Method for reducing welding deformation of iron tower truss

By adjusting the welding parameters and sequence, argon-rich gas protection welding is adopted, combined with positioning welding and round-trip linear transfer method, the problem of large deformation of tower truss is solved, and the maximum deformation of welding is controlled below 1.4mm.

CN119057182AInactive Publication Date: 2024-12-03HENAN DINGLI POLES & TOWERS COMPANY
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411347352.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-26
Publication Date
2024-12-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the prior art, the welding deformation of tower truss is relatively large and difficult to control below 2mm. Especially when carbon dioxide gas protective welding is used, there is a large welding deformation problem.

Method used

By adjusting the welding parameters and welding sequence, argon-rich gas 80%Ar+20%CO2 protective welding is used. The welding parameters are gas flow rate 15-20ml/min, current 100-120A, voltage 17-19V, welding speed 500-700mm/min , and ER50-6 welding wire is used, the diameter of the welding wire is 1.0mm, and the welding sequence is from the internal weld to the external weld. Combined with positioning welding and round-trip linear transportation and adjustment, the angle between the welding gun and the welding direction is 70°-90°.

Benefits of technology

The maximum deformation amount after welding of tower truss is effectively reduced, and controlled below 1.4mm, significantly reducing the welding deformation amount.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119057182A_ABST
    Figure CN119057182A_ABST
Patent Text Reader

Abstract

The invention provides a method for reducing welding deformation of an iron tower truss, which comprises the following steps of: placing the truss on a welding platform frame, and fixing a clamp between every two nodes on two sides of the truss, so that a gap between the contact surfaces of the truss and the welding platform frame is less than 1mm; argon-rich gas 80% Ar and 20% CO2 shielded welding is adopted, and the welding parameters are as follows: the gas flow is 15-20 ml / min, the welding current is 100-120 A, the welding voltage is 17-19 V, and the welding speed is 500-700 mm / min; one end of the truss is a starting point end, the other end of the truss is a tail end, node jumping welding is conducted from the starting point end to the tail end, then the starting point end is returned, and the remaining nodes of the section are welded from the starting point end to the tail end. By adjusting the welding parameters and the welding sequence, the maximum deformation of the iron tower truss after welding is 1.4 mm.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of welding, in particular to a method for reducing welding deformation of an iron tower truss. Background Art

[0002] The pipe used for the tower truss is 80mm in diameter, 4mm in wall thickness, and 7650mm in length. The thin wall and long pipe are prone to welding deformation, which requires the deformation to be controlled within 3mm. In the prior art, argon arc welding is used for welding, and the maximum deformation is about 2.4mm. If carbon dioxide gas shielded welding is used for welding, the gas flow rate is 18-25ml / min, ER50-6 welding wire is used, the wire diameter is 1.2mm, the current is controlled at 210-250A, the voltage is controlled at 23-25V, and the welding speed is controlled at 350-410mm / min, there is a problem of large welding deformation, and how to further reduce the deformation and control the maximum deformation below 2mm is also a problem that needs to be solved. Summary of the invention

[0003] The present invention provides a method for reducing the welding deformation of an iron tower truss. By adjusting welding parameters and welding sequence, the maximum deformation of the iron tower truss after welding is 1.4 mm.

[0004] The technical solution of the present invention is achieved as follows: A method for reducing the welding deformation of a tower truss comprises the following steps:

[0005] (1) Place the truss on the welding platform frame, and fix the clamps between every two nodes on both sides of the truss so that the gap between the truss and the welding platform frame is less than 1mm;

[0006] (2) Using argon-rich gas 80% Ar + 20% CO2 shielded welding, the welding parameters are: gas flow 15-20ml / min, welding current 100-120A, welding voltage 17-19V, welding speed 500-700mm / min;

[0007] (3) One end of the truss is the starting end, and the other end is the end. The nodes are welded from the starting end to the end, and then return to the starting end and weld the remaining nodes of the section from the starting end to the end.

[0008] Furthermore, in step (3), the internal welds and the intersection center of the truss are welded first, and then the external welds of the truss are welded.

[0009] Furthermore, in step (3), the quality of the tack weld is checked before welding. The tack weld position is the heel and toe of the intersection center; the tack weld length is 15-20 mm, and the thickness is the same as the formal weld.

