Shale effective porosity determination method considering lamellar fracture and matrix pore and application

Through the effective porosity measurement of helium and mathematical model fitting, the problem of inability to distinguish between the porosity of the shale in shale porosity measurement is solved, and the accurate determination of shale porosity and storage space evaluation is achieved, which reduces the Experimental cost.

CN119000458AActive Publication Date: 2024-11-22PETROCHINA CO LTD

Patent Information

Application Number
CN202310563795.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-18
Publication Date
2024-11-22
Estimated Expiration
2043-05-18

AI Technical Summary

Technical Problem

The prior art is difficult to accurately determine the porosity of shale, especially the inability to distinguish between the porosity of the shale and the matrix, resulting in poor accuracy of shale storage space evaluation.

Method used

Through the helium effective porosity determination method, combined with mathematical model fitting experimental data, the effective porosity, matrix porosity and sewing porosity of shale rock samples were determined, and their respective quantification was achieved.

Benefits of technology

It improves the accuracy of shale porosity measurement, saves experimental costs, time and labor costs, and provides more accurate storage space evaluation and dessert prediction basis.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119000458A_ABST
    Figure CN119000458A_ABST
Patent Text Reader

Abstract

The invention discloses a shale effective porosity determination method giving consideration to lamellar fractures and matrix pores and application. The method comprises the following steps: carrying out a helium porosity determination experiment on a shale sample until a first set time is reached, obtaining a plurality of experimental data containing data pairs of experimental time and porosity, and obtaining a shale porosity determination result by fitting the experimental data on the basis of a mathematical model of shale effective porosity and experimental time. And obtaining a fitting relationship between the effective porosity of the rock sample and the experiment time, and respectively determining the effective porosity, the matrix porosity and the lamellar fracture porosity of the rock sample according to the selection direction of the rock sample and the fitting relationship. According to the method, the shale sample matrix porosity and the lamellar fracture porosity can be quantified respectively, and key parameters are provided for pure shale oil resource evaluation, sweet spot prediction and reserve submission.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of petroleum exploration, and in particular to a method for determining effective porosity of shale taking both lamellae fractures and matrix pores into consideration and its application. Background Art

[0002] The world is rich in shale oil and gas resources. With the advancement and widespread application of technologies such as horizontal drilling and volume fracturing, vigorously exploring and developing unconventional oil and gas resources has become one of the trends in the development of world energy. Porosity is one of the key parameters for oil and gas resource evaluation, and is of great significance for determining the reservoir space, fluid saturation and geological reserves of rocks. Affected by the extremely low permeability and complex mineral components of shale, especially the characteristics of micro-nano pores and lamellae, coupled with different understandings of the test methods in different laboratories, the test results between different laboratories are poorly reproducible, making it difficult to accurately characterize the porosity of shale.

[0003] Pure shales formed by sedimentation in continental lake basin environments, represented by Gulong Shale in China, are characterized by high clay content, extremely developed laminae and lamellae, diverse reservoir space, and the development of special matrix pore-lamellae composite reservoir space, accounting for 70% of the total reservoir space. The pore types of Gulong Shale are mainly intercrystalline pores of clay minerals, intergranular dissolution pores of clastic minerals, and organic pores. The pore development is small in scale, poor in connectivity, and strong in heterogeneity; the development of millimeter-level laminar structure lays the foundation for the extremely developed lamellae. The width of lamellae can reach up to millimeter level, with an effective porosity of 1.18%, and the contribution rate to the reservoir space is up to 14%. The high porosity area is connected to the fracture vertically up to 250μm, connecting the upper and lower fractures. The large number of developed lamellae not only increases the seepage channels of shale, but also is an effective reservoir space, which is of great significance. However, the evaluation of the dual reservoir space of lamellae and pore-fracture composite is difficult to carry out due to the limitations of testing methods and complex structures.

