Conformal film for shoemaking, press machine and method for manufacturing footwear product by using conformal film

Through the multi-directional compression force of the conformal film, the problem of sole deformation caused by traditional presses is solved, the stable combination of sole and upper is achieved, and the joint quality and material utilization are improved.

CN119014645APending Publication Date: 2024-11-26NIKE INNOVATE CV
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411109337.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2017-11-22
Filing Date
2018-11-16
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

When traditional presses join the sole with the lasted upper, it is easy to cause unexpected deformation of the sole, resulting in insufficient combination of the sole and the upper. In addition, traditional presses cannot fully conform to surround the lasted upper and sole, resulting in unstable engagement.

Method used

A conformal film is used to assist in joining the upper and sole through the multi-directional compression force of its peripheral part, transition part and conformal part, providing a suitable pressure difference to ensure a stable combination of the sole and the upper and avoid deformation of the sole.

Benefits of technology

It effectively avoids unexpected deformation of the sole, ensures the full integration of the sole and the upper, improves the stability and quality of the joint, and reduces the use and production costs of materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119014645A_ABST
    Figure CN119014645A_ABST
Patent Text Reader

Abstract

The invention provides a conformal film for shoemaking, a press machine and a method for manufacturing a shoe product by using the conformal film. A low pressure operated conformal film for making an article of footwear includes a peripheral portion having a thickness in the range of 1 mm to 15 mm and forming an outer periphery of the conformal film. The conformal film also includes a transition having a thickness in the range of 1 mm to 4 mm between the first surface and the second surface, where the transition extends inward of the outer periphery. The conformal film also includes a conformal portion extending from the transition portion in a direction of the second surface and forming a receiving cavity, the conformal portion having a thickness in a range of 1 mm to 4 mm. The peripheral portion, the transition portion, and the conformal portion are in a unified configuration comprising a common material composition.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of an application with a filing date of November 16, 2018, application number 202210138736.X, and invention name “Conformal film, press for shoemaking, and method for manufacturing footwear using conformal film”.

[0002] The application with the application date of November 16, 2018, the application number is 202210138736.X, and the invention name is “Conformal film for shoemaking, press and method for manufacturing footwear products using conformal film” is a divisional application of the application with the application date of November 16, 2018, the application number is 201880075475.3, and the invention name is “Conformal film for shoemaking, press and method for manufacturing footwear products using conformal film” (formerly known as “Conformal film for shoemaking”). Technical Field

[0003] The invention relates to a conformal film for making shoes, a press machine and a method for making shoes using the conformal film. Background Art

[0004] Conventionally, footwear can be manufactured by bonding a sole to a lasted upper portion. Pressure, temperature and / or time are adjusted to achieve the bond between the sole and the lasted upper. The application of pressure can be achieved by a press that effectively assists in supplying a compressive force between the sole and the lasted upper as an adhesive or other bonding material bonds the sole to the lasted upper. Summary of the invention

[0005] Embodiments herein contemplate a conformal film for assisting in joining a first article to a second article. The conformal film includes a peripheral portion having a thickness in the range of 1 mm to 15 mm ("mm") and forming an outer periphery of the conformal film. The conformal film also includes a transition portion having a thickness in the range of 1 mm to 4 mm between a first surface and a second surface. The transition portion extends inwardly of the outer periphery formed by the peripheral portion. The conformal film also includes a conformal portion extending upwardly from the transition portion in the direction of the second surface and forming a receiving cavity. The conformal portion has a thickness in the range of 1 mm to 4 mm. The peripheral portion, the transition portion, and the conformal portion are a unitary structure comprising a common material composition.

[0006] This summary is provided for the purpose of teaching but not for the purpose of limiting the scope of the methods and systems which are provided in full detail below. BRIEF DESCRIPTION OF THE DRAWINGS

[0007] The invention is described in detail herein with reference to the accompanying drawings, in which:

[0008] Figure 1 A press with a conformal membrane according to embodiments herein is shown.

[0009] Figure 2 Shown in a closed and fixed configuration according to embodiments herein Figure 1 The press shown.

[0010] Figure 3 According to the embodiment of this article, along Figure 2 A cross-sectional view of the press machine taken along cutting line 3-3.

[0011] Figure 4 A perspective view of a conformal film according to embodiments herein is shown.

[0012] Figure 5 According to the embodiments herein, Figure 4 A side view of the conformal film is shown.

[0013] Figure 6 According to the embodiments herein, Figure 4 Front view of the conformal film shown.

[0014] Figure 7 According to the embodiments herein, Figure 4 Plan view of the conformal film shown.

[0015] Figure 8 According to the embodiment of this article, along Figure 4 A cross-sectional view of the conformal film taken along the cutting line 8-8.

[0016] Fig. 9 A flow chart illustrating an exemplary method of manufacturing an article of footwear with a conformal film according to embodiments herein is shown.

[0017] Description of Figure Numbers

[0018] 100: press;

[0019] 102: fixing element;

[0020] 104: membrane chamber;

[0021] 106: Stressors;

[0022] 108: temperature source;

[0023] 110: Time control;

[0024] 112: Pressure control;

[0025] 114: membrane fixing member;

[0026] 116: Membrane container;

[0027] 200: conformal film;

[0028] 202: conformal film first surface;

[0029] 204: conformal film second surface;

[0030] 206: longitudinal direction;

[0031] 208: longitudinal length;

[0032] 209: receiving cavity length;

[0033] 210: horizontal direction;

[0034] 212: horizontal width;

[0035] 214: peripheral part;

[0036] 216: Peripheral thickness;

[0037] 218: first surface of the peripheral portion;

[0038] 220: second surface of the peripheral portion;

[0039] 222: outer perimeter;

[0040] 224: Transitional Department;

[0041] 226: Transition thickness;

[0042] 228: first surface of transition portion;

[0043] 230: second surface of transition portion;

[0044] 232: internal direction;

[0045] 234: Conformal Department;

[0046] 235: first surface of the conformal portion;

[0047] 236: Z direction;

[0048] 237: second surface of the conformal portion;

[0049] 238: receiving cavity;

[0050] 240: first half of the receiving cavity;

[0051] 242: Width of the first half of the receiving cavity;

