Light-emitting element, display device, method for manufacturing light-emitting element, and method for manufacturing display device

By providing a low-density second region in the light emitting layer and filling an inorganic matrix, the problem of reducing luminescence efficiency caused by foreign matter intrusion is solved, the voltage requirement is reduced and the overall performance of the light emitting element is improved.

CN119054415APending Publication Date: 2024-11-29SHARP DISPLAY TECHNOLOGY CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202280094914.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2022-06-03
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

In a light emitting layer with quantum dots as luminescent material, intrusion of foreign matter such as moisture or air causes propagation and permeation between quantum dots, resulting in a decrease in luminescence efficiency and an increase in voltage, and when the quantum dot density is reduced to prevent this problem, luminescence is emitted. The efficiency is further reduced.

Method used

A light emitting layer with a plurality of quantum dots is adopted, and a first region and a second region are provided in the lamination direction. The quantum dot density of the second region is low and is filled with an inorganic matrix to prevent foreign matter from penetration, and the quantum dots are controlled during the manufacturing process. and the thickness of the inorganic matrix to protect quantum dots, reduce surfactivity and oxidation reactions.

Benefits of technology

The voltage increase required to achieve a predetermined brightness is reduced, and the luminous efficiency is improved, and the deterioration of the luminous layer caused by foreign matter intrusion is prevented, thereby maintaining the efficient performance of the luminous emitting element.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119054415A_ABST
    Figure CN119054415A_ABST
Patent Text Reader

Abstract

A light-emitting element (1) is provided with a first electrode (2), a second electrode (3), and a light-emitting layer (4) having a plurality of quantum dots (5), and the light-emitting layer (4) has a first region (P1) in which a first light-emitting layer (6) is provided and a second region (P2) in which a second light-emitting layer (8) is provided when viewed from the first electrode (2) toward the second electrode (3), i.e., in a lamination direction. The density of the quantum dots (5) in the second light-emitting layer (8) is lower than the density of the quantum dots (5) in the first light-emitting layer (6), and the second light-emitting layer (8) is filled with an inorganic compound (10) between the plurality of quantum dots (5).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a light-emitting element including quantum dots, a display device including the light-emitting element as a light-emitting element, and methods for manufacturing the same. Background Art

[0002] Patent Document 1 discloses a light-emitting element including a light-emitting layer having semiconductor nanocrystals (quantum dots) as a light-emitting material. Prior art literature Patent Literature

[0003] Patent Document 1: Japanese Patent Application Publication No. 2007-95685 Summary of the invention Technical Problems to be Solved by the Invention

[0004] If foreign matter such as moisture or air intrudes into the light-emitting layer having quantum dots as the light-emitting material, the foreign matter may spread between the multiple quantum dots and penetrate the entire light-emitting layer, which may cause the degradation of a large number of quantum dots in the light-emitting layer and reduce the light-emitting efficiency of the light-emitting element.

[0005] In order to prevent the propagation of foreign matter between quantum dots, it is also considered to reduce the density of quantum dots in the light-emitting layer. In this case, it becomes difficult for carriers injected into the quantum dots to be transported through the quantum dots, the luminous efficiency of the light-emitting layer is reduced, or the voltage applied to the light-emitting element required to obtain a specified brightness is increased. Solutions for solving problems

[0006] A light-emitting element involved in one embodiment of the present invention includes: a first electrode, a second electrode, and a light-emitting layer having a plurality of quantum dots between the first electrode and the second electrode, wherein the light-emitting layer has a first region having a first light-emitting layer and a second region having a second light-emitting layer when viewed from the first electrode toward the second electrode, i.e., in the stacking direction, wherein the density of the quantum dots in the second light-emitting layer is lower than the density of the quantum dots in the first light-emitting layer, and the second light-emitting layer is filled with an inorganic matrix between the plurality of quantum dots.

[0007] A display device involved in one embodiment of the present disclosure includes a substrate and a red light-emitting element, a green light-emitting element and a blue light-emitting element on the substrate, and each of the red light-emitting element, the green light-emitting element and the blue light-emitting element is a light-emitting element involved in one embodiment of the present disclosure.

[0008] In addition, one embodiment of the present invention relates to a method for manufacturing a light-emitting element, which is a method for manufacturing a light-emitting element including a first electrode, a second electrode, and a light-emitting layer having a plurality of quantum dots between the first electrode and the second electrode, including a light-emitting layer forming step of forming the light-emitting layer, wherein the light-emitting layer has a first region having a first light-emitting layer and a second region having a second light-emitting layer when viewed from the direction of the first electrode toward the second electrode, i.e., the stacking direction, the density of the quantum dots in the second light-emitting layer is lower than the density of the quantum dots in the first light-emitting layer, and the second light-emitting layer is filled with an inorganic matrix between the plurality of quantum dots.

[0009] In addition, a method for manufacturing a display device according to one embodiment of the present invention includes: a substrate preparation step, which prepares a substrate having a plurality of sub-pixel regions; and a light-emitting element formation step, which forms the light-emitting element in each of the sub-pixel regions on the substrate by using a method for manufacturing a light-emitting element according to one embodiment of the present invention. Effects of the Invention

[0010] The increase in applied voltage required to obtain a predetermined brightness is reduced, and the decrease in luminous efficiency of the light-emitting element as a whole due to the mixing of foreign matter into the light-emitting layer is reduced. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is a cross-sectional view of the light emitting element involved in Embodiment 1. Figure 2 It is a cross-sectional view showing the operation of the above-mentioned light emitting element. Figure 3 This is another cross-sectional view showing the operation of the light emitting element. Figure 4 is a cross-sectional view of a light emitting element according to a comparative example. Figure 5 It is a cross-sectional view showing the operation of the above-mentioned light emitting element. Figure 6 This is another cross-sectional view showing the operation of the light emitting element. Figure 7 : is a graph showing the relationship between voltage and luminance related to the operation of the light emitting element in Embodiment 1. Figure 8 It is a cross-sectional view showing the operation of the light emitting element when there is no foreign matter. Fig. 9 : is a graph showing the relationship between voltage and brightness related to the operation of the above-mentioned light-emitting element when there is no foreign matter. Fig.10 It is a cross-sectional view showing the operation of the light emitting element when there is foreign matter. Fig.11This is a graph showing the relationship between voltage and brightness related to the operation when there is foreign matter in the above-mentioned light-emitting element. Fig.12 It is a schematic diagram for explaining an image displayed on a screen by a light-emitting element according to a comparative example. Fig.13 FIG. 1 is a schematic diagram showing an image displayed on a screen by the light emitting element according to the first embodiment. Fig.14 It is a schematic diagram for explaining an image displayed on a screen by a light-emitting element according to another comparative example. Fig.15 This is a diagram for explaining the density of quantum dots formed in the first region where the light-emitting layer of the light-emitting element according to the first embodiment is provided. Fig.16 This is a diagram for explaining the density of quantum dots formed in the second region provided in the light-emitting layer. Fig.17 This is a cross-sectional view of a light emitting element according to a modification of the first embodiment. Fig.18 : is a graph showing the relationship between voltage and brightness related to the operation of the above-mentioned light emitting element. Fig.19 It is a cross-sectional view showing the operation of the light emitting element when there is no foreign matter. Fig. 20 : is a graph showing the relationship between voltage and brightness related to the operation of the above-mentioned light-emitting element when there is no foreign matter. Fig.21 It is a cross-sectional view showing the operation of the light emitting element when there is foreign matter. Fig. 22 This is a graph showing the relationship between voltage and brightness related to the operation when there is foreign matter in the above-mentioned light-emitting element. Fig.23 This is a cross-sectional view showing a method for manufacturing a light-emitting element according to Embodiment 1. Fig.24 It is a cross-sectional view showing a method for manufacturing the light emitting element. Fig.25 It is a cross-sectional view showing a method for manufacturing the light emitting element. Fig.26 It is a cross-sectional view showing a method for manufacturing the light emitting element. Fig. 27 It is a cross-sectional view showing a method for manufacturing the light emitting element. Fig.28 It is a cross-sectional view showing a method for manufacturing the light emitting element. Fig.29 It is a cross-sectional view showing a method for manufacturing the light emitting element. Fig.30It is a top view of the display device according to the first embodiment. Fig.31 It is a top view of a display device according to a modification of the first embodiment. Fig.32 FIG. 1 is a plan view of a display device according to another modification of the first embodiment. Fig.33 It is a diagram showing the energy levels of a red light-emitting element, a green light-emitting element, and a blue light-emitting element provided on the above-mentioned display device. Fig.34 It is a top view of the display device according to the second embodiment. Fig.35 Schematic diagram showing the average density of quantum dots in a plurality of divided regions of the light-emitting layer of the light-emitting element according to the third embodiment. Fig.36 is a histogram showing the average density of the above-mentioned quantum dots. Fig.37 is a schematic diagram showing another average density of the above-mentioned quantum dots. Fig.38 is a histogram showing another average density of the above-mentioned quantum dots. Fig.39 is a schematic diagram showing another average density of the quantum dots. Fig.40 is a histogram showing another average density of the quantum dots. Fig.41 is a schematic diagram showing another average density of the quantum dots. Fig.42 is a histogram showing another average density of the quantum dots. DETAILED DESCRIPTION

