Multi-core optical fiber

By using an outer cladding with a high refractive index in the multi-core optical fiber to surround the inner cladding, forming a rotatable symmetrical configuration, the problem of increasing the difficulty of core recognition in the prior art is solved, and a stable core recognition effect is achieved.

CN119013594APending Publication Date: 2024-11-22SUMITOMO ELECTRIC INDUSTRIES LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380019968.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-24
Filing Date
2023-03-17
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the prior art, when the end surface of a multi-core optical fiber is observed by side illumination, the brightness of the mark and core is easily affected by the incident direction of the illumination light, resulting in increased difficulty in core recognition.

Method used

Using an outer cladding that is higher than the inner cladding, multiple cores and marks are arranged by forming a plan pattern of one rotational symmetry. The outer cladding surrounds the inner cladding to ensure that the observation light propagates within the outer cladding and enters the inner cladding. , realize the uniformization of the end face image, and stabilize the identification of cores and marks.

Benefits of technology

The marks and core brightness changes caused by the observation direction of light incident are effectively suppressed, and a stable core recognition effect is achieved, ensuring that the brightness uniformity of the inner cladding is achieved regardless of the side of the observation light incident from, and the reliability of core recognition is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119013594A_ABST
    Figure CN119013594A_ABST
Patent Text Reader

Abstract

An MCF according to an embodiment stably identifies a core. The MCF is provided with a glass optical fiber and a resin coating. The glass optical fiber includes a plurality of cores, a mark, and a cladding. In a cross-section of the MCF, the arrangement of the centers of the plurality of cores and the center of the mark has no rotational symmetry with respect to the center of the cross-section. The cladding includes an inner cladding surrounding the plurality of cores and the mark, and an outer cladding disposed on an outer peripheral surface of the inner cladding and having a refractive index higher than a refractive index of the inner cladding.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a multi-core optical fiber (hereinafter referred to as “MCF”).

[0002] This application claims the priority based on Japanese Patent Application No. 2022-048368 filed on March 24, 2022, is based on the content thereof, and is incorporated into this specification by reference to the entire content thereof. Background Art

[0003] For example, as described in Patent Document 1, in an MCF, a mark having a refractive index different from that of the cladding is introduced into the cladding. It is known that in the cross section of the MCF obtained by cutting at any position along the length direction, multiple cores can be identified separately. The marks in the cladding are arranged at positions where the distances to the multiple cores are uneven. In the case of a mark having a refractive index higher than that of the cladding, the mark has a diameter smaller than the diameter of the core or a refractive index lower than the refractive index of the core. As a result, the coupling between the mode propagating in the core and the mode propagating in the mark is suppressed, and noise is suppressed from mixing into the signal light propagating in the core.

[0004] In the case of identifying multiple cores separately by observing the end face of the MCF cut at any position along the length direction, end face observation by side lighting is performed. In this end face observation, illumination light is irradiated from the side of the MCF near the cutting position. When the illumination light propagates in the MCF, the illumination light is restricted in the high refractive index area and propagates with low propagation loss. On the other hand, it leaks and propagates with high propagation loss in the low refractive index area. As a result, in the end face image of the MCF, the higher the refractive index area, the brighter it appears, and the lower the refractive index area, the darker it appears. By identifying the cores and marks based on the end face image showing such light and dark, multiple cores can be identified separately.

[0005] Prior art literature

[0006] Patent Literature

[0007] Patent Document 1: Japanese Patent Application Publication No. 2011-170099 Summary of the invention

[0008] The MCF involved in the present disclosure comprises a glass optical fiber and a resin coating. The glass optical fiber includes a plurality of cores extending along a central axis (hereinafter referred to as "optical fiber axis"), a marker extending along the plurality of cores, and a cladding surrounding the plurality of cores and the marker. The resin coating is disposed on the outer peripheral surface of the glass optical fiber. In particular, on a cross section of the MCF orthogonal to the optical fiber axis, the arrangement of the centers of the plurality of cores and the centers of the markers has no rotational symmetry relative to the center of the cross section. Furthermore, the cladding is composed of an inner cladding and an outer cladding. The inner cladding surrounds the plurality of cores and the markers while being in contact with the plurality of cores and the markers. The outer cladding is disposed on the outer peripheral surface of the inner cladding and has a refractive index higher than that of the inner cladding. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 It is a diagram showing an example of the structure of the MCF involved in the present disclosure and an example of an observation device for the end surface of the MCF.

