Laminating method for hot-bending special-shaped screen

By using a combination of sealant and filler during the bonding process of hot-bending special-shaped screens, the problems of macular, light leakage and bubbles that occur after bonding in the existing technology are solved, the product pass rate and production efficiency are improved, and the product is saved resource.

CN119062638APending Publication Date: 2024-12-03SUZHOU TONGLI PHOTOELECTRIC CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411228614.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-03
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The existing bonding methods of hot-bending special-shaped covers and LCMs have bad problems such as macula, light leakage, and bubbles after bonding, resulting in low product pass rate, large loss of production operations, and waste of manpower and resources.

Method used

Using a bonding method of hot-bending special-shaped screen, by setting sealant on the LCM and setting LCM on the contour groove of the fitting fixture, when the hot-bending special-shaped cover plate is pressed on the sealant, ensure that The original shape fits with LCM, and fills the container into the storage space through the glue injection port. The filler can flow into the corners to avoid bad problems, improve product pass rate, and reduce production losses.

Benefits of technology

The complete fit between the hot-bent special-shaped cover plate and the LCM is achieved, avoiding problems such as macular spots, light leakage, and bubbles after bonding, improving product qualification rate, reducing production operations losses, and saving manpower and resources.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119062638A_ABST
    Figure CN119062638A_ABST
Patent Text Reader

Abstract

The invention relates to a fitting method for a hot-bending special-shaped screen. The fitting method of the hot-bending special-shaped screen comprises the following steps that a hot-bending special-shaped cover plate, an LCM and a fitting jig are provided, the fitting jig comprises a jig body and a plurality of limiting protrusions, a profiling groove used for containing the LCM is formed in the jig body, and the limiting protrusions are arranged along the outline of the jig body and form a profiling limiting space used for containing the hot-bending special-shaped cover plate; a circle of sealant which does not form a closed loop is coated along the contour edge of the LCM, and a first opening is reserved; the LCM is arranged in the profiling groove, the hot-bending special-shaped cover plate is arranged in the profiling limiting space and attached to the side, provided with the sealant, of the LCM, the hot-bending special-shaped cover plate, the LCM and the sealant define a containing space, and a glue injection opening communicated with the containing space is formed in the first opening; filling glue is injected into the containing space from the glue injection opening and cured, and the hot-bending special-shaped screen is obtained. By means of the arrangement, the problems that the product percent of pass is low, production operation loss is large, and manpower and resources are wasted are solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of laminating technology, and in particular to a laminating method for heat-bent special-shaped screens. Background Art

[0002] With the continuous development of the electronic products industry, the display screens in electronic products are becoming more and more diversified. Among them, the hot-bent special-shaped screens are loved and sought after by consumers. The hot-bent special-shaped screens include hot-bent special-shaped cover plates and LCM (LCD Module, liquid crystal display module).

[0003] At present, the bonding method of the heat-bent special-shaped cover plate and the LCM is usually to use OCA (Optically Clear Adhesive) optical adhesive for bonding. Specifically, the OCA optical adhesive film is first bonded to the heat-bent special-shaped cover plate, and then the LCM is bonded to the side of the OCA optical adhesive film facing away from the heat-bent special-shaped cover plate.

[0004] However, the above-mentioned bonding method has problems such as yellow spots, light leakage, bubbles, etc. after bonding, resulting in a low product qualification rate, large production operation losses, and a waste of manpower and resources. Summary of the invention

[0005] Based on this, it is necessary to provide a method for bonding hot-bent special-shaped screens to address the problems of low product qualification rate, large production operation losses, and waste of manpower and resources in the current process of bonding hot-bent special-shaped screens.

[0006] A method for laminating a heat-bent special-shaped screen comprises the following steps:

[0007] S1. Provide a heat-bent special-shaped cover plate, an LCM and a fitting jig, wherein the fitting jig comprises a jig body and a plurality of limiting protrusions, wherein the jig body is provided with a contoured groove for placing the LCM, and the plurality of limiting protrusions are arranged around the contour of the jig body and form a contoured limiting space for placing the heat-bent special-shaped cover plate;

[0008] S2, applying a circle of sealant that does not form a closed loop along the contour edge of the LCM to reserve a first opening;

[0009] S3, placing the LCM in the profiling groove, placing the heat-bent special-shaped cover plate in the profiling limiting space and attaching it to the side of the LCM where the sealant is provided, so that the heat-bent special-shaped cover plate, the LCM and the sealant form a containing space, and forming a glue injection port communicating with the containing space at the first opening;

[0010] S4, injecting filling glue into the accommodating space from the glue injection port and curing the filling glue to obtain the thermally bent special-shaped screen.

