Preparation method of V-shaped gate silicon carbide VDMOS with low gate charge
By adopting V-type gate structure and well region design in silicon carbide VDMOS devices, the problem of high gate charge of existing devices is solved, and faster switching speeds and higher frequency performance are achieved.
Patent Information
- Application Number
- CN202410950991.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-19
Smart Images

Figure CN118983221A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for preparing a V-type gate silicon carbide VDMOS with low gate charge. Background Art
[0002] Silicon carbide VDMOS is a typical representative of silicon carbide power devices, and is widely used in electric vehicles, aerospace, power conversion and other fields. As the power system has higher and higher requirements for power density, the operating frequency of silicon carbide VDMOS is also getting higher and higher, which requires the gate charge of the device to be as low as possible to reduce switching losses, increase switching speed, and achieve high frequency, high efficiency and high power density; however, the gate charge of existing devices is still relatively high, so it is urgent to reduce its gate charge. Summary of the invention
[0003] The technical problem to be solved by the present invention is to provide a method for preparing a V-gate silicon carbide VDMOS with low gate charge, which adopts a V-gate device structure, requires a small inversion thickness for gate control, and has a small gate charge, and can effectively improve the switching speed of the device.
[0004] The present invention is implemented as follows: a method for preparing a V-type gate silicon carbide VDMOS with low gate charge, comprising the following steps:
[0005] Step 1: depositing metal on the lower side of the silicon carbide substrate to form a drain metal layer; epitaxially growing on the silicon carbide substrate to form a drift layer;
[0006] Step 2: using ion implantation to form a current equalizing region in the drift layer;
[0007] Step 3, forming a barrier layer on the drift layer, etching the barrier layer to form a through hole, and forming a P-type well region in the drift layer by ion implantation;
[0008] Step 4: remove the original barrier layer, re-form the barrier layer, etch the barrier layer to form a through hole, and form a P-type source region in the drift layer by ion implantation;
[0009] Step 5, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, and forming an N-type source region in the drift layer by ion implantation;
[0010] Step 6, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, and then wet etching the N-type source region and the P-type well region to form a V-shaped groove; then performing dry oxygen oxidation in the V-shaped groove to form an insulating dielectric layer, wherein the insulating dielectric layer is provided with a V-shaped groove;
[0011] Step 7, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, depositing metal, and forming a gate metal layer;
[0012] Step 8: remove the original barrier layer, re-form the barrier layer, etch the barrier layer to form a through hole, and etch the drift layer until the upper side of the P-type source region, deposit metal to form a source metal layer, and then remove the barrier layer to complete the preparation.
[0013] The advantages of the present invention are:
[0014] 1. The device adopts a V-type gate device structure. The gate control requires less inversion thickness and smaller gate charge, which can effectively improve the switching speed of the device;
[0015] Second, the V-type gate is prone to form electric field concentration at the sharp part of the gate of the device, thereby affecting the reliability of the gate. However, the present invention constructs a P-type well region at the sharp part of the gate, and the P-type well region can effectively suppress the electric field concentration in this area;
[0016] 3. The source metal layer of the device is in direct contact with the P-type source region, and the P-type source region is in direct contact with the N-type drift layer without passing through the P-type well region, which can reduce the conduction loss of the body diode;
[0017] 4. The N-type current sharing area of the device is distributed in the N-type drift layer close to the P-type well area, but there is a 300nm thick N-type drift layer between the P-type well area. This can avoid the N-type current sharing to protect the sharp part of the P-type well area on the gate while sharing the current from the gate. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] The present invention will be further described below in conjunction with embodiments with reference to the accompanying drawings.
[0019] Figure 1 The present invention is a flow chart of a method for preparing a V-type gate silicon carbide VDMOS with low gate charge.
[0020] Figure 2 A cross-sectional view of the process of a V-type gate silicon carbide VDMOS with low gate charge according to the present invention Figure 1 .
[0021] Figure 3 A cross-sectional view of the process of a V-type gate silicon carbide VDMOS with low gate charge according to the present invention Figure 2 .
[0022] Figure 4 A cross-sectional view of the process of a V-type gate silicon carbide VDMOS with low gate charge according to the present invention Figure 3 .
