Scratch-resistant pre-coating film production process and device
By adding UV coatings, anti-blocking agents, and silica during the pre-coated film production process to form a wear-resistant coating, the problem of poor scratch resistance of the pre-coated film is solved, and the scratch resistance and service life of the pre-coated film are improved.
Patent Information
- Application Number
- CN202411228330.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-03
- Publication Date
- 2024-11-29
AI Technical Summary
Existing pre-coated films have poor scratch resistance and are easily scratched during use, affecting the appearance of the product.
Using high-molecular-weight polypropylene as raw material, UV coating, anti-blocking agent and silica are added in a mixer to form a wear-resistant coating. The wear-resistant coating and adhesive layer are coated on both sides of the substrate layer, cured using a UV curing machine, combined with the anti-static operation of the protective layer, and finally the pre-coated film is produced by winding it up with a winding machine.
It improves the scratch resistance of the pre-coated film, reduces the chance of scratches during use, and ensures the product's appearance and service life.
Smart Images

Figure CN119035050A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of pre-coating film production, and in particular to a scratch-resistant pre-coating film production process and device. Background Art
[0002] Pre-coated film can protect products, improve product quality, and improve product appearance. It is widely used in book packaging and lamination protection of industrial products. However, traditional pre-coated film has poor adhesion. Various fillers and additives are usually present on printed or digital products, which makes it impossible to stably coat the pre-coated film.
[0003] In the prior art, the adhesion-enhancing layer is configured with a water-based adhesive, and a (modified) acrylic emulsion or a (modified) polyurethane emulsion is mixed with an adhesion promoter in an appropriate proportion to produce a water-based adhesive that has good adhesion to ink. The adhesive has good adhesion to a variety of inks and has excellent bonding strength to printed products produced by various printing technologies, especially digital printing technologies, and can perfectly realize embossing, rolling and other protrusion processes after lamination.
[0004] However, in the above-mentioned prior art, the scratch resistance of the pre-coated film is poor and it is easily scratched during use, which affects the appearance of the product. Summary of the invention
[0005] The purpose of the present invention is to provide a scratch-resistant pre-coated film production process and device to solve the problem that the pre-coated film in the prior art has poor scratch resistance and is easily scratched during use, which affects the appearance of the product.
[0006] To achieve the above object, the present invention provides a scratch-resistant pre-coated film production process, comprising the following steps:
[0007] Take out the adhesive, place it in a heating box, heat it to 100°C, and evenly apply it on one side of the substrate layer using a glue coating machine;
[0008] Maintaining the temperature of the adhesive during coating;
[0009] Using high molecular weight polypropylene as raw material, UV coating, anti-adhesive agent and silicon dioxide are added in a mixer in sequence and stirred to obtain a wear-resistant coating;
[0010] Evenly apply the wear-resistant coating on the other side of the substrate layer, and perform a curing operation using a light curing machine;
[0011] At the same time, after the adhesive is cooled and solidified, the pre-coated film is placed on the conveyor for transportation;
[0012] Unwinders are arranged on both the upper and lower sides of the pre-coated film, and a protective layer is arranged on the unwinder to perform a static electricity removal operation on the protective layer;
[0013] The upper and lower protective layers are conveyed simultaneously, and the protective layers are attached to the surfaces of the adhesive layer and the wear-resistant coating;
[0014] After lamination, the film is rolled up by a winder to complete the production of pre-coated film;
[0015] When it is needed, unroll it and cut it as needed, and tear off the protective layer before use.
[0016] Wherein, in the step of maintaining the temperature of the adhesive during the coating process:
[0017] Keep the temperature of the adhesive at 80-100°C.
[0018] Among them, in the step of adding UV coating, anti-adhesive agent and silicon dioxide in a mixer and stirring:
[0019] The stirring time was 1 h and the stirring rate was 300 rpm.
[0020] Wherein, the adhesive is hot melt adhesive, the base material layer is BOPP film, and the protective layer is PE protective film.
