Range preparation method of metastable-phase rare earth nickel-based oxide electronic phase change material

By providing homogeneous crystal nuclei for oxide raw materials and using high oxygen pressure conditions to prepare metastable rare earth nickel-based oxide ceramics, the problems of cumbersome preparation process and difficulty in bulk preparation in the existing technology are solved, and efficient and simple The ceramic preparation and performance regulation meet a variety of application needs.

CN119038995AActive Publication Date: 2024-11-29UNIV OF SCI & TECH BEIJING
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411058654.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-11-29
Estimated Expiration
2044-08-02

AI Technical Summary

Technical Problem

The prior art is difficult to quickly, efficiently and in large quantities in the preparation of metastable rare earth nickel-based oxide ceramics, which limits its application in fields such as strong correlation logic devices and mutant sensitive resistor devices.

Method used

By providing rare earth nickel-based oxide homogeneous crystal nuclei for oxide raw materials, the forward Gibbs free energy of the synthesis reaction is reduced, and metastable rare earth nickel-based oxide ceramics are prepared in a step under high oxygen pressure conditions, simplifying the process flow. Avoid additional removal of cosolvents to achieve bulk preparation.

Benefits of technology

It realizes efficient and simple preparation of high-quality metastable rare earth nickel-based oxide ceramics, reduces the preparation cost, meets the application needs of the mutation thermistor devices and infrared camouflage coatings, and regulates the hardness, morphology and Electric transport characteristics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119038995A_ABST
    Figure CN119038995A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation method of a metastable-phase rare earth nickel-based strong correlation oxide material, and belongs to the field of phase change materials and functional materials. According to the method, the target rare earth nickel-based oxide is used as homogeneous seed crystal, the heterogeneous nucleation process is promoted, and the forward Gibbs free energy of the synthesis reaction is reduced, so that the thermodynamic metastable-phase rare earth nickel-based oxide ceramic is prepared under the condition of high oxygen pressure. According to the invention, the distortion degree of NiO6 and BO6 octahedrons is influenced by regulating and controlling the types and proportions of Re-site and B-site elements, so that the phase transition temperature and the electrical transport characteristic of the metastable-phase rare earth nickel-based oxide are regulated and controlled; the synthesis pressure of the material can be remarkably reduced, the technological process for preparing the material is simplified, and the amount-released preparation of the metastable-phase rare earth nickel-based oxide is realized, so that the preparation requirements of strong correlation logic devices, mutation type sensitive resistance devices and infrared camouflage devices are met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the fields of oxide semiconductors, phase change materials and functional materials. Background Art

[0002] Among many oxide semiconductors, the metastable rare earth nickel-based oxide ReNiO3 has a typical CaTiO3 perovskite structure, in which Re is mainly rare earth and alkaline earth elements. ReNiO3 has a characteristic temperature (T MIT ) triggered metal-insulator phase transition characteristics, which MIT The above has an orthorhombic crystal structure (space group: Pbnm). At this time, the crystal structure of ReNiO3 is highly symmetric and the material is metallic. When the temperature is reduced to T MIT When the ReNiO3 changes to a monoclinic crystal structure (space group: P21 / n), the nickel element undergoes valence bond disproportionation and reduces the symmetry of the NiO6 octahedron, and the electrical transport properties of ReNiO3 change from metallic properties to semiconductor properties. [1-3] The electrical transport properties of metastable rare earth nickel-based oxides can be regulated by adjusting the type of Re-site elements. As the radius of the rare earth ions decreases, the degree of distortion of the NiO6 octahedron in ReNiO3 gradually increases, the stability of the semiconductor phase relative to the metal phase in the material increases, and the metal-insulator transition temperature T MIT Therefore, by designing the average ionic radius of the rare earth elements occupying the Re position of the ReNiO3 perovskite structure, T MIT Continuous adjustment in a wide temperature range. In practical applications, this feature helps to prepare a wide temperature range of mutation thermistor devices, which has considerable application value in the fields of strong correlation logic devices, infrared camouflage devices, etc. [4-6] .

[0003] At present, the synthesis of metastable rare earth nickel-based oxides must rely on high-pressure synthesis and high oxygen pressure solvent reaction methods. In the high-pressure synthesis method, rare earth oxides, NiO and KClO4 are first mixed and sealed in a platinum capsule; finally, a cylindrical graphite heater and a large press are used to synthesize the material at 950 ℃ and 6 GPa. In the high oxygen pressure solvent reaction method, the corresponding oxide raw materials are first weighed according to the stoichiometric ratio, the solvent is weighed in proportion and mixed with the oxide, and after the mixture is evenly mixed, it is placed in a high-pressure tube furnace to obtain a rare earth nickel-based oxide block at 800 ℃ and 7 MPa; the block is ground into powder, and the solvent and other water-soluble impurities are removed by water washing, ultrasound, and centrifugation. After drying, a metastable rare earth nickel-based oxide powder is obtained; a binder is added to the powder and cold pressed into a sheet, and then sintered under the same high oxygen pressure conditions to obtain a metastable rare earth nickel-based oxide ceramic. The existing methods for synthesizing metastable rare earth nickel-based oxides are complicated and require synthesis under high pressure at the GPa level or the removal of the co-solvent, and metastable rare earth nickel-based oxide ceramics cannot be obtained in one step. In addition, the high oxygen pressure co-solvent reaction method requires the co-solvent to completely dissolve the raw oxide, and the target output is limited by the amount of co-solvent used, which cannot meet the large-scale preparation of metastable rare earth nickel-based oxide ceramics.

[0004] In summary, the current field lacks an effective method for rapid, efficient and large-scale preparation of metastable rare earth nickel-based oxide ceramics, which limits the application of this material in strongly correlated logic devices and mutation-sensitive resistor devices.

[0005] [1]CATALAN G. Progress in perovskite nickelate research [J]. PhaseTransitions, 2008, 81(7-8): 729-49.

[0006] [2]MARíA LUISA M. Structural, magnetic and electronic properties of perovskites (R = rare earth) [J]. J Phys: Condens Matter, 1997, 9(8): 1679.

