Preparation method of high-concentration formaldehyde
By using exhaust gas instead of steam in silver catalytic oxidation method, a methanol-air-exhaust gas ternary mixture is formed for oxidation reaction, the problems of low concentration and high wastewater in the existing formaldehyde production are solved, and the preparation and environmental protection of high concentrations of formaldehyde are achieved benefit.
Patent Information
- Application Number
- CN202411148029.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-11-22
AI Technical Summary
In the existing formaldehyde production process, the output concentration is low and accompanied by a large amount of wastewater, which leads to economic and environmental protection problems and has a high investment cost.
Based on the silver catalytic oxidation method, by replacing the by-product exhaust gas with steam, a methanol-air-exhaust gas ternary mixture is formed for oxidation reaction, which increases the formaldehyde concentration and is treated through the absorption tower to obtain high concentration of formaldehyde and reduces exhaust emissions.
The preparation of high concentration of formaldehyde has been achieved, the exhaust gas treatment volume and wastewater generation have been reduced, the production cost has been reduced, the green chemical policy requirements have been met, and the product quality and safety have been improved.
Smart Images

Figure SMS_2 
Figure SMS_4
Abstract
Description
Technical Field
[0001] The invention relates to a method for preparing formaldehyde, in particular to a method for preparing high-concentration formaldehyde, which uses by-product tail gas to replace steam and has low cost, less by-product tail gas, less tail gas emission and simple operation, and belongs to the technical field of fine chemical industry. Background Art
[0002] Formaldehyde is a popular chemical product with a wide range of uses, simple production process and sufficient supply of raw materials. Formaldehyde is used in synthetic resins, surfactants, plastics, rubber, leather, papermaking, dyes, pharmaceuticals, pesticides, photographic films, explosives, building materials, as well as in disinfection, fumigation and preservation processes. Formaldehyde is the backbone of the methanol downstream product tree, with an annual global output of about 25 million tons, and about 30% of methanol is used to produce formaldehyde.
[0003] Formaldehyde is mainly synthesized through methanol oxidation. According to different production processes, methanol-air oxidation is divided into silver-catalyzed oxidation and iron-molybdenum-catalyzed oxidation. The main difference is the metering ratio of methanol to air and the catalyst used. In terms of investment cost, the investment in iron-molybdenum-catalyzed oxidation process for production equipment with the same production capacity is 3 to 4 times that of silver-catalyzed oxidation process. Therefore, silver-catalyzed oxidation has the advantage of low cost.
[0004] Currently, industrial formaldehyde is generally a low-concentration aqueous solution, which is not convenient for long-distance transportation from an economic point of view, and it is easy to produce a lot of wastewater during use. Therefore, from an economic and environmental perspective, it is of great significance to produce high-concentration and stable formaldehyde. Summary of the invention
[0005] In view of the shortcomings of the prior art, the present invention provides a method for preparing high-concentration formaldehyde. The method is improved on the basis of the currently mature silver-catalyzed oxidation process for preparing formaldehyde, and utilizes by-product tail gas instead of steam to produce formaldehyde, thereby increasing the concentration of the obtained formaldehyde and reducing the emission of tail gas, and has better prospects for industrial application.
[0006] The specific technical solutions of the present invention are as follows: A method for preparing high-concentration formaldehyde, the method comprising the following steps: (1) The methanol evaporator is heated, and then methanol, air and water vapor are introduced into the evaporator respectively to form a methanol-air-water vapor ternary mixed gas; (2) passing the above ternary mixed gas into an oxidizer for oxidation reaction to generate formaldehyde; (3) The formaldehyde and tail gas mixture obtained after the reaction is absorbed in an absorption tower to obtain high-concentration formaldehyde. A portion of the remaining tail gas is recycled to step (1) to completely replace water vapor to form a methanol-air-tail gas ternary mixture, and the remaining tail gas is incinerated.