[0010] Furthermore, in step (3), a reciprocating linear adjustment method is used for welding; when the arc is started, the backward welding is smoothly fused with the positioning weld, and the arc is well fused with the positioning weld at the end; the welding is carried out from top to bottom, and the elongation of the welding wire is not more than 10-15mm; the angle between the welding gun and the welding direction is 70°-90° when welding.

[0011] Furthermore, in step (3), the gap between the weld groups is 0-1 mm, the weld foot hf = 4-5 mm, and is not greater than 1.2 times the plate thickness.

[0012] Furthermore, in step (2), ER50-6 welding wire is used, and the diameter of the welding wire is 1.0 mm.

[0013] Furthermore, in step (3), before welding, ventilation is performed for 1-2 seconds in advance; after welding is stopped, the ventilation is delayed for 2-3 seconds.

[0014] Beneficial effects of the present invention:

[0015] By adjusting the welding parameters and the welding sequence, the maximum deformation of the tower truss after welding is 1.4 mm, and the maximum welding deformation is controlled below 2 mm. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0017] Figure 1 It is a structural diagram of the intersecting center;

[0018] Figure 2 Schematic diagram of the end structure of the truss. DETAILED DESCRIPTION

[0019] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0020] Example 1

[0021] A method for reducing welding deformation of a tower truss comprises the following steps:

[0022] (1) Place the truss (tower main frame) on the welding platform frame, and fix the F-type clamp between every two nodes on both sides of the truss to ensure that the gap between the truss and the welding platform frame is less than 1mm;

[0023] Check whether the integral fixing plates at both ends of the tower body and the middle fixing plates are installed in place, and whether the contact surface gap is qualified (the contact surface gap is less than 1mm);

[0024] Evenly spray the anti-splash liquid on the nodes on both sides of the truss, and be careful not to spray too much;

[0025] (2) Carbon dioxide shielded welding is adopted, and the welding parameters are as follows: a mixed gas of 80% Ar + 20% CO2 is adopted, and the gas flow rate is 15-20 ml / min; an ER50-6 welding wire is adopted, the wire diameter is 1.0 mm, the welding current is 100-120 A, the welding voltage is 17-19 V, and the welding speed is 500-700 mm / min; before welding, the gas is ventilated 1-2 seconds in advance; after stopping welding, the gas is stopped for 2-3 seconds;

[0026] (3) Reduce the pollution of the welding part. Before welding, use a wire wheel to completely remove the slag and debris that have not been removed. Do not start the arc on the workpiece surface outside the welding position. When adjusting the welding current, find another arc starting plate.

[0027] Welding sequence of welds:

[0028] 1) Check the quality of positioning welding before welding. The quality requirements of positioning welding are: the welding quality is equivalent to the formal weld; the positioning welding position is the heel and toe of the intersection center, such as Figure 1 As shown; the positioning weld length is 15-20mm, and the thickness is the same as the formal weld;

[0029] 2) The truss is taken as a whole, with one end of the truss as the starting end and the other end as the end. Two people form a group, one person for one side, and weld nodes from the starting end to the end (that is, weld at intervals), then return to the starting end and weld the remaining nodes of the section from the starting end to the end;

[0030] 3) After the internal welding and intersection center of the truss are completed, the external welds are welded. The welding sequence of the external welds is the same as that of the internal ones.

[0031] Welding requirements: Before welding, cut off the small ball at the end of the welding wire to avoid defects at the moment of arc starting; when welding, hold the gun with both hands, one hand as a fixed bracket, and the other hand to hold the welding gun for operation; start the arc decisively, and adjust it quickly, basically adopting a reciprocating linear adjustment method for welding; when starting the arc, the weld will be smoothly fused with the positioning weld at the back, and the arc will be well fused with the positioning weld at the end; weld from top to bottom to ensure fusion; the elongation of the welding wire is generally not more than 10-15mm; the angle between the welding gun and the welding direction is 70°-90° when welding, and it should not be tilted too much to avoid incomplete gas coverage and cause pores.

[0032] Welding quality requirements: Ensure that the weld gap is 0-1mm; weld foot hf = 4-5mm, try to ensure that it is not greater than 1.2 times the plate thickness; the quality of positioning welds is the same as that of formal welds; the welds are free of welding defects such as slag inclusions, undercuts, pores, lack of fusion, cracks, incomplete welding, arc scratches, and poor joints.

