Large-size PCB manufacturing method
By setting up positioning holes and rivet holes with pre-scaling shrinkage on large-sized PCBs and using semi-cured sheets to cure, the problem of inconsistency of core plates caused by shrinkage is solved, rivet alignment and leveling are achieved, and the conductivity of PCBs is improved and durability, reducing signal interference and noise.
Patent Information
- Application Number
- CN202410988835.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-07-23
AI Technical Summary
When manufacturing large-size PCBs, the expansion and shrinkage coefficients of core plates of different thicknesses or different copper thicknesses are inconsistent, resulting in the problem of not inserting the rivets during compression and rivets or the compression layer is biased.
By drilling positioning holes and rivet holes on the core plate, setting the pre-swell shrinkage amount to differentiate the design of the shrinkage coefficient, drilling the holes separately, and using semi-cured sheets to reinforce them during the pressing process to ensure hierarchical structure stability and signal transmission.
Effectively solve the problem of inconsistency in core plates caused by shrinkage in large-size PCB manufacturing, ensure rivet alignment and leveling, improve the conductivity and durability of the PCB, reduce signal interference and noise, and enhance the space and reliability between components. sex.
Smart Images

Figure CN119072010A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of PCB manufacturing, and in particular to a method for manufacturing a large-size PCB board. Background Art
[0002] Circuit board, also known as circuit board or printed circuit board, referred to as PCB (Printed Circuit Board), is one of the important components of the electronics industry. It is the support of electronic components and the carrier of electrical connection. The size of PCB depends on the processing size capacity of the equipment. Most equipment has a processing size capacity of 610*760mm, but clients often have large-size boards. However, conventional processes and practices cannot produce large-size boards. They are mainly limited by the capacity of OPE (punching rivet hole machine) and the capacity of hot melt machine in the pressing process. OPE (punching rivet hole machine) uses the center of the board as the origin and uses a coefficient of 1:1 to punch out rivet holes. Therefore, there will be no situation where core boards of different thicknesses cannot be inserted into rivets. The super capacity of OPE for large-size boards uses a drill to drill rivet holes. Due to the influence of expansion and contraction, the expansion and contraction coefficients of core boards of different thicknesses or different copper thicknesses are inconsistent, which leads to the failure to insert rivets or biased pressing layers during pressing and riveting. To this end, we propose a method for making large-size PCB boards. Summary of the invention
[0003] In order to solve the above problems, the present invention provides a method for manufacturing a large-size PCB board. The present invention can solve the problems of inconsistent expansion and contraction coefficients of core boards of different thicknesses or different copper thicknesses due to expansion and contraction when manufacturing large-size PCBs, and the problem that rivets cannot be inserted or the pressing layer is biased during pressing and riveting.
[0004] To achieve the above object, the technical solution adopted by the present invention is: A method for manufacturing a large-size PCB board, comprising: A plurality of positioning holes containing a first pre-expansion amount are drilled in the core plate, and the circuit pattern range is determined according to the positioning holes; Determine a rivet hole circuit pattern range that overlaps with the locating hole circuit pattern range according to the locating hole circuit pattern range, and drill a plurality of rivet holes with a second pre-expansion amount within the rivet hole circuit pattern range; The first pre-expansion and shrinkage amount is the sum of the etching expansion and shrinkage amount and the pressing expansion and shrinkage amount of the core board during the process from cutting to pressing, and the second pre-expansion and shrinkage amount is the etching expansion and shrinkage amount of the core board during the process from cutting to etching.
[0005] Taking the expansion and contraction factors into consideration, the expansion and contraction coefficients of the rivet holes and the graphics are designed differently and drilled separately to solve the problems of inconsistent expansion and contraction coefficients of core boards of different thicknesses or copper thicknesses caused by expansion and contraction when manufacturing large-size PCBs, and the problem of rivets not being able to be inserted or the pressing layer being biased during press-fit riveting.
[0006] Preferably, the etching expansion and contraction amount is expressed as: SK=(LS) / L; Among them, SK is the etching expansion and contraction, L is the theoretical distance between the two selected positioning holes, and S is the actual distance between the two selected positioning holes after etching; The expression of the compression expansion and contraction amount is: YH= (SD) / L; Among them, YH is the expansion and contraction amount of pressing, and D is the actual distance between the two positioning holes selected after pressing.
[0007] Taking the expansion and contraction factors into consideration, the expansion and contraction coefficients of the rivet holes and the graphics are designed differently, and the holes are drilled separately. By setting positioning holes and rivet holes with pre-expansion, the influence of the positioning holes and rivet holes during the pressing and etching process can be offset. This can solve the problem of inconsistent expansion and contraction coefficients of core boards of different thicknesses or different copper thicknesses due to expansion and contraction when manufacturing large-size PCBs, and the problem of rivets not being able to be inserted or the pressing layer being biased during pressing and riveting.