[0010] Figure 2 It is a diagram showing a cross-sectional structure of an MCF according to the present disclosure.

[0011] Figure 3 It is a diagram for explaining an example of the cross-sectional structure of each of the MCF according to the present disclosure and the MCF according to the comparative example. DETAILED DESCRIPTION

[0012] [Technical Problems to be Solved by the Present Disclosure]

[0013] The inventors studied the above-mentioned prior art and found the following technical problems. That is, in the above-mentioned prior art, when observing the end face of the MCF by side lighting, the brightness of the mark and the core in the end face changes depending on which side of the optical fiber the illumination light enters, making it difficult to identify the core.

[0014] The present disclosure has been made to solve the above-mentioned technical problems, and an object of the present disclosure is to provide an MCF having a structure for realizing stable core identification.

[0015] [Effects of the present disclosure]

[0016] According to the MCF of the present disclosure, core identification can be performed stably.

[0017] [Description of Embodiments of the Present Disclosure]

[0018] First, the contents of the embodiments of the present disclosure are listed separately and described.

[0019] MCF of the present disclosure

[0020] (1) It has a glass optical fiber and a resin coating. The glass optical fiber includes a plurality of cores extending along the optical fiber axis, a mark extending along the plurality of cores, and a cladding surrounding the plurality of cores and the marks. The resin coating is provided on the outer peripheral surface of the glass optical fiber. In particular, in a cross section of the MCF orthogonal to the optical fiber axis, the arrangement of the centers of the plurality of cores and the centers of the marks relative to the center of the cross section has no rotational symmetry because they form a plane figure with first rotational symmetry. Furthermore, the cladding is composed of an inner cladding and an outer cladding. The inner cladding surrounds the plurality of cores and the marks while in contact with the plurality of cores and the marks. The outer cladding is provided on the outer peripheral surface of the inner cladding and has a refractive index higher than that of the inner cladding. It should be noted that the optical fiber axis is equivalent to the central axis of the MCF. The outer peripheral surface of the glass optical fiber is equivalent to the outer peripheral surface of the cladding. The center of the cross section is equivalent to the position where the cross section intersects with the optical fiber axis.

[0021] As described above, the MCF disclosed in the present invention is configured such that an inner cladding in which a plurality of cores and marks are arranged is surrounded by an outer cladding having a refractive index higher than that of the inner cladding. In this configuration, even when the illumination light for observing the end face of the optical fiber (hereinafter referred to as "observation light") is irradiated to a single side of the MCF, a portion of the observation light will propagate in the outer cladding. In this way, not only the side irradiated with the observation light, but also the observation light that goes around to the opposite side of the inner cladding can easily enter the inner cladding, so that an end face image of the inner cladding with uniform brightness as a whole can be obtained. In other words, the brightness variation of the marks and cores caused by the incident direction of the observation light is effectively suppressed, and the core identification can be stably performed.

[0022] (2) In (1) above, in the cross section of the MCF, when the diameter of the outer cladding is set to 2A and the diameter of the inner cladding is set to 2B, the ratio B / A of the radius B of the inner cladding to the radius A of the outer cladding can be greater than 1 / 3 and less than 2 / 3. When the ratio B / A is less than 1 / 3, the outer cladding becomes too thick, so the degree of freedom of arrangement of the multiple cores and marks in the inner cladding is limited. On the other hand, when the ratio B / A is greater than 2 / 3, the outer cladding becomes too thin, so a sufficient amount of observation light cannot be transmitted to the back side of the MCF that is not irradiated with the observation light.

[0023] (3) In the above (1) or (2), the absolute value of the relative refractive index difference of the inner cladding with respect to the refractive index of the outer cladding is preferably not less than 0.02% and not more than 0.3%. In this case, since a portion of the observation light is appropriately confined in the outer cladding, it can propagate in the outer cladding while being partially coupled with the mode in the inner cladding.