[0007] [3]VARIGNON J, GRISOLIA MN, ÍñIGUEZ J, et al. Complete phase diagram of rare-earth nickelates from first-principles [J]. npj Quantum Materials, 2017, 2 (1)

[0008] [4]SHAHSAFI A, RONEY P, ZHOU Y, et al. Temperature-independent thermal radiation [J]. Proc Natl Acad Sci USA, 2019, 116(52): 26402-6.

[0009] [5]TORRISS B, CHAKER M, MARGOT J. Electrical and Fourier transforminfrared properties of epitaxial SmNiO3 tensile strained thin film [J]. ApplPhys Lett, 2012, 101(9).

[0010] [6]GIRARDOT C, KREISEL J, PIGNARD S, et al. Raman scattering investigation across the magnetic and metal-insulator transition in rareearth nickelateRNiO3 (R=Sm, Nd) thin films [J]. Phys Rev B, 2008, 78(10) Summary of the invention

[0011] The purpose of the present invention is to provide a method for mass-producing metastable rare earth nickel-based oxide ceramics; the main idea is to provide rare earth nickel-based oxide homogeneous nuclei for oxide raw materials, promote the non-uniform nucleation and growth process of the crystals, reduce the forward Gibbs free energy of the synthesis reaction, thereby preparing metastable rare earth nickel-based oxide ceramics in one step without further removing the co-solvent, and can meet the potential application needs of sudden-type sensitive resistor devices.

[0012] A method for preparing a metastable rare earth nickel-based oxide material, characterized in that:

[0013] 1) designing a metastable rare earth nickel-based oxide material component according to target electrical transport and phase change characteristics, and selecting Re, Ni, and transition element precursors according to the selected material components and weighing them according to the target metastable rare earth nickel-based oxide stoichiometric ratio;

[0014] 2) weighing 0.1-50% molar ratio of the Ni element precursor as the target metastable rare earth nickel-based oxide as the nucleation seed crystal according to the amount of the precursor used, and fully mixing the seed crystal with the precursor and cold pressing them into sheets;

[0015] 3) Selecting the heat treatment temperature and oxygen pressure according to the target metastable rare earth nickel-based oxide: heating the cold-pressed reactants to a high temperature in a high oxygen pressure atmosphere and then keeping the temperature for 0.1-48 h, slowly cooling to room temperature after the temperature is maintained, taking out the sample, grinding it into powder, and cold-pressing it into a sheet again, heating it to a high temperature in a high oxygen pressure atmosphere and then keeping the temperature for 0.1-48 h, repeating the above operation 1-5 times until a pure metastable rare earth nickel-based oxide ceramic is obtained;

[0016] 4) Further introduce electrodes and other functional layer materials based on metastable rare earth nickel-based oxide ceramics to prepare mutation thermistor devices and strongly correlated logic devices; or grind into powder to prepare infrared camouflage coatings and laser protection coatings;

[0017] The above steps can realize the effective synthesis of rare earth nickel-based oxides with metal-insulator phase transition and hydrogen-induced electronic phase transition and in a thermodynamically metastable state. The method used does not contain any liquid phase substances, is easy to operate and can achieve large-scale preparation. By adjusting the ratio of precursor to seed crystal, oxygen partial pressure and heat treatment process, the hardness, morphology and electrical transport properties of metastable rare earth nickel-based oxide ceramics can be regulated.

[0018] Furthermore, the chemical composition of the synthesized metastable rare earth nickel-based oxide in step 1) is ReNi 1-x B x O3; wherein Re is a single rare earth element or a combination of multiple rare earth elements, including La, Pr, Nd, Sm, Eu, Gd, Dy, Ho, Er, Tm, Yb, Lu, Y; B is a single transition element or a combination of multiple transition elements, including Cr, Mn, Fe, Co; by designing the Re and B element components, the phase transition temperature and resistivity mutation degree of the rare earth nickel-based oxide metal insulator can be controlled. In a preferred embodiment, the sintered Nd 0.5 Sm 0.5 The electrical transport properties of NiO3 were characterized and the Nd 0.5 Sm 0.5 The phase transition temperature of NiO3 is around 300 K, which is within the phase transition temperature range of NdNiO3 and SmNiO3. 0.9 Mn 0.1 The electrical transport properties of O3 were characterized, and it was found that the doping of Mn element adjusted the phase transition temperature of NdNiO3 from around 200 K to around 100 K.

[0019] Furthermore, the precursors described in step 1) include oxides, carbonates, nitrates and acetates of rare earth, Ni and transition elements; for carbonate, nitrate and acetate precursors, the corresponding oxides of rare earth, Ni and transition elements can be obtained by pre-calcining and decomposition; the pre-calcining temperature should be 1-200°C higher than the decomposition temperature of the corresponding carbonate, nitrate and acetate; in a preferred embodiment, the raw materials for preparing EuNiO3 are Eu2O3, NiCO3 and EuNiO3 seed crystals, the decomposition temperature of NiCO3 is 270°C, and the NiCO3 powder is pre-calcined at 470°C and then mixed with other powders; in another preferred embodiment, the raw materials for preparing GdNiO3 are Gd2O3, Ni(CH3COO)2 and GdNiO3 seed crystals, the decomposition temperature of Ni(CH3COO)2 is 310°C, and the raw material powders are mixed and pre-calcined at 311°C.

[0020] Furthermore, the particle size of the metastable rare earth nickel-based oxide nucleation seed crystals described in step 2) is 0.1-100 μm, preferably 1-10 μm; by changing the size of the seed crystal grains, the non-uniform nucleation process can be regulated, thereby further regulating the purity, electrical transport properties and mechanical properties of the metastable rare earth nickel-based oxide ceramics; in a preferred embodiment, the raw material for preparing PrNiO3 is Pr6O 11 , NiO, and 10 μm PrNiO3 seed crystals, the raw materials are mixed evenly, and then a binder is added and cold pressed into a block; in another preferred embodiment, the raw materials for preparing NdNiO3 are Nd2O3, NiO, and 1 μm NdNiO3 seed crystals, the raw materials are mixed evenly, and then a binder is added and cold pressed into a block.