[0008] Preferably, after drilling a plurality of rivet holes with a second pre-expansion amount within the rivet hole line pattern, the method comprises: Obtain the drilled core boards, arrange the core boards in layer order, add prepregs between two adjacent core boards, and press the core boards and the prepregs into a core board with a sequential structure using a press.
[0009] When a multi-layer PCB is composed of different layers of sheets inside, the reinforcing sheet is used to clamp the layers and press them tightly together. This helps to ensure the flatness of the PCB and the stability of the overall structure. The PCB will generate heat during operation, and the reinforcing sheet can help improve the heat dissipation capacity of the PCB. By contacting the PCB, the reinforcing sheet can effectively absorb and disperse the heat on the circuit board to reduce the rise in component temperature, maintain the stability of the circuit, and enhance the heat dissipation effect of the PCB.
[0010] Preferably, after the core plate and PP are pressed into a core plate with a sequential structure by a press, the method further comprises: Drilling a via hole in the core plate, and cleaning the burrs on the positioning hole, the rivet hole and the via hole; After the burrs are removed, the via holes are copper plated.
[0011] The burrs on the hole may weaken the signal transmission strength, reduce the transmission distance, and even cause signal interference. Removing the burrs can ensure the stability and reliability of signal transmission; Copper has good corrosion resistance. Through copper plating technology, a dense copper film can be formed in the hole, which effectively protects the positioning holes and rivet holes from environmental erosion, helps prevent the positioning holes and rivet holes from being corroded by environmental factors such as humidity and corrosive gases, thereby enhancing the overall durability of the PCB.
[0012] Preferably, after removing the burrs, copper plating the positioning holes and rivet holes is performed, the method comprises: Depositing copper on the surface of the core board to obtain a core board covered with a copper layer; The surface of the copper layer is plated to obtain a circuit pattern, and the copper layer is etched to remove unnecessary copper foil.
[0013] Copper is an excellent conductive material. Copper plating can significantly increase the conductivity and current flow on the core board, thereby improving the performance and reliability of the circuit. Copper plating can enhance the corrosion resistance and mechanical strength of the core board, so that the circuit board can maintain stable and reliable performance under various environmental conditions.
[0014] Preferably, the process of performing plate making processing on the surface of the copper layer to obtain a circuit pattern, and etching the copper layer to remove unnecessary copper foil comprises: Performing solder resist treatment on the core board and performing gold plating treatment on the surface of the circuit pattern; Perform performance test and appearance inspection on the gold-plated core board.
[0015] Gold has excellent electrical conductivity. By plating gold on the PCB line pattern, the conductivity of the circuit board can be significantly improved. This not only helps to reduce line impedance, but also improves signal transmission efficiency, ensuring that electronic equipment maintains stability and reliability when running at high speed. The gold plating layer forms a protective film on the surface of the PCB, which has good corrosion resistance and oxidation resistance. It can prevent the circuit board from being corroded by environmental factors such as air, moisture, and chemicals, thereby extending the service life of the PCB.
[0016] Preferably, the performance test includes an insulation resistance test, a welding test and a signal test.
[0017] Through performance testing, the electrical performance, physical performance, reliability and other aspects of the PCB can be comprehensively evaluated to ensure that the PCB meets the design requirements and relevant standards, which helps to promptly discover and fix potential problems and improve the overall quality of the product.
[0018] Preferably, the diameters of the positioning holes and the rivet holes are 2 mm.
[0019] When the diameter of the positioning hole is 2mm, precise alignment can be achieved, so that the core board can fit accurately, and the electrical performance and reliability of the circuit board can be improved. If the rivet diameter is too large, it will be difficult to form the upsetting head, and the sheet material will be easily deformed; if the diameter is too small, the rivet strength will be insufficient. The selection of the rivet diameter depends on the aperture of the riveted part. Generally, the aperture is 1-2mm. If it is larger than 2mm, it may be loose. However, within a reasonable range, positioning holes and rivet holes of different diameters can be used as alternatives for this application.
[0020] Preferably, before drilling a plurality of positioning holes containing the first pre-expansion amount in the core plate, the method further comprises: Cut the large-sized substrate into several core boards of the same size.
[0021] Preferably, the length of the core plate is between 760 mm and 1245 mm.
[0022] When the size is between 760mm-1245mm, it is a large-size PCB board, and PCB boards of different sizes obtained through this application can be used as alternatives to this application.
[0023] Large PCB board size allows designers to separate circuit components and wiring space farther apart, helping to reduce signal interference and noise. This layout is especially important for applications that require high-precision or high-speed signals, as it can significantly improve the accuracy and stability of signal transmission.