[0033] Welding repair: If there are welding defects such as slag inclusion, undercut, porosity, lack of fusion, cracks, etc. in the weld, it is necessary to use a grinder to mechanically remove the defects and then re-weld; if the weld defect position cannot be removed by a grinder, use a conical grinder to clean it; after the repair welding is completed, ensure a smooth transition of the joint.

[0034] like Figure 2 As shown, the welded truss main pipes are numbered and then tested for straightness and verticality. The test results are as follows:

[0035]

[0036] Using the welding method of this embodiment, three trusses were welded, and the maximum deformation was 1.4 mm.

[0037] Comparative Example 1

[0038] This embodiment is basically the same as embodiment 1, except that in step 2), the truss is taken as a whole, one end of the truss is the starting end, and the other end is the end end, two people are selected as a group, one person welds from the middle point of the truss to the end end, and the other person welds from the starting end to the middle point of the truss.

[0039] like Figure 2 As shown, the welded truss main pipes are numbered and then tested for straightness and verticality. The test results are as follows:

[0040] Straightness: The maximum deformation of the welding straightness of truss main pipes 2, 3 and 4 is 2.5-2.75mm, and the maximum deformation of truss main pipe 1 is 3mm.

[0041] Verticality: The maximum deformation of truss main pipe 2, truss main pipe 3 and truss main pipe 4 during welding is 1-1.75mm, and the maximum deformation of truss main pipe 1 is 2mm.

[0042] Moreover, with this welding method, the middle part of the truss is greatly deformed, with the maximum deformation reaching 3mm.

[0043] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for reducing welding deformation of a tower truss, characterized in that: The following steps are involved: (1) Place the truss on the welding platform frame, and fix the clamps between every two nodes on both sides of the truss so that the gap between the truss and the welding platform frame is less than 1mm; (2) Using argon-rich gas 80% Ar + 20% CO2 shielded welding, the welding parameters are: gas flow 15-20ml / min, welding current 100-120A, welding voltage 17-19V, welding speed 500-700mm / min; (3) One end of the truss is the starting end, and the other end is the end. The nodes are welded from the starting end to the end, and then return to the starting end and weld the remaining nodes of the section from the starting end to the end.

2. A method for reducing welding deformation of a tower truss according to claim 1, characterized in that: In step (3), the inner welds and the intersection center of the truss are welded first, and then the outer welds of the truss are welded.

3. A method for reducing welding deformation of a tower truss according to claim 1, characterized in that: In step (3), check the quality of the tack weld before welding. The location of the tack weld is the heel and toe of the intersection center; the length of the tack weld is 15-20mm, and the thickness is the same as the formal weld.

4. A method for reducing welding deformation of a tower truss according to claim 1, characterized in that: In step (3), welding is carried out by a reciprocating linear motion method; when the arc is started, the backward welding is smoothly fused with the positioning weld, and the arc is well fused with the positioning weld at the end; the welding is carried out from top to bottom, and the elongation of the welding wire is not greater than 10-15mm; when the welding gun is used for welding, the angle between the welding gun and the welding direction is 70°-90°.

5. A method for reducing welding deformation of a tower truss according to any one of claims 1 to 4, characterized in that: In step (3), the gap between the welds is 0-1 mm, the weld foot hf is 4-5 mm, and is not greater than 1.2 times the plate thickness.

6. A method for reducing welding deformation of a tower truss according to claim 1, characterized in that: In step (2), ER50-6 welding wire is used, and the diameter of the welding wire is 1.0 mm.

7. A method for reducing welding deformation of a tower truss according to claim 1, characterized in that: In step (3), before welding, ventilation is performed for 1-2 seconds in advance; after welding is stopped, the ventilation is delayed for 2-3 seconds.

Citation Information

Patent Citations

  • Welding method for high-strength steel truss-type cantilever crane

    CN102489888A

  • Surfacing method for antiseptic wear-resisting layer of dovetail groove

    CN103008833A

  • Flux copper gasket method submerged arc welding technology of Q420 high-strength steel thick plate

    CN110640279A

  • Welding method and construction method for large internal-floating-roof storage tank

    CN111715978A

  • Air separation unit tower equipment assembly welding method

    CN116689914A