[0007] At the beginning of the process, when no tail gas is generated, the present invention first prepares a methanol-air-water vapor ternary mixed gas according to a conventional process for reaction to obtain formaldehyde, and the concentration of this part of formaldehyde is about 37-45%. When the process stably generates tail gas, the water vapor in step (1) is gradually replaced by the tail gas generated by the process itself. Since the tail gas does not contain water, the concentration of the obtained formaldehyde is greatly improved, so a high-concentration formaldehyde can be obtained. The high-concentration formaldehyde described in the present invention is a high-concentration formaldehyde generated after the tail gas completely replaces the water vapor. The concentration of the high-concentration formaldehyde is greater than or equal to 50wt%. The concentration of the formaldehyde obtained by the process of the present invention is about 53wt%-57wt%, for example, 53%, 54%, 55%, 56%, 57%.
[0008] After the tail gas completely replaces the water vapor, the preparation method of high-concentration formaldehyde comprises the following steps: (S1) heating the methanol evaporator, and then introducing methanol, air and tail gas into the evaporator respectively to form a methanol-air-tail gas ternary mixed gas; (S2) passing the ternary mixed gas into an oxidizer for oxidation reaction to generate formaldehyde; (S3) The formaldehyde and tail gas mixture obtained after the reaction is absorbed by an absorption tower to obtain high-concentration formaldehyde, and a portion of the remaining tail gas is recycled to step (S1), and the rest of the tail gas is incinerated.
[0009] Furthermore, in step (1), when water vapor is introduced, the temperature in the methanol evaporator is 100-110°C. When the tail gas completely replaces the water vapor, the temperature in the methanol evaporator is 115-120°C, for example, 115°C, 116°C, 117°C, 118°C, 119°C, 120°C. When the tail gas replaces the water vapor, the evaporation temperature needs to be increased to obtain a stable ternary mixed gas that meets the requirements, otherwise the composition of the methanol-air-tail gas ternary mixed gas input to the oxidizer is unstable and the methanol content cannot meet the use requirements.
[0010] Furthermore, in step (1), methanol continuously enters the methanol evaporator at a flow rate of 2.9-3.1 t / h. At this flow rate, the production efficiency can be improved, and the obtained ternary mixed gas has a stable composition, and can efficiently obtain high-concentration formaldehyde that meets the requirements.
[0011] Furthermore, in step (1), the molar ratio of air to methanol is 1.7-2.1:1, for example, 1.7:1, 1.8:1, 1.9:1, 2.0:1, 2.1:1, preferably 1.9:1.
[0012] Furthermore, in step (1), the amount of air fed into the methanol evaporator is controlled by a Roots blower, which is provided with a variable frequency adjustment, and the air volume can be adjusted according to the ratio.
[0013] Furthermore, in step (1), methanol is purified by a purifier and filtered by a filter before entering the methanol evaporator. Air is filtered by a filter before entering the methanol evaporator.
[0014] Furthermore, in step (1), the ratio of the mass of water vapor or tail gas to the total mass of air and methanol is 1:2.8-3.5, for example, 1:2.8, 1:2.9, 1:3.0, 1:3.1, 1:3.2, 1:3.3, 1:3.4, 1:3.5.
[0015] Furthermore, in step (2), the temperature in the oxidizer is 590-690°C, for example, 590°C, 600°C, 610°C, 620°C, 630°C, 640°C, 650°C, 660°C, 670°C, 680°C, 690°C.
[0016] Furthermore, in step (2), the pressure in the oxidizer is less than 0.04 MPa, for example, 0.030 MPa, 0.031 MPa, 0.032 MPa, 0.033 MPa, 0.034 MPa, 0.035 MPa, 0.036 MPa, 0.037 MPa, 0.038 MPa, 0.039 MPa, and any range of values therebetween.
[0017] Furthermore, in step (2), a silver catalyst is provided in the oxidizer, and the silver catalyst used in the present invention is the same as the silver catalyst used in the preparation of formaldehyde reported in the prior art, such as an electrolytic silver catalyst. The thickness of the silver layer in the oxidizer is maintained at 1.8-2.2 cm.
