Concrete structure crack detection method based on quantum measurement technology

Through the multi-beam particle beam scanning and fixed-point detection method using quantum measurement technology in concrete structures, the problems of low crack detection efficiency and limited depth in the concrete structure in the prior art are solved, and efficient and accurate crack detection is achieved, satisfying the Inspection requirements for existing hydraulic concrete structures.

CN119065013AActive Publication Date: 2024-12-03SI CHUAN YANG GUANG MO XIN KE JI YOU XIAN GONG SI

Patent Information

Application Number
CN202411564442.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-11-05
Publication Date
2024-12-03
Estimated Expiration
2044-11-05

AI Technical Summary

Technical Problem

The existing crack detection methods for concrete structures are inefficient. Traditional ultrasonic and surface wave detection can only detect depths within 500mm, and may cause irreversible damage to the structure. The existing particle-based method has limited design strategies when laying grid lines. The detection efficiency still needs to be improved.

Method used

Using the crack detection method of concrete structures based on quantum measurement technology, by emitting multiple beams of concrete particle beams on the plane of concrete structure, scanning and detecting and recording electrical signal data, first determine the crack boundary range, and then set detection points within this range for fixed-point detection , improve detection efficiency and accuracy.

Benefits of technology

It realizes efficient and accurate non-destructive detection of concrete structure cracks, can detect depth up to 500m, and identify seams with a width of 0.1 microns, reducing construction workload and safety risks, and improving the accuracy and efficiency of detection results.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119065013A_ABST
    Figure CN119065013A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of concrete material detection, in particular to a concrete structure crack detection method based on a quantum measurement technology, which comprises the following steps of: S10, transmitting a concrete particle beam perpendicular to a plane, scanning and detecting from one side of the plane to the other side, converting received electromagnetic particle characterization physical quantity to obtain electric signal data, and transmitting the electric signal data to a server; recording a first position of the detection point when the electric signal data is changed for the first time and a second position of the detection point when the electric signal data is changed for the last time; s20, carrying out scanning detection on the basis of the second direction of the plane, and recording a third position and a fourth position of the detection point when the electric signal data is changed for the first time and the last time; and S30, setting a plurality of detection points in a range defined by the first, second, third and fourth positions, and determining the size parameters of the crack according to the electric signal data of all the detection points. According to the invention, the concrete detection efficiency can be improved, and great technical progress is made in the field of concrete detection.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of concrete material detection, and in particular to a concrete structure crack detection method based on quantum measurement technology. Background Art

[0002] Concrete structures are widely used in hydropower and hydraulic bridge piers, reservoirs and dams, highways, high-speed railways and other bridge piers. Due to the stress and material changes of the concrete structure's own components, micro cracks (lines) will occur. Cracks in concrete structures are caused by factors such as the load borne by the structure, shrinkage and deformation of concrete materials, temperature changes, and corrosion of steel bars in concrete. Cracks seriously affect the service life of concrete structures. Detecting and identifying the crack morphology and degree of damage inside concrete structures is the basis for deciding whether to repair and adopting repair standards.

[0003] Traditional non-destructive testing methods for concrete mainly include ultrasonic testing and surface wave testing, which can generally only detect cracks within a depth of 500 mm. Three-dimensional seismic wave detection cannot be used for crack detection in concrete dams or bridge piers, because detection requires a certain intensity of earthquake source, which will cause irreversible damage to the concrete structure. With the development of quantum particle technology, concrete crack detection technology based on quantum particles has emerged. For example, the Chinese invention with application number CN202410025818.2 proposed "A method for concrete detection based on quantum particles", which can directly detect cracks in concrete structures, eliminate the interference caused by the complex extension of concrete structure cracks and differences in manual interpretation, and cracks with a width greater than or equal to 0.5 mm can be fully identified. Although this method has designed a variety of strategies when arranging grid lines, the applicant found in continued research that the detection efficiency of this method still needs to be improved. Summary of the invention

[0004] The purpose of the present invention is to provide a concrete structure crack detection method based on quantum measurement technology, which can not only realize crack detection in the concrete structure, but also improve the detection efficiency.

[0005] In order to achieve the above object, the present invention provides the following technical solutions:

[0006] A method for detecting cracks in a concrete structure based on quantum measurement technology comprises the following steps:

[0007] S10, on a plane of the concrete structure, based on the first direction of the plane, the particle host emits a concrete particle beam perpendicular to the plane, scans and detects from one side of the plane to the other side, records the physical quantity represented by the received electromagnetic particles, and converts and obtains electrical signal data, determines whether the electrical signal data changes, and records the first position of the detection point when the electrical signal data changes for the first time and the second position of the detection point when the electrical signal data changes for the last time;

[0008] S20, based on a second direction of the plane perpendicular to the first direction, scanning and detecting from one side of the plane to the other side, recording and receiving physical quantities representing electromagnetic particles, and converting and obtaining electrical signal data, determining whether the electrical signal data has changed, and recording a third position of the detection point when the electrical signal data changes for the first time and a fourth position of the detection point when the electrical signal data changes for the last time;

[0009] S30, taking the range defined by the first position, the second position, the third position and the fourth position as the fixed-point detection range, setting a number of detection points within the fixed-point detection range, at each detection point the particle host emits a concrete particle beam perpendicular to the plane, records the received electromagnetic particle representation physical quantity, and converts it to obtain electrical signal data, and determines the size parameters of the crack according to the electrical signal data of all detection points.