[0021] Furthermore, in step 3), the mechanical pressure range of the cold pressing process is 0.01-10 GPa, preferably 0.1-1 GPa; the density of the cold pressed block can be controlled by changing the mass of the powder sample, the size of the cold pressing mold and the pressure of the tablet press, thereby further controlling the thermodynamic process during sintering; in a preferred embodiment, the mechanical pressure of cold pressing when preparing PrNiO3 ceramics is 1 GPa, 0.2 g of raw material powder is weighed, a mold with a diameter of 6 mm is used, and the corresponding tablet press pressure is 3t; in another preferred embodiment, the preparation of Ho 0.8 Y 0.2 The mechanical pressure of cold pressing of NiO3 ceramics is 0.1 GPa. 2.2 g of raw material powder is weighed and a mold with a diameter of 20 mm is used, corresponding to a tablet press pressure of 3 t.

[0022] Furthermore, in the heating process of step 3), the temperature and time required for heating and heat preservation are jointly regulated by the ratio of precursor to seed crystal and the seed crystal particle size, and the heat preservation temperature is 300-1100 ° C. By changing the heat preservation temperature, the diffusion rate of the raw material and the non-uniform nucleation process can be regulated, thereby further regulating the mechanical properties of the rare earth nickel-based oxide ceramics, and the preferred heat preservation temperature is 800 ° C; the single heat preservation time is 0.1-48 h, and the purity of the metastable rare earth nickel-based oxide can be regulated by changing the heat preservation time, and the preferred single heat preservation time is 24 h; the oxygen pressure is 0.2-50 MPa, and the reaction thermodynamic process can be regulated by changing the oxygen pressure, thereby regulating the electrical transport properties of the rare earth nickel-based oxide ceramics, and the preferred oxygen pressure is 1-10 MPa; by grinding the sample into powder and sintering it multiple times, the degree of mixing of homogeneous crystal nuclei and oxide raw materials can be controlled, thereby further controlling the purity and electrical transport properties of rare earth nickel-based oxides, and the preferred sintering times are 1-5 times; in a preferred embodiment, the raw materials for preparing SmNiO3 are Sm2O3, NiO, and SmNiO3 seed crystals. After the raw materials are mixed evenly, a binder is added and cold pressed into sheets. After being kept at 800 °C for 24 h under an oxygen pressure of 1 MPa, SmNiO3 ceramics are obtained; in another preferred embodiment, NdNi is prepared 0.9 Fe 0.1 The raw materials of O3 are Nd2O3, NiO, Fe2O3, NdNi 0.9 Fe 0.1 O3 seed crystal, the raw materials were mixed evenly and then a binder was added and cold pressed into sheets, which were kept at 10 MPa oxygen pressure and 800 °C for 24 h. The sintered block was ground into powder, and then a binder was added and kept at 10 MPa oxygen pressure and 800 °C for 24 h. After repeating the above process 4 times, NdNi 0.9 Fe 0.1 O3 ceramics.

[0023] The present invention relates to a technical method for preparing thermodynamically metastable rare earth nickel-based oxide ceramics under high oxygen pressure conditions by using target rare earth nickel-based oxide as homogeneous seed crystals to promote non-uniform nucleation process and reduce forward Gibbs free energy of synthesis reaction. Compared with the traditional high-pressure synthesis method, the method can significantly reduce the synthesis pressure of the material and can synthesize thermodynamically metastable materials under MPa pressure; compared with the high oxygen pressure co-solvent reaction method, the method can simplify the process flow of material preparation, directly obtain high-quality rare earth nickel-based oxide ceramics, without the need to add additional co-solvents, reduce the preparation cost, and realize the mass preparation of metastable rare earth nickel-based oxides; the method can realize the regulation of the types and proportions of Re and B-site elements, affect the distortion degree of NiO6 and BO6 octahedrons, and thus realize the regulation of the phase transition temperature and electrical transport characteristics of metastable rare earth nickel-based oxides. The prepared ceramics can be applied to strongly correlated logic devices and mutation thermistor devices, and the prepared ceramics can be further ground into powder and applied to the preparation of infrared camouflage coatings and laser protective coatings. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 This is an X-ray diffraction diagram of PrNiO3 powder prepared by the seed crystal method proposed in the present invention. It can be seen that the main phase of the prepared powder is PrNiO3.

[0025] Figure 2 This is an X-ray diffraction diagram of SmNiO3 powder prepared by the seed crystal method proposed in the present invention. It can be seen that the main phase of the prepared powder is SmNiO3.

[0026] Figure 3 This is an X-ray diffraction diagram of GdNiO3 powder prepared by the seed crystal method proposed in the present invention. It can be seen that the main phase of the prepared powder is GdNiO3.

[0027] Figure 4 This is the electrical transport characteristic curve of NdNiO3 ceramics prepared by the seed crystal method proposed in the present invention. It can be seen that NdNiO3 ceramics have a metal-insulator transition near 200 K.

[0028] Figure 5 This is the electrical transport characteristic curve of the SmNiO3 ceramic prepared by the seed crystal method proposed in the present invention. It can be seen that the SmNiO3 ceramic has a metal-insulator transition near 400 K. DETAILED DESCRIPTION

[0029] Unless otherwise specified, the various raw materials used in the present invention can be obtained from the market or prepared according to conventional methods in the art. Unless otherwise defined or specified, all professional and scientific terms used herein have the same meanings as those familiar to those skilled in the art. In addition, any methods and materials similar or equivalent to those described herein can be applied to the method of the present invention.

[0030] Other aspects of the present invention will be apparent to those skilled in the art in view of the disclosure herein.

[0031] The present invention will be further described below in conjunction with specific examples. It should be understood that these examples are only used to illustrate the present invention and are not intended to limit the scope of the present invention. The experimental methods in the following examples without specifying specific conditions are usually carried out under conventional conditions or under conditions recommended by the manufacturer.