[0052] 244: second half of the receiving cavity;

[0053] 246: Receiver second half width;

[0054] 248: conformal thickness;

[0055] 250: sole;

[0056] 252: Upper;

[0057] 254: toe tip;

[0058] 256: Follow end. DETAILED DESCRIPTION

[0059] The manufacture of shoes such as sports shoes is traditionally carried out by joining different parts. For example, the upper is a part of the footwear that extends around the wearer's foot to fix the footwear to the wearer. The upper can be formed of various materials, such as leather, membranes, textiles, printed materials, etc. In some examples, the upper is a part of the shoe that includes a fixing structure (e.g., a lacing hole for the shoelace), an ankle opening that allows the wearer's foot to be put on and taken off, and other structures. The shape of the upper is determined in part when it is joined with other parts. In some manufacturing situations, a cobblers last (also known as a "last") is embedded in the upper (or the upper is formed around the last) so that the upper obtains the shape of the last. When the upper is placed on the last or otherwise formed around the last, this combination is often referred to as a "lasted upper". A lasted upper is an upper with a last, which is used to provide support and size guidance to the upper during the manufacturing process. As additional parts / components are engaged with the lasted upper, the shape of the upper becomes more stable so that once the last is removed, the size and shape of the upper is maintained or at least influenced by the last.

[0060] Another common component of footwear is the sole. In some examples, the sole may be referred to as a "bottom unit." The sole may be a collection of multiple components (e.g., an outsole, a midsole, and / or an insole). Additional components may also be incorporated, such as cushioning elements (e.g., springs), stabilizing elements (e.g., torsion bars), etc. that combine to form the sole. The sole is traditionally the portion that extends between the upper and the underlying ground and on which the wearer of the shoe moves.

[0061] The sole may be formed of a variety of materials. For example, the sole may be formed of leather, felt, textiles, and / or polymer-based materials (e.g., natural or synthetic). Different portions of the sole may be formed of different materials. For example, the outsole (e.g., the ground contacting portion) may be formed of rubber (e.g., synthetic or natural), and the midsole may be formed of a foamed polymer (e.g., ethylene-vinyl acetate (EVA), polyurethane (PU)). As will be discussed below, a conformal film may be suitable for assisting in joining an upper to a sole comprised of a foamed material (e.g., EVA or PU). Other foamed materials include, but are not limited to, low-density polyethylene, polyimide foam, polypropylene foam, polystyrene foam, polyvinyl chloride foam, silicone foam, and the like.

[0062] The upper is traditionally joined to the sole. In some examples, the upper is joined to the sole via a sewing operation. In another example, the upper is joined to the sole via a bonding process. The bonding process can be achieved by welding, melting and / or adhesive bonding. In an exemplary embodiment, an adhesive material (e.g., liquid, paste, film) is applied to at least one of the sole contact surface of the upper and / or the upper contact surface of the sole. The adhesive may be active or activated to facilitate the bonding between the upper and the sole (e.g., mechanical bonding and / or chemical bonding). The bonding may be enhanced by applying pressure (e.g., applying a force that passes through the upper to the sole and / or applying a force that passes through the sole to the upper). In addition to pressure, it is envisioned that heat energy (e.g., heat) may also be applied to the upper and / or the sole to assist in bonding the upper and the sole. In addition, it is envisioned that a prescribed period of time during which heat energy and / or pressure is applied to the upper and / or the sole will assist in achieving the bonding between the upper and the sole. As will be discussed below, the conformal film is effective to provide sufficient pressure at the desired location to assist in joining the upper and the sole, such as through the use of an adhesive or other bonding material.

[0063] However, in some conventional joining techniques, when used to join a compressible sole element (e.g., EVA, PU or other foamed polymer-based material) to a lasted upper, the application of pressure during the joining process can cause permanent and unintended deformation of the compressible sole and thus cause the compressible sole to deform in an unintended shape when joined to the upper. In other words, the lack of a conformable membrane provided herein in a conventional press can cause deformation of the sole, wherein the deformation is at least partially maintained after the upper is joined to the deformed sole. As previously noted, the construction of footwear can rely on the continuous layering and joining of multiple materials and multiple parts to maintain the shape of the upper defined by the last once the last is removed after the joining occurs. However, if a lasted upper is joined to a sole that has been deformed by a conventional press, the sole may (completely or partially) return to the original, undeformed shape of the sole once the last is removed after the sole and upper are joined. This return of the sole to its pre-deformation shape after engagement with the upper may cause the upper to deform relative to the shape of the upper defined by the last. Therefore, conventional presses that apply pressure to the sole to assist in engaging the sole and the upper may introduce deformation of the sole during the pressing operation, which results in unintended deformation of the sole and / or the upper after the pressing operation.

[0064] It should be understood that different sole materials may be more prone to unexpected permanent deformation. Therefore, conventional presses may produce acceptable results for some shoe material combinations. However, as materials advance and the application of a larger number of materials (e.g., foamed polymers) is used to form components of footwear, the advancement of presses enables these materials to be integrated into footwear. For example, when a conventional press is used to join a sole with a shoe last, a sole formed by certain materials produces an unsatisfactory combination (e.g., a bonding gap). When the extrusion from a conventional press applies the extrusion on the shoe last for a specified time (e.g., 30 seconds, 25 seconds) or more, the material will deform and result in insufficient bonding. In addition, a reduced force may be applied to compensate for the non-conformal nature of a conventional press. However, a reduction in force (or time) may result in insufficient bonding (e.g., incomplete bonding). Additionally, conventional presses may cause one or more portions (eg, a foamed sole portion) to visually deform due to linear application of force through the press, as opposed to the wraparound manner achieved by the embodiments of conformal films provided herein.

[0065] Thus, the embodiments provided herein are related to a conformal film for assisting in joining a first product and a second product. A conformal film is a film that conforms to a lasted upper and a sole so as to encapsulate the lasted upper and the sole with a compressive force perpendicular to multiple surfaces (e.g., the sole ground contact surface, the sole sidewall, the inner side of the upper, the outer side of the upper, the upper heel end, the upper, the toe cap). The multi-directional compressive force provided by the conformal film fixes the sole and the lasted upper for the bonding / joining process without deforming the foaming material (e.g., the sole). This is in contrast to conventional presses, which are unable to fully conform around the lasted upper and the sole and / or rely on higher pressures to facilitate conformality of the press. In contrast to the multi-directional compressive force provided by the conformal film, conventional presses concentrate pressure across the sole in a more linear manner. In addition, conventional presses that may have a "conformal" film can only be "conformed" at pressures significantly higher than the pressures provided in conjunction with the embodiments herein.

