Ceramic copper-clad carrier plate with stripping test structure and manufacturing method of ceramic copper-clad carrier plate
By setting a peel test area on the ceramic copper clad carrier plate and etching the isolation ring groove, the problem of poor sampling detection reliability in the prior art is solved, and batch peel strength detection of the ceramic copper clad carrier plate is realized, which improves the detection reliability and efficiency.
Patent Information
- Application Number
- CN202411233415.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-04
- Publication Date
- 2024-12-03
AI Technical Summary
The binding strength detection of existing ceramic copper clad carrier plates requires sampling for peeling tests, resulting in poor reliability and the inability to effectively inspect all products in a batch.
A peel test area is set on the ceramic copper clad carrier plate, the adhesive layer is scraped off and the isolation layer is covered, and the isolation ring groove is etched after sintering to form a peel test piece, allowing the peel strength of each product to be tested without destroying the ceramic substrate.
The peel strength test of all products in the same batch is realized, which improves the detection reliability, simplifies the testing process, and ensures that the peel strength of the entire carrier plate is qualified.
Smart Images

Figure CN119059834A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of ceramic copper-clad carrier boards, and in particular to a ceramic copper-clad carrier board with a peeling test structure and a manufacturing method thereof. Background Art
[0002] Ceramic copper-clad substrate is a composite material that combines metal copper foil with a ceramic substrate. It utilizes the high thermal conductivity, high mechanical strength and high insulation of ceramics, as well as the good conductivity and solderability of metal copper foil. It is widely used in power electronics, high-power electronic modules and other fields.
[0003] In the manufacturing process of ceramic copper-clad substrates, the sintering step is one of the key steps. Through the sintering step, the copper foil and the ceramic substrate can be tightly bonded at high temperature. In the sintering manufacturing process of ceramic copper-clad substrates, sintering is generally carried out in batches. In order to ensure the quality of the ceramic copper-clad substrates after sintering, the ceramic copper-clad substrates need to be subjected to a peel test to detect the bonding strength between the copper foil and the ceramic substrate. At present, it is usually necessary to conduct a peel test inspection on a batch of ceramic copper-clad substrates, and the peel test process requires the destruction of the entire ceramic copper-clad substrate. The existing whole-sheet destructive peel test method cannot test all ceramic copper-clad substrates in a batch, and can only rely on the sampling results of the same batch to infer the bonding strength of other untested ceramic copper-clad substrates. The reliability is not good. Based on the above background, the inventor has designed a ceramic copper-clad carrier with a peeling test structure and a manufacturing method thereof to solve the above problems, and thus proposed the present application. Summary of the invention
[0004] The purpose of the present application is to provide a ceramic copper-clad carrier with a peeling test structure and a manufacturing method thereof, so as to solve the problem that the bonding strength of the ceramic copper-clad carrier in the prior art needs to be estimated based on the peeling test results of the sampled ceramic copper-clad carrier, which is unreliable.
[0005] In order to solve the above technical problems, the present invention adopts the following solutions: On the one hand, the present application provides a method for manufacturing a ceramic copper-clad carrier with a peeling test structure, comprising manufacturing a ceramic substrate and a copper plate body of a copper-clad carrier body, wherein a peeling test area is provided on the copper-clad carrier body, and the peeling test area includes a first area and a second area that are adjacently arranged; The manufacturing method comprises the following steps: S1, scraping off the adhesive layer located in the first area on the ceramic substrate or the copper plate body; S2, setting an isolation layer at the position where the adhesive layer is scraped off in the first area; S3, sintering to obtain a copper-clad substrate body; S4. Etch an isolation ring groove located within the peel test area and spanning the first area and the second area, to form a peel test piece disposed within the isolation ring groove and spanning the first area and the second area.
[0006] Optionally, the material of the adhesive layer is solder paste or cuprous oxide; Before the step S1, there is also a step S0 of obtaining a ceramic substrate with solder paste coated on its surface or a copper plate body with a cuprous oxide layer on its surface.
[0007] Optionally, the isolation layer is a silicon oxide plate fixed within the first area or magnesium oxide powder laid in a powder form within the first area.
[0008] Optionally, the isolation ring groove includes a first isolation segment and a second isolation segment respectively located within the first area and the second area and buckled together to form a ring; The first isolation segment and the second isolation segment are in a C shape or / and a U shape; The peel test piece includes a clamping segment and a test segment respectively located within the first isolation segment and the second isolation segment.
