Method for improving measurement stability of cold rolling mill inlet thickness gauge

By setting up a purge pipeline and a compressed gas delivery pipe at the inlet of the cold rolling mill, the impact of rolling flue gas and lubricating liquid on the thickness gauge is solved, and the measurement stability and accuracy are improved.

CN119035279AActive Publication Date: 2024-11-29CHINALCO RUIMIN CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411287998.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-14
Publication Date
2024-11-29
Estimated Expiration
2044-09-14

AI Technical Summary

Technical Problem

When the cold rolling mill is working, the flue gas and lubricating fluid generated by the rolling roll affect the measurement accuracy of the thickness gauge, resulting in poor measurement stability.

Method used

It is designed to set up a purge pipeline in the conveying direction of the strip material to transport compressed gas to purge oil on the surface of the strip material, and to form a positive pressure inside the thickness gauge through the compressed gas delivery pipe to prevent flue gas and oil from entering the thickness gauge.

Benefits of technology

Effectively reduce the impact of oil on measurement accuracy, improve measurement stability, prevent flue gas from entering the thickness gauge, and enhance measurement accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119035279A_ABST
    Figure CN119035279A_ABST
Patent Text Reader

Abstract

The invention relates to a method for improving the measurement stability of a thickness gauge at an inlet of a cold rolling mill, a purging pipeline is arranged between the thickness gauge and an input roller group, and the thickness gauge is connected with a compressed gas conveying pipe; the method comprises the steps that a strip passes through the input roller set, the thickness gauge, the tensioning roller set and the rolling roller set, the tensioning roller set presses the strip downwards, the blowing pipeline conveys compressed gas to the left side below the ray emitting end of the thickness gauge, the compressed gas blows oil on the surface of the strip, the compressed gas conveying pipe conveys the compressed gas to the interior of the thickness gauge, and the rolling roller set presses the strip downwards. Positive pressure is formed in the thickness gauge, and smoke generated when the strip is rolled by the rolling roller set is prevented from entering the thickness gauge. Oil on the surface of the strip is blown through compressed gas, oil on the surface of the strip is reduced, it is effectively avoided that the oil leaks to the thickness gauge, and then the measurement precision of the thickness gauge is affected, meanwhile, gas is introduced into the thickness gauge to form positive pressure, smoke cannot enter the thickness gauge, and it is avoided that the smoke influences the measurement precision.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for improving the measurement stability of a cold rolling mill entrance thickness gauge. Background Art

[0002] When the cold rolling mill is working, a thickness gauge is usually installed at the entrance to measure the thickness of the strip. The cold rolling mill will generate a lot of smoke when rolling the strip, and the rollers need to spray coolant and lubricant when working. However, when the cold rolling mill is working, the rollers generate a lot of smoke when rolling the strip, which will affect the measurement accuracy of the thickness gauge. At the same time, the coolant and lubricant on the rollers are easy to leak along the strip to the bottom of the ray emitting end of the thickness gauge. The thickness gauge relies on emitting rays and receiving feedback rays to achieve thickness measurement. When there is oil on the surface of the strip, the rays emitted by the thickness gauge will be blocked by the oil. At this time, the detection accuracy of the thickness gauge will be affected, making the measurement stability of the thickness gauge less than ideal. For this reason, it is necessary to make improvements to the above technical problems to improve the measurement stability of the thickness gauge, and this case arises from this. Summary of the invention

[0003] The present invention makes improvements on the problems existing in the above-mentioned prior art, that is, the technical problem to be solved by the present invention is to provide a method for improving the measurement stability of a thickness gauge at the entrance of a cold rolling mill, which has a reasonable design and can improve the measurement stability of the thickness gauge.

