Processing method for synchronously sintering passive device and chip and semiconductor assembly

CN119028848AActive Publication Date: 2024-11-26JIANGXI WANNIANXIN MICROELECTRONICS CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411137694.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-26
Estimated Expiration
2044-08-19

AI Technical Summary

Technical Problem

The pressure-sintering process of passive devices and chips in existing semiconductor power module packages is low in efficiency, resulting in many processes, high costs and risk of substrate oxidation, especially the problem of thermistor PTC being easily broken.

Method used

The device groove is opened on the copper-clad ceramic substrate and the adapted steel mesh is assembled, sintered silver is coated and scraped. After high-temperature pre-baking, the copper-clad ceramic substrate of the passive device and chip is raised and lowered by a sintering furnace mold. Pressure is applied on both sides for synchronous sintering.

Benefits of technology

This reduces the sample preparation process during the packaging process, improves processing efficiency, reduces the risk of substrate oxidation, and realizes high reliability, low-cost synchronous sintering packaging between passive devices and chips.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028848A_ABST
    Figure CN119028848A_ABST
Patent Text Reader

Abstract

The invention discloses a processing method for synchronous sintering of a passive device and a chip and a semiconductor component, and the processing method comprises the steps: forming a device groove in the surface layer of a top surface copper layer in a copper-clad ceramic substrate, and assembling a steel mesh matched with the size of the groove in the device groove, the initial printing position of the steel mesh is coated with a sintered silver welding material, scraping is conducted through a scraper, sintered silver is laid in a plurality of printing areas at the opening of the steel mesh in a through printing mode, and a passive device and a chip are assembled after the copper-clad ceramic substrate is subjected to high-temperature pre-baking; the upper side and the lower side of the copper-clad ceramic substrate assembled with the passive device and the chip are pressurized and sintered at high temperature, so that the passive device and the chip are synchronously sintered and fixed to obtain the semiconductor assembly. According to the processing method, the device groove is arranged and the steel mesh is assembled in combination with the size of the passive device, and synchronous sintering of the passive device and the chip is realized through two times of sintering, so that a sample preparation process in a packaging process is reduced, pressure head molds of different specifications do not need to be manufactured, and the packaging processing efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor packaging, and in particular to a processing method for synchronously sintering a passive device and a chip and a semiconductor assembly. Background Art

[0002] At present, in the pressure sintering process of semiconductor power module packaging, the basic thickness of different devices is different. For example, passive devices such as gate resistor Rg and positive temperature coefficient thermistor PTC are relatively thick. The thickness of the above two devices is usually greater than the thickness of SiC MOSFET chips. Due to the large difference in thickness between these two passive devices and the chip, after welding on the copper-clad ceramic substrate, the top cannot be on the same horizontal plane and synchronous pressure sintering cannot be performed. The following method is usually used.

[0003] One method is to sinter the chip first, then add a process to sinter a passive device (device A: such as gate resistor Rg), and then add a process to sinter the next passive device (such as device B: positive temperature coefficient thermistor PTC). This treatment method is inefficient. The bonding strength between the device and the copper-clad ceramic substrate is insufficient after sintering. There are many processes, and the copper layer on the surface of the substrate is more prone to oxidation. In addition, only one device B is used in a module. When device B is sintered alone, the pressure per unit area is too high, so device B is easy to break;

[0004] Another method is to use a customized pressure head mold with different height planes. This method can only produce corresponding customized molds according to fixed models of device A and device B. If different performance chips are matched with different models of passive devices for installation, multiple molds need to be customized again. Not only are the number of modules large, but the mold cost is too high, and it is troublesome to manage and use, resulting in low processing and manufacturing efficiency.

[0005] These two methods have many processes or require many customized molds, which will increase the cost and have poor processing efficiency. Therefore, the pressure sintering process for passive components and chips in the prior art method has the problem of low processing efficiency. Summary of the invention

[0006] The embodiment of the present invention provides a processing method for synchronously sintering a passive device and a chip and a semiconductor component, aiming to solve the problem of low processing efficiency in the pressure sintering process of the passive device and the chip in the prior art method.