[0023] Figure 5 A cross-sectional view of the process of a V-type gate silicon carbide VDMOS with low gate charge according to the present invention Figure 4 .
[0024] Figure 6 A cross-sectional view of the process of a V-type gate silicon carbide VDMOS with low gate charge according to the present invention Figure 5 .
[0025] Figure 7 A cross-sectional view of the process of a V-type gate silicon carbide VDMOS with low gate charge according to the present invention Figure 6 .
[0026] Figure 8 A cross-sectional view of the process of a V-type gate silicon carbide VDMOS with low gate charge according to the present invention Figure 7 .
[0027] Fig. 9 A cross-sectional view of the process of a V-type gate silicon carbide VDMOS with low gate charge according to the present invention Figure 8 .
[0028] Fig.10 A cross-sectional view of the process of a V-type gate silicon carbide VDMOS with low gate charge according to the present invention Figure 9 .
[0029] Fig.11 A cross-sectional view of the process of a V-type gate silicon carbide VDMOS with low gate charge according to the present invention Figure 10 .
[0030] Fig.12 The schematic diagram of a V-type gate silicon carbide VDMOS with low gate charge according to the present invention. DETAILED DESCRIPTION
[0031] In order to facilitate understanding of the present application, the present application will be described more fully below with reference to the relevant drawings. Embodiments of the present application are provided in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present application more thorough and comprehensive.
[0032] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application.
[0033] It should be understood that when an element or layer is referred to as "on ...", "adjacent to ...", "connected to" or "coupled to" other elements or layers, it can be directly on, adjacent to, connected to or coupled to other elements or layers, or there can be intervening elements or layers. On the contrary, when an element is referred to as "directly on ...", "in contact with ...", "directly connected to" or "directly coupled to" other elements or layers, there is no intervening element or layer. It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, regions, layers, doping types and / or parts, these elements, components, regions, layers, doping types and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer, doping type or part from another element, component, region, layer, doping type or part. Therefore, without departing from the teachings of the present invention, the first element, component, region, layer, doping type or part discussed below can be represented as a second element, component, region, layer or part.
[0034] Spatially relative terms such as "under," "beneath," "below," "under," "above," "above," and the like may be used herein to describe the relationship of one element or feature described in the figures to other elements or features. It should be understood that, in addition to the orientations described in the figures, spatially relative terms also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is flipped, an element or feature described as "under other elements" or "under it" or "under it" will be oriented as being "above" the other elements or features. Thus, the exemplary terms "under" and "under" may include both upper and lower orientations. In addition, the device may also include additional orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptors used herein are interpreted accordingly.
[0035] When used herein, the singular forms "a", "an", and "said / the" may also include plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "include / comprise" or "have" and the like specify the presence of stated features, wholes, steps, operations, components, parts, or combinations thereof, but do not exclude the possibility of the presence or addition of one or more other features, wholes, steps, operations, components, parts, or combinations thereof. At the same time, in this specification, the term "and / or" includes any and all combinations of the relevant listed items.
[0036] like Figures 1 to 11 As shown, the embodiment of the present application provides a method for preparing a V-gate silicon carbide VDMOS with low gate charge, comprising the following steps:
[0037] Step 1: depositing metal on the lower side of the silicon carbide substrate 1 to form a drain metal layer 9; epitaxially growing on the silicon carbide substrate 1 to form a drift layer 2;
[0038] Step 2: forming a current equalizing region 21 in the drift layer 2 by ion implantation, wherein the ion implantation energy is 300-400kev;
[0039] Step 3, forming a barrier layer a on the drift layer 2, etching the barrier layer a to form a through hole, and forming a P-type well region 4 in the drift layer 2 by ion implantation, with an ion implantation energy of 200-300kev;
[0040] Step 4, remove the original barrier layer a, re-form the barrier layer a, etch the barrier layer a to form a through hole, and form a P-type source region 3 in the drift layer 2 by ion implantation, with the ion implantation energy of 200-300kev;
[0041] Step 5, removing the original barrier layer a, re-forming the barrier layer a, etching the barrier layer a to form a through hole, and forming an N-type source region 5 in the drift layer 2 by ion implantation, with the ion implantation energy being 10-200kev;
[0042] Step 6, removing the original barrier layer a, re-forming the barrier layer a, etching the barrier layer a to form a through hole, and then wet etching the N-type source region 5 and the P-type well region 4 to form a V-shaped groove 41; then performing dry oxygen oxidation in the V-shaped groove 41 to form an insulating dielectric layer 6, wherein the insulating dielectric layer 6 is provided with a V-shaped groove 61;
[0043] Step 7, removing the original barrier layer a, re-forming the barrier layer a, etching the barrier layer a to form a through hole, depositing metal, and forming a gate metal layer 8;
[0044] Step 8, remove the original barrier layer a, re-form the barrier layer a, etch the barrier layer a to form a through hole, and etch the drift layer 2 until the upper side of the P-type source region 3, deposit metal to form a source metal layer 7, and then remove the barrier layer a to complete the preparation.