[0066] The conformal film includes a peripheral portion having a thickness in the range of 1 mm to 15 mm ("mm") and forming an outer periphery of the conformal film. In some embodiments, the peripheral portion has a thickness in the range of 5 mm to 15 mm, 8 mm to 12 mm, or about 10 mm in another example. The conformal film also includes a transition portion having a thickness in the range of 1 mm to 4 mm between the first surface and the second surface. The transition portion extends inwardly of the outer periphery formed by the peripheral portion. The conformal film also includes a conformal portion extending from the transition portion in the direction of the second surface and forming a receiving cavity. The conformal portion has a thickness in the range of 1 mm to 4 mm. The peripheral portion, the conformal portion, and the transition portion may have the same thickness or different thicknesses. The conformal portion and the transition portion may have the same thickness or different thicknesses. The peripheral portion, the transition portion, and the conformal portion are a unitary structure comprising a common material composition.

[0067] In addition, it is envisioned that a conformal film is implemented in the manufacture of footwear, such that a method for manufacturing footwear using a conformal film for joining a sole and an upper includes positioning the upper on a fixing element (e.g., an extruded support). The method includes sealing the conformal film on the upper and the sole located on the fixing element. In this example, the first surface of the conformal film contacts the sole and the upper. The conformal film may be a conformal film described in the previous paragraph or any derivative provided herein. The method continues with the following steps: reducing the pressure difference after a predetermined time period (e.g., greater than 25 seconds, greater than 30 seconds, greater than 35 seconds). In an exemplary embodiment, the pressure difference may be in the range of 0.5 bar to 3.9 bar (i.e., 50 kPa to 390 kPa).

[0068] Conformal films and contemplated methods of use provide a means to join an upper and a sole in a manner that causes less deformation of the upper and / or the sole relative to conventional presses (e.g., film presses). In some instances, the properties of the conformal film (e.g., thickness and material composition) enable the film to conform around the sole and upper portion to apply pressure (and in some instances, heat) across multiple surfaces (e.g., toe cap, heel counter, inner side of the upper, outer side of the upper, across the transition from the sole to the upper (e.g., biteline), sidewall of the sole) during joining of the upper portion and the sole at relatively low pressures. This is in contrast to conventional press films of thicker or different material compositions, which apply a more linear force extending linearly through the sole and / or upper (as opposed to surrounding from multiple directions) at higher pressures (e.g., 4 bar or greater), thereby causing deformation of the sole and / or upper during the pressing operation.

[0069] With reference generally to the accompanying drawings and with reference specifically to Figure 1 , Figure 1 Shown is a press 100 that fixes a shoe upper 252 and a sole 250 with a last to a fixing element 102 according to an embodiment herein. Note that the press 100 is suitable for keeping the relative position of the upper and the sole while the upper and the sole are engaged. For example, adhesive can be applied (e.g., sprayed, brushed, rolled, applied, printed) to the sole, the upper, or the combination of the sole and the upper. In addition, it is envisioned that the upper 252 and / or the sole 250 can be formed by one or more materials (e.g., hot melt adhesive, fusible polymer) that can be engaged with other components under pressure and / or heat. The sole 250 and the upper 252 then have the pressure applied by the conformal film 200 contained in the film container 116 (e.g., lid). Because the film container 116 is positioned above the sole 250 and the upper 252, the combination of the components is at least partially received in the receiving cavity 238 of the conformal film 200. The receiving cavity is intentionally deformed (e.g., molded or otherwise formed) from the planar configuration of the conformal film 200 so that multiple surfaces of the shoe to be formed (e.g., medial side, lateral side, toe cap at toe end 254, heel counter at heel end 256, bite line) are contacted by the conformal film 200 during the pressing operation. The film container 116 can be secured to the press 100 in a closed, operative arrangement by a film fastener 114 (e.g., a releasable latching mechanism). The film fastener 114 effectively holds the film container 116 and the associated conformal film 200 in position relative to the footwear to which pressure is applied.

[0070] With respect to pressure, it is contemplated that pressure may be applied to the sole 250 and the upper 252 by the press 100 in one or more ways. For example, the fixing element 102 may effectively apply a linear force, such as by a cylinder, a linear actuator, etc. This linear force is applied via the last 120 (such as in Figure 3 The conformal membrane 200 in contact with the upper 252 and / or the sole 250 encounters resistance to the linear force. Additionally or alternatively, it is contemplated that the fixing element 102 is effective to adjust the position of the upper 252 and the sole 250 in the receiving cavity 238. For example, the fixing element 102 may be raised or lowered (see the diagram shown) based on expected pressure, component size, component shape, etc. Figure 1 The fixing element 102 may be stationary and non-movable in some embodiments.