[0010] In the above scheme, the first position, the second position, the third position, and the fourth position are first determined by scanning detection, and then the crack boundary range is delineated by these four positions, and then detection points are arranged within the boundary range for refined fixed-point detection. Scanning detection only focuses on whether the electrical signal data changes without performing detailed calculations. Therefore, compared with directly arranging a large number of grid lines in the plane for fixed-point refined detection, it saves time for large-area point arrangement, can quickly detect the crack morphology, and improve work efficiency. Moreover, the scanning detection method is more conducive to the one-time accurate determination of the boundary range, avoiding inaccurate boundaries due to large detection point spacing, and can also avoid low detection efficiency due to multiple reductions in the detection point spacing.

[0011] The concrete particle beams emitted by the particle measuring host are multiple concrete particle beams, which are cylindrical.

[0012] In the above scheme, the concrete particle beam is a multi-beam concrete particle beam, and the energy of N-beam concrete particle beam is N times that of a single-beam concrete particle beam. Therefore, this can enhance the energy of the received electromagnetic particles representing the physical quantity. When judging whether a change has occurred and performing corresponding conversion based on the electrical signal data obtained by converting the physical quantity represented by the electromagnetic particles, compared with a single-beam concrete particle beam, the change amount can be amplified N times, which is more conducive to accurate judgment, avoids the situation where small changes cannot be accurately identified, and improves the accuracy of the detection results.

[0013] In S30, the ranges defined by S1-S, S2+S, S3-S, and S4+S are the fixed-point detection ranges, S1, S2, S3, and S4 represent the first position, the second position, the third position, and the fourth position, respectively, and S represents the distance moved in the direction away from the crack.

[0014] The range delineated by S1, S2, S3, and S4 is the initial fixed-point detection range, and the range delineated by S1-S, S2+S, S3-S, and S4+S is the revised fixed-point detection range. In the above scheme, a certain margin is reserved on the initially determined boundary range, that is, the initially determined boundary range is expanded a little to improve the fault tolerance, which can further improve the accuracy of the crack boundary range and avoid missing boundary points due to excessive scanning speed during scanning detection.

[0015] In S30, the process of setting a plurality of detection points within the fixed-point detection range includes: arranging a plurality of transverse detection lines and longitudinal detection lines at equal intervals within the fixed-point detection range, and arranging a plurality of detection points at equal intervals along the transverse detection lines and longitudinal detection lines, respectively.

[0016] The detection points on the transverse detection line and the longitudinal detection line can overlap or be independent of each other. By arranging the detection points at equal intervals, the detection points can be distributed more evenly, which is conducive to more accurately obtaining the three-dimensional spatial distribution of the crack based on the detection point data.

[0017] If the crack is a crack that is at a non-right angle to the detection plane, then in S30, the process of obtaining the response depth of the crack based on the electrical signal data of one detection point includes:

[0018] A concrete particle beam is emitted vertically downward from the detection point, and the detection depth is continuously increased for detection. It is determined whether the electrical signal data obtained by converting the physical quantity represented by the received electromagnetic particles has changed. The depth value corresponding to the first change in the electrical signal data and the depth value corresponding to the last change are recorded. The difference between the two depth values ​​is the response depth value of the crack.

[0019] If the crack is a vertical crack, then in S30, from the first position to the second position, it is determined whether the electrical signal data obtained by the conversion of each detection point has changed, and the fifth position and time of the detection point when the electrical signal data changes for the first time and the sixth position and time of the detection point when the electrical signal data changes for the last time are recorded, and the width of the crack is calculated according to the following formula: , W represents the width of the crack, S EF represents the distance between the fifth position and the sixth position, and d represents the length of the concrete particle beam range;

[0020] From the third position to the fourth position, determine whether the electrical signal data obtained by the conversion of each detection point has changed, record the seventh position and time of the detection point when the electrical signal data changes for the first time, and the eighth position and time of the detection point when the electrical signal data changes for the last time, and calculate the length of the crack according to the following formula: , L represents the width of the crack, S GHIndicates the distance between the seventh position and the eighth position.

[0021] S EF Calculated by the following formula: , t E ,t F They are respectively the direction from the first position to the second position, the time when the electrical signal data changes for the first time, and the time when it changes for the last time, and V is the horizontal moving speed of the particle host.

[0022] In S30, during the fixed-point detection process in the direction from the first position to the second position, the position at which the change in the electrical signal data is the largest is determined, and a concrete particle beam is emitted vertically downward at this position. The detection depth is gradually increased until the electrical signal data no longer changes. The electrical signal data and depth data at this time are recorded. The depth data is the response depth value of the crack.

