Dianion oil-soluble ionic liquid as well as preparation method and application thereof
By clicking chemical reactions to increase the carbon chain length of the ionic liquid, the preparation of double anionic oil-soluble ionic liquids solves the problems of low solubility and insufficient lubricity of traditional ionic liquids, and significantly improves the corrosion and tribological properties of lubricating oils. It is suitable for complex processes condition.
Patent Information
- Application Number
- CN202411250253.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-06
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Traditional ionic liquids have low solubility in non-polar hydrocarbon oil, which limits its application as a lubricant additive, and its lubricating performance is insufficient to meet the needs of modern complex working conditions.
By clicking on chemical reactions to increase the carbon chain length of the ionic liquid, prepare a bianionic oil-soluble ionic liquid, reduce its polarity and improve oil solubility, and use bianionic ionic liquid [HDHE][DEHP] as a lubricating oil additive to enhance its corrosion resistance and tribological properties.
It significantly improves the corrosion resistance, tribological properties and extreme pressure resistance of lubricating oil, reduces the friction coefficient and wear volume, improves the flatness of the lubricated surface, and is suitable for modern complex working conditions.
Smart Images

Figure FT_1 
Figure FT_2 
Figure FT_3
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of tribology and relates to an ionic liquid, in particular to a di-anionic oil-soluble ionic liquid and a preparation method thereof. The ionic liquid is mainly used as a lubricating oil additive. Background Art
[0002] Friction and wear are key factors that lead to energy loss and mechanical failure during the operation of mechanical parts. Among the many available solutions, lubrication has proven to be one of the most effective ways. However, traditional lubricants are no longer suitable for the requirements of the modern environment in terms of lubricity and durability. In order to overcome these limitations, a large number of performance additives such as friction reducers and anti-wear agents, preservatives, etc. have been developed to improve the performance of base oils and extend the service life of equipment. At present, the complex working conditions have posed a huge challenge to the performance of traditional additives. Therefore, it is very necessary to synthesize new lubricant additives suitable for various working conditions, which has broad application prospects.
[0003] Ionic liquids have attracted a lot of attention in many fields such as lubrication and catalysis due to their unique properties such as low volatility, non-flammability and wide liquid range. Ionic liquids have been proven to be very promising lubricants and lubricant additives in the field of tribology. Adding extremely low concentrations of ionic liquids to base oil can achieve the effective lubricity of pure ionic liquids. However, due to the high polarity of ionic liquids themselves, their solubility in non-polar hydrocarbon oils is extremely low, which greatly limits their application. In view of this, this study started with molecular structure design and prepared a double anionic ionic liquid that is highly soluble in n-hexadecane base oil by increasing the carbon chain length of the ionic liquid through click chemistry reactions. This ionic liquid can significantly improve the load-bearing capacity, corrosion resistance and tribological properties of the base oil. This ionic liquid does not contain halogens such as sulfur and has good corrosion resistance, and is expected to be widely used in the fields of mechanical engineering and tribology. Summary of the invention
[0004] The present invention aims to provide a method for preparing a di-anionic oil-soluble ionic liquid to solve the problems of poor oil solubility and insufficient lubricity of traditional ionic liquids.
[0005] 1. Preparation of dianionic oil-soluble ionic liquids The preparation method of the di-anionic oil-soluble ionic liquid comprises the following steps: 1) Preparation of [DETA][DEHP] ionic liquids First, diethylenetriamine is placed in a round-bottom flask, and then diisooctyl phosphate is added dropwise into the round-bottom flask, and the mixture is stirred and reacted at room temperature for 12 to 24 hours, and then vacuum dried to obtain diethylenetriammonium diisooctyl phosphate ionic liquid, which is denoted as [DETA][DEHP]; the molar ratio of diethylenetriamine to diisooctyl phosphate is 1:1 to 1.005.
[0006] 2) Preparation of [TEEA][DEHP] ionic liquid [DETA][DEHP] ionic liquid was added into a round-bottom flask and an appropriate amount of methanol was added, and then 1,2-epoxytetradecane was slowly added thereto, and the reaction was fully stirred at room temperature for 6 to 12 hours. After the solvent was evaporated off, the mixture was vacuum dried for 12 hours to obtain dihydroxypentadecylaminoethylammonium salt diisooctyl diphosphate ionic liquid, denoted as [TEEA][DEHP]; the molar ratio of diethylenetriammonium salt diisooctyl phosphate ionic liquid to 1,2-epoxytetradecane was 1:2 to 2.001.