[0071] The pressure may alternatively or additionally be generated by the press 100 through the pressurization of the conformal film 200. Figure 3In an exemplary embodiment of the present invention, a positive pressure relative to ambient pressure can be introduced into the volume enclosed by the film container 116 and the conformal film 200. The increased pressure forms a pressure difference on the opposite surfaces of the conformal film 200. Since the conformal film 200 deforms under the pressure difference, the pressure difference causes the conformal film 200 to conform around the upper 252 and the sole 250. It is this deformation that causes the conformal film 200 to wrap around some parts of the upper 252 and the sole 250, thereby generating a pressure that keeps the upper 252 and the sole 250 in a fixed relative position during the joining operation. Depending on the pressure difference, sufficient pressure can be applied to the upper 252 and the sole 250 to assist in joining (e.g., bonding via adhesive curing) these components. Exemplary pressure differences include 0.5 bar to up to 3.9 bar relative to ambient pressure. In an exemplary embodiment, above 3.9 bar, the conformal film may fail mechanically after a certain number of extrusion cycles or the extruded article may deform unexpectedly and permanently during the extrusion operation. Although it is envisioned that the pressure difference is higher than 0.5 bar and lower than 3.9 bar, the embodiments herein are implemented at a pressure difference within the provided range to reduce the unexpected deformation of the extruded product. The low-conformal film of the conventional press can be operated at a pressure difference of 4 bar or higher than 4 bar to conform and comply with the extruded product. This increased pressure can make the conventional die-casting conformal, but it can damage the extruded product (such as a part of a shoe product) or otherwise cause the extruded product to have unexpected deformation. Therefore, compared to conventional die-casting, the implementation of the conformal film provided herein operates at a lower pressure difference to achieve conformal between the film and the extruded product. In additional embodiments, the pressure difference is expressed as atmospheric pressure and is within the range of 1 to 3 bar, 1 to 2 bar, 1 to 1.5 bar, 1 to 1.3 bar, 1 to 1.2 bar, 1.1 to 1.4 bar and / or 1.25 to 1.35 bar. Various pressure difference conditions are selected based on the material to be combined, the extrusion time, the conformality of the film, etc. to provide flexibility. Thus, based on the factors contemplated herein, various pressure differential ranges may be applied to achieve bonding of the shoe components while minimizing unintended, permanent deformation of the shoe components.

[0072] Figure 2A press 100 having a film container 116 in a closed and fixed setting is shown according to an embodiment herein. The closed setting is a configuration that enables the press 100 to effectively apply pressure to the shoe assembly during the bonding operation. An input mechanism of the press 100 is also shown. A time control 110, a pressure control 112, and a temperature control 118 are shown. The input mechanism enables the user to adjust the parameters of the same name (e.g., time, temperature, pressure). However, it is envisioned that one or more of the input mechanisms are omitted or changed in exemplary embodiments. For example, a computer instruction may be transmitted to the press from a controller, and the controller controls the time, pressure, and / or temperature applied to a specific (or general) component. In addition, it is envisioned that one or more of the time, temperature, or pressure may not be adjusted in some instances.

[0073] Figure 3 According to the embodiment of this article, along Figure 2 A toe-to-heel perspective view is provided to show the fixing element 102 holding the last 120 in a certain position so that the upper 252 and the sole 250 can be contacted by the conformal membrane 200. Figure 3The conformal membrane 200 is shown during a pressure differential that causes the conformal membrane 200 to conform to the lasted upper 252 and the sole 250. The pressure source 106 provides an exemplary pressure source to form a pressure differential. The pressure source can provide a compressible or incompressible material (e.g., gas or liquid) from an external source (e.g., a tank, a pump, and a compressor) to the membrane chamber 104. The membrane chamber 104 is surrounded and formed by the membrane container 116 and the conformal membrane 200. The membrane chamber 104 effectively receives a pressurized material (e.g., a pressurized gas) and provides a certain volume for the pressurized material to surround some portions of the conformal membrane 200 from within the conformal membrane 200 and apply force to the portions. The pressure can be controlled using one or more mechanisms (e.g., a regulator, etc.). Unlike conventional die-casting that operates at 4 bar and above, the embodiments herein contemplate operating at lower pressures (e.g., 0.5 bar to 3.9 bar), and thus conventional macro-level control of pressure may result in unexpected permanent deformation of the extruded article, because the macro-level control (e.g., analog regulators with a tolerance of 1 bar or greater) has a large tolerance for the operation of pressure. This large tolerance will result in a greater pressure difference at the conformal film provided herein, resulting in unexpected permanent deformation of the extruded article. Therefore, in exemplary embodiments, such macro-level control of pressures with a pressure difference of 4 bar or greater than 4 bar cannot effectively control a pressure difference in the range of 0.5 bar to 3.9 bar. In addition, in exemplary embodiments, such macro-level control of pressures with a pressure difference of 4 bar or greater than 4 bar cannot effectively control a pressure difference in the range of 1 bar to 2 bar. Therefore, the embodiments herein contemplate upgrading the pressure control mechanism to a micro-level control (e.g., a digital regulator with a tolerance of 0.9 bar or less), which is capable of maintaining the pressure differential within a tighter tolerance than the pressure mechanism of a conventional press. Control of the increased pressure tolerance can provide better durability of the conformal film (e.g., a reduction in pressurization potential) and allow for more consistent operation at the lower pressures provided herein. In other words, in the exemplary embodiments herein, since the embodiments herein contemplate operating at a lower pressure differential than a standard press, greater control of the pressure differential will gain results from the conformal film press.

[0074] exist Figure 3Optional heating source 108 is also shown in the figure. Heating source 108 can be a resistive heating element, an infrared heating element, an inductive heating element, etc. As another option, in some embodiments, it is envisioned that the pressurized material can be heated outside the film chamber 104 and introduced at a temperature higher (or lower) than the ambient conditions. Heat can be used to activate, melt or solidify one or more materials (e.g., bonding materials). For example, a low melting point adhesive having a deformation temperature (e.g., melting temperature) lower than that of the film, the upper and the sole can be placed between the upper and the sole. Before or after conforming the conformal film 200 around some parts of the sole and the upper, heat can be generated or applied to activate the low melting point adhesive. Then, the heat energy can be reduced while maintaining the pressure from the conformal film 200 until the low melting point adhesive (or any bonding material) has sufficient bonding between the components. It is envisioned that the heating source 108 is optional and can be omitted in the embodiments envisioned herein.

[0075] Figure 3 The three regions of the conformal film 200 are described below. Figures 4 to 8 The peripheral portion 214, the transition portion 224, and the conformal portion 234 are discussed in more detail in FIG. Figure 3 As shown in , conformal membrane 200 surrounds and encircles upper 252 and portions of sole 250 on multiple surfaces and from multiple directions. It is this conformality with multiple surfaces and components that enables conformal membrane 200 to effectively bond upper 252 to sole 250.