[0023] For different cracks, different calculation methods are used according to the characteristics of the cracks, which can help improve the accuracy of the three-dimensional spatial distribution of the cracks.

[0024] Compared with the prior art, the present invention can not only realize non-destructive crack detection, but also has high accuracy and high efficiency. The specific description is as follows:

[0025] 1) The detection method is non-contact detection, which greatly improves work efficiency and ensures safe detection.

[0026] Traditional ultrasonic crack detection requires placing detectors near the cracks, which greatly increases the workload of crack detection construction, including the manual placement of detectors and the use of coupling agents. In addition, crack detection in power stations and bridge piers requires the setting up of ladders and hanging baskets, which also increases the safety risks of construction workers.

[0027] Particle detection is a non-contact detection method. There is no need to place detectors near the cracks, which greatly saves the detection construction workload and reduces the risk of safe operations. It meets the current needs of enterprises for efficient and safe production.

[0028] 2) The detection and data acquisition does not harm the concrete.

[0029] Traditional surface wave crack detection requires drilling and impact hammer excitation operations, which destroys the original concrete structure.

[0030] Quantum particle detection uses electromagnetic waves and quantum technology, which is completely harmless to concrete structures and does not cause any damage to concrete at all.

[0031] 3) There is a significant improvement in the depth of crack detection.

[0032] Traditional ultrasonic and surface wave detection can only detect cracks within 500mm, while particle detection can detect cracks up to 500m, which is sufficient to detect cracks in existing concrete structures, with a depth accuracy of centimeters.

[0033] 4) More precise crack width identification.

[0034] In terms of the detected crack width, it can identify micro cracks (lines) with a minimum width of 0.1, which fully meets the current requirements for hydraulic concrete crack detection.

[0035] 5) There is data response only for the detection target, and other interference factors such as steel bars and stress are not affected. The detection results are directly used without the elimination of noise reduction, anti-interference and other factors, making the detection more efficient.

[0036] 6) The method of scanning detection first and then detailed detection can save a lot of time for point arrangement and conversion, and improve detection efficiency.

[0037] 7) The multi-beam particle wave detection method is adopted to improve the sensitivity and accuracy of detection. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.

[0039] Figure 1 Flow chart of a method for detecting cracks in a concrete structure based on quantum measurement technology in an embodiment.

[0040] Figure 2a A schematic diagram of the vertical crack and the concrete particle beam range. Figure 2b This is another schematic diagram of the vertical crack and the concrete particle beam range. Figure 2c This is a schematic diagram of the boundary points of the fixed-point detection range. Figure 2d Schematic diagram of depth conversion of vertical cracks.

[0041] Figure 3a Schematic diagram of a crack that is not at a right angle to the plane. Figure 3b Schematic diagram of crack conversion for particle detection.

[0042] Figure 4 A schematic diagram of a vertical crack in the example.

[0043] Figure 5 Schematic diagram of a crack in an example that is not at a right angle to the plane. DETAILED DESCRIPTION

[0044] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only a part of the embodiments of the present invention, rather than all the embodiments. The components of the embodiments of the present invention generally described and shown in the drawings here can be arranged and designed in various different settings. Therefore, the following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the claimed invention, but merely represents the selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without making creative work belong to the scope of protection of the present invention.

[0045] See also Figure 1 In this embodiment, a method for detecting cracks in a concrete structure based on quantum measurement technology is proposed, comprising the following steps:

[0046] S10, on a plane of the concrete structure, based on the first direction of the plane, the particle host emits multiple beams of a certain intensity perpendicular to the plane ( ) is used to scan and detect from one side of the plane to the other side, receive electromagnetic particles representing physical quantities, and convert them into electrical signal data, determine whether the electrical signal data has changed, and record the first position of the detection point when the electrical signal data changes for the first time and the second position of the detection point when the electrical signal data changes for the last time.

[0047] Concrete particle beam refers to an electromagnetic particle beam with a quantum physical state of a concrete structure. During the entire detection process, the quantum physical state energy of the electromagnetic particle beam and the concrete structure, under the action of the particle physics field, continuously produce the same amount of particle interactions. When the same particles act, the returned particle physical state parameters are the same, and when different particles (such as microcracks) are present, the returned particle characteristics have certain differences in jumps and intervals. When there are cracks in the concrete structure, the concrete particle beam and the matter in the crack will undergo a series of quantum interactions such as quantum entanglement and superposition, which will cause the electromagnetic particle characterization physical quantities (magnetic rotation intensity angle, momentum, time difference) received by the particle host to change; conversely, if there are no cracks, the received electromagnetic particle characterization physical quantities will not change. Therefore, the spatial morphology of the crack can be determined by whether the received quantum physical field energy changes.