[0018] Furthermore, the main reaction and side reaction occurring during the reaction of the raw materials of the present invention are as follows: Main reaction: Side effects: Furthermore, the ternary mixed gas of the present invention undergoes oxidation and dehydrogenation of methanol under the action of a silver catalyst, producing a coexisting gas of formaldehyde and tail gas, and releasing a large amount of reaction heat. The main components of the tail gas are nitrogen and hydrogen.
[0019] Furthermore, the process of absorbing the mixture of formaldehyde and tail gas can adopt the method disclosed in the prior art, for example, the mixture of formaldehyde and tail gas is absorbed by 1# absorption tower and 2# absorption tower to obtain high-concentration formaldehyde. The function of 1# absorption tower is to absorb high-concentration formaldehyde, and the 1# absorption tower is filled with low-concentration formaldehyde in 2# absorption tower. The function of 2# absorption tower is to control the formaldehyde content of tail gas, and the 2# absorption tower is filled with soft water pumped from the soft water storage tank. The mixture of formaldehyde and tail gas is introduced from the bottom of the absorption tower, and low-concentration formaldehyde or soft water is sprayed from top to bottom in the absorption tower to absorb formaldehyde. The large amount of heat carried by the mixture of formaldehyde and tail gas is heat exchanged by soft water, and low-pressure steam is produced as a by-product. A part of the tail gas remaining after absorption in the absorption tower is recycled to step (1) to completely replace water vapor, and the remaining tail gas is all transported to the incinerator for incineration treatment. The heat generated by incineration is heat exchanged with soft water, and ≥0.8MPa steam is produced as a by-product.
[0020] Furthermore, the present invention is an improvement on the existing process of preparing formaldehyde by silver-catalyzed oxidation, and the technical solutions or process parameters not described in detail are selected according to the prior art.
[0021] The beneficial effects of the present invention are as follows: 1. The present invention uses tail gas to completely replace water vapor to form a new ternary mixed gas of methanol-air-tail gas for reaction, thereby reducing the amount of steam used and the amount of tail gas treated.
[0022] 2. The present invention has low pollution, energy conservation and environmental protection, reduces energy consumption by more than 20%, reduces production costs, reduces process safety hazards, and has a high product yield and high formaldehyde concentration, reduces wastewater by more than 30%, and meets the national green chemical policy requirements.
[0023] 3. The formaldehyde solution obtained by the present invention has a high formaldehyde content and a colorless and transparent appearance. It can replace low-concentration formaldehyde to reduce the amount of wastewater generated, and can replace part of paraformaldehyde to reduce production costs.
[0024] 4. The present invention adopts a silver-catalyzed oxidation process with relatively small investment and more mature technology to prepare formaldehyde, with a formaldehyde content of 55±2%, high concentration, less time consumption, high degree of automation, simple operation, and good product quality, which meets the requirements of clean and green production. DETAILED DESCRIPTION
[0025] The following is a description of exemplary embodiments of the present invention, including various details of the embodiments of the present invention to aid understanding, which should be considered as merely exemplary. Therefore, it should be appreciated by those of ordinary skill in the art that various changes and modifications may be made to the embodiments described herein without departing from the scope and spirit of the present invention. Likewise, for clarity and simplicity, descriptions of well-known functions, operations, and structures are omitted in the following description.
[0026] Unless otherwise defined, the technical and scientific terms in this specification have the same meaning as those commonly understood by those skilled in the art. Although similar or identical methods and materials as those described herein may be used in experiments or practical applications, the present invention still describes the materials and methods below. In the event of a conflict, the present specification, including definitions, shall prevail.
[0027] In the following examples, the methanol and silver catalyst used are commercially available products.
[0028] In the following examples, methanol consumption refers to the consumption of methanol corresponding to the production of one ton of 100% formaldehyde content.
[0029] Example 1 A method for preparing high-concentration formaldehyde, the steps are as follows: 1. The raw methanol is pumped from the methanol storage tank to the methanol purifier and filtered by the methanol filter, and then enters the methanol evaporator at a flow rate of 3t / h.