[0007] In a first aspect, an embodiment of the present application provides a processing method for synchronously sintering a passive device and a chip, wherein the processing method comprises:

[0008] According to the size of each passive component, a device groove is formed in the surface layer of the top copper layer of the copper-clad ceramic substrate;

[0009] Installing a steel mesh matching the size of the groove at the groove of the device;

[0010] Applying sintered silver solder material at the starting printing position of the steel mesh; the starting printing position is the outer edge of the printing area formed at the opening of the steel mesh;

[0011] Use a scraper to scrape the surface of the steel mesh closely, so that the sintered silver solder material is spread flatly on the surface of the printing area;

[0012] Pre-baking the copper-clad ceramic substrate covered with sintered silver solder material at high temperature;

[0013] The passive components and the chip are respectively mounted in the chip mounting area corresponding to the printing area, and the passive components and the chip are contacted and bonded with the sintered silver;

[0014] The upper and lower sides of the copper-clad ceramic substrate on which the passive components and the chip are assembled are pressurized by a sintering furnace mold and sent into a high-temperature environment for sintering, so as to sinter and fix the passive components and the chip synchronously.

[0015] In a second aspect, an embodiment of the present application further provides a processing method for synchronously sintering a passive device and a chip, wherein the processing method comprises:

[0016] According to the size of each passive component, a device groove is formed in the surface layer of the top copper layer of the copper-clad ceramic substrate;

[0017] Assemble the passive components and chips with silver film on the bottom into the chip mounting areas corresponding to the device grooves:

[0018] The upper and lower sides of the copper-clad ceramic substrate on which the passive components and the chip are assembled are pressurized by a sintering furnace mold and sent into a high-temperature environment for sintering, so as to sinter and fix the passive components and the chip synchronously.

[0019] In a third aspect, an embodiment of the present application further provides a semiconductor component, wherein the semiconductor component is processed by the processing method described in the first aspect or the second aspect, and the semiconductor component includes a copper-clad ceramic substrate, a passive device and a chip;

[0020] The copper-clad ceramic substrate comprises a front copper layer, a back copper layer, and a ceramic layer sandwiched between the front copper layer and the back copper layer;

[0021] A device groove is provided on the front copper layer of the copper-clad ceramic substrate; sintered silver is laid on the bottom surface of the device groove, and the passive device is bonded and fixed on the sintered silver on the bottom surface of the device groove;

[0022] Sintered silver is provided between the front copper layer of the copper-clad ceramic substrate and the chip, and the chip is bonded and fixed on the sintered silver of the front copper layer;

[0023] The top surface height of the chip is flush with the top surface height of the passive component.

[0024] The embodiment of the present invention provides a processing method and a semiconductor component for synchronous sintering of passive devices and chips. The processing method includes opening a device groove in the surface layer of the top copper layer in a copper-clad ceramic substrate, assembling a steel mesh matched with the size of the groove at the device groove, coating a sintered silver welding material at the starting printing position of the steel mesh and scraping it with a scraper, spreading the sintered silver leak printing on multiple printing areas at the opening of the steel mesh, assembling passive devices and chips after high-temperature pre-baking the copper-clad ceramic substrate, pressurizing and sintering at high temperature the upper and lower sides of the copper-clad ceramic substrate assembled with the passive devices and chips, thereby synchronously sintering and fixing the passive devices and chips to obtain a semiconductor component. The above-mentioned processing method sets the device groove and assembles the steel mesh in combination with the size of the passive device, and realizes the synchronous sintering and fixing of the passive device and the chip through two sintering steps, thereby reducing the sample preparation steps in the packaging process, eliminating the need to make multiple pressure head molds of different specifications, and improving the efficiency of the packaging process; and also reduces the risk of substrate oxidation that is prone to occur in a multi-step sintering process, solves the problem of easy breakage of thermistor PTC during the sintering process, and realizes high-reliability, low-cost synchronous sintering packaging of passive devices and chips. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying any creative work.

[0026] Figure 1 A method flow chart of a method for synchronously sintering a passive device and a chip provided in an embodiment of the present invention;

[0027] Figure 2 Another method flow chart of the processing method for synchronously sintering passive components and chips provided by an embodiment of the present invention;

[0028] Figure 3 A side structural diagram of a ceramic substrate provided in an embodiment of the present invention;

[0029] Figure 4 A side structural diagram of a ceramic substrate and a steel mesh provided in an embodiment of the present invention;

[0030] Figure 5 Another side structural diagram of the ceramic substrate and steel mesh provided in an embodiment of the present invention;

[0031] Figure 6 An application structure diagram of a ceramic substrate provided by an embodiment of the present invention;

[0032] Figure 7 A schematic diagram of a processing process of a semiconductor component provided by an embodiment of the present invention;

[0033] Figure 8 A schematic diagram of another processing process of a semiconductor component provided by an embodiment of the present invention;

[0034] Fig. 9 A partial structural diagram of a processing process of a semiconductor component provided by an embodiment of the present invention;

[0035] Fig.10 A schematic diagram of another processing process of a semiconductor component provided by an embodiment of the present invention;