[0048] In this embodiment, multiple beams are emitted simultaneously when emitting concrete particle beams. This has the advantage of enhancing signal energy, making the changes in the physical quantities represented by the received electromagnetic particles more obvious, which is beneficial to improving the accuracy of crack identification. Figure 2aIn this embodiment, based on the particle host used, the multiple concrete particle beams are cylindrical with a diameter of 30 mm. Of course, the shapes and sizes of the multiple concrete particle beams can be designed in different ways.

[0049] like Figure 2a As shown, assuming that the center of the crack is at point O and the boundary of the crack is around point O, the electrical signal data will change when scanning around point O. When detecting outside points J and K (line segment JK is perpendicular to the crack direction), there is no crack and the emitted concrete particle beam hardly changes. When detecting between points J and K, the electrical signal data obtained by converting the physical quantity represented by the magnetic particles received by the particle host will change, and the process change from point J to point O will gradually increase because the crack area involved will gradually increase. At point O, the change in the electrical signal data reaches the maximum value (maximum energy loss), and the process change from point O to point K will gradually decrease because the crack area involved will gradually decrease.

[0050] Therefore, in the process of scanning and detecting from one side of the concrete structure plane to the other side, when the converted electrical signal data changes for the first time, it means that the crack area has just begun to be involved, and when it changes for the last time, it means that the crack area is about to be left. Therefore, the position of the detection point when the electrical signal data changes for the first time and the position of the detection point when it changes for the last time are recorded to facilitate the determination of the boundary point of the crack.

[0051] S20, based on the second direction of the plane perpendicular to the first direction, scan and detect from one side of the plane to the other side, receive electromagnetic particles representing physical quantities, and convert them to obtain electrical signal data, determine whether the electrical signal data has changed, and record the third position of the detection point when the electrical signal data changes for the first time and the fourth position of the detection point when the electrical signal data changes for the last time.

[0052] That is, the boundary area in the other direction of the crack is determined in the same manner as S10. Figure 3a As shown, S10 first scans and detects from left to right, and S20 scans and detects from front to back to determine the boundary of the crack.

[0053] S30, taking the range defined by the first position, the second position, the third position and the fourth position as the fixed-point detection range, setting a number of detection points within the fixed-point detection range, at each detection point the particle host emits a concrete particle beam perpendicular to the plane, records the received physical quantities representing the magnetic particles, and converts them into electrical signal data, and determines the size parameters of the cracks based on the electrical signal data of all detection points.

[0054] After steps S10 and S20 determine the boundary range, S30 performs fixed-point detection within the boundary range, and determines the three-dimensional spatial distribution of the cracks based on the data received during detection. The solution disclosed in CN202410025818.2 directly arranges a large number of grid lines in the plane, and calculates the crack width and depth based on the data detected at the grid points, that is, the data of each detection point must be calculated, while in the solution of this embodiment, the boundary range of the concrete crack is first scanned and detected, and only a number of detection points are arranged within the boundary range for fixed-point detection. The scanning and detection process does not require calculation, and only needs to compare whether the data received successively have changed. Therefore, compared with the method of first arranging a large number of grid points and then determining the range of the cracks at each measuring point, it saves time for large-area point arrangement, can quickly detect the crack morphology, and improves work efficiency.

[0055] like Figure 2a As shown, the reference numeral 10 represents a vertical crack, the reference numeral 20 represents the concrete particle beam range, and the two boundary points of the crack are between point J and point O, and between point O and point K. In fact, as long as the area explored by the concrete particle beam contains the crack, the converted electrical signal data will change. Figure 2a The figure shows an ideal state, which does not mean that the first time the converted electrical signal data changes, it is exactly at the position shown by point J, or the last time the converted electrical signal data changes, it is exactly at the position shown by point K. Therefore, more detailed detection is required to more accurately determine the boundary of the crack.

[0056] It is worth noting that if the scanning speed is too fast, making the detection point span larger, it may appear Figure 2b The situation shown is that when the electrical signal data obtained by conversion is detected at the previous position without any change, but when a change is detected at the next position, the detection area has covered more crack areas, which will not be conducive to accurately determining the boundary points of the cracks. Therefore, more preferably, after detecting the first position of the detection point when the first change occurs and the second position of the detection point when the last change occurs, the first position can be moved a certain distance away from the crack as the first boundary point of the fixed-point detection, and the second position can be moved a certain distance away from the crack as the second boundary point of the fixed-point detection, and the same applies to the third and fourth positions. That is to say, in step S30, if Figure 2c As shown, it is more preferred to use the ranges defined by S1-S, S2+S, S3-S, and S4+S as the fixed-point detection range, where S1, S2, S3, and S4 represent the first position, the second position, the third position, and the fourth position, respectively, and S represents the distance moved away from the crack. Figure 2a For example, S1-S represents a distance S moved to the left from the first position, and S2+S represents a distance S moved to the right from the second position.