[0045] like Fig.12 As shown, the silicon carbide VDMOS obtained by the above manufacturing method includes:
[0046] Silicon carbide substrate 1,
[0047] A drift layer 2, wherein the lower side of the drift layer 2 is connected to the upper side of the silicon carbide substrate 1, and a current balancing layer 21 is provided in the drift layer 2;
[0048] A P-type source region 3, the lower side of the P-type source region 3 is connected to the upper side of the drift layer 2;
[0049] A P-type well region 4, wherein the lower side of the P-type well region 4 is connected to the upper side of the drift layer 2;
[0050] An N-type source region 5, wherein the lower side of the N-type source region 5 is connected to the P-type well region 4;
[0051] An insulating dielectric layer 6, wherein the insulating dielectric layer 6 is V-shaped and connected to the P-type well region 4 and the N-type source region 5 respectively; a V-shaped groove 61 is provided in the insulating dielectric layer 6;
[0052] A source metal layer 7, wherein the source metal layer 7 is connected to the P-type source region 3 and the N-type source region 5 respectively;
[0053] A gate metal layer 8, wherein the gate metal layer 8 is disposed in the V-shaped groove 61;
[0054] and, a drain metal layer 9, wherein the drain metal layer 9 is connected to the lower side of the silicon carbide substrate 1;
[0055] A V-shaped groove 41 is formed in the N-type source region 5 and the P-type well region 4 , and the insulating dielectric layer 6 is disposed in the V-shaped groove 41 .
[0056] The silicon carbide substrate 1 is of N-type, and its doping concentration is 2e18cm -3 The drift layer 2 is of N type, and its doping concentration is 2e16cm -3 The current balancing region 21 is of N-type, and its doping concentration is 6e17cm -3 The doping concentration of the P-type source region 3 is 8e18cm -3 The doping concentration of the P-type well region 4 is 1e17cm -3 The doping concentration of the N-type source region 5 is 2e18cm -3 . The insulating dielectric layer 6 is silicon dioxide, the gate metal layer 8, the source metal layer 7 and the drain metal layer 9 are all Al. The thickness of the N-type silicon carbide substrate 1 of the device is 1μm, the thickness of the N-type drift layer 2 is 10-20μm, the thickness of the N-type current equalizing region 21 is 300nm, the distance from the upper side of the N-type current equalizing region 21 to the upper side of the N-type drift layer 2 is 300nm, the thickness of the P-type source region 3 is 300nm, the thickness of the P-type well region 4 is 300nm, the distance from the bottom of the P-type well region 4 to the bottom of the insulating dielectric layer is 50nm, the thickness of the N-type source region 5 is 600nm, the thickness of the source metal layer 7 is 600nm, the sidewall thickness of the insulating dielectric layer 6 is 20nm, and the device withstand voltage is 800-1200V;
[0057] The concentration of the N-type silicon carbide substrate 1 is to form a low-resistance ohmic contact with the drain metal layer 9 to reduce the on-resistance of the device. Its thickness is based on the design conditions of the device epitaxial thickness (N-type drift layer 2) to ensure support and improve process stability. The thickness and doping concentration of the N-type drift layer 2 are a compromise between on-resistance and withstand voltage. The P-type source region 3 is designed to reduce the on-resistance of the device body diode and improve the body diode freewheeling capability. The N-type current equalizing region 21 is to reduce the on-resistance of the device and realize the equalization of the internal current of the device. Its concentration, thickness and position relationship are to realize that the electrons from the N-type source region 5 enter the N-type drift layer 2 above the N-type current equalizing region 21 through the inverted P-type well region 4. When entering the N-type current equalizing region 21, the lateral resistance value is smaller and the lateral diffusion of the current is larger, which avoids the current from being concentrated in the middle area of the device and improves the reliability of the device.