[0076] As previously provided, the low conformal (or non-conformal) film of the conventional press, on the contrary, permanently deforms the sole 250 (e.g., compresses the foam material) during the pressing operation because it cannot fully conform and therefore applies more concentrated and unidirectional pressure to the sole. The permanent deformation of the unacceptable pressed portion may also be caused by the fact that the conventional press film is operated at higher pressures (e.g., 4 bar and above) to achieve a certain degree of conformality between the conventional press film and the pressed component. The use of higher pressure differentials on the conventional press machine compensates for the low conformal film material, which translates into potential destructive forces applied to the pressed article. If heat energy is applied to the process to activate or cure the bonding material, this unintended deformation can be further exaggerated. This increased heat energy can cause the material (e.g., PU, ​​EVA) forming the sole to become more compliant and therefore more susceptible to undesirable deformation under a certain pressure from the press. Thus, by wrapping the compliant film around the various surfaces of the components to be joined from multiple directions, the pressure of the press is applied across a larger surface area at more directional angles, allowing the same materials that may unexpectedly deform under traditional films to be effectively joined with conformal film 200.

[0077] Figure 4A stereogram of a conformal film 200 is shown according to an embodiment herein. For reference purposes, a longitudinal direction 206 and a lateral direction 210 are generally shown. As contemplated, a conformal film is used in conjunction with a footwear article, the conformal film having a receiving cavity formed into a shape similar to the intended receiving portion of the footwear article. This usual and expected deformation is placed under a certain pressure differential, limiting creases or other film deviations to form a compliant conformal with the underlying footwear component. In other words, in some instances, the receiving cavity has a similar shape to the article to which it is expected to conform under a certain pressure differential. This coordination between the receiving cavity shape and the footwear article allows the film to have a more consistent conformal with the component to be joined under a certain pressure differential.

[0078] exist Figure 4 200, the perimeter portion 214, the transition portion 224, and the conformal portion 234 are shown. In addition, the outer perimeter 222 is shown as forming the outermost portion of the conformal film 200. The conformal film second surface 204 is also shown. The conformal film second surface 204 is opposite to the conformal film first surface 202, as shown in FIG. Figure 8 Best visible in.

[0079] Figure 5 A side view of conformal film 200 is shown according to embodiments herein. A z-direction 236 is shown. Z-direction 236 is the direction in which conformal portion 234 extends from transition portion 224. Figure 6 A front view of a conformal film 200 is shown, according to embodiments herein.

[0080] Figure 7 According to the embodiments herein, Figures 4 to 6 A plan view of the conformal film 200 is shown. Figure 7 206. For example, a receiving cavity first half section 240 and a receiving cavity second half section 244 are shown along the longitudinal direction 206. In addition, a series of arrow indicators 232 are shown to show the "inside" direction relative to the outer periphery 222 in the plan view plane of the conformal film 200.

[0081] Conformal portion 234 includes receiving cavity 238. Receiving cavity first half section 240 has a maximum width 242, and receiving cavity second half section 244 has an exemplary width 246. The width of the receiving cavity portion is measured in lateral direction 210. In this example, since the receiving cavity is shaped to conform to the article of footwear, maximum width 242 of receiving cavity first half section 240 is greater than any width (e.g., width 246) of receiving cavity second half section 244. It is contemplated that the receiving cavity may have any shape depending on the article to be compressed by the conformal film.

[0082] The conformal film 200 has a length 208 measured from the outer perimeter 222 in the longitudinal direction 206. The conformal film 200 has a width 212 measured from the outer perimeter 222 in the transverse direction 210. In an exemplary embodiment, it is contemplated that the length 208 is in the range of 400 mm to 500 mm. In an exemplary embodiment, it is contemplated that the length 208 is in the range of 425 mm to 475 mm. In an exemplary embodiment, it is contemplated that the length 208 is in the range of 450 mm to 465 mm. In an exemplary embodiment, it is contemplated that the width 212 is in the range of 200 mm to 300 mm. In an exemplary embodiment, it is contemplated that the width 212 is in the range of 210 mm to 250 mm. In an exemplary embodiment, it is contemplated that the width 212 is in the range of 220 mm to 240 mm. In view of the exemplary ranges provided, it is contemplated that the outer perimeter 222 may define a planar surface area of ​​0.08 square meters to 0.15 square meters. This area enables sufficient conformal film material to conform to the component to be compressed while minimizing the material and weight associated with conformal film 200. The length and width may depend on the style, size, or type of article to be compressed by conformal film 200.

[0083] In addition, conformal portion 234 has a maximum length 209. In an exemplary embodiment, it is envisioned that length 209 is in the range of 350 mm to 450 mm. In an exemplary embodiment, it is envisioned that length 209 is in the range of 375 mm to 425 mm. In an exemplary embodiment, it is envisioned that length 209 is in the range of 395 mm to 415 mm. In an exemplary embodiment, it is envisioned that maximum width 242 is in the range of 150 mm to 250 mm. In an exemplary embodiment, it is envisioned that maximum width 242 is in the range of 175 mm to 225 mm. In an exemplary embodiment, it is envisioned that maximum width 242 is in the range of 190 mm to 210 mm. In an exemplary embodiment, the length 209 and width 242 of the receiving cavity are selected to provide a receiving cavity of sufficient size for the component to be received therein while limiting excess conformal film material. For example, the length and width of receiving cavity 238 may be 1% to 10% larger than similar measurements of the component to be received therein to achieve easy insertion and removal without introducing unintended deformation when the film conforms to the underlying component.

[0084] Figure 8 According to the embodiment of this article, along Figure 48 is a cross-section of the conformal film 200 of FIG. 2. The perimeter portion 214 has a perimeter portion first surface 218 and a perimeter portion second surface 220, with a thickness 216 defined therebetween. The transition portion 224 has a transition portion first surface 228 and a transition portion second surface 230, with a thickness 226 defined therebetween. The conformal portion 234 has a conformal portion first surface 235 and a conformal portion second surface 237, with a thickness 248 defined therebetween.

[0085] The thickness of the conformal portion 234, the transition portion 224, and the peripheral portion 214 affects the ability of the conformal film 200 to conform to the product under a certain pressure difference. The historical film in the historical press may have a greater thickness in various parts. Traditionally, a greater thickness may have been implemented to enable the material forming the traditional film to have a longer life during industrial applications. However, the conformal film 200 can operate under different conditions (e.g., temperature, pressure, time) to bond and / or form more compliant parts from different materials, and therefore may have a thinner (e.g., smaller) thickness than the traditional film. In some examples, as the thickness of a portion of the conformal film decreases, the conformal film may become more compliant and can conform to the underlying product. However, if the thickness is reduced too much, the conformal film may be subject to fatigue and failure in actual industrial applications. Therefore, in an exemplary embodiment, it is envisioned that various thickness ranges are provided to provide sufficient compliance to the conformal film 200 while achieving sufficient service life.

