Organic light-emitting device

By introducing alternating high-doping-concentration or high-carrier-mobility-rate regions of hole injection layer and electron injection layer into organic light-emitting devices, carrier injection and migration are optimized, solving the problem of exciton and polaron quenching under high brightness and improving the brightness stability and efficiency of the device.

CN118984601APending Publication Date: 2024-11-19GUAN YEOLIGHT TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411072796.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-06
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

In organic light-emitting devices, the quenching phenomenon between excitons and polarons at high brightness leads to efficiency roll-off, which is difficult to solve effectively with existing technologies.

Method used

By introducing alternating regions of high doping concentration or high carrier migration rate in the hole injection layer and electron injection layer, carrier injection and migration are optimized to reduce the quenching probability of excitons and polarons.

Benefits of technology

This effectively reduces the quenching probability between excitons and polarons, avoids the roll-off of luminous efficiency at high brightness, and improves the brightness stability and efficiency of organic light-emitting devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118984601A_ABST
    Figure CN118984601A_ABST
Patent Text Reader

Abstract

The organic light-emitting device comprises an anode, a hole injection layer, an organic light-emitting layer, an electron injection layer and a cathode which are sequentially stacked, at least one of the hole injection layer and the electron injection layer comprises a plurality of first regions and a plurality of second regions; wherein the first areas and the second areas are alternately arranged; in the same film layer, the doping concentration of the first region is greater than the doping concentration of the second region, or in the same film layer, the carrier migration rate of the first region in the thickness direction is greater than the carrier migration rate of the second region in the thickness direction; and when the hole injection layer and the electron injection layer both comprise a first region and a second region, the vertical projection of the first region of the hole injection layer on the electron injection layer is overlapped with the first region of the electron injection layer. According to the invention, the quenching probability of excitons and polarons can be reduced, and efficiency roll-off under high brightness is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of organic light emitting technology, and in particular to an organic light emitting device. Background Art

[0002] In the actual application of organic light-emitting devices, when the current increases and the brightness rises, there are too many excitons in the light-emitting layer, and quenching between triplet excitons and between triplet excitons and polarons will occur, resulting in efficiency roll-off of the organic light-emitting device at high brightness. Summary of the invention

[0003] The present invention provides an organic light-emitting device to reduce the probability of exciton and polaron quenching and avoid efficiency roll-off at high brightness.

[0004] According to one aspect of the present invention, there is provided an organic light emitting device, comprising:

[0005] An anode, a hole injection layer, an organic light-emitting layer, an electron injection layer and a cathode are stacked in sequence;

[0006] At least one of the hole injection layer and the electron injection layer comprises a plurality of first regions and a plurality of second regions; wherein the first regions and the second regions are arranged alternately; in the same film layer, the doping concentration of the first region is greater than the doping concentration of the second region, or, in the same film layer, the carrier migration rate of the first region along the thickness direction is greater than the carrier migration rate of the second region along the thickness direction;

[0007] When both the hole injection layer and the electron injection layer include a first region and a second region, the first region of the hole injection layer overlaps with the first region of the electron injection layer in a vertical projection of the electron injection layer.

[0008] Optionally, when the doping concentration of the first region is greater than the doping concentration of the second region, the Fermi level difference between the first region and the second region is greater than 0.4 eV;

[0009] When the carrier mobility rate of the first region along the thickness direction is greater than the carrier mobility rate of the second region along the thickness direction, the ratio of the carrier mobility rate of the first region along the thickness direction to the carrier mobility rate of the second region along the thickness direction is greater than or equal to 10.

[0010] Optionally, the first region is a doped region, and the second region is a non-doped region; or, the first region is a doped region, and the second region is a hollow region; or, the first region is a non-doped region, and the second region is a hollow region.

[0011] Optionally, in the same film layer, along the direction from the first region to the adjacent second region, the sizes of the adjacent first region and the adjacent second region are both smaller than 2 times of the exciton diffusion distance.

[0012] Optionally, at least one layer of the anode and the cathode includes a non-hollow area and a hollow area;

[0013] A vertical projection of the non-hollowed-out area on the organic light-emitting layer overlaps with a vertical projection of the first region on the organic light-emitting layer.

[0014] Optionally, the anode and the cathode are a metal layer having a hollow area, a metal oxide layer having a hollow area, or a metal nanowire layer.

[0015] According to another aspect of the present invention, there is provided an organic light emitting device, comprising:

[0016] An anode, a hole injection layer, at least two organic light-emitting layers, an electron injection layer and a cathode are stacked in sequence; a charge generation layer is arranged between each two adjacent organic light-emitting layers;

[0017] The charge generation layer includes a first N-type layer and a first P-type layer, and at least one of the first N-type layer and the first P-type layer includes a plurality of third regions and a plurality of fourth regions; wherein the third regions and the fourth regions are arranged alternately, and when both the first N-type layer and the first P-type layer include the third region and the fourth region, the third regions of the first N-type layer and the first P-type layer overlap each other at a vertical projection of the organic light-emitting layer; in the same film layer, the doping concentration of the third region is greater than the doping concentration of the fourth region, or, in the same film layer, the carrier migration rate of the third region along the thickness direction is greater than the carrier migration rate of the fourth region along the thickness direction;

[0018] Alternatively, the charge generation layer includes a second N-type layer, a metal layer, and a second P-type layer stacked in sequence, and at least one of the second N-type layer, the metal layer, and the second P-type layer includes a plurality of fifth regions and a plurality of sixth regions; wherein the fifth region and the sixth region are arranged alternately, and when two or more film layers in the second N-type layer, the metal layer, and the second P-type layer include the fifth region and the sixth region, the fifth regions of the two or more film layers overlap with each other at a vertical projection of the organic light-emitting layer; when the second N-type layer and the second P-type layer include the fifth region and the sixth region, in the same film layer, the doping concentration of the fifth region is greater than the doping concentration of the sixth region, or, in the same film layer, the carrier migration rate of the fifth region along the thickness direction is greater than the carrier migration rate of the sixth region along the thickness direction; when the metal layer includes the fifth region and the sixth region, the sixth region is a hollow region.

[0019] Optionally, at least one of the hole injection layer and the electron injection layer includes a plurality of seventh regions and a plurality of eighth regions; wherein the seventh regions and the eighth regions are arranged alternately; in the same film layer, the doping concentration of the seventh region is greater than the doping concentration of the eighth region, or, in the same film layer, the carrier migration rate of the seventh region along the thickness direction is greater than the carrier migration rate of the eighth region along the thickness direction;

[0020] When the charge generation layer includes a first P-type layer and a first N-type layer, a vertical projection of the seventh region on the organic light-emitting layer overlaps with a vertical projection of the third region on the organic light-emitting layer;

[0021] When the charge generation layer includes a second N-type layer, a metal layer, and a second P-type layer, a vertical projection of the seventh region on the organic light-emitting layer overlaps with a vertical projection of the fifth region on the organic light-emitting layer.

[0022] Optionally, when the doping concentration of the seventh region is greater than the doping concentration of the eighth region, the Fermi level difference between the seventh region and the eighth region is greater than 0.4 eV;

[0023] When the carrier mobility rate of the seventh region along the thickness direction is greater than the carrier mobility rate of the eighth region along the thickness direction, the ratio of the carrier mobility rate of the seventh region along the thickness direction to the carrier mobility rate of the eighth region along the thickness direction is greater than or equal to 10.

[0024] Optionally, when the doping concentration of the third region is greater than the doping concentration of the fourth region, the Fermi level difference between the third region and the fourth region is greater than 0.4 eV;

[0025] When the carrier mobility rate of the third region along the thickness direction is greater than the carrier mobility rate of the fourth region along the thickness direction, the ratio of the carrier mobility rate of the third region along the thickness direction to the carrier mobility rate of the fourth region along the thickness direction is greater than or equal to 10;

[0026] When the doping concentration of the fifth region is greater than the doping concentration of the sixth region, the Fermi level difference between the fifth region and the sixth region is greater than 0.4 eV;

[0027] When the carrier mobility rate of the fifth region along the thickness direction is greater than the carrier mobility rate of the sixth region along the thickness direction, the ratio of the carrier mobility rate of the fifth region along the thickness direction to the carrier mobility rate of the sixth region along the thickness direction is greater than or equal to 10.