[0024] Larger PCBs allow for more space between components, making the assembly process easier. Larger PCBs mean faults are easier to identify and locate, reducing repair costs and downtime.
[0025] The beneficial effects of the present invention are: The present invention drills a positioning hole with a first pre-expansion amount at the edge of the core board, determines the circuit pattern position range according to the positioning hole, determines the rivet hole circuit pattern position range that overlaps with the circuit pattern position range determined by the positioning hole, and drills a plurality of rivet holes with a second pre-expansion amount within the rivet hole circuit pattern range. The present application takes into account the expansion and contraction factors, and differentiates the expansion and contraction coefficients of the rivet holes and the graphics, and drills the holes separately. The first pre-expansion and contraction amount is the sum of the etching expansion and contraction amount and the pressing expansion and contraction amount of the core board during the process from cutting to etching, and the second pre-expansion and contraction amount is the etching expansion and contraction change amount of the core board during the process from cutting to etching. The present invention can solve the problem of inconsistent expansion and contraction coefficients of core boards of different thicknesses or different copper thicknesses due to expansion and contraction when manufacturing large-size PCBs, and the problem of rivets not being able to be inserted or the pressing layer being biased during pressing and riveting. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1This is a flow chart of a method for manufacturing a large-size PCB board in a specific implementation of the present invention; Figure 2 It is a design drawing for making a large-size PCB board in the specific implementation of the present invention; Figure 3 It is a conventional production design drawing for a large-size PCB board with inconsistent core board thickness / copper thickness in a specific implementation of the present invention; Figure 4 It is a conventional production design drawing for a large-size PCB board with consistent core board thickness and copper thickness in a specific implementation of the present invention; Figure 5 It is a position distribution diagram of the positioning holes and rivet holes in a specific embodiment of the present invention.
[0027] Figure symbols: 1. Positioning hole; 2. Rivet hole. DETAILED DESCRIPTION
[0028] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0029] See also Figure 1-Figure 5 As shown, the present invention relates to a method for manufacturing a large-size PCB board.
[0030] Example 1
[0031] refer to Figure 1 As shown, a method for manufacturing a large-size PCB board includes: Cut the large-sized substrate into several core boards that meet the size of the PCB board, and the size of the core board is between 760mm and 1245mm; A plurality of positioning holes 1 containing a first pre-expansion amount are drilled in the core plate, and the position range of the circuit pattern is determined according to the positioning holes 1; According to the line pattern position range of the positioning hole 1, a line pattern range of the rivet hole 2 that overlaps with the line pattern position range of the positioning hole 1 is determined, and according to the line pattern position range of the rivet hole 2, a plurality of rivet holes 2 with a second pre-expansion amount are drilled in the core plate; The present application can solve the problem that the expansion and contraction coefficients of core boards of different thicknesses or different copper thicknesses are inconsistent due to expansion and contraction, thereby causing the rivet to fail to be inserted or the pressing layer to be biased during press-fit riveting, by aligning the circuit graphic position range of the positioning hole 1 and the rivet hole 2.
[0032] The first pre-expansion amount is the sum of the etching expansion and contraction amount and the pressing expansion and contraction amount of the core board during the process from cutting to etching, and the second pre-expansion amount is the etching expansion and contraction change amount of the core board during the process from cutting to etching.
[0033] The expression of etching expansion and contraction is: SK=(LS) / L; Wherein, SK is the etching expansion and contraction, L is the theoretical distance between the two positioning holes 1, and S is the actual distance between the two positioning holes 1 after etching; The expression of the compression expansion and contraction amount is: YH= (SD) / L; Wherein, YH is the expansion and contraction amount of pressing, and D is the actual distance between the two positioning holes 1 after pressing.
[0034] For example, for TU865 material, the expansion and shrinkage change SK after etching is 0.05%, and the expansion and shrinkage change YH after pressing is 0.07%. Therefore, the first pre-expansion and shrinkage of the positioning hole is 0.05+0.07=0.12%, and the second pre-expansion and shrinkage of the rivet hole is 0.05%. Therefore, the pre-expansion and shrinkage coefficient of the positioning hole is 1.0012, and the pre-expansion and shrinkage coefficient of the rivet hole is 1.0005.
[0035] In actual operation, there can be multiple positioning holes 1 on the core plate. In theory, any two positioning holes 1 can be selected, as long as the two positioning holes 1 measured before and after are the same.
[0036] refer to Figure 5 As shown, in this embodiment, the number of positioning holes is 4 and they are symmetrically arranged at the four corners of the PCB board. This method can form a multi-point surface positioning method, and this layout makes the positioning more accurate. Because the four corners are used as fixed points, the position of the PCB can be ensured to be stable during processing, testing and assembly, reducing offset and error.