[0011] In one of the embodiments, in step S2, a second opening spaced apart from the first opening is reserved, and in step S3, after the heat-bent special-shaped cover plate is attached to the side of the LCM where the sealant is provided, an exhaust port connected to the accommodating space is formed at the second opening.

[0012] In one embodiment, in step S2, it further includes pre-embedding a first embedded part and a second embedded part at the first opening and the second opening respectively;

[0013] In step S3, after the heat-bent special-shaped cover plate is attached to the side of the LCM where the sealant is provided, the first embedded part and the second embedded part are pulled out after the sealant is naturally cured to form the injection port and the exhaust port.

[0014] In one embodiment, the first embedded part and / or the second embedded part is a double-sided adhesive tape.

[0015] In one embodiment, the natural curing time of the sealant is not less than 4 hours.

[0016] In one embodiment, in step S2, the specific steps are:

[0017] S21, placing the LCM in a dispensing fixture;

[0018] S22, using a glue dispensing machine to apply a circle of the sealant that does not form a closed loop along the contour edge of the LCM, and reserve the first opening.

[0019] In one of the embodiments, the dispensing air pressure value used in the dispensing machine ranges from 0.5 MPa to 0.7 MPa.

[0020] In one embodiment, in step S4, the following steps are also specifically included:

[0021] S41, using a glue mixer to fill the containing space with the filling glue from the glue injection port to obtain a semi-finished module;

[0022] S42, curing the filling glue at high temperature to obtain the heat-bent special-shaped screen.

[0023] In one embodiment, the curing temperature of the filling glue ranges from 45°C to 85°C.

[0024] In one embodiment, the sealant is RTV glue.

[0025] The above-mentioned method for bonding the heat-bent special-shaped screen is to set the sealant on the LCM and set the LCM on the contoured groove of the bonding fixture. When the heat-bent special-shaped cover is pressed on the sealant, it is also located in the contoured limiting space of the bonding fixture, ensuring that the heat-bent special-shaped cover is bonded to the LCM according to the original shape, and achieving complete bonding between the heat-bent special-shaped cover and the edge of the LCM. Then, the filling glue is canned into the accommodation space formed by the heat-bent special-shaped cover, LCM and sealant through the glue injection port. The filling glue can flow to fill every corner of the accommodation space, avoiding the occurrence of yellow spots, light leakage, bubbles and other undesirable problems after bonding, improving the product qualification rate, reducing production operation losses, and saving manpower and production resources. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] The drawings constituting a part of the present application are used to provide a further understanding of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application.

[0027] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0028] FIG1 is a schematic diagram of the structure of the bonding fixture provided in the present application.

[0029] FIG. 2 is a flow chart of a method for bonding a heat-bent special-shaped screen provided by the present invention.

[0030] in:

[0031] 10. Fit the fixture;

[0032] 100, fixture body; 110, first fitting portion; 120, second fitting portion; 130, connecting portion; 140, contoured groove;

[0033] 200, limiting protrusion; 300, contoured limiting space. DETAILED DESCRIPTION

[0034] In order to make the above-mentioned purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present application, so the present application is not limited by the specific embodiments disclosed below.

[0035] In the description of the present application, it should be understood that if the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential", etc. appear, the orientation or position relationship indicated by these terms is based on the orientation or position relationship shown in the accompanying drawings, which is only for the convenience of describing the present application and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application.

[0036] In addition, if the terms "first" or "second" appear, these terms are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include at least one of the features. In the description of this application, if the term "plurality" appears, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0037] In this application, unless otherwise clearly specified and limited, if the terms "installed", "connected", "connected", "fixed" and the like appear, these terms should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integrated connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to the specific circumstances.

