Bonding method and system, medium and program product
By controlling the orientation and magnetic field orientation of conductive particles, the bad bonding problems caused by uneven breaking of conductive particles are solved, stable conduction and insulation of electrodes are achieved, and product yield and reliability are improved.
Patent Information
- Application Number
- CN202411184685.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-27
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure CN119053055A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of liquid crystal display technology, and in particular to a bonding method, system, medium and program product. Background Art
[0002] Anisotropic conductive film (ACF), as a thin film adhesive material, is widely used in the connection of circuits such as display screens with precise spacing electrode conduction, touch screens with low temperature conduction, and IC cards. Using ACF to fix electronic devices such as ICs on circuit boards to achieve electrical connection is called bonding. Bonding requires that the electrodes are conductive in the vertical direction and insulated in the horizontal direction, that is, the electrodes of the upper and lower devices are electrically connected, and the left and right electrodes of the same device do not interfere with each other.
[0003] In the related bonding technology, the conductive particles inside the ACF are usually controlled to attach an insulating shell to the outside, and the conductive particles are non-conductive at this time. The upper and lower electrodes are vertically hot-pressed, and the insulating shell is deformed and broken during the hot-pressing process, and the conductive particles are conductive again, so that the ACF forms a conductive path in the vertical direction of the electrode; and between the left and right electrodes without pressure, the insulating shell keeps insulation in the horizontal direction.
[0004] However, in the related art, the conductive particles are not ideally or evenly broken, which may affect the conduction of the electrode in the vertical direction, or may not be insulated in the horizontal direction, resulting in poor bonding and low product yield. Summary of the invention
[0005] The present application provides a bonding method, system, medium and program product for reducing the incidence of poor bonding.
[0006] In a first aspect, the present application provides a bonding method, which is applied to a bonding system, and the method includes: pre-attaching an anisotropic conductive film to the electrode surface of a lower device; the anisotropic conductive film contains a plurality of conductive particles, an insulating shell is attached to the outside of the conductive particles, and the conductive particles can be controlled in their orientation by magnetic force; the lower device and the upper device are aligned so that the electrodes of the two are aligned to a preset position; pre-pressing the upper device and heating the entire component to a preset temperature to initially soften the anisotropic conductive film; while maintaining the pre-pressing and heating the entire component, applying local pressure to the upper device so that the conductive particles inside the anisotropic conductive film are deformed under the wrapping of the insulating shell and form a conductive path between the corresponding upper and lower electrodes; while maintaining the local pressure and heating the entire component, applying a magnetic field to control the orientation of the conductive particles so that the long axis direction of the conductive particles is consistent with the connection direction of the upper and lower electrodes, and the conductive particles between adjacent electrodes are insulated; cooling the entire component and removing the local pressure to complete the bonding of the upper device and the lower device.
[0007] In the above embodiment, the bonding system pre-attaches the anisotropic conductive film to the surface of the lower device electrode, the conductive particles can be oriented by magnetic force, and then the upper and lower components are aligned, pre-pressing and heating are applied to soften the conductive film, and then the main pressure is applied to break the shell of the conductive particles and form a conductive path between the upper and lower electrodes, and at the same time, a magnetic field is applied to control the orientation of the conductive particles in the vertical direction, and the adjacent electrodes are kept insulated, and finally the bonding is completed by cooling and removing the pressure. The degree of breakage and orientation of the conductive particles in the ACF can be controlled, so that they are conductive in the vertical direction and insulated in the horizontal direction, reducing the incidence of poor bonding.
[0008] In combination with some embodiments of the first aspect, in some embodiments, the lower device and the upper device are aligned so that the electrodes of the two are aligned to a preset position, specifically including: obtaining the CAD design drawings of the lower device and the upper device, performing image processing on the CAD design drawings, and extracting the shape, size and relative position information of each electrode; calculating the alignment parameters when the electrodes of the two are aligned based on the shape, size and relative position information of the electrodes of the lower device and the upper device; clamping and fixing the lower device and the upper device on an alignment device, and controlling the relative movement of the lower device and the upper device until the actual position relationship between the two meets the alignment parameters.
[0009] In the above embodiment, when the bonding system aligns the lower device and the upper device, it obtains the CAD design drawing, extracts the electrode shape, size and relative position information, calculates the alignment parameters, and clamps the two devices on the alignment device for relative movement until the actual position relationship meets the alignment parameters. Combined with the closed-loop control method of actual relative movement feedback, fast and accurate alignment can be achieved.
[0010] In combination with some embodiments of the first aspect, in some embodiments, pre-pressure is applied to the upper device and the entire component is heated to a preset temperature to initially soften the anisotropic conductive film, specifically including: obtaining material parameters of the anisotropic conductive film, and determining the target pre-pressure and target heating temperature required for initial softening according to the material parameters; clamping the lower device, the anisotropic conductive film and the upper device in a hot pressing device, and applying the target pre-pressure to the upper device by adjusting the hot pressing device; powering on the hot pressing device for heating, monitoring the real-time temperature of the inner cavity of the hot pressing device, and dynamically adjusting the heating control of the hot pressing device according to the temperature feedback signal until the temperature of the inner cavity of the hot pressing device stabilizes at the target heating temperature and maintains the preset heating time.
[0011] In the above embodiment, when the bonding system applies pre-pressure and heats the upper device, the target pressure and temperature required for softening are determined by obtaining the conductive film material parameters, the component is clamped in the hot pressing device to apply the target pre-pressure, powered on for heating, and monitored and adjusted in real time until it stabilizes at the target temperature and maintains it for a certain period of time. The initial softening degree of the conductive film can be accurately controlled, which can reduce the difficulty of breaking the conductive particles and avoid excessive softening affecting the insulation performance.
[0012] In combination with some embodiments of the first aspect, in some embodiments, before the step of pre-bonding the anisotropic conductive film on the electrode surface of the lower device, the method also includes: obtaining the dimensional parameters of the upper device and the lower device after actual processing and preparation, comparing them with the design values, calculating the dimensional deviation, and determining whether the dimensional deviation is within the error range; if the dimensional deviation exceeds the error range, outputting an alarm message and terminating subsequent bonding operations.
[0013] In the above embodiment, before the conductive film is pre-attached, the bonding system obtains the size parameters of the upper and lower components after actual processing, compares them with the design values, calculates the deviation, and determines whether it exceeds the error range. If it exceeds, an alarm is triggered to terminate the bonding. It can effectively identify unqualified components with excessive dimensions, prevent them from entering the bonding process, and control the bonding defect rate from the source.
[0014] In combination with some embodiments of the first aspect, in some embodiments, after the steps of obtaining the dimensional parameters of the upper device and the lower device after actual processing and preparation, comparing them with the design values, calculating the dimensional deviation, and judging whether the dimensional deviation is within the error range, the method further includes: if the dimensional deviation is within the error range, correcting the pre-attachment position and pre-attachment angle of the anisotropic conductive film according to the dimensional deviation; adjusting the position and angle of the anisotropic conductive film so that it reaches the pre-attachment position and pre-attachment angle.
[0015] In the above embodiment, when the detected size deviation does not exceed the error range, the bonding system corrects the pre-attachment position and angle of the conductive film according to the deviation amount, and adjusts the conductive film to reach the corrected position and angle, thereby reducing the risk of poor bonding and improving product yield.