[0028] Optionally, in the same film layer, along the direction from the third region to the adjacent fourth region, the sizes of the adjacent third region and the adjacent fourth region are both less than 2 times the exciton diffusion distance;

[0029] The third region is a doped region and the fourth region is a non-doped region, or the third region is a doped region and the fourth region is a hollow region, or the third region is a non-doped region and the fourth region is a hollow region.

[0030] Optionally, in the same film layer, along the direction from the fifth region to the adjacent sixth region, the sizes of the adjacent fifth region and the adjacent sixth region are both less than 2 times the exciton diffusion distance;

[0031] When the second N-type layer and the second P-type layer include a fifth region and a sixth region, the fifth region is a doped region and the sixth region is a non-doped region, or the fifth region is a doped region and the sixth region is a hollow region, or the fifth region is a non-doped region and the sixth region is a hollow region.

[0032] The organic light-emitting device of the embodiment of the present invention comprises an anode, a hole injection layer, an organic light-emitting layer, an electron injection layer and a cathode which are stacked in sequence; at least one of the hole injection layer and the electron injection layer comprises a plurality of first regions and a plurality of second regions; the first regions and the second regions are arranged alternately; the doping concentration of the first region is greater than the doping concentration of the second region, or the carrier migration rate of the first region along the thickness direction is greater than the carrier migration rate of the second region along the thickness direction. The first region can inject more electrons or holes into the organic light-emitting layer, and more holes in the region corresponding to the first region in the organic light-emitting layer recombine with electrons to generate excitons. The second region injects less electrons or holes into the organic light-emitting layer, or does not inject electrons or holes, and the region corresponding to the second region of the organic light-emitting layer generates few excitons or no excitons, and the region corresponding to the second region of the organic light-emitting layer generates few polarons or no polarons. The excitons in the region corresponding to the first region in the organic light-emitting layer diffuse to the region corresponding to the second region in the organic light-emitting layer, so that each region of the organic light-emitting layer emits light. Since the excitons in the organic light-emitting layer corresponding to the second region diffuse, there are few or no polarons in the organic light-emitting layer corresponding to the second region, thereby reducing the quenching probability between excitons and polarons and avoiding the roll-off of the luminous efficiency of the organic light-emitting device at high brightness.

[0033] It should be understood that the contents described in this section are not intended to identify the key or important features of the embodiments of the present invention, nor are they intended to limit the scope of the present invention. Other features of the present invention will become easily understood through the following description. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0035] Figure 1 is a schematic diagram of an organic light-emitting device provided by an embodiment of the present invention;

[0036] Figure 2 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention;

[0037] Figure 3 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention;

[0038] Figure 4 is a schematic diagram of a hole injection layer;

[0039] Figure 5 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention;

[0040] Figure 6 is a schematic diagram of an anode provided by an embodiment of the present invention;

[0041] Figure 7 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention;

[0042] Figure 8 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention;

[0043] Fig. 9 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention;

[0044] Fig.10 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention;

[0045] Fig.11 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention;

[0046] Fig.12 is a schematic diagram of a doping layer provided by an embodiment of the present invention;

[0047] Fig.13 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention;

[0048] Fig.14 It is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention. DETAILED DESCRIPTION

[0049] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.

[0050] It should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0051] An embodiment of the present invention provides an organic light emitting device, Figure 1 is a schematic diagram of an organic light-emitting device provided by an embodiment of the present invention, Figure 2 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention, Figure 3 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention, Figure 4 is a schematic diagram of a hole injection layer, see Figure 1-Figure 4 , the organic light emitting device comprises:

[0052] An anode 10, a hole injection layer 20, an organic light emitting layer 30, an electron injection layer 40 and a cathode 50 are stacked in sequence;

[0053] At least one of the hole injection layer 20 and the electron injection layer 40 includes a plurality of first regions 11 and a plurality of second regions 12; wherein the first regions 11 and the second regions 12 are arranged alternately; in the same film layer, the doping concentration of the first region 11 is greater than the doping concentration of the second region 12, or, in the same film layer, the carrier migration rate of the first region 11 along the thickness direction is greater than the carrier migration rate of the second region 12 along the thickness direction.

[0054] When both the hole injection layer 20 and the electron injection layer 40 include the first region 11 and the second region 12 , the vertical projection of the first region 11 of the hole injection layer 20 overlaps with the first region 11 of the electron injection layer 40 .

[0055] The hole injection layer 20 is in contact with the anode 10. The electron injection layer 40 is in contact with the cathode 50. The hole injection layer 20 is used to inject holes into the organic light-emitting layer 30. The electron injection layer 40 is used to inject electrons into the organic light-emitting layer 30. At least one of the hole injection layer 20 and the electron injection layer 40 includes a plurality of first regions 11 and a plurality of second regions 12, and only the hole injection layer 20 includes a plurality of first regions 11 and a plurality of second regions 12. Figure 1 ), or only the electron injection layer 40 may include a plurality of first regions 11 and a plurality of second regions 12 ( Figure 2 ), or the electron injection layer 40 and the hole injection layer 20 may both include a plurality of first regions 11 and a plurality of second regions 12 ( Figure 3 The carrier migration rate of the first region 11 along the thickness direction is the carrier migration rate in the direction from the first region 11 to the organic light emitting layer 30. The carrier migration rate of the second region 12 along the thickness direction is the carrier migration rate in the direction from the second region 12 to the organic light emitting layer 30.

[0056] Specifically, refer to Figure 1 When the hole injection layer 20 includes the first region 11 and the second region 12, the doping concentration of the first region 11 is greater than the doping concentration of the second region 12 or the carrier migration rate of the first region 11 along the thickness direction is greater than the carrier migration rate of the second region 12 along the thickness direction, so that the first region 11 can inject more holes into the organic light-emitting layer 30, and more holes in the region corresponding to the first region 11 in the organic light-emitting layer 30 are recombined with electrons to generate excitons. Since the doping concentration of the second region 12 is low or the carrier migration rate is low, the second region 12 injects fewer holes or no holes into the organic light-emitting layer 30, and the region corresponding to the second region 12 of the organic light-emitting layer 30 generates few excitons or no excitons, and the region corresponding to the second region 12 of the organic light-emitting layer 30 generates few polarons or no polarons. The excitons in the region corresponding to the first region 11 in the organic light-emitting layer 30 diffuse to the region corresponding to the second region 12 in the organic light-emitting layer 30, so that each region of the organic light-emitting layer 30 emits light. Since the excitons in the area corresponding to the second area 12 in the organic light-emitting layer 30 diffuse, there are few or no polarons in the area corresponding to the second area 12 in the organic light-emitting layer 30, thereby reducing the quenching probability between excitons and polarons and avoiding the roll-off of the luminous efficiency of the organic light-emitting device at high brightness.

[0057] refer to Figure 2When the electron injection layer 40 includes the first region 11 and the second region 12, the doping concentration of the first region 11 is greater than the doping concentration of the second region 12 or the carrier migration rate of the first region 11 along the thickness direction is greater than the carrier migration rate of the second region 12 along the thickness direction, so that the first region 11 can inject more electrons into the organic light-emitting layer 30, and more holes and electrons in the region corresponding to the first region 11 in the organic light-emitting layer 30 are recombined to generate excitons. Since the doping concentration of the second region 12 is low or the carrier migration rate is low, the second region 12 injects less electrons or no electrons into the organic light-emitting layer 30, and the region corresponding to the second region 12 of the organic light-emitting layer 30 generates few excitons or no excitons, and the region corresponding to the second region 12 of the organic light-emitting layer 30 generates few polarons or no polarons. The excitons in the region corresponding to the first region 11 in the organic light-emitting layer 30 diffuse to the region corresponding to the second region 12 in the organic light-emitting layer 30, so that each region of the organic light-emitting layer 30 emits light. Since the excitons in the region corresponding to the second region 12 in the organic light-emitting layer 30 diffuse, there are few or no polarons in the region corresponding to the second region 12 in the organic light-emitting layer 30, thereby reducing the quenching probability between excitons and polarons and avoiding the roll-off of the luminous efficiency of the organic light-emitting device at high brightness.

