Method and equipment for detecting gas adsorption capacity of material
By introducing specific gas into the experimental cavity and recording concentration changes, combined with constant temperature and high-purity nitrogen purge, the accuracy and operation complexity of gas adsorption capacity detection in the prior art are solved, and the accuracy of the detection results are achieved and highly adaptable gas adsorption capacity detection.
Patent Information
- Application Number
- CN202411087187.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-22
AI Technical Summary
The existing gas adsorption capacity detection methods cannot accurately detect the adsorption performance of materials on specific gases, and are complex in operation, greatly affected by electrode process errors, and their practicality is limited.
By entering specific gas into the experimental cavity, recording the gas concentration changes until it is stable, calculating the adsorption capacity, using fixed flow and constant temperature devices to ensure detection accuracy, combining asbestos materials to reduce the impact of the airflow, and using high-purity nitrogen purge and fluorescence reaction detection Changes in gas concentration.
The accuracy of the detection results and the convenience of operation are achieved, the impact of ambient temperature is reduced, and the adaptability and accuracy of the detection are improved.
Smart Images

Figure CN119000466A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of inspection and detection technology, and in particular to a method and equipment for detecting the gas adsorption capacity of a material. Background Art
[0002] The phenomenon that gas or steam is captured by the solid surface and attached to the surface to form a single or multiple gas molecular layers is called adsorption. Adsorption capacity refers to the weight or amount of adsorbate adsorbed by a unit weight of adsorbent at a certain temperature and a certain adsorbate concentration. It is the ability of filter material or ion exchanger to adsorb a certain substance or ion, that is, the adsorption amount. By exploring the adsorption capacity of a material for a specific gas, the material with the best adsorption for the specific gas can be selected, which is of great significance in the selection of air purification materials, mask filter materials, filter cigarette holder materials and other fields. Chinese patent 2008101276992 discloses "Sample placement device for detecting trace pollutant gas adsorption filter material", and the authorization announcement number is CN101625295B. The sample placement device can provide the necessary performance data (temperature, dew point, pressure and concentration, etc.) of the adsorption effect of the filter material to be tested on a specific gas. However, the device cannot detect and provide technical parameters of the adsorption performance of the filter material for a specific gas. Another Chinese patent application 2023105595775 discloses "A method for measuring gas adsorption based on an applied electric field", and the application publication number is CN116593534A. This measurement method coats the gas-sensitive material on an acrylic plate, places the acrylic plate between two flat electrodes, and adjusts the distance between the two flat electrodes by a spiral micrometer and a cylinder, thereby adjusting the surrounding electric field. After the gas is introduced, the resistance of the gas-sensitive material is measured, and the gas adsorption performance of the gas-sensitive material is measured according to the change in resistance value. This method has high process requirements for the flat electrode and the electrode distance adjustment mechanism, and the process error of the electrode has a great influence on the detection results. Its practicality is subject to certain limitations. Summary of the invention
[0003] In view of the above technical problems, the object of the present invention is to provide a method and a device for detecting the gas adsorption capacity of a material with accurate detection results, strong adaptability and convenient operation.
[0004] The gas adsorption capacity detection method of a material described in the present invention comprises the following steps:
[0005] Step 1: introduce a specific gas into the experimental channel with an empty experimental cavity, so that the specific gas enters from the input port of the experimental channel and is discharged from the output port, and detects the concentration change of the specific gas at the output port of the experimental channel until the concentration of the specific gas at the output port reaches a stable value, and records the time t from the start of introducing the specific gas to the concentration of the specific gas at the output port reaching a stable value 1 ;
[0006] Step 2: Fill the test chamber with the material to be tested and record the weight m of the material to be tested xf , introduce a fixed flow of specific gas into the experimental channel of the experimental cavity with the material to be tested, and record the gas flow rate V at the input port 1 And the intake air concentration I 0 , detect the concentration change of the specific gas at the output port of the experimental channel until the specific gas concentration at the output port reaches a stable value, and record the stable gas concentration value I t And the time t from the start of the introduction of a specific gas to the time when the concentration of the specific gas at the output port reaches a stable value 2 , Gas flow rate V at the output port 2 ;
[0007] The adsorption capacity of the material to be detected for the specific gas is obtained by the following calculation formula:
[0008]
[0009] Among them: a 0 is the adsorption capacity, in mg g -1 ;
[0010] V 1 is the gas flow rate at the inlet, in m 3 ·min -1 ;
[0011] V 2 is the gas flow rate at the outlet, in m 3 ·min -1 ;
[0012] m xf is the mass of adsorbent in adsorption experiment, in g;
[0013] I 0 is the inlet concentration of a specific gas, in mg·m -3 ;
[0014] t f is the adsorption time, t f =t 2 -t 1 , the unit is min;
[0015] I t It is the gas concentration value when the specific gas concentration at the output port reaches a stable value, in mg·m -3 .