[0016] In combination with some embodiments of the first aspect, in some embodiments, after cooling the overall component and removing the local pressure to complete the step of bonding the upper device and the lower device, the method further includes: transferring the overall component after bonding to an aging device, and placing it under preset environmental conditions for a preset test time; placing the aged overall component in a detection device, and performing an electrical parameter test on the device using an electrical performance testing instrument; the electrical parameter test includes continuity, insulation, polarity, resistance, capacitance and signal delay; comparing the test results with the theoretical design values to determine the overall component that has passed the electrical performance test.
[0017] In the above embodiment, after the bonding system is completed, the device is transferred to the aging device and placed in a preset environment for a certain period of time, and then the electrical parameters including continuity, insulation, polarity, resistance, capacitance, signal delay, etc. are tested, and the results are compared with the theoretical design values to screen out qualified devices. The aging test can simulate the environmental stress in the actual use of the product and test the consistency and stability of its electrical performance.
[0018] In combination with some embodiments of the first aspect, in some embodiments, after comparing the test results with the theoretical design values to determine the devices that have passed the electrical performance test, the method also includes: counting the number of devices that have passed the electrical performance test and calculating the electrical yield; when the electrical yield is lower than the electrical yield threshold, analyzing the failure mode that causes the device performance to fail; optimizing the bonding process parameters based on the failure mode; the bonding process parameters include the pressure, heating temperature, holding time and magnetic field strength of the bonding process.
[0019] In the above embodiment, the bonding system further counts the number of devices that pass the test and calculates the electrical yield. When the yield is lower than the threshold, the failure mode that leads to failure is analyzed, and the bonding process parameters such as pressure, temperature, time, and magnetic field strength are optimized in combination with the failure mode. The key factors affecting poor bonding can be found, and the bonding process level can be continuously improved.
[0020] In a second aspect, an embodiment of the present application provides a binding system, which includes: one or more processors and a memory; the memory is coupled to the one or more processors, the memory is used to store computer program code, the computer program code includes computer instructions, and the one or more processors call the computer instructions to enable the binding system to perform the method described in the first aspect and any possible implementation method of the first aspect.
[0021] In a third aspect, an embodiment of the present application provides a computer program product comprising instructions, and when the computer program product is run on a bonding system, the bonding system executes the method described in the first aspect and any possible implementation manner of the first aspect.
[0022] In a fourth aspect, an embodiment of the present application provides a computer-readable storage medium, comprising instructions, which, when executed on a binding system, enable the binding system to execute the method described in the first aspect and any possible implementation of the first aspect.
[0023] It can be understood that the bonding system provided in the second aspect, the computer program product provided in the third aspect, and the computer storage medium provided in the fourth aspect are all used to execute the method provided in the embodiment of the present application. Therefore, the beneficial effects that can be achieved can refer to the beneficial effects in the corresponding method, and will not be repeated here.
[0024] One or more technical solutions provided in the embodiments of the present application have at least the following technical effects or advantages: 1. Since the anisotropic conductive film is pre-attached to the electrode surface of the lower device before bonding and the orientation of the conductive particles can be controlled by magnetic force, the conductive film can be easily and tightly fitted to the lower device, laying the foundation for the subsequent magnetic field to control the orientation of the conductive particles. This effectively solves the problem of poor bonding between the conductive film and the device and the difficulty in controlling the orientation of the conductive particles in the prior art, resulting in a high bonding failure rate, thereby achieving the purpose of reducing the incidence of bonding failures.
[0025] 2. Because the actual size parameters of the upper and lower devices after processing are obtained before the pre-attachment of the conductive film, and then compared with the design value, the size deviation is calculated and it is judged whether it exceeds the error range. Therefore, the device with processing size deviation can be identified in advance to avoid it from entering the subsequent bonding process. The problem of the existing technology that devices with unqualified processing size participate in bonding, resulting in an increase in the bonding defect rate, is effectively solved, thereby achieving the purpose of controlling product quality from the source and reducing the risk of bonding defects.
[0026] 3. After the bonding is completed, the device is transferred to the aging device, placed under preset environmental conditions for a certain period of time, and then subjected to comprehensive tests on its electrical properties such as continuity, insulation, polarity, resistance, capacitance, signal delay, etc., and the results are compared with theoretical values to screen qualified products. Therefore, the true performance of the device's electrical performance under environmental stress can be known, and its electrical reliability can be comprehensively evaluated. This effectively solves the problem in the existing technology that it is difficult to fully consider the reliability of use by only routine sampling after bonding, thereby achieving the purpose of effectively improving product reliability and service life. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 It is a flow chart of the bonding method in the embodiment of the present application; Figure 2 is another flow chart of the bonding method in the embodiment of the present application; Figure 3 It is a schematic diagram of a physical device structure of a bonding system in an embodiment of the present application. DETAILED DESCRIPTION
[0028] The terms used in the following embodiments of the present application are only for the purpose of describing specific embodiments, and are not intended to be used as limitations to the present application. As used in the specification of the present application, the singular expressions "one", "a kind of", "above", "the" and "this" are intended to also include plural expressions, unless there is a clear indication to the contrary in the context. It should also be understood that the term "and / or" used in the present application refers to any or all possible combinations comprising one or more of the listed items.
[0029] In the following, the terms "first" and "second" are used for descriptive purposes only and are not to be understood as suggesting or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features, and in the description of the embodiments of the present application, unless otherwise specified, "plurality" means two or more.
[0030] For ease of understanding, a scenario using the bonding method in the related art is introduced below.
[0031] In related technologies, anisotropic conductive film (ACF) is usually used to achieve chip-to-chip interconnection. The ACF is placed between two chips, and softened by heating and pressurizing. The conductive particles gather under pressure to form a conductive path in the Z direction to achieve chip electrode interconnection. However, this method is extremely sensitive to process parameters. Any slight deviation in heating temperature, pressure, and time will lead to unreliable connection. For example, when bonding chips, the ACF softens at 180°C, and the pressure needs to be precisely controlled at 20N. Too low pressure will cause the insulating shell of the particles to fail to break, and conduction will be affected. In addition, the distribution of ACF conductive particles is random, and connection defects are prone to occur. This makes the ACF method have a low yield and difficult to apply to industrial mass production.
[0032] The magnetic conductive film interconnection method in the embodiment of the present application is used to guide the conductive particles to align in a directional manner through a magnetic field, forming a dense conductive path perpendicular to the plane of the conductive film, thereby achieving stable and reliable interconnection. The following describes the scenario in which the bonding method in the present application is used.
[0033] This application proposes a novel device interconnection method, which uses a conductive film filled with magnetic particles and uses a magnetic field to induce the particles to align in a directional manner to form a Z-direction conductive path. When bonding the chips, a softened conductive film filled with magnetic particles is placed between the chips, and a magnetic field perpendicular to the surface of the conductive film is applied. Under the action of the magnetic field, the particles move and gather along the direction of the magnetic lines of force to form a conductive path perpendicular to the chip. In addition, the particles are oriented in the magnetic field, which significantly improves the connection consistency and reliability.
[0034] It can be seen that the magnetic conductive film interconnection method of the embodiment of the present application can not only achieve stable interconnection, but also effectively reduce the damage to the device during the interconnection process, improve the consistency of interconnection quality, and thus achieve low-cost, high-yield device interconnection packaging.
[0035] For ease of understanding, the following describes the process of the method provided by this implementation in combination with the above scenario. Figure 1 , which is a flow chart of the bonding method in the embodiment of the present application.
[0036] S101, pre-attaching anisotropic conductive film to the electrode surface of the lower device.