[0021] The present invention also provides a scratch-resistant pre-coated film production device, which uses the above-mentioned scratch-resistant pre-coated film production device, including a box body, a pre-coated film unwinder, a pre-coated film winder, two protective layer unwinders and a laminating unit, the pre-coated film unwinder and the pre-coated film winder are symmetrically arranged at the two ends of the box body, the pre-coated film unwinder and the pre-coated film winder are provided with a substrate layer, the two protective layer unwinders are fixedly connected to the box body and are symmetrically distributed on both sides of the substrate layer, the protective layer unwinder is provided with a protective layer, and the laminating unit is arranged on the box body.
[0022] The scratch-resistant pre-coated film production device further includes two static eliminators, both of which are arranged inside the box and are respectively located on one side of the corresponding protective layer unwinding machine.
[0023] Among them, the bonding unit includes a first cylinder, a frame, multiple second cylinders, multiple support blocks, multiple slides and two rollers, the first cylinder is fixedly connected to the box and is located above the box, the output end of the first cylinder passes through the box and is fixedly connected to the frame, the frame has two first slide grooves, multiple second cylinders are fixedly connected to the frame and are sequentially distributed on both sides of the frame, the output ends of multiple second cylinders are respectively fixedly connected to the corresponding support blocks, one end of multiple slides is respectively fixedly connected to the corresponding support blocks, the other end of multiple slides is slidably connected to the first slide groove, the two ends of the two rollers are respectively rotatably connected to the corresponding slides, and the two rollers are symmetrically arranged on both sides of the substrate layer.
[0024] The present invention discloses a production process and device for a scratch-resistant pre-coated film. The adhesive is taken out and placed in a heating box. After being heated to 100°C, the adhesive is evenly applied to one side of a substrate layer by a glue coating machine. The temperature of the adhesive is maintained during the coating process. Polypropylene polymer is used as a raw material. UV coating, anti-adhesive agent and silicon dioxide are sequentially added to a mixer for stirring to obtain a wear-resistant coating. The wear-resistant coating is evenly applied to the other side of the substrate layer, and a light curing machine is used for curing. After the adhesive is cooled and cured, the pre-coated film is placed on a conveyor for transportation. Unwinders are arranged on both the upper and lower sides of the pre-coated film, and a protective layer is arranged on the unwinder to remove static electricity from the protective layer. The upper and lower protective layers are conveyed simultaneously, and the surfaces of the adhesive layer and the wear-resistant coating are coated with a protective layer. Laminating the protective layer; after lamination, it is reeled up by a winder to complete the production of the pre-coated film; when it is needed, it is unrolled and cut as needed, and the protective layer can be torn off before use; the temperature during application determines the melting state and leveling performance of the hot melt adhesive, so it is necessary to maintain it at 80-100°C to avoid uneven application. The flexibility, wear resistance, scratch resistance and durability of the wear-resistant coating can be improved by UV coating, and the adhesion between plastic films can be prevented by anti-adhesion agents, which are wax, fatty acid metal salts or calcium carbonate. Silica can improve the structural strength of the wear-resistant coating and further improve the wear resistance and scratch resistance, thereby improving the scratch resistance of the pre-coated film, reducing scratches during use, and ensuring the beauty and service life of the product. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art are briefly introduced below.
[0026] Figure 1 It is a schematic structural diagram of the second embodiment of the present invention.
[0027] Figure 2 is a cross-sectional view of a second embodiment of the present invention.
[0028] Figure 3 The present invention Figure 2 AA line section view.
[0029] Figure 4 The present invention Figure 2 Enlarged view of the local structure at point B.
[0030] Figure 5 It is a schematic structural diagram of the cutting assembly of the present invention.
[0031] Figure 6 It is a structural schematic diagram of the segmentation component of the present invention.
[0032] Figure 7It is a cross-sectional view of the splitting assembly of the present invention.
[0033] Figure 8 It is a top view of the segmentation assembly of the present invention.
[0034] Fig. 9 It is a flow chart of the steps of the scratch-resistant pre-coated film production process of the present invention.