[0016] Through this solution, it is only necessary to detect the time when a specific gas reaches a stable value at the output port of the experimental chamber and the change in gas concentration to calculate the adsorption capacity of the adsorption material for this gas. The detection result is accurate, adaptable and easy to operate.
[0017] Preferably, in step 1 and step 2, the experimental chamber is in a set constant temperature state.
[0018] Through this solution, the influence of ambient temperature on the detection results can be reduced.
[0019] Preferably, in step 2, before the experimental cavity is filled with the material to be tested, the experimental channel is purged with high-purity nitrogen until the concentration of the specific gas at the detection output port is 0; the method for detecting the concentration change of the specific gas at the output port of the experimental channel is as follows: the specific gas discharged from the output port of the experimental channel is absorbed by the solution, and the concentration of the specific gas in the solution is calculated through fluorescence reaction at regular intervals.
[0020] Through this solution, the change of gas concentration at the output port can be detected.
[0021] Preferably, in step 2, before the experimental cavity is filled with the material to be tested, the experimental channel is purged with high-purity nitrogen until the concentration of the specific gas at the detection output port is 0; the concentration change of the specific gas at the output port of the experimental channel is detected by using a specific gas detection instrument to detect the gas concentration at the output port.
[0022] Through this solution, the change of gas concentration at the output port can be detected.
[0023] Preferably, the experimental cavity is cylindrical, and asbestos material is filled at both ends of the experimental cavity where the material to be tested is filled.
[0024] Through this solution, the asbestos material can reduce the impact of airflow on the adsorption material and improve the accuracy of the detection result.
[0025] Preferably, the specific gas is benzene or toluene, and the material to be detected is graphene or activated carbon or silicon dioxide.
[0026] Through this solution, the accuracy of the detection results is higher.
[0027] The detection device for a gas adsorption capacity detection method of a material described in the present invention comprises an experimental channel with an input port and an output port, wherein an experimental cavity for filling the material to be detected is arranged in the experimental channel, and asbestos material is filled at both ends of the filling place of the material to be detected in the experimental cavity; an input gas flow meter is arranged on the input port, and an output gas flow meter and an output gas concentration detection device are arranged on the output port.
[0028] Through this solution, the gas flow rate and gas concentration at the output port of the experimental channel can be accurately detected.
[0029] Preferably, a constant temperature device is provided on the experimental chamber.
[0030] Through this solution, the influence of ambient temperature on the detection results can be reduced.
[0031] Preferably, the output gas concentration detection device is a gas concentration detector.
[0032] Through this solution, the change of gas concentration at the output port can be detected.
[0033] Preferably, the output gas concentration detection device is a solvent absorption device for absorbing the gas discharged from the output port.
[0034] Through this solution, the change of gas concentration at the output port can be detected.
[0035] Due to the adoption of the above technical scheme, the present invention detects the time for a specific gas to reach a stable value at the output port of the experimental chamber and the change in gas concentration and obtains the adsorption capacity of the adsorption material for this gas through calculation. The detection result is accurate, adaptable and easy to operate. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] In order to more clearly illustrate the technical solution of the present invention, the drawings required for use in the description will be briefly introduced below. Obviously, the drawings in the following description are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without paying any creative work.