[0057] According to the development direction of the cracks, the cracks can be subdivided into cracks that are not at right angles to the detection plane (or can be further refined to less than 85°) and vertical cracks. Cracks that are not at right angles to the detection plane are cracks that develop in the horizontal direction but are not at right angles to the plane, for example Figure 3a As shown in the figure, vertical cracks refer to cracks that are perpendicular to the horizontal reference plane when viewed from the outside surface. The angle between the crack and the vertical line does not exceed 5°. They are generally developed in the vertical direction downward from the reference plane. The cracks usually mentioned refer to cracks that are not at right angles to the detection plane. Vertical cracks are generally rare, but they exist objectively in the concrete structure of dams, for example.

[0058] It should be noted here that vertical cracks appear on the outer surface of the concrete structure, so by observing the surface of the concrete structure, it can be determined whether it is a vertical crack. However, vertical cracks will also develop and extend into the concrete structure, that is, the crack depth and length and width displayed on the surface of the concrete structure are not the actual size of the vertical crack, so accurate detection is still required to provide accurate data support for whether to repair the cracks and the repair standards.

[0059] In S30, the process of setting a plurality of detection points within the fixed-point detection range may be:

[0060] Arrange several horizontal detection lines and longitudinal detection lines within the fixed-point detection range, and then arrange several detection points along the horizontal detection lines and longitudinal detection lines respectively. The detection points on the horizontal detection lines and longitudinal detection lines can overlap or be independent of each other. When the detection points on the horizontal detection lines and longitudinal detection lines overlap, the intersection of the detection lines is a detection point. The detection points can also be arranged in a triangular point arrangement, a circular point arrangement, a fixed-point oblique measurement method, a conical point arrangement detection method, etc.

[0061] The spacing between the transverse detection lines is preferably equal, the spacing between the longitudinal detection lines is preferably equal, and the spacing between the detection points is also preferably equal.

[0062] Theoretically, whether it is a vertical crack or a crack that is not at a right angle to the detection plane, in order to obtain the three-dimensional shape of the crack, the three characteristic data of the length, width and height of the crack must be detected, and the detection method can be the same. However, the inventor found during the research process that the characteristic data calculation method of the crack that is not at a right angle to the detection plane is used to calculate the characteristic data of the vertical crack, and the error between the result and the actual size is relatively large. Therefore, different processing methods are used for the two types of cracks in this embodiment.

[0063] (a) For cracks that are not at right angles to the detection plane.

[0064] The electrical signal data of all detection points on a detection line can be used to obtain a cross-sectional fracture line. By combining the electrical signal data of all detection points on all grid lines, the three-dimensional morphological characteristics of the fracture can be obtained.

[0065] For reference Figure 3b In the figure, reference numeral 30 indicates a crack that is not at a right angle to the detection plane, and reference numeral 40 indicates a concrete structure. For the electrical signal data of a detection point, the time difference △t and depth of the crack can be obtained by the following method:

[0066] 1. The particle response time difference △t from the plane detection point A to the preset detection depth h0 (point D):

[0067]

[0068] t0: The particle response time when the emitted concrete particle beam travels from the plane detection point A to the point D at the preset detection depth h0 without cracks;

[0069] t1: The particle response time of the emitted concrete particle beam from the plane detection point A to the point D at the preset detection depth h0 when there is a crack;

[0070] 2. The crack depth is determined by:

[0071] The concrete particle beam is emitted vertically downward from the detection point A, and the detection depth is continuously changed for detection. It is judged whether the electrical signal data obtained by converting the received electromagnetic particle representation physical quantity has changed. The electromagnetic particle representation physical quantity received when the electrical signal data changes for the first time is the electromagnetic particle representation physical quantity received when detecting point B on the upper boundary surface of the crack; the detection depth is continued to be increased, and the electromagnetic particle representation physical quantity received when the electrical signal data changes for the last time is the electromagnetic particle representation physical quantity received when detecting point C on the lower boundary surface of the crack; the detection depth is further increased, and the electromagnetic particle representation physical quantity received when adjusted to the preset detection depth is the electromagnetic particle representation physical quantity received when detecting point D. Among them, there are obvious changes in the electrical signal data at the upper boundary point B and the lower boundary point C, which correspond to the depth h at the upper boundary surface of the crack. AB It is the depth of the upper boundary point B of the crack from the reference surface point A, corresponding to the depth h at the lower boundary surface of the crack AC It is the depth of the lower boundary point C of the crack from the reference surface point A; That is, the crack response depth value along the detection direction.

[0072] For Figure 3aThe cracks shown were detected using the method described in this embodiment and the method disclosed in CN202410025818.2, and the results are shown in Table 1 below. The results show that the method described in this embodiment can improve the detection efficiency.

[0073] Table 1: Test results of two methods

[0074]

[0075] (ii) For vertical cracks.

[0076] In S30, from the first position to the second position, it is determined whether the electrical signal data obtained by the conversion of each detection point has changed, and the fifth position of the detection point when the electrical signal data changes for the first time and the sixth position of the detection point when the electrical signal data changes for the last time are recorded. The width of the crack is calculated according to the following formula: , W represents the width of the crack, S EF represents the distance between the fifth position and the sixth position, which are the two boundary points of the vertical crack area, for example Figure 2a Points E and F are shown, and d represents the length of the concrete particle beam range, as shown in Figure 2a shown.