[0024] (4) In any one of (1) to (3) above, the arrangement of the centers of the plurality of cores may have rotational symmetry with respect to the center of the cross section.

[0025] Each of the aspects listed in the column “Description of Embodiments of the Present Disclosure” may be applied to each of all the remaining aspects or to all combinations of the remaining aspects.

[0026] [Details of the embodiments of the present disclosure]

[0027] Hereinafter, the specific structure of the MCF of the present disclosure will be described in detail with reference to the accompanying drawings. It should be noted that the present disclosure is not limited to these examples, but is shown by the claims, and is intended to include all variations within the meaning and scope equivalent to the claims. In addition, the same elements are marked with the same figure numbers in the description of the drawings, and repeated descriptions are omitted.

[0028] Figure 1 : is a diagram showing an example of the structure of the MCF involved in the present disclosure and an example of an observation device for the end surface of the MCF ( Figure 1 (referred to as “end face observation” in the text). Figure 1 The upper part ( Figure 1 ” (referred to as “observation object (optical fiber structure)” in FIG. 1 ) shows an example of a representative structure of the MCF 100 involved in the present disclosure. Figure 1 The lower part ( Figure 1 2 (referred to as “observation device” in the figure) shows a schematic structure of an observation device for observing the end surface of the MCF involved in the present disclosure.

[0029] Figure 1 The observation object shown in the upper part, namely, MCF100, comprises a glass optical fiber 110 and a resin coating 140 provided on the outer peripheral surface of the glass optical fiber 110. The glass optical fiber 110 includes two cores 111, 112, a cladding 120, and a marker 130. More than three cores can also be applied to MCF100. The two cores 111, 112 extend along the optical fiber axis AX which is the central axis of the MCF100. The marker 130 extends along the two cores 111, 112. The cladding 120 surrounds the two cores 111, 112 and the marker 130. It should be noted that the marker 130 has a refractive index different from that of the cladding 120. The cladding 120 includes an inner cladding 121 and an outer cladding 122. The inner cladding 121 surrounds the two cores 111, 112 and the mark 130. The outer cladding 122 is disposed on the outer peripheral surface of the inner cladding 121 and has a refractive index higher than that of the inner cladding 121. When observing the end face through side lighting, as shown in FIG. Figure 1 As shown in the upper part of FIG. 1 , a part of the resin coating 140 covering the front end portion of the glass optical fiber 110 including the end face is removed.

[0030] The end surface observation of MCF100 having the above structure is as follows: Figure 1The observation device shown in the lower part of the MCF 100 is used for observation. That is, the observation device includes a light source 501, a mirror element 502, and a camera 503 as an end face imaging camera. In the end face observation of the MCF 100, first, the observation light LL is irradiated from the light source 501 to the side of the front end portion of the glass optical fiber 110 including the end face. The observation light LL incident on the glass optical fiber 110 is emitted from the end face of the glass optical fiber 110 toward the mirror element 502, and is reflected by the mirror element 502. Furthermore, the observation light LL reflected by the mirror element 502 reaches the imaging surface of the camera 503. When the observation light LL propagates in the glass optical fiber 110, the observation light LL is restricted in the high refractive index regions such as the two cores 111 and 112 and propagates with low propagation loss. On the other hand, in the low refractive index regions such as the cladding 120, the observation light LL propagates with high propagation loss while leaking to the outside. Thus, by setting a sufficient propagation distance, in the end face image of the glass optical fiber 110, the higher the refractive index region is displayed brighter, and the lower the refractive index region is displayed darker. However, since leakage to the outside is easy to occur in the low refractive index region, and intrusion from the outside is easy to occur, when the propagation distance is sufficiently shortened, in the end face image of the glass optical fiber 110, there is a case where the higher the refractive index region is displayed darker, and the lower the refractive index region is displayed brighter. By identifying the two cores 111, 112 and the mark 130 based on the end face image showing such light and dark, the two cores 111, 112 can be identified separately.