[0038] In the present application, unless otherwise clearly specified and limited, if there is a description that a first feature is "above" or "below" a second feature, etc., or similar descriptions appear, it may mean that the first and second features are in direct contact, or that the first and second features are in indirect contact through an intermediate medium. Moreover, the first feature being "above", "above" and "above" the second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. The first feature being "below", "below" and "below" the second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0039] It should be noted that if an element is referred to as being "fixed to" or "disposed on" another element, it may be directly on the other element or there may be a central element. If an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. If any, the terms "vertical", "horizontal", "upper", "lower", "left", "right" and similar expressions used in this application are for illustrative purposes only and do not represent the only implementation method.

[0040] The applicant has found through research that the current bonding method of the heat-bent special-shaped cover plate and LCM is usually bonded with OCA (Optically Clear Adhesive), specifically, the OCA optical adhesive film is first bonded to the heat-bent special-shaped cover plate, and then the LCM is bonded to the side of the OCA optical adhesive film away from the heat-bent special-shaped cover plate. However, the above bonding method has problems such as yellow spots, light leakage, bubbles, etc. after bonding, resulting in low product qualification rate, large production operation loss, and waste of manpower and resources.

[0041] In order to solve the above problems, referring to FIG. 1 and FIG. 2, FIG. 1 shows a schematic diagram of the structure of a bonding jig 10 in an embodiment of the present application, and FIG. 2 shows a flow chart of a bonding method for a heat-bent special-shaped screen in an embodiment of the present application. The bonding method for a heat-bent special-shaped screen provided in an embodiment of the present application includes the following steps:

[0042] Step S1, providing a hot-bent special-shaped cover plate, LCM and a fitting jig 10, the fitting jig 10 includes a jig body 100 and a plurality of limiting protrusions 200, the jig body 100 is provided with a contoured groove 140 for placing the LCM, the plurality of limiting protrusions 200 are arranged at intervals around the contour of the jig body 100, and a contoured limiting space 300 for placing the hot-bent special-shaped cover plate is formed between the plurality of limiting protrusions 200. In the specific setting, the jig body 100 includes a first fitting portion 110, a second fitting portion 120 and a connecting portion 130 connecting the first fitting portion 110 and the second fitting portion 120, wherein the horizontal height of the first fitting portion 110 is arranged above the horizontal height of the second fitting portion 120, and the connecting portion 130 is used to transition the first fitting portion 110 and the second fitting portion 120. The first fitting portion 110 and the second fitting portion 120 are both provided with a contoured groove 140, and the tops of the first fitting portion 110, the second fitting portion 120 and the connecting portion 130 are all provided with limiting protrusions 200, and the contoured limiting space 300 surrounded by multiple limiting protrusions 200 is adapted to the shape of the hot-bent special-shaped cover plate.

[0043] Step S2, apply a circle of sealant without forming a closed loop along the contour edge of the LCM, and the position where the sealant is not applied is the reserved first opening. It should be noted that the setting of the first opening is to facilitate the glue injection operation in the subsequent steps after the glue injection port is formed.

[0044] Step S3, place the side of the LCM facing away from the sealant in the profiling groove 140, and place the heat-bent special-shaped cover plate in the profiling limiting space 300 and fit it to the side of the LCM with the sealant, so that the heat-bent special-shaped cover plate, the LCM and the sealant form a containing space, and the first opening forms a glue injection port connected to the containing space. In specific operations, one LCM may be provided in each profiling groove 140, so that the heat-bent special-shaped cover plate and multiple LCMs can be bonded. In order to ensure the bonding effect, the heat-bent special-shaped cover plate and the LCM are usually wiped before bonding to ensure the cleanliness of the heat-bent special-shaped cover plate and the LCM.

[0045] Step S4, injecting filling glue into the accommodation space from the glue injection port and curing it to obtain a heat-bent special-shaped screen. In the specific setting, when the filling glue fills the accommodation space, it will also seal the glue injection port to form a whole bonding layer. In order to ensure the sealing of the glue injection port, after the filling glue fills the accommodation space, the glue injection port can be re-coated with sealant. In order to ensure the cleanliness of the heat-bent special-shaped screen, after step S4, the following step is also included: using a glue cleaning stick to remove the overflowed glue.