[0058] When the device is turned off, the gate is at zero voltage, the drain is subjected to high voltage, and the space charge region constructed by the N-type drift layer 2, the P-type well region 4, and the P-type source region 3 is subjected to high voltage; when a positive voltage is applied to the device gate, the P-type well region 4 is inverted near the gate insulating dielectric layer 6, forming a conductive channel along the insulating dielectric layer 6 to achieve conduction. Since the inversion is only performed in the P-type well region 4, and there is an N-type current-equalizing region 21 to complete the electric field shielding of the gate to the drain, the gate-drain capacitance and the gate-source capacitance are reduced, and the gate charge of the device is reduced;
[0059] The present invention constructs a P-type well region at the sharp part of the gate, thereby protecting the sharp corner of the gate and improving the reliability of the device on the basis of ensuring the reduction of the gate charge of the device.
[0060] Although the specific implementation modes of the present invention are described above, those skilled in the art should understand that the specific implementation modes described are only illustrative and are not intended to limit the scope of the present invention. Equivalent modifications and changes made by those skilled in the art in accordance with the spirit of the present invention should be included in the scope of protection of the claims of the present invention.
Claims
1. A method for preparing a V-gate silicon carbide VDMOS with low gate charge, characterized in that: The steps include: Step 1: depositing metal on the lower side of the silicon carbide substrate to form a drain metal layer; epitaxially growing on the silicon carbide substrate to form a drift layer; Step 2: using ion implantation to form a current equalizing region in the drift layer; Step 3, forming a barrier layer on the drift layer, etching the barrier layer to form a through hole, and forming a P-type well region in the drift layer by ion implantation; Step 4: remove the original barrier layer, re-form the barrier layer, etch the barrier layer to form a through hole, and form a P-type source region in the drift layer by ion implantation; Step 5, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, and forming an N-type source region in the drift layer by ion implantation; Step 6, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, and then wet etching the N-type source region and the P-type well region to form a V-shaped groove; then performing dry oxygen oxidation in the V-shaped groove to form an insulating dielectric layer, wherein the insulating dielectric layer is provided with a V-shaped groove; Step 7, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, depositing metal, and forming a gate metal layer; Step 8: remove the original barrier layer, re-form the barrier layer, etch the barrier layer to form a through hole, and etch the drift layer until the upper side of the P-type source region, deposit metal to form a source metal layer, and then remove the barrier layer to complete the preparation.
2. The method for preparing a V-gate silicon carbide VDMOS with low gate charge according to claim 1, characterized in that: The doping concentration of the silicon carbide substrate is 2e18cm -3 The doping concentration of the drift layer is 2e16cm -3 The doping concentration of the current balancing region is 6e17cm -3 The doping concentration of the P-type source region is 8e18cm -3 The doping concentration of the P-type well region is 1e17cm -3 The doping concentration of the N-type source region is 2e18cm -3 .
3. The method for preparing a V-gate silicon carbide VDMOS with low gate charge according to claim 1, characterized in that: The distance between the upper side of the current balancing region and the upper side of the drift layer is 300 nm.
4. The method for preparing a V-gate silicon carbide VDMOS with low gate charge according to claim 1, characterized in that: The thickness of the flow-averaging region is 300 nm.
5. The method for preparing a V-gate silicon carbide VDMOS with low gate charge according to claim 1, characterized in that: The side wall thickness of the insulating dielectric layer is 20 nm.
Citation Information
Cited By
Low-on-resistance trench gate silicon carbide VDMOS (Vertical Double-diffused Metal Oxide Semiconductor) and preparation method thereof
CN119403161A