Microchannel device

By designing the overlapping structure of the working electrode and the ion selective component on the porous substrate and the independent arrangement of the reference electrode, the problem of insufficient bubbles and sample penetration between the paper substrate electrode and the ion selective film is solved, and high stability is achieved and high-precision microfluidic path measurement.

CN119072627APending Publication Date: 2024-12-03CANON KK
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380035920.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-28
Filing Date
2023-04-10
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

In the prior art, bubble formation between the paper substrate electrode and the ion-selective film causes unstable measurements, and the sample cannot fully penetrate into the membrane area, affecting the measurement accuracy.

Method used

Design a microfluidic path device, using a porous substrate as the flow path area, the working electrode and the ion selective component overlap on the plane X-side surface of the porous substrate, and the reference electrode is arranged in the area B except area A , formed in the same porous substrate, ensuring a sufficient contact area between the ion selective film and the sample.

Benefits of technology

A small microfluidic device with high measurement stability is achieved, which avoids the problems of bubble adhesion and insufficient sample penetration and improves the measurement accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119072627A_ABST
    Figure CN119072627A_ABST
Patent Text Reader

Abstract

Provided is a thin microfluidic device capable of stable measurement. Provided is a microfluidic device using a porous substrate, the microfluidic device having a flow path region utilizing porosity, and having a region A in a part of the flow path region, in which a component having ion selectivity is present in pores of the porous substrate. In the region A, a component having ion selectivity is present in pores on one plane X side of the porous substrate, and the other plane Y side is a flow path having voids. The working electrode is provided on the plane X-side surface of the region A such that at least a portion of the working electrode overlaps the component having ion selectivity. The reference electrode is provided in a region B other than the region A of the flow path region. The region A and the region B are formed on the same porous substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a micro-channel device in which electrodes are formed by a channel using a porous substrate. Background Art

[0002] In recent years, the research and development of microfluidic devices that allow biochemical analysis to be performed efficiently (micro, fast, and simply) in a single chip by using microfluidic channels with micro sizes has become a focus of attention in a wide range of fields. The wide range of fields includes not only biochemical research but also medicine, innovative drug development, health care, environment, food, etc. Among them, paper-based paper microanalysis chips have many advantages of light weight, low cost, no need for power supply, and high disposability compared to existing devices. Therefore, it is expected to be used as an inspection device for developing countries with insufficient medical equipment, medical care in remote areas or disaster sites, and airports where the spread of infectious diseases needs to be checked near water. Since paper-based paper microanalysis chips are low in cost and easy to handle, paper-based paper microanalysis chips have also become a focus of attention, such as health care devices that can manage or monitor his or her own health status.

[0003] As an example of a paper microanalysis chip, in Patent Document 1, two paper substrates each having an electrode printed on its surface are used, an ion selective membrane is held between the two, and a predetermined solution is dispensed to each paper substrate, resulting in a structure similar to an ion selective electrode and a reference electrode each having an internal liquid. With this structure, an ion electrode method can be performed, and the ion concentration of a sample can be measured. Non-Patent Document 1 describes a method in which an ion selective electrode and a reference electrode are formed on a single paper substrate, and the ion concentration of a sample can be measured using the ion electrode method.

[0004] Prior art literature

[0005] Patent Literature

[0006] Patent Document 1: U.S. Patent Application Publication No. 2016 / 033438

[0007] Non-patent literature

[0008] Non-patent document 1: Nipapan Ruecha, Orawon Chailapakul, Koji Suzuki, and Daniel Chitterio, "Potential ion sensing device based entirely on inkjet printing paper", Analytical Chemistry, 89, pp. 10608-10616, published on August 29, 2017 Summary of the invention

[0009] Problem that the invention aims to solve

[0010] However, in the case of the method described in Patent 1, there is a porous substrate layer between the working electrode and the ion selective membrane, and when a liquid replacing the internal solution is filled, when bubbles are formed at the electrode interface, there is a possibility that the measured value is unstable. In addition, since the ion selective membrane is sandwiched by two paper substrates, not only the thickness of the electrode and the ion selective membrane but also the thickness equivalent to the two sheets of porous substrates is required as the thickness of the analysis chip.

[0011] In the case of the method described in Non-Patent Document 1, a sufficient amount of sample cannot penetrate into the region of the paper substrate where the ion selective membrane is formed, so the contact area between the sample and the ion selective membrane is insufficiently provided and becomes unstable, with the result that the measurement accuracy may be affected.

[0012] An object of one aspect of the present disclosure is to obtain stable measurement using a configuration in which a working electrode and an ion selective membrane are in contact with each other, resulting in miniaturization by forming all electrodes on a single porous substrate, and to achieve stable measurement by sufficiently ensuring the contact area between the ion selective membrane and a sample without increasing the electrode area.