[0004] At present, there are many methods for measuring shale porosity, mainly including qualitative and quantitative aspects. The qualitative evaluation method of reservoir space is represented by optical microscopy and scanning electron microscopy, which is limited to distinguishing pore types and pore-fracture combinations in a two-dimensional plane. Quantitative volume evaluation technologies represented by saturated liquid method, gas expansion method (GIP, Gas Injection Porosimetry), gas adsorption method, high-pressure mercury injection, nuclear magnetic resonance and image analysis have realized the quantitative evaluation of pore structure and reservoir space and obtained pore throat system data information. The saturated liquid method is divided into WIP (Water Immersion Porosimetry) method and DLP (Dual Liquid Porosimetry) method. Shale mineral components and pore wettability are complex and diverse, especially containing a large amount of easily swellable clay minerals. It is difficult to accurately measure shale porosity using the saturated liquid method; and the DLP method in the saturated liquid method requires core slices as the measurement object, which has strong limitations. The commonly used GIP method is based on Boyle's law. Helium is now used as a carrier. The pressure change is measured by filling the sample pores with a known pressure, and the effective porosity of the shale plug sample is indirectly measured. Foreign scholars mainly use the GRI (Gas Research Institute) method to measure the total porosity of shale. This method is a special GIP method, which is mainly used for shale gas reservoir evaluation. The measurement object is crushed particles. There is a large error in the measurement of its apparent volume, and the measurement results are greatly affected by the sample pretreatment and experimental parameter settings. The CO2 adsorption method and the N2 adsorption method have advantages in measuring the pore size of shale micropores (<2nm) and mesopores (2~50nm), respectively. Like the liquid measurement method, it is not only controlled by the size relationship between the molecular diameter and the pore diameter, but also the shale pore is difficult to quantify the gas adsorption effect. Mercury injection tests are mostly used to characterize information about macropores (>50nm) in shales: the theoretical lower limit of effective pores reflected by ordinary mercury injection (30MPa) is about 24.5nm, high-pressure mercury injection (413MPa) can reach 1.8nm, and constant-rate mercury injection technology (about 6MPa) can simultaneously reflect pore and throat information. Shale has the characteristics of low porosity and low permeability, and high displacement pressure is required to promote mercury injection into the sample. However, artificial fractures are easily generated in the process, and the overall mercury removal efficiency of shale is low, resulting in destructive experiments, and the test samples cannot be used for other tests. Nuclear magnetic resonance obtains information such as shale porosity, pore size distribution, pore connectivity, and movable fluid without damaging the sample, but the process requires specific parameter evaluation for different reservoirs, and the interpretation uncertainty is large; and it is affected by multiple factors such as the test environment, instrument parameters, micropores of the sample, paramagnetic substances, and fluid types. Image analysis methods are currently used to characterize pore structure and connectivity through micro-nano CT and focused ion beam field emission scanning electron microscopy analysis technology. However, this method is greatly limited by resolution and can only characterize pore throats of 50 nm and above.

[0005] Porosity testing methods all have a lot of limitations, and a single method is difficult to accurately characterize the actual reservoir space of shale. Helium porosity measurement is an effective porosity testing method widely used in domestic laboratories. The important parameters of this method are the quantitative evaluation of the apparent volume and skeleton volume, and are secondly affected by conditions such as temperature, pressure gauge accuracy and stability. Summary of the invention

[0006] The embodiment of the present invention provides a method and application for determining the effective porosity of shale taking into account both lamellae fractures and matrix pores, which can realize the separate quantification of the matrix porosity and lamellae fracture porosity of shale samples, and provide a basis for resource evaluation and sweet spot prediction.

[0007] In a first aspect, an embodiment of the present invention provides a method for determining effective porosity of shale taking into account both lamellae fractures and matrix pores, comprising performing the following steps for at least one shale sample:

[0008] Performing a helium effective porosity measurement experiment on the rock sample until a first set time is reached, and obtaining a plurality of experimental data including data pairs of experimental time and effective porosity;

[0009] Based on the mathematical model system of effective porosity and experimental time, a first fitting relationship between the effective porosity of the rock sample and the experimental time is obtained by fitting the experimental data. According to the rock sample selection direction and the first fitting relationship, the effective porosity, matrix porosity and lamellae porosity of the rock sample are respectively determined.

[0010] In a second aspect, an embodiment of the present invention provides a method for evaluating the reservoir space of a shale reservoir, comprising using the method described above to respectively determine the effective porosity, matrix porosity, and lamellar fracture porosity of a rock sample in a shale reservoir;

[0011] The reservoir space of shale reservoirs is evaluated based on the determined effective porosity, matrix porosity and lamellae porosity.