[0012] (Implementation Method 1) Figure 1 1 is a cross-sectional view of a light-emitting element 1 according to Embodiment 1. The light-emitting element 1 includes a first electrode 2, a second electrode 3, and a light-emitting layer 4 having a plurality of quantum dots (QD, Quantum Dot) 5 between the first electrode 2 and the second electrode 3. The first electrode 2 may be an anode. The second electrode 3 may be a cathode. A hole transport layer 13 may be formed between the light-emitting layer 4 and the first electrode 2. An electron transport layer 14 may also be formed between the light-emitting layer 4 and the second electrode 3.

[0013] In this specification, "quantum dot" refers to a dot with a maximum width of 100 nm or less. The shape of the quantum dot is not particularly limited as long as it satisfies the above-mentioned maximum width range, and is not limited to a spherical three-dimensional shape (circular cross-sectional shape). The shape of the quantum dot can be, for example, a polygonal cross-sectional shape, a rod-shaped three-dimensional shape, a branch-shaped three-dimensional shape, a three-dimensional shape with a concave-convex surface, or a combination thereof.

[0014] Typically, quantum dots can be made of semiconductors. Semiconductors can have a certain band gap. Semiconductors can be materials that can emit light, and can at least contain the following materials. Semiconductors can emit red, green and blue light, respectively. Semiconductors include at least one selected from the group consisting of II-VI compounds, III-V compounds, chalcogenides and perovskite compounds. Among them, II-VI compounds refer to compounds containing II group elements and VI group elements, and III-V compounds refer to compounds containing III group elements and V group elements. In addition, II group elements include 2 group elements and 12 group elements, III group elements include 3 group elements and 13 group elements, V group elements include 5 group elements and 15 group elements, and VI group elements can include 6 group elements and 16 group elements.

[0015] The II-VI group compound includes, for example, at least one selected from the group consisting of MgS, MgSe, MgTe, CaS, CaSe, CaTe, SrS, SrSe, SrTe, BaS, BaSe, BaTe, ZnS, ZnSe, ZnTe, CdS, CdSe, CdTe, HgS, HgSe and HgTe.

[0016] The Group III-V compound includes, for example, at least one selected from the group consisting of GaAs, GaP, InN, InAs, InP, and InSb.

[0017] Chalcogenide is a compound containing a Group VI A (16) element, and contains, for example, CdS or CdSe. Chalcogenide may also contain a mixed crystal of these.

[0018] The perovskite compound has a composition represented by the general formula CsPbX 3 , for example. The constituent element X includes at least one selected from the group consisting of Cl, Br, and I, for example.

[0019] Here, element group numbering using Roman numerals is based on the old IUPAC (International Union of Pure and Applied Chemistry) method or the old CAS (Chemical Abstracts Service) method, and element group numbering using Arabic numerals is based on the current IUPAC method.

[0020] When viewed in the direction from the first electrode 2 to the second electrode 3, that is, in the stacking direction, the light-emitting layer 4 has a first region P1 provided with the first light-emitting layer 6 and a second region P2 provided with the second light-emitting layer 8. Figure 1 As shown, when the light-emitting layer 4 is cut along a plane parallel to the stacking direction, the light-emitting layer 4 has, on its cross section, a first region P1 provided with the first light-emitting layer 6 and a second region P2 provided with the second light-emitting layer 8. In addition, the cut surface may be selected from any plane parallel to the stacking direction, and it is sufficient to confirm that the light-emitting layer 4 has the first region P1 provided with the first light-emitting layer 6 and the second region P2 provided with the second light-emitting layer 8 in at least one cross section.

[0021] The density of the quantum dots 5 in the second light-emitting layer 8 is lower than the density of the quantum dots 5 in the first light-emitting layer 6 .

[0022] The spaces between the plurality of quantum dots 5 of the second light-emitting layer 8 are filled with an inorganic compound 10. The inorganic compound 10 is composed of an inorganic matrix. In this specification, "inorganic matrix" refers to a component composed of inorganic materials that contains and holds other substances. That is, the inorganic matrix mentioned here refers to a component composed of inorganic materials that contains and holds quantum dots 5. The inorganic matrix is ​​an element constituting a film in which quantum dots are distributed.

[0023] The inorganic matrix is ​​preferably filled in the light-emitting layer 4. The inorganic matrix may fill the region other than the quantum dots 5 in the light-emitting layer 4. The inorganic matrix may bury the region other than the quantum dots 5 in the light-emitting layer 4. In addition, the outer edge of the light-emitting layer 4 does not need to be formed only by the inorganic matrix, and it does not exclude that a portion of the quantum dots 5 are exposed from the inorganic matrix.

[0024] The inorganic matrix may be a part of the light-emitting layer 4 other than the quantum dots 5 .

[0025] The inorganic matrix may contain a plurality of quantum dots 5. The inorganic matrix may also be formed to fill the space formed between the plurality of quantum dots 5. The inorganic matrix may partially or completely fill the space between the quantum dots 5.

[0026] The inorganic matrix preferably has a thickness of 1000 nm in the plane direction perpendicular to the film thickness direction. 2A continuous film of an area of ​​more than 100 nm. A continuous film refers to an area on a plane that is not separated by materials other than the material constituting the continuous film. The inorganic matrix may also use the same material as the shell material of the quantum dot 5. In this case, the average distance between adjacent cores (inter-core distance) may be more than 3 nm, or more than 5 nm. Alternatively, the average distance between the adjacent cores may be more than 0.5 times the average core diameter. The inter-core distance is the average value of the shortest distance between 20 adjacent cores in cross-sectional observation. The inter-core distance may be kept wider than the distance when the shell materials are in contact with each other. The average core diameter is the average value of the core diameters of 20 adjacent cores in cross-sectional observation. The core diameter may be the diameter of a circle having the same area as the core area in cross-sectional observation.

[0027] The concentration of the inorganic matrix in the light-emitting layer 4 can be 9% to 70% when measured based on the area ratio in the image processing in the cross-sectional observation. In addition, when the quantum dot 5 is a core / shell structure, the concentration of the shell can be 0% to 58%. In addition, when the shell material and the inorganic matrix material are the same (the constituent elements are the same), it is substantially difficult to distinguish between the shell and the inorganic matrix, so the concentration of the region combining the inorganic matrix and the shell can be the numerical range of the concentration of the inorganic matrix plus the numerical range of the concentration of the shell.