[0007] 3) Preparation of [HDHE][DEHP] ionic liquid The obtained [TEEA][DEHP] ionic liquid was added to a round-bottom flask and an appropriate amount of methanol was added, and then 1,7-octadiene diepoxide was slowly added thereto, and the reaction was stirred for 6 to 12 hours at room temperature. After the solvent was evaporated, it was vacuum dried for 12 hours to obtain a dianionic oil-soluble ionic liquid, which was recorded as [HDHE][DEHP]; the molar ratio of dihydroxypentadecanylaminoethylammonium salt diisooctyl diphosphate ionic liquid to 1,7-octadiene diepoxide was 1:1 to 1.001.
[0008] The structural formula of the dianionic oil-soluble ionic liquid is as follows: Where R=C 12 H 25 It is n-dodecyl.
[0009] The invention first synthesizes a diethylenetriammonium salt diisooctyl phosphate ionic liquid, and then uses an "epoxy group" and an "amine group" to undergo a click chemical reaction to increase the carbon chain length of the diethylenetriammonium salt diisooctyl phosphate ionic liquid. The ionic liquid after the carbon chain length is increased undergoes a click chemical reaction with a "diepoxy" compound to prepare a dianionic oil-soluble ionic liquid with good oil solubility, high bearing capacity and excellent tribological performance.
[0010] 2. Structure of dianionic oil-soluble ionic liquids The present invention analyzes the nuclear magnetic hydrogen spectrum and infrared spectrum of the synthesized ionic liquid. The nuclear magnetic hydrogen spectrum and infrared spectrum of the dianionic oil-soluble ionic liquid and the intermediate product are as follows: Figure 1.
[0011] From the H-NMR spectrum, we can see that the characteristic peak of “epoxy” is at 850 cm -1 ~ 950cm -1 , the characteristic peak of the epoxy group disappears after the click chemistry reaction. The infrared spectrum shows that the "epoxy group" reacts with the "amine group", indicating that the double anion oil-soluble ionic liquid is finally successfully synthesized.
[0012] 3. Application of [HDHE][DEHP] ionic liquids in lubricating oils 1. Anti-corrosion performance test of [HDHE][DEHP] ionic liquid as an additive for n-hexadecane base oil The anti-corrosion experiment directly reflects the adsorption capacity of ionic liquids on the substrate surface. This experiment used the copper corrosion experiment to examine the anti-corrosion effect of pure hexadecane (16C) and four different concentrations of [HDHE][DEHP] ionic liquids in hexadecane (see Figure 2 ), the corrosion level of the base oil n-hexadecane is 1b, and the corrosion level of the oil samples containing different concentrations of ionic liquids is 1a. The results show that the addition of [HDHE][DEHP] ionic liquids can significantly improve the anti-corrosion effect.
[0013] 2. Tribological performance test of n-hexadecane as lubricant additive The tribological properties of the [HDHE][DEHP] ionic liquid of the present invention as a lubricant and a lubricating additive were investigated on an Optimol SRV-V fretting friction and wear tester, and a comparative test was conducted with n-hexadecane base oil. The friction test lasted for 30 min at a temperature of 25 °C, a load of 200 N, and a frequency of 25 Hz. The upper test ball was a GCr15 steel ball, and the lower test plate was a GCr15 steel plate. The friction test results are shown in Table 1. After the friction test, the microscopic morphology of the worn surface of the steel plate was detected by scanning electron microscopy. The results are shown in Table 1. Figure 3 .
[0014] from Figure 3 It can be seen that the plowing and adhesive wear phenomena are obvious on the surface lubricated by the base oil. The addition of additives can significantly improve this phenomenon, and the lubricated surface becomes smoother and flatter, indicating that the ionic liquid has excellent anti-wear properties.
[0015] As can be seen from Table 1, the friction coefficient after ionic liquid lubrication is significantly reduced compared to pure n-hexadecane base oil, and the wear volume of the wear surface is also significantly reduced. [HDHE][DEHP] ionic liquid additives significantly improve the tribological behavior of the base oil and have excellent wear reduction and anti-wear properties.
