Combustion-supporting method for fractional addition of sintering fuel

By adding fine fuel in batches in the sintering process and using the mixing device to make full contact with the tooth roller, the problem of poor outer wrapping effect under high negative pressure air is solved, and the ignition efficiency and fuel consumption of sintered gas are improved. , significantly improve the quality index of sintered ore.

CN118998770AInactive Publication Date: 2024-11-22扬州欧谱机械制造有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411122641.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-11-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the high negative pressure exhaust sintering process, the secondary added fuel is easily drawn into the flue on the surface of the mixture particles, resulting in a reduced fuel addition effect and it is difficult to achieve the purpose of energy saving and consumption reduction.

Method used

The fine fuel is used to pass through the conveying device to the fuel silo of the sintering machine, and is metered and conveyed to the nine-roller cloth machine through an electronic belt scale and a screw conveyor, and is fully mixed with the ore mixture to be sintered, and is turned multiple times by using the mixing device and the tooth roller. and contact the fuel to wrap the mixture particles, and finally flatten the surface of the material through the pressing device and enter the igniter for sintering.

Benefits of technology

The ignition efficiency of sintered gas is improved, the ignition temperature is reduced, the gas consumption is reduced by more than 20%, and the sintering combustion consumption is reduced by 2 to 3 kg/t, which improves the particle-grade composition and metallurgical performance of sintered ore, and significantly improves the fuel utilization efficiency.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a sintering fuel fractional addition combustion-supporting method which comprises the following steps: in the ferrous metallurgy industry, under the condition that sintered ore, fuel ore and a mixer are uniformly mixed in a sintering process, secondary fuel addition combustion-supporting ore combustion is carried out; comprising the following process steps that S1, fineness fuel is conveyed to a fuel bin of a sintering machine head through a conveying device to serve as secondary adding sintering fuel till the fuel bin is full; a fuel adding combustion-supporting technology is adopted, fine-particle fuel is distributed on the surface layer of a sintering machine, the combustion activity of a surface-layer mixture is improved, the sintering gas ignition efficiency is greatly improved, the ignition temperature can be reduced by 100 DEG C or above, the ignition quality can be met, the gas consumption can be averagely reduced by 20% or above, and the effect is remarkable. The surface layer combustion heat of the sintered ore is enhanced, the surface layer quality of the sintered ore is improved, the quality indexes such as the size fraction composition, the drum strength and the metallurgical performance of the sintered ore are improved, and the sintering burnup is reduced by 2 kg / t. And meanwhile, the sintering return mine rate is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of combustion support, and in particular to a method for adding sintering fuel in batches to support combustion. Background Art

[0002] The traditional fuel addition technology is the sintering fuel addition technology, which is to mix a part of the fuel with the sintering mixed ore, return ore, and flux according to a ratio, and add the other part of the fuel after the sintering mixture is mixed once. The purpose is to wrap this part of the fuel on the surface of the mixture particles, keep the fuel with a larger active reaction surface, increase its combustion rate, optimize the reaction atmosphere, and achieve the purpose of sintering energy saving and reducing fuel consumption by optimizing the addition ratio.

[0003] However, with the development of sintering technology, high-vacuum exhaust sintering technology is widely used. The secondary added fuel wrapped on the surface of the mixture particles will be sucked into the flue by the high-vacuum exhaust, which will reduce the sintering effect of the secondary addition of fuel. Summary of the invention

[0004] The purpose of the present invention is to solve the above-mentioned problems of the background technology and to provide a method for adding sintering fuel in batches to assist combustion.

[0005] The purpose of the present invention can be achieved through the following technical solutions:

[0006] A method for adding sintering fuel in batches to support combustion, comprising the following process steps:

[0007] S1, fine fuel is delivered to the fuel bunker at the head of the sintering machine through the conveying device as secondary sintering fuel until the fuel bunker is filled;

[0008] S2. The secondary fuel stored in the fuel bin is then measured and transported to the sintered ore layer under the nine-roller distributor by an electronic belt scale and a screw conveyor, and is fully mixed with the ore mixture to be sintered. The amount of the secondary fuel added is 1-2‰ of the total mass of the sintered ore mixture per ton. The secondary fuel is distributed horizontally along the trolley at the material surface below the nine-roller distributor;

[0009] S3. The surface of the primary mixture is turned over several times by the mixing device of the newly equipped sintering machine, and the secondary sintering fuel is added at the same time. The secondary sintering fuel is fully contacted with the surface of the primary mixture by the toothed roller until the particles of the surface mixture are wrapped with the fuel to obtain the secondary mixture. Finally, the material surface is flattened by the pressing device, and the secondary mixture with a flat surface enters the igniter for ignition and sintering.

