Mixed conditioner containing silicone oil and vegetable fat

By modifying the mixture of silicone oil and vegetable oil, a mixed conditioning agent containing modified hydroxyl silicone oil was prepared, which solved the problem of insufficient stability of silicone oil conditioning agents and improved the stability of the product and the smoothness and shine of the hair.

CN118986791APending Publication Date: 2024-11-22FOSHAN HEDE NEW MATERIAL CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411456309.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-18
Publication Date
2024-11-22

Smart Images

  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention belongs to the technical field of conditioner preparation, and particularly relates to a mixed conditioner containing silicone oil and vegetable fat. The preparation method of the mixed conditioner provided by the invention comprises the following steps: mixing modified silicone oil, coconut oil, Morocco nut oil, an emulsifier and water to obtain the mixed conditioner, the modified silicone oil is modified hydroxyl silicone oil, and the preparation method comprises the following steps: mixing allyl-1, 2, 4-trimethyl-1, 2, 4-trimethyl-1, 2, 4-trimethyl-1, 2, 4-trimethyl-1, 2, 4- The preparation method comprises the following steps: mixing 1, 3-sultone, a first organic solvent, water, sodium hypochlorite, copper chloride and tetrabutylammonium bromide, reacting, concentrating an organic layer, mixing with an alkaline aqueous solution, carrying out hydrolysis reaction, concentrating, adding boron trifluoride diethyl etherate and bis [2-[2-(2-chloroethyoxyl) ethyoxyl] ethyl] ether into a concentrated product, stirring, reacting, adding hydroxyl silicone oil, continuously reacting, filtering, washing, and drying to obtain a finished product. Adding a second organic solvent into the reaction liquid for extraction, and concentrating and washing an organic layer to obtain the modified hydroxyl silicone oil. The mixed conditioner prepared by the invention is beneficial to improving the smoothness, softness and stability of hair.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of conditioning agent preparation, and in particular relates to a mixed conditioning agent comprising silicone oil and vegetable oil, and further relates to a mixed conditioning agent comprising silicone oil and vegetable oil and having the function of enhancing hair gloss and hydrophobicity. Background Art

[0002] As people's living standards improve, their requirements for shampoo and hair care products are getting higher and higher. As an indispensable ingredient in shampoo and hair care products, conditioners have received more and more attention and research. At present, the types of domestic conditioners can be roughly divided into quaternary ammonium salt conditioners, cationic polymer conditioners, silicone conditioners, etc.

[0003] Silicone oil has good hydrophobicity and low surface tension. Adding silicone oil to shampoo and hair care products can make it easy to adhere to hair due to its excellent wettability and hydrophobicity, achieving the effect of smoothing rough hair. At the same time, its excellent film-forming properties can make hair smoother. However, silicone oil has insufficient affinity for water, resulting in poor stability of products with silicone oil as the main ingredient. Summary of the invention

[0004] Therefore, the technical problem to be solved by the present invention is to overcome the defect of poor stability of conditioner products using silicone oil as the main ingredient, and further provide a mixed conditioner containing silicone oil and vegetable oil.

[0005] In order to solve the above problems, the scheme of the present invention is as follows: A method for preparing a mixed conditioner comprises the following steps: Mixing modified silicone oil, coconut oil, argan oil, emulsifier and water, stirring to obtain the mixed conditioner; The modified silicone oil is a modified hydroxy silicone oil. The preparation method of the modified hydroxy silicone oil comprises the following steps: mixing propenyl-1,3-sultone, a first organic solvent, water, sodium hypochlorite, a first catalyst and a quaternary ammonium salt and reacting them, standing and stratifying after the reaction, separating an organic layer, concentrating the organic layer under reduced pressure, and then mixing the concentrated product with an alkaline aqueous solution and performing a hydrolysis reaction, and concentrating under reduced pressure after the hydrolysis reaction is completed, and then adding a second catalyst and bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether to the concentrated product to stir the reaction, and then adding hydroxy silicone oil to continue stirring the reaction, and after the reaction is completed, adding a second organic solvent to the reaction solution for extraction, concentrating the organic layer under reduced pressure, and washing the concentrate to obtain the modified hydroxy silicone oil; The first catalyst is selected from cupric chloride; The quaternary ammonium salt is selected from tetrabutylammonium bromide; The second catalyst is boron trifluoride etherate.