[0046] The above-mentioned method for bonding the heat-bent special-shaped screen is to set the sealant on the LCM and set the LCM on the contour groove 140 of the bonding fixture 10. When the heat-bent special-shaped cover plate is pressed on the sealant, it is also located in the contour limiting space 300 of the bonding fixture 10, ensuring that the heat-bent special-shaped cover plate is bonded to the LCM according to the original shape, and achieving complete bonding between the heat-bent special-shaped cover plate and the edge of the LCM. Then, filler glue is injected into the accommodation space formed by the heat-bent special-shaped cover plate, LCM and sealant through the glue injection port. The filler glue can flow and fill every corner in the accommodation space, avoiding the occurrence of yellow spots, light leakage, bubbles and other undesirable problems after bonding, improving the product qualification rate, reducing production operation losses, and saving manpower and production resources.

[0047] It should be noted that when a single LCM does not meet the requirements after bonding, the defective LCM can be disassembled separately and then bonded using the bonding fixture 10, which can ensure that the relative positions of the two LCMs remain unchanged and the defective LCM can be replaced quickly and conveniently.

[0048] In order to ensure that the filling glue fills the entire accommodating space, a preferred implementation method is to reserve a second opening spaced apart from the first opening in step S2, and in step S3, after the hot-bent special-shaped cover plate is attached to the side of the LCM where the sealant is provided, an exhaust port connected to the accommodating space is formed at the second opening. Through the above arrangement, in the process of the filling glue flowing from the injection port to the accommodating space and filling the accommodating space, the existence of the exhaust port facilitates the release of the pressure generated during the injection of glue, and facilitates the discharge of gas in the accommodating space, so that the filling glue fills the entire accommodating space, avoiding the occurrence of bubbles in the local accommodating space that affect the bonding effect. In specific operations, when the filling glue fills the accommodating space, it will also seal the injection port and the exhaust port to form a whole bonding layer.

[0049] In order to ensure that the injection port and the exhaust port are not blocked by the sealant after the hot-bent special-shaped cover plate is attached to the LCM, specifically, in step S2, it also includes pre-embedding the first embedded part and the second embedded part at the first opening and the second opening respectively, and then proceeding to step S3, setting the LCM in the profiling groove 140, the hot-bent special-shaped cover plate is located in the profiling limit space 300 and attached to the side of the LCM where the sealant is provided, and after the sealant is naturally cured, the first embedded part and the second embedded part are pulled out, and the first opening and the second opening are respectively formed as the injection port and the exhaust port. It should be noted that the height of the cured sealant is greater than the height of the first embedded part and also greater than the height of the second embedded part.

[0050] In specific settings, the first embedded part and / or the second embedded part are preferably double-sided adhesive tape. The length and width of the double-sided adhesive tape are set according to actual conditions. This application does not limit the length and width of the double-sided adhesive tape. For example, the width of the double-sided adhesive tape is 1.5 mm and the length is 2 mm.

[0051] In order to allow the sealant to cure at an appropriate time, more specifically, the natural curing time of the sealant is preferably not less than 4 hours. In specific settings, the natural curing time of the sealant can be any value of 5 hours, 8 hours, or greater than 4 hours. Through the above settings, insufficient curing of the sealant caused by the natural curing time of the sealant being less than 4 hours is avoided, ensuring that the sealant is fully cured and the hot-bent special-shaped cover plate is tightly combined with the LCM.

[0052] In order to facilitate the application of sealant on the contour edge of the LCM, a preferred implementation manner, in step S2, includes the following specific steps:

[0053] Step S21, setting the LCM in a dispensing jig. In the specific setting, the dispensing jig has a positioning frame that matches the shape of the LCM. The LCM is set in the positioning frame to facilitate the subsequent dispensing operation; Step S22, using a dispensing machine to apply a circle of sealant that does not form a closed loop along the contour edge of the LCM, reserving a first opening. In the specific setting, a second opening will also be reserved.