[0035] 101-box, 102-pre-coated film unwinder, 103-pre-coated film winder, 104-protective layer unwinder, 105-base material layer, 106-protective layer, 107-static eliminator, 108-first cylinder, 109-frame, 110-second cylinder, 111-support block, 112-slide plate, 113-roller, 114-first slide groove, 201-electronic slide rail, 202-first slider, 203-third cylinder, 204-cutting blade, 301-support plate, 302-second slide groove, 303-second slider, 304-fourth cylinder, 305-moving block, 306-fifth cylinder, 307-third slider, 308-third slide groove, 309-sixth cylinder, 310-mounting plate, 311-dividing blade. DETAILED DESCRIPTION
[0036] Embodiments of the present invention are described in detail below. Examples of the embodiments are shown in the accompanying drawings. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, but should not be construed as limiting the present invention.
[0037] First embodiment
[0038] See also Fig. 9 ,in Fig. 9 The present invention provides a process for producing a scratch-resistant pre-coated film, comprising the following steps:
[0039] S1: Take out the adhesive, place it in a heating box, heat it to 100° C., and then evenly apply it on one side of the substrate layer 105 using a glue coating machine;
[0040] S2: Maintain the temperature of the adhesive during the coating process, keeping the temperature of the adhesive at 80-100°C;
[0041] S3: Using high molecular weight polypropylene as raw material, UV coating, anti-adhesive agent and silica were added into a mixer in sequence and stirred for 1 hour at a stirring rate of 300 rpm to obtain a wear-resistant coating;
[0042] S4: uniformly coating the wear-resistant coating on the other side of the substrate layer 105, and performing a curing operation using a light curing machine;
[0043] S5: After the adhesive is cooled and solidified, the pre-coated film is placed on a conveyor for transportation;
[0044] S6: Unwinders are arranged on both the upper and lower sides of the pre-coated film, a protective layer 106 is arranged on the unwinders, and a static electricity removal operation is performed on the protective layer 106;
[0045] S7: The upper and lower protective layers 106 are conveyed simultaneously, and the protective layers 106 are attached to the surfaces of the adhesive layer and the wear-resistant coating;
[0046] S8: After lamination, the film is rolled up by a winder to complete the production of the pre-coated film;
[0047] S9: When it is needed, unwind it and cut it as needed, and tear off the protective layer 106 before use.
[0048] Among them, first take out the adhesive and place it in a heating box, heat it to 100°C, and then evenly apply it on one side of the substrate layer 105 through a glue coating machine; maintain the temperature of the adhesive during the coating process; use high molecular weight polypropylene as a raw material, add UV coating, anti-adhesion agent and silica in a mixer in sequence and stir to obtain a wear-resistant coating; evenly apply the wear-resistant coating on the other side of the substrate layer 105, and use a light curing machine to perform a curing operation; at the same time, after the adhesive is cooled and cured, place the pre-coated film on a conveyor for transportation; unwinders are set on both the upper and lower sides of the pre-coated film, and a protective layer 106 is set on the unwinder, and the protective layer 106 is subjected to a static electricity removal operation; the upper and lower protective layers 106 are conveyed at the same time, and the protective layer 106 is laminated on the surface of the adhesive layer and the wear-resistant coating; after laminating, it is rolled up by a winder to complete the production of the pre-coated film; when it is needed, it is unrolled and cut according to needs, and the protective layer 106 can be torn off before use;
[0049] The temperature during application determines the melting state and leveling performance of the hot melt adhesive, so it needs to be kept at 80-100°C to avoid uneven application. UV coating can improve the flexibility, wear resistance, scratch resistance and durability of the wear-resistant coating. Anti-adhesion agents can prevent adhesion between plastic films. Anti-adhesion agents are wax, fatty acid metal salts or calcium carbonate. Silica can improve the structural strength of the wear-resistant coating and further improve the wear resistance and scratch resistance.
[0050] Second embodiment
[0051] See also Figures 1 to 4 ,in Figure 1 is a schematic structural diagram of a second embodiment of the present invention, Figure 2 is a cross-sectional view of a second embodiment of the present invention, Figure 3 The present invention Figure 2 AA line section view, Figure 4 The present invention Figure 2The present invention provides a scratch-resistant pre-coated film production device, comprising a box 101, a pre-coated film unwinder 102, a pre-coated film winder 103, two protective layer unwinders 104, a laminating unit and two static eliminators 107, wherein the laminating unit comprises a first cylinder 108, a frame 109, a plurality of second cylinders 110, a plurality of support blocks 111, a plurality of slide plates 112 and two rollers 113.