[0006] The modification process schematic diagram of the modified hydroxy silicone oil of the present invention is as follows: .

[0007] Preferably, the mass ratio of the propenyl-1,3-sultone, the first organic solvent, water, sodium hypochlorite, the first catalyst and the quaternary ammonium salt is (120-125): (150-200): (150-200): (110-130): (2-4): (0.2-0.8); When allyl-1,3-sultone, the first organic solvent, water, sodium hypochlorite, the first catalyst and the quaternary ammonium salt are mixed and reacted, the reaction temperature is 75-80° C. and the reaction time is 2-8 hours.

[0008] Preferably, the first organic solvent is selected from one of dichloroethane, carbon tetrachloride and toluene.

[0009] Preferably, the alkaline aqueous solution is selected from one of a sodium hydroxide aqueous solution and a potassium hydroxide aqueous solution, and the mass concentration of the alkaline aqueous solution is 30-40%; The mass ratio of the propenyl-1,3-sultone to the alkaline aqueous solution is 1:(0.8-1.2).

[0010] Preferably, the molar ratio of propenyl-1,3-sultone to bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether is 1:(3-3.2); The added mass of the second catalyst is 1.5-3% of propenyl-1,3-sultone; The added mass of the hydroxy silicone oil is 3-5 times that of propenyl-1,3-sultone.

[0011] Preferably, in the preparation method of the modified hydroxy silicone oil, the stirring reaction temperature is 50-60°C, the stirring reaction time is 1-4h, and the continued stirring reaction temperature is 50-60°C, and the continued stirring reaction time is 1-4h.

[0012] Preferably, the hydrolysis reaction temperature is 40-50°C, and the hydrolysis reaction time is 1-3h; The second organic solvent is selected from dichloromethane, and the washing step is performed with water.

[0013] Preferably, silicone oil, coconut oil, argan oil, emulsifier and water are mixed and stirred at a temperature of 45-55° C. for 2-5 hours.

[0014] Preferably, the mass ratio of the silicone oil, coconut oil, argan oil, emulsifier and water is (35-45): (1-5): (1-5): (1-9): (40-60); The emulsifier is selected from TEA dodecylbenzenesulfonate (CAS No. 90194-42-6).

[0015] Optionally, the coconut oil can be selected from medium-carbon chain coconut oil, and the silicone oil can be selected from nano-scale or micron-scale particle size silicone oil. The present invention does not specifically limit the viscosity of the hydroxy silicone oil, and the commonly used hydroxy silicone oil in the art can realize the present invention. Optionally, the viscosity of the hydroxy silicone oil is 50-200CP.

[0016] The present invention also provides a mixed conditioner comprising silicone oil and vegetable oil, wherein the mixed conditioner is prepared by the above-mentioned preparation method.

[0017] The technical solution of the present invention has the following advantages: The preparation method of the mixed conditioner provided by the present invention comprises the following steps: mixing and stirring modified silicone oil, coconut oil, argan oil, an emulsifier and water; the obtained mixed conditioner can combine the excellent spreadability of coconut oil, the high refractive index property of argan oil and the repairability of silicone oil; and the formed conditioning agent is beneficial to improving the smoothness, softness and glossiness of hair.