[0028] The inorganic matrix may be solid at ordinary temperature.

[0029] The light-emitting layer 4 may also be composed of quantum dots 5 and an inorganic matrix. When analyzing the light-emitting layer 4, the intensity of the carbon chain structure detected may also be below the noise. When the light-emitting layer 4 does not contain an organic ligand, the intensity of the carbon chain structure detected is weak to below the noise.

[0030] The inorganic material constituting the inorganic matrix preferably has a band gap wider than the band gap of the constituent material of the quantum dot 5. The inorganic material constituting the inorganic matrix may be a semiconductor material or an insulator material. The inorganic material constituting the inorganic matrix may also be a sulfide semiconductor. The inorganic material constituting the inorganic matrix includes, for example, metal sulfides and / or metal oxides. Metal sulfides may be, for example, zinc sulfide (ZnS), zinc magnesium sulfide (ZnMgS, ZnMgS2), gallium sulfide (GaS, Ga2S3), zinc tellurium sulfide (ZnTeS), magnesium sulfide (MgS), zinc gallium sulfide (ZnGa2S4), and magnesium sulfide (MgGa2S4). Metal oxides may be zinc oxide (ZnO), titanium oxide (TiO2), tin oxide (SnO2), tungsten oxide (WO3), and zirconium oxide (ZrO2). In addition, the chemical formula recorded in brackets after the compound name is a representative example. In addition, with respect to the composition ratio recorded in the chemical formula, it is preferred if the composition of the actual compound is stoichiometric as shown in the chemical formula, but it may not necessarily be stoichiometric.

[0031] In addition, the structure of the above inorganic matrix is ​​observed with a width of about 100 nm in the cross-section observation of the light-emitting layer 4. It is sufficient to know that it is the above structure, and it is not necessary to observe the entire light-emitting layer 4.

[0032] In addition, the inorganic matrix only needs to be mainly composed of an inorganic material, and there is no problem in adding a material different from the main inorganic material as an additive.

[0033] The second light-emitting layer 8 may also be filled with organic compounds between the plurality of quantum dots 5. The plurality of quantum dots 5 of the first light-emitting layer 6 may be filled with inorganic compounds 10 or organic compounds.

[0034] In a display including an LED (Light Emitting Diode) element having quantum dots 5, pixels may not emit light due to foreign matter including oxygen or water.

[0035] When the density of quantum dots 5 is high, the actual thickness of the medium (or inorganic medium) protecting the surface defects of quantum dots 5 is thin, so the surface activity of quantum dots 5 is high and easy to react. In addition, the number of quantum dots 5 in a certain volume where oxygen and water diffuse increases. Therefore, if foreign matter containing oxygen and water enters the pixel when manufacturing the display, the quantum dots 5 will be oxidized in a chain reaction, and sometimes the entire pixel will become non-luminous. That is, dark spots are generated in the image display of the display. On the other hand, if the density of quantum dots 5 is reduced, the thickness of the inorganic medium around the quantum dots 5 becomes thicker, so it is difficult to inject current, the luminous efficiency is reduced, and the power consumption of the entire display increases, so the density of quantum dots 5 cannot be reduced in the entire pixel.

[0036] Therefore, in the first embodiment, the second region P2 where the density of the quantum dots 5 is low is provided in the stacking surface of the light emitting layer 4 of each pixel in the display.

[0037] Figure 2It is a cross-sectional view showing the operation of the light emitting element 1 . Figure 3 This is another cross-sectional view showing the operation of the light emitting element 1 .

[0038] In the second region P2 where the second light-emitting layer 8 has a low QD density, the inorganic medium containing the inorganic compound 10 that protects the QD surface defects of the quantum dots 5 is substantially thick. Therefore, in the second region P2, the activity of the QD surface becomes low, making it difficult to react, and the number of quantum dots 5 that enter a certain volume where oxygen and water diffuse is small. Figure 2 As shown, even if foreign matter 15 containing oxygen and water enters the light-emitting layer 4, Figure 3 As shown, even if the oxidation of the quantum dots 5 in the first region P1 has already been progressed, the oxidation is difficult to proceed in the quantum dots 5 in the second region P2. Figure 2 and Figure 3 The shaded color of the quantum dot 5 shown indicates that the darker the color, the more severe the oxidation. The same applies to the following figures.

[0039] On the other hand, in the first region P1 provided with the first light-emitting layer 6, since the density of the quantum dots 5 is greater than that in the second region P2, current injection into the first light-emitting layer 6 becomes easier, and the driving voltage of the first light-emitting layer 6 is reduced. Therefore, the light-emitting element 1 involved in this embodiment can reduce the increase in power consumption by the first light-emitting layer 6, and reduce the possibility of becoming a non-luminescent element due to the invasion of foreign matter by the second light-emitting layer 8.

[0040] Figure 4 It is a cross-sectional view of a light emitting element 91 according to a comparative example. Figure 5 It is a cross-sectional view showing the operation of the light emitting element 91 . Figure 6 2 is another cross-sectional view showing the operation of the light emitting element 91. The same components as those described above are denoted by the same reference numerals, and detailed description thereof will not be repeated.

[0041] The light emitting element 91 includes a first electrode 2, a second electrode 3, and a light emitting layer 94 having a plurality of quantum dots 5 between the first electrode 2 and the second electrode 3. The light emitting layer 94 corresponds to the reference Figure 1 The first light-emitting layer 6.

[0042] The quantum dots 5 are nanometer-sized and highly active and reactive. When the density of the quantum dots 5 is high, the thickness of the inorganic medium that protects the surface defects of the quantum dots 5 is thin. Therefore, the surface activity of the quantum dots 5 is high, and they are easy to react. Moreover, the number of quantum dots 5 that enter a certain volume where oxygen and water diffuse is large. Therefore, Figure 5 As shown, when foreign matter 15 containing oxygen and water enters the light-emitting layer 94, the quantum dots 5 are oxidized in a chain reaction, as shown in FIG. Figure 6 As shown, the entire pixel of the light emitting element 91 does not emit light.

[0043] Figure 7 Graph showing the relationship between voltage and brightness related to the operation of the light emitting element 1. The horizontal axis represents the voltage applied between the first electrode 2 and the second electrode 3 of the light emitting element 1 to make the light emitting element 1 emit light. The vertical axis represents the brightness of the light emitting element 1 emitted by the voltage.

[0044] Curve C1 shows the voltage-luminance characteristics of quantum dots 5 in first region P1 of light-emitting layer 4 where the QD density is high. Curve C2 shows the voltage-luminance characteristics of quantum dots 5 in second region P2 of light-emitting layer 4 where the QD density is low.

[0045] As shown in the curve C1, the voltage V driving the quantum dots 5 in the first region P1 is the voltage V when the brightness L is zero. th1 Above, when the brightness L is L max When V 1max the following.

[0046] In the second region P2, the density of the quantum dots 5 is lowered compared to the first region P1, and the protection of the quantum dots 5 is strengthened, but on the other hand, current injection becomes difficult and the voltage V becomes higher.

[0047] As shown in the curve C2, the voltage V driving the quantum dots 5 in the second region P2 becomes a voltage V when the brightness L is zero. th1 Large voltage V th2 , at brightness L max When the voltage becomes V 2max .

[0048] Figure 8 It is a cross-sectional view showing the operation of the light emitting element 1 when there is no foreign matter 15 . Fig. 9 1 is a graph showing the relationship between voltage and brightness in relation to the operation of the light emitting element 1 when there is no foreign matter 15. The same components as those described above are denoted by the same reference numerals, and detailed description thereof will not be repeated.