[0032] Example 1: The raw powders used in this experiment are Nd2O3, NiO, and NdNiO3. First, weigh the corresponding oxide powders according to the element ratio of Nd: Ni = 1: 1, pour the raw powders into an agate mortar and mix them, then add 1 μm NdNiO3 as a homogeneous seed crystal according to the ratio of Nd2O3: NdNiO3 = 1: 0.01 and continue to grind until uniform. Weigh 0.2 g of the mixed powder and add polyvinyl alcohol solution. After grinding and drying, apply 3 t of pressure to cold press into a 6 mm diameter disc. After pre-burning to remove polyvinyl alcohol, put it in a high pressure furnace and fill it with oxygen to 7 MPa. Raise the temperature to 800 ℃ and keep it warm for 24 h, and finally slowly cool it to room temperature. Take out the sintered block and grind it into a uniform and fine powder, add polyvinyl alcohol solution and cold press it into a sheet, and put it in a high pressure furnace after pre-burning, and fill it with oxygen to 7 MPa. Raise the temperature to 800 ℃ and keep it warm for 24 h, and finally slowly cool it to room temperature. Take out the sintered block and grind it into a uniform and fine powder, add polyvinyl alcohol solution and cold press it into a sheet, and put it in a high pressure furnace after pre-burning, and fill it with oxygen to 7 MPa. Raise the temperature to 800 ℃ and keep it warm for 24 h, and finally slowly cool it to room temperature. The above process is repeated 5 times to obtain NdNiO3 ceramics. Further introduction of electrodes into the ceramics can prepare mutation thermistor devices. Grinding the NdNiO3 ceramics into powder can also be further used in infrared camouflage coatings.

[0033] Example 2: The raw material powders used in this experiment are Pr6O 11 , NiO, PrNiO3. First, press Pr6O 11The oxide raw materials were weighed at a ratio of NiO: NiO = 1: 6, and 10 μm PrNiO3 powder was weighed as homogeneous seed crystals according to NiO: PrNiO3 = 1: 0.05. The above oxide raw materials and homogeneous seed crystals were poured into an agate mortar and mixed for 20 min. 0.2 g of the mixed powder was weighed and added with 2 drops of polyvinyl alcohol solution. After mixing evenly, 2.5 t pressure was applied to cold press into a 6 mm diameter disc. The disc was pre-sintered at 600 ° C in air for 2 h to remove the polyvinyl alcohol, and then kept at 800 ° C and 7 MPa oxygen pressure for 24 h. Finally, it was slowly cooled to room temperature to obtain PrNiO3 ceramics. The proportion of PrNiO3 phase in the sample was 96.26%, and repeated grinding and sintering were not required. Further introduction of electrodes into PrNiO3 ceramics can prepare magnetic electronic devices, and grinding PrNiO3 ceramics into powders can also be further used in infrared camouflage coatings.

[0034] Example 3: The raw material powders used in this experiment are Sm2O3, NiO, and SmNiO3 with a diameter of 1 μm. First, the oxide powders and homogeneous seed crystals are weighed in a ratio of Sm2O3: NiO: SmNiO3 = 1: 2: 0.04, the above raw materials are poured into an agate mortar and mixed evenly, and then loaded into a quartz tube, put into a high-pressure tube furnace, filled with 1 MPa oxygen pressure, kept at 800 ° C for 24 h, taken out, ground into powder, and added with polyvinyl alcohol solution. The powder is cold-pressed into a disc with a diameter of 6 mm by a tablet press under a pressure of 3 t, pre-sintered at 600 ° C in air for 4 h to remove polyvinyl alcohol, and then the disc is placed in a high-pressure tube furnace, kept at 800 ° C, 1 MPa oxygen pressure for 24 h, and then slowly cooled to room temperature to obtain SmNiO3 ceramics. Further introducing electrodes into SmNiO3 ceramics can produce mutation thermistor devices, and grinding SmNiO3 ceramics into powder can be further used in infrared camouflage coatings.

[0035] Example 4: The raw material powders used in this experiment are Sm2O3, Nd2O3, NiO, Nd 0.5 Sm 0.5 NiO3. First, weigh the corresponding oxide powder according to the element ratio of Nd: Sm: Ni = 1: 1: 1, pour it into the agate mortar and mix it evenly, then press NiO: Nd 0.5 Sm 0.5 Weigh Nd in a ratio of NiO3=1:0.1 0.5 Sm 0.5 NiO3, Nd 0.5 Sm 0.5After NiO3 is ball-milled to a particle size of 1 μm, it is added to an agate mortar and continued to be ground for 20 min. 0.2 g of the mixed powder is weighed and 1 drop of polyvinyl alcohol solution is added. After mixing and drying, it is poured into a mold with a diameter of 6 mm and cold-pressed into a sheet under a mechanical pressure of 2 GPa. After pre-sintering in air to remove polyvinyl alcohol, it is placed in a high-pressure tube furnace and kept at 800 °C for 24 h at 10 MPa oxygen pressure. After slowly cooling to room temperature, the block is taken out and ground into powder until the powder is uniform and fine. Polyvinyl alcohol solution is continued to be added and cold-pressed into a sheet. After keeping at 800 °C for 24 h at 10 MPa oxygen pressure, the block is taken out and ground into powder. 0.2 g of the powder is weighed and 4 drops of polyvinyl alcohol solution are added. After mixing evenly, it is cold-pressed into a disc with a diameter of 6 mm. It is pre-sintered at 600 °C for 4 h in air to remove polyvinyl alcohol. Finally, it is kept at 800 °C for 24 h at 10 MPa oxygen pressure. After slowly cooling to room temperature, Nd 0.5 Sm 0.5 NiO3 ceramics. 0.5 Sm 0.5 Further introduction of electrodes into NiO3 ceramics can produce mutation-type thermistor devices, and grinding the ceramics into powder can be further applied to infrared camouflage coatings.