[0077] Similarly, for the length detection of the crack area, from the third position to the fourth position, determine whether the electrical signal data obtained by the conversion of each detection point has changed, record the seventh position of the detection point when the electrical signal data changes for the first time and the eighth position of the detection point when the electrical signal data changes for the last time, and convert the length of the crack according to the following formula: , L represents the width of the crack, S GH represents the distance between the seventh position and the eighth position, d represents the length of the concrete particle beam range, and when the concrete particle beam range is a circle, it is the diameter.

[0078] S EF It is calculated by:

[0079] , where t E ,t F They are respectively the direction from the first position to the second position, the time when the electrical signal data changes for the first time, and the time when it changes for the last time, and V is the horizontal moving speed of the particle host.

[0080] The crack width detection data of a certain crack depth in a certain case is shown in Table 2 below:

[0081] Table 2: Crack width test data for a certain crack depth

[0082]

[0083] E0 represents the initial value, E1 represents the measured energy value received by the instrument when encountering a crack. Indicates the change value, , , , n represents the number of particle beams, μ represents the ratio of the measured energy value to the initial value, t1~t 13 It represents the time corresponding to detection points 1 to 13, and h represents Planck's constant.

[0084] During the fixed-point detection process, determine the position where the electrical signal data changes the most, that is, Figure 2a At point O shown in the figure, the detection depth is gradually increased until the electrical signal intensity data obtained by converting the physical quantity represented by the electromagnetic particles responded by the quantum sensor no longer changes, and the electrical signal data and depth data at this time are recorded, such as Figure 2d As shown in the figure is the depth of the crack.

[0085] Based on the completion of the particle detection cases of concrete gate piers of hydropower stations and reservoir dams, a large amount of particle measurement data was obtained, and it was verified as an effective detection technology through actual measurement. For example: particle detection of cracks in the water diversion pier of a hydropower station, particle detection of concrete cracks in the gate pier of a hydropower station, and particle detection of cracks in the 23# concrete of a reservoir.

[0086] For details of some actual particle detection data, please see Tables 3 to 6 below.

[0087] Table 3: Partial detection data of the 1# dike support pier of a hydropower station

[0088]

[0089] Table 4: Partial data of the detection of the left pier of the No. 1 flood discharge gate of a hydropower station

[0090]

[0091] Table 5: Particle data of 23# crack detected on the top of a reservoir

[0092]

[0093] Table 6: Horizontal and vertical particle data of 23# crack at the bottom of a reservoir dam

[0094]

[0095] Based on mathematical modeling data processing, the three-dimensional morphological description of microcracks is completed through computer three-dimensional modeling, such as Figure 4 , Figure 5 As shown. Figure 4This is a V-V' section view of a crack in a reservoir dam. The scale is 1:1000. The dam top elevation is 1182.6m and the direction is 222°. In the figure, h1 represents the crack elevation, h2 represents the dam excavation surface, h3 represents the dam foundation surface, h4 represents the reservoir water level, the shaded part indicated by number 30 represents the crack range, and number 40 represents the concrete structure.

[0096] After using particle detection to detect cracks in the diversion gate pier of a hydropower station, drilling verification was carried out on the cracks in the gate pier. The actual drilling verification data showed that the extension length and depth data of the cracks (lines) detected by particle detection were basically consistent, with a consistency rate of 95%.

[0097] The following is an illustration of a real case.

[0098] Experimental purpose: To collect basic data on hydraulic concrete crack detection using particle detection technology at the Qingfengling Teaching Power Station, and obtain the compliance rate of particle detection technology in crack detection. At the same time, the magnetotelluric detector was used to detect cracks under the same conditions, and the detection effects of the two detection technologies were compared.

[0099] Introduction to the detection object: The detection target is the cement staircase next to the gravity dam of the Qingfengling Teaching Power Station. The cracks on the staircase are clearly visible, and the size of the staircase is 0.8×0.8m. The crack is narrow on the left, with a width of 2-3mm, and gradually increases to 7-8mm to the right. The overall occurrence of the crack is gentle, with an inclination of about 1-2°, and can reach 15° to the left. The left side of the crack is about 12cm away from the detection platform, and gradually transitions to 3cm. Through laser naked eye observation, the crack extends inward and almost penetrates the staircase platform.

[0100] The particle detection result data are shown in Table 7 below:

[0101] Table 7: Particle detection results data

[0102]

[0103] The detection results show that the particle host can detect cracks and has a fast response speed.

[0104] The instrument's crack depth data is concentrated between 0.5 and 0.7 m. Detection points 7 and 8 have the smallest signal response units of 7 to 8, and correspond to the narrowest crack at the actual position (upper left corner of the steps); while points 4 and 5 where the crack is wider correspond to the maximum instrument response unit of 23 to 25.

[0105] The collected particle crack detection data are analyzed and sorted indoors to ultimately form a three-dimensional image.