[0049] When the foreign matter 15 does not invade the light-emitting layer 4, the voltage V th1 ~V 1max Therefore, the light emitting element 1 is driven within the range of V th2 (>V 1max ) in the second region P2 does not emit light.

[0050] Fig.10 It is a cross-sectional view showing the operation of the light emitting element 1 when there is a foreign object 15 . Fig.111 is a graph showing the relationship between voltage and brightness in relation to the operation when foreign matter 15 is present in light emitting element 1. Components identical to those described above are denoted by the same reference numerals, and detailed description of these components will not be repeated.

[0051] When the foreign matter 15 invades the light-emitting layer 4, the oxidation of the quantum dots 5 in the first region P1 is easy to proceed. Therefore, at least the electronic energy level of the surface (and the inside) of the quantum dots 5 in the first region P1 changes greatly, and it is difficult to inject current into the carrier transport layer suitable for the electronic energy level of the unoxidized quantum dots 5. In other words, it is difficult for current to flow in the first region P1. Therefore, in the above case, current is injected only into the second region P2. That is, by applying the voltage V th2 ~V 2max The light-emitting element 1 is driven within a range so that the quantum dots 5 included in the second region P2 of the light-emitting layer 4 emit light.

[0052] As a specific driving method, after manufacturing a display including the light emitting element 1, as a test drive, a voltage V 1max All pixels are driven. Furthermore, by finding the non-luminous pixels, it is determined that the non-luminous pixels have foreign matter 15, and it is determined that the luminous pixels do not have foreign matter. Then, the judgment result is fed back to the driving unit of the light-emitting element 1. The driving unit drives the non-luminous pixels judged to have foreign matter based on the curve C2, and drives the luminous pixels judged to have no foreign matter based on the curve C1.

[0053] This driving method can be implemented within the scope of inspection generally performed for correcting brightness variations of pixels in the manufacturing process of a display.

[0054] Alternatively, the relationship between the driving current and the brightness of the first area P1 can be measured in advance, and the driving current based on them can be used to drive both the pixels without the foreign matter 15 and the pixels with the foreign matter 15 with a constant current. The pixels without the foreign matter 15 can emit light at a specified brightness. In the pixels with the foreign matter 15, since the area of ​​the second area P2 is smaller than the area of ​​the first area P1, the current density driving the second area P2 becomes larger accordingly, so that the reduction in the light-emitting area caused by the light emission only in the second area can be automatically compensated, and the brightness of the pixel can be maintained to a certain extent. In this way, the dark spot 20 ( Fig.12 ) is not noticeable to the human eye.

[0055] Fig.12 It is a schematic diagram for explaining an image displayed on a screen by the light emitting element 91 according to the comparative example. Fig.13 FIG. 1 is a schematic diagram showing an image displayed on a screen by the light emitting element 1 according to the first embodiment. Fig.14Schematic diagram for explaining an image displayed on a screen by a light emitting element 81 according to another comparative example. Components identical to the above-described components are denoted by the same reference numerals, and detailed descriptions of these components will not be repeated.

[0056] The light emitting layer 94 of the light emitting element 91 has only the first region P1. The light emitting layer 84 of the light emitting element 81 has only the second region P2.

[0057] [Table 1] As shown in Table 1, the power consumption of the display device in which the light emitting layer 94 includes the light emitting element 91 having only the first region P1 is set to 100%. Since the inorganic dielectric portion of the light emitting element 91 is thinned, Fig.12 As shown, non-luminous pixels are produced due to QD degradation caused by foreign matter 15.

[0058] In the case where the light-emitting layer 84 is a light-emitting element 81 having only the second region P2, it is difficult to inject current due to the low density of the quantum dots 5, and the luminous efficiency is reduced (set to 1 / 2 of the luminous efficiency of the light-emitting element 91 having only the first region P1), and the power consumption of the display is 200%. On the other hand, the inorganic compound 10 of the inorganic medium portion becomes thicker, and the protection of the quantum dots 5 becomes stronger. Therefore, since the quantum dots 5 are not degraded due to foreign matter 15, Fig.14 As shown, no non-luminous pixels are generated.

[0059] In the light emitting element 1 according to the first embodiment, in the pixel without the foreign matter 15, only the first region P1 (area ratio 0.9) is made to emit light. The second region P2 does not contribute to the light emission. Therefore, since the driving current of the first region P1 is increased to obtain the same brightness (1 / 0.9 times) as the light emitting element 91 of only the first region P1, the power consumption of the light emitting element 1 is increased compared with the light emitting element 91.

[0060] In the pixel with foreign matter 15, the first area P1 becomes non-luminescent due to weak protection of the quantum dot 5. Therefore, only the second area P2 (area ratio 0.1) is driven. Therefore, the current driving the pixel becomes larger (1 / 0.1×2=20 times), but since the number of pixels with foreign matter 15 is very small compared to the number of pixels without foreign matter 15, it does not contribute to the overall power consumption of the display.

[0061] To reduce the power consumption of the display of this embodiment to 150% or less, the area ratio of the second region P2 may be set to 0.33 or less. In order to ensure the light emission brightness of the pixel where the foreign matter 15 is located, the area ratio of the second region P2 is preferably 0.1 or more.

[0062] That is, the area ratio of the second region P2 to the total area of ​​the first region P1 and the second region P2 is preferably 10% to 33%. For example, in any cross section along the stacking direction of the light-emitting layer 4, the area of ​​the second region P2 is preferably 10% to 33% of the total area of ​​the first region P1 and the second region P2.

[0063] Fig.15 It is a diagram for explaining the density of the quantum dots 5 formed in the first region P1 where the light-emitting layer 4 of the light-emitting element 1 is provided. Fig.16 This is a diagram for explaining the density of the quantum dots 5 formed in the second region P2 provided in the light-emitting layer 4 .

[0064] The structure of the light emitting element 1 according to the first embodiment can be verified by cross-sectional TEM (Transmission Electron Microscopy). The density of the quantum dots 5 can be determined by the area filling rate of the cross section along the stacking direction of the light emitting layer 4 (the ratio of the cross-sectional area of ​​the quantum dots 5 to the entire area).

[0065] In the case of the densest packing (quantum dots 5 are spherical), the area filling rate is 91%. If the particle size of the quantum dots 5 is d (= 5 nm) and the distance between the quantum dots 5 is L, the area filling rate is given by [Mathematical formula 1] If the distance L is greater than 2nm (ZnS lattice constant 0.5nm×4 layers) (area filling rate less than 46%), the surface defects of the quantum dots 5 are fully protected by the inorganic compound 10, and the quantum dots 5 will not be oxidized. In addition, if the area filling rate is less than 30%, current injection cannot be performed, and the quantum dots 5 do not emit light. Therefore, the area filling rate of the second region P2 is preferably 30% to 46%. For the first region P1, in order to improve current injection, the distance L is preferably less than 1nm (ZnS lattice constant 0.5nm×2 layers) (area filling rate greater than 63%).

[0066] In summary, the area filling rate of the first region P1 is preferably 63% to 91%. In addition, the density of the quantum dots 5 in the second region P2 is preferably 30% to 46%.

[0067] When the shape of the quantum dot 5 is a cube, the diameter d (=5 nm) is taken as the length of one side of the cube, and the area filling rate at the time of closest packing is taken as 100%, and the calculation is carried out to fall within the following range.

[0068] That is, the area filling rate of the first region P1 is preferably 69% to 100%, and the density of the quantum dots 5 in the second region P2 is preferably 30% to 51%.

[0069] Fig.17 2 is a cross-sectional view of a light emitting element 1A according to a modification of Embodiment 1. The same components as those described above are denoted by the same reference numerals, and detailed descriptions of these components will not be repeated.