[0036] Fig.11 Another partial structural diagram of the processing process of the semiconductor component provided by the embodiment of the present invention;

[0037] Fig.12 A schematic diagram of another processing process of a semiconductor component provided by an embodiment of the present invention;

[0038] Fig.13 A schematic diagram of a subsequent processing process of a semiconductor component provided by an embodiment of the present invention;

[0039] Fig.14 A schematic diagram of another processing process of a semiconductor component provided by an embodiment of the present invention;

[0040] Fig.15 A schematic diagram of another processing process of a semiconductor component provided by an embodiment of the present invention;

[0041] Fig.16 A schematic diagram of a subsequent processing process of a semiconductor component provided by an embodiment of the present invention;

[0042] Fig.17 A schematic diagram of another subsequent processing process of a semiconductor component provided by an embodiment of the present invention;

[0043] Fig.18 A schematic diagram of another subsequent processing process of a semiconductor component provided by an embodiment of the present invention;

[0044] Fig.19 A schematic diagram of a subsequent processing process of a semiconductor component provided by an embodiment of the present invention;

[0045] Fig. 20 An overall structural diagram of a semiconductor component provided by an embodiment of the present invention;

[0046] Fig.21 Another overall structural diagram of a semiconductor component provided by an embodiment of the present invention.

[0047] Figure numerals: 1. copper-clad ceramic substrate; 2. steel mesh; 3. chip; 4. device A; 5. device B; 6. sintered silver soldering material; 61. sintered silver; 7. scraper; 8. sintering furnace mold; 81. upper mold; 82. lower mold; 11. ceramic layer; 12. top copper layer; 13. bottom copper layer; 121. device groove. DETAILED DESCRIPTION

[0048] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0049] It should be understood that when used in this specification and the appended claims, the terms "include" and "comprises" indicate the presence of described features, integers, steps, operations, elements and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or combinations thereof.

[0050] It should also be understood that the terms used in the present specification are only for the purpose of describing specific embodiments and are not intended to limit the present invention. As used in the present specification and the appended claims, the singular forms "a", "an" and "the" are intended to include the plural forms unless the context clearly indicates otherwise. It should also be further understood that the term "and / or" used in the present specification and the appended claims refers to any combination of one or more of the associated listed items and all possible combinations, and includes these combinations.

[0051] See also Figure 1 As shown in the figure, an embodiment of the present application discloses a processing method for synchronous sintering of passive components and chips, wherein the processing method includes steps S110 to S170.

[0052] S110, opening a device groove in the surface layer of the top copper layer of the copper-clad ceramic substrate according to the size of each passive device.

[0053] A device groove 121 can be opened in the surface layer of the top copper layer 12 of the copper-clad ceramic substrate 1 according to the size of the passive device. The size of the opened device groove 121 corresponds to the size of the passive device. The device groove 121 is also a groove structure for assembling the device. Generally speaking, the outer dimensions of the device groove 121 are larger than the outer dimensions of the passive device. The structure of the copper-clad ceramic substrate 1 with the device groove 121 is as follows: Figure 6 shown.

[0054] like Figure 3 As shown, the depth of the device groove 121 for placing device A4 (device A4 is used to refer to gate resistor Rg in the following description) can be defined as Z1, and the depth of the device groove 121 for placing device B5 (device B5 is used to refer to positive temperature coefficient thermistor PTC in the following description) can be defined as Z2; wherein, device A4 and device B5 are both passive devices. The thickness of device A4 is Za, the thickness of device B5 is Zb, and the thickness of chip 3 is Zc. The depth of the device groove 121 can be calculated, that is, the depth of the device groove 121 is set to the difference between the thickness of device A4 and chip 3, and the difference between the thickness of device B5 and chip 3. That is, Z1 = Za-Zc, Z2 = Zb-Zc.

[0055] like Figure 4 As shown, the length of the device groove 121 for placing device A4 can be defined as X1, and the length of the device groove 121 for placing device B can be defined as X2. The length of device A4 is Xa, the length of device B is Xb, Xs is the single-side reserved overflow value of the sintered silver 61 at the bottom of the device in the X direction, Xg is the length value of the bottom surface of the L-shaped concave platform in the steel mesh 2 in the X direction, Hg is the thickness value of the bending part of the groove position of the steel mesh 2, and Xj is the gap value between the steel mesh 2 and the side wall of the device groove 121 in the X direction. Then, the length of the device groove 121 for placing device A4 in the X direction can be obtained as X1=Xa+(Xs+Xg+Hg+Xj)×2, and the length of the device groove 121 for placing device B in the X direction can be obtained as X2=Xb+(Xs+Xg+Hg+Xj)×2.