[0052] Among them, the pre-coated film unwinder 102 and the pre-coated film winder 103 are symmetrically arranged at the two ends of the box body 101, and the pre-coated film unwinder 102 and the pre-coated film winder 103 are provided with a substrate layer 105, the two protective layer unwinders 104 are fixedly connected to the box body 101 and are symmetrically distributed on both sides of the substrate layer 105, the protective layer unwinder 104 is provided with a protective layer 106, and the laminating unit is arranged on the box body 101. The box body 101 supports the entire device, the pre-coated film unwinder 102 can unwind the substrate layer 105 coated with the wear-resistant coating and the adhesive layer, the pre-coated film winder 103 can wind up the substrate layer 105 bonded with the protective layer 106, and the protective layer unwinder 104 unwinds the protective layer 106 and then transports it to both sides of the substrate layer 105. Then, through the bonding unit, the two protective layers 106 are respectively bonded to both sides of the substrate layer 105, that is, on the outer surfaces of the adhesive layer and the wear-resistant coating.
[0053] Secondly, the two static eliminators 107 are both arranged inside the box 101 and are respectively located on one side of the corresponding protective layer unwinding machine 104. The static eliminator 107 can eliminate static electricity on the protective layer 106 when it is unwinding, so as to avoid the absorption of dust and debris on the protective layer 106 due to static electricity, thereby affecting the lamination quality and effect.
[0054] At the same time, the first cylinder 108 is fixedly connected to the box body 101 and is located above the box body 101. The output end of the first cylinder 108 passes through the box body 101 and is fixedly connected to the frame 109. The frame 109 has two first slide grooves 114. Multiple second cylinders 110 are fixedly connected to the frame 109 and are sequentially distributed on both sides of the frame 109. The output ends of multiple second cylinders 110 are respectively fixedly connected to the corresponding support blocks 111, one ends of multiple slide plates 112 are respectively fixedly connected to the corresponding support blocks 111, and the other ends of multiple slide plates 112 are slidably connected to the first slide groove 114. The two ends of the two roller bodies 113 are respectively rotatably connected to the corresponding slide plates 112, and the two roller bodies 113 are symmetrically arranged on both sides of the substrate layer 105. The frame 109 supports the second cylinder 110, and the first cylinder 108 is started to drive the frame 109 to move downward, and adjust the position in the box 101 so that the substrate layer 105 is located in the center of the frame 109. Then the second cylinder 110 is started to drive the support block 111 and the slide plate 112 to move. The slide plate 112 slides in the first slide groove 114, so that the two rollers 113 move relative to each other, and then the rollers 113 and the substrate layer 105 come into contact and roll, rolling the two protective layers 106 to flatten the protective layers 106.
[0055] When using a scratch-resistant pre-coated film production process of the present embodiment, the pre-coated film unwinding machine 102 can unwind the substrate layer 105 coated with the wear-resistant coating and the adhesive layer, and the protective layer unwinding machine 104 unwinds the protective layer 106. When the protective layer 106 is then transported to both sides of the substrate layer 105, the first cylinder 108 is started to drive the frame 109 to move downward, and the position in the box 101 is adjusted so that the substrate layer 105 is located at the center of the frame 109. Then, the second cylinder 110 is started to drive the support block 111 and the slide plate 112 to move. The slide plate 112 is moved on the first slide. The groove 114 slides, causing the two roller bodies 113 to move relative to each other, and then the roller bodies 113 roll in contact with the substrate layer 105, rolling the two protective layers 106, flattening the protective layers 106, and respectively attaching the two protective layers 106 to the two sides of the substrate layer 105, that is, to the outer surfaces of the adhesive layer and the wear-resistant coating. Finally, the pre-coated film winder 103 can rewind the substrate layer 105 with the protective layer 106 attached. Through the above-mentioned structural arrangement, the protective layer 106 of the pre-coated film can be attached and rewound without manual operation, thereby improving the production efficiency of the pre-coated film.