[0070] The light-emitting element 1A includes a first electrode 2, a second electrode 3, and a light-emitting layer 4A having a plurality of quantum dots 5 between the first electrode 2 and the second electrode 3. The light-emitting layer 4A has a first region P1 having a first light-emitting layer 6 and a second region P2A having a second light-emitting layer 8A in a direction from the first electrode 2 to the second electrode 3, i.e., in a stacking direction.

[0071] The density of the quantum dots 5 along the stacking direction in the second light-emitting layer 8A is the same as the density of the quantum dots 5 along the stacking direction in the first light-emitting layer 6. However, the density of the quantum dots 5 along the crossing direction intersecting the stacking direction in the second light-emitting layer 8A is lower than the density of the quantum dots 5 along the crossing direction in the first light-emitting layer 6.

[0072] Thus, the second region P2A has substantially the same QD density in the longitudinal direction as the first region P1, and only has a smaller QD density in the lateral direction. Water and oxygen caused by foreign matter diffuse only into the first region P1, and do not diffuse into the second region P2A.

[0073] Fig.18 2 is a graph showing the relationship between voltage and luminance related to the operation of the light emitting element 1A. The same components as those described above are denoted by the same reference numerals, and detailed description of these components will not be repeated.

[0074] Curve C3 represents the voltage-luminance characteristics of quantum dots 5 in the first region P1 with high QD density along the above-mentioned intersection direction of the light-emitting layer 4A. Curve C4 represents the voltage-luminance characteristics of quantum dots 5 in the second region P2A with low QD density along the above-mentioned intersection direction of the light-emitting layer 4A.

[0075] Since the QD density in the longitudinal direction of the first region P1 and the second region P2A is the same, Fig.18 As shown, both have a light-emitting threshold voltage V th1 (=V th2 ) emits light. However, compared with the first region P1, the lateral QD density of the second region P2A is low, so Fig.18 As shown, under the same voltage, the brightness of the quantum dots 5 in the second region P2A shown by the curve C4 is small.

[0076] In this way, since the light emission threshold voltage can be made the same in the first region P1 and the second region P2A, the driving voltage of the pixel having foreign matter can be reduced.

[0077] Fig.19It is a cross-sectional view showing the operation of the light emitting element 1A when there is no foreign matter. Fig. 20 Graph showing the relationship between voltage and brightness in relation to the operation of the light emitting element 1A when there is no foreign matter. Components identical to the above components are denoted by the same reference numerals, and detailed description of these components will not be repeated.

[0078] When the foreign matter 15 does not invade the light emitting layer 4A, the voltage V th1 ~V 1max Then, as shown by curve C5, the brightness becomes the sum of the brightness of the quantum dots 5 in the first region P1 and the brightness of the quantum dots 5 in the second region P2A.

[0079] Fig.21 It is a cross-sectional view showing the operation of the light emitting element 1A when there is foreign matter. Fig. 22 1A is a graph showing the relationship between voltage and brightness in relation to the operation of the light emitting element 1A when foreign matter is present. Components identical to the above-described components are denoted by the same reference numerals, and detailed descriptions of these components will not be repeated.

[0080] When foreign matter 15 enters the light emitting layer 4, only the second region P2A is driven. th2 ~V 2max The second region P2A is driven within a range of , so that the second region P2A emits light. Since the second region P2A has a lower brightness than the first region P1 at the same voltage, the brightness is compensated by driving with a high voltage. At this time, the first region P1 does not emit light.

[0081] As a driving method, after manufacturing a display including the light emitting element 1A, V 1max Drive all pixels by finding the brightness that does not reach L max The pixels are used to determine whether there is a foreign object and provide feedback to the driver.

[0082] Figure 23 to Figure 29 2 is a cross-sectional view showing a method for manufacturing the light emitting element 1 according to Embodiment 1. The same components as those described above are denoted by the same reference numerals, and detailed descriptions of these components will not be repeated.

[0083] First, a layer from the first electrode 2 to the hole transport layer 13 is formed by a general method such as evaporation, sputtering, coating, inkjet, etc. Fig.23 As shown, the portion of the hole transport layer 13 corresponding to the first region P1 is covered with the first resist layer 16 .

[0084] Then, if Fig.24 As shown, the second light emitting layer 8 of the second region P2 is formed by coating or the like.

[0085] Then, if Fig.25 As shown, the first resist layer 16 is removed from the hole transport layer 13 .

[0086] Then, if Fig.26 As shown, the second light emitting layer 8 of the second region P2 is covered with the second resist layer 17. In the second light emitting layer 8 of the second region P2, since the density of the quantum dots 5 is low, the quantum dots 5 are strongly protected, and therefore, the quantum dots 5 are not easily degraded by coating and peeling of the second resist layer 17.

[0087] Then, if Fig. 27 As shown, the first light emitting layer 6 is formed in the first region P1 by coating or the like.

[0088] Then, if Fig.28 As shown, the second resist layer 17 is removed from the second light emitting layer 8 .

[0089] Then, the electron transport layer 14 and the second electrode 3 are formed by a common method such as vapor deposition, sputtering, coating, ink jetting, etc., thereby completing the light emitting element 1 .

[0090] The following solutions can be used as the quantum dot solution for forming the first light-emitting layer 6 in the first region P1 and the quantum dot solution for forming the second light-emitting layer 8 in the second region P2.

[0091] In the case of an inorganic solution, quantum dots 5 and a ZnS precursor (zinc thiourea, etc.) are mixed and coated (solvent: DMF (N, N-dimethylformamide, N, N-dimethylformamide) etc.), and the ZnS precursor is reacted by heating at 250°C for 30 minutes to form ZnS. Furthermore, by changing the ratio between quantum dots 5 and the ZnS precursor, the density of quantum dots 5 in ZnS can be changed.

[0092] In the case of an organic solution, a dispersion solution (solvent: hexane, octane, etc.) of quantum dots 5 having organic ligands is applied. Heating may be performed to volatilize the solvent after application.

[0093] In this way, the second region P2 is manufactured earlier than the first region P1, and thus the second light-emitting layer 8 formed with the thick inorganic compound 10 having a protective function is formed earlier than the first light-emitting layer 6. Therefore, the second light-emitting layer 8 can be prevented from being degraded by the implementation of the subsequent steps. In particular, in the case of forming the ZnS of the second light-emitting layer 8 by heating a solution containing a ZnS precursor, the damage caused by the heating is difficult to propagate to the first light-emitting layer 6 and the like by the above-mentioned manufacturing method.

[0094] Fig.301 is a plan view of a display device 18 according to Embodiment 1. The same components as those described above are denoted by the same reference numerals, and detailed descriptions of these components will not be repeated.

[0095] The display device 18 includes a substrate 19 and a red light emitting element 12R, a green light emitting element 12G, and a blue light emitting element 12B on the substrate 19. The red light emitting element 12R, the green light emitting element 12G, and the blue light emitting element 12B are configured similarly to the light emitting element 1 described above.

[0096] That is, the red light-emitting element 12R has a first light-emitting layer 6R corresponding to the first region P1R having a high density of quantum dots 5, and a second light-emitting layer 8R corresponding to the second region P2R having a low density of quantum dots 5. The green light-emitting element 12G has a first light-emitting layer 6G corresponding to the first region P1G having a high density of quantum dots 5, and a second light-emitting layer 8G corresponding to the second region P2G having a low density of quantum dots 5. The blue light-emitting element 12B has a first light-emitting layer 6B corresponding to the first region P1B having a high density of quantum dots 5, and a second light-emitting layer 8B corresponding to the second region P2B having a low density of quantum dots 5.