[0056] like Figure 5As shown, the width of the device groove 121 for placing device A4 can be defined as Y1, and the width of the device groove 121 for placing device B can be defined as Y2. The width of device A4 is Ya, the width of device B is Yb, Ys is the single-side reserved overflow value of the sintered silver 61 at the bottom of the device in the Y direction, Yg is the length value of the bottom surface of the L-shaped concave platform in the steel mesh 2 in the Y direction, Hg is the thickness value of the bending part of the groove position of the steel mesh 2, and Yj is the gap value between the steel mesh 2 and the side wall of the device groove 121 in the Y direction. Similarly, the width of the device groove 121 for placing device A4 in the Y direction can be obtained as Y1=Ya+(Ys+Yg+Hg+Yj)×2, and the width of the device groove 121 for placing device B in the Y direction can be obtained as Y2=Yb+(Ys+Yg+Hg+Yj)×2.

[0057] S120, assembling a steel mesh matching the size of the groove at the device groove.

[0058] The steel mesh 2 is installed at the device groove 121, and the steel mesh 2 installed in each groove corresponds to the size of the groove, wherein the steel mesh 2 is a 3D printed steel mesh 2. The specific setting position of the steel mesh 2 is as follows: Figures 3 to 5 shown.

[0059] S130, coating a sintered silver solder material at the starting printing position of the steel mesh.

[0060] Furthermore, the opening in the center of the steel mesh 2 forms a printing area, and each steel mesh 2 corresponds to a printing area, and the multiple steel meshes 2 formed form multiple printing areas. The sintered silver solder material 6 is coated on the starting printing position of the printing area corresponding to the steel mesh 2. The starting printing position is the outer edge of the printing area formed by the opening of the steel mesh 2.

[0061] S140, using a scraper to scrape the surface of the steel mesh closely, so that the sintered silver solder material is spread evenly and covers the surface of the printing area.

[0062] Use a scraper 7 to scrape the surface of the steel mesh 2 so that the sintered silver soldering material 6 is spread and covered on the surface of the printing area. The thickness of the sintered silver soldering material 6 spread on the surface of the printing area is equal to the thickness of the steel mesh 2. Afterwards, use a scraper 77 to scrape the surface of the steel mesh 2 so that the sintered silver soldering material 6 coated in step S130 is spread and covered on the surface of the printing area. After the coated sintered silver soldering material 6 is coated, the thickness of the sintered silver soldering material 6 spread on the surface of the printing area can be equal to the thickness of the steel mesh 2. In the specific operation process of the steps of this application, it is necessary to use a matching 3D steel mesh 2 and a 3D scraper 7. The 3D scraper 7 used in this application is a split scraper 7 different from the conventional integrated scraper 7. The blade of the scraper 7 corresponding to the printing area position needs to be separated, movable up and down and rotatable. The specific scraper 7 preparation structure and device are not within the scope of the key discussion of this article.

[0063] In a specific embodiment, step S140 specifically includes the following steps: the scraper moves parallel to the surface of the steel mesh at an angle of 60°; when the scraper extends into the L-shaped concave platform of the steel mesh, the rear end of the blade of the scraper moves vertically along the inner wall of one side of the steel mesh, and the inner wall of the steel mesh is a vertical wall surface wrapped around the side wall of the device groove; the front end of the scraper is against the top surface of the L-shaped concave platform in the steel mesh and moves horizontally to scrape the surface layer of the sintered silver solder material flat so that the sintered silver solder material is flattened. ; The scraper forms an angle of 60° with the top surface of the L-shaped recess; when the scraper contacts the edge of the L-shaped recess of the steel mesh and slides upward from the L-shaped recess, the direction of the scraper is adjusted to be vertical, and the side of the scraper is close to the inner wall of the other side of the steel mesh for vertical movement; the front end of the scraper completely slides out of the L-shaped recess in the steel mesh, and the scraper is adjusted to form an angle of 60° with the surface of the steel mesh and continues to move parallel; repeat the above steps until the surfaces of all printing areas are flatly covered with the sintered silver soldering material.

[0064] Specifically, the scraper can be used to move parallel to the surface of the steel mesh at an angle of 60°. That is, the bottom blade of the 3D scraper is close to the front of the 3D steel mesh, forming a conventional printing angle of 60° with the front of the steel mesh, and then it starts to move steadily in the Y direction to scrape the sintered silver across the front of the 3D steel mesh. The specific operation process is as follows: Figure 7 shown.