[0058] In addition, reference Figure 3When both the hole injection layer 20 and the electron injection layer 40 include the first region 11 and the second region 12, the vertical projection of the first region 11 of the hole injection layer 20 on the electron injection layer 40 overlaps with the first region 11 of the electron injection layer 40. In this way, the first region 11 of the electron injection layer 40 injects more electrons into the organic light-emitting layer 30, the first region 11 of the hole injection layer 20 injects more holes into the organic light-emitting layer 30, and more holes in the organic light-emitting layer 30 corresponding to both the electron injection layer 40 and the first region 11 of the hole injection layer 20 are combined with electrons to generate excitons. The second region 12 of the electron injection layer 40 injects fewer electrons or no electrons into the organic light-emitting layer 30, the second region 12 of the hole injection layer 20 injects fewer holes or no holes into the organic light-emitting layer 30, and the region of the organic light-emitting layer 30 corresponding to the second region of the hole injection layer 20 and the second region 12 of the electron injection layer 40 generates few excitons or no excitons, thereby generating few polarons or no polarons. Excitons in the region of the organic light-emitting layer 30 corresponding to both the electron injection layer 40 and the first region 11 of the hole injection layer 20 diffuse to the region of the organic light-emitting layer 30 corresponding to the second region 12 of the electron injection layer 40 and the hole injection layer 20, so that each region of the organic light-emitting layer 30 emits light. Since the excitons in the region corresponding to the second region 12 of the electron injection layer 40 and the hole injection layer 20 in the organic light-emitting layer 30 diffuse, there are few or no polarons in the region corresponding to the second region 12 of the electron injection layer 40 and the hole injection layer 20 in the organic light-emitting layer 30, so the quenching probability between excitons and polarons can be reduced, and the light-emitting efficiency roll-off of the organic light-emitting device at high brightness can be avoided.

[0059] Exemplarily, the vertical projection of the first region 11 of the hole injection layer 20 on the electron injection layer 40 overlaps with the first region 11 of the electron injection layer 40, and the vertical projection of the second region 12 of the hole injection layer 20 on the electron injection layer 40 overlaps with the second region 12 of the electron injection layer 40. In this way, the electron injection layer 40 and the hole injection layer 20 can be prepared using the same mask, which can reduce the process cost.

[0060] The organic light-emitting device of the embodiment of the present invention comprises an anode 10, a hole injection layer 20, an organic light-emitting layer 30, an electron injection layer 40 and a cathode 50 which are stacked in sequence; at least one of the hole injection layer 20 and the electron injection layer 40 comprises a plurality of first regions 11 and a plurality of second regions 12; the first regions 11 and the second regions 12 are arranged alternately; the doping concentration of the first region 11 is greater than the doping concentration of the second region 12, or the carrier migration rate of the first region 11 along the thickness direction is greater than the carrier migration rate of the second region 12 along the thickness direction, so that the first region 11 can inject more electrons or holes into the organic light-emitting layer 30, and more holes in the region corresponding to the first region 11 in the organic light-emitting layer 30 are recombined with electrons to generate excitons. The second region 12 injects less electrons or holes into the organic light-emitting layer 30, or does not inject electrons or holes, and the region corresponding to the second region 12 of the organic light-emitting layer 30 generates few excitons or no excitons, and the region corresponding to the second region 12 of the organic light-emitting layer 30 generates few polarons or no polarons. The excitons in the region corresponding to the first region 11 in the organic light-emitting layer 30 diffuse to the region corresponding to the second region 12 in the organic light-emitting layer 30, so that each region of the organic light-emitting layer 30 emits light. Since the excitons in the region corresponding to the second region 12 in the organic light-emitting layer 30 diffuse, there are few or no polarons in the region corresponding to the second region 12 in the organic light-emitting layer 30, so the quenching probability between the excitons and the polarons can be reduced, and the luminous efficiency roll-off of the organic light-emitting device at high brightness can be avoided.

[0061] On the basis of the above embodiment, optionally, when the doping concentration of the first region 11 is greater than the doping concentration of the second region 12, the Fermi level difference between the first region 11 and the second region 12 is greater than 0.4 eV;

[0062] When the carrier mobility rate of the first region 11 along the thickness direction is greater than the carrier mobility rate of the second region 12 along the thickness direction, the ratio of the carrier mobility rate of the first region 11 along the thickness direction to the carrier mobility rate of the second region 12 along the thickness direction is greater than or equal to 10.

[0063] Specifically, when the hole injection layer 20 includes the first region 11 and the second region 12, the Fermi energy difference between the first region 11 and the second region 12 is greater than 0.4 eV. When the electron injection layer 40 includes the first region 11 and the second region 12, the Fermi energy difference between the first region 11 and the second region 12 is greater than 0.4 eV. During the evaporation process of the electron injection layer 40 or the hole injection layer 20, different doping concentrations in the first region 11 and the second region 12 can be achieved by shielding with a mask. After the evaporation of the electron injection layer 40 or the hole injection layer 20 is completed, the electron injection layer 40 or the hole injection layer 20 can be irradiated with ultraviolet light by shielding with a mask, and the mobility of the illuminated area decreases, while the non-illuminated area remains unchanged, thereby forming a mobility gap.

[0064] refer to Figure 1 When the hole injection layer 20 includes the first region 11 and the second region 12, since holes need to cross an energy barrier during the process of being injected from the hole injection layer 20 into the organic light-emitting layer 30, the Fermi level difference between the first region 11 and the second region 12 of the hole injection layer 20 is set to be greater than 0.4 eV, so that the potential barrier crossed by the holes in the first region 11 of the hole injection layer 20 during the process of being injected into the organic light-emitting layer 30 is smaller, which can improve the hole injection efficiency. The potential barrier crossed by the holes in the second region 12 of the hole injection layer 20 during the process of being injected into the organic light-emitting layer is larger, and holes cannot be injected into the organic light-emitting layer 30 or only a small number of holes can be injected, thereby ensuring that the region corresponding to the organic light-emitting layer 30 and the second region 12 generates fewer polarons or no polarons.

[0065] When the hole injection layer 20 includes the first region 11 and the second region 12, the ratio of the carrier migration rate of the first region 11 along the thickness direction to the carrier migration rate of the second region 12 along the thickness direction is greater than or equal to 10, so that the hole injection rate of the first region 11 of the hole injection layer 20 is faster, and the first region 11 can inject more holes into the organic light-emitting layer 30, and the second region 12 of the hole injection layer 20 injects fewer holes into the organic light-emitting layer 30, thereby ensuring that the area corresponding to the organic light-emitting layer 30 and the second region 12 generates fewer polarons or no polarons.

[0066] refer to Figure 2 When the electron injection layer 40 includes the first region 11 and the second region 12, since electrons need to cross an energy level barrier during the process of being injected from the electron injection layer 40 into the organic light-emitting layer 30, the Fermi level difference between the first region 11 and the second region 12 of the electron injection layer 40 is set to be greater than 0.4 eV, so that the potential barrier crossed by the electrons in the first region 11 of the electron injection layer 40 during the process of being injected into the organic light-emitting layer 30 is smaller, which can improve the electron injection efficiency. The potential barrier crossed by the electrons in the second region 12 of the electron injection layer 40 during the process of being injected into the organic light-emitting layer is larger, and electrons cannot be injected into the organic light-emitting layer 30 or only a small number of electrons can be injected, thereby ensuring that the region corresponding to the organic light-emitting layer 30 and the second region 12 generates fewer polarons or no polarons.

[0067] When the electron injection layer 40 includes the first region 11 and the second region 12, the ratio of the carrier migration rate of the first region 11 along the thickness direction to the carrier migration rate of the second region 12 along the thickness direction is greater than or equal to 10, so that the electron injection rate of the first region 11 of the electron injection layer 20 is faster, and the first region 11 can inject more electrons into the organic light-emitting layer 30, and the second region 12 of the electron injection layer 40 injects fewer electrons into the organic light-emitting layer 30, thereby ensuring that the region corresponding to the organic light-emitting layer 30 and the second region 12 generates fewer polarons or no polarons.

[0068] Based on the above embodiments, optionally, the first region 11 is a doped region and the second region 12 is a non-doped region; or, the first region 11 is a doped region and the second region 12 is a hollow region, or the first region 11 is a non-doped region and the second region 12 is a hollow region.

[0069] Specifically, the second region 12 is a hollow region, that is, the second region 12 has no electron injection material or hole injection material, the hole injection layer 20 is in a grid shape or the electron injection layer 40 is in a grid shape.