[0012] The beneficial effects of the above technical solution provided by the embodiment of the present invention include at least:

[0013] (1) Current porosity measurements usually only obtain the value of effective porosity or total porosity, and are unable to quantitatively distinguish the effective porosity contributed by the lamellar fracture reservoir space and the matrix reservoir space. The shale effective porosity measurement method provided in the embodiment of the present invention takes both lamellar fractures and matrix pores into consideration. By using a helium measurement method, a porosity measurement experiment is conducted for a sufficient time, so that helium molecules can fully penetrate into the lamellar fractures and matrix pores of the rock sample, and the obtained effective porosity has a higher accuracy. In addition, the effective porosity, matrix porosity and lamellar fracture porosity of the rock sample are determined according to the rock sample selection direction and the fitting relationship between porosity and time, thereby achieving the quantitative characterization of matrix porosity and lamellar fracture porosity, and providing a basis for shale reservoir resource evaluation and sweet spot prediction.

[0014] (2) There are differences in the reasonable experimental time for helium porosity determination of different types of shales. Reasonable time determines a more accurate porosity value and controls the experimental cost, time and labor cost. The embodiment of the present invention provides a method for determining the effective porosity of shale that takes into account both lamellae fractures and matrix pores, and establishes a model relationship between effective porosity and experimental time; a mathematical model is established to determine the required optimal experimental time, and experimental data is obtained. The mathematical model is used to fit the experimental data to obtain a first fitting relationship between the effective porosity of the rock sample and the experimental time, and the effective porosity, matrix porosity and lamellae fracture porosity of the rock sample are determined based on the first fitting relationship. This not only ensures the accuracy of various effective porosity values, but also saves experimental cost, time and labor cost.

[0015] Other features and advantages of the present invention will be described in the following description, and partly become apparent from the description, or understood by practicing the present invention. The purpose and other advantages of the present invention can be realized and obtained by the structures particularly pointed out in the written description, claims, and drawings.

[0016] The technical solution of the present invention is further described in detail below through the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:

[0018] Figure 1 This is a flow chart of a method for determining effective porosity of shale in Example 1 of the present invention;

[0019] Figure 2 This is a schematic diagram of the structure of the parallel bedding plug sample B25-1 in Example 2 of the present invention;

[0020] Figure 3 This is a schematic diagram of the structure of the vertical bedding plug sample B25-2 in Example 2 of the present invention;

[0021] Figure 4 This is a graph showing the relationship between the helium effective porosity and the measurement time of the B25-1 sample in Example 2 of the present invention;

[0022] Figure 5 This is a graph showing the relationship between the helium effective porosity and the measurement time of the B25-2 sample in Example 2 of the present invention;

[0023] Figure 6 This is a prediction diagram of the helium effective porosity of the B25-1 sample in Example 2 of the present invention;

[0024] Figure 7 This is a distribution diagram of the predicted range of helium effective porosity of the B25-2 sample in Example 2 of the present invention. DETAILED DESCRIPTION

[0025] The exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although the exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art.

[0026] It should be understood that the terms described in the present invention are only for describing special embodiments and are not intended to limit the present invention. In addition, for the numerical range in the present invention, it should be understood that each intermediate value between the upper and lower limits of the scope is also specifically disclosed. Each smaller range between the intermediate value in any stated value or stated range and any other stated value or intermediate value in the described range is also included in the present invention. The upper and lower limits of these smaller ranges can be independently included or excluded in the scope.

[0027] Unless otherwise indicated, all technical and scientific terms used herein have the same meanings as commonly understood by those skilled in the art to which the invention belongs. Although the present invention describes only preferred methods and materials, any methods and materials similar or equivalent to those described herein may also be used in the implementation or testing of the present invention. All documents mentioned in this specification are incorporated by reference to disclose and describe the methods and / or materials related to the documents. In the event of a conflict with any incorporated document, the content of this specification shall prevail.

[0028] In the description of the present invention, it should be noted that the terms "include", "including", "have", "contain" and the like are open terms, meaning including but not limited to.

[0029] Helium effective porosity measurement is an effective porosity test method widely used in domestic laboratories. The inventors found in their work that the accuracy of shale effective porosity determined by the existing technology of helium effective porosity measurement needs to be improved, and the existing technology can only measure the effective porosity of shale, and cannot distinguish between matrix pores and lamellae fracture pores. After further research and development, the inventors made the present invention. The embodiments of the present invention provide a shale effective porosity measurement method and application that takes into account both lamellae fractures and matrix pores, which can achieve the separate quantification of shale rock sample matrix porosity and lamellae fracture porosity.