[0065] Furthermore, when the scraper scrapes the L-shaped concave platform of the steel mesh and goes down into the L-shaped concave platform, the rear end of the scraper blade in the printing direction moves vertically along the inner side wall of one side of the steel mesh, that is, the rear end of the scraper blade moves vertically downward until the bottom of the blade contacts the top surface of the L-shaped concave platform in the steel mesh and stops. The inner side wall of the steel mesh is a vertical wall surface wrapped around the side wall of the device groove. The specific operation process is as follows Figure 8 shown.

[0066] Continue to move the scraper in the printing direction to smoothly print the sintered silver on the printing area corresponding to the device groove. At this time, the thickness of the sintered silver solder material on the surface of the printing area is equal to the thickness of the steel mesh. During this process, the scraper is kept at a 60° angle with the top surface of the L-shaped concave platform. The specific operation process is as follows: Fig. 9 shown.

[0067] When the scraper touches the edge of the L-shaped concave platform and slides upward from the L-shaped concave platform, adjust the direction of the scraper to be vertical. At this time, the side of the scraper is close to the inner wall of the other side of the steel mesh and moves vertically. The specific operation process is as follows: Fig.10 shown.

[0068] Continue to move forward until the scraper contacts the side wall on the left side of the steel mesh opening in the device groove. At this time, the scraper briefly stops moving in the Y direction and moves upward in the vertical direction until the front end of the scraper blade coincides with the top edge of the left side of the steel mesh opening in the device groove. The specific operation process is as follows: Fig.11 shown.

[0069] The front end of the scraper completely slides out of the L-shaped concave platform in the steel mesh, then adjust the scraper to a 60° angle with the surface of the steel mesh and continue to move parallel, that is, at this time, rotate the split scraper counterclockwise until the split scraper and the steel mesh maintain a 60° conventional printing angle. At this time, the split scraper surface and the integral scraper surface at the printing chip position overlap again. The specific operation process is as follows: Fig.12 shown.

[0070] Continue to move along the Y direction to complete the printing of sintered silver in the chip printing area. The specific operation process is as follows: Fig.13 Repeat the above steps until the surfaces of all printing areas are flatly covered with the sintered silver solder material, and move the scraper to the printing area corresponding to device A. Its working principle is similar to the specific operation process of flatly covering the printing area of ​​device B with the sintered silver solder material. The specific operation process is as follows Fig.14 shown.

[0071] Lift the 3D steel mesh upwards and demould to complete the printing process. At this time, the sintered silver will slightly overflow to the surroundings, and the overall sintered silver thickness will decrease slightly, but the sintered silver at all positions is still the same thickness. Fig.15As shown. Among them, the outer dimensions of the sintered silver solder material laid flat in the printing area are all larger than the outer dimensions of the passive devices and chips assembled in the chip mounting area corresponding to the printing area. After the sintered silver solder material is laid flat on the surface of the printing area, the outer dimensions of the sintered silver solder material laid flat are all larger than the outer dimensions of the passive devices and chips to be assembled. The specific structure is as follows Fig.15 shown.

[0072] S150, pre-baking the copper-clad ceramic substrate covered with the sintered silver solder material at high temperature.

[0073] The copper-clad ceramic substrate flatly covered with sintered silver solder material is pre-baked at high temperature.

[0074] Before installing chips and devices on sintered silver, it is necessary to pre-bake it at high temperature to remove some filling materials that increase fluidity inside the material, and pre-solidify it. The baking parameters are set according to the recommended parameters in the characteristic table of the sintered silver material itself. After baking, the thickness of the sintered silver will be further reduced, but the thickness of the sintered silver at all positions remains the same. The structure of the copper-clad ceramic substrate after high-temperature pre-baking is as follows: Fig.16 shown.

[0075] S160, respectively assembling the passive components and the chip in the chip mounting area corresponding to the printing area, and contacting and bonding the passive components and the chip with the sintered silver.

[0076] The passive components and chips are assembled in the printing area respectively. At this time, the passive components and chips are in contact with and bonded to the sintered silver at the bottom. The obtained device structure is as follows: Fig.17 shown.

[0077] In a specific embodiment, step S160 specifically includes the following steps: assembling the passive components and the chip in the mounting area corresponding to the printing area and performing a pressurization treatment so that the passive components and the chip are in contact with and bonded to the sintered silver; the pressure of the pressurization treatment is 15-35 kg / cm 2 ; The duration of the pressure treatment is 0.25-5 minutes.

[0078] Specifically, after the passive components and chips are assembled in the printing area, they can be pressurized by external equipment, that is, pressure is applied to the upper ends of the passive components and chips, so that the passive components and chips can be closely contacted and bonded with the sintered silver; wherein the pressure of the pressurization treatment can be 15-35kg / cm 2 The duration of the pressure treatment is 0.25-5 minutes.