[0056] See also Figure 5 ,in Figure 5101 is a schematic diagram of the structure of the cutting assembly of the present invention. The scratch-resistant pre-coated film production device further includes a cutting assembly, which is arranged inside the box 101.
[0057] The cutting assembly includes an electronic slide rail 201, a first slider 202, a third cylinder 203 and a cutting blade 204. The electronic slide rail 201 is fixedly connected to the box body 101 and is located on the inner top wall of the box body 101. The first slider 202 is slidably connected to the electronic slide rail 201. The third cylinder 203 is fixedly connected to the first slider 202 and is located below the first slider 202. The output end of the third cylinder 203 is fixedly connected to the cutting blade 204.
[0058] When using a scratch-resistant pre-coated film production process of the present embodiment, the electronic slide rail 201 is started, driving the first slider 202 to move, so that the third cylinder 203 and the cutting blade 204 move in the box 101, and the cutting position is adjusted. Then the third cylinder 203 is started, driving the cutting blade 204 to move, and the protective layer 106 and the substrate layer 105 can be cut, so that the pre-coated film can be cut when the pre-coated film winder 103 needs to be replaced. Then the staff can re-dock the cut pre-coated film with the new pre-coated film winder 103 and continue to wind it. In this way, the pre-coated film can be automatically cut without manual operation, thereby improving production efficiency.
[0059] See also Figures 6 to 8 , Figure 6 is a schematic diagram of the structure of the segmentation component of the present invention, Figure 7 is a cross-sectional view of a splitting assembly of the present invention, Figure 8 It is a top view of the segmentation assembly of the present invention.
[0060] The scratch-resistant pre-coated film production device also includes a splitting component, and the splitting component is arranged on the box body.
[0061] The splitting assembly includes a support plate 301, a second slide groove 302, a plurality of second sliders 303, a fourth cylinder 304, a moving block 305, a plurality of fifth cylinders 306, a third slider 307 and a plurality of splitting units, wherein the support plate 301 has a third slide groove 308, the support plate 301 is fixedly connected to the box body and is located above the box body, the second slide groove 302 is fixedly connected to the support plate 301 and is located below the support plate 301, a plurality of second sliders 303 are all slidably connected to the second slide groove 302, the fourth cylinder 304 is fixedly connected to the box body and is located The box is close to one side of the pre-coated film winder, the output end of the fourth cylinder 304 is fixedly connected to the moving block 305, and the plurality of fifth cylinders 306 are all rotatably connected to the moving block 305 and are sequentially distributed on the outside of the moving block 305, the output ends of the plurality of fifth cylinders 306 are respectively rotatably connected to the corresponding second sliders 303, one end of the third slider 307 is slidably connected to the third slide groove 308, and the other end of the third slider 307 is fixedly connected to the moving block 305, and the plurality of splitting units are respectively arranged below the corresponding second sliders 303.
[0062] The splitting unit includes a sixth cylinder 309, a mounting plate 310 and a splitting blade 311. The sixth cylinder 309 is fixedly connected to the second slider 303 and is located below the second slider 303. The output end of the sixth cylinder 309 is fixedly connected to the mounting plate 310, and the splitting blade 311 is bolted to the bottom of the mounting plate 310.
[0063] Among them, the support plate 301 supports the second slide groove 302, and the fourth cylinder 304 is started, which can drive the moving block 305 to move, and the third slider 307 slides in the third slide groove 308 to improve stability, so that the moving block 305 can adjust the inclination angles of multiple fourth cylinders 304, and the fourth cylinder 304 is started, and the output end drives the second slider 303 to slide in the second slide groove 302, so as to adjust the spacing of multiple segmentation units. When the segmentation unit is started, the pre-coated film can be divided into multiple parts for later use; when the sixth cylinder 309 is started, it can drive the segmentation blade 311 to move downward, and then the pre-coated film is continuously transported and rolled up, and it is segmented. The installation package installs and fixes the segmentation blade 311. Through the above-mentioned structural setting, the spacing between the multiple segmentation blades 311 can be freely adjusted, and the pre-coated film can be segmented into different widths, which has high flexibility in use.