[0106] The detection effect of magnetotelluric detector on crack interface is poor, and it fails to effectively reflect the interface difference position caused by step cracks.

[0107] Conclusion: (1) The particle detector can detect cracks in hydraulic concrete. As long as there are cracks, the instrument will respond. (2) The minimum crack width that the instrument can currently detect is 0.1 mm, that is, the resolution of the device reaches 0.1 mm. (3) The width of the crack is positively correlated with the response unit of the instrument. That is, the wider the crack, the higher the response unit of the instrument, and the smaller the crack, the lower the response unit. (4) For a crack with a width of 0.1 mm, the instrument responds to 3 to 5 units.

[0108] The detailed principle of the particle host and particle detection is as follows:

[0109] First, the cold atom-quantum particle device is used in the laboratory to systematically obtain the quantum particle spectrum of the concrete structure; then, the multiple physical quantities that can be detected by the quantum state of the concrete crack (texture) standard block (crack width is 0.1-5.0mm) are obtained in the laboratory through the concrete structure quantum particle spectrum. The quantum state characterization physical quantity refers to the digital information electrical signal of the concrete structure that can be identified by the quantum particle host in the laboratory. Finally, the multiple physical quantities that characterize the quantum state of the crack (texture) of the concrete structure are converted into digital signals in the laboratory. During the on-site measurement, the digital signal is input into the reserve unit of the quantum particle host, and the host emits the concrete particle beam by exciting the emission unit.

[0110] The emitted concrete particle wave beam will generate quantum entanglement, superposition, collapse and other quantum physical field states with the structural concrete and its contact surface (undamaged and damaged areas). Specifically, the concrete quantum ground state wave function is obtained from the quantum particle map. Field energy wave function of concrete structure with external environment Mutual quantum interactions produce a series of quantum phenomena such as quantum superposition, entanglement, collapse, tunneling, and transition, forming the wave function after the interaction. .

[0111] On the contact surface of the concrete structure crack, a slight change in the quantum magnetic deflection angle and the reflection of part of the energy occurred, resulting in energy loss. The wave function equation after quantum action is: Among them, after the quantum action, the main change of the quantum wave function is the difference in magnetic rotation intensity and momentum difference On the contact surface of the concrete structure crack, the quantum Hall effect mainly occurs, and its principle is as follows:

[0112] Usually Ohm's law states that the steady-state current is proportional to the electric field on the substance. , in the presence of a magnetic field β, to be corrected, where δ is the conductivity of the material, in the absence of a magnetic field, isotropic medium, the current polar vector can be constructed using the vector ε axis, vector β:

[0113]

[0114] Note: Electromagnetic field, electric field and electric current all refer to the situation under quantum state conditions, in which a phenomenological constant related to magnetoresistance appears. The magnetic field introduces an effective anisotropy - the electric field, which induces electric charge in a vertical direction through Lorent work and the resulting bending of particle trajectories.

[0115] In the region of quantum particles with quantum state fields (0-10T), under such conditions, the quantum cyclotron frequency has an order of magnitude of energy.

[0116] The quantum Hall effect can be detected at the interface between two semiconductors such as GaAs and Ga1-xAs by inversion layer detection with high precision and low collision rate. ;

[0117] Wc is , magnetic deflection angle; τ is .

[0118] Quantum Hall conductance is the reciprocal of resistance, that is:

[0119]

[0120] In the formula:

[0121]

[0122] At integer values ​​of parameter V, the standard sample is observed, that is, the integer quantum Hall effect.

[0123] A further and more detailed explanation of the quantum principle is as follows:

[0124] On the concrete structure surface and its contact surface, the density change verifies the properties of the density matrix. For a pure state (no coupling with the environment, no damage), the density matrix is ​​equivalent to the wave function.

[0125] When the system is in a pure state Any state of the entire system can be expressed as a superposition of these basic states:

[0126]

[0127] The amplitude Ckiv can be time dependent and it will be normalized as follows:

[0128]

[0129] let is an arbitrary operator acting only on system variables, and its detection result is expressed as the expected value ( ) describes, in the environmental quality subnumber, The matrix elements of are diagonal:

[0130]

[0131] therefore, The expected value of takes the following form:

[0132]

[0133] Define the Hilbert space density matrix of the action detection subsystem , as the result of tracking and detecting spatial environment variables.

[0134]

[0135] Among them, the overline indicates that the detection space environment state is "averaged", and the matrix unit is the matrix of the above formula All expectations have been determined:

[0136]

[0137] tr refers only to the state trace of the system, according to the normalized formula:

[0138]

[0139] The density matrix is ​​normalized to:

[0140]

[0141] Operators The distribution function ω(α) for different values ​​of α is expressed as:

[0142]

[0143] When the system is in a mixed state and the variables are entangled with the detection space environment, the density matrix provides the probabilities of all detection results under incomplete information conditions.