[0004] In order to achieve the above-mentioned purpose, the technical scheme adopted by the present invention is: a method for improving the measurement stability of a thickness gauge at the entrance of a cold rolling mill, comprising an input roll group, a thickness gauge, a liftable tensioning roll group and a rolling roll group arranged in sequence from right to left along the conveying direction of the strip, a purge pipeline located above the strip is arranged between the thickness gauge and the input roll group, and the purge pipeline conveys compressed gas toward the lower left side of the ray emitting end of the thickness gauge; the thickness gauge is connected to a compressed gas conveying pipe; the method is: the strip passes through the input roll group, the thickness gauge, the tensioning roll group and the rolling roll group in sequence from right to left, the tensioning roll group presses down the strip, the purge pipeline conveys compressed gas toward the lower left side of the ray emitting end of the thickness gauge, the compressed gas conveyed by the purge pipeline purges the oil on the surface of the strip, and the compressed gas conveying pipe conveys compressed gas toward the inside of the thickness gauge, so that a positive pressure is formed inside the thickness gauge to prevent the smoke generated when the rolling roll group rolls the strip from entering the inside of the thickness gauge.

[0005] Furthermore, when the thickness of the strip is greater than 1 mm, the pressure of the compressed gas transported by the purge pipeline is 5 bar; when the thickness of the strip is less than 1 mm, the pressure of the compressed gas transported by the purge pipeline is 3 bar.

[0006] Furthermore, the positive pressure formed inside the thickness gauge is 0.5 bar.

[0007] Furthermore, the angle between the output port of the purge pipeline and the horizontal plane is 30 degrees.

[0008] Furthermore, the compressed gases transported by the purge pipeline and the compressed gas delivery pipe are all dried and dehydrated gases.

[0009] Furthermore, a protection frame is provided on the right side of the thickness gauge, the lower end of the protection frame extends to below the ray emitting end of the thickness gauge, and the protection frame is driven by a longitudinal moving component to move forward and backward.

[0010] Compared with the prior art, the present invention has the following effects: the present invention is reasonably designed, and compressed gas is delivered to the left side below the ray emitting end of the thickness gauge through the purging pipeline, and the compressed gas purges the oil on the surface of the strip, thereby reducing the oil on the surface of the strip, effectively avoiding the leakage of oil to the bottom of the ray emitting end of the thickness gauge during the rolling process, thereby affecting the measurement accuracy of the thickness gauge, and improving the measurement stability; at the same time, gas is introduced into the thickness gauge to form a positive pressure, so that the smoke generated during the rolling of the strip cannot enter the thickness gauge, thereby avoiding the smoke from affecting the measurement accuracy of the thickness gauge. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is a schematic diagram of the structure of an embodiment of the present invention. DETAILED DESCRIPTION

[0012] The present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.

[0013] In the description of the present invention, it should be understood that the terms "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0014] like Figure 1As shown, the present invention provides a method for improving the measurement stability of a thickness gauge at the entrance of a cold rolling mill, comprising an input roller group 2, a thickness gauge 3, a liftable tensioning roller group 4 and a rolling roller group 5 which are sequentially arranged from right to left along the conveying direction of a strip 1, the strip 1 passes through the input roller group 2, the thickness gauge 3, the tensioning roller group 4 and the rolling roller group 5 in sequence from right to left, the input roller group 2 conveys the strip 1 from right to left, the thickness gauge 3 measures the thickness of the strip, the tensioning roller group 4 presses down the strip, and the rolling roller group 5 cold rolls the strip, all of which are consistent with the existing cold rolling The structure on the machine is the same, and the specific improvements are: a purge pipeline 6 located above the strip 1 is arranged between the thickness gauge 3 and the input roller group 2, and the purge pipeline 6 is inclined with the left end low and the right end high. The purge pipeline 6 transports compressed gas to the left side below the ray emitting end of the thickness gauge 3, and the compressed gas is used to purge the oil on the surface of the strip 1; the thickness gauge 3 is connected to the compressed gas delivery pipe 7, and the compressed gas delivery pipe 7 is used to input compressed gas into the thickness gauge 3 so that a positive pressure is formed inside the thickness gauge. The method for improving the measurement stability of the thickness gauge at the entrance of the cold rolling mill is as follows: the strip 1 passes through the input roller group 2, the thickness gauge 3, the tensioning roller group 4 and the rolling roller group 5 from right to left in sequence, the tensioning roller group 4 presses down the strip, and the purge pipeline 6 delivers compressed gas to the left side below the ray emitting end of the thickness gauge 3. The compressed gas delivered by the purge pipeline 6 purges the oil on the surface of the strip 1 to reduce the oil on the surface of the strip, effectively avoiding the leakage of oil to the bottom of the ray emitting end of the thickness gauge during the rolling process, thereby affecting the measurement accuracy of the thickness gauge, and improving the measurement stability; and the compressed gas delivery pipe 7 delivers compressed gas to the inside of the thickness gauge 3, so that a positive pressure is formed inside the thickness gauge, so that the smoke generated when the rolling roller group rolls the strip enters the inside of the thickness gauge, and the smoke is avoided. The influence of the measurement accuracy of the thickness gauge.