[0054] In the specific operation, three-axis dispensing is generally used for dispensing. It should be noted that by applying sealant on LCM using the dispensing mode, sealant with uneven thickness can be formed on the surface of LCM to compensate for the warping of the hot-bent special-shaped cover plate, so that the sealant matches the warped surface of the hot-bent special-shaped cover plate, avoiding the current flat OCA optical adhesive film covering the LCM and the hot-bent special-shaped cover plate, which will cause the unevenness around the bonding area between the two. After the LCM and the heat-bent special-shaped cover plate are sealed and attached with sealant, the accommodating space formed by the LCM, the heat-bent special-shaped cover plate and the sealant is filled with filling glue, ensuring that there is sufficient glue in the gap between the LCM and the heat-bent special-shaped cover plate with a certain warpage, avoiding light leakage and easy appearance of bubbles caused by using a flat glue layer to cover the heat-bent special-shaped cover plate with a certain warpage in the dry glue process, thereby solving the problem that the heat-bent special-shaped cover plate is difficult to combine with the LCM due to the certain warpage of the heat-bent special-shaped cover plate.

[0055] In order to ensure that the dispensing machine can have a suitable dispensing speed when applying sealant on LCM, specifically, the dispensing air pressure value used in the dispensing machine ranges from 0.5 MPa to 0.7 MPa. In the specific setting, the dispensing air pressure value can be any value between 0.55 MPa, 0.6 MPa, 0.67 MPa and 0.5 MPa-0.7 MPa. Through the above setting, it is avoided that the dispensing air pressure value is less than 0.5 MPa, which causes the sealant to be discharged slowly, affecting the production efficiency, and it is also avoided that the dispensing air pressure value is greater than 0.7 MPa, which causes the dispensing speed to be too fast. When the dispensing speed is too fast, it is easy to cause a large amount of sealant to accumulate at a certain point of the LCM, resulting in sealant waste, and when too much sealant is attached to the hot-bent special-shaped cover plate, the sealant flows within a certain range, which increases the difficulty and labor cost of cleaning the sealant after the sealant is solidified.

[0056] In order to ensure the filling efficiency of the filling glue, a preferred implementation manner, in step S4, specifically further includes the following steps:

[0057] S41. Use a glue mixer to fill the containing space with the filling glue from the glue injection port to obtain a semi-finished module. When setting it specifically, it is also necessary to set the parameters of the glue mixer, including the amount of glue injection. The specific amount of glue injection is calculated according to the volume of the containing space and the density of the filling glue. The volume of the containing space is multiplied by the density of the filling glue to obtain the budgeted amount of glue injection. A tolerance range of 5g-10g is added to the budgeted amount of glue injection to obtain the specific amount of glue injection. In order to ensure the efficiency of the filling glue, the injection speed range of the filling glue is preferably any value between 0.1g / s and 0.15g / s. Through the above setting, it is avoided that when the injection speed is greater than 0.15g / s, the filling glue is injected too fast to generate bubbles, and when the injection speed is less than 0.1g / s, the injection efficiency of the filling glue is also avoided. When it is used specifically, the needle of the glue mixer is inserted into the glue injection port to inject the filling glue until the filling glue completely fills the entire containing space.

[0058] S42, high-temperature curing of the filling glue to obtain a hot-bent special-shaped screen. In the specific setting, the curing temperature range of the filling glue is preferably between 55°C-85°C. In the specific setting, the formed semi-finished module is placed in a heating chamber for high-temperature curing. The curing temperature of the filling glue can be any value between 60°C, 70°C and 55°C-85°C. Through the above setting, when the curing temperature of the filling glue is less than 55°C, the curing time of the filling glue is too long, which affects the production efficiency. It is also avoided that when the curing temperature of the filling glue is greater than 85°C, it will cause adverse effects on the functions of the hot-bent special-shaped cover plate and the LCM.

[0059] During the specific operation, the semi-finished module can be placed in an oven for high-temperature curing. Specifically, the semi-finished module can be placed in a turnover plate, and the turnover plate carrying the semi-finished module can be placed in an oven for high-temperature curing. It should be emphasized that this application does not limit the high-temperature curing time of the filling glue, which can be set according to the use requirements. Exemplarily, the high-temperature curing time of the filling glue is not less than 1h.

[0060] In order for the sealant to firmly connect the LCM and the hot-bent special-shaped cover plate, the sealant is preferably RTV glue. It should be noted that RTV glue is room temperature vulcanized silicone rubber (RTV) glue, which has good bonding properties, moisture-proof and shock-proof functions, and has excellent properties such as strong plasticity, strong fluidity, non-toxicity, no pollution and no corrosion, and also has good electrical insulation and arc resistance.