[0016] 3. [HDHE][DEHP] ionic liquid extreme pressure resistance test The extreme pressure performance of the [HDHE][DEHP] ionic liquid of the present invention was investigated on an MRS-1J four-ball friction and wear tester. The upper and lower test balls used in this experiment were made of AISI52100 steel with a diameter of 12.7 mm, a surface roughness of 0.025 μm, and a hardness of 60-63 HRC. The experimental results are shown in Table 2.
[0017] It can be seen from Table 2 that the di-anionic oil-soluble ionic liquid significantly improves the extreme pressure resistance of n-hexadecane base oil.
[0018] In summary, the present invention provides a double anionic oil-soluble ionic liquid with a novel structure, a simple preparation method, and no active elements such as halogens and sulfur. The carbon chain length of the ionic liquid is increased by a click chemistry reaction to reduce the polarity of the ionic liquid, thereby improving the oil solubility of the ionic liquid, improving the selectivity of the ionic liquid as a lubricating material and the tribological properties as an additive, and is expected to promote the wide application of the ionic liquid as a lubricating oil additive in the field of lubrication engineering. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 The present invention provides hydrogen nuclear magnetic spectrum and infrared spectrum of the dianionic oil-soluble ionic liquid and its intermediate synthetic product prepared by the present invention.
[0020] Figure 2 Comparison of the anti-corrosion experiments of n-hexadecane and di-anionic oil-soluble ionic liquids with different concentrations as n-hexadecane lubricant additives. (a) blank control sample, (b) n-hexadecane, (cf) n-hexadecane with 1wt%~4wt% [HDHE][DEHP] added.
[0021] Figure 3 Scanning electron microscopy of the worn surface after friction test of n-hexadecane and dianionic oil-soluble ionic liquid as n-hexadecane additive. DETAILED DESCRIPTION
[0022] The present invention is further explained below with reference to specific embodiments.
[0023] Example 1 (1) Preparation of [DETA][DEHP] ionic liquids Take 2.06 g of diethylenetriamine in a round-bottom flask, place the round-bottom flask in an oil bath and start stirring. Add 6.43 g of diisooctyl phosphate dropwise, and react at room temperature after the addition is complete. The reaction lasts for 12 to 24 hours to ensure that the reagents react completely. Use a vacuum drying oven to dry the volatile impurities in the product to obtain a light yellow liquid, which is recorded as [DETA][DEHP].
[0024] 1 H NMR (chloroform-d, 600 MHz) δ 0.82–0.97 (m, 12 H, CH3), 1.17–1.55 (m, 18 H, CH, CH2), 2.76–2.98 (m, 8 H, N–CH2–CH2–N + ), 3.60–3.80 (m, 4H, O–CH2–C), 4.81–5.29 (s, 2H, –N + H2). (2) Preparation of [TEEA][DEHP] ionic liquid Take 4.25g [DETA][DEHP] and dissolve it in methanol and add it dropwise to the round-bottom flask. Place the round-bottom flask in an oil bath and start stirring. Take 4.24g of 1,2-epoxytetradecane and add it dropwise. After the addition is complete, stir the reaction at 25°C for 6 to 12 hours to ensure that the reagents react completely. Use a rotary evaporator to remove the methanol, and then place it in a vacuum drying oven to dry for 10 to 12 hours. The resulting product is a light yellow liquid, recorded as [TEEA][DEHP].
[0025] 1 H NMR (chloroform-d, 600 MHz) δ 0.74–1.01 (m, 18 H, CH3), 1.12–1.64 (m, 62 H, CH, CH2), 2.19–2.64 (m, 4 H, C–CH2–N), 2.62–3.17 (m, 8 H, N–CH2–CH2–N + ), 3.60–3.80 (m, 6H, O–CH2–C, CH–O), 5.13–6.09 (s, 2H, –N + H2). (3) Preparation of [HDHE][DEHP] ionic liquid Take 4.25g of [TEEA][DEHP], dissolve it in methanol and add it dropwise to a round-bottom flask. Place the round-bottom flask in an oil bath and start stirring. Take 0.71g of 1,7-octadiene diepoxide and add it dropwise. After the addition is complete, stir and react at 25°C for 6 to 12 hours to ensure that the reagents react completely. Use a rotary evaporator to remove the methanol, and then place it in a vacuum drying oven to dry for 10 to 12 hours. The resulting product is a highly viscous dark red liquid, recorded as [HDHE][DEHP].