[0070] The first region 11 is a doped region and the second region 12 is a non-doped region, or when the first region 11 is a doped region and the second region 12 is a hollow region, or when the first region 11 is a non-doped region and the second region 12 is a hollow region, only the first region 11 transmits carriers (electrons / holes) to the organic light-emitting layer 30, and excitons are only generated in the region of the organic light-emitting layer 30 corresponding to the first region 11. The light emission in the region corresponding to the organic light-emitting layer 30 and the second region 12 is achieved by exciton diffusion. There are no polarons in the region corresponding to the organic light-emitting layer 30 and the second region 12. Therefore, the quenching between excitons and polarons can be further reduced, and the luminous efficiency roll-off under high brightness can be further improved.

[0071] On the basis of the above embodiment, optionally, in the same film layer, along the direction from the first region 11 to the adjacent second region 12 , the sizes of the adjacent first region 11 and the adjacent second region 12 are both smaller than 2 times the exciton diffusion distance.

[0072] Specifically, refer to Figure 4, the excitons in the region corresponding to the second region 12 in the organic light-emitting layer 30 are diffused from the excitons in the region corresponding to the first region 11. If the sizes of the adjacent first region 11 and second region 12 are too large, the excitons cannot diffuse to the entire region corresponding to the second region 12 in the organic light-emitting layer 30, affecting the luminescence of the organic light-emitting layer 30. Along the direction from the first region 11 to the adjacent second region 12, the sizes of the adjacent first region 11 and second region 12 are both less than 2 times the exciton diffusion distance, so that the excitons in the region corresponding to the first region 11 in the organic light-emitting layer 30 can diffuse to various positions of the region corresponding to the second region 12 in the organic light-emitting layer 30, so that various positions of the organic light-emitting layer 30 can emit light.

[0073] Exemplary, reference Figure 4 , taking the first region 11 and the second region 12 adjacent to each other along the first direction X as an example, the first region 11 points to the direction of the second region 12, that is, along the first direction X, the first dimension D1 of the first region 11 and the second dimension D2 of the second region 12 are both less than 2 times of the exciton diffusion distance. Optionally, the first dimension D1 and the second dimension D2 are in the range of 10-300nm. For example, the first dimension D1 is 20nm, 50nm, 100nm, 150nm, 200nm or 300nm, etc., and the second dimension D2 is 20nm, 50nm, 100nm, 150nm, 200nm or 300nm, etc.

[0074] Taking the first region 11 and the second region 12 adjacent to each other along the second direction Y as an example, along the direction from the first region 11 to the second region 12, that is, along the second direction Y, the third dimension D3 of the first region 11 and the fourth dimension D4 of the second region 12 are both less than 2 times the exciton diffusion distance. Optionally, the third dimension D3 and the fourth dimension D4 are in the range of 10-300nm. For example, the third dimension D3 is 20nm, 50nm, 100nm, 150nm, 200nm or 300nm, and the fourth dimension D4 is 20nm, 50nm, 100nm, 150nm, 200nm or 300nm, etc.

[0075] Figure 5 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention, Figure 6 is a schematic diagram of an anode provided by an embodiment of the present invention, with reference to Figure 5 and Figure 6 , based on the above embodiment, optionally, at least one layer of the anode 10 and the cathode 50 includes a non-hollow area 21 and a hollow area 22;

[0076] The vertical projection of the non-hollow area 21 on the organic light-emitting layer 30 overlaps with the vertical projection of the first area 11 on the organic light-emitting layer 30 .

[0077] Specifically, at least one of the anode 10 and the cathode 50 includes a hollow area 22 and a non-hollow area 21, that is, at least one of the anode 10 and the cathode 50 is in a grid shape. When the anode 10 includes the non-hollow area 21 and the hollow area 22, only the non-hollow area 21 of the anode 10 injects holes into the organic light-emitting layer 30, so that excitons are generated only in the region of the organic light-emitting layer 30 corresponding to the non-hollow area 21, further ensuring that no polarons are generated in the region of the organic light-emitting layer 30 corresponding to the hollow area 22, and further reducing the quenching of excitons and polarons.

[0078] When the cathode 50 includes a non-hollow area 21 and a hollow area 22, only the non-hollow area 21 of the cathode 50 injects electrons into the organic light-emitting layer 30, so that excitons are generated only in the area corresponding to the organic light-emitting layer 30 and the non-hollow area 21, further ensuring that no polarons are generated in the area corresponding to the organic light-emitting layer 30 and the hollow area 22, further reducing the quenching of excitons and polarons.

[0079] The vertical projection of the non-hollow area 21 on the organic light-emitting layer 30 coincides with the vertical projection of the first area 11 on the organic light-emitting layer 30, so that the area corresponding to the first area 11 and the non-hollow area 21 in the organic light-emitting layer 30 is the same area. The area corresponding to the first area 11 and the non-hollow area 21 in the organic light-emitting layer 30 has a higher carrier recombination rate and can generate more excitons. More excitons can diffuse to the area corresponding to the second area 11 and the non-hollow area 21 in the organic light-emitting layer 30, thereby improving the luminous efficiency.

[0080] On the basis of the above embodiment, optionally, the anode 10 and the cathode 50 are a metal layer having a hollow region 22 , a metal oxide layer having a hollow region 22 , or a metal nanowire layer.

[0081] Specifically, the anode 10 and the cathode 50 may be patterned metal layers or patterned metal oxide layers. For example, the metal oxide layer may be an indium tin oxide (ITO) layer. In addition, the anode 10 may also be formed using metal nanowires. The diameter of the metal nanowires may be 5-200 nm, and the distance between the metal nanowires may be 5-200 nm. For example, the diameter of the metal nanowires may be 10 nm, 20 nm, 50 nm, 100 nm, or 150 nm, and the distance between the metal nanowires may be 10 nm, 20 nm, 50 nm, 100 nm, or 150 nm, etc.

[0082] An embodiment of the present invention further provides an organic light emitting device, Figure 7 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention, Figure 8 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention, Fig. 9 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention, Fig.10is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention, Fig.11 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention, Fig.12 is a schematic diagram of a first P-type layer provided in an embodiment of the present invention, referring to Figure 7-Figure 12 , the organic light emitting device comprises:

[0083] An anode 10, a hole injection layer 20, at least two organic light-emitting layers 30, an electron injection layer 40 and a cathode 50 are stacked in sequence; a charge generation layer 60 is disposed between each two adjacent organic light-emitting layers 30;

[0084] refer to Figure 7-Figure 8 , the charge generation layer 60 includes a first N-type layer 62 and a first P-type layer 61, at least one of the first N-type layer 62 and the first P-type layer 61 includes a plurality of third regions 13 and a plurality of fourth regions 14; wherein the third regions 13 and the fourth regions 14 are arranged alternately, and when both the first N-type layer 62 and the first P-type layer 61 include the third regions 13 and the fourth regions 14, the vertical projections of the third regions 13 of the first N-type layer 62 and the first P-type layer 61 on the organic light-emitting layer 30 overlap each other; in the same film layer, the doping concentration of the third region 13 is greater than the doping concentration of the fourth region 14, or, in the same film layer, the carrier migration rate of the third region 13 along the thickness direction is greater than the carrier migration rate of the fourth region 14 along the thickness direction;

[0085] Alternatively, refer to Figure 9-11 The charge generation layer 60 includes a second N-type layer 65, a metal layer 63, and a second P-type layer 64 which are stacked in sequence, and at least one of the second N-type layer 65, the metal layer 63, and the second P-type layer 64 includes a plurality of fifth regions 15 and a plurality of sixth regions 16; wherein the fifth regions 15 and the sixth regions 16 are arranged alternately, and when two or more film layers in the second N-type layer 65, the metal layer 63, and the second P-type layer 64 include the fifth region 15 and the sixth region 16, the vertical projections of the fifth regions 15 of the two or more film layers on the organic light-emitting layer 30 overlap with each other; when the second N-type layer 65 and the second P-type layer 64 include the fifth region 15 and the sixth region 16, in the same film layer, the doping concentration of the fifth region 15 is greater than the doping concentration of the sixth region 16, or, in the same film layer, the carrier migration rate of the fifth region 15 along the thickness direction is greater than the carrier migration rate of the sixth region 16 along the thickness direction; when the metal layer 63 includes the fifth region 15 and the sixth region 16, the sixth region 16 is a hollow region.

[0086] Specifically, refer to Figure 7 and Figure 8 When the charge generation layer 60 includes the first N-type layer 62 and the first P-type layer 61 , the first P-type layer 61 is disposed on a side of the first N-type layer 62 adjacent to the cathode 50 .