[0010] As a further solution of the present invention: in step S3, the amount of the secondary sintering fuel added is calculated as 2 kg per ton of sintered ore.

[0011] As a further solution of the present invention: the sintering fuel is selected from environmentally friendly recycled coke powder or anthracite.

[0012] As a further solution of the present invention: the particle size of the sintering fuel is 0 to 3 mm.

[0013] As a further solution of the present invention: the surface thickness of the mixture accounts for 6-8% of the total thickness of the mixture.

[0014] As a further solution of the present invention: the ore mixture to be sintered is a mixture of sintered mixed ore, return ore and flux according to a proportion.

[0015] The beneficial effects of the present invention are as follows: the fuel addition combustion-supporting technology utilizes fine-grained fuel to spread on the surface of the sintering machine to enhance the combustion activity of the surface mixture, greatly improving the ignition efficiency of the sintering gas, and can reduce the ignition temperature by more than 100°C to meet the ignition quality. The gas consumption can be reduced by more than 20% on average, with significant results.

[0016] The combustion heat of the surface layer of sintered ore is enhanced, the quality of the surface layer of sintered ore is improved, the quality indicators such as the particle size composition, drum strength, and metallurgical properties of the sintered ore are improved, the sintering fuel consumption is reduced by 2 to 3 kg / t, and the sintering return ore is reduced by 50%. DETAILED DESCRIPTION

[0017] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0018] A method for adding sintering fuel in batches to assist combustion, in the ferrous metallurgical industry, the sintering process is to mix the sintered ore, the fuel ore and the mixer, and then add the secondary fuel to assist combustion ore, including the following process steps:

[0019] S1, fine fuel is delivered to the fuel bunker at the head of the sintering machine through the conveying device as secondary sintering fuel until the fuel bunker is filled;

[0020] S2. The secondary added fuel stored in the fuel bin is then transported to the surface of the sintered ore under the nine-roller distributor by an electronic belt scale and a screw conveyor, and is fully mixed with the mixture of the ore to be sintered. The amount of the secondary added sintering fuel is about 1-2‰ of the total mass of the mixture of the ore to be sintered per ton. The secondary fuel is arranged on the surface material layer of the sintered ore under the nine-roller distributor, and is distributed horizontally along the trolley at the material surface;

[0021] S3. The surface of the primary mixture is turned over several times by the mixing device of the newly configured sintering machine, and the secondary sintering fuel is added at the same time. The secondary sintering fuel is fully contacted with the surface of the primary mixture by the toothed roller until the particles of the surface mixture are wrapped with the fuel to obtain the secondary mixture. Finally, the material surface is flattened by the pressing device, and the secondary mixture with a flat surface enters the igniter for ignition and sintering.

[0022] In step S3, the amount of secondary sintering fuel added is calculated as 2 kg per ton of sintered ore.

[0023] The sintering fuel is selected from coke powder or anthracite. The coke is the material with a size of ≤3 after crushing and screening, and the anthracite is the fuel dust removal ash. Both are environmentally friendly and can be reused to save energy and reduce consumption.

[0024] The particle size of the sintering fuel of the environmentally friendly collection is 0 to 3 mm.

[0025] The surface thickness of the mixture accounts for 6 to 8% of the total thickness of the mixture.

[0026] The ore mixture to be sintered is prepared by mixing sintered mixed ore, return ore and flux in a certain proportion.