[0036] Example 5: The powders used in this experiment are Nd2O3, NiO, MnO2, NdNi with a particle size of 10 μm 0.9 Mn 0.1 O3. First, weigh the oxide powder according to the ratio of Nd2O3:NiO:MnO2 =1:1.8:0.2, and then weigh the oxide powder according to the ratio of Nd2O3:NdNi 0.9 Mn 0.1 Weigh homogeneous seed crystals in a ratio of NdNiO3 =1:0.02 and use a ball mill to grind 0.9 Mn 0.1 O3 ball milled to a particle size of 1 μm, the above raw materials were poured into an agate mortar and mixed evenly, 0.2 g of powder was weighed and added with 2 drops of polyvinyl alcohol solution, mixed evenly, and then 3 t mechanical pressure was applied to cold press into a disc with a diameter of 6 mm, pre-sintered at 600 ° C in air for 4 h to remove polyvinyl alcohol, and the disc was placed in a high-pressure tube furnace filled with 7 MPa oxygen pressure, kept at 800 ° C for 24 h, slowly cooled to room temperature and taken out, the disc was ground into powder, added with adhesive and cold pressed into a sheet, and kept at 800 ° C and 7 MPa oxygen pressure for 24 h again. After repeating the above process 3 times, NdNi 0.9 Mn 0.1 O3 ceramics. In NdNi 0.9 Mn 0.1 Further introduction of electrodes into O3 ceramics can produce mutation-type thermistor devices, and grinding the ceramics into powder can be further applied to infrared camouflage coatings.

[0037] Example 6: The powders used in this experiment are Eu2O3, NiCO3, and EuNiO3 with a particle size of 2 μm. First, weigh Eu2O3 and NiCO3 powders according to the element ratio of Eu:Ni=1:1, put NiCO3 powder into an air furnace, pre-sinter at 470℃ for 12 h, and then pour it into an agate mortar, weigh homogeneous seed crystals of EuNiO3 according to the ratio of NiCO3:EuNiO3=1:0.05, pour it into the mortar, add polyvinyl alcohol solution and mix with the above powders for 20 min. Weigh 0.2 g of the ground and dried powder, apply 3 tons of mechanical pressure on a tablet press to cold press it into tablets, pre-sinter it into a high-pressure tube furnace and fill it with oxygen to 7 MPa, keep it at 800 ℃ for 24 h, slowly cool it down, take out the sintered block and grind it into powder, add polyvinyl alcohol solution, cold press it into small discs with a diameter of 6 mm, pre-sinter it at 600 ℃ in air for 4 h to remove polyvinyl alcohol, then put it into a high-pressure tube furnace and keep it at 7 MPa oxygen pressure for 24 h, repeat the above process 4 times, and slowly cool it down to obtain EuNiO3 ceramics. Further introduction of electrodes into the ceramics can prepare magnetic electronic devices. Grinding EuNiO3 ceramics into powder can also be further used in infrared camouflage coatings.

[0038] Example 7: The raw material powders used in this experiment include Gd2O3, Ni(CH3COO)2, and GdNiO3 seed crystals. The corresponding oxide powders and homogeneous seed crystals are weighed according to the ratio of Gd2O3:Ni(CH3COO)2:GdNiO3=1:2:0.1. The weighed raw material powders are poured into an agate mortar and mixed evenly. The powders are placed in an air furnace and pre-sintered at 311°C for 12 h. 0.2 g of the pre-sintered powder is weighed and added to a polyvinyl alcohol solution and ground for 20 min. A mechanical pressure of 3 t is applied and the powders are cold pressed into a 6 mm diameter disc. After pre-sintering to remove the polyvinyl alcohol adhesive, the discs are loaded into a quartz tube and placed in a high-pressure tube furnace and kept warm at 800°C and 8 MPa oxygen pressure for 24 h. After slowly cooling, the block is taken out and ground into powder and a polyvinyl alcohol solution is added. 0.2 g of the powder is weighed and cold pressed into a sheet using a 6 mm diameter mold. The discs are pre-sintered at 600°C in air for 1 h to remove the polyvinyl alcohol, continue to put it into a high-pressure tube furnace, fill it with 8 MPa oxygen pressure, keep it at 800℃ for 24 h, repeat the above process 4 times to obtain GdNiO3 ceramics. Further introduction of electrodes into the ceramics can prepare magnetic electronic devices, and grinding the GdNiO3 ceramics into powder can be further used in infrared camouflage coatings.

[0039] Example 8: The raw materials used in this experiment are Nd2O3, NiO, Fe2O3, NdNi 0.9 Fe 0.1O3 seed crystal, weigh the corresponding oxide powders Nd2O3, NiO and Fe2O3 according to the element ratio Nd:Ni:Fe=10:9:1, pour them into an agate mortar and mix them evenly, then according to the ratio NiO:NdNi 0.9 Fe 0.1 O3=10:1 Weigh homogeneous seed crystals, pour them into an agate mortar and mix them with the previous oxide powders, then add polyvinyl alcohol solution and continue grinding for 20 min, cold press them into multiple small discs with a mold with a diameter of 6 mm, pre-sinter them at 600 °C in air for 1 h to remove polyvinyl alcohol, put them in a high-pressure tube furnace and fill them with 10 GPa oxygen pressure, keep them at 800 °C for 24 hours, remove them after cooling to room temperature, grind the sintered small discs into powder, continue to add adhesive and cold press them into sheets, keep them at 800 °C, 10 MPa for 24 h, repeat the above process 5 times, and finally slowly cool them to room temperature to obtain NdNi 0.9 Fe 0.1 O3 ceramics, further introduction of electrodes into ceramics can prepare abrupt thermistor devices. 0.9 Fe 0.1 O3 ground into powder can also be further used in infrared camouflage coatings.

[0040] Example 9: The raw material powders used in this experiment are Ho2O3, Y2O3, NiNO3, Ho 0.8 Y 0.2 NiO3 seed crystal. First, weigh Ho2O3, Y2O3 and NiNO3 powders according to the element ratio of Ho: Y: Ni = 8: 2: 10, mix the powders evenly and put them into an air furnace for pre-calcination at 300 ° C for 12 h, then 0.8 Y 0.2 NiO3=10:1 Weigh homogeneous seed crystals, pour the seed crystals and pre-sintered powders into an agate mortar and grind for 20 min, weigh 2.2 g of powder, add 0.5 mL of polyvinyl alcohol solution and continue grinding, use a mold with a diameter of 20 mm and add 3 t pressure to press it into a disc, pre-sinter it at 600 ℃ in air for 3 h to remove polyvinyl alcohol, then put it into a high-pressure tube furnace, keep it at 800 ℃, 9 MPa for 24 h, slowly cool it down, take out the sintered block and grind it into powder, add polyvinyl alcohol solution and cold press it into a disc with a diameter of 20 mm, then keep it at 800 ℃, 9 MPa oxygen pressure for 24 h, repeat the above process 4 times, and get Ho after cooling to room temperature. 0.8 Y 0.2 NiO3 ceramics, further introduction of electrodes into ceramics can prepare magnetic electronic devices, 0.8 Y 0.2 NiO3 ground into powder can also be further used in infrared camouflage coatings.