[0031] Figure 2 is a diagram showing a cross-sectional structure of an MCF involved in the present disclosure ( Figure 2 double cladding structure). Figure 2 The upper part ( Figure 2 The cross-sectional structure is shown in FIG. Figure 1 The cross-sectional structure of the MCF100 according to the present disclosure is obtained by taking the line II shown in the upper part of FIG. Figure 2 The middle part ( Figure 2 The refractive index distribution is shown in Fig. Figure 2 The refractive index distribution 150 is a refractive index distribution of each part obtained by the line L shown in the upper part. Figure 2 The lower part ( Figure 2 2 is a diagram for explaining the propagation state of the observation light in the glass optical fiber 110 from which the resin coating 140 is removed in the MCF 100. It should be noted that Figure 2 The optical fiber cross section shown in the lower part is the cross section of the glass optical fiber 110 in the MCF100 without the resin coating 140, which is equivalent to the cross section along Figure 1 A portion of the optical fiber cross section obtained by line II shown in the upper part.

[0032] like Figure 2As shown in the upper part of , the glass optical fiber 110 of MCF100 includes a cladding 120, and the cladding 120 has a double cladding structure, which is composed of an inner cladding 121 with a diameter of 2B and an outer cladding 122 with a diameter of 2A. In the inner cladding 121 with a diameter of 2B, two cores 111, 112 and a mark 130 are arranged along the length direction of MCF100. The arrangement of the centers of the two cores 111, 112 and the center of the mark 130 relative to the center of the cross section has no rotational symmetry because they constitute a plane figure with one rotational symmetry. That is, the element configuration consisting of only the two cores 111, 112 has rotational symmetry because it constitutes a plane figure with two rotational symmetry, but the element configuration that also includes the mark 130 loses rotational symmetry.

[0033] In addition, MCF100 has Figure 2 The refractive index distribution 150 shown in the middle of FIG. That is, the two cores 111 and 112 arranged in a manner sandwiching the optical fiber axis AX each have a refractive index n1. The inner cladding 121 has a refractive index n2 lower than the refractive index n1 of the two cores 111 and 112. The outer cladding 122 has a refractive index n2 lower than the refractive index n1 of the two cores 111 and 112 and higher than the refractive index n2 of the inner cladding 121. C It should be noted that, in this specification, “the refractive index of the cladding 120 ” refers to the refractive index n of the outer cladding 122 . C . In addition, the refractive index of the mark 130 only needs to be different from the refractive index n2 of the inner cladding 121. For example, the refractive index of the mark 130 may have a relative refractive index difference of 0.25% or more with the refractive index n2 of the inner cladding 121. This enables reliable identification. For example, the mark 130 may have a refractive index higher than the refractive index n2, and the product of the relative refractive index difference and the mark radius may be less than 1.0 [%·μm]. This suppresses the loss caused by the coupling of the mode propagating in the core with the mode in the mark.

[0034] In addition, the cores 111 and 112 of MCF100 each have at least one mode for waveguide of light of wavelength 1550nm, which is a representative communication wavelength. The waveguide mode of one core has sufficiently low inter-core crosstalk with the waveguide modes of other cores. For example, any inter-core crosstalk may be below -60dB / km. In this case, the noise caused by the crosstalk becomes a negligible level. For example, it may be that the crosstalk between signal lights propagating in opposite directions between any cores is -60dB / km, or the crosstalk between signal lights propagating in the same direction is -60dB / km. In this case, by appropriately selecting the propagation direction, the noise caused by the crosstalk becomes a negligible level. In order to suppress the crosstalk to the above level at a wavelength of 1550nm, the center-to-center distance between adjacent cores may be 30μm or more. In addition, the center-to-center distance between adjacent cores may also be 50μm or less. Thus, even when the outer cladding 122 is made thick enough, leakage loss caused by mode coupling from the cores 111 and 112 to the outer cladding 122 can be suppressed. Furthermore, the effective refractive index of the waveguide mode between adjacent cores can differ by more than 0.01%. Thus, even when the center-to-center distance between adjacent cores is short, crosstalk can be suppressed. The core diameter can be more than 8 μm and less than 15 μm, and the relative refractive index difference between the cores 111 and 112 and the inner cladding 121 can be more than 0.3% and less than 0.5%. Thus, crosstalk can be suppressed, and noise caused by high-order modes can be suppressed.