[0097] The ratio between the area of ​​the first region P1R and the area of ​​the second region P2R, the ratio between the area of ​​the first region P1G and the area of ​​the second region P2G, and the ratio between the area of ​​the first region P1B and the area of ​​the second region P2B are equal.

[0098] Each light-emitting element of the display device 18 involved in this embodiment can also be manufactured by the same manufacturing method as the light-emitting element 1 involved in the previous embodiment. Here, in the manufacturing method of the display device 18, the first electrode 2 and the light-emitting layer 4 of the light-emitting element 1 can be formed in each sub-pixel region of the substrate 19, and the remaining layers are formed in common for multiple sub-pixel regions.

[0099] In this case, for example, the light-emitting layer 4 of each light-emitting element of the display device 18 can also be formed by using a pattern of a resist. For example, in the manufacturing method of the display device 18 involved in the present embodiment, a substrate 19 having a plurality of sub-pixel regions is prepared, on which a first electrode 2 is formed in common for each sub-pixel region, and a hole transport layer 13 is formed in common for a plurality of sub-pixel regions. Next, a first resist layer 16 is formed for each sub-pixel region. Next, a second light-emitting layer 8 is formed in common for a plurality of sub-pixel regions by the above method. Next, the second light-emitting layer 8 is patterned by removing the first resist layer 16. Next, a second resist layer 17 is formed at a position including the upper surface of the second light-emitting layer 8. Next, a first light-emitting layer 6 is formed in common for a plurality of sub-pixel regions by the above method. Next, the first light-emitting layer 6 is patterned by removing the second resist layer 17. Next, the remaining electron transport layer 14 and the second electrode 3 are formed in common for a plurality of sub-pixel regions. As described above, the display device 18 can be manufactured. The patterning of the first light-emitting layer 6 and the second light-emitting layer 8 in each light-emitting element of the display device 18 may be performed for each light-emitting element emitting the same wavelength.

[0100] Fig.31 Components identical to those described above are denoted by the same reference numerals, and detailed descriptions of these components will not be repeated.

[0101] In the display device 18A, among the red light emitting element 12R, the green light emitting element 12G, and the blue light emitting element 12B, only the blue light emitting element 12B is configured similarly to the above-mentioned light emitting element 1 .

[0102] That is, the red light emitting element 12R has only the first region P1R with a high density of quantum dots 5. The green light emitting element 12G has only the first region P1G with a high density of quantum dots 5. And the blue light emitting element 12B has both the first region P1B with a high density of quantum dots 5 and the second region P2B with a low density of quantum dots 5.

[0103] The reason why the second region P2B with a low density of quantum dots 5 is provided only on the blue light-emitting element 12B is that the blue light-emitting quantum dots 5 of the blue light-emitting element 12B are more easily degraded by oxygen, moisture, etc. than the quantum dots 5 of the red light-emitting element 12R and the green light-emitting element 12G.

[0104] Fig.32 It is a plan view showing the structure of a display device 18B according to another modification. Fig.3318B is a diagram showing the energy levels of red light emitting element 12R, green light emitting element 12G, and blue light emitting element 12B provided on display device 18B. Components identical to the above components are denoted by the same reference numerals, and detailed descriptions of these components will not be repeated.

[0105] For two of the red light emitting element 12R, the green light emitting element 12G, and the blue light emitting element 12B, the light emitting element with a shorter light emitting wavelength is regarded as a short wavelength element, and the light emitting element with a longer light emitting wavelength is regarded as a long wavelength element. Here, in a combination of at least one of the short wavelength element and the long wavelength element, in any cross section of the display device 18B along the stacking direction of the short wavelength element or the long wavelength element, the cross section of the light emitting layer 4 of the short wavelength element and the cross section of the light emitting layer 4 of the long wavelength element are compared. At this time, in the cross section, the ratio of the area of ​​the second region P2R, P2G, or P2B to the total area of ​​the light emitting layer 4 of the short wavelength element is smaller than the ratio of the area of ​​the second region P2R, P2G, or P2B to the total area of ​​the light emitting layer 4 of the long wavelength element.

[0106] For example, the red light-emitting element 12R has a first light-emitting layer 6R corresponding to a first region P1R having a high density of quantum dots 5, and a second light-emitting layer 8R corresponding to a second region P2R having a low density of quantum dots 5. The green light-emitting element 12G has a first light-emitting layer 6G corresponding to a first region P1G having a high density of quantum dots 5, and a second light-emitting layer 8G corresponding to a second region P2G having a low density of quantum dots 5. The blue light-emitting element 12B has a first light-emitting layer 6B corresponding to a first region P1B having a high density of quantum dots 5, and a second light-emitting layer 8B corresponding to a second region P2B having a low density of quantum dots 5.

[0107] The ratio of the area of ​​the second region P2B to the total area of ​​the first region P1B and the second region P2B is smaller than the ratio of the area of ​​the second region P2G to the total area of ​​the first region P1G and the second region P2G. Furthermore, the ratio of the area of ​​the second region P2G to the total area of ​​the first region P1G and the second region P2G is smaller than the ratio of the area of ​​the second region P2R to the total area of ​​the first region P1R and the second region P2R. That is, the area ratios of the second regions P2R, P2G, and P2B increase in the order of the second region P2R, the second region P2G, and the second region P2B.

[0108] When the hole transportation layer (HTL) 13 and the electron transportation layer (ETL) 14 are set to be shared by each color, the side with a short luminous wavelength (large band gap and shallow CBM (Conduction Band Minimum)) is more likely to cause electron deficiency and excess holes. Therefore, even in the second region P2R, P2G, and P2B where the density of quantum dots 5 is low (effectively suppressing the injection of holes with thick inorganic compounds and lower mobility than electrons), it is easy to achieve carrier balance. Therefore, the shorter the luminous wavelength, the greater the brightness of the second region P2R, P2G, and P2B, so the area ratio of the second region P2R, P2G, and P2B can be reduced. That is, the side with a shorter luminous wavelength can increase the area ratio of the first region P1R, P1G, and P1B, thereby reducing the power consumption of the display.

[0109] Therefore, the area ratio of the first region of the light-emitting element with a shorter emission wavelength is larger than the area ratio of the first region of the light-emitting element with a longer emission wavelength. That is, for example, the area ratio of the first region P1B of the blue light-emitting element 12B with a shorter emission wavelength is larger than the area ratios of the first region P1R and the first region P1G of the red light-emitting element 12R and the green light-emitting element 12G with a longer emission wavelength. Moreover, the area ratio of the first region P1G of the green light-emitting element 12G with a shorter emission wavelength is larger than the area ratio of the first region P1R of the red light-emitting element 12R with a longer emission wavelength.

[0110] (Implementation Method 2) Fig.34 1 is a plan view of a display device 18C according to Embodiment 2. The same components as those described above are denoted by the same reference numerals, and detailed descriptions of these components will not be repeated.

[0111] The display device 18C includes a substrate 19, and a red light emitting element 12R, a green light emitting element 12G, and a blue light emitting element 12B on the substrate 19. In any cross section along the stacking direction of the light emitting layer 4 of the red light emitting element 12R, the first region P1R is sandwiched by the second region P2R. In addition, in any cross section along the stacking direction of the light emitting layer 4 of the green light emitting element 12G, the first region P1G is sandwiched by the second region P2G. In any cross section along the stacking direction of the light emitting layer 4 of the blue light emitting element 12B, the first region P1B is sandwiched by the second region P2B.

[0112] The second region P2R surrounds the first region P1R when viewed from the stacking direction of the light emitting layer 4. The second region P2G surrounds the first region P1G when viewed from the stacking direction. The second region P2B surrounds the first region P1B when viewed from the stacking direction of the light emitting layer 4.