[0018] Furthermore, in order to improve the stability of the conditioner, the present invention further modifies the silicone oil used, firstly halogenating and hydrolyzing allyl-1,3-sultone, and then further hydrolyzing it under alkaline conditions to obtain a sulfonate with trihydroxyl groups, and then reacting the trihydroxyl sulfonate with bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether under the action of a catalyst to form an ether, which is further combined with hydroxy silicone oil to form a modified hydroxy silicone oil, which not only introduces a hydrophilic sulfonic acid group, but also connects the hydroxy silicone oils to each other through a long ether chain of the trihydroxyl sulfonate, thereby greatly improving the hydrophilicity and stability of the modified hydroxy silicone oil. DETAILED DESCRIPTION

[0019] The following examples are provided for further understanding of the present invention, but are not intended to limit the best mode of implementation and do not limit the scope of protection of the present invention.

[0020] The experimental steps or conditions not specified in the following embodiments of the present invention can be implemented according to the conventional experimental steps and conditions used in the existing literature in the field. The reagents or instruments used without specifying the manufacturer are all conventional reagents or instruments that can be purchased commercially.

[0021] Example 1 This embodiment provides a method for preparing a mixed conditioning agent, comprising the following steps: 1) 120g of propenyl-1,3-sultone, 150g of dichloroethane, 180g of water, 111.6g of sodium hypochlorite, 2.5g of copper chloride and 0.5g of tetrabutylammonium bromide were mixed and reacted at a temperature of 78°C for 5h. After the reaction was completed, the mixture was allowed to stand and the organic layer was separated. The organic layer was concentrated under reduced pressure to remove the organic solvent. The concentrated product was then mixed with 100g of a 35% sodium hydroxide aqueous solution and subjected to a hydrolysis reaction at a temperature of 45°C for 1.5h. The hydrolysis reaction was completed. After that, the mixture was concentrated under reduced pressure to remove water, and then 2 g of boron trifluoride etherate and 957 g of bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether were added to the concentrated product, stirred and reacted at 55°C for 2 h, and then 400 g of hydroxy silicone oil (viscosity 150CP) was added and stirred and reacted at 55°C for 2 h. After the reaction, 400 g of dichloromethane was added to the reaction solution for extraction, and the organic layer was concentrated under reduced pressure to remove the organic solvent and unreacted bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether, and the concentrate was washed with water to obtain modified hydroxy silicone oil; 2) 40 g of modified hydroxy silicone oil, 3 g of coconut oil, 3 g of argan oil, 4 g of TEA dodecylbenzenesulfonate and 50 g of water were mixed and stirred at 50° C. for 2.5 h to obtain the mixed conditioner.

[0022] Example 2 This embodiment provides a method for preparing a mixed conditioning agent, comprising the following steps: 1) 120g of propenyl-1,3-sultone, 150g of dichloroethane, 180g of water, 115g of sodium hypochlorite, 2.0g of copper chloride and 0.8g of tetrabutylammonium bromide were mixed and reacted at a temperature of 78°C for 5h. After the reaction was completed, the mixture was allowed to stand and the layers were separated. The organic layer was concentrated under reduced pressure to remove the organic solvent. The concentrated product was then mixed with 105g of a 35% sodium hydroxide aqueous solution and subjected to a hydrolysis reaction at a temperature of 45°C for 1.5h. After the hydrolysis reaction was completed, , concentrate under reduced pressure to remove water, then add 2g of boron trifluoride etherate and 965g of bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether to the concentrated product, stir and react at 55°C for 2h, then add 400g of hydroxy silicone oil (viscosity 150CP) and continue to stir and react at 55°C for 2h. After the reaction, add 400g of dichloromethane to the reaction solution for extraction, concentrate the organic layer under reduced pressure to remove the organic solvent and unreacted bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether, and wash the concentrate with water to obtain modified hydroxy silicone oil; 2) 40 g of modified hydroxy silicone oil, 3.5 g of coconut oil, 3.2 g of argan oil, 4 g of TEA dodecylbenzenesulfonate and 50 g of water were mixed and stirred at 50° C. for 2.5 h to obtain the mixed conditioner.