[0035] from Figure 1 The observation light LL irradiated from the light source 501 shown in the lower part of the glass optical fiber 110 to the side is incident on the glass optical fiber 110. Figure 2 As shown in the lower part of , a part of the observation light LL propagates in the outer cladding 122. That is, the observation light LL leaks into the inner cladding 121 while propagating in the outer cladding 122, and reaches the back side of the glass optical fiber 110 irradiated with the observation light LL. In this way, the observation light LL incident on the glass optical fiber 110 is partially reflected at the interface between the inner cladding 121 and the outer cladding 122, and the partially reflected observation light LL is multiply reflected in the outer cladding 122. As a result, since the observation light LL is uniformly dispersed and / or uniformly diffused in the outer cladding 122 while coupling with the cores 111, 112 and the marker 130, the light amount of the observation light LL coupled with the cores 111, 112 and the marker 130 is stable regardless of the incident direction of the observation light LL.

[0036] It should be noted that, regarding the appropriate thickness of the outer cladding 122, when the diameter of the outer cladding 122 is set to 2A and the diameter of the inner cladding 121 is set to 2B, the ratio B / A of the radius B of the inner cladding 121 to the radius A of the outer cladding 122 is preferably not less than 1 / 3 and not more than 2 / 3. When the ratio B / A is less than 1 / 3, the outer cladding 122 becomes too thick, so the degree of freedom of arrangement of the cores 111, 112 and the marker 130 in the inner cladding 121 is limited. On the other hand, when the ratio B / A is greater than 2 / 3, the outer cladding 122 becomes too thin, so a sufficient amount of observation light LL cannot be propagated to the back side of the glass optical fiber 110 that is not irradiated with the observation light LL.

[0037] Furthermore, the refractive index n of the outer cladding 122 is C The absolute value of the relative refractive index difference of the reference inner cladding 121 is preferably 0.02% to 0.3%. In this case, since part of the observation light LL is appropriately confined in the outer cladding 122 , it can propagate in the outer cladding 122 while being partially coupled with the mode in the inner cladding 121 .

[0038] Figure 3 : is a diagram for explaining an example of the cross-sectional structure of each of the MCF involved in the present disclosure and the MCF involved in the comparative example ( Figure 3 (referred to as “cross-sectional structure” in the text). Figure 3 The upper part ( Figure 3 2 (denoted as “2 cores” in FIG. 1 ) shows the cross-sectional structures of MCF600A according to the comparative example and MCF100A ( 100 ) according to the present embodiment. Figure 3 The lower part ( Figure 3 4 cores) shows the cross-sectional structure of the MCF600B involved in the comparative example and the MCF100B involved in the present embodiment. It should be noted that, Figure 3 The fiber cross sections shown correspond to the Figure 1 A portion of the optical fiber cross section obtained by line II shown in the upper part.

[0039] Figure 3 The MCF600A involved in the comparative example shown in the upper part of is a 2-core MCF. The MCF600A includes a glass optical fiber 610A and a resin coating 640. The glass optical fiber 610A includes two cores 611 and 612 extending along the optical fiber axis AX, a cladding 620, and a marker 630. However, in the MCF600A involved in the comparative example, the cladding 620 in the glass optical fiber 610A has a single structure. In addition, Figure 3The MCF600B involved in the comparative example shown in the lower part of is a 4-core MCF. The MCF600B includes a glass optical fiber 610B and a resin coating 640. The glass optical fiber 610B includes four cores 611, 612, 613, 614 extending along the optical fiber axis AX, a cladding 620, and a marker 630. The MCF600B involved in this comparative example is also the same as the MCF600A, and the cladding 620 in the glass optical fiber 610B has a single structure.