[0144] The above description is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A method for detecting cracks in concrete structures based on quantum measurement technology, characterized in that: The following steps are involved: S10, on a plane of the concrete structure, based on the first direction of the plane, the particle host emits a concrete particle beam perpendicular to the plane, scans and detects from one side of the plane to the other side, receives electromagnetic particles to represent physical quantities, and converts them to obtain electrical signal data, determines whether the electrical signal data changes, and records the first position of the detection point when the electrical signal data changes for the first time and the second position of the detection point when the electrical signal data changes for the last time; S20, based on a second direction of the plane perpendicular to the first direction, scanning and detecting from one side of the plane to the other side, receiving electromagnetic particles representing physical quantities, and converting and obtaining electrical signal data, determining whether the electrical signal data has changed, and recording a third position of the detection point when the electrical signal data changes for the first time and a fourth position of the detection point when the electrical signal data changes for the last time; S30, taking the range defined by the first position, the second position, the third position and the fourth position as the fixed-point detection range, setting a number of detection points within the fixed-point detection range, at each detection point the particle host emits a concrete particle beam perpendicular to the plane, records the received electromagnetic particle representation physical quantity, and converts it to obtain electrical signal data, and determines the size parameters of the crack according to the electrical signal data of all detection points.

2. The method for detecting cracks in concrete structures based on quantum measurement technology according to claim 1 is characterized in that: The concrete particle beams emitted by the particle host are multiple concrete particle beams.

3. The method for detecting cracks in concrete structures based on quantum measurement technology according to claim 2 is characterized in that: The multiple concrete particle beams are cylindrical in shape.

4. The method for detecting cracks in concrete structures based on quantum measurement technology according to claim 1 is characterized in that: In S30, the ranges defined by S1-S, S2+S, S3-S, and S4+S are the fixed-point detection ranges, S1, S2, S3, and S4 represent the first position, the second position, the third position, and the fourth position, respectively, and S represents the distance moved in the direction away from the crack.

5. The method for detecting cracks in concrete structures based on quantum measurement technology according to claim 1 is characterized in that: In S30, the process of setting a plurality of detection points within the fixed-point detection range includes: arranging a plurality of transverse detection lines and longitudinal detection lines at equal intervals within the fixed-point detection range, and arranging a plurality of detection points at equal intervals along the transverse detection lines and longitudinal detection lines, respectively.

6. The method for detecting cracks in concrete structures based on quantum measurement technology according to claim 1 is characterized in that: If the crack is a crack that is at a non-right angle to the detection plane, then in S30, the process of obtaining the response depth of the crack based on the electrical signal data of one detection point includes: A concrete particle beam is emitted vertically downward from the detection point, and the detection depth is continuously increased for detection. It is determined whether the electrical signal data obtained by converting the physical quantity represented by the received electromagnetic particles has changed. The depth value corresponding to the first change in the electrical signal data and the depth value corresponding to the last change are recorded. The difference between the two depth values ​​is the response depth value of the crack.

7. The method for detecting cracks in concrete structures based on quantum measurement technology according to claim 1, characterized in that: If the crack is a vertical crack, then in S30, from the first position to the second position, it is determined whether the electrical signal data obtained by the conversion of each detection point has changed, and the fifth position and time of the detection point when the electrical signal data changes for the first time and the sixth position and time of the detection point when the electrical signal data changes for the last time are recorded, and the width of the crack is calculated according to the following formula: , W represents the width of the crack, S EF represents the distance between the fifth position and the sixth position, and d represents the length of the concrete particle beam range; From the third position to the fourth position, determine whether the electrical signal data obtained by the conversion of each detection point has changed, record the seventh position and time of the detection point when the electrical signal data changes for the first time, and the eighth position and time of the detection point when the electrical signal data changes for the last time, and calculate the length of the crack according to the following formula: , L represents the width of the crack, S GH Indicates the distance between the seventh position and the eighth position.

8. The method for detecting cracks in concrete structures based on quantum measurement technology according to claim 7 is characterized in that: S EF Calculated by the following formula: , t E ,t F They are respectively the direction from the first position to the second position, the time when the electrical signal data changes for the first time, and the time when it changes for the last time, and V is the horizontal moving speed of the particle host.

9. The method for detecting cracks in concrete structures based on quantum measurement technology according to claim 7, characterized in that: In S30, during the fixed-point detection process in the direction from the first position to the second position, the position at which the change in the electrical signal data is the largest is determined, and a concrete particle beam is emitted vertically downward at this position. The detection depth is gradually increased until the electrical signal data no longer changes. The electrical signal data and depth data at this time are recorded. The depth data is the response depth value of the crack.

Citation Information

Patent Citations

  • Inhomogeneity detection system

    CA1314072C

  • Method for detecting coal mining earth surface crack patterns

    CN104267449A

  • Method for acquiring ground crack morphology based on ground penetrating radar

    CN109696674A

  • Eddy current detection device based on superconducting quantum interferometer

    CN111351844A

  • Underground goaf detection method based on quantum detection technology

    CN116520451A

Cited By

  • Ground fracture detection method

    CN119667795A