[0041] Example 10: The raw material powders used in this experiment are Dy2O3, Co3O4, NiO, DyNi with a diameter of 10 μm 0.8 Co 0.2 O3 seed crystal. First, weigh the corresponding oxide powder according to the element ratio Dy:Ni:Co=1:0.8:0.2, and then weigh NiO:DyNi 0.8 Co 0.2 O3=10:1 weighing DyNi 0.8 Co 0.2 O3 homogeneous seed crystals were ball-milled to a particle size of 1 μm using a ball mill. The seed crystals and the above oxide powders were then poured into an agate mortar and mixed evenly. 0.2 g of powder was weighed, 1 drop of polyvinyl alcohol solution was added and mixed for 10 min, and a mold with a diameter of 6 mm was used to apply a pressure of 3 t to cold-press the pieces. The pieces were kept warm at 500 °C in air for 1 h to remove the polyvinyl alcohol solution. The pre-sintered small discs were placed in a quartz tube, placed in a high-pressure tube furnace and filled with 7 MPa of oxygen, and then kept warm at 900 °C for 24 h. The sintered blocks were ground into uniform powders, cold-pressed into pieces after adding polyvinyl alcohol solution, and sintered again at 900 °C and 7 MPa for 24 h. The above process was repeated 3 times to obtain DyNi 0.8 Co 0.2 O3 ceramics, further introducing electrodes into ceramics can prepare strongly correlated logic devices, 0.8 Co 0.2 O3 ground into powder can also be further used in laser protective coatings.

[0042] Example 11: The raw materials used in this experiment are Ho2O3, CrO2, NiO and HoNi 0.9 Cr 0.1 O3 powder. First, the ratio of Ho2O3:CrO2:NiO:HoNi 0.9 Cr 0.1 Weigh each oxide powder and homogeneous seed crystal in a ratio of 5:1:9:1, pour the above powder into an agate mortar and mix evenly, weigh 0.2 g of the mixed powder and add the polyvinyl alcohol solution to continue mixing, pour the dried powder into a cold pressing mold with a diameter of 6 mm, apply a mechanical pressure of 2 GPa and keep it for 5 min, put the cold pressed block into an air furnace, keep it at 500 °C for 1 h to remove the polyvinyl alcohol, put the pre-sintered block into a high-pressure tube furnace, keep it at 900 °C, 5 MPa for 24 h, cool to room temperature, take out the sintered block and grind it into powder, add the polyvinyl alcohol solution again and cold press it into a sheet, pre-sinter it at 500 °C for 2 h, keep it at 900 °C, 5 MPa for 24 h, and slowly cool it to obtain HoNi 0.9 Cr 0.1O3 ceramics, further introducing electrodes into ceramics can prepare strongly correlated logic devices, 0.9 Cr 0.1 O3 ground into powder can also be further used in infrared camouflage coatings.

[0043] Example 12: The raw material powders used in this experiment are Er2O3, NiO, and ErNiO3. First, weigh the corresponding oxide powders in the ratio of Er:Ni=1:1, pour the raw material powders into an agate mortar and mix them, then add 1 μm ErNiO3 as a homogeneous seed crystal in the ratio of Er2O3:ErNiO3=1:0.01 and continue to grind until uniform. Weigh 0.2 g of the mixed powder and add polyvinyl alcohol solution. After grinding and drying, cold press it into a disc with a diameter of 6 mm. After pre-sintering, put it in a high-pressure furnace and fill it with oxygen to 7MPa. Raise the temperature to 800 ℃ and keep it warm for 24 h, and finally slowly cool it to room temperature. Take out the agglomerated powder and grind it again, add a binder and cold press it into a sheet, put it in a high-pressure furnace, keep it warm at 800 ℃ and 7 MPa for 24 h, and finally slowly cool it to room temperature. Repeat the above process 5 times to obtain ErNiO3 ceramics. Further introducing electrodes into the ceramics can prepare mutation thermistor devices. Grinding the ErNiO3 ceramics into powder can also be further used in infrared camouflage coatings.

[0044] Example 13: The raw material powders used in this experiment are Tm2O3, Yb2O3, NiO, Tm 0.5 Yb 0.5 NiO3. First, weigh the corresponding oxide powder according to the element ratio of Tm: Yb: Ni = 1:1:1, pour it into an agate mortar and mix it evenly, then press NiO: Tm 0.5 Yb 0.5 Weigh Tm in the ratio of NiO3=1:0.1 0.5 Yb 0.5 NiO3, Tm 0.5 Yb 0.5 After NiO3 is ball-milled to a particle size of 1 μm, it is added to an agate mortar and continued to be ground for 20 min. 0.2 g of the mixed powder is weighed and 1 drop of polyvinyl alcohol solution is added. After mixing and drying, it is poured into a mold with a diameter of 6 mm and cold-pressed into a sheet under a mechanical pressure of 2 GPa. After pre-burning in air to remove polyvinyl alcohol, it is placed in a quartz tube and placed in a high-pressure tube furnace. It is kept at 800 °C under 10 MPa oxygen pressure for 24 h. After slowly cooling to room temperature, the block is taken out and ground into powder until the powder is uniform and fine. Polyvinyl alcohol solution is continued to be added and cold-pressed into a sheet. It is kept at 800 °C under 10 MPa oxygen pressure for 24 h. The above process is repeated 3 times. After slowly cooling, Tm 0.5 Yb 0.5 NiO3 ceramics. At Tm 0.5 Yb0.5 Further introduction of electrodes into NiO3 ceramics can produce mutation-type thermistor devices, and grinding the ceramics into powder can be further applied to infrared camouflage coatings.