[0040] on the other hand, Figure 3 The MCF100A according to the present embodiment shown in the upper part of Figure 1 The upper part and Figure 2 The MCF100 shown in the upper part is a 2-core MCF. Figure 1 The upper part and Figure 2 The glass optical fiber 110 shown in the upper part of the glass optical fiber 110 is a glass optical fiber 110A and a resin coating 140. The glass optical fiber 110A includes two cores 111 and 112 extending along the optical fiber axis AX, a cladding 120, and a marker 130. In the MCF100A, the cladding 120 in the glass optical fiber 110A has a double cladding structure, which is composed of an inner cladding 121 and an outer cladding 122. The inner cladding 121 surrounds the two cores 111 and 112 and the marker 130, and the outer cladding 122 is provided on the outer peripheral surface of the inner cladding 121 and has a higher refractive index than the inner cladding 121. In addition, Figure 3 The MCF100B shown in the lower part of the present embodiment is a 4-core MCF. The MCF100B includes a glass optical fiber 110B and a resin coating 140. The glass optical fiber 110B includes four cores 111, 112, 113, and 114 extending along the optical fiber axis AX, a cladding 120, and a marker 130. The MCF100B is also the same as the MCF100A, and the cladding 120 in the glass optical fiber 110B has a double cladding structure.

[0041] The MCF600A and 600B involved in the comparative example both have a cladding 620 of a single structure. Therefore, when the end face of the MCF is observed by side lighting, the brightness of the two cores 611 and 612 and the mark 630 in the cross section also changes according to the incident direction of the observation light LL, resulting in a situation where the core identification becomes difficult. It should be noted that such an undesirable situation may also occur in the case of the comparative example having four cores 611, 612, 613, and 614. On the other hand, according to the MCF100A and 100B involved in this embodiment, after the observation light LL is incident on the glass optical fiber 110A and 110B, it leaks into the inner cladding 121 while propagating in the outer cladding 122 and reaches the back side of the glass optical fiber 110A and 110B. As a result, since the observation light LL is evenly dispersed and / or evenly diffused in the outer cladding 122 and then coupled to the two cores 111, 112 and the mark 130, the light amount of the observation light LL coupled to the two cores 111, 112 and the mark 130 is stable regardless of the incident direction of the observation light LL. Such an effect can also be obtained in the present embodiment having four cores 111, 112, 113, 114.

[0042] Description of Reference Numerals

[0043] 100, 100A, 100B: MCF

[0044] 110, 110A, 110B: Glass optical fiber

[0045] 111, 112, 113, 114: core

[0046] 120: Cladding

[0047] 121: Inner cladding

[0048] 122: Outer cladding

[0049] 130: Mark

[0050] 140: Resin coating

[0051] 150: Refractive index distribution

[0052] 501: Light source

[0053] 502: Mirror element

[0054] 503: Camera

[0055] AX: Fiber Axis

[0056] L: Line

[0057] LL: Observe the light.

Claims

1. A multi-core optical fiber having: A glass optical fiber including a plurality of cores extending along a central axis, respectively, a marker extending along the plurality of cores, and a cladding surrounding the plurality of cores and the marker; and A resin coating is provided on the outer peripheral surface of the glass optical fiber, In a cross section of the multi-core optical fiber orthogonal to the central axis, the arrangement of the centers of the plurality of cores and the center of the mark has no rotational symmetry with respect to the center of the cross section, The cladding includes an inner cladding surrounding the plurality of cores and the mark and an outer cladding provided on an outer peripheral surface of the inner cladding and having a refractive index higher than that of the inner cladding.

2. The multi-core optical fiber according to claim 1, wherein: In the cross section of the multi-core optical fiber, a ratio B / A of a radius B of the inner cladding to a radius A of the outer cladding is not less than 1 / 3 and not more than 2 / 3.

3. The multi-core optical fiber according to claim 1 or 2, wherein: An absolute value of a relative refractive index difference of the inner cladding layer with respect to a refractive index of the outer cladding layer is 0.02% or more and 0.3% or less.

4. The multi-core optical fiber according to any one of claims 1 to 3, wherein: The arrangement of the centers of the plurality of cores has rotational symmetry with respect to the center of the cross section.