[0027] In another embodiment, a method for adding sintering fuel in batches to support combustion includes the following process steps:

[0028] S1. Use a small amount of fine fuel through a pneumatic conveyor to the fuel bunker at the head of the sintering machine as secondary sintering fuel until the fuel bunker is filled;

[0029] S2. The secondary added fuel stored in the fuel bin is then measured and transported to the surface of the sintered ore below the nine-roller distributor by an electronic belt scale and a screw conveyor, and is fully mixed with the mixture of the ore to be sintered. The amount of the secondary added sintering fuel is 1-2‰ of the total mass of the mixture of the ore to be sintered per ton. The obtained primary mixture is distributed laterally along the trolley at the material surface after being distributed by the nine-roller distributor;

[0030] S3. The surface of the primary mixture is turned over several times by the mixing device of the newly added sintering machine, and the secondary sintering fuel is added at the same time (the addition amount is calculated based on 2 kg per ton of sintered ore). The secondary sintering fuel is fully contacted with the surface of the primary mixture by the toothed roller until the particles of the surface mixture are wrapped with the fuel to obtain the secondary mixture. Finally, the material surface is flattened by the pressing device, and the secondary mixture with a flat surface enters the igniter for ignition and sintering.

[0031] The sintering fuel is selected from environmentally friendly recycled coke powder or anthracite with a particle size of ≤3mm;

[0032] The ore mixture to be sintered is a mixture of sintered mixed ore, return ore and flux in a reasonable ratio (the ratio varies with the different ore grades, but the fuel ratio is about 1-2‰).

[0033] The surface thickness of the mixture accounts for 6-8% of the total thickness of the mixture.

[0034] In another embodiment, a method for adding sintering fuel in batches to support combustion includes the following process steps:

[0035] S1. Use a small amount of fine fuel through a pneumatic conveyor to the fuel bunker at the head of the sintering machine as a one-time addition of sintering fuel until the fuel bunker is filled;

[0036] S2, the primary added fuel stored in the fuel bin is then measured and transported to the surface of the sintered ore below the nine-roller distributor by an electronic belt scale and a screw conveyor, and is fully mixed with the mixture of the ore to be sintered. The amount of the secondary added sintering fuel is 1-2‰ of the total mass of the mixture of the ore to be sintered per ton, and the secondary added sintering fuel screw conveyor is horizontally distributed along the trolley on the surface of the sintered ore under the nine-roller distributor;

[0037] S3. The surface of the primary mixture is turned over several times by the mixing device of the newly equipped sintering machine, and the secondary sintering fuel is added at the same time (the addition amount is calculated based on 2 kg per ton of sintered ore). The secondary sintering fuel is fully contacted with the surface of the primary mixture by the toothed roller until the particles of the surface mixture are wrapped with the fuel to obtain the secondary mixture. Finally, the material surface is flattened by the pressing device, and the secondary mixture with a flat surface enters the igniter for ignition and sintering.

[0038] Wherein, the sintering fuel is selected from coke powder or anthracite with a particle size of 3 mm;

[0039] The ore mixture to be sintered is a mixture of sintered mixed ore, return ore and flux in a reasonable ratio (the ratio varies with the different ore grades, but the fuel ratio is about 1-2‰).

[0040] The surface thickness of the mixture accounts for 6-8% of the total thickness of the mixture.

[0041] In another embodiment, a method for adding sintering fuel in batches to support combustion includes the following process steps:

[0042] S1. Use a small amount of fine fuel through a pneumatic conveyor to the fuel bunker at the head of the sintering machine as secondary sintering fuel until the fuel bunker is filled;

[0043] S2, the primary added fuel stored in the fuel bin is then measured and transported to the sintered ore layer below the nine-roller distributor by an electronic belt scale and a screw conveyor, and is fully mixed with the ore mixture to be sintered. The amount of the secondary added sintering fuel is 1-2‰ of the total mass of the ore mixture to be sintered per ton, and is distributed horizontally along the trolley via a screw conveyor;

[0044] S3. The surface of the primary mixture is turned over several times by the mixing device of the sintering machine, and the secondary sintering fuel is added at the same time (the addition amount is calculated based on 2 kg per ton of sintered ore). The secondary sintering fuel is fully contacted with the surface of the primary mixture by the toothed roller until the particles of the surface mixture are wrapped with the fuel to obtain the secondary mixture. Finally, the material surface is flattened by the pressing device, and the secondary mixture with a flat surface enters the igniter for ignition and sintering.

[0045] Wherein, the sintering fuel is selected from coke powder or anthracite, with a particle size of ≤3mm;

[0046] The ore mixture to be sintered is a mixture of sintered mixed ore, return ore and flux in a reasonable ratio (the ratio varies with the different ore grades, but the fuel ratio is about 1-2‰).