[0045] Example 14: The raw material powders used in this experiment include Lu2O3, Ni(CH3COO)2, and LuNiO3 seed crystals. The corresponding oxide powders and homogeneous seed crystals are weighed according to the ratio of Lu2O3:Ni(CH3COO)2:LuNiO3=1:2:0.1. The weighed raw material powders are poured into an agate mortar and mixed evenly. The powders are placed in an air furnace and pre-sintered at 311°C for 12 h. 0.2 g of the pre-sintered powder is weighed and added to a polyvinyl alcohol solution and ground for 20 min. A mechanical pressure of 3 t is applied to cold-press the powder into a 6 mm diameter disc. After pre-sintering to remove the polyvinyl alcohol adhesive, the disc is placed in a quartz tube and placed in a high-pressure tube furnace and kept warm at 800°C and 10 MPa oxygen pressure for 24 h. After slowly cooling, the block is taken out and ground and then the polyvinyl alcohol solution is added. 0.2 g of the powder is weighed and cold-pressed into a sheet using a 6 mm diameter mold. The sheet is pre-sintered in air at 600°C for 1 h to remove the polyvinyl alcohol. The sheet is then placed in a high-pressure tube furnace and filled with 10 MPa oxygen pressure, kept at 800 ℃ for 24 h, and repeated the above process 4 times to obtain LuNiO3 ceramics. Further introduction of electrodes into the ceramics can be used to prepare magnetic electronic devices. Grinding the LuNiO3 ceramics into powder can also be further used in laser protective coatings.

[0046] Example 15: The main raw material powders used in this experiment are Y2O3, NiO, and YNiO3 seed crystals. First, the corresponding oxide powders Y2O3 and NiO are weighed according to the element ratio of Y:Ni=1:0.05, poured into an agate mortar and mixed evenly, then YNiO3 homogeneous seed crystals are weighed according to the ratio of NiO:YNiO3=10:1, the seed crystals are added to the agate mortar and continued to mix for 20 min, polyvinyl alcohol solution is added as a binder, and after mixing and drying, 0.2 g of powder is weighed and poured into a mold with a diameter of 6 mm, and a mechanical pressure of 2 GPa is added to cold-press it into a sheet, and after pre-sintering at 500°C for 1 h, it is put into a high-pressure tubular furnace, filled with 7 MPa of oxygen pressure, and kept warm at 800°C for 24 h. After slowly cooling to room temperature, the sintered block is taken out and ground into a fine and uniform powder, polyvinyl alcohol solution is added to cold-press it into a small disc with a diameter of 6 mm, and then it is again sintered at 800°C for 7 MPa conditions for 24 hours, repeat the above process 3 times, and obtain YNiO3 ceramics after cooling. Further introduction of electrodes into the ceramics can prepare magnetoelectronic devices, and grinding the YNiO3 ceramics into powder can be further used in infrared camouflage coatings.

[0047] Example 16: The raw material powders used in this experiment are La2O3, Sm2O3, Ni(CH3COO)2, La 0.8 Sm0.2 NiO3 seed crystal, in the proportion of La2O3: Sm2O3: Ni(CH3COO)2: La 0.8 Sm 0.2 NiO3=4:1:10:0.5. Weigh the corresponding oxide powders and homogeneous seed crystals, pour the weighed raw powders into an agate mortar and mix them evenly, put them into an air furnace and pre-sinter them at 311 ℃ for 12 hours, weigh 0.2 g of the pre-sintered powder, add polyvinyl alcohol solution and grind for 20 min, add 3 t of mechanical pressure and cold press them into a 6 mm diameter disc, pre-sinter to remove the polyvinyl alcohol adhesive, put them into a quartz tube and put them into a high-pressure tube furnace at 800 ℃ and 9 MPa oxygen pressure for 24 hours, slowly cool them down, take out the blocks, grind them, add polyvinyl alcohol solution, weigh 0.2 g of powder, cold press them into a 6 mm diameter mold, pre-sinter them at 500 ℃ in air for 1 hour to remove polyvinyl alcohol, continue to put them into a high-pressure tube furnace, fill them with 9 MPa oxygen pressure, and keep them at 800 ℃ for 24 hours. Repeat the above process 4 times to obtain La 0.8 Sm 0.2 NiO3 ceramics, further introduction of electrodes into ceramics can prepare magnetic electronic devices, 0.8 Sm 0.2 NiO3 ceramics ground into powder can also be further used in infrared camouflage coatings.

[0048] Example 17: The raw materials used in this experiment are Nd2O3, Sm2O3, NiO, MnO2, Nd 0.2 Sm 0.8 Ni 0.8 Mn 0.2 O3 seed crystal, weigh the corresponding oxide powders Nd2O3, Sm2O3, NiO and MnO2 according to the element ratio Nd: Sm: Ni: Mn: = 2: 8: 8: 2, pour them into an agate mortar and mix them evenly, then add NiO: Nd 0.2 Sm 0.8 Ni 0.8 Mn 0.2 O3=10:1 Weigh homogeneous seed crystals, pour them into an agate mortar and mix them with the previous oxide powders, then add polyvinyl alcohol solution and continue grinding for 20 min, use a 6 mm diameter mold to cold press into multiple small discs, pre-sinter at 600 ° C in air for 1 h to remove polyvinyl alcohol, put them into a high-pressure tube furnace filled with 10 GPa oxygen pressure, keep them at 800 ° C for 24 hours, remove them after cooling to room temperature, grind the sintered small discs into powder, continue to add adhesive and cold press them into sheets, keep them at 800 ° C, 10 MPa for 24 h, repeat the above process 5 times, and finally slowly cool them to room temperature to obtain Nd 0.2 Sm 0.8 Ni 0.8 Mn0.2 O3 ceramics, further introduction of electrodes into ceramics can prepare abrupt thermistor devices. 0.2 Sm 0.8 Ni 0.8 Mn 0.2 O3 ground into powder can also be further used in infrared camouflage coatings.

[0049] The above description is only a preferred embodiment of the present invention and is not intended to limit the scope of the substantial technical content of the present invention. The substantial technical content of the present invention is broadly defined in the scope of the claims of the application. Any technical entity or method completed by others, if it is exactly the same as that defined in the scope of the claims of the application or an equivalent variation, will be deemed to be included in the scope of the claims.

