Self-lubricating carbon slide plate

By prefabing liquid-containing materials on the carbon skateboard, the friction loss problem of carbon skateboard caused by unevenness of the power grid is solved, extending its service life and reducing costs.

CN119017943APending Publication Date: 2024-11-26高迪峰
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411189036.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

In dry climates, carbon skateboards have increased friction losses due to unevenness of the power grid, which has a short life and high cost.

Method used

Prefabricated liquid-containing material on the carbon skateboard. By punching holes on the carbon skateboard and filling it with oil-absorbing material, the material is fully absorbed in the lubricant and fixed, ensuring that the lubricant is slowly released during use to reduce friction losses.

Benefits of technology

It extends the service life of the carbon skateboard, reduces wear, and the liquid-absorbing material absorbs air moisture and remains moist during the cooling process, further extending the material life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119017943A_ABST
    Figure CN119017943A_ABST
Patent Text Reader

Abstract

The invention discloses a self-lubricating carbon slide plate which comprises a carbon slide plate and liquid-containing materials, and the carbon slide plate is provided with a plurality of liquid-containing materials; the liquid-containing material is of a columnar structure and is fixedly connected with the carbon slide plate in a limiting manner. According to the self-lubricating carbon sliding plate, the purpose of self-lubricating protection is achieved through structural arrangement.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of rail transportation equipment, in particular to a self-lubricating carbon slide plate. Background Art

[0002] When the train is running, there is constant friction between the carbon slide plate on the pantograph and the contact grid. In dry climate areas and sections with poor grid flatness, the carbon slide plate is abraded, has a short lifespan, and is expensive.

[0003] This invention prefabricates the lubricating liquid in the carbon slide board. When the train is running and there is friction between the carbon slide board and the power grid, the lubricating liquid will be released at the same time, thereby reducing the friction loss of the carbon slide board and extending the service life of the carbon slide board. Summary of the invention

[0004] The purpose of the present invention is to provide a self-lubricating carbon slide plate to solve the problems raised in the above background technology.

[0005] To achieve the above-mentioned object, the present invention provides the following technical solutions: a self-lubricating carbon slide plate, comprising a carbon slide plate and a liquid-containing material, wherein a plurality of liquid-containing materials are arranged on the carbon slide plate;

[0006] The liquid-containing material is arranged in a columnar structure and is fixedly connected to the carbon slide plate in a limited position.

[0007] A method for manufacturing a self-lubricating carbon slide plate:

[0008] S1. Punch several holes on the carbon slide;

[0009] S2, making the oil absorbing material into a cylindrical shape according to the hole size of the carbon slide plate;

[0010] S3, press the cylindrical part into the hole;

[0011] S4. Soak the carbon slide assembly in lubricating liquid to allow the oil absorbing material to fully absorb the oil;

[0012] S5. Take out and dry.

[0013] A method for manufacturing a self-lubricating carbon slide plate:

[0014] S1. Punch several holes on the carbon slide;

[0015] S2, placing the carbon slide plate into the mold;

[0016] S3, hot extruding the oil absorbing material into the hole of the carbon slide plate, and demoulding;

[0017] S4. Soak the carbon slide assembly in lubricating liquid to allow the oil absorbing material to fully absorb the oil;

[0018] S5. Take out and dry.

[0019] Compared with the prior art, the present invention has the following beneficial effects:

[0020] Preform several through holes evenly on the carbon slide plate, and the positions can be arranged according to different usage conditions. Put the liquid absorbing material in the through holes, and the material can be inorganic liquid absorbing material (such as clay, bentonite, etc.) or organic liquid absorbing material (such as polyacrylate, rubber, etc.). Soak the prepared carbon slide plate in the lubricating liquid to allow the liquid absorbing material to fully absorb the lubricating liquid.