[0030] Embodiment 1

[0031] Embodiment 1 of the present invention provides a method for measuring the effective porosity of shale taking into account both lamellae fractures and matrix pores.

[0032] The national standard stipulates that the porosity value measured when the helium effective porosity measurement experiment is carried out for 25 minutes shall be used as the effective porosity value of the shale. However, the inventors have found in a large number of experiments that as the experimental time gradually increases, gas molecules are continuously injected into the shale pores, that is, the porosity value measured in the experiment gradually increases with the increase of the experimental time, but the increase in magnitude gradually decreases with the extension of the experimental time. Considering the experimental cost, time and manpower cost, it is impossible to increase the experimental time of each helium porosity measurement experiment to a sufficiently long time in actual work. Therefore, in this embodiment, helium porosity measurement experiments are first carried out on multiple shale samples respectively until the second set time is reached, and a general relationship (mathematical model) between porosity and experimental time is established based on the experimental data. Based on the established mathematical model of porosity and experimental time, in the subsequent helium porosity measurement experiment, the experimental time does not need to reach the second set time. According to empirical statistics, the experimental time reaches the first set time. According to the experimental data combined with the pre-established mathematical model of porosity and experimental time, the first fitting relationship between the porosity of the rock sample and the experimental time is obtained, which can meet the experimental accuracy requirements.

[0033] Specifically, the second set time is usually set to be greater than 50 hours; the first set time is set according to sample differences and is usually set to 15 to 25 hours.

[0034] The above mathematical model is pre-established in the following way:

[0035] A helium effective porosity measurement experiment is performed on multiple shale samples until a second set time is reached, and multiple experimental data including data pairs of experimental time and effective porosity are obtained. The experimental data are fitted to obtain a second fitting relationship between the effective porosity and the experimental time; a mathematical model of the effective porosity and the experimental time is established through the second fitting relationship of each of the multiple shale samples.

[0036] Specifically, the mathematical model of effective porosity and experimental time is:

[0037] Porosity=a×t b +c

[0038] Where Porosity is the effective porosity, t is the experimental time, and a, b, and c are constants to be determined.

[0039] Reference Figure 1 As shown, the method for determining the effective porosity of shale taking into account both lamellae fractures and matrix pores provided in the first embodiment of the present invention comprises performing the following steps respectively for at least one shale rock sample:

[0040] Step S11: performing a helium effective porosity measurement experiment on the rock sample until a first set time is reached, and obtaining a plurality of experimental data including data pairs of experimental time and effective porosity.

[0041] During the helium effective porosity measurement experiment, the effective porosity is determined in real time through the apparent volume of the rock sample and the real-time determined skeleton volume. Therefore, the key to improving the accuracy of effective porosity experimental data is to accurately obtain the apparent volume and skeleton volume.

[0042] In this embodiment, the measurement method is used to determine the apparent volume of the rock sample. The rock sample adopts a plunger sample, that is, the rock sample is cylindrical, and is processed by wire cutting. The apparent volume of the rock sample is measured using an electronic vernier caliper. The outer diameter and length of the rock sample are measured with an electronic vernier caliper, and the calculated volume is used as the apparent volume of the rock sample. The measurement method can avoid the influence of water absorption and expansion of clay minerals during the liquid measurement method and reduce the error in the measurement process. In addition, wire cutting is used in the above-mentioned rock sample cutting process, which can avoid cracks caused by manual processing and ensure the integrity of the rock sample; at the same time, the surface of the rock sample obtained by wire cutting is smoother, which can improve the accuracy of the apparent volume of the rock sample determined by the measurement method.

[0043] The equilibration time, gas injection direction, injection pressure, ambient temperature and pressure gauge sensitivity all affect the accurate acquisition of the skeleton volume.

[0044] In this embodiment, a high-precision pressure sensor is used to measure the pressure; under the conditions of constant ambient temperature and injection pressure, a helium effective porosity measurement experiment is carried out on the rock sample, so that the instrument is kept under constant temperature conditions, which can avoid external interference and thus improve the measurement accuracy.