Claims

1. A method for preparing a metastable rare earth nickel-based oxide material, characterized in that: 1) designing a metastable rare earth nickel-based oxide material component according to target electrical transport and phase change characteristics, and selecting Re, Ni, and transition element precursors according to the selected material components and weighing them according to the target metastable rare earth nickel-based oxide stoichiometric ratio; 2) weighing 0.1-50% molar ratio of the Ni element precursor as the target metastable rare earth nickel-based oxide as the nucleation seed crystal according to the amount of the precursor used, and fully mixing the seed crystal with the precursor and cold pressing them into sheets; 3) Selecting the heat treatment temperature and oxygen pressure according to the target metastable rare earth nickel-based oxide: heating the cold-pressed reactants to a high temperature in a high oxygen pressure atmosphere and then keeping the temperature for 0.1-48 h, slowly cooling to room temperature after the temperature is maintained, taking out the sample, grinding it into powder, and cold-pressing it into a sheet again, heating it to a high temperature in a high oxygen pressure atmosphere and then keeping the temperature for 0.1-48 h, repeating the above operation 1-5 times until a pure metastable rare earth nickel-based oxide ceramic is obtained; 4) Further introduce electrodes and other functional layer materials based on metastable rare earth nickel-based oxide ceramics to prepare mutation thermistor devices and strongly correlated logic devices; or grind into powder to prepare infrared camouflage coatings and laser protection coatings; The above steps can realize the effective synthesis of rare earth nickel-based oxides with metal-insulator phase transition and hydrogen-induced electronic phase transition and in a thermodynamically metastable state. The method used does not contain any liquid phase substances, is easy to operate and can achieve large-scale preparation. By adjusting the ratio of precursor to seed crystal, oxygen partial pressure and heat treatment process, the hardness, morphology and electrical transport properties of metastable rare earth nickel-based oxide ceramics can be regulated.

2. The method for preparing the metastable rare earth nickel-based oxide material according to claim 1, characterized in that: Step 1) The chemical composition of the synthesized metastable rare earth nickel-based oxide is ReNi 1-x B x O3; wherein Re is a single rare earth element or a combination of multiple rare earth elements, including La, Pr, Nd, Sm, Eu, Gd, Dy, Ho, Er, Tm, Yb, Lu, Y; B is a single transition element or a combination of multiple transition elements, including Cr, Mn, Fe, Co; the phase transition temperature and resistivity mutation degree of rare earth nickel-based oxide metal insulator can be regulated by designing the Re and B element components.

3. The method for preparing the metastable rare earth nickel-based oxide material according to claim 1, characterized in that: Step 1) The precursor includes oxides, carbonates, nitrates and acetates of rare earth, Ni and transition elements; for carbonate, nitrate and acetate precursors, the corresponding oxides of rare earth, Ni and transition elements can be obtained by pre-calcining and decomposition; the pre-calcining temperature should be 1-200°C higher than the decomposition temperature of the corresponding carbonate, nitrate and acetate.

4. The method for preparing the metastable rare earth nickel-based oxide material according to claim 1, characterized in that: Step 2) The particle size of the metastable rare earth nickel-based oxide nucleation seed crystal is 0.1-100 μm; by changing the size of the seed crystal grains, the non-uniform nucleation process can be regulated, thereby further regulating the purity, electrical transport properties and mechanical properties of the metastable rare earth nickel-based oxide ceramic.

5. The method for preparing the metastable rare earth nickel-based oxide material according to claim 1, characterized in that: Step 3) The mechanical pressure range during the cold pressing process is 0.01-10 GPa; by changing the mass of the powder sample, the size of the cold pressing mold and the pressure of the tablet press, the density of the cold pressed block can be regulated, thereby further regulating the thermodynamic process during sintering.

6. The method for preparing the metastable rare earth nickel-based oxide material according to claim 5, characterized in that: Step 3) During the heating process, the temperature and time required for heating and insulation are jointly regulated by the ratio of precursor to seed crystal and the seed crystal particle size. The insulation temperature is 300-1100°C. By changing the insulation temperature, the diffusion rate of the raw materials and the non-uniform nucleation process can be regulated, thereby further regulating the mechanical properties of the rare earth nickel-based oxide ceramics; the single insulation time is 0.1-48 h, and the purity of the metastable rare earth nickel-based oxide can be regulated by changing the insulation time; the oxygen pressure is 0.2-50 MPa, and the reaction thermodynamic process can be regulated by changing the oxygen pressure, thereby regulating the electrical transport properties of the rare earth nickel-based oxide ceramics; by grinding the sample into powder and sintering it multiple times, the mixing degree of the homogeneous crystal nucleus and the oxide raw material can be regulated, thereby further regulating the purity and electrical transport properties of the rare earth nickel-based oxide.

7. The method for preparing the metastable rare earth nickel-based oxide material according to claim 1, characterized in that: The raw materials for preparing SmNiO3 are Sm2O3, NiO, and SmNiO3 seed crystals. After the raw materials are mixed evenly, a binder is added and cold pressed into sheets. After being kept at 800 °C for 24 h under 1 MPa oxygen pressure, SmNiO3 ceramics are obtained. 0.9 Fe 0.1 The raw materials of O3 are Nd2O3, NiO, Fe2O3, NdNi 0.9 Fe 0.1 O3 seed crystal, the raw materials were mixed evenly and then a binder was added and cold pressed into sheets, which were kept at 10 MPa oxygen pressure and 800 °C for 24 h. The sintered block was ground into powder, and then a binder was added and kept at 10 MPa oxygen pressure and 800 °C for 24 h. After repeating the above process 4 times, NdNi 0.9 Fe 0.1 O3 ceramics.

Citation Information

Patent Citations

  • Synthesis method of metastable-state rare-earth nickel-based perovskite oxide powder material

    CN109503165A

  • Composite modification method for strength of rare earth nickel-based oxide electronic phase change material

    CN114436655A

  • Thermal shock resistant magnesium-zirconium ceramic powder and preparation method thereof

    CN115010172A

  • Synthesis method of rare earth cobalt-based oxide electronic phase change material

    CN115353151A

  • Preparation method of rare earth alkaline earth manganese-based perovskite electronic phase change ceramic material

    CN116903369A