[0015] During the operation of the cold rolling mill, when the thickness of the strip is large, the downward pressure of the tensioning roller group is shallow. At this time, a relatively large pressure is required for blowing to ensure that the oil can be blown clean; when the thickness of the strip is small, the downward pressure of the tensioning roller group is deep, and the strip forms a concave curved shape. At this time, the oil on the surface of the strip can partially flow out from the front and rear sides. At this time, a relatively small pressure can be used for blowing to avoid splashing back to the thickness gauge due to excessive gas pressure. Based on this, in this embodiment, when the thickness of the strip 1 is greater than or equal to 1mm, the pressure of the compressed gas delivered by the purge pipeline 6 is 5bar; when the thickness of the strip 1 is less than 1mm, the pressure of the compressed gas delivered by the purge pipeline 6 is 3bar.

[0016] In this embodiment, when the compressed gas delivery pipe 7 delivers compressed gas to the inside of the thickness gauge 3 to form a positive pressure, the positive pressure formed inside the thickness gauge can be 0.5 bar. At this time, the pressure inside the thickness gauge is greater than the external pressure, and the smoke generated by rolling cannot enter the thickness gauge. It should be noted that the thickness gauge should be sealed in advance.

[0017] In this embodiment, in order to improve the purging effect, the angle between the output port of the purging pipeline 6 and the horizontal plane is 30 degrees, that is, the purging pipeline adopts an inclined purging method.

[0018] In this embodiment, the compressed gas delivered by the purge pipeline 6 and the compressed gas delivery pipe 7 is dried and dehydrated compressed gas.

[0019] In this embodiment, a protection frame 8 is provided on the right side of the thickness gauge 3, the lower end of the protection frame 8 extends to below the ray emitting end of the thickness gauge 3, and the protection frame is driven by the longitudinal moving assembly to move forward and backward. By providing the protection frame, it is possible to effectively avoid the situation where the strip hits the thickness gauge during the strip threading process (the strip passes through the input roller group) when the cold rolling mill just starts working.

[0020] In this embodiment, the input roller group 2 is two input rollers distributed up and down. The tensioning roller group 4 includes three first tensioning rollers 12, second tensioning rollers 13 and third tensioning rollers 14 arranged from left to right. The second tensioning roller is driven to rise and fall by the upper lifting assembly 9, and the first tensioning roller and the third tensioning roller are driven to rise and fall by the lower lifting assembly 10. The upper lifting assembly and the lower lifting assembly are respectively connected to the solenoid valve to facilitate the control of the lifting distance. It should be noted that when in use, the lifting distance of the three tensioning rollers when the thickness of the strip is greater than or equal to 1mm and the lifting distance of the three tensioning rollers when the thickness of the strip is less than 1mm are set in advance, and they can be switched according to the thickness of the strip when the cold rolling mill starts working.

[0021] In this embodiment, the rolling roller group 5 is two rolling rollers distributed up and down, and a cooling liquid and lubricating liquid spraying pipeline 11 is arranged on the right side of each rolling roller.