[0086] According to embodiments herein, it is contemplated that the perimeter thickness 216 is in the range of 1 mm to 15 mm. According to embodiments herein, it is contemplated that the perimeter thickness 216 is in the range of 5 mm to 15 mm. According to embodiments herein, it is contemplated that the perimeter thickness 216 is in the range of 8 mm to 12 mm. According to embodiments herein, it is contemplated that the perimeter thickness 216 is about 10 mm. According to embodiments herein, it is contemplated that the transition thickness 226 is in the range of 1 mm to 4 mm. According to embodiments herein, it is contemplated that the transition thickness 226 is about 2 mm. According to embodiments herein, it is contemplated that the conformal thickness 248 is in the range of 1 mm to 4 mm. According to embodiments herein, it is contemplated that the conformal thickness 248 is about 2 mm. In an exemplary embodiment, the perimeter thickness 216, the transition thickness 226, and the conformal thickness 248 may be the same. In an exemplary embodiment, the perimeter thickness 216, the transition thickness 226, and / or the conformal thickness 248 may be different.

[0087] In an exemplary embodiment, it is contemplated that the conformal portion 234 and the transition portion 224 have similar thicknesses. This common thickness may cause the transition portion 224 to similarly conform to the conformal portion 234 during a pressure differential, thereby preventing regions of greater elongation in the conformal portion 234. In some examples, the transition portion 224 completely borders or surrounds the conformal portion 234. In other words, the transition portion 224 provides a functional transition extending in the z-direction between the peripheral portion 214 and the conformal portion 234. By surrounding the conformal portion 234, the transition portion 224 enables the conformal portion 234 to conform to a received article even at the outermost portions of the conformal portion 234.

[0088] In an exemplary embodiment, the peripheral portion thickness 216 may be greater than the transition portion thickness 226 to increase life, service life, and concentration of compression energy around the received article. Since the thickness of the conformal film affects functional properties (e.g., elongation), the conformal film 200 is more susceptible to deformation due to pressure differentials at locations with less thickness (i.e., thinner areas). Therefore, by reducing the thickness of the conformal film 200 at the receiving cavity 238 and close to the article to be received, the conformal film 200 is more conformal around the received article than at the peripheral portion 214 with a greater thickness. In an exemplary embodiment, since the peripheral portion 214 has a greater thickness and thus has less conformality, the peripheral portion 214 is less susceptible to fatigue failure due to repeated conformality during pressure differential cycles.

[0089] Figure 8 The extension height 258 of the conformal portion 234 from the transition portion 224 is shown. According to embodiments herein, the height 258 is in the range of 70 mm to 110 mm. According to embodiments herein, the height 258 is in the range of 80 mm to 100 mm. According to embodiments herein, the height 258 is about 90 mm (e.g., within 10%). Conventional membranes may have a height significantly less than the conformal membrane 200. In these examples, the smaller height inhibits the membrane from surrounding multiple surfaces of the article, and thus materials that are prone to deformation under the directional compression of the conventional membrane (e.g., the foamed polymer of the sole) may deform. The conformal membrane 200 having a greater height than the conventional membrane is instead allowed to surround the sole and at least a portion of the upper, thereby encapsulating the article with a unified pressure rather than a directional pressure (e.g., from the membrane linearly toward the fixing element).

[0090] In an exemplary embodiment, the perimeter portion first surface 218 and the perimeter portion second surface 220 are positioned above the transition portion second surface 230. In addition, since the conformal portion 234 extends (e.g., Figure 8222), and thus in the exemplary embodiment it is contemplated that the perimeter portion first surface 218 and the perimeter portion second surface 220 are positioned on the same side of the transition portion second surface 230. This offset between the perimeter portion 214 and the transition portion 224 enables the conformal film 200 to be more conformal around the received article in the inner direction relative to the outer perimeter 222. In other words, in the exemplary embodiment, as a pressure differential is applied, the offset in the vertical placement of the perimeter portion 214 and the transition portion 224 enables a transfer of vertical placement to horizontal conformality.

[0091] The conformal film 200 is formed of a conformal material. In one embodiment, the conformal film is formed of a material composition comprising rubber (e.g., natural rubber), silicon dioxide (i.e., silica), and calcium carbide. Additional materials may be included in the composition. In an exemplary embodiment, the material composition of the conformal film 200 is composed of 75% to 85% rubber by weight and 5% to 15% silicon dioxide by weight. In an exemplary embodiment, the material composition of the conformal film 200 is composed of 5% to 15% calcium carbide by weight and 5% to 15% silicon dioxide by weight. In an exemplary embodiment, the material composition of the conformal film 200 is composed of 8% to 12% dispersible silica by weight. In an exemplary embodiment, the material composition of the conformal film 200 is composed of 75% to 85% rubber by volume and 5% to 15% silicon dioxide by volume. In an exemplary embodiment, the material composition of conformal film 200 is composed of 5% to 15% by volume calcium carbide and 5% to 15% by volume silicon dioxide. In an exemplary embodiment, the material composition of conformal film 200 is composed of 8% to 12% by volume dispersible silica. In an exemplary embodiment, the percentages of the composition are determined prior to combination.

[0092] Conformal film is envisioned to be a unitary material extending between two or more parts. For example, it is envisioned that conformal portion 234 and transition portion 224 are formed of the same material, such that the composition of the materials forming the parts is homogenous. Similarly, it is envisioned that peripheral portion 214, transition portion 224, and conformal portion 234 are unitary and formed of a common material. A unitary construction is a single entity having a uniform material composition. For example, two or more parts of a conformal film can be generated simultaneously. In an example, a molding operation that combines to form two or more parts can be performed. In an alternative manufacturing process, it is envisioned that a common material is subtractively formed (e.g., ground) to form a conformal film. In this example, the parts formed by subtraction are unitary because the parts all start from a common source material without subsequent joining.