[0047] The surface thickness of the mixture accounts for 6-8% of the total thickness of the mixture.

[0048] Fuel addition and combustion-supporting technology is a new type of sintering fuel addition technology. It uses a small part of environmentally friendly blanking to be pneumatically conveyed to the fuel bin at the head of the sintering machine, and then conveyed to the material surface after the nine-roller mixed material is distributed horizontally along the trolley through the electronic belt scale and the mixed material surface is turned over by the mixer, and the fuel and the surface mixed material are fully contacted by the toothed roller. The material surface is flattened by the pressing device and enters the igniter for ignition and sintering. Fuel addition and combustion-supporting technology, whose fuel comes from environmentally friendly secondary reuse, is quite energy-saving.

[0049] The fuel addition combustion-supporting technology uses fine-grained fuel to spread on the surface of the sintering machine to improve the combustion activity of the surface mixture, greatly reducing the ignition efficiency of the sintering gas. The ignition temperature can be reduced by more than 100°C to meet the ignition quality. The gas consumption can be reduced by more than 20% on average, with significant results.

[0050] The combustion heat of the surface layer of sintered ore is enhanced, the surface quality of sintered ore is improved, the quality indicators such as the particle size composition, drum strength, and metallurgical properties of sintered ore are improved, and the sintering fuel consumption is reduced by 2 to 3 kg / t.

[0051] Improve the utilization efficiency of sintering fine-grain fuel (dust removal can be done by the fuel system, or coking coal can be used to screen out fine materials ≤3mm) to give full play to the fuel combustion efficiency.

[0052] The 400㎡ sintering process saves 12,000 tons of fuel annually, which can create an annual benefit of more than 15 million yuan. It also reduces gas consumption, which can create an annual benefit of 3 million yuan, and can create an annual benefit of 18 million yuan.

[0053] The environmental protection benefits are significant, emissions are reduced at the source, and pollutant emissions are reduced.

[0054] The above is a detailed description of an embodiment of the present invention, but the content is only a preferred embodiment of the present invention and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made according to the scope of application of the present invention should still fall within the scope of the claims of the present invention.

Claims

1. A method for adding sintering fuel in batches to support combustion, characterized in that: The process steps include: S1, fine fuel is delivered to the fuel bunker at the head of the sintering machine through the conveying device as secondary sintering fuel until the fuel bunker is filled; S2. The secondary added fuel stored in the fuel bin is then transported to the surface of the sintered ore under the nine-roller distributor by an electronic belt scale and a screw conveyor, and is fully mixed with the mixture of the ore to be sintered. The amount of the secondary added sintering fuel is about 1-2‰ of the total mass of the mixture of the ore to be sintered per ton. The secondary fuel is arranged on the surface material layer of the sintered ore under the nine-roller distributor, and is distributed horizontally along the trolley at the material surface; S3. The surface of the primary mixture is turned over several times by the mixing device of the newly configured sintering machine, and the secondary sintering fuel is added at the same time. The secondary sintering fuel is fully contacted with the surface of the primary mixture by the toothed roller until the particles of the surface mixture are wrapped with the fuel to obtain the secondary mixture. Finally, the material surface is flattened by the pressing device, and the secondary mixture with a flat surface enters the igniter for ignition and sintering.

2. A method for adding sintering fuel in batches to support combustion according to claim 1, characterized in that: In step S3, the amount of secondary sintering fuel added is calculated as 2 kg per ton of sintered ore.

3. A method for adding sintering fuel in batches to support combustion according to claim 1, characterized in that: The sintering fuel is selected from coke powder or anthracite. The coke is the material with a size of ≤3 after crushing and screening, and the anthracite is the fuel dust removal ash. Both are environmentally friendly and can be reused to save energy and reduce consumption.

4. A method for adding combustion-supporting sintering fuel in batches according to claim 3, characterized in that: The particle size of the sintering fuel of the environmentally friendly collection is 0 to 3 mm.

5. A method for adding sintering fuel in batches to support combustion according to claim 1, characterized in that: The surface thickness of the mixture accounts for 6 to 8% of the total thickness of the mixture.

6. A method for adding sintering fuel in batches to support combustion according to claim 1, characterized in that: The ore mixture to be sintered is prepared by mixing sintered mixed ore, return ore and flux in a certain proportion.