[0045] Regarding the optimization of the gas injection direction, firstly, the rock samples are cut according to the relationship between shale and lamellae, at least one shale rock sample is a first rock sample with an axial direction parallel to the lamellae direction; or, at least one shale rock sample is a second rock sample with an axial direction perpendicular to the lamellae direction; or, at least one shale rock sample is a first rock sample with an axial direction parallel to the lamellae direction and a second rock sample with an axial direction perpendicular to the lamellae direction, and the first rock sample and the second rock sample are taken from the same depth of the same core (so that the first rock sample and the second rock sample can represent the rock samples at the same position). The rock sample is a plunger sample, and the injection direction is perpendicular to the axial direction of the rock sample, so the injection direction is perpendicular to the lamellae direction of the first rock sample and parallel to the lamellae direction of the second rock sample.

[0046] The axial direction here refers to the direction perpendicular to the cross section of the rock sample.

[0047] Step S12: Based on the mathematical model of shale effective porosity and experimental time, a first fitting relationship between the effective porosity of the rock sample and the experimental time is obtained by fitting the experimental data. The effective porosity, matrix porosity and lamellae porosity of the rock sample are determined according to the rock sample selection direction and the first fitting relationship.

[0048] The rock sample selection direction here refers to the relationship between the axial direction of the rock sample obtained by cutting and the direction of the rock sample lamellae. Taking the first rock sample and the second rock sample as examples, the injection direction is perpendicular to the lamellae direction of the first rock sample and parallel to the lamellae direction of the second rock sample. Therefore, for the first rock sample, the gas molecules are first injected into the matrix pores of the rock sample and then into the lamellae of the rock sample; for the second rock sample, the fluid is first injected into the lamellae of the rock sample and then into the matrix pores of the rock sample.

[0049] Therefore, according to the first fitting relationship, the first porosity when the effective porosity change gradient begins to be less than the first gradient threshold and the second porosity when the porosity change gradient begins to be less than the second gradient threshold can be determined respectively, and the first porosity is used as the effective porosity of the rock sample; if the shale rock sample is the first rock sample, the second porosity is determined as the matrix porosity of the rock sample, and the difference between the effective porosity and the matrix porosity is determined as the lamellar fracture porosity; if the shale rock sample is the second rock sample, the second porosity is determined as the lamellar fracture porosity of the rock sample, and the difference between the effective porosity and the lamellar fracture porosity is determined as the matrix porosity.

[0050] The porosity change gradient here is defined as the ratio of the difference between the porosity at the current moment and the porosity at the moment before the current moment to the difference between the two corresponding moments. The first gradient threshold is less than the second gradient threshold, which can be understood as the first porosity being the porosity when the porosity basically does not change with time; the second porosity is the porosity at the inflection point in the relationship curve corresponding to the second fitting relationship.

[0051] Current porosity measurements usually only obtain the value of effective porosity or total porosity, and are unable to quantitatively distinguish the effective porosity contributed by lamina reservoir space and matrix reservoir space. The first embodiment of the present invention provides a method for determining the effective porosity of shale that takes both lamina and matrix pores into consideration. By using a helium measurement method, an effective porosity measurement experiment is conducted for a sufficient time, so that helium molecules can fully penetrate into the lamina and matrix pores of the rock sample, and the obtained effective porosity has a higher accuracy. In addition, the effective porosity, matrix porosity and lamina porosity of the rock sample are determined according to the rock sample selection direction and the fitting relationship between porosity and time, thereby achieving the quantitative characterization of the matrix porosity and lamina porosity.

[0052] The helium porosity measurement experiment time must be long enough to obtain a more accurate porosity value, so it requires higher experimental cost, time and labor cost. The shale porosity measurement method that takes into account both lamellae fractures and matrix pores provided in Example 1 of the present invention pre-establishes a mathematical model of porosity and experimental time; obtains experimental data using an experimental time much shorter than that required to establish the mathematical model; and according to the mathematical model, the experimental data is fitted using the mathematical model to obtain a first fitting relationship between the porosity of the rock sample and the experimental time; and the effective porosity, matrix porosity and lamellae fracture porosity of the rock sample are determined according to the first fitting relationship. This not only ensures the accuracy of various porosity values, but also saves experimental cost, time and labor cost.