[0087] refer to Figure 7 , when the first N-type layer 62 includes the third region 13 and the fourth region 14, the doping concentration of the third region 13 of the first N-type layer 62 is greater than the doping concentration of the fourth region 14 of the first N-type layer 62, or the carrier mobility rate of the third region 13 of the first N-type layer 62 along the thickness direction is greater than the carrier mobility rate of the fourth region 14 of the first N-type layer 62 along the thickness direction. Figure 8 When the first P-type layer 61 includes multiple third regions 13 and multiple fourth regions 14, the doping concentration of the third region 13 of the first P-type layer 61 is greater than the doping concentration of the fourth region 14 of the first P-type layer 61, or the carrier mobility rate of the third region 13 of the first P-type layer 61 along the thickness direction is greater than the carrier mobility rate of the fourth region 14 of the first P-type layer 61 along the thickness direction.

[0088] When the first N-type layer 62 or the first P-type layer 61 includes the third region 13 and the fourth region 14, the third region 13 can inject more electrons or holes into the organic light-emitting layers 30 on both sides, respectively, and more holes in the region corresponding to the third region 13 in the organic light-emitting layer 30 recombine with electrons to generate excitons. Since the fourth region 14 has a low doping concentration or a low carrier migration rate, the fourth region 14 injects fewer electrons or holes into the organic light-emitting layer 30, or no electrons or holes, and the region corresponding to the fourth region 14 of the organic light-emitting layer 30 generates few excitons or no excitons, so that the region corresponding to the fourth region 14 of the organic light-emitting layer 30 generates few polarons or no polarons. The excitons in the region corresponding to the third region 13 in the organic light-emitting layer 30 diffuse to the region corresponding to the fourth region 14 in the organic light-emitting layer 30, so that each region of the organic light-emitting layer 30 emits light. Since the excitons in the region corresponding to the fourth region 14 in the organic light-emitting layer 30 diffuse, there are few or no polarons in the region corresponding to the fourth region 14 in the organic light-emitting layer 30, thereby reducing the quenching probability between excitons and polarons and avoiding efficiency roll-off of the organic light-emitting device at high brightness.

[0089] refer to Figure 8, when both the first N-type layer 62 and the first P-type layer 61 include the third region 13 and the fourth region 14, the third region 13 of the first N-type layer 62 and the first P-type layer 61 overlap each other in the vertical projection of the organic light-emitting layer 30 (the overlapping region is called the overlapping region). Since the third region 13 of the first N-type layer 62 and the first P-type layer 61 can both inject more holes or electrons, the organic light-emitting layer 30 has more holes and electrons that recombine to produce excitons in the region corresponding to the overlapping region, ensuring that the organic light-emitting layer 30 can produce more excitons. At the same time, it is ensured that the region corresponding to the fourth region 14 of the organic light-emitting layer 30 can have fewer electrons and holes that recombine, produce fewer polarons, reduce the quenching probability of polarons and excitons, and avoid the efficiency roll-off of the organic light-emitting device at high brightness. Exemplarily, the third region 13 of the first N-type layer 62 and the first P-type layer 61 overlap each other in the vertical projection of the organic light-emitting layer 30 and can overlap.

[0090] refer to Figure 9-11 When the charge generation layer 60 includes a second P-type layer 64 , a metal layer 63 and a second N-type layer 65 , the second P-type layer 64 is disposed on a side of the metal layer 63 adjacent to the cathode 50 , and the second N-type layer 65 is disposed on a side of the metal layer 63 adjacent to the anode 10 .

[0091] refer to Fig. 9 , the second N-type layer 65 includes a plurality of fifth regions 15 and a plurality of sixth regions 16, the doping concentration of the fifth region 15 of the second N-type layer 65 is greater than the doping concentration of the sixth region 16 of the second N-type layer 65, or the carrier mobility rate of the fifth region 15 of the second N-type layer 65 along the thickness direction is greater than the carrier mobility rate of the sixth region 16 of the second N-type layer 65 along the thickness direction. Fig.10 The second P-type layer 64 includes a plurality of fifth regions 15 and a plurality of sixth regions 16, the doping concentration of the fifth region 15 of the second P-type layer 64 is greater than the doping concentration of the sixth region 16 of the second P-type layer 64, or the carrier migration rate of the fifth region 15 of the second P-type layer 64 along the thickness direction is greater than the carrier migration rate of the sixth region 16 of the second P-type layer 64 along the thickness direction.

[0092] refer to Fig. 9 and Fig.10When the second N-type layer 65 or the second P-type layer 64 includes a plurality of fifth regions 15 and a plurality of sixth regions 16, the fifth region 15 can inject more electrons or holes into the organic light-emitting layers 30 on both sides, respectively, and more holes in the region corresponding to the fifth region 15 in the organic light-emitting layer 30 recombine with electrons to generate excitons. Since the doping concentration of the sixth region 16 is low or the carrier migration rate is low, the sixth region 16 injects less electrons or holes into the organic light-emitting layer 30, or does not inject electrons or holes, and the region corresponding to the sixth region 16 of the organic light-emitting layer 30 generates few excitons or no excitons, so that the region corresponding to the sixth region 16 of the organic light-emitting layer 30 generates few polarons or no polarons. The excitons in the region corresponding to the fifth region 15 in the organic light-emitting layer 30 diffuse to the region corresponding to the sixth region 16 in the organic light-emitting layer 30, so that each region of the organic light-emitting layer 30 emits light. Since the excitons in the region corresponding to the sixth region 16 in the organic light-emitting layer 30 diffuse, there are few or no polarons in the region corresponding to the sixth region 16 in the organic light-emitting layer 30, thereby reducing the quenching probability between excitons and polarons and avoiding efficiency roll-off of the organic light-emitting device at high brightness.

[0093] refer to Fig.11 When the metal layer 63 includes the fifth region 15 and the sixth region 16, the sixth region 16 is a hollow region. Only the non-hollow region (fifth region 15) of the metal layer 63 injects holes or electrons into the organic light-emitting layer 30, so that excitons are generated only in the region of the organic light-emitting layer 30 corresponding to the fifth region 15, ensuring that no polarons are generated in the region of the organic light-emitting layer 30 corresponding to the sixth region 16, thereby reducing the quenching of excitons and polarons.

[0094] In addition, when two or more film layers in the second N-type layer 65, the metal layer 63, and the second P-type layer 64 all include the fifth region 15 and the sixth region 16, the fifth regions 15 of the two or more film layers overlap each other in the vertical projections of the organic light-emitting layer 30. This arrangement allows the overlapping area of ​​the fifth region 15 to inject more electrons or holes into the organic light-emitting layer 30, so that the area corresponding to the overlapping area of ​​the organic light-emitting layer 30 and the fifth region 15 has more holes and electrons that recombine to produce excitons, ensuring that the organic light-emitting layer 30 can produce more excitons. At the same time, it is ensured that the area corresponding to the organic light-emitting layer 30 and the sixth region 16 can have fewer electrons and holes that recombine, produce fewer polarons, reduce the quenching probability of polarons and excitons, and avoid the roll-off of the light-emitting efficiency of the organic light-emitting device at high brightness. Exemplarily, the vertical projections of the fifth region 15 of the second N-type layer 65, the metal layer 63, and the second P-type layer 64 overlap each other in the organic light-emitting layer 30.

[0095] In the organic light-emitting device of the embodiment of the present invention, the charge generation layer 60 includes a first N-type layer 62 and a first P-type layer 61, at least one of the first N-type layer 62 and the first P-type layer 61 includes a plurality of third regions 13 and a plurality of fourth regions 14; or, the charge generation layer 60 includes a second N-type layer 65, a metal layer 63, and a second P-type layer 64 stacked in sequence, at least one of the second N-type layer 65, the metal layer 63, and the second P-type layer 64 includes a plurality of fifth regions 15 and a plurality of sixth regions 16. The third region 13 and the fifth region 15 have a high doping concentration or a high carrier migration rate, so that the third region 13 and the fifth region 15 can inject more carriers (electrons or holes) into the organic light-emitting layer 30, and more holes in the organic light-emitting layer 30 corresponding to the third region 13 and the fifth region 15 are recombined with electrons to generate excitons. Since the fourth region 14 and the sixth region 16 have a low doping concentration or a low carrier migration rate or the sixth region 16 of the metal layer 63 is a hollow region, the fourth region 14 and the sixth region 16 inject fewer or no carriers into the organic light-emitting layer 30, and the region of the organic light-emitting layer 30 corresponding to the fourth region 14 and the sixth region 16 generates few or no excitons, and the region of the organic light-emitting layer 30 corresponding to the fourth region 14 and the sixth region 16 generates few or no polarons. The excitons in the region of the organic light-emitting layer 30 corresponding to the third region 13 and the fifth region 15 diffuse to the region of the organic light-emitting layer 30 corresponding to the fourth region 14 and the sixth region 16, so that each region of the organic light-emitting layer 30 emits light. Since the excitons in the organic light-emitting layer 30 corresponding to the fourth region 14 and the sixth region 16 diffuse, there are few or no polarons in the region corresponding to the fourth region 14 and the sixth region 16 in the organic light-emitting layer 30, thereby reducing the quenching probability between excitons and polarons and avoiding the roll-off of the light-emitting efficiency of the organic light-emitting device at high brightness.