[0023] Example 3 This embodiment provides a method for preparing a mixed conditioning agent, comprising the following steps: 1) 120g of propenyl-1,3-sultone, 150g of dichloroethane, 180g of water, 115g of sodium hypochlorite, 2.0g of copper chloride and 0.8g of tetrabutylammonium bromide were mixed and reacted at a temperature of 78°C for 5h. After the reaction was completed, the mixture was allowed to stand for stratification, and the organic layer was separated. The organic layer was concentrated under reduced pressure to remove the organic solvent. The concentrated product was then mixed with 100g of a 35% sodium hydroxide aqueous solution and subjected to a hydrolysis reaction at a temperature of 45°C for 1.5h. After the hydrolysis reaction was completed, The mixture was concentrated under reduced pressure to remove water, and then 2.5 g of boron trifluoride etherate and 960 g of bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether were added to the concentrated product, and the mixture was stirred and reacted at 55°C for 3 h. Then 400 g of hydroxy silicone oil (viscosity 150 CP) was added, and the mixture was stirred and reacted at 55°C for 2 h. After the reaction, 400 g of dichloromethane was added to the reaction solution for extraction. The organic layer was concentrated under reduced pressure to remove the organic solvent and unreacted bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether, and the concentrate was washed with water to obtain modified hydroxy silicone oil. 2) 42 g of modified hydroxy silicone oil, 3.0 g of coconut oil, 3.2 g of argan oil, 3.8 g of TEA dodecylbenzenesulfonate and 50 g of water were mixed and stirred at 50° C. for 2.5 h to obtain the mixed conditioner.

[0024] Example 4 This embodiment provides a method for preparing a mixed conditioning agent, comprising the following steps: 1) 125g of propenyl-1,3-sultone, 160g of ethylene dichloride, 180g of water, 115g of sodium hypochlorite, 2.0g of cupric chloride and 0.8g of tetrabutylammonium bromide were mixed and reacted at a temperature of 78°C for 5h. After the reaction was completed, the mixture was allowed to stand and the layers were separated. The organic layer was concentrated under reduced pressure to remove the organic solvent. The concentrated product was then mixed with 100g of a 35% by mass sodium hydroxide aqueous solution and subjected to a hydrolysis reaction at a temperature of 45°C for 2h. After the hydrolysis reaction was completed, the mixture was reduced to a temperature of 45°C for 2h. The mixture was concentrated under reduced pressure to remove water, and then 2.5 g of boron trifluoride etherate and 960 g of bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether were added to the concentrated product, stirred and reacted at 55°C for 3 h, and then 400 g of hydroxy silicone oil (viscosity 150CP) was added and stirred and reacted at 55°C for 2 h. After the reaction, 400 g of dichloromethane was added to the reaction solution for extraction, and the organic layer was concentrated under reduced pressure to remove the organic solvent and unreacted bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether, and the concentrate was washed with water to obtain modified hydroxy silicone oil; 2) 42 g of modified hydroxy silicone oil, 3.5 g of coconut oil, 3.2 g of argan oil, 4.0 g of TEA dodecylbenzenesulfonate and 50 g of water were mixed and stirred at 50° C. for 2.5 h to obtain the mixed conditioner.