[0053] Embodiment 2

[0054] Embodiment 2 of the present invention provides a specific application embodiment of a shale porosity measurement method that takes both lamellae fractures and matrix pores into consideration.

[0055] In this embodiment, the samples used in the experiment were taken from the shale of the xx section of the xx basin. A total of 2 pure shale plug samples were obtained after wire cutting at the same depth of the same core, namely, parallel bedding plug sample B25-1 and vertical bedding plug sample B25-2. The bedding fracture direction of B25-1 is parallel to the axis of the rock sample, and the bedding fracture direction of B25-2 is perpendicular to the axis of the rock sample. After qualitative observation by thin section and scanning electron microscope, helium effective porosity was measured, and then numerical simulation was used for effective evaluation.

[0056] Through thin section, scanning electron microscope and nano-CT production and observation of the above samples parallel to the cylindrical surface of the plunger, the samples have developed felsic laminae, clay laminae and shell laminae, and the mineral composition is mainly clay minerals, quartz and carbonate minerals. Irregular foliation joints parallel to the bedding can be seen in the CT model. Figure 2 It can be seen that the parallel-bedding plunger sample B25-1 has two relatively straight foliation fractures, which are perpendicular to the cylindrical surface of the plunger; Figure 3 It can be seen that the vertical bedding plug sample B25-2 has two staggered lamellae and other smaller horizontal cracks, all parallel to the cylindrical surface of the plug.

[0057] The effective porosity of B25-1 and B25-2 samples was measured by helium porosity, with the initial injection pressure of 100psi and the test environment (temperature) controlled at 24±1℃. The apparent volume of B25-1 was measured to be 2.506cm in diameter, 1.954cm in length, and 23.44g in mass; the apparent volume of B25-2 was measured to be 2.494cm in diameter, 1.143cm in length, and 13.49g in mass. The results of long-term effective porosity measurements of the samples showed that the effective porosity of the parallel bedding plug sample B25-1 was 5.5% at 25 minutes as specified by the national standard, and 8.64% at 53 hours, and there was no obvious inflection point during the entire POR-T change process, showing a uniform upward trend; the effective porosity of the vertical bedding plug sample B25-2 was 6.68% at 25 minutes as specified by the national standard, and 8.38% at 53 hours, and there was a slow upward trend after an obvious inflection point during the entire POR-T change process.

[0058] By means of numerical experiments, the physical experimental results are fitted to predict the effective porosity value at a later time. The effective porosity, pressure, and temperature variation over time within 66 hours are obtained from the parallel bedding sample B25-1 experiment. The power function approximation method is used to perform curve fitting, such as Figure 4 As shown, Porosity = -28.45t -0.03272 +27.9, the approximation errors of the fitting curve are SSE = 1.17, R-square = 0.9899, ​​RMSE = 0.1855. From the above error analysis results, it can be seen that R-square is close to 1, indicating that the fitting curve is almost consistent with the scattered points, and RMSE indicates that the absolute value of the estimated error of the effective porosity is very low. Therefore, this function can be used as an approximate function curve of the effective porosity changing with time. The effective porosity, pressure, and temperature changing with time values ​​within 53 hours were obtained in the vertical bedding sample B25-2 experiment. The power function approximation method was used to fit the curve, such as Figure 5 As shown, Porosity = -10.09t -0.2261 +8.349, the approximation errors of the fitting curve are SSE=5.41, R-square=0.9117, RMSE=0.3547. From the above error analysis results, it can be seen that R-square is close to 1, indicating that the fitting curve is almost consistent with the scatter points, and RMSE indicates that the absolute value of the estimated error of the effective porosity is very low. Therefore, this function can be used as an approximation function curve of the effective porosity changing with time.

[0059] The power function obtained for the parallel bedding sample B25-1 is used to predict the results for the next 18 days, and the results are Figure 6As can be seen from the figure, the small stars represent the known experimental effective porosity data, and the dotted line represents the predicted curve. It can be seen that with the increase of time, it is expected that the effective porosity will be close to 10% when the experiment is carried out for 18 days, which is exactly 9.9782%. For the vertical bedding sample B25-2, see Figure 5 As shown, Figure 5 The scattered points in the distribution are the measured values ​​of physical experiments, and the curve is the effective porosity predicted by numerical fitting. b +c. Combine the three parameters a, b, and c within the adjustable range and draw a graph like Figure 7 The effective porosity curve range is the range of effective porosity (it can be seen that the experimental values ​​are all within the predicted range). It is estimated that when the experiment is carried out for 18 days, the maximum effective porosity is close to 9%, which is 8.1505% to be exact.