[0093] The functional properties of the conformal film 200 can be quantified to provide a conformal film range suitable for the exemplary embodiments herein. For example, according to the embodiments herein, the conformal film 200 at least in the conformal portion 234 can have a hardness of 60 to 61 Asker C when measured on an ASKER C-type durometer. According to the embodiments herein, the conformal film 200 at least in the conformal portion 234 can have a maximum tensile strength in the range of 84 kilograms per cubic centimeter (kg / cm3) to 90 kilograms per cubic centimeter. The maximum tensile strength can be tested using test protocols such as ASTM D638-14. According to the embodiments herein, the conformal film 200 at least in the conformal portion 234 can have a maximum elongation of at least 540% until it is destroyed. The maximum elongation can be tested using tests such as ASTM D-638 test protocols.

[0094] In an exemplary embodiment, the material composition of the conformal film 200 and the resulting functional properties provide a suitable material as a film to join two or more shoe parts without deforming or damaging the foamed polymer component (e.g., EVA or PU midsole element). The material composition provided herein for the conformal film 200 can save labor, cost and / or material. For example, operating at a lower pressure than a conventional film press to achieve conformity of the film to the underlying extruded article reduces subsequent intervention to correct unintended deformation of the extruded material. In addition, energy savings are achieved by using a lower pressure requirement through the conformal film operating at a lower pressure. In addition, in an exemplary embodiment, operating the conformal film at a lower pressure with the envisioned material composition enables a thinner film to be achieved, which reduces the material used to form the film, which in turn reduces material costs.

[0095] Turn reference Fig. 9 , Fig. 9 A method 900 of manufacturing a footwear product using a conformal film to join a sole and an upper is shown according to an embodiment herein. At block 902, the upper is positioned on a fixing element. The upper may be a lasted upper, wherein the last is fixed to the fixing element. At block 904, a conformal film (e.g., conformal film 200 provided herein) is sealed over the upper and the sole. In this example, the upper and the sole are positioned in a desired relative position. Prior to joining the two components, an adhesive or other bonding material may be applied.

[0096] At block 906, a pressure differential is created between opposing surfaces of the conformal membrane. For example, a pressurized fluid (e.g., a gas or liquid) may be injected into the membrane cavity, where the conformal membrane is more compliant than other materials forming the membrane cavity. As a result, the membrane cavity deforms and conforms around the lasted upper and the sole, thereby generating a compressive force to secure the sole and the lasted upper. The compressive force is applied to both the upper and the sole at multiple surfaces, including the interface between the sole and the upper. This encapsulated compression holds the sole in a defined position relative to the upper during the bonding operation.

[0097] At block 908, after a predetermined time period, the pressure differential is reduced. This time period may be 20 seconds, 25 seconds, 30 seconds, or any time suitable to allow engagement of the sole with the upper.

[0098] Conceived but not yet Fig. 9 Other steps shown in include, but are not limited to, applying thermal energy, extracting thermal energy (eg, cooling), and adjusting time, pressure, and / or temperature.

[0099] Without departing from the spirit and scope of the present disclosure, many different arrangements of the various components shown and the various components not shown may be made. The embodiments of the present disclosure have been described for illustrative and non-restrictive purposes. Alternative embodiments that do not depart from the scope of the present disclosure will become apparent to those skilled in the art. Those skilled in the art may develop alternative means to implement the above improvements without departing from the scope of the present disclosure.

[0100] It should be understood that certain features and subcombinations are of utility and may be employed without reference to other features and subcombinations and are contemplated to be within the scope of the claims. Not all steps listed in the various figures need to be performed in the particular order described.

[0101] The term "any of the clauses" or similar variations of the term used herein in conjunction with the clauses listed below is intended to be interpreted so that features of the clauses can be combined in any combination. For example, exemplary clause 4 may indicate a method / apparatus as described in any of clauses 1 to 3, which is intended to be interpreted so that features of clauses 1 and 4 can be combined, elements of clauses 2 and 4 can be combined, elements of clauses 3 and 4 can be combined, elements of clauses 1, 2, and 4 can be combined, elements of clauses 2, 3, and 4 can be combined, elements of clauses 1, 2, 3, and 4 can be combined, and / or other variations. In addition, the term "any of the clauses" or similar variations of the term are intended to include "any of the clauses" or other variations of this term, as indicated by some of the examples provided above. In addition, it is contemplated that the clauses may be drafted as embodiments claimed herein.

[0102] Example clauses

[0103] 1. A conformal film for assisting in joining a first product and a second product, the conformal film comprising: a peripheral portion having a thickness in a range of 1 mm to 15 mm, forming an outer periphery of the conformal film; a transition portion having a thickness in a range of 1 mm to 4 mm between a first surface and a second surface, wherein the transition portion extends inwardly of the outer periphery formed by the peripheral portion; and a conformal portion extending from the transition portion in a direction of the second surface and forming a receiving cavity, the conformal portion having a thickness in a range of 1 mm to 4 mm, wherein the peripheral portion, the transition portion and the conformal portion are a unitary structure composed of a common material.

[0104] 2. The conformal film of clause 1, wherein the first article is a foamed polymer-based article.

[0105] 3. The conformal film of clause 2, wherein the first article is a shoe midsole and the second article is a shoe upper.

[0106] 4. The conformal film of any one of clauses 1 to 3, wherein the perimeter portion further comprises a first surface and a second surface, both of the perimeter portion first surface and the perimeter portion second surface being positioned on the same side of the transition second surface as the conformal portion.

[0107] 5. A conformal film as described in any one of clauses 1 to 4, wherein the peripheral portion has a thickness in the range of 8 mm to 12 mm.

[0108] 6. The conformal film of any one of clauses 1 to 5, wherein the outer perimeter defines a plan area of ​​0.08 square meters to 0.15 square meters.

[0109] 7. A conformal film as described in any one of clauses 1 to 6, wherein the outer perimeter has a longitudinal length in the range of 400 mm to 500 mm and a transverse length in the range of 200 mm to 300 mm.

[0110] 8. A conformal film as described in any of clauses 1 to 7, wherein the transition portion completely interfaces with the conformal portion and joins the conformal portion and the peripheral portion.