[0013] Solutions for solving problems

[0014] An aspect of the present invention provides a microfluidic device using a porous substrate. The microfluidic device has a flow path region using a porous body, the flow path region partially has a region A in which a component with ion selectivity exists in the pores in the porous substrate, and in the region A, the component with ion selectivity exists in the pores on the plane X side of one side of the porous substrate, and the plane Y side of the other side of the porous substrate is a flow path with empty pores, a working electrode is provided on the surface on the plane X side of the region A in a manner that at least partially overlaps with the component with ion selectivity, and a reference electrode is provided in a region B of the flow path region other than the region A, and the region A and the region B are formed in the same porous substrate.

[0015] Effects of the Invention

[0016] According to aspects of the present disclosure, a small-sized micro-flow channel device having high measurement stability can be provided. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 This is a top view of the microchannel device M1 after the channel wall 11 is formed in Example 1.

[0018] Figure 2A This is a schematic diagram of the micro-channel device M1 after various electrodes are formed in Example 1.

[0019] Figure 2BThis is a schematic diagram of the micro-channel device M1 after various electrodes are formed in Example 1.

[0020] Figure 3A Schematic diagram illustrating the permeation of a sample in the micro-channel device M1 of Example 1.

[0021] Figure 3B Schematic diagram illustrating the permeation of a sample in the micro-channel device M1 of Example 1.

[0022] Figure 4A This is a schematic diagram of the microchannel device M2 after the channel wall 12 is formed in Example 2.

[0023] Figure 4B This is a schematic diagram of the microchannel device M2 after the channel wall 12 is formed in Example 2.

[0024] Figure 5A This is a schematic diagram of the micro-channel device M2 after various electrodes are formed in Example 2.

[0025] Figure 5B This is a schematic diagram of the micro-channel device M2 after various electrodes are formed in Example 2.

[0026] Fig. 6A This is a schematic diagram of a conventional configuration example in which a working electrode is covered with an ion-selective membrane.

[0027] Figure 6B This is a schematic diagram of a conventional configuration example in which a working electrode is covered with an ion-selective membrane. DETAILED DESCRIPTION

[0028] Hereinafter, exemplary embodiments of the present invention will be described with reference to the accompanying drawings. The following embodiments are illustrative and are not intended to limit the present invention to the details of the embodiments. In the following drawings, constituent elements that are not necessary for describing the embodiments are omitted from the drawings.

[0029] The micro-flow channel device according to the present invention is a micro-flow channel device that uses a porous substrate and has a flow channel region surrounded by a flow channel wall.

[0030] Examples of porous substrates include paper showing moderate porosity and hydrophilicity, such as filter paper, ordinary paper, high-quality paper, watercolor paper, drawing paper, and synthetic paper; however, the porous substrate is not limited to paper. The porous substrate may be a synthetic resin porous film or cloth, a fiber product, etc.

[0031] The flow path region includes a working electrode arrangement portion (region A) and a reference electrode arrangement portion (region B). A region connecting the working electrode arrangement portion (region A) and the reference electrode arrangement portion (region B) may be provided, and a distribution portion may be further provided.

[0032] Examples of the material of the flow path wall include hydrophobic resin; however, the material of the flow path wall is not limited to the hydrophobic resin.

[0033] Examples of a method of forming the flow path wall include a method of printing using a hydrophobic resin as a toner by an electrophotographic method and melting and permeating the resin by heating. Examples of the resin include thermoplastic resins.

[0034] Thermoplastic resin is not limited. Examples of thermoplastic resins include the following known resins. Examples of thermoplastic resins include polyester resins, vinyl resins, acrylic resins, styrene acrylic resins, polyethylene, polypropylene, polyolefins, ethylene-vinyl acetate copolymer resins, and ethylene-acrylic acid copolymer resins. Among the above resins, polyester resins or styrene acrylic resins are preferred, and styrene acrylic resins are more preferred.

[0035] The method of forming the flow path wall is not limited to the method of melting and infiltrating the resin by heating, and may be a method of infiltrating wax using a wax printer or a method of infiltrating the resin by screen printing.

[0036] <Working Electrode Arrangement Section>

[0037] The microfluidic device has a working electrode arrangement portion (region A) in the portion of the flow path region where the ion-selective component exists in the pores in the porous substrate. In the working electrode arrangement portion (region A), the ion-selective component exists in the pores on the plane X side of one side of the porous substrate, and an ion-selective membrane is formed. The plane Y side of the other side of the porous substrate is a flow path with empty pores.

[0038] The working electrode is provided on the surface on the plane X side of the ion selective membrane formed in the working electrode arrangement portion (region A).