[0060] The overall performance is that the helium effective porosity curve of the parallel bedding sample B25-1 shows an early inflection point with no obvious, and an overall uniform upward trend. The effective porosity value at 25 minutes is 5.5%, the effective porosity value at 53 hours is 8.64%, and the effective porosity at 18 days is close to 10%. The helium effective porosity curve of the vertical bedding sample B25-2 shows an early and obvious inflection point, and an overall slow upward trend in the later period. The effective porosity value at 25 minutes is 6.68%, the effective porosity value at 53 hours is 8.38%, and the effective porosity at 18 days is close to 9%.

[0061] Experimental effect analysis of Example 2 of the present invention:

[0062] Pure shale has well-developed lamellae fractures, and densely developed lamellae fractures are not only seepage channels for oil and gas resources, but also important storage spaces. For tight oil and gas reservoirs with generally poor physical properties, the relative error of porosity measurement is greater due to the low effective porosity, so accurate measurement of porosity is particularly important. The standard for the current helium porosity measurement requires that the measurement equilibrium time be 25 minutes, and the experimental result is the total effective porosity of the sample. In the practice of this method, the effective porosity values ​​obtained in the 25-minute test were 5.5% and 6.68%, respectively, corresponding to the measured values ​​of 8.64% and 8.38% for 66 hours and 53 hours, with errors of 59% and 25.4%, and corresponding to the 18-day predicted maximum values ​​of 10% and 9%, with errors of 45% and 25.7%. In addition, the maximum contact surface of the parallel bedding sample with helium during the test is parallel to the bedding plane, so the contribution period of pores and fractures in this process is basically the same, and the POR-T curve first shows a less obvious inflection point, and the effective porosity value rises evenly; the maximum contact surface of the vertical bedding sample with helium during the test is perpendicular to the bedding plane, so in the early stage of helium effective porosity determination, the main features are the well-connected lamellae fractures, followed by other smaller pores, resulting in the POR-T curve first showing an early and obvious inflection point, and the effective porosity value slowly rising in the later stage. Therefore, the important parameters of helium effective porosity determination, balance time and gas injection direction, have been further optimized, and the lamellae fractures have been effectively characterized.

[0063] Based on the inventive concept of the present invention, an embodiment of the present invention also provides a method for evaluating the reservoir space of a shale reservoir, comprising using the method as described above to determine the effective porosity, matrix porosity and lamina porosity of a rock sample in a shale reservoir; and performing a reservoir space evaluation on the shale reservoir based on the determined effective porosity, matrix porosity and lamina porosity.

[0064] It should be understood that the specific order or hierarchy of steps in the disclosed process is an example of an exemplary method. Based on design preferences, it should be understood that the specific order or hierarchy of steps in the process can be rearranged without departing from the scope of protection of the present disclosure. The attached method claims present the elements of the various steps in an exemplary order and are not intended to be limited to the specific order or hierarchy described.

[0065] In the above detailed description, various features are grouped together in a single embodiment to simplify the disclosure. This method of disclosure should not be interpreted as reflecting an intention that the embodiments of the claimed subject matter require more features than are clearly stated in each claim. On the contrary, as reflected in the appended claims, the invention is in a state of having less than all the features of the disclosed individual embodiments. Therefore, the appended claims are hereby expressly incorporated into the detailed description, with each claim standing on its own as a separate preferred embodiment of the invention.

[0066] The above description includes examples of one or more embodiments. Of course, it is impossible to describe all possible combinations of components or methods for the purpose of describing the above embodiments, but it should be recognized by those skilled in the art that the various embodiments can be further combined and arranged. Therefore, the embodiments described herein are intended to cover all such changes, modifications and variations that fall within the scope of protection of the appended claims. In addition, with respect to the term "comprising" used in the specification or claims, the word is covered in a manner similar to the term "including", just as "including," explained as a transitional word in the claims. In addition, any term "or" used in the specification of the claims is intended to represent "non-exclusive or". The terms "first" and "second" are used for descriptive purposes only and are not to be understood as indicating or implying relative importance.