[0111] 9. The conformal film of any one of clauses 1 to 8, wherein the conformal portion has a durometer hardness in the range of 60 Asker C to 61 Asker C.

[0112] 10. The conformal film of any one of clauses 1 to 9, wherein the conformal portion has a tensile strength in a range of 84 kg / cm3 to 90 kg / cm3.

[0113] 11. The conformal film of any one of clauses 1 to 10, wherein the conformal portion has a percent elongation of at least 540% elongation prior to failure of the conformal portion.

[0114] 12. The conformal film of any one of clauses 1 to 11, wherein the transition portion and the conformal portion have the same durometer hardness, tensile strength, or elongation.

[0115] 13. The conformal film of any one of clauses 1 to 12, wherein the conformal portion extends from the transition portion second surface in a range of 70 mm to 110 mm.

[0116] 14. A conformal film as described in any one of clauses 1 to 13, wherein the conformal portion extends within a range of 80 mm to 100 mm from the transition portion second surface.

[0117] 15. The conformal film of any one of clauses 1 to 14, wherein the receiving cavity has a width in a transverse direction at a first half section in the longitudinal direction that is greater than a width in the transverse direction at a second half section in the longitudinal direction.

[0118] 16. The conformal film of any one of clauses 1 to 15, wherein the conformal portion has a thickness of 2 millimeters.

[0119] 17. A conformal film as described in any one of clauses 1 to 16, wherein the material composition includes natural rubber, silicon dioxide and calcium carbide.

[0120] 18. A conformal film as described in any one of clauses 1 to 17, wherein the material composition consists of 75% to 85% rubber and 5% to 15% silica by weight.

[0121] 19. A conformal film as described in any one of clauses 1 to 18, wherein the material composition comprises 5% to 15% silicon dioxide and 5% to 15% calcium carbide by weight.

[0122] 20. The conformal film of any one of clauses 1 to 19, wherein the material composition comprises dispersible silica in the range of 8% to 12% by weight of the material composition.

[0123] 21. A press having a conformal film for assisting in joining a first article to a second article, the press comprising: a conformal film comprising: (1)

[0124] (1) a peripheral portion having a thickness in the range of 1 mm to 15 mm, forming the outer periphery of the conformal membrane; (2) a transition portion having a thickness in the range of 1 mm to 4 mm between the first surface and the second surface, wherein the transition portion extends inwardly of the outer periphery formed by the peripheral portion; and (3) a conformal portion extending from the transition portion in the direction of the second surface and forming a receiving cavity, the conformal portion having a thickness in the range of 1 mm to 4 mm, wherein the peripheral portion, the transition portion and the conformal portion are a unitary structure composed of a common material; and a pressure source coupled to the press fluid to control the pressure difference between the first surface of the transition portion and the second surface of the transition portion to 0.5 bar to 3.9 bar.

[0125] 22. A method for manufacturing a footwear product using a conformal film, wherein the conformal film is used to join a sole and an upper, the method comprising: positioning the upper on a fixing element; sealing the conformal film on the upper and the sole located on the fixing element, wherein a first surface of the conformal film contacts the sole and the upper, the conformal film comprising: (1) a peripheral portion having a thickness in a range of 5 mm to 15 mm, forming an outer periphery of the conformal film; and (2) a transition portion having a thickness in a range of 1 mm to 4 mm between the first surface and the second surface, wherein the transition portion extends from the first surface to the second surface. The peripheral portion forms an inner extension of the outer periphery; and (3) a conformal portion extending from the transition portion in the direction of the second surface and forming a receiving cavity, the conformal portion having a thickness in the range of 1 mm to 4 mm, wherein the peripheral portion, the transition portion and the conformal portion are a unitary structure composed of a common material; and generating a pressure difference experienced between the first surface of the conformal membrane and the relative second surface of the conformal membrane, wherein the pressure at the second surface of the conformal membrane is a pressure greater than the pressure at the first surface; and reducing the pressure difference after a predetermined time period.

[0126] 23. The method of clause 22, wherein the pressure difference is in the range of 0.5 bar to 3.9 bar.

[0127] 24. A method as described in any of clauses 22 to 23, wherein the predetermined time period is at least 25 seconds.

Claims

1. A press machine adapted to maintain the relative position of an upper and a sole unit while the upper and the sole unit are joined, the press machine include: a membrane chamber surrounded and formed by a membrane container and an associated conformal membrane, the membrane chamber being configured to effectively receive a pressurized material and provide a volume for the pressurized material to surround and apply a force to portions of the conformal membrane from within the membrane chamber; a membrane fixture configured to allow the membrane container to be secured to the press in a closed, operative arrangement by the membrane fixture; as well as A securing element is configured to retain the last in a position that allows the upper and the sole unit to be contacted by the conformal membrane.

2. The press of claim 1, wherein the membrane retainer is further configured to allow the membrane retainer to effectively retain the membrane container and the associated conformal membrane in a position relative to the article of footwear to which the pressure is applied.

3. The press of claim 1 further comprising one or more mechanisms for controlling pressure.

4. The press of claim 3, wherein the one or more mechanisms are regulators.

5. The press of claim 1, further comprising a heating source, wherein the heating source is a resistive heating element, an infrared heating element, or an inductive heating element. The press of claim 1 , wherein the pressurized material is a pressurized gas.

7. The press of claim 1 wherein the membrane retainer is a releasable mechanism.

8. A conformal membrane for use in conjunction with an article of footwear, wherein the conformal membrane has a receiving cavity, the receiving cavity being formed into a shape similar to a portion of the article of footwear intended to be received, the receiving cavity having a first receiving cavity half section and a second receiving cavity half section, and the maximum width of the first receiving cavity half section measured in a lateral direction is greater than any width of the second receiving cavity half section.

Citation Information

Patent Citations

  • Bottom-down last for 3D forming

    CN105072941A

  • System and method for applying heat and pressure to three-dimensional articles

    CN105072942A

  • Method of Sticking Shoe Soles to Shoe Uppers and Press therefor.

    GB1181632A

  • hydraulic press for shoe with cooling device

    KR200314882Y1

  • Vacuum Formed Knit Sole System for an Article of Footwear Incorporating a Knitted Component