[0079] S170, pressurizing the upper and lower sides of the copper-clad ceramic substrate on which the passive components and the chip are assembled through a sintering furnace mold and sending it into a high-temperature environment for sintering, so as to sinter and fix the passive components and the chip synchronously.

[0080] The upper and lower sides of the copper-clad ceramic substrate on which the passive components and chips are assembled are pressurized by a sintering furnace mold and sent into a high-temperature environment for sintering, so as to sinter and fix the passive components and the chips simultaneously. The pressure for pressurizing the upper and lower sides of the copper-clad ceramic substrate on which the passive components and chips are assembled is 150-250kg / cm 2 , and the pressure applied to the upper and lower sides of the copper-clad ceramic substrate on which the passive devices and chips are assembled is greater than the pressure of the pressurization treatment; the baking temperature of the high-temperature pre-baking is lower than the temperature for sintering in a high-temperature environment.

[0081] The upper and lower sides of the copper-clad ceramic substrate on which the passive components and chips are mounted are pressurized by the sintering furnace mold 8. The specific operation process is as follows: Fig.18 and Fig.19 As shown, the sintering furnace mold 8 includes an upper mold 81 and a lower mold 82 . Fig.18 The operation process of pressing the upper mold down. Fig.19 The specific structure after the upper mold is pressed down into place. Keep the upper and lower sides of the copper-clad ceramic substrate under pressure and send it into a high-temperature environment for sintering. At this time, the passive components and the chip can be sintered and fixed synchronously. At this time, the thickness of the sintered silver will be further reduced, but the thickness of the sintered silver at all positions remains the same. At this point, the synchronous sintering of device A, device B, and chip C is completed. The semiconductor component obtained after sintering is as follows Fig. 20 As shown, it can be seen that Fig. 20 The thickness of the sintered silver after medium sintering and fixing is smaller than the thickness of the sintered silver after high temperature pre-baking.

[0082] The pressure on the upper and lower sides of the copper-clad ceramic substrate where passive components and chips are assembled is 150-250kg / cm 2 The pressure applied here is greater than the pressure of the above-mentioned pressure treatment. The pressure applied to the upper and lower sides of the copper-clad ceramic substrate on which the passive components and chips are mounted is about 6 times the pressure of the above-mentioned pressure treatment. The temperature of the sintering in the high-temperature environment here is higher than the baking temperature of the above-mentioned high-temperature pre-baking.

[0083] The passive components are placed on the sintered silver laid in the corresponding device grooves on the front copper layer circuit surface of the copper-clad ceramic substrate, and the chip is placed on the sintered silver pre-set at the corresponding sintering position on the front copper layer circuit surface of the copper-clad ceramic substrate, and the thickness of the sintered silver is kept consistent, which can ensure that the top of each passive component and the chip are on the same horizontal plane, and can be sintered in one step. The actual application effect is as follows: Figure 6shown.

[0084] See also Figure 2 As shown in the figure, the embodiment of the present application also discloses a processing method for synchronous sintering of passive components and chips, wherein the processing method includes steps S210 to S230.

[0085] S210, opening a device groove in the surface layer of the top copper layer of the copper-clad ceramic substrate according to the size of each passive device.

[0086] The operation steps of opening the device groove here are the same as the above S110, and will not be described in detail here.

[0087] S220, respectively assembling the passive components and chips with silver films bonded to the bottom in the chip mounting areas corresponding to the device grooves.

[0088] At this time, the passive components with silver film bonded to the bottom and the chips with silver film bonded to the bottom can be directly mounted in the chip mounting area corresponding to the device groove, that is, the silver film is used here instead of sintered silver for chip mounting.

[0089] Before the passive device and chip with the silver film bonded to the bottom are respectively mounted in the chip mounting area corresponding to the device groove, the method further includes: placing the silver film on the bottom surface of the passive device or chip; applying a specific pressure on the silver film to press and bond the silver film to the back surface of the passive device or the back surface of the chip, and the silver film is broken at the edge of the passive chip or at the edge of the chip to obtain the passive device and chip with the silver film bonded to the bottom; the specific pressure is 1-4 kg / cm 2 .

[0090] Specifically, if the passive components and chips are mounted with silver film, the Xs and Ys (the single-side reserved overflow value of the sintered silver at the bottom of the device) defined above can be set to 0. The specific operation process of silver film bonding is to use a loader to pick up the passive components and chips, first place the passive components or chips on top of the silver film, and then apply a specific pressure to allow the bottom of the passive components or chips to contact the pre-baked silver film. The pre-baked silver film is equivalent to the above-mentioned sintered silver. At this time, the bottom edge of the passive component or chip exerts a greater pressure on the silver film, which will cut off the silver film. The bottom of the passive component and chip will be bonded to the silver film material, and then mounted. Therefore, the size of the silver film bonded to the bottom is consistent with the outer dimensions of the passive component or chip. The pressure for pressurization is 1-4kg / cm 2 .