[0025] Example 5 This embodiment provides a method for preparing a mixed conditioning agent, comprising the following steps: 1) 125g of propenyl-1,3-sultone, 150g of dichloroethane, 180g of water, 115g of sodium hypochlorite, 2.0g of cupric chloride and 0.8g of tetrabutylammonium bromide were mixed and reacted at a temperature of 78°C for 5h. After the reaction was completed, the mixture was allowed to stand and the organic layer was separated. The organic layer was concentrated under reduced pressure to remove the organic solvent. The concentrated product was then mixed with 100g of a 35% by mass sodium hydroxide aqueous solution and subjected to a hydrolysis reaction at a temperature of 45°C for 2h. After the hydrolysis reaction was completed, the mixture was decompressed and the mixture was stirred for 2 hours. The mixture was concentrated under reduced pressure to remove water, and then 2.5 g of boron trifluoride etherate and 960 g of bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether were added to the concentrated product, stirred and reacted at 55°C for 3 h, and then 400 g of hydroxy silicone oil (viscosity 150CP) was added and stirred and reacted at 55°C for 2 h. After the reaction, 400 g of dichloromethane was added to the reaction solution for extraction, and the organic layer was concentrated under reduced pressure to remove the organic solvent and unreacted bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether, and the concentrate was washed with water to obtain modified hydroxy silicone oil; 2) 45 g of modified hydroxy silicone oil, 4.0 g of coconut oil, 3.2 g of argan oil, 4.5 g of TEA dodecylbenzenesulfonate and 50 g of water were mixed and stirred at 50° C. for 2.5 h to obtain the mixed conditioner.

[0026] Comparative Example 1 This comparative example provides a method for preparing a mixed conditioning agent, comprising the following steps: 40 g of hydroxy silicone oil (viscosity 150 CP), 3 g of coconut oil, 3 g of argan oil, 4 g of TEA dodecylbenzenesulfonate and 50 g of water were mixed and stirred at 50° C. for 2.5 hours to obtain the mixed conditioner.

[0027] Comparative Example 2 This comparative example provides a method for preparing a mixed conditioning agent, which differs from Example 1 in that in step 1): 2 g of boron trifluoride etherate, 35 g of sodium hydroxide, 957 g of bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether and 400 g of hydroxy silicone oil (viscosity 150CP) are mixed and stirred for reaction at 55°C for 2 h. After the reaction is completed, 400 g of dichloromethane is added to the reaction solution for extraction, the organic layer is concentrated under reduced pressure to remove the organic solvent and unreacted bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether, and the concentrate is washed with water to obtain modified hydroxy silicone oil.

[0028] Comparative Example 3 This comparative example provides a method for preparing a mixed conditioner, which differs from Example 1 in that in step 1): 125 g of sodium 2-hydroxyethyl sulfonate, 2 g of boron trifluoride etherate, 35 g of sodium hydroxide and 957 g of bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether were stirred and reacted at 55°C for 2 h, and then 400 g of hydroxy silicone oil (viscosity 150CP) was added and the reaction was continued at 55°C with stirring for 2 h. After the reaction, 400 g of dichloromethane was added to the reaction solution for extraction, and the organic layer was concentrated under reduced pressure to remove the organic solvent and unreacted bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether, and the concentrate was washed with water to obtain modified hydroxy silicone oil.

[0029] Test Example 1 The mixed conditioners prepared in the above examples and comparative examples were placed at constant temperatures of 25° C. and 45° C. for 3 months, and were observed after 3 months to see whether they were stratified or turbid. The test results are shown in Table 1.

[0030]

[0031] Test Example 2 The mixed conditioner obtained in the above embodiment was subjected to sensory evaluation test, and the test method was as follows: the test sample was human hair, and the evaluators were selected from people aged 20-30 years old, a total of 50 people, and scored according to the following evaluation indicators: smoothness after shampooing, softness after shampooing, easy combing of wet hair (no knots), easy combing of dry hair (no knots), glossiness after shampooing. Scoring criteria: the total score is 10 points, 1 point is the worst, 10 points are the best, and the higher the score, the better the effect. Finally, the average score is taken. The test results are shown in Table 2.

[0032]

[0033] Obviously, for ordinary technicians in the field, other modifications can be made based on the above embodiments, and the obvious modifications brought about by these modifications are still within the protection scope of the present invention.