[0037] Among them, anisotropic conductive film refers to a thin film material that conducts electricity in the vertical direction and insulates in the horizontal direction, and contains conductive particles wrapped in an insulating shell. The lower device refers to the lower component of the two devices to be bonded, and an electrode is provided on its surface. The electrode is used to form an electrical connection with the electrode of the upper device. Pre-bonding refers to the operation of attaching the anisotropic conductive film to the surface of the electrode of the lower device before bonding.
[0038] It should be noted that the conductive particles described in the present invention are made of metal materials and are wrapped with an insulating shell on the outside, and the insulating shell can be broken under the action of pressure. The shape of the conductive particles can be designed to be spherical, cylindrical, truncated cone, cone barrel, or even teardrop-shaped, because the cylindrical, truncated cone, and cone barrel require less force to break the shell than the spherical shape, and in some cases, a combination of particles of various shapes can also be performed. When the conductive particles cover the insulating shell, they will be fixed in the z direction and an insulating coating will be applied on their sides. As a result, the conductive particles can form an effect of being conductive in the z direction and insulating in the xy direction.
[0039] If they are arranged vertically in the anisotropic conductive film under the control of a magnetic field, the anisotropic conductive film can maintain the characteristics of being conductive in the z direction and insulating in the xy direction. It should be emphasized that even if no magnetic field is applied, according to the probability distribution, the conductive particles can still maintain a direct z-direction conductivity of about 50% when the insulating shell is not broken; in addition, in the xy direction, due to the 50% distribution characteristics, if the left and right electrodes need to be conductive, firstly, the conductive particles need to reach a specified density, and secondly, all the conductive particles need to be in close contact laterally. This probability decreases exponentially by 50% according to the direction and number of the conductive particles. When the particle density is controlled, the conduction in the xy direction is basically a zero probability event. The orientation of the magnetically controllable conductive particles is due to the fact that the electric particles are filled with magnetic materials. Under the action of an external magnetic field, their long axis direction will be arranged along the direction of the magnetic lines of force.
[0040] The bonding system usually attaches anisotropic conductive film to the electrode surface of the lower device before assembling the two devices to be bonded. The conductive film and the electrode must fit tightly without bubbles. Specifically, the bonding system first delivers the coiled conductive film to the top of the lower device, cuts the conductive film into a shape that matches the size of the lower device by shearing or punching, and aligns it with the electrode position for bonding. To enhance the bonding strength, hot melt adhesive can be applied to the back of the conductive film before bonding. The conductive film and the electrode are precisely aligned and cannot be offset. The conductive particles are randomly oriented when attached.
[0041] S102, aligning the lower device and the upper device so that the electrodes of the two devices are aligned to a preset position.
[0042] Among them, alignment refers to adjusting the relative positions of the upper and lower devices so that the electrodes of the two can be accurately aligned. The preset position represents the relative position relationship of the upper and lower device electrodes determined according to the device design drawings and represents the optimal alignment state, usually represented by a three-dimensional coordinate value.
[0043] After the lower device and the conductive film are bonded, the bonding system will align the upper and lower components. The alignment accuracy directly affects whether the electrode can be reliably conductive. Specifically, the bonding system first moves the upper device to the top of the lower device, takes the upper device through a robotic arm or adsorption mechanism, and adjusts its relative position and angle with the lower device. At the same time, the bonding system collects the surface images of the two devices in real time through the visual system, extracts and matches the electrode features, calculates the deviation between the current position and the preset position, and performs feedback control. The alignment is considered completed until the deviation is reduced to within the set threshold.
[0044] S103, applying pre-pressure to the upper device and heating the entire component to a preset temperature to initially soften the anisotropic conductive film.
[0045] Among them, pre-pressing refers to applying a small pressure to the upper device after the alignment is completed, so that the anisotropic conductive film and the upper device are in initial contact. The integral component refers to the overall structure composed of the upper and lower components and the middle conductive film after the alignment is completed. The preset temperature is a temperature value that is pre-set according to the material properties of the conductive film and can make it initially softened. Initial softening refers to the state where the conductive film has just begun to soften after being heated, but has not yet reached the state of being completely melted.
[0046] After the bonding system completes the alignment of the upper and lower components, it applies pre-pressure to the upper component through the pressure head and other mechanisms, so that the upper and lower components are close together and the anisotropic conductive film is clamped in between. The pre-pressure is small, and only the components are initially in contact. Then, the bonding system heats the entire component to slowly increase its temperature. Specifically, the heating device cooperates with the pressure head and heats it through the built-in heating wire. The bonding system detects the component temperature in real time and controls the heating power according to the feedback signal until the temperature reaches and stabilizes at the preset temperature. After being softened by heat, the conductive film becomes flexible and easy to deform under subsequent high pressure. However, the degree of softening is limited, and the insulating shell of the conductive particles is basically intact.
[0047] Pre-pressing and heating can be achieved in the following ways: Optionally, the bonding system consults the softening temperature data table according to the material composition and thickness of the conductive film and other parameters to obtain the temperature range required for softening, and selects a suitable value from it as the preset temperature. The pressure head slowly presses down to the set pressure value and maintains the pressure, while the heating device obtains temperature feedback and controls the power, so that the component is heated to the preset temperature within tens of seconds; Optionally, use infrared sensors and other temperature measuring components to obtain the temperature distribution map of the entire component in real time, find the cold spot area, and focus on heating it to achieve uniform temperature in all parts; Optionally, the component is first locally preheated to soften the outer layer of the conductive film, and then pre-pressing is applied to improve the coverage of the conductive film. It is understandable that the pre-pressing and heating conditions can be appropriately adjusted according to factors such as the material, thickness, and batch differences of the conductive film in order to obtain the best softening effect, which is not limited here.
[0048] S104, while maintaining the pre-pressure and heating of the entire component, applying local pressure to the upper device, so that the conductive particles inside the anisotropic conductive film are deformed under the wrapping of the insulating shell, and a conductive path is formed between the corresponding upper and lower electrodes.
[0049] The basic pressure refers to the pressure value that is further increased on the basis of the pre-pressure to fully deform the anisotropic conductive film. Under the action of the basic pressure, the conductive particles will break through the outer insulating layer and squeeze between the corresponding upper and lower electrodes to form a conductive path. The upper and lower electrodes correspond to each other in the vertical direction of the device. The conductive path refers to the channel formed by the conductive particles between the electrodes that can effectively conduct the current.
[0050] While maintaining the pre-pressure and preset temperature of the entire component, the bonding system begins to apply the main pressure to the upper device. The main pressure is much greater than the pre-pressure, usually 1-2 orders of magnitude higher. The conductive film will deform significantly under this high pressure, and squeeze and flow around, filling the upper and lower device electrode areas more densely. At the same time, the outer shell of the conductive particles that are under the greatest pressure and located between the corresponding electrodes is squeezed first, exposing the internal conductive particles. Under continuous squeezing, the exposed conductive particles will fully contact the upper and lower electrodes, and eventually form a through conductive path. The conductive particles are small and numerous, and multiple parallel paths will be formed between a single pair of electrodes, thereby ensuring the reliability of interconnection.
[0051] S105. While maintaining the original pressure and heating the entire component, a magnetic field is applied to control the orientation of the conductive particles so that the long axis direction of the conductive particles is consistent with the connection direction of the upper and lower electrodes, and the conductive particles between adjacent electrodes are insulated.