[0037] In the selection of theoretical distance, only positioning hole 1 can be selected, and rivet hole 2 cannot be selected, because the expansion and contraction of rivet hole 2 are different. During pressing, the rivet on rivet hole 2 will not change with the expansion and contraction of the core board after being fixed. That is, rivet hole 2 only has etching expansion and contraction, and there is no pressing expansion and contraction. Positioning hole 1 will expand and contract during etching and during pressing. During etching, the expansion and contraction of positioning hole 1 and rivet hole 2 remain consistent.
[0038] In this embodiment, the size of the PCB board generated by this method is generally 1000mm, which is a large-size PCB board. Compared with the traditional small-size 760mm PCB board, the PCB board of this application can carry more electronic components and complex circuit layouts, thereby achieving higher integration.
[0039] 1000mm PCB boards allow designers to separate circuit components and wiring space further apart, helping to reduce signal interference and noise. This layout is especially important for applications that require high-precision or high-speed signals because it can significantly improve the accuracy and stability of signal transmission.
[0040] The 1000mm size PCB board allows for more space between components, making the assembly process easier. Larger PCBs mean it is easier to identify and locate faults, thereby reducing repair costs and downtime.
[0041] refer to Figure 2-Figure 3 As shown, compared with the traditional technology, this method takes the expansion and contraction factors into consideration. In view of the inconsistent thickness of the core board, the expansion and contraction coefficients of the rivet hole 2 and the graphics are designed differently and drilled separately.
[0042] The traditional approach to the situation where the core board thickness or copper thickness is inconsistent does not take into account the expansion and contraction coefficient of the rivet hole 2 and the expansion and contraction coefficient of the pattern. The expansion and contraction of the positioning hole 1 and the rivet hole 2 are consistent. After etching, the rivet hole 2 becomes misaligned. The misalignment of the rivet hole 2 makes it difficult to insert the rivet during press-fit riveting. All core boards change in different amounts, resulting in layer deviation after pressing.
[0043] This solution takes the expansion and contraction factors into consideration. In the case of inconsistent core board thickness, a rivet hole 2 with a second pre-expansion amount is provided. The second pre-expansion amount is provided to offset the actual expansion and contraction of the rivet hole 2 after the core board is etched, so that the rivet hole 2 will not be misaligned. The positioning hole 1 with the first pre-expansion amount is provided to offset the actual expansion and contraction of the core board pattern after pressing, so that the pressing layer will not be biased. The positioning hole 1 with the first pre-expansion amount and the rivet hole 2 with the second pre-expansion amount are provided to prevent the core board from being unable to be inserted into the rivet or the pressing layer from being biased during pressing and riveting.
[0044] refer to Figure 4 As shown, for the case where the thickness of the core board is consistent, the conventional method is: when drilling the core board, the positioning hole 1 and the rivet hole 2 expand and contract at the same time as the core board belt. After the core board has undergone the pressing and etching processes, the expansion and contraction changes of all core boards are consistent, and the rivet hole 2 is aligned, so there will be no problem of rivets not being able to be inserted during riveting or layer deviation during pressing.
[0045] In the traditional method, the expansion and contraction of the positioning hole 1 and the rivet hole 2 are consistent, but in the present application, the pre-expansion and contraction of the positioning hole 1 is the sum of the etching expansion and contraction of the core board from cutting to etching and the pressing expansion and contraction, so that the expansion and contraction of all core board patterns after pressing is 1:1, and the pre-expansion and contraction of the rivet hole 2 is the etching expansion and contraction change of the core board from cutting to etching, so that the expansion and contraction of the rivet hole 2 after etching is 1:1, Figure 2The different expansion and contraction after etching refers to the different expansion and contraction of the core board pattern. The expansion and contraction of the core board pattern after pressing is 1:1. After etching, the expansion and contraction of the rivet hole 2 is 1:1.
[0046] The size range of this method is that the long dimension of PNL is 1000mm, while the existing dimensions are mostly around 610*760mm. This method can solve the problem of inconsistent expansion and contraction coefficients of core boards of different thicknesses or different copper thicknesses due to expansion and contraction when manufacturing large-size PCBs, and the problem of rivets not being able to be inserted or the pressing layer being biased during press-fitting and riveting.
[0047] The diameter of the positioning hole 1 and the rivet hole 2 of the present application is 2mm. The selection of the rivet diameter is mainly determined by the thickness of the plate and the riveting form. If the rivet diameter is too large, it is difficult to form the head and the plate is easily deformed; if the diameter is too small, the rivet strength is insufficient. The selection of the rivet diameter depends on the hole diameter of the riveted part. Generally, the hole diameter is 1-2mm. If it is larger than 2mm, it may be loose.