[0039] The working electrode is preferably in full contact with the ion selective membrane at the surface opposite to the plane X side of the porous substrate in the region A. With such a configuration, direct contact of the liquid that has permeated into the flow path without passing through the ion selective membrane with the working electrode can be suppressed, so only ions selected by the ion selective membrane can contact the working electrode, and contact of other ions with the working electrode can be suppressed.

[0040] Preferably, the working electrode arrangement portion (region A) has a portion ( Figure 5B 13) in (b) and the porous body is buried to not be used as a flow path portion ( Figure 5B 12) in (b), and to cross the portion that becomes the flow path ( Figure 5B 13) in (b) and the portion not used as a flow path ( Figure 5BThere is an ion-selective part ( Figure 5B This will allow only the ions selected by the ion selective membrane 22 to contact the working electrode 31 and prevent other ions from contacting the working electrode 31.

[0041] <Reference Electrode Arrangement Section>

[0042] A reference electrode is provided in a region B of the flow path region excluding the region A, that is, in a reference electrode arrangement portion excluding the working electrode arrangement portion.

[0043] [Example 1]

[0044] <Substrate / Flow path>

[0045] Will refer to Figure 1 The base material of the micro-channel device M1 will be described. Figure 1 The top view of the micro-channel device M1 before various electrodes are formed is schematically shown.

[0046] In the present embodiment, paper is used as the porous substrate S1. The material is cellulose, the thickness is 100 μm, and the porosity is 50%. Due to the micro-air gaps between the cellulose fibers, the capillary phenomenon works, and the porous substrate S1 has high hydrophilicity and serves as a flow path for the liquid to penetrate smoothly. The hydrophobic resin is infiltrated into the area that is part of the porous substrate S1 to form a flow path wall 11 with a height H1 = 10 mm and a width L1 = 22 mm. The flow path wall 11 is formed by using a hydrophobic resin as a toner and printing using an electrophotographic method (the method described in Japanese Patent Gazette No. 2021-037612) and melting and infiltrating the resin by heating.

[0047] The area within the flow path wall 11 includes an area into which the hydrophobic resin that becomes the flow path wall does not penetrate, and this area becomes the flow path of the porous body using the porous substrate S1. The flow path is composed of a flow path with a width of 2 mm and extending from the working electrode arrangement part S1b, the reference electrode arrangement part S1c and the distribution part S1d or from the distribution part S1d to the working electrode arrangement part S1b and a flow path with a width of 2 mm and extending from the distribution part S1d to the reference electrode arrangement part S1c. The working electrode is arranged in the working electrode arrangement part S1b, and the reference electrode is arranged in the reference electrode arrangement part S1c. The distribution part S1d is located between the working electrode arrangement part S1b and the reference electrode arrangement part S1c. The working electrode arrangement part S1b and the reference electrode arrangement part S1c are both square shapes with each side of 6 mm, and the distribution part S1d is a circle with a diameter of 3 mm. The size, shape, etc. of the flow path in Example 1 are as described above; however, the size, shape, etc. of the flow path are not limited thereto.

[0048] In the following, reference will be made to Figure 2A and Figure 2B The formation of various components of the micro-channel device M1 will be described. Figure 2A It is a top view of the micro-channel device M1 after various electrodes and the like are formed. Figure 2B A cross section taken along the dashed line D1 is shown.

[0049] <Ion Selective Membrane>

[0050] As for the ion selective membrane 21, a membrane for selectively reacting with Na ions and measuring the Na ion concentration is obtained by mixing the materials described in Table 1 below, stirring the mixture until the mixture is completely dissolved, and applying the dissolved mixture to the working electrode arrangement portion S1b. The material type and ratio are not limited thereto. The configuration only needs to have ion selectivity, so an ion carrier corresponding to the type of ion to be measured or a material and ratio suitable for the configuration can be selected as needed.

[0051] [Table 1]

[0052] Ionophore Bis[(12-crown-4)methyl]2-dodecyl-2-malonic acid dimethyl ester 0.3wt% Anion scavenger NaTFPB (Tetrakis[3,5-bis(trifluoromethyl)phenylboronic acid, sodium salt) 0.05wt% Plasticizers Dioctyl Sebacate 6.4wt% Support Polyvinyl chloride 3.25wt% Solvents Cyclohexanone 90wt%