[0096] Fig.13 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention, Fig.14 is a schematic diagram of another organic light-emitting device provided by an embodiment of the present invention, with reference to Fig.13 and Fig.14 , based on the above embodiment, optionally, at least one of the hole injection layer 20 and the electron injection layer 40 includes a plurality of seventh regions 17 and a plurality of eighth regions 18; wherein the seventh regions 17 and the eighth regions 18 are arranged alternately; in the same film layer, the doping concentration of the seventh region 17 is greater than the doping concentration of the eighth region 18, or, in the same film layer, the carrier migration rate of the seventh region 17 along the thickness direction is greater than the carrier migration rate of the eighth region 18 along the thickness direction;

[0097] refer to Fig.13, when the charge generation layer 60 includes the first P-type layer 61 and the first N-type layer 62 , the vertical projection of the seventh region 17 on the organic light-emitting layer 30 overlaps with the vertical projection of the third region 13 on the organic light-emitting layer 30 ;

[0098] When the charge generation layer 60 includes the second P-type layer 64 , the metal layer 63 and the second N-type layer 65 , the vertical projection of the seventh region 17 on the organic light emitting layer 30 overlaps with the vertical projection of the fifth region 15 on the organic light emitting layer 30 .

[0099] Specifically, refer to Fig.13 , only the hole injection layer 20 may include a plurality of seventh regions 17 and eighth regions 18. Fig.14 Alternatively, only the electron injection layer 40 may include the seventh region 17 and the eighth region 18. Alternatively, both the hole injection layer 20 and the electron injection layer 40 may include the seventh region 17 and the eighth region 18.

[0100] refer to Fig.13 When the hole injection layer 20 includes the seventh region 17 and the eighth region 18, the doping concentration of the seventh region 17 is greater than the doping concentration of the eighth region 18 or the carrier migration rate of the seventh region 17 along the thickness direction is greater than the carrier migration rate of the eighth region 18 along the thickness direction, so that the seventh region 17 can inject more holes into the organic light-emitting layer 30, and more holes in the region corresponding to the seventh region 17 in the organic light-emitting layer 30 are recombined with electrons to generate excitons. Since the doping concentration of the eighth region 18 is low or the carrier migration rate is low, the eighth region 18 injects fewer holes or no holes into the organic light-emitting layer 30, and the region corresponding to the eighth region 18 of the organic light-emitting layer 30 generates few excitons or no excitons, and the region corresponding to the eighth region 18 of the organic light-emitting layer 30 generates few polarons or no polarons. The excitons in the region corresponding to the seventh region 17 in the organic light-emitting layer 30 diffuse to the region corresponding to the eighth region 18 in the organic light-emitting layer 30, so that each region of the organic light-emitting layer 30 emits light. Since the excitons in the area corresponding to the eighth area 18 in the organic light-emitting layer 30 diffuse, there are few or no polarons in the area corresponding to the eighth area 18 in the organic light-emitting layer 30, thereby reducing the quenching probability between excitons and polarons and avoiding the roll-off of the light-emitting efficiency of the organic light-emitting device at high brightness.

[0101] refer to Fig.14When the electron injection layer 40 includes the seventh region 17 and the eighth region 18, the doping concentration of the seventh region 17 is greater than the doping concentration of the eighth region 18 or the carrier migration rate of the seventh region 17 along the thickness direction is greater than the carrier migration rate of the eighth region 18 along the thickness direction, so that the seventh region 17 can inject more electrons into the organic light-emitting layer 30, and more holes and electrons in the region corresponding to the seventh region 17 in the organic light-emitting layer 30 are recombined to generate excitons. Since the doping concentration of the eighth region 18 is low or the carrier migration rate is low, the eighth region 18 injects less electrons or no electrons into the organic light-emitting layer 30, and the region corresponding to the eighth region 18 of the organic light-emitting layer 30 generates few excitons or no excitons, and the region corresponding to the eighth region 18 of the organic light-emitting layer 30 generates few polarons or no polarons. The excitons in the region corresponding to the seventh region 17 in the organic light-emitting layer 30 diffuse to the region corresponding to the eighth region 18 in the organic light-emitting layer 30, so that each region of the organic light-emitting layer 30 emits light. Since the excitons in the region corresponding to the eighth region 18 in the organic light-emitting layer 30 diffuse, there are few or no polarons in the region corresponding to the eighth region 18 in the organic light-emitting layer 30, thereby reducing the quenching probability between excitons and polarons and avoiding efficiency roll-off of the organic light-emitting device at high brightness.

[0102] refer to Fig.13 , the vertical projection of the seventh region 17 on the organic light-emitting layer 30 overlaps with the vertical projection of the third region 13 on the organic light-emitting layer 30, so that the area corresponding to the area where the organic light-emitting layer 30 overlaps with the third region 13 and the seventh region 17 has more holes and electrons that recombine to generate excitons, ensuring that the organic light-emitting layer 30 can generate more excitons. At the same time, it is ensured that the area corresponding to the organic light-emitting layer 30 and the eighth region 18 and the fourth region 14 can have fewer electrons and holes that recombine, generate fewer polarons, reduce the quenching probability of polarons and excitons, and avoid efficiency roll-off of the organic light-emitting device at high brightness.

[0103] refer to Fig.14 , the vertical projection of the seventh region 17 on the organic light-emitting layer 30 overlaps with the vertical projection of the fifth region 15 on the organic light-emitting layer 30, and the vertical projection of the eighth region 18 on the organic light-emitting layer 30 overlaps with the vertical projection of the sixth region 16 on the organic light-emitting layer 30. This allows the organic light-emitting layer 30, the fifth region 15, and the seventh region 17 to overlap with each other, so that the region corresponding to the region where the fifth region 15 and the seventh region 17 overlap has more holes and electrons that recombine to produce excitons, ensuring that the organic light-emitting layer 30 can produce more excitons. At the same time, it ensures that the region corresponding to the organic light-emitting layer 30, the eighth region 18, and the sixth region 16 can have fewer electrons and holes that recombine, produce fewer polarons, reduce the quenching probability of polarons and excitons, and avoid efficiency roll-off at high brightness of the organic light-emitting device. Exemplary, refer to Fig.13, the vertical projections of the third region 13 and the seventh region 17 on the organic light-emitting layer 30 overlap, and the vertical projections of the fourth region 14 and the eighth region 18 on the organic light-emitting layer 30 overlap. Fig.14 , the vertical projections of the fifth region 15 and the seventh region 17 on the organic light-emitting layer 30 overlap, and the vertical projections of the sixth region 16 and the eighth region 18 on the organic light-emitting layer 30 overlap.

[0104] Optionally, when the doping concentration of the seventh region 17 is greater than the doping concentration of the eighth region 18, the Fermi level difference between the seventh region 17 and the eighth region 18 is greater than 0.4 eV;

[0105] When the carrier mobility rate of the seventh region 17 along the thickness direction is greater than the carrier mobility rate of the eighth region 18 along the thickness direction, the ratio of the carrier mobility rate of the seventh region 17 along the thickness direction to the carrier mobility rate of the eighth region 18 along the thickness direction is greater than or equal to 10.