[0091] S230, pressurizing the upper and lower sides of the copper-clad ceramic substrate on which the passive components and the chip are assembled through a sintering furnace mold and sending it into a high-temperature environment for sintering, so as to sinter and fix the passive components and the chip synchronously.

[0092] The specific process of pressurizing and sintering here is similar to the above step S170, and will not be described in detail here. Fig.21 shown.

[0093] The embodiment of the present invention further provides a semiconductor component, which is processed by the processing method described in the above embodiment, such as Fig. 20 and Fig.21 As shown, the semiconductor component includes a copper-clad ceramic substrate 1, a passive device and a chip 3; the copper-clad ceramic substrate 1 includes a front copper layer, a back copper layer, and a ceramic layer 11 sandwiched between the front copper layer and the back copper layer; a device groove 121 is provided on the front copper layer of the copper-clad ceramic substrate 1; sintered silver 61 is laid on the bottom surface of the device groove 121, and the passive device is bonded and fixed to the sintered silver 61 on the bottom surface of the device groove 121; sintered silver 61 is provided between the front copper layer of the copper-clad ceramic substrate 1 and the chip 3, and the chip 3 is bonded and fixed to the sintered silver 61 of the front copper layer; the top surface height of the chip 3 is flush with the top surface height of the passive device.

[0094] The processing method and semiconductor component for synchronous sintering of passive devices and chips provided in the embodiments of the present invention include opening a device groove in the surface layer of the top copper layer in a copper-clad ceramic substrate, assembling a steel mesh matched with the groove size at the device groove, coating a sintered silver welding material at the starting printing position of the steel mesh and scraping it with a scraper, spreading the sintered silver leak printing on multiple printing areas at the opening of the steel mesh, assembling passive devices and chips after high-temperature pre-baking the copper-clad ceramic substrate, pressurizing and sintering at high temperature the upper and lower sides of the copper-clad ceramic substrate assembled with the passive devices and chips, thereby synchronously sintering and fixing the passive devices and chips to obtain a semiconductor component. The above-mentioned processing method sets the device groove and assembles the steel mesh in combination with the size of the passive device, and realizes the synchronous sintering and fixing of the passive device and the chip through two sintering steps, thereby reducing the sample preparation steps in the packaging process, eliminating the need to make multiple pressure head molds of different specifications, and improving the efficiency of the packaging process; and also reduces the risk of substrate oxidation that is prone to occur in a multi-step sintering process, solves the problem of easy breakage of thermistor PTC during the sintering process, and realizes high-reliability, low-cost synchronous sintering packaging of passive devices and chips.

[0095] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can easily think of various equivalent modifications or replacements within the technical scope disclosed by the present invention, and these modifications or replacements should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention shall be based on the protection scope of the claims.

Claims

1. A processing method for synchronous sintering of passive components and chips, It is characterized in that The processing method comprises: According to the size of each passive component, a device groove is formed in the surface layer of the top copper layer of the copper-clad ceramic substrate; Installing a steel mesh matching the size of the groove at the groove of the device; Applying sintered silver solder material at the starting printing position of the steel mesh; the starting printing position is the outer edge of the printing area formed at the opening of the steel mesh; Use a scraper to scrape the surface of the steel mesh closely, so that the sintered silver solder material is spread flatly on the surface of the printing area; Pre-baking the copper-clad ceramic substrate covered with sintered silver solder material at high temperature; The passive components and the chip are respectively mounted in the chip mounting area corresponding to the printing area, and the passive components and the chip are contacted and bonded with the sintered silver; The upper and lower sides of the copper-clad ceramic substrate on which the passive components and the chip are assembled are pressurized by a sintering furnace mold and sent into a high-temperature environment for sintering, so as to sinter and fix the passive components and the chip synchronously.