[0048] Obtain the standard core board with the holes drilled, arrange the standard core boards in order of layers, add prepreg PP between two adjacent core boards, the prepreg PP plays a key bonding role in the production of multilayer boards, and the treated fiberglass cloth is impregnated with resin glue, and then heat-treated (pre-baked) to make the resin enter the B stage to make a sheet material. This material will soften under heating and pressure, fill the blank area between layers, and then cool and react to solidify, thereby tightly bonding the layers in the multilayer board together.
[0049] The stacked PCB boards are placed in a heat press or similar equipment, heated to a high specific temperature, wherein the heating temperature is determined according to the PCB material and design requirements, and high pressure is applied through a hydraulic system, wherein the pressure is determined according to the PCB material and design requirements. The high temperature and high pressure melt the adhesive between the conductive layer and the insulating layer and firmly connect them together. The core board and PP are pressed into a core board with a sequential structure through a press. After the heating and pressurization are completed, the PCB board is taken out of the heat press and solidified during the cooling process, which makes the adhesive harden again and ensures the structural stability of the PCB board.
[0050] Preferably, the gel time is usually 180 seconds, which indicates the curing speed of the prepreg PP under specific conditions.
[0051] The glue content is generally 50%, which indicates the resin content in the semi-cured sheet PP, affecting its bonding and insulation properties.
[0052] The fluidity is usually 24%, which indicates the fluidity of the prepreg PP under heating and pressure, affecting its ability to fill the blank areas between layers.
[0053] In some other embodiments, within a reasonable range, the gelation time, gel content and fluidity may include any values, which may serve as alternatives of the present application.
[0054] Place the prepared PCB board on the drilling machine to ensure that the board surface is flat and free of impurities. According to the requirements of the drilling file, select the appropriate drill bit and install it on the drilling machine. Adjust the parameters of the drilling machine, such as speed, feed speed, etc., to adapt to PCB boards of different materials and thicknesses.
[0055] Start the drilling machine and automatically or manually control the drill to drill holes on the PCB board according to the requirements of the drilling file. During the drilling process, it is necessary to ensure that the parameters such as the position, depth and angle of the drill are accurate to avoid damage to the PCB board or affect subsequent processes.
[0056] Drilling holes in the core plate and removing burrs from the holes; After the burrs are removed, copper is plated inside the hole, and the hole wall of the drilled hole is metalized by chemical copper deposition or electroplating, so that the pins of the electronic components are connected to the internal circuits.
[0057] After copper plating in the hole, the PCB and copper foil need to be placed in an electrolytic cell. Current is injected into the electrolytic cell through a power supply to cause copper ions to undergo an oxidation-reduction reaction in the electrolyte and deposit the copper layer on the surface of the substrate. Before copper plating on the PCB, degreasing is required: the purpose of this step is to remove oil stains, fingerprints, oxides on the board surface and dust in the holes. Alkaline degreasing can adjust the charge of the hole wall from negative to positive, thereby facilitating the adsorption of colloidal palladium in subsequent processes. The second is micro-etching: this step is used to further remove oxides on the board surface and roughen the board surface to ensure good bonding between the subsequent copper plating layer and the base copper of the substrate. Circuit production is performed on the substrate after copper plating. Circuit production includes the following steps: 1. Graphic Design and Preparation Circuit design: Based on product requirements and functional specifications, use circuit design software (such as Cadence, AltiumDesigner, etc.) to perform circuit design, including layout and routing.
[0058] Graphic output: Convert the designed circuit graphics into the format required for production, usually Gerber file or other CAD data format.
[0059] 2. Graphic transfer to the board Film method: Prepare dry film: Select dry film suitable for the board and circuit design to ensure its adhesion and etching resistance.
[0060] Film sticking: Use a film sticking machine or manually to evenly stick the dry film on the copper surface of the board.
[0061] Exposure: Place the board with the film on it in an exposure machine and irradiate it with ultraviolet light to cause a chemical reaction in the photosensitive material in the circuit pattern.
[0062] Development: The unexposed part of the dry film is removed by the developer to expose the copper surface to be etched.
[0063] Inkjet printing method: Prepare inkjet printer: Use a specialized inkjet printer and conductive ink.
[0064] Printing: Print the circuit graphics directly onto the copper surface of the board, and the conductive material in the ink will form the circuit pattern.
[0065] Curing: Curing the ink by heating or UV light to enhance adhesion and conductivity.
[0066] 3. Etching and film removal Etching: Prepare etching solution: Select suitable etching solution to ensure its etching rate and uniformity on copper.
[0067] Etching process: Place the plate with film or printed pattern into the etching machine, and the etching liquid will etch away the unprotected copper layer to form a circuit pattern.
[0068] Post-etching cleaning: After etching is completed, use a cleaning agent and water to thoroughly clean the etching solution and residues on the surface of the board.