[0113] At the periphery of the red light-emitting element 12R, the green light-emitting element 12G, and the blue light-emitting element 12B, foreign matter and impurities can easily invade from the cross section of the light-emitting layer 4, and the quantum dot 5 can be easily degraded. Therefore, by forming the second regions P2R, P2G, and P2B at the periphery of the red light-emitting element 12R, the green light-emitting element 12G, and the blue light-emitting element 12B, respectively, the quantum dot 5 can be protected from degradation. In addition, although the diagram shows a case where all the light-emitting elements have the above-mentioned structure, this is not necessarily the case. As long as one light-emitting element also has the above-mentioned structure, the above-mentioned effect can be achieved. In addition, the structure in the cross section does not need to be confirmed in multiple cross sections, as long as the above-mentioned structure can be confirmed in at least one cross section. This is because the above-mentioned effect is achieved at least in its cross section.

[0114] (Implementation Method 3) Fig.35 Schematic diagram showing the average density of the quantum dots 5 in the 20 divided regions Q1 to Q20 of the light emitting layer 4 of the light emitting element 1 according to the third embodiment. Fig.36 2 is a histogram showing the average density of the quantum dots 5 in the light emitting layer 4. The same components as those described above are denoted by the same reference numerals, and detailed description of these components will not be repeated.

[0115] In any cross section of the light-emitting layer 4 along the stacking direction, a range of 600 nm in a direction orthogonal to the stacking direction is divided into 20 segmented regions Q1 to Q20 with a width of 30 nm. In addition, for any segmented region among the segmented regions Q1 to Q20 and any other segmented regions, it is determined whether the first average density D1 representing the average density of quantum dots in any segmented region and the second average density D2 representing the average density of quantum dots in any other segmented region satisfy D2<0.7×D1. Furthermore, if any of the multiple combinations of the segmented regions Q1 to Q20 and any other segmented regions also satisfy D2<0.7×D1, the light-emitting layer 4 satisfies condition 1 of D2<0.7×D1.

[0116] In this case, the area greater than (D1+D2) / 2 in the divided areas Q1 to Q20 of the light-emitting layer 4 can be regarded as the first area P1, and the area less than (D1+D2) / 2 can be regarded as the second area P2. In addition, the density of an arbitrarily determined value can be set to D3, the area with a density greater than D3 can be set to the first area P1, and the area with a density less than D3 can be set to the second area P2. In the case of calculation by any method, when the divided areas Q1 to Q20 of the light-emitting layer 4 satisfy the above-mentioned condition 1, it can be considered that the light-emitting layer 4 has a first light-emitting layer 6 and a second light-emitting layer 8 with a density of quantum dots 5 lower than that of the first light-emitting layer 6. The width of the divided areas Q1 to Q20 can be 20nm to 40nm, which is about 2 to 3 times the particle size of the quantum dots 5.

[0117] In addition, the density of the quantum dot 5 is obtained by image processing in the cross-sectional TEM image, and is classified into about 10 levels from density 0 to the maximum as the ratio of the quantum dot area in the segmented area of ​​a fixed area (the above-mentioned fixed width × layer thickness). In addition, in the case where a quantum dot crosses the boundary with the adjacent segmented area, the area of ​​the quantum dot is divided by the boundary line, and in each area, the divided part is counted as the area of ​​the quantum dot.

[0118] Furthermore, when the average density of the quantum dots 5 in each of the divided regions Q1 to Q20 is divided into 10 levels from 0 to the maximum, it is assumed that the histogram obtained by accumulating the number of divided regions in each level satisfies condition 2 having at least two local maxima.

[0119] In this case, the area above (D1+D2) / 2 in the divided areas Q1 to Q20 of the light-emitting layer 4 can be regarded as the first area P1, and the area below (D1+D2) / 2 can be regarded as the second area P2. In other words, when the divided areas Q1 to Q20 of the light-emitting layer 4 satisfy the above condition 2, it can be considered that the light-emitting layer 4 has the first light-emitting layer 6 and the second light-emitting layer 8 having a density of quantum dots 5 lower than that of the first light-emitting layer 6.

[0120] exist Fig.35 In FIG. 1 , the average density of the quantum dots 5 in each of the divided regions Q1 to Q20 is recorded as a numerical value.

[0121] For example, if the combination of segmented area Q2 with an average density of quantum dots 5 of 9 and segmented area Q16 with an average density of quantum dots 5 of 4 is considered among a plurality of combinations of any segmented area among segmented areas Q1 to Q20 and any other segmented areas, then since the first average density D1 = 9 and the second average density D2 = 4, it becomes 0.7×D1=6.3, satisfying condition 1 of D2=0.7×D1. Furthermore, Fig.36The histogram shown has two local maxima of density 5 and density 8, thus satisfying condition 2. Therefore, it can be considered that the light emitting layer 4 according to this embodiment has a first light emitting layer 6 and a second light emitting layer 8. The threshold between the first region P1 and the second region P2 is (D1+D2) / 2=6.5.

[0122] Fig.37 Schematic diagram showing the average density of the quantum dots 5 in the light-emitting layer 4 according to another embodiment. Fig.38 2 is a histogram showing another average density of the quantum dots 5 in the light emitting layer 4. The same components as those described above are denoted by the same reference numerals, and detailed descriptions of these components will not be repeated.

[0123] exist Fig.37 , the average density of the quantum dots 5 in each of the divided regions Q1 to Q20 according to another embodiment is described in numerical values.

[0124] For example, if a combination of segmented area Q8 with an average density of quantum dots 5 of 9 and segmented area Q18 with an average density of quantum dots 5 of 7 is considered among any of the segmented areas Q1 to Q20 and multiple combinations of any other segmented areas, the first average density D1 = 9 and the second average density D2 = 7, which is 0.7×D1=6.3, which does not satisfy condition 1 of D2=0.7×D1, but Fig.38 The histogram shown has two local maxima of density 7 and density 9, thus satisfying condition 2. Therefore, it can be considered that the light emitting layer 4 according to this embodiment has a first light emitting layer 6 and a second light emitting layer 8. The threshold between the first region P1 and the second region P2 is (D1+D2) / 2=8.

[0125] Fig.39 Schematic diagram showing the average density of the quantum dots 5 in the light-emitting layer 4 according to still another embodiment. Fig.40 2 is a histogram showing another average density of the quantum dots 5 in the light emitting layer 4. The same components as those described above are denoted by the same reference numerals, and detailed description of these components will not be repeated.

[0126] exist Fig.39 , the average density of the quantum dots 5 in each of the divided regions Q1 to Q20 according to other embodiments is also described in numerical values.

[0127] Fig.40The histogram shown has a maximum value of density 8, so it does not meet condition 2. However, if the combination of segmented area Q5 with an average density of quantum dots 5 of 9 and segmented area Q15 with an average density of quantum dots 5 of 6 is considered among a plurality of combinations of any segmented area among segmented areas Q1 to Q20 and any other segmented areas, the first average density D1 = 9 and the second average density D2 = 6, which becomes 0.7 × D1 = 6.3, satisfying condition 1 of D2 = 0.7 × D1. Therefore, it can be considered that the light-emitting layer 4 of this embodiment has a first light-emitting layer 6 and a second light-emitting layer 8. The threshold value between the first area P1 and the second area P2 is (D1 + D2) / 2 = 7.5.

[0128] Fig.41 It is a schematic diagram showing still another average density of the quantum dots 5 in the light-emitting layer according to the comparative example. Fig.42 2 is a histogram showing another average density of the quantum dots 5 in the light-emitting layer according to the comparative example. Components identical to the above-described components are denoted by the same reference numerals, and detailed descriptions of these components will not be repeated.

[0129] exist Fig.41 In FIG. 1 , the average density of the quantum dots 5 in each of the divided regions Q1 to Q20 according to the comparative example is described in numerical values.