[0106] Based on the above embodiment, optionally, refer to Figure 7-Figure 12 , when the doping concentration of the third region 13 is greater than the doping concentration of the fourth region 14, the Fermi level difference between the third region 13 and the fourth region 14 is greater than 0.4 eV;

[0107] When the carrier mobility rate of the third region 13 along the thickness direction is greater than the carrier mobility rate of the fourth region 14 along the thickness direction, the ratio of the carrier mobility rate of the third region 13 along the thickness direction to the carrier mobility rate of the fourth region 14 along the thickness direction is greater than or equal to 10;

[0108] When the doping concentration of the fifth region 15 is greater than the doping concentration of the sixth region 16 , the Fermi level difference between the fifth region 15 and the sixth region 16 is greater than 0.4 eV;

[0109] When the carrier mobility rate of the fifth region 15 along the thickness direction is greater than the carrier mobility rate of the sixth region 16 along the thickness direction, the ratio of the carrier mobility rate of the fifth region 15 along the thickness direction to the carrier mobility rate of the sixth region 16 along the thickness direction is greater than or equal to 10.

[0110] refer to Figure 7-Figure 8When the first P-type layer 61 includes the third region 13 and the fourth region 14, since holes need to cross an energy barrier during the process of being injected from the first P-type layer 61 to the organic light-emitting layer 30, the Fermi level difference between the third region 13 and the fourth region 14 of the first P-type layer 61 is set to be greater than 0.4 eV, so that the potential barrier crossed by the holes in the third region 13 of the first P-type layer 61 during the process of being injected into the organic light-emitting layer 30 is smaller, which can improve the hole injection efficiency. The potential barrier crossed by the holes in the fourth region 14 of the first P-type layer 61 during the process of being injected into the organic light-emitting layer is larger, and holes cannot be injected into the organic light-emitting layer 30 or only a small number of holes can be injected, thereby ensuring that the region corresponding to the organic light-emitting layer 30 and the fourth region 14 generates fewer polarons or no polarons.

[0111] When the first P-type layer 61 includes the third region 13 and the fourth region 14, the ratio of the carrier migration rate of the third region 13 along the thickness direction to the carrier migration rate of the fourth region 14 along the thickness direction is greater than or equal to 10, so that the hole injection rate of the third region 13 of the first P-type layer 61 is faster, and the third region 13 can inject more holes into the organic light-emitting layer 30. The fourth region 14 of the first P-type layer 61 injects holes into the organic light-emitting layer 30 at a slower rate and injects fewer holes, thereby ensuring that the organic light-emitting layer 30 generates fewer polarons or no polarons in the region corresponding to the fourth region 14.

[0112] refer to Figure 8 When the first N-type layer 62 includes the third region 13 and the fourth region 14, since electrons need to cross an energy level barrier during the process of being injected from the first N-type layer 62 to the organic light-emitting layer 30, the Fermi level difference between the third region 13 and the fourth region 14 of the first N-type layer 62 is set to be greater than 0.4 eV, so that the potential barrier crossed by the electrons in the third region 13 of the first N-type layer 62 during the process of being injected into the organic light-emitting layer 30 is smaller, which can improve the electron injection efficiency. The potential barrier crossed by the electrons in the fourth region 14 of the first N-type layer 62 during the process of being injected into the organic light-emitting layer is larger, and electrons cannot be injected into the organic light-emitting layer 30 or only a small number of electrons can be injected, thereby ensuring that the region corresponding to the organic light-emitting layer 30 and the fourth region 14 generates fewer polarons or no polarons.

[0113] When the first N-type layer 62 includes the third region 13 and the fourth region 14, the ratio of the carrier migration rate of the third region 13 along the thickness direction to the carrier migration rate of the fourth region 14 along the thickness direction is greater than or equal to 10, so that the electron injection rate of the third region 13 of the first N-type layer 62 is faster, and the third region 13 can inject more electrons into the organic light-emitting layer 30, and the fourth region 14 of the first N-type layer 62 injects fewer electrons into the organic light-emitting layer 30, thereby ensuring that the region corresponding to the organic light-emitting layer 30 and the fourth region 14 generates fewer polarons or no polarons.

[0114] When the doping concentration of the fifth region 15 is greater than the doping concentration of the sixth region 16, the Fermi level difference between the fifth region 15 and the sixth region 16 is greater than 0.4 eV and the carrier mobility rate of the fifth region 15 along the thickness direction is greater than the carrier mobility rate of the sixth region 16 along the thickness direction, the ratio of the carrier mobility rate of the fifth region 15 along the thickness direction to the carrier mobility rate of the sixth region 16 along the thickness direction is greater than or equal to 10, which is similar to the effect of the above embodiment and will not be repeated here.

[0115] Based on the above embodiment, optionally, continue to refer to Fig.12 In the same film layer, along the direction from the third region 13 to the adjacent fourth region 14, the sizes of the adjacent third region 13 and the adjacent fourth region 14 are both less than twice the exciton diffusion distance.

[0116] Specifically, refer to Fig.11 and Fig.12 , the excitons in the region corresponding to the fourth region 14 in the organic light-emitting layer 30 are diffused from the excitons in the region corresponding to the third region 13. If the sizes of the adjacent third region 13 and fourth region 14 are too large, the excitons cannot diffuse to the entire region corresponding to the fourth region 14 in the organic light-emitting layer 30, affecting the luminescence of the organic light-emitting layer 30. Along the direction from the third region 13 to the adjacent fourth region 14, the sizes of the adjacent third region 13 and fourth region 14 are both less than 2 times the exciton diffusion distance, so that the excitons in the region corresponding to the third region 13 in the organic light-emitting layer 30 can diffuse to various positions of the region corresponding to the fourth region 14 in the organic light-emitting layer 30, so that various positions of the organic light-emitting layer 30 can emit light.

[0117] Exemplary, reference Fig.12, taking the third region 13 and the fourth region 14 adjacent along the first direction X as an example, along the direction from the third region 13 to the fourth region 14, that is, along the first direction X, the fifth dimension D5 of the third region 13 and the sixth dimension D6 of the fourth region 14 are both less than 2 times the exciton diffusion distance. Optionally, the fifth dimension D5 and the sixth dimension D6 are in the range of 10-300nm. Taking the third region 13 and the fourth region 14 adjacent along the second direction Y as an example, along the direction from the third region 13 to the fourth region 14, that is, along the second direction Y, the seventh dimension D7 of the third region 13 and the eighth dimension D8 of the fourth region 14 are both less than 2 times the exciton diffusion distance. Optionally, the seventh dimension D7 and the eighth dimension D8 are in the range of 10-300nm. For example, the fifth dimension D5 is 20nm, 50nm, 100nm, 150nm, 200nm or 300nm, etc., the sixth dimension D6 is 20nm, 50nm, 100nm, 150nm, 200nm or 300nm, etc., the seventh dimension D7 is 20nm, 50nm, 100nm, 150nm, 200nm or 300nm, etc., and the eighth dimension D8 is 20nm, 50nm, 100nm, 150nm, 200nm or 300nm, etc.

[0118] Based on the above embodiments, optionally, the third region 13 is a doped region and the fourth region 14 is a non-doped region, or the third region 13 is a doped region and the fourth region 14 is a hollow region, or the third region 13 is a non-doped region and the fourth region 14 is a hollow region.

[0119] Specifically, the fourth region 14 is a hollow region, that is, the first P-type layer 61 or the first N-type layer 62 is in a grid shape.

[0120] When the third region 13 is a doped region and the fourth region 14 is a non-doped region, or when the third region 13 is a doped region and the fourth region 14 is a hollow region, or when the third region 13 is a non-doped region and the fourth region 14 is a hollow region, only the third region 13 transmits carriers (electrons / holes) to the organic light-emitting layer 30, and excitons are only generated in the region corresponding to the organic light-emitting layer 30 and the third region 13. The light emission in the region corresponding to the organic light-emitting layer 30 and the fourth region 14 is achieved by exciton diffusion. There are no polarons in the region corresponding to the organic light-emitting layer 30 and the fourth region 14. Therefore, the quenching between excitons and polarons can be further reduced, and the luminous efficiency roll-off under high brightness can be further improved.

[0121] In addition, reference Figure 7-Figure 12, the anode 10 and the cathode 50 may also include a hollow area and a non-hollow area. The vertical projection of the non-hollow area on the organic light-emitting layer 30 overlaps with the vertical projection of the third area 13 or the fifth area 15 on the organic light-emitting layer 30. Exemplarily, the vertical projection of the non-hollow area on the organic light-emitting layer 30 coincides with the vertical projection of the third area 13 or the fifth area 15 on the organic light-emitting layer 30.

