing head and the polishing disc remains stopped, the holding ring maintains a pressure of 2psi, the internal support ring continues to maintain a pressure of 2psi, and the pressure of the pressure membrane is detected to see if it is maintained within the range of (-7psi to -4.6psi), which is completed within 2s.
[0081] S206, the rotation speed of the polishing head and the polishing disc remains stopped, the holding ring maintains a pressure of 2psi, the internal support ring continues to maintain a pressure of 2psi, the pressure of the pressure membrane is maintained within the range of (-7psi to -4.6psi), and the internal support ring is checked to see if it is maintaining a pressure of 2psi. This is completed within 10s.
[0082] S207, the rotation speed of the polishing head and the polishing disc remains stopped, the holding ring is subjected to VAC pressure, the internal support ring continues to maintain 2psi pressure, the pressure of the pressure membrane is maintained within the range of (-7psi to -4.6psi), and the pressure of the holding ring is detected to be maintained within the range of (-7psi to -4.6psi), and it is completed within 5s.
[0083] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.
Claims
1. A wafer adsorption method for adsorbing a wafer on a polishing pad after a CMP polishing machine finishes the grinding process; The CMP polishing machine comprises: Polishing discs; A polishing pad, located on one side of the polishing disc; A polishing head is away from the polishing disk and arranged opposite to the polishing pad; the polishing head comprises a retaining ring, an internal support ring, a pressure membrane, a pressure regulating device and an air inlet device; the internal support ring is located at the inner ring of the polishing head on the side facing the polishing pad; the retaining ring is located at the outer ring of the polishing head on the side facing the polishing pad, the retaining ring is concentrically arranged with the internal support ring and surrounds the internal support ring; the pressure membrane is located on the side of the internal support ring facing the wafer; the pressure regulating device is located on the side of the retaining ring facing away from the polishing pad; the air inlet device is located on the side of the pressure regulating device facing away from the retaining ring; the retaining ring, the internal support ring and the pressure membrane form a semi-enclosed area, the wafer is suitable for being arranged on the side of the polishing pad facing away from the polishing disk, and is located inside the semi-enclosed area; Characterized in that, the wafer adsorption method comprises: Controlling the polishing head and the polishing plate to stop rotating, adjusting the pressure of the retaining ring to a first pressure, and releasing the pressure of the internal support ring and the pressure of the pressure membrane to 0 psi; The pressure of the retaining ring and the pressure of the internal support ring are adjusted to a second pressure, the pressure of the pressure film is adjusted to a preset negative pressure, and the polishing head starts to absorb the wafer; The pressure of the retaining ring is released and adjusted to the preset negative pressure, and the polishing head absorbs the wafer and lifts it up.
2. The wafer adsorption method according to claim 1, It is characterized in that Before the step of controlling the polishing head and the polishing plate to stop rotating, the wafer adsorption method further includes: Controlling the polishing head and the polishing disk to reduce the rotation speed so as to reduce the friction between the wafer and the polishing head and the polishing pad; The pressure of the retaining ring is adjusted to a second pressure, and the pressure of the inner support ring and the pressure of the pressure membrane are released.
3. The wafer adsorption method according to claim 2, It is characterized in that After adjusting the pressure of the retaining ring and the pressure of the inner support ring to a second pressure, the wafer adsorption method further includes: Detecting whether the wafer is in a balanced state.
4. The wafer adsorption method according to claim 3, It is characterized in that Before the step of releasing the pressure of the retaining ring and adjusting the pressure to the preset negative pressure, the wafer adsorption method further includes: The internal support ring is used to detect whether the pressure of the pressure film reaches a preset negative pressure, and to confirm whether the wafer is separated from the polishing pad.
5. The wafer adsorption method according to claim 4, It is characterized in that The pressure of the pressure film and the pressure of the retaining ring are adjusted to the preset negative pressure through a vacuum operation.
6. The wafer adsorption method according to claim 1, It is characterized in that The pressure of the retaining ring, the pressure of the internal support ring and the pressure of the pressure membrane are all adjusted by the pressure regulating device and the air inlet device.
7. The wafer adsorption method according to claim 1, It is characterized in that The first pressure is lower than the second pressure.
8. The wafer adsorption method according to claim 1, It is characterized in that The first pressure is 1.2 psi to 1.8 psi; The second pressure is 2 psi to 3 psi; The preset negative pressure is -7psi to -4.6psi.
9. The wafer adsorption method according to claim 8, It is characterized in that The first pressure is 1.5 psi; The second pressure is 2 psi.
10. The wafer adsorption method according to claim 1, It is characterized in that The polishing pad is a soft pad without grooves.
Citation Information
Patent Citations
Wafer grinding method, device and equipment
CN117773767A
Wafer polishing device and manufacture of wafer
JP2000343410A
Method for polishing wafer and polishing head
JP2003163193A
Cited By
Grinding device and method for relieving impact of pressure film on wafer
CN120116143A
A grinding device and method for reducing the impact of a pressure membrane on a wafer
CN120116143B