[0009] Optionally, the area of the first isolation segment is greater than or equal to the area of the second isolation segment; The width distance between the clamping segment and the side wall of the first isolation segment is greater than the width distance between the test segment and the side wall of the second isolation segment.
[0010] Optionally, both the first isolation segment and the second isolation segment are in a U shape; The shape of the peel test piece is in a long strip shape.
[0011] Optionally, the length of the clamping segment is less than or equal to the length of the test segment.
[0012] Optionally, the peel test area is located in the corner area of the copper-clad carrier board body.
[0013] On the other hand, the present application provides a ceramic copper-clad carrier board with a peel test structure, which is manufactured by the manufacturing method of a ceramic copper-clad carrier board with a peel test structure as described in any one of the above.
[0014] Optionally, the peel test area is located in the corner area of the copper-clad carrier board body; It further includes a product area located in the middle area of the copper-clad carrier board body, and a gap area located between the product area and the peel test area and used for cutting.
[0015] The beneficial effects of the present invention relative to the prior art are as follows: The present application provides a peeling test area on the copper-clad carrier body, and performs the steps of scraping off the adhesive layer in the first area of the peeling test area, covering the isolation layer, etc., so that after the copper-clad carrier body is sintered to form the copper-clad carrier body, the first area of the peeling test area of the copper-clad carrier body forms a non-adhesive area. On this basis, an isolation ring groove spanning the first area and the second area is etched in the peeling test area, so that the peeling test area can form a peeling test piece located in the isolation ring groove and spanning the arrangement. In the copper-clad carrier body manufactured by the above method, the portion of the peeling test piece located in the first area is in a non-adhesive free state. Therefore, when testing the peeling strength, it is only necessary to clamp the portion of the peeling test piece located in the first area and test the adhesive strength between the peeling test piece and the second area to complete the peeling strength test.
[0016] Compared with the prior art, the copper-clad carrier body manufactured by the manufacturing method of the present application has the advantages of not needing to destroy the ceramic substrate, and being able to set a peeling test area on all products of the same batch to test the peeling strength of each copper-clad carrier body. There is no need to rely on sample sampling to infer the peeling strength of products of the same batch, and the reliability is good. In addition, when testing the peeling strength, it is sufficient to clamp the peeling test piece in the first area, and the testing process is also extremely simple.
[0017] In addition, the peel test area is set at the corner area of the copper-clad carrier body. On the one hand, it can be directly cut off when the small pieces are subsequently divided to avoid affecting the product area in the middle area of the copper-clad carrier body. On the other hand, the corner area of the copper-clad carrier body is generally a weak area of bonding strength. The qualified peel test results at the corner area can ensure that the peel strength of each position of the entire copper-clad carrier body is qualified. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 This is a schematic diagram of the process of Example 1 of the present application.
[0019] Figure 2 This is a schematic diagram of the structure of Example 2 of the present application.
[0020] Figure 3 for Figure 2 Schematic diagram of the cross-sectional structure of AA.
[0021] Figure 4 for Figure 3 A local enlarged schematic diagram of point B in the middle.
[0022] Figure 5 This is a structural diagram of Example 3 of the present application.
[0023] Description of reference numerals: 1-copper plate body, 11-product area, 12-peeling test area, 121-first area, 122-second area, 13-isolation ring groove, 131-first isolation section, 132-second isolation section, 14-gap area, 2-peeling test piece, 21-clamping section, 22-test section, 3-isolation layer, 4-ceramic substrate, 5-adhesive layer. DETAILED DESCRIPTION
[0024] The present invention will be further described in detail below in conjunction with embodiments and drawings, but the embodiments of the present invention are not limited thereto.
[0025] In the description of the present invention, it should be noted that the terms "center", "up", "down", "left", "right", "vertical", "longitudinal", "lateral", "horizontal", "inside", "outside", "front", "back", "top", "bottom" and the like indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings, or are the directions or positional relationships in which the inventive product is usually placed when used. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present invention.
[0026] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "disposed", "opened", "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0027] The present invention will be described in detail below with reference to the accompanying drawings and in combination with embodiments.
[0028] Embodiment 1: like Figure 1 As shown, a method for manufacturing a ceramic copper-clad carrier with a peeling test structure provided in this embodiment includes manufacturing a ceramic substrate 4 and a copper plate body 1 of a copper-clad carrier body, wherein a peeling test area 12 is provided on the copper-clad carrier body, and the peeling test area 12 includes a first area 121 and a second area 122 that are arranged adjacent to each other; The manufacturing method comprises the following steps: S1, scraping off the adhesive layer 5 located in the first area 121 on the ceramic substrate 4 or the copper plate body 1; S2, setting the isolation layer 3 at the position where the adhesive layer 5 is scraped off in the first area 121; S3, sintering to obtain a copper-clad substrate body; S4 , etching out the isolation ring groove 13 located in the peeling test area 12 and spanning the first area 121 and the second area 122 , to form the peeling test piece 2 located in the isolation ring groove 13 and spanning the first area 121 and the second area 122 .