[0052] While maintaining the original pressure and heating, the bonding system applies a magnetic field to the entire component. The magnetic field is strong and its direction is perpendicular to the device surface and parallel to the direction of the upper and lower electrode lines. Driven by the magnetic field force, the conductive particles will rotate so that their long axes are consistent with the direction of the magnetic lines. That is, the long axis direction of the conductive particles will coincide with the virtual line running through the corresponding electrode. In this way, the conductive particles between the electrodes will be straightened and arranged as neatly as possible, forming the shortest path between the electrodes, further reducing the interconnection resistance. For the conductive particles between adjacent electrodes, the magnetic field will insulate them. Because the long axis directions of the conductive particles in adjacent electrode regions are not consistent, the magnetic field will cause them to be arranged in their respective directions and staggered.
[0053] It should be noted that the magnetic field can also be applied at the beginning of the experiment, that is, before maintaining the pressure and heating the entire component in this step. The present invention preferably maintains the pressure and heats the entire component in order to control the distribution direction of the conductive particles in the gap between the electrodes so that they are all arranged vertically, completely avoiding the situation of conduction in the xy direction.
[0054] In some embodiments, the bonding system can control the magnetic field in the following ways: Optionally, electromagnets are arranged on the upper and lower surfaces of the integral component, and a strong current is passed to generate a vertical magnetic field. By adjusting the spacing and deflection angle of the upper and lower electromagnets, the magnetic field can evenly cover the bonding area; Optionally, a permanent magnet array is used to surround the integral component, and by adjusting the angle and attraction spacing between the permanent magnets, the desired magnetic field is formed in the bonding area; Optionally, a high magnetic permeability material is added to the conductive film, and under the action of an external magnetic field, the doped particles will be magnetized and disrupt the local magnetic field distribution, making the force on the conductive particles more complicated and preventing adjacent conductive particles from contacting. It can be understood that there are many ways to apply the magnetic field, such as inserting a magnetic field generating device, using special magnetic materials, etc., as long as the desired magnetic field can be formed in the key area, it is not limited here.
[0055] S106, cooling the entire component and removing the pressure, completing the bonding of the upper device and the lower device.
[0056] After being kept under the magnetic field for a certain period of time, the bonding system begins to cool down and remove the pressure. The temperature of the entire component gradually decreases under natural cooling or active cooling, and the anisotropic conductive film cools and solidifies. The pressure head is slowly lifted to gradually relieve the pressure on the component until the pressure is completely removed. At this point, the conductive film has been bonded between the upper and lower components and a reliable conductive connection has been formed in the electrode area. At the same time, the insulation performance between adjacent electrodes is good. That is, the upper and lower components have been bonded as one, and the bonding process is completed.
[0057] In some embodiments, the bonding system can implement cooling and pressure relief in the following ways: Optionally, turn off the power of the heating device, introduce a cooling medium such as cold air, cold water, etc., and adjust the flow rate to control the temperature of the component to drop at a set rate until it cools to the ambient temperature. At the same time, the pressure head is slowly lifted at a speed that matches the temperature drop rate, so that the pressure of the component drops synchronously; Optionally, a blower is set to blow cold air evenly on each surface of the component to avoid excessive temperature gradients that cause the component to warp and deform. The pressure head is evacuated in multiple stages, first slightly lifted to eliminate the main pressure, then slowly raised and paused, and finally lifted and disengaged; Optionally, a cooling and pressure relief curve opposite to the heating and pressing process is applied, and the real-time temperature and pressure changes are tracked through the feedback system, and the target curve is dynamically matched to achieve stable and controllable cooling and pressure relief. It can be understood that the cooling and pressure relief strategy needs to be comprehensively considered based on factors such as the properties of the conductive film material, the size and structure of the device, etc., in order to take into account both efficiency and bonding quality, which is not limited here.
[0058] The following is a more detailed description of the process of the method provided by this implementation. Figure 2 , is another flow chart of the bonding method in the embodiment of the present application.
[0059] S201, obtaining the dimensional parameters of the upper device and the lower device after actual processing and preparation, comparing them with the design values, calculating the dimensional deviation, and determining whether the dimensional deviation is within the error range.
[0060] Among them, the upper device and the lower device represent the two devices to be bonded. The dimensional parameters after the actual processing and preparation are the actual dimensions of the device obtained by measurement after the device is prepared. The design value is used to represent the theoretical dimensions of the device specified in the design drawing. The dimensional deviation represents the difference between the actual dimension and the design dimension. The error range refers to the allowable range of dimensional deviation pre-set according to the functional requirements of the device and the processing technology capabilities, which is usually defined by positive and negative tolerances.
[0061] Before the bonding system officially performs the pre-attachment of the anisotropic conductive film, it is necessary to detect the key dimensions of the upper and lower components that have been actually processed, and compare the measured actual values with the theoretical values marked on the design drawings to determine whether the dimensional deviation is within an acceptable range. Specifically, the bonding system uses a CCD camera to capture a high-definition image of the device surface, uses an image processing algorithm to extract the edge contour, and converts the actual size based on the calibration data; at the same time, the system automatically retrieves the product drawings and reads the corresponding dimension markings as the design value. Both are input into the mathematical model to calculate the deviation value, and then the deviation value is compared with the preset error range to determine the dimensional compliance.
[0062] In some embodiments, the size detection and comparison can be achieved in a variety of ways: Optionally, the bonding system uses contact measurement, such as a three-dimensional coordinate measuring machine with a micro probe, which contacts the device surface point by point to obtain spatial coordinate data, calculates the size result, and then compares the measured value with the CAD drawing data to obtain the deviation value; Optionally, the bonding system uses optical non-contact measurement, such as a laser radar scanner, which projects a light beam to the device surface to obtain a reflection signal, analyzes the reflection pattern characteristics to calculate the three-dimensional size of the object being measured, and compares the measurement result with the parameterized three-dimensional model to evaluate the size deviation; Optionally, manually use a measuring tool such as a vernier caliper to perform sampling inspection at the key features of the device, manually record the readings and enter them into the system, and the system automatically retrieves the design parameters and completes the deviation calculation and qualification judgment. It is understandable that the size detection method can also use other contact, non-contact means, or a combination of man and machine, as long as the actual value can be accurately obtained and its deviation can be evaluated, which is not limited here.
[0063] S202: If the size deviation exceeds the error range, an alarm message is output and subsequent bonding operations are terminated.
[0064] Among them, outputting alarm information means that the bonding system issues abnormal prompts through sound and light alarms, display screens and other devices to remind operators to pay attention. Terminating subsequent bonding operations means that after the bonding system detects serious dimensional abnormalities, it automatically stops or skips subsequent bonding operations such as attachment, heating, and pressing to isolate the abnormal device.
[0065] As described in step S201, after the bonding system measures the actual size of the upper and lower components and calculates the deviation from the design value, it will determine whether the deviation value exceeds the preset allowable range. Once it is found that the upper or lower limit is exceeded, the system will respond in time. Specifically, the bonding system informs the operator that the size of this component is seriously exceeded and is a defective product by flashing an alarm light, sounding a buzzer, etc. At the same time, the system immediately suspends the subsequent processing flow of the component to prevent it from being sent to the bonding process. These measures can effectively prevent poor bonding due to size defects of the component itself.