[0026] 1 H NMR (chloroform-d, 600 MHz) δ 0.79–1.02 (m, 18 H, CH3), 1.12–1.64 (m, 62 H, CH, CH2), 2.19–2.64 (m, 4 H, C–CH2–N), 2.62–3.17 (m, 8 H, N–CH2–CH2–N + ), 3.60–3.80 (m, 6H, O–CH2–C, CH–O), 5.13–6.09 (s, 2H,–N + H2). Take 0.04g of [HDHE][DEHP] ionic liquid in a 20ml reagent bottle and add 3.96g of pure hexadecane base oil to prepare an oil sample with a mass concentration of 1%. Figure 2 The tribological properties are shown in Table 1, and the extreme pressure resistance properties are shown in Table 2.
[0027] Example 2 The preparation of [HDHE][DEHP] dianionic oil-soluble ionic liquid is the same as in Example 1. 0.08 g of [HDHE][DEHP] ionic liquid is placed in a 20 ml reagent bottle and 3.92 g of pure hexadecane base oil is added to prepare an oil sample with a mass concentration of 2%. Figure 2 The tribological properties are shown in Table 1, and the extreme pressure resistance properties are shown in Table 2.
[0028] Example 3 The preparation of [HDHE][DEHP] dianionic oil-soluble ionic liquid is the same as in Example 1. 0.12 g of [HDHE][DEHP] ionic liquid is placed in a 20 ml reagent bottle and 3.88 g of pure hexadecane base oil is added to prepare an oil sample with a mass concentration of 3%. Figure 2 The tribological properties are shown in Table 1, and the extreme pressure resistance properties are shown in Table 2.
[0029] Example 4 The preparation of [HDHE][DEHP] dianionic oil-soluble ionic liquid is the same as in Example 1. 0.16 g of [HDHE][DEHP] ionic liquid is placed in a 20 ml reagent bottle and 3.84 g of pure hexadecane base oil is added to prepare an oil sample with a mass concentration of 4%. Figure 2 The tribological properties are shown in Table 1, and the extreme pressure resistance properties are shown in Table 2.
Claims
1. A dianionic oil-soluble ionic liquid, the structural formula of which is as follows: R is n-dodecyl.
2. A method for preparing the dianionic oil-soluble ionic liquid according to claim 1, characterized in that: The following steps are involved: 1) Preparation of [DETA][DEHP] ionic liquids Add diisooctyl phosphate dropwise into diethylenetriamine, fully stir and react for 12-24 hours at room temperature, and vacuum dry to obtain diethylenetriammonium diisooctyl phosphate ionic liquid; 2) Preparation of [TEEA][DEHP] ionic liquid The diethylenetriammonium salt diisooctyl phosphate ionic liquid is dissolved in methanol, and then 1,2-epoxytetradecane is slowly added thereto, and the mixture is stirred and reacted for 6 to 12 hours at room temperature, and the solvent is evaporated off and vacuum dried to obtain the dihydroxypentadecylaminoethylammonium salt diisooctyl diphosphate ionic liquid; 3) Preparation of [HDHE][DEHP] ionic liquid The obtained dihydroxypentadecanylaminoethylammonium salt diisooctyl diphosphate ionic liquid is dissolved in methanol, and then 1,7-octadiene diepoxide is slowly added thereto, and the reaction is fully stirred at room temperature for 6 to 12 hours. After the solvent is evaporated off, the mixture is vacuum dried to obtain a dianionic oil-soluble ionic liquid.
3. The method for preparing a dianionic oil-soluble ionic liquid according to claim 2, characterized in that: In step 1), the molar ratio of diethylenetriamine to diisooctyl phosphate is 1:1 to 1.
005.
4. The method for preparing a dianionic oil-soluble ionic liquid according to claim 2, characterized in that: In step 2), the molar ratio of the diethylenetriammonium diisooctyl phosphate ionic liquid to 1,2-epoxytetradecane is 1:2 to 2.
001.
5. The method for preparing a dianionic oil-soluble ionic liquid according to claim 2, characterized in that: In step 3), the molar ratio of the dihydroxypentadecanylaminoethylammonium salt diisooctyl diphosphate ionic liquid to the 1,7-octadiene diepoxide compound is 1:1 to 1.
001.
6. Use of the oil-soluble dianionic oil-soluble ionic liquid as claimed in claim 1 as an additive for n-hexadecane lubricating oil.
Citation Information
Patent Citations
Preparation method and application of binary ionic liquid eutectic
CN118222343A
Polycationized phospholipid derivative
WO2010026621A1