[0037] Figure 1 It is a schematic structural diagram of an embodiment of the detection device of the present invention. DETAILED DESCRIPTION
[0038] In order to make the purpose, features and advantages of the present invention more obvious and easy to understand, the technical solutions in the present invention are described clearly and completely in conjunction with the accompanying drawings. Obviously, the embodiments described below are only part of the embodiments of the present invention, not all of them. Based on the embodiments in this patent, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of this patent.
[0039] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.
[0040] The terms "first", "second", "third", "fourth", etc. (if any) in the specification and claims of the present invention and the drawings are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that the numbers used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions.
[0041] like Figure 1 As shown, the detection device for the gas adsorption capacity detection method of a material of the present invention comprises an experimental channel 3 with an input port 1 and an output port 2. The experimental channel 3 is a circular tubular structure, and its two ends are respectively connected to an input end cover 11 and an output end cover 12 by threads. The input end cover 11 is provided with an input port 1, and the output end cover 12 is provided with an output port 2. The experimental channel 3 is provided with an experimental cavity for filling the material to be detected. The experimental cavity is a cylindrical cavity located in the inner cavity of the experimental channel 3. Asbestos material is filled at both ends of the place where the material to be detected is filled in the experimental cavity; the input port 1 is provided with an input gas flowmeter 4, and the input gas flowmeter 4 is used to detect the gas flow entering the experimental channel 3 through the input port 1; the output port 2 is provided with an output gas flowmeter 5 and an output gas concentration detection device 6, and the output gas flowmeter 5 is used to detect the gas flow discharged from the output port 2 of the experimental channel 3, and the output gas concentration detection device 6 is used to detect the concentration of the gas discharged from the output port 2.
[0042] In addition, in order to reduce the influence of the ambient temperature on the detection data, a constant temperature device is provided on the experimental chamber, which can adopt various existing temperature adjustment devices such as water bath heating or thermal radiation heating.
[0043] The output gas concentration detection device 6 can adopt a gas concentration detector for the gas to be detected, or it can adopt a solvent absorption device for absorbing the gas discharged from the output port. The gas discharged from the output port 2 of the experimental channel 3 is passed into the absorption device, and the concentration of the gas discharged from the output port 2 is detected by the fluorescent reaction of the solvent after absorbing the gas.
[0044] The gas adsorption capacity detection method of a material described in the present invention adopts the above detection device and comprises the following steps:
[0045] Step 1: introduce a specific gas into the experimental channel with an empty experimental cavity, so that the specific gas enters from the input port of the experimental channel and is discharged from the output port, and detects the concentration change of the specific gas at the output port of the experimental channel until the concentration of the specific gas at the output port reaches a stable value, and records the time t from the start of introducing the specific gas to the concentration of the specific gas at the output port reaching a stable value 1;
[0046] Step 2: Before officially starting the test, use 99.999% high-purity nitrogen to purge the experimental channel until the specific gas concentration at the test output port is 0. Then, fill the test cavity with the material to be tested and record the weight m of the material to be tested. xf , introduce a fixed flow of specific gas into the experimental channel of the experimental cavity with the material to be tested, and record the gas flow rate V at the input port 1 And the intake air concentration I 0 , detect the concentration change of the specific gas at the output port of the experimental channel until the specific gas concentration at the output port reaches a stable value, and record the stable gas concentration value I t And the time t from the start of the introduction of a specific gas to the time when the concentration of the specific gas at the output port reaches a stable value 2 , Gas flow rate V at the output port 2 ;
[0047] There are two methods for detecting the concentration change of the specific gas at the output port of the experimental channel:
[0048] One is to use the solution to absorb the specific gas discharged from the output port of the experimental channel, and calculate the concentration of the specific gas in the solution through fluorescence reaction at regular intervals. When the difference in the concentration data of the specific gas detected several times in a row is less than a specific threshold, it can be considered that the concentration of the specific gas has reached a stable value.