Claims

1. A method for determining effective porosity of shale taking into account both lamellae fractures and matrix pores. It is characterized in that The method comprises performing the following steps respectively for at least one shale rock sample: Performing a helium porosity measurement experiment on the rock sample until a first set time is reached, and obtaining a plurality of experimental data including data pairs of experimental time and effective porosity; Based on the mathematical model of shale effective porosity and experimental time, a first fitting relationship between the effective porosity of the rock sample and the experimental time is obtained by fitting the experimental data. The effective porosity, matrix porosity and lamellae fracture porosity of the rock sample are determined according to the rock sample selection direction and the first fitting relationship.

2. The method according to claim 1, It is characterized in that The at least one shale rock sample is a first rock sample whose axial direction is parallel to the shale fracture direction; or, The at least one shale rock sample is a second rock sample whose axis is perpendicular to the shale fracture direction; or, The at least one shale rock sample comprises a first rock sample whose axis is parallel to the shading fracture direction and a second rock sample whose axis is perpendicular to the shading fracture direction. The first rock sample and the second rock sample are taken from the same depth of the same core.

3. The method according to claim 2, It is characterized in that According to the rock sample selection direction and the first fitting relationship, the effective porosity, matrix porosity and lamellar fracture porosity of the rock sample are determined respectively, including: According to the first fitting relationship, a first porosity when the effective porosity change gradient begins to be less than a first gradient threshold and a second porosity when the porosity change gradient begins to be less than a second gradient threshold are determined respectively, and the first porosity is used as the effective porosity of the rock sample, and the first gradient threshold is less than the second gradient threshold; If the shale rock sample is the first rock sample, the second porosity is determined as the matrix porosity of the rock sample, and the difference between the effective porosity and the matrix porosity is determined as the lamellar fracture porosity; If the shale rock sample is the second rock sample, the second porosity is determined as the lamellar fracture porosity of the rock sample, and the difference between the effective porosity and the lamellar fracture porosity is determined as the matrix porosity.

4. The method according to claim 1, It is characterized in that The helium effective porosity measurement experiment on the rock sample comprises: Under the conditions of constant ambient temperature and injection pressure, helium effective porosity measurement experiments were carried out on rock samples.

5. The method according to claim 1, It is characterized in that The mathematical model is established in the following way: Performing helium effective porosity measurement experiments on multiple shale samples respectively until a second set time is reached, obtaining multiple experimental data including data pairs of experimental time and effective porosity, and fitting the experimental data to obtain a second fitting relationship between effective porosity and experimental time; A mathematical model of shale effective porosity and experimental time is established through the second fitting relationship of each of the multiple shale samples.

6. The method according to claim 5, It is characterized in that The second set time is greater than 50 hours.

7. The method according to claim 5, It is characterized in that The first set time is 15 to 25 hours.

8. The method according to claim 5, It is characterized in that The mathematical model is: Porosity=a×t b +c Where Porosity is the effective porosity, t is the experimental time, and a, b, and c are constants to be determined.

9. The method according to claim 1, It is characterized in that The shale rock sample is a plunger sample obtained by wire cutting method.

10. The method according to claim 1, It is characterized in that The helium effective porosity measurement experiment is performed on the rock sample until a first set time is reached to obtain experimental data including multiple experimental times and effective porosity data, and further includes: The apparent volume of the rock sample is determined by measurement.

11. A method for evaluating the reservoir space of a shale reservoir. It is characterized in that include: Using the method described in any one of claims 1 to 10, respectively determining the effective porosity, matrix porosity and lamellae porosity of the rock sample in the shale reservoir; The reservoir space of shale reservoirs is evaluated based on the determined effective porosity, matrix porosity and lamellae porosity.

Citation Information

Patent Citations

  • Method for determining different types of porosity of shale

    CN110487693A

  • Pore formation and evolution evaluation method for continental facies shale oil reservoir of large freshwater lake basin

    CN111610130A

  • Method and device for measuring effective porosity of shale rock

    CN111650108A

  • Method for measuring porosity of stratified shale bedding seam

    CN116106193A

  • Method for determining a quantity of gas adsorbed in a porous medium

    US20210255084A1

Cited By

  • Improved GIP porosity determination method based on pressure attenuation

    CN119715300A