[0130] For example, if the combination of segmented area Q16 with an average density of quantum dots 5 of 9 and segmented area Q2 with an average density of quantum dots 5 of 7 is considered among a plurality of combinations of any segmented area among segmented areas Q1 to Q20 and any other segmented areas, the first average density D1 = 9 and the second average density D2 = 7, thus becoming 0.7×D1=6.3, which does not satisfy condition 1 of D2=0.7×D1. Furthermore, Fig.42 The histogram shown has one local maximum value of the density 8 and thus does not satisfy the condition 2. Therefore, the light-emitting layer of the comparative example cannot be regarded as having the first light-emitting layer 6 and the second light-emitting layer 8 .

[0131] The present invention is not limited to the above-mentioned embodiments, and various changes can be made within the scope of the claims. The embodiments obtained by appropriately combining the technical means disclosed in different embodiments are also included in the technical scope of the present invention. Moreover, new technical features can be formed by combining the technical methods disclosed in each embodiment. Description of Reference Numerals

[0132] 1 Light-emitting element 2First electrode 3. Second electrode 4 Luminous Layer 5 quantum dots 6First light-emitting layer 8 Second light-emitting layer 10Inorganic compounds (inorganic matrix) 12R red light emitting element 12G green light emitting element 12B blue light emitting element 18 Display devices P1 first area P2 Second Area Q1~Q20 division area

Claims

1. A light emitting element, characterized in that: include: a first electrode, a second electrode, and a light-emitting layer having a plurality of quantum dots between the first electrode and the second electrode, The light-emitting layer has a first region where the first light-emitting layer is provided and a second region where the second light-emitting layer is provided, when viewed from the direction from the first electrode to the second electrode, that is, in the stacking direction. The density of the quantum dots in the second light-emitting layer is lower than the density of the quantum dots in the first light-emitting layer, The second light-emitting layer is filled with an inorganic matrix between the plurality of quantum dots.

2. The light emitting element according to claim 1, characterized in that In any cross-section of the light-emitting layer along the stacking direction, when a range of 600nm in a direction orthogonal to the stacking direction is divided into 20 segmented regions with a width of 30nm, a first average density D1 of quantum dots in a first segmented region among the segmented regions and a second average density D2 of quantum dots in a second segmented region different from the first segmented region satisfy D2<0.7×D1.

3. The light emitting element according to claim 1 or 2, characterized in that: In any cross-section of the light-emitting layer along the stacking direction, when a range of 600 nm in a direction orthogonal to the stacking direction is divided into 20 segmented areas with a width of 30 nm, and the average density of quantum dots in each segmented area is divided from 0 to 10 levels, a histogram obtained by accumulating the number of segmented areas at each level has at least 2 maximum values.

4. The light emitting element according to any one of claims 1 to 3, characterized in that In any cross section of the light-emitting layer along the stacking direction, the first region is sandwiched by the second region.

5. The light emitting element according to any one of claims 1 to 4, characterized in that: When viewed in the stacking direction, the second region surrounds the first region.

6. The light emitting element according to any one of claims 1 to 5, characterized in that In any cross section of the light-emitting layer along the stacking direction, the area of ​​the second region is greater than or equal to 10% and less than or equal to 33% of the total area of ​​the first region and the second region.

7. The light emitting element according to any one of claims 1 to 6, characterized in that: In any cross section of the first light-emitting layer along the stacking direction, an area filling rate of the quantum dots in the first light-emitting layer is 63% or more and 91% or less.

8. The light emitting element according to any one of claims 1 to 7, characterized in that: In any cross section of the second light-emitting layer along the stacking direction, an area filling rate of the quantum dots in the second light-emitting layer is greater than or equal to 30% and less than or equal to 46%.

9. The light emitting element according to any one of claims 1 to 8, characterized in that: The inorganic matrix is ​​filled in the light-emitting layer.

10. The light emitting element according to any one of claims 1 to 8, characterized in that: The inorganic matrix has an area of ​​1000 nm in a plane direction intersecting the stacking direction. 2 Continuous film above.

11. A display device, characterized in that: The invention comprises a substrate and a red light emitting element, a green light emitting element and a blue light emitting element on the substrate, Each of the red light emitting element, the green light emitting element, and the blue light emitting element is the light emitting element according to any one of claims 1 to 10.

12. The display device according to claim 11, characterized in that For any two of the red light emitting elements, the green light emitting elements and the blue light emitting elements, when the light emitting element with a shorter light emitting wavelength is set as a short wavelength element and the light emitting element with a longer light emitting wavelength is set as a long wavelength element, In at least one combination of the short-wavelength element and the long-wavelength element of the display device, and in any cross-section of the short-wavelength element or the long-wavelength element along the stacking direction, the ratio of the area of ​​the second region to the total area of ​​the light-emitting layer of the short-wavelength element is smaller than the ratio of the area of ​​the second region to the total area of ​​the light-emitting layer of the long-wavelength element.

13. A display device, characterized in that: The invention comprises a substrate and a red light emitting element, a green light emitting element and a blue light emitting element on the substrate, Among the red light emitting element, the green light emitting element, and the blue light emitting element, only the blue light emitting element is the light emitting element according to any one of claims 1 to 10.

14. A method for manufacturing a light-emitting element, comprising a first electrode, a second electrode, and a light-emitting layer having a plurality of quantum dots between the first electrode and the second electrode, characterized in that: The method comprises a step of forming a light-emitting layer, wherein the light-emitting layer has a first region provided with a first light-emitting layer and a second region provided with a second light-emitting layer when viewed from the direction from the first electrode to the second electrode, that is, in the stacking direction. The density of the quantum dots in the second light-emitting layer is lower than the density of the quantum dots in the first light-emitting layer, The second light-emitting layer is filled with an inorganic matrix between the plurality of quantum dots.

15. The method for manufacturing a light emitting element according to claim 14, characterized in that: The light emitting layer forming step comprises: A first light-emitting layer forming step of forming the first light-emitting layer; and A second light-emitting layer forming step of forming the second light-emitting layer.

16. The method for manufacturing a light emitting element according to claim 15, characterized in that: The first light emitting layer forming step is performed after the second light emitting layer forming step.

17. The method for manufacturing a light emitting element according to claim 15, wherein: The second light emitting layer forming step comprises: a film forming step of forming a second light-emitting material layer, wherein the second light-emitting material layer contains a second light-emitting material in which a precursor of the inorganic matrix and the quantum dots are mixed; and A heating step is performed after the film forming step, wherein the second light-emitting material layer is heated to form the inorganic matrix from the precursor to obtain the second light-emitting layer.

18. A method for manufacturing a display device, characterized in that: include: A substrate preparation step, which prepares a substrate having a plurality of sub-pixel regions; as well as A light emitting element forming step of forming the light emitting element in each of the sub-pixel regions on the substrate by the light emitting element manufacturing method according to claim 14.

19. The method for manufacturing a display device according to claim 18, characterized in that: The light emitting layer forming step in the light emitting element forming step includes: a resist layer forming step of forming a first resist layer in each of the sub-pixel regions; A second light-emitting material layer film-forming step, which forms a second light-emitting material layer after the resist layer film-forming step, wherein the second light-emitting material layer contains a second light-emitting material in which a precursor of the inorganic matrix and the quantum dots are mixed; A second light emitting material layer patterning step, after the second light emitting material layer film forming step, removing the first resist layer and patterning the second light emitting material layer for each of the sub-pixel regions to form the second light emitting layer; a coating step of forming a second resist layer on the upper surface of the second light-emitting layer after the second light-emitting material layer patterning step; A first light-emitting layer forming step, after the film coating step, forming the first light-emitting layer for each of the sub-pixel regions; The cover film removal step is to remove the second resist layer after the first light emitting layer forming step.