[0022] It should be noted that the thickness gauge is an existing mature product. Its ray emitting end and ray reflecting end are distributed upward and downward, and the strip passes between the two. Its specific structure and detection principle will not be repeated here.

[0023] If the present invention discloses or involves components or structures that are fixedly connected to each other, then, unless otherwise stated, the fixed connection can be understood as: a detachable fixed connection (for example, connection using bolts or screws), and can also be understood as: a non-detachable fixed connection (for example, riveting, welding). Of course, the mutual fixed connection can also be replaced by an integrated structure (for example, manufactured by one-piece molding using a casting process) (except when it is obviously impossible to use an one-piece molding process).

[0024] In addition, unless otherwise stated, the terms used to indicate positional relationships or shapes in any of the technical solutions disclosed in the present invention include states or shapes that are approximate, similar, or close to them.

[0025] Any component provided by the present invention may be assembled from a plurality of separate components, or may be a separate component manufactured by an integral forming process.

[0026] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, ordinary technicians in the field should understand that the specific implementation methods of the present invention can still be modified or some technical features can be replaced by equivalents without departing from the spirit of the technical solution of the present invention, which should be included in the scope of the technical solution for protection of the present invention.

Claims

1. A method for improving the measurement stability of a thickness gauge at the entrance of a cold rolling mill, comprising an input roller group, a thickness gauge, a lifting and lowering tensioning roller group and a rolling roller group arranged in sequence from right to left along the strip conveying direction, Features: A purge pipeline located above the strip is provided between the thickness gauge and the input roller group, and the purge pipeline conveys compressed gas toward the lower left side of the ray emitting end of the thickness gauge; the thickness gauge is connected to the compressed gas conveying pipe; the method is as follows: the strip passes through the input roller group, the thickness gauge, the tensioning roller group and the rolling roller group from right to left in sequence, the tensioning roller group presses down the strip, the purge pipeline conveys compressed gas toward the lower left side of the ray emitting end of the thickness gauge, the compressed gas conveyed by the purge pipeline purges the oil on the surface of the strip, and the compressed gas conveying pipe conveys compressed gas toward the inside of the thickness gauge, so that a positive pressure is formed inside the thickness gauge, and smoke generated when the rolling roller group rolls the strip is prevented from entering the inside of the thickness gauge.

2. A method for improving the measurement stability of a cold rolling mill entrance thickness gauge according to claim 1, Features: When the thickness of the strip is greater than 1 mm, the pressure of the compressed gas delivered by the purge pipeline is 5 bar; when the thickness of the strip is less than 1 mm, the pressure of the compressed gas delivered by the purge pipeline is 3 bar.

3. A method for improving the measurement stability of a cold rolling mill entrance thickness gauge according to claim 1, Features: The positive pressure formed inside the thickness gauge is 0.5 bar.

4. A method for improving the measurement stability of a cold rolling mill entrance thickness gauge according to claim 1, Features: The angle between the output port of the purge pipeline and the horizontal plane is 30 degrees.

5. A method for improving the measurement stability of a cold rolling mill entrance thickness gauge according to claim 1, Features: The compressed gases transported by the purge pipeline and the compressed gas delivery pipe are all dried and dehydrated gases.

6. A method for improving the measurement stability of a cold rolling mill entrance thickness gauge according to claim 1, Features: A protection frame is arranged on the right side of the thickness gauge, the lower end of the protection frame extends to below the ray emitting end of the thickness gauge, and the protection frame is driven by a longitudinal moving assembly to move forward and backward.

Citation Information

Patent Citations

  • Purging press ring device for cool rolling and foil rolling X-ray thickness tester

    CN103157674A

  • Rolled plate strip thickness detection device and control system

    CN112605133A

  • Thickness gauge stability detection device

    CN211100798U

  • A surface defect detection device for hot-rolled strip steel

    CN218835597U

  • KR20240002516A