[0029] Optionally, the material of the adhesive layer 5 is solder paste or cuprous oxide; Before step S1, there is step S0 of obtaining a ceramic substrate 4 with solder paste adhered on the surface or a copper plate body 1 with a cuprous oxide layer on the surface.
[0030] In this embodiment, by setting a peeling test area 12 on the copper-clad carrier body, and by scraping off the adhesive layer 5 in the first area 121 of the peeling test area 12, covering the isolation layer 3 and other steps, after sintering to form the copper-clad carrier body, the first area 121 of the peeling test area 12 of the copper-clad carrier body can be formed into a non-adhesive area. On this basis, an isolation ring groove 13 spanning the first area 121 and the second area 122 is etched in the peeling test area 12, so that the peeling test area 12 can form a peeling test piece 2 located in the isolation ring groove 13 and spanning the arrangement; in the copper-clad carrier body manufactured by the above method, the portion of the peeling test piece 2 located in the first area 121 is in a non-adhesive free state, so when testing the peeling strength, it is only necessary to clamp the portion of the peeling test piece 2 located in the first area 121 to test the adhesive strength between the peeling test piece 2 and the second area 122, so as to complete the peeling strength test.
[0031] Compared with the prior art, the copper-clad carrier body manufactured by the manufacturing method of the present application has the advantages of not needing to destroy the ceramic substrate 4, and being able to set a peeling test area 12 on all products of the same batch to test the peeling strength of each copper-clad carrier body. There is no need to rely on sample sampling to infer the peeling strength of products of the same batch, and the reliability is good. In addition, when testing the peeling strength, it is sufficient to clamp the peeling test piece 2 in the first area 121, and the testing process is also extremely simple.
[0032] Specifically, in this embodiment, the isolation layer 3 is a silicon oxide plate fixed in the first area 121 or magnesium oxide powder laid in the first area 121 in powder form. By setting the magnesium oxide powder or silicon oxide plate, the copper plate body 1 and the ceramic substrate 4 at the position of the first area 121 can be prevented from combining in the subsequent sintering process, so that the first area 121 of the copper-clad carrier body peeling test area 12 becomes a non-bonding area, so that after etching the isolation ring groove 13, the part of the peeling test piece 2 located in the first area 121 is in a non-bonding free state, which is convenient for the tester to clamp the peeling test piece 2 for peeling test. The technician can also use other materials that can prevent the copper plate body 1 and the ceramic substrate 4 from combining as the isolation layer 3, and no further examples are given here.
[0033] Specifically, in this embodiment, the isolation ring groove 13 includes a first isolation section 131 and a second isolation section 132 that are respectively located in the first region 121 and the second region 122 and are buckled together to form a ring shape. The first isolation section 131 and the second isolation section 132 are in a C shape or / and a U shape. The peeling test piece 2 includes a clamping section 21 and a test section 22 that are respectively located in the first isolation section 131 and the second isolation section 132. By setting the isolation ring groove 13, the peeling test piece 2 is completely isolated from other positions of the copper plate body 1, which can avoid the influence of the peeling test on other positions of the copper plate body 1.
[0034] The first isolation section 131 can separate the clamping section 21 from the copper plate body 1, and the second isolation section 132 can separate the test section 22 from the copper plate body 1. Moreover, the first isolation section 131 and the second isolation section 132 are buckled together to form a ring shape, so that the influence on the copper plate body 1 during the peeling process can be avoided, and the peeling test piece 2 can be directly peeled off during the peeling test without affecting the copper plate body 1.
[0035] Specifically, in this embodiment, the area of the region of the first isolation section 131 is greater than or equal to the area of the region of the second isolation section 132. The width distance between the clamping section 21 and the side wall of the first isolation section 131 is greater than the width distance between the test section 22 and the side wall of the second isolation section 132, which is convenient for the tester to firmly clamp the clamping section 21 of the peeling test piece 2. At the same time, it can avoid the entire peeling test area 12 occupying too large an area, reduce the area ratio of the peeling test area 12, and reduce the cost of the peeling test.