Claims

1. A method for preparing a mixed conditioner, characterized in that: The steps include: Mixing modified silicone oil, coconut oil, argan oil, emulsifier and water, stirring to obtain the mixed conditioner; The modified silicone oil is a modified hydroxy silicone oil. The preparation method of the modified hydroxy silicone oil comprises the following steps: mixing propenyl-1,3-sultone, a first organic solvent, water, sodium hypochlorite, a first catalyst and a quaternary ammonium salt and reacting them, standing and stratifying after the reaction, separating an organic layer, concentrating the organic layer under reduced pressure, and then mixing the concentrated product with an alkaline aqueous solution and performing a hydrolysis reaction, and concentrating under reduced pressure after the hydrolysis reaction is completed, and then adding a second catalyst and bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether to the concentrated product to stir the reaction, and then adding hydroxy silicone oil to continue stirring the reaction, and after the reaction is completed, adding a second organic solvent to the reaction solution for extraction, concentrating the organic layer under reduced pressure, and washing the concentrate to obtain the modified hydroxy silicone oil; The first catalyst is selected from cupric chloride; The quaternary ammonium salt is selected from tetrabutylammonium bromide; The second catalyst is boron trifluoride etherate.

2. The preparation method according to claim 1, characterized in that: The mass ratio of the propenyl-1,3-sultone, the first organic solvent, water, sodium hypochlorite, the first catalyst and the quaternary ammonium salt is (120-125): (150-200): (150-200): (110-130): (2-4): (0.2-0.8); When allyl-1,3-sultone, the first organic solvent, water, sodium hypochlorite, the first catalyst and the quaternary ammonium salt are mixed and reacted, the reaction temperature is 75-80° C. and the reaction time is 2-8 hours.

3. The preparation method according to claim 1, characterized in that: The first organic solvent is selected from one of dichloroethane, carbon tetrachloride and toluene.

4. The preparation method according to claim 1, characterized in that: The alkaline aqueous solution is selected from a sodium hydroxide aqueous solution and a potassium hydroxide aqueous solution, and the mass concentration of the alkaline aqueous solution is 30-40%; The mass ratio of the propenyl-1,3-sultone to the alkaline aqueous solution is 1:(0.8-1.2).

5. The preparation method according to claim 1, characterized in that: The molar ratio of the propenyl-1,3-sultone to bis[2-[2-(2-chloroethoxy)ethoxy]ethyl]ether is 1:(3-3.2); The added mass of the second catalyst is 1.5-3% of propenyl-1,3-sultone; The added mass of the hydroxy silicone oil is 3-5 times that of propenyl-1,3-sultone.

6. The preparation method according to claim 1, characterized in that: In the preparation method of the modified hydroxy silicone oil, the stirring reaction temperature is 50-60° C., the stirring reaction time is 1-4 hours, and the continued stirring reaction temperature is 50-60° C., and the continued stirring reaction time is 1-4 hours.

7. The preparation method according to claim 1, characterized in that: The hydrolysis reaction temperature is 40-50°C, and the hydrolysis reaction time is 1-3h; The second organic solvent is selected from dichloromethane, and the washing step is performed with water.

8. The preparation method according to claim 1, characterized in that: Mix silicone oil, coconut oil, argan oil, emulsifier and water, stirring at a temperature of 45-55°C for 2-5 hours.

9. The preparation method according to claim 1, characterized in that: The mass ratio of the silicone oil, coconut oil, argan oil, emulsifier and water is (35-45): (1-5): (1-5): (1-9): (40-60); The emulsifier is selected from TEA dodecylbenzenesulfonate.

10. A mixed conditioning agent comprising silicone oil and vegetable oil, characterized in that: The mixed conditioner is prepared by the preparation method according to any one of claims 1 to 9.

Citation Information

Patent Citations

  • Washing agent composition for colored hairs and preparation method for washing agent composition

    CN102772336A

  • Pet fur conditioning oil capable of inhibiting bacteria and repelling mosquitoes and preparation method thereof

    CN112716836A

  • Preparation method and application of high-humidity-heat-resistant self-extinction waterborne polyurethane

    CN116589653A

  • Efficient repairing conditioner based on silicone oil mixture and preparation method of efficient repairing conditioner

    CN117598931A

  • Active composition for reducing dandruff

    CN117982351A