[0030] 2. While feeding methanol, air and water vapor are simultaneously fed into the methanol evaporator to form a ternary mixed gas. The molar ratio of air to methanol is controlled to be 1.9:1, and the air is filtered through an air filter and sent to the bottom of the methanol evaporator by a Roots blower. The mass ratio of water vapor to the total amount of methanol and air is controlled to be 1:3, and the water vapor (0.5MPa) is sent to the bottom of the methanol evaporator by a steam distributor after passing through a steam filter. The temperature inside the methanol evaporator is 105°C.
[0031] 3. The ternary mixed gas enters the flame arrester from the top of the methanol evaporator and enters the oxidizer through the pipeline for oxidation reaction. The temperature of the oxidizer is controlled at 650°C and the pressure is 0.035MPa. The silver layer in the oxidizer is maintained at 2cm for oxidation reaction.
[0032] 4. The formaldehyde and tail gas mixture flowing out of the oxidizer first passes through the 1# absorption tower to absorb high-concentration formaldehyde, and then passes through the 2# absorption tower to control the formaldehyde content of the tail gas. The formaldehyde content in the tail gas of the 2# absorption tower is controlled between 0.02% and 0.05% by controlling the amount of soft water used, and the absorbed formaldehyde concentration is 45wt%.
[0033] 5. A portion of the tail gas generated after formaldehyde absorption is transported to the bottom of the methanol evaporator to replace water vapor to form a ternary mixed gas. The temperature in the methanol evaporator is adjusted to 117°C.
[0034] 6. The methanol-air-exhaust gas ternary mixture is treated according to the above steps 3 and 4. The output formaldehyde concentration is 55.1wt%. It is calculated that the amount of methanol consumed for 1 ton of formaldehyde product (calculated based on 100% formaldehyde content) is 1.189 tons.
[0035] Example 2 A method for preparing high-concentration formaldehyde, the steps are as follows: 1. The raw methanol is pumped from the methanol storage tank to the methanol purifier and filtered by the methanol filter, and then enters the methanol evaporator at a flow rate of 3.1t / h.
[0036] 2. While feeding methanol, air and tail gas are simultaneously fed into the methanol evaporator to form a ternary mixed gas. The molar ratio of air to methanol is controlled to be 1.9:1, and the air is filtered through an air filter and sent to the bottom of the methanol evaporator by a Roots blower. The mass ratio of tail gas to the total amount of air and methanol is controlled to be 1:3, and the tail gas (<0.5MPa) is sent to the bottom of the methanol evaporator by a steam distributor. The temperature in the methanol evaporator is 125°C.
[0037] 3. The ternary mixed gas enters the flame arrester from the top of the methanol evaporator and enters the oxidizer through the pipeline for oxidation reaction. The temperature of the oxidizer is controlled at 660°C and the pressure is 0.035MPa. The silver layer in the oxidizer is maintained at 2cm for oxidation reaction.
[0038] 4. The formaldehyde and tail gas mixture flowing out of the oxidizer first passes through the 1# absorption tower to absorb high-concentration formaldehyde, and then passes through the 2# absorption tower to control the formaldehyde content in the tail gas. The formaldehyde content in the tail gas of the 2# absorption tower is controlled between 0.02% and 0.05% by controlling the amount of soft water used.
[0039] 5. The concentration of the output formaldehyde is 53.9wt%. It is calculated that the amount of methanol consumed for 1 ton of formaldehyde product (calculated based on 100% formaldehyde content) is 1.196 tons.
[0040] Example 3 A method for preparing high-concentration formaldehyde, the steps are as follows: 1. The raw methanol is pumped from the methanol storage tank to the methanol purifier and filtered by the methanol filter, and then enters the methanol evaporator at a flow rate of 2.9t / h.