[0036] Specifically, in this embodiment, both the first isolation section 131 and the second isolation section 132 are in a U shape. The shape of the peeling test piece 2 is in a long strip shape. Technicians can also, according to needs, set the first isolation section 131 and the second isolation section 132 to be in a C shape and a U shape respectively, or set both the first isolation section 131 and the second isolation section 132 to be in a C shape. Technicians can also set the first isolation section 131 and the second isolation section 132 to other shapes, which will not be elaborated with examples here.
[0037] Specifically, in this embodiment, the length of the clamping section 21 is less than or equal to the length of the test section 22, which can ensure that the test section 22 has sufficient length to ensure the stability and reliability of the peeling test results. Technicians can also, according to the actual lengths of the test section 22 and the clamping section 21, set the length of the test section 22 to be shorter than the length of the clamping section 21. In this embodiment, the specific lengths of the clamping section 21 and the test section 22 and the specific ratio between them can be set by technicians according to the size data of the copper-clad carrier board body.
[0038] Specifically, in this embodiment, the peel test area 12 is located in the corner area of the copper-clad carrier body. The peel test area 12 of this embodiment is set in the corner area of the copper-clad carrier body. On the one hand, it can be directly cut off when the small pieces are subsequently divided to avoid affecting the product area 11 in the middle area of the copper-clad carrier body. On the other hand, the corner area of the copper-clad carrier body is generally a weak area of bonding strength. The qualified peel test results in the corner area can ensure that the peel strength of each position of the entire copper-clad carrier body is qualified.
[0039] Example 2 like Figures 2 to 4 As shown, a ceramic copper-clad carrier board with a peeling test structure of this embodiment is manufactured by the manufacturing method of a ceramic copper-clad carrier board with a peeling test structure of the above-mentioned embodiment 1.
[0040] Specifically, in this embodiment, the peeling test area 12 is located at the corner area of the copper-clad carrier body; The invention also includes a product area 11 located in the middle area of the copper-clad carrier body, and a gap area 14 located between the product area 11 and the peeling test area 12 and used for cutting. Figure 2 As shown, the peeling test area 12 is located in the corner area of the copper-clad carrier body, and a gap area 14 is also provided between the peeling test area 12 and the product area 11. On the one hand, when the copper-clad carrier body is subsequently divided into small pieces, part of the peeling test area 12 can be directly cut off without affecting the product area 11 of the copper-clad carrier body. In addition, the corner area of the copper-clad carrier body is generally a weak area of bonding strength. The qualified peeling test result at the corner area can ensure that the peeling strength of each position of the entire copper-clad carrier body is qualified. In this embodiment, four peeling test areas 12 are provided at the four corner areas of the copper-clad carrier body, and the four peeling test areas 12 are provided with isolation ring grooves 13 and peeling test sheets 2 with the same structure.
[0041] In this embodiment, Figures 2 to 4 As shown, the entire peeling test piece 2 is located in the isolation ring groove 13, so that the peeling test piece 2 is completely isolated from other positions of the copper plate body 1, avoiding that the test section 22 of the peeling test piece 2 is peeled off from the adhesive layer 5 between the ceramic substrate 4 and the peeling test piece 2, and affecting other positions of the copper plate body 1.
[0042] In this embodiment, Figure 4 As shown, since the peeling test piece 2 includes a clamping section 21 located in the first area 121 and a test section 22 located in the second area 122, and an isolation layer 3 is provided between the first area 121 and the clamping section 21, the end of the clamping section 21 away from the test section 22 is in a free state, which is convenient for the tester to clamp.
[0043] In this embodiment, the isolation ring groove 13 includes a first isolation section 131 and a second isolation section 132 that are respectively located in the first region 121 and the second region 122 and are connected end to end to form a ring; The first isolation section 131 and the second isolation section 132 are in a C shape or / and a U shape; The area of the region of the first isolation section 131 is greater than or equal to the area of the region of the second isolation section 132; The width distance between the clamping section 21 and the side wall of the first isolation section 131 is greater than the width distance between the test section 22 and the side wall of the second isolation section 132, which is convenient for the tester to firmly hold the clamping section 21 of the peeling test piece 2. At the same time, it can avoid the entire peeling test area 12 occupying too large an area, reduce the area ratio of the peeling test area 12, and reduce the cost of the peeling test.
[0044] Embodiment 3 As Figure 5 shown, a ceramic copper-clad carrier board with a peeling test structure in this embodiment is manufactured by the manufacturing method of a ceramic copper-clad carrier board with a peeling test structure in Embodiment 1 above. There is one peeling test area 12 on the copper-clad carrier board, and an isolation ring groove 13 and a peeling test piece 2 with the same structure as that in Embodiment 2 are arranged in the peeling test area 12.