[0021] Production process: Option 1

[0022] 1. Punch several holes on the carbon skateboard;

[0023] 2. Make the oil absorbing material into a cylindrical shape according to the hole size of the carbon slide plate;

[0024] 3. Press the cylindrical part into the hole;

[0025] 4. Soak the carbon slide assembly in lubricating liquid to allow the oil absorbing material to fully absorb the oil;

[0026] 5. Take out and dry.

[0027] Production process: Option 2

[0028] 1. Punch several holes on the carbon skateboard;

[0029] 2. Place the carbon skateboard into the mold;

[0030] 3. Hot extrude the oil absorbing material into the hole of the carbon slide plate and demould;

[0031] 4. Soak the carbon slide assembly in lubricating liquid to allow the oil absorbing material to fully absorb the oil;

[0032] 5. Take out and dry.

[0033] During the use of the carbon skateboard, the absorbent material will slowly release lubricating fluid as it rubs, thus reducing wear. After the train is running, the absorbent material will absorb moisture from the air during the process of cooling from hot to cold, thus keeping the material moist and extending its life.

[0034] Alternatives

[0035] The lubricating liquid can be liquids such as lubricating oil or water, and the liquid absorbing material can be arranged anywhere on the carbon skateboard.

[0036] The entire carbon skateboard can also be made of porous conductive material to form an entire oil-containing carbon skateboard, which can achieve a better long life effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 It is a schematic diagram of the main structure of the present invention;

[0038] Figure 2 It is a split diagram of the main body of the present invention.

[0039] In the figure: 01-carbon slide plate; 02-liquid material. DETAILED DESCRIPTION

[0040] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0041] See also Figure 1-2 , the present invention provides a technical solution: a self-lubricating carbon slide plate, comprising a carbon slide plate 01 and a liquid-containing material 02, wherein a plurality of liquid-containing materials 02 are arranged on the carbon slide plate 01;

[0042] The liquid-containing material 02 is arranged in a columnar structure and is fixedly connected to the carbon slide plate 01 in a limited manner.

[0043] A method for manufacturing a self-lubricating carbon slide plate:

[0044] S1. Punch several holes on the carbon slide;

[0045] S2, making the oil absorbing material into a cylindrical shape according to the hole size of the carbon slide plate;

[0046] S3, press the cylindrical part into the hole;

[0047] S4. Soak the carbon slide assembly in lubricating liquid to allow the oil absorbing material to fully absorb the oil;

[0048] S5. Take out and dry.

[0049] A method for manufacturing a self-lubricating carbon slide plate:

[0050] S1. Punch several holes on the carbon slide;

[0051] S2, placing the carbon slide plate into the mold;

[0052] S3, hot extruding the oil absorbing material into the hole of the carbon slide plate, and demoulding;

[0053] S4. Soak the carbon slide assembly in lubricating liquid to allow the oil absorbing material to fully absorb the oil;

[0054] S5. Take out and dry.

[0055] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A self-lubricating carbon slide plate, characterized in that: It comprises a carbon slide plate (01) and a liquid-containing material (02), wherein a plurality of liquid-containing materials (02) are arranged on the carbon slide plate (01); The liquid-containing material (02) is arranged in a columnar structure and is fixedly connected to the carbon slide plate (01) in a limited position.

2. A method for manufacturing a self-lubricating carbon slide plate, using the self-lubricating carbon slide plate described in claim 1, characterized in that: S1. Punch several holes on the carbon slide board; S2, making the oil absorbing material into a cylindrical shape according to the hole size of the carbon slide plate; S3, press the cylindrical part into the hole; S4. Soak the carbon slide assembly in lubricating liquid to allow the oil absorbing material to fully absorb the oil; S5. Take out and dry.

3. A method for manufacturing a self-lubricating carbon slide plate, using the self-lubricating carbon slide plate described in claim 1, characterized in that: S1. Punch several holes on the carbon slide board; S2, placing the carbon slide plate into the mold; S3, hot extruding the oil absorbing material into the hole of the carbon slide plate, and demoulding; S4. Soak the carbon slide assembly in lubricating liquid to allow the oil absorbing material to fully absorb the oil; S5. Take out and dry.