2. The method for synchronously sintering a passive component and a chip according to claim 1, It is characterized in that The scraper is used to scrape the surface of the steel mesh closely so that the sintered silver solder material is spread flat on the surface of the printing area, including: The scraper moves parallel to the surface of the steel mesh at an angle of 60°; When the scraper extends into the L-shaped concave platform of the steel mesh, the rear end of the blade of the scraper moves vertically along the inner side wall of one side of the steel mesh, and the inner side wall of the steel mesh is a vertical wall surface wrapped around the side wall of the device groove; The front end of the scraper is against the top surface of the L-shaped concave platform in the steel mesh and moves horizontally to scrape the surface of the sintered silver solder material flat so that the sintered silver solder material is spread flat; the scraper and the top surface of the L-shaped concave platform form an angle of 60°; When the scraper contacts the edge of the L-shaped concave platform of the steel mesh and slides upward from the L-shaped concave platform, the direction of the scraper is adjusted to be vertical, and the side surface of the scraper is close to the inner side wall of the other side of the steel mesh to move vertically; The front end of the scraper is completely slid out of the L-shaped concave platform in the steel mesh, and the scraper is adjusted to form an angle of 60° with the surface of the steel mesh and continue to move parallel to it; The above steps are repeated until the surfaces of all printing areas are evenly covered with the sintered silver solder material.

3. The method for synchronously sintering a passive component and a chip according to claim 2, It is characterized in that The thickness of the sintered silver solder material spread on the surface of the printing area is equal to the thickness of the steel mesh.

4. The method for synchronously sintering a passive component and a chip according to claim 3, It is characterized in that The outer dimensions of the sintered silver solder material laid flat in the printing area are larger than the outer dimensions of the passive components and chips mounted in the chip mounting area corresponding to the printing area.

5. The processing method for synchronously sintering a passive component and a chip according to any one of claims 1 to 4, It is characterized in that The method of assembling the passive components and the chip in the chip mounting area corresponding to the printing area, and contacting and bonding the passive components and the chip with sintered silver, comprises: The passive components and the chip are respectively mounted in the mounting area corresponding to the printing area and subjected to a pressurization treatment so that the passive components and the chip are in contact with and bonded to the sintered silver; the pressure of the pressurization treatment is 15-35kg / cm 2 ; The duration of the pressure treatment is 0.25-5 minutes.

6. The method for synchronously sintering a passive component and a chip according to claim 5, It is characterized in that The pressure applied to the upper and lower sides of the copper-clad ceramic substrate on which the passive components and chips are mounted is 150-250 kg / cm 2 , and the pressure applied to the upper and lower sides of the copper-clad ceramic substrate on which the passive components and chips are mounted is greater than the pressure of the pressurizing treatment.

7. The method for synchronously sintering a passive component and a chip according to claim 6, It is characterized in that The baking temperature of the high-temperature pre-baking is lower than the temperature of sintering in a high-temperature environment.

8. A processing method for synchronous sintering of passive components and chips, It is characterized in that The processing method comprises: According to the size of each passive component, a device groove is formed in the surface layer of the top copper layer of the copper-clad ceramic substrate; Assemble the passive components and chips with silver film on the bottom into the chip mounting areas corresponding to the device grooves: The upper and lower sides of the copper-clad ceramic substrate on which the passive components and the chip are assembled are pressurized by a sintering furnace mold and sent into a high-temperature environment for sintering, so as to sinter and fix the passive components and the chip synchronously.

9. The method for synchronously sintering a passive component and a chip according to claim 8, It is characterized in that Before the passive components and chips with silver films bonded to the bottom are respectively mounted in the chip mounting areas corresponding to the device grooves, the method further includes: placing a silver film on the bottom surface of the passive device or chip; A specific pressure is applied to the silver film to press and bond the silver film to the back of the passive device or the back of the chip, and the silver film is broken at the edge of the passive chip or at the edge of the chip to obtain a passive device and chip with a silver film bonded to the bottom; the specific pressure is 1-4 kg / cm 2 .

10. A semiconductor component, It is characterized in that The semiconductor component is obtained by processing using the processing method according to any one of claims 1 to 9, and the semiconductor component includes a copper-clad ceramic substrate, passive devices and a chip; The copper-clad ceramic substrate comprises a front copper layer, a back copper layer, and a ceramic layer sandwiched between the front copper layer and the back copper layer; A device groove is provided on the front copper layer of the copper-clad ceramic substrate; sintered silver is laid on the bottom surface of the device groove, and the passive device is bonded and fixed on the sintered silver on the bottom surface of the device groove; Sintered silver is provided between the front copper layer of the copper-clad ceramic substrate and the chip, and the chip is bonded and fixed on the sintered silver of the front copper layer; The top surface height of the chip is flush with the top surface height of the passive component.

Citation Information

Patent Citations

  • Power device and preparation method thereof

    CN116864404A

  • Connecting element, welded connection, method for producing a metal part comprising the connecting element, connection kit, and method for connecting a metal part to a lead

    EP4287242A1

  • Low-profile electronic circuit module and method for manufacturing the same

    US20040183186A1