[0045] In this embodiment, a gap area 14 is provided between the peeling test area 12 and the product area 11, which is convenient for dividing small products in subsequent tests.
[0046] This embodiment is also manufactured by the manufacturing method described in Embodiment 1, and the rest of the structure of this embodiment is the same as that of Embodiment 2, and will not be described in detail here.
[0047] It can be understood that the above embodiments are merely exemplary embodiments adopted to illustrate the principle of the present invention. However, the present invention is not limited thereto. For those of ordinary skill in the art, various deformations and improvements can be made without departing from the spirit and essence of the present invention, and these deformations and improvements are also regarded as the protection scope of the present invention.
Claims
1. A method for manufacturing a ceramic copper-clad carrier board with a peeling test structure, comprising manufacturing a ceramic substrate (4) and a copper plate body (1) of the copper-clad carrier board body, characterized in that: On the copper-clad carrier board body, there is a peel test area (12), and the peel test area (12) includes a first area (121) and a second area (122) arranged adjacent to each other; The manufacturing method includes the following steps: S1. Scrape off the adhesive layer (5) on the ceramic substrate (4) or the copper plate body (1) within the first area (121); S2. Set an isolation layer (3) at the position where the adhesive layer (5) has been scraped off within the first area (121); S3. Sinter to obtain the copper-clad carrier board body; S4. Etch an isolation ring groove (13) within the peel test area (12) and spanning the first area (121) and the second area (122), and form a peel test piece (2) located within the isolation ring groove (13) and spanning the first area (121) and the second area (122) for setting; 2. The method for manufacturing a ceramic copper-clad carrier with a peeling test structure according to claim 1, characterized in that: The material of the adhesive layer (5) is solder paste or cuprous oxide; Before the step S1, there is also a step S0 of obtaining a ceramic substrate (4) with solder paste adhered to its surface or a copper plate body (1) with a cuprous oxide layer on its surface.
3. The method for manufacturing a ceramic copper-clad carrier with a peeling test structure according to claim 1, characterized in that: The isolation layer (3) is a silica plate fixed within the first area (121) or magnesium oxide powder laid in a powder form within the first area (121).
4. The method for manufacturing a ceramic copper-clad substrate with a peeling test structure according to claim 1, characterized in that: The isolation ring groove (13) includes a first isolation section (131) and a second isolation section (132) respectively located within the first area (121) and the second area (122) and buckled to form a ring; The first isolation section (131) and the second isolation section (132) are in a C shape or / and a U shape; The peel test piece (2) includes a clamping section (21) and a test section (22) respectively located within the first isolation section (131) and the second isolation section (132).
5. The method for manufacturing a ceramic copper-clad carrier with a peeling test structure according to claim 4, characterized in that: The area of the first isolation section (131) is greater than or equal to the area of the second isolation section (132); The width distance between the clamping section (21) and the side wall of the first isolation section (131) is greater than the width distance between the test section (22) and the side wall of the second isolation section (132).
6. The method for manufacturing a ceramic copper-clad carrier with a peeling test structure according to claim 4, characterized in that: Both the first isolation section (131) and the second isolation section (132) are in a U shape; The shape of the peel test piece (2) is strip-shaped.
7. The method for manufacturing a ceramic copper-clad carrier with a peeling test structure according to claim 4, characterized in that: The length of the clamping section (21) is less than or equal to the length of the test section (22).
8. The method for manufacturing a ceramic copper-clad carrier with a peeling test structure according to claim 1, characterized in that: The peel test area (12) is located in the corner area of the copper-clad carrier board body.
9. A ceramic copper-clad carrier with a peeling test structure, characterized in that: Manufactured by the manufacturing method of a ceramic copper-clad carrier board with a peel test structure according to any one of claims 1-8.
10. The ceramic copper-clad carrier with a peeling test structure according to claim 9, characterized in that: The peel test area (12) is located in the corner area of the copper-clad carrier board body; It further includes a product area (11) located in the middle area of the copper-clad carrier board body, and a gap area (14) located between the product area (11) and the peel test area (12) and used for cutting.
Citation Information
Patent Citations
Buried high-brightness light emitting diode structure
CN102208506A
Preparation method of peel strength test sample and peel strength test sample
CN114295434A
Peel strength PCB test board and preparation method and application thereof
CN115290557A
Peeling test method for copper-clad ceramic substrate