[0069] To remove the membrane: For boards made using the dry film method, the remaining dry film needs to be removed after etching. This is usually done using a stripping solution or mechanical stripping.
[0070] For inkjet printing, this step can be skipped if the ink has already cured and no further processing is required.
[0071] 4. Subsequent processing and inspection Tin stripping: If a tin layer is used for protection during the circuit production process, a tin stripping liquid is needed to remove the excess tin layer.
[0072] Circuit inspection: Use a magnifying glass or microscope to carefully inspect the etched circuit to ensure that the circuit is complete and there is no break or short circuit.
[0073] Cleaning and Drying: Give the panels a final clean to ensure that there is no residue on the surface, then dry them for subsequent processing.
[0074] Solder mask processing flow: Prepare solder mask ink: According to the design requirements, select the appropriate solder mask ink. This ink has specific adhesion and etching resistance, which can protect the parts of the circuit board that do not need to be soldered.
[0075] Apply solder mask ink: Use special coating equipment or manual method to evenly apply solder mask ink on the surface of the circuit board. This process must ensure that the ink layer thickness is uniform and free of bubbles and impurities.
[0076] Pre-baking: Pre-bake the applied solder mask ink to dry and solidify it by heating. The pre-baking temperature and time need to be adjusted according to the characteristics of the ink and the requirements of the circuit board.
[0077] Exposure: Use an exposure machine to expose the pre-baked circuit board. During the exposure process, the ink of the part that needs to be welded is cured by precisely controlling the light source and exposure time, while the part that does not need to be welded remains uncured.
[0078] Development: The exposed circuit board is placed in a developer to remove the uncured solder mask ink through a chemical reaction, exposing the metal part to be soldered. The development process requires strict control of time and temperature to avoid damage to the circuit board.
[0079] Post-processing: The developed circuit board is cleaned and dried to remove residual developer and impurities. Then a quality inspection is carried out to ensure the integrity and accuracy of the solder mask layer.
[0080] Gold plating process: Surface cleaning and preparation: Before starting gold plating, the surface of the circuit board needs to be thoroughly cleaned to remove oil, oxides and other impurities. This can be achieved by using a cleaning agent or acid or alkaline cleaning.
[0081] Activation treatment: Use an activator to treat the surface of the circuit board to increase the adsorption capacity of metal ions. This helps the adhesion and uniformity of the gold layer in the subsequent gold plating process.
[0082] Gold plating: Place the processed circuit board into the gold plating solution, and use electrochemical methods to reduce the gold ions to a gold layer on the metal surface of the circuit board. This process requires the control of parameters such as current, voltage and time to ensure that the thickness and quality of the gold layer meet the requirements.
[0083] Post-processing and cleaning: After the gold plating is completed, the circuit board needs to be post-processed, such as cleaning and drying. This helps to remove residual gold plating liquid and other impurities, while ensuring the stability and corrosion resistance of the gold layer.
[0084] Example 2
[0085] Preferably, at least two positioning holes 1 are set at the diagonal of the core board, which helps to ensure the standardization and uniformity of the PCB board design. For different boards of the same product, if the PCB dimensions are the same, the positions of the positioning holes 1 must also be unified, which helps to improve production efficiency and product quality.
[0086] In some other embodiments, the number and location of the positioning holes should be determined according to the actual requirements of the PCB. For example, for a PCB that requires high-precision processing, the number of positioning holes may need to be increased to improve stability, while for cost-sensitive application scenarios, the number of positioning holes needs to be controlled as much as possible while ensuring accuracy.
[0087] refer to Figure 5 As shown, in this embodiment, the large-sized substrate is cut into a plurality of core boards that meet the size of the PCB board, and the size is between 760mm-1245mm; The positioning holes 1 are arranged at the four corners of the core board. Positioning holes 1 with a first expansion and contraction amount are drilled at the four corners of the core board. The circuit pattern position range is determined by the positioning holes 1. The circuit pattern position range determined by the positioning holes 1 is used as the circuit pattern position range of the rivet holes 2 to expand and set the rivet holes 2. Rivet holes 2 with a second expansion and contraction amount are provided along the board edge where the positioning holes 1 are located. The rivet holes 2 and the positioning holes 1 are symmetrically arranged on both sides of the center point of the positioning holes 1.
[0088] When the positioning holes 1 are set at the four corners or diagonals of the core board, that is, the distance is far, multi-point surface positioning can be formed, thereby improving the positioning accuracy. This ensures that the patch, soldering, reflow soldering, solder paste printing and other processes in the production process can be accurately operated and reduce errors. The farther the positioning holes 1 are, the less signal interference between different circuit parts. In the design of high-frequency and high-speed circuits, maintaining a sufficient distance can reduce cross interference between signals and improve signal quality.