[0066] The following measures can be taken to deal with out-of-tolerance devices: Optionally, the bonding system automatically transfers out-of-tolerance devices to the defective product buffer area, where they are stored centrally and re-inspected regularly. For devices that still fail the re-inspection, the system classifies them as scrapped products and records their model and batch information for traceability; Optionally, the bonding system prints labels indicating the device number, reason for failure, disposal opinions, etc., and pastes them on the outer packaging of the device, and then manually determines whether it can be reworked and fills in the processing results; Optionally, for devices with a large deviation, the system directly transmits a signal to the central control system, triggers interlocking protection, stops the production line, and promptly notifies relevant personnel to come and handle it. It is understandable that the disposal methods for out-of-tolerance devices vary from company to company, such as transferring to a third party for rework, directly scrapping, etc., but the basic logic is to isolate abnormal incoming materials and curb the outflow of defective products, which is not limited here.
[0067] S203 , if the size deviation is within the error range, correcting the pre-attachment position and pre-attachment angle of the anisotropic conductive film according to the size deviation.
[0068] Among them, correcting the pre-attachment position and angle of the anisotropic conductive film means adjusting the originally planned attachment position and angle of the ACF film according to the size deviation value of the upper and lower devices measured in step S201 to compensate for the deviation. The pre-attachment position represents the plane coordinate position of the ACF film relative to the reference device. The pre-attachment angle refers to the angle posture of the ACF film plane relative to the device plane.
[0069] As mentioned above, when the bonding system detects that the size deviation of the upper and lower components is within an acceptable range, although the components can enter the subsequent bonding process, this deviation will affect the subsequent alignment accuracy if it is not compensated. Specifically, the system inputs the deviation value into the mathematical model, and solves the required displacement and rotation angle of the ACF film in each direction through coordinate transformation, thereby obtaining the corrected attachment position coordinates and angle values. This correction will be executed when the ACF film is moved in the next step, which will play a role in compensating for the component processing error and improving the bonding accuracy, thus laying the foundation for subsequent bonding.
[0070] S204, adjusting the position and angle of the anisotropic conductive film to achieve a pre-attachment position and pre-attachment angle.
[0071] The actual position and angle of the ACF are adjusted to match the pre-attachment position and angle calculated in step S203, that is, the pre-attachment position and angle are achieved. The ACF to be adjusted is usually supplied in the form of a roll tray or a transfer frame.
[0072] After completing the correction calculation of the ACF film attachment position and angle, the bonding system begins to adjust the actual posture of the ACF film to match it with the correction value. Specifically, the system grabs the ACF film through a robotic arm or vacuum adsorption, and controls the actuator to drive the ACF film to translate to the corrected position on the three coordinate axes of XYZ, and rotate the ACF film around each axis to the corrected angle. After the posture adjustment is completed, the ACF film is accurately aligned above the device electrode area, ready for the next step of pre-bonding.
[0073] S205, pre-attaching the anisotropic conductive film to the electrode surface of the lower device.
[0074] Referring to step S101, the bonding system will pre-attach the anisotropic conductive film to the electrode surface of the lower device.
[0075] S206 , aligning the lower device and the upper device so that the electrodes of the two devices are aligned to a preset position.
[0076] Referring to step S102, the bonding system aligns the electrodes of the two devices to a preset position.
[0077] In some embodiments, the bonding system obtains the CAD design drawings of the lower device and the upper device, performs image processing on the CAD design drawings, and extracts the shape, size, and relative position information of each electrode; calculates the alignment parameters when the electrodes of the lower device and the upper device are aligned based on the shape, size, and relative position information of the electrodes of the two devices; clamps and fixes the lower device and the upper device on the alignment device, and controls the relative movement of the lower device and the upper device until the actual position relationship between the two meets the alignment parameters.
[0078] Specifically, CAD design drawings refer to drawings of device structures drawn using computer-aided design software, including layouts of each functional layer, dimensioning and other information. Image processing refers to the application of computer vision and graphics algorithms to extract and analyze feature parameters in CAD drawings. Alignment parameters are used to indicate the relative positional relationship that the device body should satisfy when the electrodes of the two devices to be bonded completely overlap, such as spacing, angles, etc. The alignment device is a precision mechanical device that can achieve high-precision alignment of two devices through motion control and visual guidance.
[0079] Specifically, in order to achieve precise device alignment, the bonding system must first obtain the CAD drawing of the device to be bonded to understand its structural layout. Then, the CAD drawing is processed by image recognition to extract characteristic parameters such as the device electrode contour and center of gravity. Based on these parameters, the system uses mathematical operations such as coordinate transformation to derive the relative posture relationship of the device body when the electrodes of the two devices are aligned, and generates alignment parameters. During actual alignment, the system clamps the device on the alignment device, controls the movement and rotation of the platform, collects the device position information in real time and compares it with the target alignment parameters, and makes the device move relative to each other through closed-loop control until the actual position relationship completely matches the alignment parameters. This process needs to be carried out under a microscope to achieve micron-level alignment accuracy.
[0080] S207 , applying pre-pressure to the upper device and heating the entire component to a preset temperature to initially soften the anisotropic conductive film.
[0081] Referring to step S103, the bonding system initially softens the anisotropic conductive film.
[0082] In some embodiments, the bonding system obtains the material parameters of the anisotropic conductive film, determines the target pre-pressure and target heating temperature required for initial softening according to the material parameters; clamps the lower device, the anisotropic conductive film and the upper device in a hot pressing device, and applies the target pre-pressure to the upper device by adjusting the hot pressing device; energizes and heats the hot pressing device, monitors the real-time temperature of the inner cavity of the hot pressing device, and dynamically adjusts the heating control of the hot pressing device according to the temperature feedback signal until the temperature of the inner cavity of the hot pressing device stabilizes at the target heating temperature and maintains the preset heating time.
[0083] Specifically, the anisotropic conductive film is a polymer composite material filled with conductive particles, which can soften under certain conditions and produce Z-direction conductivity. Material parameters represent the physical and chemical properties of the anisotropic conductive film, such as softening temperature, conductivity, etc. Softening refers to the process in which the matrix resin of the anisotropic conductive film changes from a solid state to a fluid state under the action of heat and pressure. Pre-pressure is used to indicate the initial pressure applied to the anisotropic conductive film to bring it into close contact with the surface of the device. The target heating temperature refers to the theoretical optimal temperature value required to soften the anisotropic conductive film. The hot pressing device is an instrument with dual functions of heating and pressing, and is commonly used for bonding anisotropic conductive films.
[0084] Specifically, in order to achieve the initial softening of the anisotropic conductive film, the bonding system first obtains the physical properties of the film material, focusing on its softening characteristics. Based on the empirical model, the system calculates the target pre-pressure and heating temperature required to soften the anisotropic conductive film. Then, the system stacks the device and the conductive film layer by layer, places them in the hot press, and applies pre-pressure to the device through air pressure or hydraulic cylinders. The hot press device is powered on and heated, and the temperature change of its inner cavity is monitored by thermocouples, and the real-time temperature signal is fed back to the controller in real time. The controller implements closed-loop control through algorithms such as PID, dynamically adjusts the current passed into the hot press device, and gradually increases the temperature of the inner cavity and stabilizes at the target temperature. After the temperature reaches the standard, it needs to be maintained for a period of time to ensure that the conductive film is fully softened. The entire process is controlled by an automatic program to obtain the best softening effect.