[0049] Another method is to set a detection instrument for the specific gas at the output port of the experimental channel, and use the detection instrument to detect the gas concentration at the output port. When the detection instrument shows that the change amplitude of the gas concentration is less than a specific threshold within a certain period of time, it can be considered that the specific gas concentration has reached a stable value.
[0050] After the concentration of the specific gas at the output port reaches a stable value, the adsorption capacity of the material to be detected for the specific gas is obtained by the following calculation formula:
[0051]
[0052] Among them: a 0 is the adsorption capacity, in mg g -1 ;
[0053] V 1 is the gas flow rate at the inlet, in m 3 ·min -1 ;
[0054] V 2 is the gas flow rate at the outlet, in m 3 ·min -1 ;
[0055] m xf is the weight of the material to be tested, in g;
[0056] I 0 is the inlet concentration of a specific gas, in mg·m -3 ;
[0057] t f is the adsorption time, t f =t 2 -t 1 , the unit is min;
[0058] I t It is the gas concentration value when the specific gas concentration at the output port reaches a stable value, in mg·m -3 .
[0059] In this formula, V 1 -V 2 The actual flow rate of a specific gas entering the experimental chamber can be obtained (V 1 -V 2 )*I 0 t f The total volume of the specific gas actually entering the experimental chamber can be obtained by multiplying the flow rate of the specific gas actually entering the experimental chamber by the adsorption time. The total volume of the specific gas actually entering the experimental chamber can be obtained by multiplying the total volume of the specific gas actually entering the experimental chamber by the intake concentration.
[0060] The total amount of specific gas discharged from the output port is calculated, and the total amount of specific gas actually entering the experimental cavity is subtracted from the total amount of specific gas discharged from the output port to obtain the total amount of specific gas adsorbed by the material to be detected in the experimental cavity. The total amount of specific gas adsorbed by the material to be detected is divided by the weight of the material to be detected to calculate the amount of specific gas adsorbed by the material to be detected per unit weight, that is, the adsorption capacity of the material to be detected for the specific gas.
[0061] As a further improvement of the present invention, in step one and step two, the experimental chamber is in a set constant temperature state.
[0062] As a specific embodiment of the present invention, the specific gas is selected from benzene or toluene, and the material to be detected is selected from graphene or activated carbon or silicon dioxide. Each combination selects three specific gases of different concentrations for detection three times. The detection data are shown in Table 1 below:
[0063]
[0064]
[0065] From the above tests, it can be seen that the adsorption capacity of the material for a specific gas has little to do with the concentration of the specific gas. As long as the adsorption time is sufficient, the final adsorption capacity data is basically consistent.
[0066] As a comparative experiment, after completing the above embodiments, the material to be detected in the experimental cavity is taken out, the material to be detected is sealed, and the specific gas adsorbed in the material to be detected is released by thermal analysis and precisely measured to obtain the total amount of the specific gas actually adsorbed by the material to be detected. Then, the total amount of the specific gas actually adsorbed by the material to be detected is divided by the weight of the material to be detected. In this way, the adsorption capacity a of the material to be detected for the specific gas can also be obtained. 1 The data obtained from the comparative experiment are shown in Table 2 below:
[0067]
[0068]
[0069] After verification by comparative examples, the gas adsorption capacity detection method of the material of the present invention obtains the adsorption capacity a 0 The adsorption capacity a obtained by thermal desorption 1 The error between the two is extremely small, and the detection result of the invention is accurate, adaptable and easy to operate.