[0089] Example 3
[0090] After the PCB is prepared based on the above embodiment 1, it is necessary to perform a performance test on the prepared PCB. Preparation before the test: Before starting the test, the test environment needs to be prepared first to ensure that the test environment meets the test requirements, such as temperature, humidity, electrostatic protection, etc. At the same time, prepare the equipment and tools required for the test, such as an oscilloscope, a signal generator, a multi-function tester, etc., and calibrate them to ensure the accuracy of the test.
[0091] Understanding of product requirements and specifications: Carefully study the design documents and specifications of the PCB to understand the specific requirements and specifications of the product, including electrical performance, size, shape, material, etc. This will help determine the focus and methods of testing, as well as set appropriate test parameters.
[0092] Appearance inspection: Carefully inspect the appearance of the PCB to see if there are any obvious damage, stains or defects. This includes checking whether the solder mask is intact, without bubbles or cracks, and whether the gold plating is uniform and not falling off.
[0093] The performance testing courses include: Electrical performance test: Use multi-function testers, oscilloscopes and other equipment to test the electrical performance of the PCB. The test content may include conductivity, insulation, resistance, capacitance, inductance and other parameters to ensure that the electrical performance of the circuit board meets the design requirements. The specific values of the parameters depend on the PCB material and design requirements.
[0094] Functional testing: According to the specific functions and requirements of the product, design corresponding test plans to verify the functions of the PCB. This can be achieved by simulating actual working conditions, applying signals or voltages to the circuit board, and observing its output or response.
[0095] Reliability test: Conduct reliability test on PCB to evaluate its stability and durability in various harsh environments. The test contents may include temperature cycle test, humidity test, vibration test, etc. to simulate various situations that the product may encounter in actual use. The specific values of the test parameters are determined according to the PCB material and design requirements. After the test, the finished PCB of the size required by the customer is produced according to the customer's requirements.
[0096] Example 4
[0097] The size of the PCB produced in this application is between 760mm-1245mm, mostly 1000mm. The size of the PCB board produced by this solution is the optimal result of this method, but it is not the only result. PCB boards of different sizes produced by this method can be used as alternatives to this solution. However, it is worth noting that although large-size PCBs allow designers to separate circuit components and wiring spaces further apart, which helps reduce signal interference and noise, in some cases, if the line is too long, the impedance will increase accordingly, thereby weakening the anti-noise ability.
[0098] Large-size PCBs may reduce total cost by reducing the amount of area required to pay for, but the unit cost may be higher, and longer lines may lead to higher material costs.
[0099] When the PCB size is too small, due to space limitations, the components are arranged too closely, which may cause signal interference and increased noise, affecting signal quality.
[0100] Too small a PCB size may make the assembly process difficult, and fault identification and location may also become more complicated, increasing repair costs and downtime. Due to the small PCB size and short distance between components, poor heat dissipation may occur, thus affecting device performance.
[0101] Example 5
[0102] In summary, the design principle of this scheme can be obtained: Cutting: Cut the large-sized substrate into small-sized core boards that meet the PNL size of the PCB board; Drilling positioning hole 1: using pre-expansion on the core board, drill positioning hole 1 with the first expansion amount on the edge of the board (the expansion amount is given by the pressing engineer based on the material, board thickness, and copper thickness), and determine the position range of the positioning hole 1 circuit pattern according to the positioning hole 1; Drilling rivet holes 2: determining a rivet hole 2 circuit pattern position range that overlaps with the locating hole 1 circuit pattern position range according to the locating hole 1 circuit pattern position range, and drilling a plurality of rivet holes 2 with a second pre-expansion amount in the core board according to the rivet hole 2 circuit pattern position range; Lamination: Arrange the laminates in order of layers, and add prepreg PP between each core board according to the customer's dielectric thickness requirements. The prepreg is completely cured by a press at high temperature and high pressure, so that all layers of core boards are pressed into a semi-finished PCB with a sequential structure.
[0103] Drilling: Drill holes on the PCB board that need to conduct the inner layer circuits, and deal with the burrs on the hole openings; Copper deposition: Copper is deposited on the PCB surface and in the holes using chemical methods to create a conductive effect.
[0104] Electroplating: Based on copper deposition, the hole copper and surface copper are electroplated to thicken them so that the surface copper and hole copper meet customer needs.
[0105] Solder mask: Print a layer of ink on the PCB surface to protect it; Text: Print the text and logo required by the customer on the outer layer of the PCB; Immersion Gold: A thin layer of gold is plated on the circuit pattern to protect the circuit; Testing: Perform performance testing and visual inspection on PCB to ensure product quality; Molding: produce PCB finished graphics of the size required by customers.