[0085] In some embodiments, the following methods can be used to achieve preliminary softening of the anisotropic conductive film: Optionally, the bonding system first consults the material specification of the conductive film to extract its softening temperature, conductive particle size, filling degree and other key parameters; then these parameters are substituted into the thermodynamic and rheological models, and the target process parameters for softening are calculated through numerical simulation, and sent to the hot pressing device; the system controls the cylinder to drive the hot pressing head to slowly press down, apply pre-pressure to the device, detect the pressure value in real time through the pressure sensor and feedback, and control the movement of the cylinder through the servo motor to achieve pressure closed-loop control; an alternating current is passed through the hot pressing head, and the resistance wire is used to generate heat to quickly heat it up. The temperature data is collected in real time through the thermocouple, and the measured temperature and the target temperature form a negative feedback control system, the alternating current frequency is adjusted, so that the temperature of the hot pressing head quickly reaches and stabilizes at the target value, and the timing is started at the same time, and the heating is stopped after maintaining the target temperature for a certain period of time. Optionally, the bonding system can also use an infrared thermometer to remotely monitor the surface temperature of the conductive film, and judge the uniformity of the softening of the conductive film in combination with its temperature cloud map; during the softening process, the system records and adjusts the movement displacement of the hot press head in real time, and reflects the softening degree of the conductive film through the displacement. When the displacement reaches the set threshold, it is considered that the softening is complete; at the same time, the system can also apply an alternating electric field to the conductive film, and use the electric field force to assist the aggregation of conductive particles, so that the conductive film obtains anisotropic conductivity. It is understandable that for different conductive film materials, there are differences in the softening process, such as using ultraviolet light irradiation, ultrasonic vibration, etc., and different heat sources can be selected according to needs, which is not limited here.
[0086] S208. While maintaining the pre-pressure and heating of the entire component, apply local pressure to the upper device, so that the conductive particles inside the anisotropic conductive film are deformed under the wrapping of the insulating shell, and a conductive path is formed between the corresponding upper and lower electrodes.
[0087] Referring to step S104 , the bonding system forms a conductive path between corresponding upper and lower electrodes.
[0088] S209, while maintaining the original pressure and heating the entire component, applying a magnetic field to control the orientation of the conductive particles so that the long axis direction of the conductive particles is consistent with the connection direction of the upper and lower electrodes, and the conductive particles between adjacent electrodes are insulated.
[0089] Referring to step S105 , the bonding system controls the orientation of the conductive particles.
[0090] S210, cooling the entire component and removing the pressure, completing the bonding of the upper device and the lower device.
[0091] Referring to step S106, the bonding system completes the bonding.
[0092] S211, transferring the bonded integral components to an aging device, and placing them under preset environmental conditions for a preset test time.
[0093] Among them, the integral component refers to the component that combines the upper and lower devices with the anisotropic conductive film in the middle after bonding. The aging device is a device that can simulate the actual use environment of the product and apply stress such as temperature, humidity, and vibration to the product. It is usually composed of units such as a temperature and humidity chamber and a vibration table. The preset environmental conditions generally refer to a combination of a series of parameters such as temperature, humidity, and vibration frequency, which are used to simulate the use conditions of the device after bonding. The preset test time indicates the duration of time required to place the device in the above environmental conditions, usually from several hours to several days.
[0094] After the bonding system completes the bonding of the upper and lower devices, it needs to transfer the devices to a special reliability screening process to assess their comprehensive performance. Aging is an accelerated screening of device reliability. Specifically, the bonding system first moves the complete bonding parts to the aging room, places them in the designated positions of the temperature and humidity box and the vibration table fixture, and connects the functional test circuit. Subsequently, the system sets the temperature and humidity cycle curve of the box according to the product reliability requirements, and starts the box to adjust the temperature and humidity according to the curve. At the same time, the vibration table is set to a specific frequency so that the devices on the fixture are subjected to mechanical stress of a certain amplitude and frequency. When the temperature, humidity and vibration environment are superimposed for a certain period of time, it is considered that an aging test is completed.
[0095] Environmental aging of devices after bonding can be achieved in the following ways: Optionally, the bonding system puts the devices in the storage basket according to product type, batch, etc., and manually moves the basket to the aging room. The tester fixes the device on the fixture of the temperature, humidity and vibration integrated test equipment according to the specifications and connects the test wire. Then the temperature range, humidity range, vibration frequency, duration and other conditions are set manually, and the test equipment is started; Optionally, the bonding system is equipped with a transmission track to automatically transfer the bonded devices to the aging line. The aging equipment is electrically connected to the upper machine, reads the aging parameters of the current product from the system database, and automatically loads the test program to complete the whole process of device clamping, parameter setting, aging start and stop, etc.; Optionally, a universal aging fixture is designed for different products. After the device is loaded into each station in the fixture, the entire fixture is loaded into a large environmental chamber, and different devices are aged once under the same environmental parameters. After completion, they are automatically split and data matching is archived. It can be understood that the aging method of the device needs to be comprehensively considered according to the characteristics of the product itself, the factory production layout and other factors to balance efficiency and reliability. No limitation is made here.
[0096] S212, placing the aged integral component in a detection device, and using an electrical performance testing instrument to perform electrical parameter testing on the device.
[0097] Among them, the detection device refers to a device that integrates multiple electrical test instruments and can perform electrical parameter measurement and functional testing on devices. Common instruments include digital multimeters, oscilloscopes, signal generators, etc. Electrical parameter testing refers to collecting the voltage and current responses of devices under excitations such as DC, AC, and pulse signals, and analyzing key electrical indicators such as the device's on / off, insulation resistance, delay, and loss.
[0098] After a period of aging test, the bonding system transfers the device from the aging device to the detection platform and starts performance testing to assess the consistency and stability of its electrical performance. Specifically, the system first clamps the device to be tested on the test fixture and connects it to various test instruments through precision probes or test sockets. Then, the system applies a power supply voltage and drive signal equivalent to the operating conditions to the device, and simultaneously collects the voltage and current responses of the device electrodes. After data collection is completed, the system processes the raw electrical data, extracts key performance indicators such as resistance, capacitance, delay, and attenuation, forms a statistical distribution, and determines whether it meets the technical specifications. The test results are used to evaluate the performance status of the device after aging.
[0099] The following methods can be used for electrical performance testing: Optionally, the bonding system arranges the devices to be tested on the turntable in an orderly manner according to type, and the turntable rotates to transport the devices to the test station in turn. At the test station, the device automatically docks with the test bench, and the system retrieves the test plan of the device from the parameter library, and controls the instrument equipment to complete a series of tests such as on-off, insulation, and delay in turn. During the process, the test data is automatically saved and archived in association with the device number; Optionally, the tester places the device in the test fixture according to the specification and manually connects the signal line. The host computer selects the test program and issues the control command, and the instrument equipment automatically switches the test function and changes the excitation signal type to achieve all-round testing. The software automatically generates reports for key parameters and indicates the items that exceed the standard, which are then manually reviewed and confirmed; Optionally, a modular and probe-based test plan is adopted, and a test module is specially designed for similar products, including various sensors and signal conditioning circuits. Automated testing can be achieved by simply connecting the device to the module. The test system obtains real-time data collected by each module through wireless communication and summarizes and analyzes it. It is understandable that the electrical performance testing methods vary depending on the device type and process characteristics, such as using flying probe, ATE, etc., which are not listed here exhaustively.
[0100] S213. Compare the test results with the theoretical design values to determine whether the overall components have passed the electrical performance test.
[0101] The test result refers to the actual electrical performance indicators of the device obtained through the electrical parameter test in step S212, such as on-off resistance, insulation resistance, delay time, etc. The theoretical design value refers to the target value and range of various electrical parameters calculated based on the theoretical model according to the device circuit schematic and layout design, which are usually specified in the technical specifications. A qualified electrical performance test means that the device test results fully meet or exceed the theoretical value requirements.