[0061] In order to ensure the quality of the provided hot-bent special-shaped cover plate, LCM and laminating jig 10, a preferred implementation manner further includes the following steps before step S1:

[0062] Check the appearance, size and function of the incoming materials, and select the hot-bent special-shaped cover plates, LCM and bonding jigs 10 that meet the requirements from the incoming materials. It is not difficult to understand that before step S1, it also includes an incoming material inspection step. The incoming material inspection refers to the quality inspection of raw materials or components by sampling, and finally makes a judgment on whether the batch of products is acceptable or rejected. The incoming materials in this application refer to hot-bent special-shaped cover plates, LCM and bonding jigs 10. By checking the appearance, size and function of the hot-bent special-shaped cover plates, LCM and bonding jigs 10 one by one, the hot-bent special-shaped cover plates, LCM and bonding jigs 10 that meet the requirements are selected for subsequent processes to avoid the mistaken delivery of defective products.

[0063] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0064] The above-described embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be construed as limiting the scope of the patent application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent application shall be subject to the attached claims.

Claims

1. A method for bonding a heat-bent special-shaped screen, characterized in that: The steps include: S1. Provide a heat-bent special-shaped cover plate, an LCM and a fitting jig, wherein the fitting jig comprises a jig body and a plurality of limiting protrusions, wherein the jig body is provided with a contoured groove for placing the LCM, and the plurality of limiting protrusions are arranged around the contour of the jig body and form a contoured limiting space for placing the heat-bent special-shaped cover plate; S2, applying a circle of sealant that does not form a closed loop along the contour edge of the LCM to reserve a first opening; S3, placing the LCM in the profiling groove, placing the heat-bent special-shaped cover plate in the profiling limiting space and attaching it to the side of the LCM where the sealant is provided, so that the heat-bent special-shaped cover plate, the LCM and the sealant form a containing space, and forming a glue injection port communicating with the containing space at the first opening; S4, injecting filling glue into the accommodating space from the glue injection port and curing the filling glue to obtain the thermally bent special-shaped screen.

2. The method for bonding a heat-bent special-shaped screen according to claim 1, characterized in that: In step S2, a second opening spaced apart from the first opening is reserved. In step S3, after the heat-bent special-shaped cover plate is attached to the side of the LCM provided with the sealant, an exhaust port communicating with the accommodating space is formed at the second opening.

3. The method for bonding a heat-bent special-shaped screen according to claim 2, characterized in that: In step S2, it also includes pre-embedding a first embedded part and a second embedded part at the first opening and the second opening respectively; In step S3, after the heat-bent special-shaped cover plate is attached to the side of the LCM where the sealant is provided, the first embedded part and the second embedded part are pulled out after the sealant is naturally cured to form the injection port and the exhaust port.

4. The method for bonding a heat-bent special-shaped screen according to claim 3, characterized in that: The first embedded part and / or the second embedded part are double-sided adhesive tapes.

5. The method for bonding a heat-bent special-shaped screen according to claim 3, characterized in that: The natural curing time of the sealant is not less than 4 hours.

6. The method for bonding a heat-bent special-shaped screen according to claim 1, characterized in that: In step S2, the specific steps are: S21, placing the LCM in a dispensing fixture; S22, using a glue dispensing machine to apply a circle of the sealant that does not form a closed loop along the contour edge of the LCM, and reserve the first opening.

7. The method for bonding a heat-bent special-shaped screen according to claim 6, characterized in that: The dispensing air pressure value used in the dispensing machine ranges from 0.5 MPa to 0.7 MPa.

8. The method for bonding a heat-bent special-shaped screen according to claim 1, characterized in that: In step S4, the following steps are specifically included: S41, using a glue mixer to fill the containing space with the filling glue from the glue injection port to obtain a semi-finished module; S42, curing the filling glue at high temperature to obtain the heat-bent special-shaped screen.

9. The method for bonding a heat-bent special-shaped screen according to claim 8, characterized in that: The curing temperature of the filling glue is in the range of 45°C to 85°C.

10. The method for bonding a heat-bent special-shaped screen according to claim 1, characterized in that: The sealant is RTV glue.