[0041] 2. While feeding methanol, air and tail gas are simultaneously fed into the methanol evaporator to form a ternary mixed gas. The molar ratio of air to methanol is controlled to be 1.7:1, and the air is filtered through an air filter and sent to the bottom of the methanol evaporator by a Roots blower. The mass ratio of tail gas to the total amount of air and methanol is controlled to be 1:3, and the tail gas (0.5MPa) is sent to the bottom of the methanol evaporator through a steam distributor. The temperature in the methanol evaporator is 115°C.
[0042] 3. The ternary mixed gas enters the flame arrester from the top of the methanol evaporator and enters the oxidizer through the pipeline for oxidation reaction. The temperature of the oxidizer is controlled at 590°C and the pressure is 0.037MPa. The silver layer in the oxidizer is maintained at 1.8cm for oxidation reaction.
[0043] 4. The formaldehyde and tail gas mixture flowing out of the oxidizer first passes through the 1# absorption tower to absorb high-concentration formaldehyde, and then passes through the 2# absorption tower to control the formaldehyde content in the tail gas. The formaldehyde content in the tail gas of the 2# absorption tower is controlled between 0.02% and 0.05% by controlling the amount of soft water used.
[0044] 5. The concentration of the output formaldehyde is 54.1wt%. It is calculated that the amount of methanol consumed by 1 ton of formaldehyde product (calculated based on 100% formaldehyde content) is 1.203 tons.
[0045] Comparative Example 1 Formaldehyde was produced according to the method of Example 2, except that in step 2, the mass ratio of tail gas to the total amount of air and methanol was controlled to be 1:4. The results showed that the oxidizer feed was abnormal because the tail gas dosage was too small, and the feeding was terminated.
[0046] Comparative Example 2 Formaldehyde was produced according to the method of Example 2, except that in step 2, the temperature in the methanol evaporator was 110° C. Finally, the methanol evaporation efficiency in the evaporator was reduced, resulting in a reduction in the feed amount to the oxidizer, causing the liquid methanol content in the evaporator to become higher and higher, making it difficult to achieve a balance between the feed methanol and the evaporated methanol, and the feeding was stopped after the methanol liquid level in the evaporator exceeded the upper limit.
Claims
1. A method for preparing high-concentration formaldehyde, characterized in that The following steps are involved: (1) The methanol evaporator is heated, and then methanol, air and water vapor are introduced into the evaporator respectively to form a methanol-air-water vapor ternary mixed gas; (2) passing the above ternary mixed gas into an oxidizer for oxidation reaction to generate formaldehyde; (3) The formaldehyde and tail gas mixture obtained after the reaction is absorbed in an absorption tower to obtain high-concentration formaldehyde. A portion of the remaining tail gas is recycled to step (1) to completely replace water vapor to form a methanol-air-tail gas ternary mixture, and the remaining tail gas is incinerated.
2. The preparation method according to claim 1, characterized in that: In step (1), when water vapor is introduced, the temperature in the methanol evaporator is 100-110°C. When the tail gas completely replaces the water vapor, the temperature in the methanol evaporator is 115-120°C.
3. The preparation method according to claim 1 or 2, characterized in that: In step (1), methanol continuously enters the methanol evaporator at a flow rate of 2.9-3.1 t / h.
4. The preparation method according to claim 1 or 2, characterized in that: In step (1), the molar ratio of air to methanol is 1.7-2.1:
1.
5. The preparation method according to claim 1 or 2, characterized in that: In step (1), the ratio of the mass of water vapor or tail gas to the total mass of air and methanol is 1:2.8-3.
5.
6. The preparation method according to claim 1, characterized in that: In step (2), the temperature in the oxidizer is 590-690°C.
7. The preparation method according to claim 1 or 6, characterized in that: In step (2), the pressure in the oxidizer is less than 0.04 MPa.
8. The preparation method according to claim 1 or 6, characterized in that: In step (2), a silver catalyst is provided in the oxidizer.
9. The preparation method according to claim 8, characterized in that: In step (2), the thickness of the silver catalyst in the oxidizer is 1.8-2.2 cm.
10. The preparation method according to any one of claims 1 to 9, characterized in that: The concentration of the obtained formaldehyde is 53wt%-57wt%.