[0122] On the basis of the above embodiment, optionally, in the same film layer, along the direction from the fifth region 15 to the adjacent sixth region 16, the sizes of the adjacent fifth region 15 and sixth region 16 are both less than twice the exciton diffusion distance; so that the excitons in the area corresponding to the third region 13 in the organic light-emitting layer 30 can diffuse to various positions of the area corresponding to the fourth region 14 in the organic light-emitting layer 30, so that various positions of the organic light-emitting layer 30 can emit light.

[0123] On the basis of the above embodiment, optionally, when the second N-type layer 65 and the second P-type layer 63 include the fifth region and the sixth region, the fifth region 15 is a doped region and the sixth region 16 is a non-doped region, or the fifth region 15 is a doped region and the sixth region 16 is a hollow region, or the fifth region 15 is a non-doped region and the sixth region 16 is a hollow region. Only the fifth region 15 transmits carriers (electrons / holes) to the organic light-emitting layer 30, and excitons are only generated in the region of the organic light-emitting layer 30 corresponding to the fifth region 15. The region of the organic light-emitting layer 30 corresponding to the sixth region 16 emits light through exciton diffusion. There is no polaron in the region of the organic light-emitting layer 30 corresponding to the sixth region 16, so the quenching between excitons and polarons can be further reduced, and the efficiency roll-off under high brightness can be further improved.

[0124] It should be understood that the various forms of processes shown above can be used to reorder, add or delete steps. For example, the steps described in the present invention can be executed in parallel, sequentially or in different orders, as long as the desired results of the technical solution of the present invention can be achieved, and this document does not limit this.

[0125] The above specific implementations do not constitute a limitation on the protection scope of the present invention. It should be understood by those skilled in the art that various modifications, combinations, sub-combinations and substitutions can be made according to design requirements and other factors. Any modification, equivalent substitution and improvement made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. An organic light-emitting device, characterized in that: include: An anode, a hole injection layer, an organic light-emitting layer, an electron injection layer and a cathode are stacked in sequence; At least one of the hole injection layer and the electron injection layer comprises a plurality of first regions and a plurality of second regions; wherein the first regions and the second regions are arranged alternately; in the same film layer, the doping concentration of the first region is greater than the doping concentration of the second region, or, in the same film layer, the carrier migration rate of the first region along the thickness direction is greater than the carrier migration rate of the second region along the thickness direction; When both the hole injection layer and the electron injection layer include a first region and a second region, the first region of the hole injection layer overlaps with the first region of the electron injection layer in a vertical projection of the electron injection layer.

2. The organic light emitting device according to claim 1, characterized in that: When the doping concentration of the first region is greater than the doping concentration of the second region, the Fermi level difference between the first region and the second region is greater than 0.4 eV; When the carrier mobility rate of the first region along the thickness direction is greater than the carrier mobility rate of the second region along the thickness direction, the ratio of the carrier mobility rate of the first region along the thickness direction to the carrier mobility rate of the second region along the thickness direction is greater than or equal to 10.

3. The organic light emitting device according to claim 2, characterized in that: The first region is a doped region, and the second region is a non-doped region; or, the first region is a doped region, and the second region is a hollow region; or, the first region is a non-doped region, and the second region is a hollow region.

4. The organic light emitting device according to claim 1, characterized in that: In the same film layer, along the direction from the first region to the adjacent second region, the sizes of the adjacent first region and the adjacent second region are both smaller than 2 times of the exciton diffusion distance.

5. The organic light emitting device according to claim 1, characterized in that: At least one layer of the anode and the cathode includes a non-hollow area and a hollow area; A vertical projection of the non-hollowed-out area on the organic light-emitting layer overlaps with a vertical projection of the first region on the organic light-emitting layer.

6. The organic light emitting device according to claim 5, characterized in that: The anode and the cathode are a metal layer with a hollow area, a metal oxide layer with a hollow area, or a metal nanowire layer.

7. An organic light-emitting device, characterized in that: include: An anode, a hole injection layer, at least two organic light-emitting layers, an electron injection layer and a cathode are stacked in sequence; a charge generation layer is arranged between each two adjacent organic light-emitting layers; The charge generation layer includes a first N-type layer and a first P-type layer, and at least one of the first N-type layer and the first P-type layer includes a plurality of third regions and a plurality of fourth regions; wherein the third regions and the fourth regions are arranged alternately, and when both the first N-type layer and the first P-type layer include the third region and the fourth region, the third regions of the first N-type layer and the first P-type layer overlap each other at a vertical projection of the organic light-emitting layer; in the same film layer, the doping concentration of the third region is greater than the doping concentration of the fourth region, or, in the same film layer, the carrier migration rate of the third region along the thickness direction is greater than the carrier migration rate of the fourth region along the thickness direction; Alternatively, the charge generation layer includes a second N-type layer, a metal layer, and a second P-type layer stacked in sequence, and at least one of the second N-type layer, the metal layer, and the second P-type layer includes a plurality of fifth regions and a plurality of sixth regions; wherein the fifth region and the sixth region are arranged alternately, and when two or more film layers in the second N-type layer, the metal layer, and the second P-type layer include the fifth region and the sixth region, the fifth regions of the two or more film layers overlap with each other at a vertical projection of the organic light-emitting layer; when the second N-type layer and the second P-type layer include the fifth region and the sixth region, in the same film layer, the doping concentration of the fifth region is greater than the doping concentration of the sixth region, or, in the same film layer, the carrier migration rate of the fifth region along the thickness direction is greater than the carrier migration rate of the sixth region along the thickness direction; when the metal layer includes the fifth region and the sixth region, the sixth region is a hollow region.

8. The organic light emitting device according to claim 7, characterized in that: At least one of the hole injection layer and the electron injection layer comprises a plurality of seventh regions and a plurality of eighth regions; wherein the seventh regions and the eighth regions are arranged alternately; in the same film layer, the doping concentration of the seventh region is greater than the doping concentration of the eighth region, or, in the same film layer, the carrier migration rate of the seventh region along the thickness direction is greater than the carrier migration rate of the eighth region along the thickness direction; When the charge generation layer includes a first P-type layer and a first N-type layer, a vertical projection of the seventh region on the organic light-emitting layer overlaps with a vertical projection of the third region on the organic light-emitting layer; When the charge generation layer includes a second N-type layer, a metal layer, and a second P-type layer, a vertical projection of the seventh region on the organic light-emitting layer overlaps with a vertical projection of the fifth region on the organic light-emitting layer; When the doping concentration of the seventh region is greater than the doping concentration of the eighth region, the Fermi level difference between the seventh region and the eighth region is greater than 0.4 eV; When the carrier mobility rate of the seventh region along the thickness direction is greater than the carrier mobility rate of the eighth region along the thickness direction, the ratio of the carrier mobility rate of the seventh region along the thickness direction to the carrier mobility rate of the eighth region along the thickness direction is greater than or equal to 10.

9. The organic light emitting device according to claim 7, characterized in that: When the doping concentration of the third region is greater than the doping concentration of the fourth region, the Fermi level difference between the third region and the fourth region is greater than 0.4 eV; When the carrier mobility rate of the third region along the thickness direction is greater than the carrier mobility rate of the fourth region along the thickness direction, the ratio of the carrier mobility rate of the third region along the thickness direction to the carrier mobility rate of the fourth region along the thickness direction is greater than or equal to 10; When the doping concentration of the fifth region is greater than the doping concentration of the sixth region, the Fermi level difference between the fifth region and the sixth region is greater than 0.4 eV; When the carrier mobility rate of the fifth region along the thickness direction is greater than the carrier mobility rate of the sixth region along the thickness direction, the ratio of the carrier mobility rate of the fifth region along the thickness direction to the carrier mobility rate of the sixth region along the thickness direction is greater than or equal to 10.

10. The organic light emitting device according to claim 7, characterized in that: In the same film layer, along the direction from the third region to the adjacent fourth region, the sizes of the adjacent third region and the adjacent fourth region are both less than 2 times the exciton diffusion distance; The third region is a doped region, and the fourth region is a non-doped region, or the third region is a doped region, and the fourth region is a hollow region, or the third region is a non-doped region, and the fourth region is a hollow region; In the same film layer, along the direction from the fifth region to the adjacent sixth region, the sizes of the adjacent fifth region and the adjacent sixth region are both less than 2 times the exciton diffusion distance; When the second N-type layer and the second P-type layer include a fifth region and a sixth region, the fifth region is a doped region and the sixth region is a non-doped region, or the fifth region is a doped region and the sixth region is a hollow region, or the fifth region is a non-doped region and the sixth region is a hollow region.