[0102] After obtaining the electrical performance test data of the device after aging, the bonding system begins to determine whether it meets the factory standards. Specifically, the system compares the measured values of various electrical parameters with the theoretical design values one by one. The on-off resistance must be within the specified resistance upper and lower limits, the insulation resistance should be higher than the standard lower limit, and the signal delay must be lower than the design upper limit. The system automatically determines whether each parameter exceeds the standard and forms a test conclusion, indicating whether the device is qualified. For unqualified devices, the system will further provide a failure mode analysis. Generally, all electrical parameters of the device must meet the standards to be considered as passed. Only devices that pass the performance test can enter the subsequent use stage.
[0103] The following measures can be adopted to achieve the comparison and screening of test results: Optionally, the bonding system forms a data pair with the test data and the theoretical standard, inputs it into the statistical analysis software, automatically generates control charts and scatter plots, and intuitively displays the distribution and discreteness of device parameters. For parameters that fall outside the specification line, the system determines them as unqualified and marks them with emphasis to form a test report; Optionally, the test results are manually registered on the quality record sheet, and then compared with the technical specification design chapters one by one to confirm whether the electrical indicators meet the requirements and fill in the conclusion. For unqualified devices, the tester must also manually fill in the analysis of the causes of the failure; Optionally, a test big data analysis platform is established to summarize the product test results, and a machine learning algorithm is used to find the correlation between the test parameters and the theoretical values, and a test result prediction model is constructed. With the help of the model, the test efficiency and accuracy can be significantly improved. It is understandable that the electrical performance test is a check link for product delivery, and its result determination must take into account production factors such as speed and cost in addition to strict data comparison. The specific implementation method is not limited.
[0104] In some embodiments, the bonding system counts the number of devices that pass the electrical performance test and calculates the electrical yield; when the electrical yield is lower than the electrical yield threshold, analyzes the failure mode that causes the device performance to fail; optimizes the bonding process parameters based on the failure mode; the bonding process parameters include the pressure, heating temperature, holding time and magnetic field strength of the bonding process.
[0105] Specifically, electrical yield refers to the ratio of the number of devices that pass the electrical performance test to the total number of devices tested, and is often used to evaluate product quality and bonding process level. The electrical yield threshold represents the minimum standard for the electrical performance pass rate of bonded devices, and is usually set according to customer requirements or industry specifications. Failure mode refers to the type of physical defects that cause device performance to fail, such as electrode detachment, open connection, etc. Bonding process parameters are used to represent the key control variables of the bonding process, and the bonding quality can be optimized by adjusting the process parameters.
[0106] Specifically, the bonding system statistically analyzes the results of electrical performance tests, calculates the electrical yield index, and compares it with the pre-set threshold. When the electrical yield is found to be lower than the threshold, the system determines that the current bonding quality is unqualified and the bonding process needs to be optimized and improved. In order to find out the cause of poor bonding, the system collects unqualified devices, uses X-rays, acoustic scanning and other methods to detect internal structural defects, and identifies major failure modes, such as uneven thickness of the conductive film and device misalignment. In response to these failure modes, the system combines the expert experience database to optimize and adjust process parameters such as bonding pressure, heating temperature, and holding time, such as increasing pressure to improve the fluidity of the conductive film, and extending the holding time to enhance the reliability of the connection. The optimized process parameters are updated to the bonding equipment, and the bonding of the new batch of products is re-implemented, and electrical measurement and evaluation are performed again to verify the optimization effect. Through the continuous cycle of test feedback and parameter optimization, the continuous improvement of the bonding process is ultimately achieved.
[0107] In some embodiments, the following measures may be taken to achieve bonding process optimization: Optionally, the bonding system statistically analyzes the electrical yield and defective rate of each batch and model of products based on electrical measurement data to form a quality report; when the electrical yield of the batch is lower than a preset threshold, the system sends an early warning to the engineer and automatically extracts the bonding parameter settings of the batch from the MES system; engineers conduct failure analysis on unqualified devices based on parameter settings, examine the bonding interface morphology through an optical microscope, and screen out key defect modes; for defect modes, engineers use the expert system knowledge base to obtain defect cause analysis and corresponding process parameter adjustment suggestions; based on the engineer's judgment, the system generates optimized bonding parameters and sends them to the bonding equipment control program. Optionally, the bonding system can also automatically capture and analyze defective images of unqualified devices through machine vision technology to identify typical failure modes; based on massive historical data, the system conducts big data mining and analysis on the correlation between various failure modes and bonding parameters, and builds a parameter-defect response model; combined with the model analysis results, the system directly calculates the optimization amount of bonding parameters to achieve automatic closed-loop optimization; at the same time, the system monitors key parameters and product quality data in real time, and uses SPC statistical process control technology to determine whether the bonding process is under control, and promptly warns of abnormal parameter deviations. It is understandable that in addition to process parameters, factors such as product design, raw materials, and environmental conditions will also affect the bonding quality, and comprehensive considerations are required for actual optimization, which will not be expanded here.
[0108] In the embodiment of the present application, a conductive film filled with magnetic particles is used as a device interconnection medium, and an external magnetic field is used to induce the particles to align in a directional manner, forming a dense conductive path in the vertical direction of the conductive film. Compared with the traditional ACF conductive film, this solution does not require the application of excessive temperature and pressure, which reduces the risk of thermal damage to the device while improving the reliability and consistency of the interconnection. And under the guidance of the magnetic field, the conductive particles can slide in the film matrix, giving the conductive film a certain flexibility, which can effectively adapt to device deformation. Therefore, this interconnection scheme can be widely used in various high-density interconnection occasions such as chip stacking packaging, COF packaging, and flexible circuit board interconnection.
[0109] The following describes the bonding system in the embodiment of the present invention from the perspective of hardware processing. Figure 3 , which is a schematic diagram of a physical device structure of a bonding system in an embodiment of the present application.
[0110] It should be noted that Figure 3 The structure of the bonding system shown is only an example and should not bring any limitation to the functions and scope of use of the embodiments of the present invention.
[0111] like Figure 3As shown, the bonding system includes a central processing unit (CPU) 301, which can perform various appropriate actions and processes according to the program stored in the read-only memory (ROM) 302 or the program loaded from the storage part 308 to the random access memory (RAM) 303, such as executing the method described in the above embodiment. In the RAM 303, various programs and data required for system operation are also stored. The CPU 301, the ROM 302 and the RAM 303 are connected to each other through the bus 304. The input / output (I / O) interface 305 is also connected to the bus 304.
[0112] The following components are connected to the I / O interface 305: an input section 306 including an audio input device, a button switch, etc.; an output section 307 including a liquid crystal display (LCD) and an audio output device, an indicator light, etc.; a storage section 308 including a hard disk, etc.; and a communication section 309 including a network interface card such as a LAN (Local Area Network) card, a modem, etc. The communication section 309 performs communication processing via a network such as the Internet. A drive 310 is also connected to the I / O interface 305 as needed. A removable medium 311, such as a magnetic disk, an optical disk, a magneto-optical disk, a semiconductor memory, etc., is installed on the drive 310 as needed so that a computer program read therefrom is installed into the storage section 308 as needed.