[0106] In summary, this solution takes expansion and contraction factors into consideration. In the case of inconsistent core board thickness, a rivet hole 2 with a second pre-expansion amount is provided. The second pre-expansion amount is provided to offset the actual expansion and contraction of the rivet hole 2 after the core board is etched, so that the rivet hole 2 will not have the problem of misalignment. The positioning hole 1 with the first pre-expansion amount is provided to offset the actual expansion and contraction of the core board pattern after pressing, so that the pressing layer will not be biased. By providing the positioning hole 1 with the first pre-expansion amount and the rivet hole 2 with the second pre-expansion amount, the problem of using a drill to drill the rivet hole 2 in the preparation process of large-size boards is solved. Due to the influence of expansion and contraction, the expansion and contraction coefficients of core boards of different thicknesses or different copper thicknesses are inconsistent, which leads to the problem that the rivet cannot be inserted or the pressing layer is biased during pressing and riveting.
[0107] The above implementation modes are merely descriptions of the preferred implementation modes of the present invention, and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary engineering and technical personnel in the field shall fall within the protection scope determined by the claims of the present invention.
Claims
1. A method for manufacturing a large-size PCB board, characterized in that: include: A plurality of positioning holes containing a first pre-expansion amount are drilled in the core plate, and the circuit pattern range is determined according to the positioning holes; Determine a rivet hole circuit pattern range that overlaps with the locating hole circuit pattern range according to the locating hole circuit pattern range, and drill a plurality of rivet holes with a second pre-expansion amount within the rivet hole circuit pattern range; The first pre-expansion and shrinkage amount is the sum of the etching expansion and shrinkage amount and the pressing expansion and shrinkage amount of the core board during the process from cutting to pressing, and the second pre-expansion and shrinkage amount is the etching expansion and shrinkage amount of the core board during the process from cutting to etching.
2. The method for manufacturing a large-size PCB board according to claim 1, characterized in that: The expression of etching expansion and contraction is: SK=(LS) / L; Among them, SK is the etching expansion and contraction, L is the theoretical distance between the two selected positioning holes, and S is the actual distance between the two selected positioning holes after etching; The expression of the compression expansion and contraction amount is: YH= (SD) / L; Among them, YH is the expansion and contraction amount of pressing, and D is the actual distance between the two positioning holes selected after pressing.
3. The method for manufacturing a large-size PCB board according to claim 1, characterized in that: After a plurality of rivet holes with a second pre-expansion amount are drilled within the rivet hole line pattern, the method comprises: Obtain the drilled core boards, arrange the core boards in layer order, add prepregs between two adjacent core boards, and press the core boards and the prepregs into a core board with a sequential structure using a press.
4. The method for manufacturing a large-size PCB board according to claim 1, characterized in that: After the core plate and PP are pressed into a core plate with a sequential structure by a press, the method comprises: Drilling a via hole in the core plate, and cleaning the burrs on the positioning hole, the rivet hole and the via hole; After the burrs are removed, the via holes are copper plated.
5. The method for manufacturing a large-size PCB board according to claim 4, characterized in that: After the burrs are removed and the positioning holes and rivet holes are copper plated, the method comprises: Depositing copper on the surface of the core board to obtain a core board covered with a copper layer; The surface of the copper layer is subjected to circuit production to obtain a circuit pattern, and the copper layer is etched to remove unnecessary copper foil.
6. The method for manufacturing a large-size PCB board according to claim 5, characterized in that: The circuit pattern is obtained by making a circuit on the surface of the copper layer, and the copper layer is etched to remove unnecessary copper foil, which includes: Performing solder resist treatment on the core board and performing gold plating treatment on the surface of the circuit pattern; Perform performance test and appearance inspection on the gold-plated core board.
7. The method for manufacturing a large-size PCB board according to claim 6, characterized in that: The performance test includes an insulation resistance test, a welding test and a signal test.
8. The method for manufacturing a large-size PCB board according to claim 1, characterized in that: The diameter of the positioning hole and the rivet hole is 2 mm.
9. The method for manufacturing a large-size PCB board according to claim 1, characterized in that: Before the core plate is drilled with a plurality of positioning holes containing the first pre-expansion amount, the method further comprises: Cut the large-sized base board into several core boards of the same size.
10. The method for manufacturing a large-size PCB board according to claim 9, characterized in that: The length of the core plate is between 760 mm and 1245 mm.
Citation Information
Patent Citations
PCB processing method capable of avoiding layer deviation after lamination
CN110536569A
HDI plate manufacturing method for improving matching precision of through holes and blind holes, and HDI plate
CN113923895A
PCB processing method, PCB and PCB drilling method
CN114554698A
Layer deviation control method for multilayer circuit board
CN117279245A
Etching method before lamination of PCB (printed circuit board) manufacturing
CN117528948A
Cited By
Circuit board pressing method, pressing device and circuit board manufacturing system
CN121218448A