[0064] What is disclosed above is only one or more preferred embodiments of the present application, and cannot be used to limit the scope of rights of the present application. Ordinary technicians in this field can understand that all or part of the processes of implementing the above embodiments and equivalent changes made according to the claims of the present application are still within the scope covered by the present application.
Claims
1. A scratch-resistant pre-coated film production process, characterized in that: The steps include: Take out the adhesive, place it in a heating box, heat it to 100°C, and evenly apply it on one side of the substrate layer using a glue coating machine; Maintaining the temperature of the adhesive during coating; Using high molecular weight polypropylene as raw material, UV coating, anti-adhesive agent and silicon dioxide are added in a mixer in sequence and stirred to obtain a wear-resistant coating; Evenly apply the wear-resistant coating on the other side of the substrate layer, and perform a curing operation using a light curing machine; At the same time, after the adhesive is cooled and solidified, the pre-coated film is placed on the conveyor for transportation; Unwinders are arranged on both the upper and lower sides of the pre-coated film, and a protective layer is arranged on the unwinder to perform a static electricity removal operation on the protective layer; The upper and lower protective layers are conveyed simultaneously, and the protective layers are attached to the surfaces of the adhesive layer and the wear-resistant coating; After lamination, the film is rolled up by a winder to complete the production of pre-coated film; When it is needed, unroll it and cut it as needed, and tear off the protective layer before use.
2. The scratch-resistant pre-coated film production process according to claim 1, characterized in that: In the steps to maintain the temperature of the adhesive during the coating process: Keep the temperature of the adhesive at 80-100°C.
3. The scratch-resistant pre-coated film production process according to claim 2, characterized in that: In the step of adding UV coating, anti-adhesive agent and silica to the mixer in sequence and stirring: The stirring time was 1 h and the stirring rate was 300 rpm.
4. The process for producing a scratch-resistant pre-coated film according to claim 3, characterized in that: The adhesive is hot melt adhesive, the substrate layer is a BOPP film, and the protective layer is a PE protective film.
5. A scratch-resistant pre-coated film production device, using the scratch-resistant pre-coated film production process according to claim 4, characterized in that: It includes a box body, a pre-coated film unwinder, a pre-coated film winder, two protective layer unwinders and a laminating unit. The pre-coated film unwinder and the pre-coated film winder are symmetrically arranged at both ends of the box body. The pre-coated film unwinder and the pre-coated film winder are provided with a substrate layer. The two protective layer unwinders are fixedly connected to the box body and are symmetrically distributed on both sides of the substrate layer. The protective layer unwinder is provided with a protective layer, and the laminating unit is arranged on the box body.
6. The scratch-resistant pre-coated film production device according to claim 5, characterized in that: The scratch-resistant pre-coated film production device also includes two static eliminators, which are both arranged inside the box and located on one side of the corresponding protective layer unwinding machine.
7. The scratch-resistant pre-coated film production device according to claim 6, characterized in that: The bonding unit includes a first cylinder, a frame, multiple second cylinders, multiple support blocks, multiple slides and two rollers. The first cylinder is fixedly connected to the box and is located above the box. The output end of the first cylinder passes through the box and is fixedly connected to the frame. The frame has two first slide grooves. Multiple second cylinders are fixedly connected to the frame and are sequentially distributed on both sides of the frame. The output ends of multiple second cylinders are respectively fixedly connected to the corresponding support blocks, one end of multiple slides is respectively fixedly connected to the corresponding support blocks, the other end of multiple slides is slidably connected to the first slide groove, the two ends of the two rollers are respectively rotatably connected to the corresponding slides, and the two rollers are symmetrically arranged on both sides of the substrate layer.
Citation Information
Patent Citations
Anti-wear matt pre-coating film, preparation method and applications thereof
CN105176429A
Laminating machine
CN203267400U
PC film double-sided compounding device
CN209851767U
Full-automatic film laminating machine
CN213081658U
Folding anti-static BOPP (biaxially-oriented polypropylene) pre-coating film
CN214881260U