[0113] In particular, according to an embodiment of the present invention, the process described above with reference to the flowchart can be implemented as a computer software program. For example, an embodiment of the present invention includes a computer program product, which includes a computer program carried on a computer-readable medium, and the computer program includes a computer program for executing the method shown in the flowchart. In such an embodiment, the computer program can be downloaded and installed from a network through the communication part 309, and / or installed from a removable medium 311. When the computer program is executed by the central processing unit (CPU) 301, various functions defined in the present invention are performed.
[0114] It should be noted that specific examples of computer-readable storage media may include, but are not limited to: an electrical connection with one or more wires, a portable computer disk, a hard disk, a random access memory (RAM), a read-only memory (ROM), an erasable programmable read-only memory (EPROM), a flash memory, an optical fiber, a portable compact disk read-only memory (CD-ROM), an optical storage device, a magnetic storage device, or any suitable combination thereof. In the present invention, a computer-readable storage medium may be any tangible medium containing or storing a program that may be used by or in combination with an instruction execution system, apparatus, or device.
[0115] The flowcharts and block diagrams in the accompanying drawings illustrate the possible architecture, functions and operations of the systems, methods and computer program products according to various embodiments of the present invention. Each box in the flowchart or block diagram may represent a module, a program segment, or a part of a code, and the above-mentioned module, program segment, or a part of a code contains one or more executable instructions for implementing the specified logical functions. It should also be noted that in some alternative implementations, the functions marked in the box may also occur in an order different from that marked in the accompanying drawings.
[0116] Specifically, the bonding system of this embodiment includes a processor and a memory. The memory stores a computer program. When the computer program is executed by the processor, the bonding method provided in the above embodiment is implemented.
[0117] As another aspect, the present invention further provides a computer-readable storage medium, which may be included in the bonding system described in the above embodiment; or may exist independently without being assembled into the bonding system. The above storage medium carries one or more computer programs, and when the above one or more computer programs are executed by a processor of the bonding system, the bonding system implements the bonding method provided in the above embodiment.
[0118] As described above, the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present application.
[0119] As used in the above embodiments, the term "when..." may be interpreted to mean "if..." or "after..." or "in response to determining..." or "in response to detecting...", depending on the context. Similarly, the phrases "upon determining..." or "if (the stated condition or event) is detected" may be interpreted to mean "if determining..." or "in response to determining..." or "upon detecting (the stated condition or event)" or "in response to detecting (the stated condition or event)", depending on the context.
[0120] Those skilled in the art can understand that to implement all or part of the processes in the above-mentioned embodiments, the processes can be completed by computer programs to instruct related hardware, and the programs can be stored in computer-readable storage media. When the programs are executed, they can include the processes of the above-mentioned method embodiments. The aforementioned storage media include: ROM or random access memory RAM, magnetic disk or optical disk and other media that can store program codes.
Claims
1. A bonding method, characterized in that: Applied to a bonding system, the method comprises: Pre-attaching anisotropic conductive film to the electrode surface of the lower device; the anisotropic conductive film contains a plurality of conductive particles, the conductive particles are attached with an insulating shell, and the conductive particles can be controlled in their orientation by magnetic force; Aligning the lower device and the upper device so that the electrodes of the two devices are aligned to a preset position; Applying pre-pressure to the upper device and heating the entire component to a preset temperature to preliminarily soften the anisotropic conductive film; While maintaining the pre-pressing and heating of the whole component, applying local pressure to the upper device, so that the conductive particles inside the anisotropic conductive film are deformed under the wrapping of the insulating shell, and a conductive path is formed between the corresponding upper and lower electrodes; Applying a magnetic field while maintaining the local pressure and heating the integral component, controlling the orientation of the conductive particles, making the long axis direction of the conductive particles consistent with the connection direction of the upper and lower electrodes, and insulating the conductive particles between adjacent electrodes; The entire assembly is cooled and the pressure is removed, completing the bonding of the upper device to the lower device.
2. The method according to claim 1, characterized in that The step of aligning the lower device with the upper device so that the electrodes of the two devices are aligned to a preset position specifically includes: Obtaining CAD design drawings of the lower device and the upper device, performing image processing on the CAD design drawings, and extracting shape, size, and relative position information of the respective electrodes; According to the shape, size and relative position information of the electrodes of the lower device and the upper device, the alignment parameters when the electrodes of the two are aligned are calculated; The lower component and the upper component are clamped and fixed on the alignment device, and the relative movement of the lower component and the upper component is controlled until the actual position relationship between the two meets the alignment parameters.
3. The method according to claim 1, characterized in that The step of applying pre-pressure to the upper device and heating the entire component to a preset temperature so as to preliminarily soften the anisotropic conductive film specifically includes: Acquiring material parameters of the anisotropic conductive film, and determining a target pre-pressure and a target heating temperature required for initial softening according to the material parameters; Clamping the lower device, the anisotropic conductive film and the upper device in a hot pressing device, and applying the target pre-pressure to the upper device by adjusting the hot pressing device; The hot pressing device is powered on for heating, the real-time temperature of the inner cavity of the hot pressing device is monitored, and the heating control of the hot pressing device is dynamically adjusted according to the temperature feedback signal until the temperature of the inner cavity of the hot pressing device is stabilized at the target heating temperature and the preset heating time is maintained.
4. The method according to claim 1, characterized in that: Before the step of pre-attaching the anisotropic conductive film to the electrode surface of the lower device, the method further includes: Obtaining the dimensional parameters of the upper device and the lower device after actual processing and preparation, comparing them with the design values, calculating the dimensional deviation, and determining whether the dimensional deviation is within the error range; If the dimensional deviation exceeds the error range, an alarm message is output and subsequent bonding operations are terminated.
5. The method according to claim 4, characterized in that After the steps of obtaining the dimensional parameters of the upper device and the lower device after actual processing and preparation, comparing them with the design values, calculating the dimensional deviation, and judging whether the dimensional deviation is within the error range, the method further includes: If the size deviation is within the error range, correcting the pre-attachment position and pre-attachment angle of the anisotropic conductive film according to the size deviation; The position and angle of the anisotropic conductive film are adjusted to reach the pre-attachment position and the pre-attachment angle.
6. The method according to claim 1, characterized in that After the steps of cooling the integral component and removing the local pressure to complete the bonding of the upper device and the lower device, the method further includes: Transferring the bonded integral component to an aging device and placing it under preset environmental conditions for a preset test time; The aged integral component is placed in a detection device, and an electrical performance test instrument is used to perform an electrical parameter test on the device; the electrical parameter test includes continuity, insulation, polarity, resistance, capacitance and signal delay; Compare the test results with the theoretical design values to determine whether the overall components have passed the electrical performance test.
7. The method according to claim 6, characterized in that After the step of comparing the test results with the theoretical design values to determine the devices that have passed the electrical performance test, the method further includes: Counting the number of devices that pass the electrical performance test and calculating the electrical yield; When the electrical yield is lower than an electrical yield threshold, analyzing a failure mode that causes unqualified device performance; The bonding process parameters are optimized in combination with the failure mode; the bonding process parameters include the pressure size, heating temperature, holding time and magnetic field strength of the bonding process.
8. A bonding system, characterized in that: The binding system includes: one or more processors and a memory; the memory is coupled to the one or more processors, the memory is used to store computer program code, the computer program code includes computer instructions, and the one or more processors call the computer instructions to enable the binding system to execute the method described in any one of claims 1-7.
9. A computer-readable storage medium comprising instructions, characterized in that: When the instructions are executed on a binding system, the binding system is caused to execute the method according to any one of claims 1 to 7.