Claims
1. A method for detecting the gas adsorption capacity of a material, characterized in that: The following steps are included: Step 1: introduce a specific gas into an experimental channel with an empty experimental cavity, so that the specific gas enters from the input port of the experimental channel and is discharged from the output port, and detects the concentration change of the specific gas at the output port of the experimental channel until the concentration of the specific gas at the output port reaches a stable value, and records the time t1 from the start of introducing the specific gas to the concentration of the specific gas at the output port reaching a stable value; Step 2: Fill the test chamber with the material to be tested and record the weight m of the material to be tested xf , introduce a fixed flow rate of specific gas into the experimental channel of the experimental cavity with the material to be tested, record the gas flow rate V1 at the input port and the inlet concentration I0, detect the concentration change of the specific gas at the output port of the experimental channel until the specific gas concentration at the output port reaches a stable value, and record the stable gas concentration value I t and the time t2 from the start of the introduction of the specific gas to the specific gas concentration at the output port reaching a stable value, and the gas flow rate V2 at the output port; The adsorption capacity of the material to be detected for the specific gas is obtained by the following calculation formula: Where: a0 is the adsorption capacity, unit is mg g -1 ; V1 is the gas flow rate at the inlet, in m 3 ·min -1 ; V2 is the gas flow rate at the output port, in m 3 ·min -1 ; m xf is the mass of adsorbent in adsorption experiment, in g; I0 is the specific gas intake concentration, in mg·m -3 ; t f is the adsorption time, t f =t2-t1, unit is min; I t It is the gas concentration value when the specific gas concentration at the output port reaches a stable value, in mg·m -3 .
2. The method for detecting the gas adsorption capacity of a material according to claim 1, characterized in that: In step 1 and step 2, the experimental chamber is in a set constant temperature state.
3. The method for detecting the gas adsorption capacity of a material according to claim 1 or 2, characterized in that: In step 2, before the test material is filled in the test cavity, the test channel is purged with high-purity nitrogen until the concentration of the specific gas at the test output port is 0; the method for detecting the concentration change of the specific gas at the output port of the test channel is as follows: The specific gas discharged from the output port of the experimental channel is absorbed by the solution, and the concentration of the specific gas in the solution is calculated through fluorescence reaction at regular intervals.
4. The method for detecting the gas adsorption capacity of a material according to claim 1 or 2, characterized in that: In step 2, before the experimental cavity is filled with the material to be tested, the experimental channel is purged with high-purity nitrogen until the concentration of the specific gas at the detection output port is 0; the concentration change of the specific gas at the output port of the experimental channel is detected by using a specific gas detection instrument to detect the gas concentration at the output port.
5. The method for detecting the gas adsorption capacity of a material according to claim 1 or 2, characterized in that: The experimental cavity is cylindrical, and asbestos material is filled at both ends of the place where the material to be tested is filled in the experimental cavity.
6. The method for detecting the gas adsorption capacity of a material according to claim 1 or 2, characterized in that: The specific gas is benzene or toluene, and the material to be detected is graphene or activated carbon or silicon dioxide.
7. A detection device for a method for detecting the gas adsorption capacity of a material according to any one of claims 1 to 6, comprising an experimental channel (3) with an input port (1) and an output port (2), characterized in that: The experimental channel (3) is provided with an experimental cavity for filling the material to be tested, and both ends of the experimental cavity where the material to be tested is filled are filled with asbestos material; the input port (1) is provided with an input gas flow meter (4), and the output port (2) is provided with an output gas flow meter (5) and an output gas concentration detection device (6).
8. The gas adsorption capacity detection device of a material according to claim 7, characterized in that: The experimental cavity is provided with a constant temperature device.
9. A gas adsorption capacity detection device for a material according to claim 7 or 8, characterized in that: The output gas concentration detection device (6) is a gas concentration detector.
10. A gas adsorption capacity detection device for a material according to claim 7 or 8, characterized in that: The output gas concentration detection device (6) is a solvent absorption device used to absorb the gas discharged from the output port.
Citation Information
Patent Citations
Adsorption performance testing device for ammonia gas
CN110849762A
Method for determining diffusion coefficient and distribution coefficient of sink material
CN111829927A
Method and device for in-situ detection of activated carbon adsorption saturation of gas phase adsorption bed
CN114813847A
System for detecting adsorption capacity of gas adsorbent and detection method thereof
CN117214318A
Method and apparatus for treating gas with inorganic adsorbent
JP1999033335A