[0053] The ion selective membrane 21 was uniformly applied to the working electrode arrangement portion S1b using a reagent spotter Biospot manufactured by MICROJET Co., Ltd. The discharge pipe diameter was Φ200μm, the droplet size was 4nL / droplet, the discharge frequency was 4Hz, and the membrane thickness was adjusted by applying five layers at a pitch of 300μm. The stage used to fix the porous substrate S1 when applying the ion selective membrane 21 was a heating stage and the temperature was set to 90°C. When the solute concentration of the solution was set to 10% by mass, the solution viscosity was relatively low, so it was easy to perform stable discharge. On the other hand, since the stage was heated, the solvent in the solution applied to the porous substrate S1 was volatilized smoothly, so the solution hardened before penetrating into the porous substrate S1 in the thickness direction to fill the flow path. Thus, even when the ion selective membrane 21 is applied to Figure 2B When the plane X side is shown, the flow path still remains at the Y side plane which is the back side of the X side, so the sample dispensed by the dispensing section S1d can completely penetrate into the working electrode arrangement section S1b. The heating of the stage is indispensable. In addition to reducing the droplet size, the flow path can also be left at the Y side plane by expanding the pitch between the printing points, reducing the printing speed, etc.

[0054] In this embodiment, the ion selective membrane 21 is coated using a spray method that discharges micro droplets; however, the method is not limited thereto. For example, the ion selective membrane 21 may be coated using a dispenser or by screen printing. Compared to the spray method, a dispenser or screen printing allows coating even with high viscosity, and therefore, by increasing the viscosity by, for example, increasing the solute concentration, it is possible to make it difficult for the ion selective membrane 21 to penetrate the material for forming the ion selective membrane 21 into the porous substrate S1 in the thickness direction.

[0055] <Working Electrode>

[0056] Ag is used as the material of the working electrode 31. A slurry obtained by dispersing Ag in a hydrophobic solvent can form a good electrode without being repelled when applied to the ion selective membrane 21 having the same hydrophobicity. The material is not limited thereto. Any material is applicable as long as the material can be stably formed on the ion selective membrane 21 and used as a working electrode.

[0057] In the coating process of the working electrode 31, the ion selective membrane 21 is coated on the porous substrate S1, and then printed using a screen printer DP-320 manufactured by NEWLONG MACHINE WORKS. The printing condition is #200, and drying is performed at a temperature of 80°C for 10 minutes. The printing shape is such that a square of 4 mm on each side of the ion selective membrane 21 (a square of 6 mm on each side) is connected to a rectangle extending from one side of the square of 4 mm on each side to the outside of the flow path wall 11 and having a width of 1 mm and a length of 5 mm. Then, the working electrode 31 can be connected to a measuring instrument for measuring the electrode potential in the area outside the flow path wall 11.

[0058] By printing the working electrode 31 directly on the ion selective membrane 21 to form a solid contact type ion selective electrode, there is no bubble attached to the electrode interface, and measurement can be performed stably.

[0059] <Reference Electrode>

[0060] Ag / AgCl is used as the material of the reference electrode 32. By using Ag / AgCl, an equilibrium reaction expressed by the following formula (1) occurs in the aqueous solution, so that the Cl around the reference electrode 32 can be - A stable potential is obtained when the concentration is stable.

[0061] [Formula 1]

[0062]

[0063] The reference electrode 32 was applied to the reference electrode arrangement portion S1c using a screen printer DP-320 manufactured by NEWLONG MACHINE WORKS. The printing condition was #200, and drying was performed at a temperature of 80°C for 10 minutes. The shape of the reference electrode 32 was such that a square of 6 mm on each side was connected to a rectangle of 1 mm in width and 3 mm in length extending from one side of the square of 6 mm on each side to the outside of the flow path wall 11. The reference electrode 32 can be connected to a measuring instrument for measuring the electrode potential in the area outside the flow path wall 11.

[0064] <Electrolyte Layer>

[0065] The electrolyte layer 41 has the function of dissolving the sample with water when the sample penetrates into the reference electrode arrangement portion S1c and making Cl - The concentration of electrolyte layer 41 is saturated to stabilize the potential of reference electrode 32. KCl is used as the material of electrolyte layer 41. KCl is easily soluble in water, and the diffusion rate of K ions and the diffusion rate of Cl ions are substantially equal to each other, so that the liquid potential is unlikely to be generated. Therefore, KCl is selected. Of course, the material of electrolyte layer 41 is not limited thereto. The material of electrolyte layer 41 only needs to stabilize the potential of reference electrode 32. For example, NaCl or the like can be used.

[0066] The electrolyte layer 41 is coated using a reagent spotter Biospot manufactured by MICROJET. A solution is prepared by dissolving KCl in pure water to have a concentration of 16wt%. The electrolyte layer 41 is completely coated on the reference electrode arrangement portion S1c with a droplet size of 6nL / drop, a discharge frequency of 10Hz, and a pitch of 300μm in both the vertical and horizontal directions, and is coated in three layers to adjust the amount of KCl. The amount of KCl is set to an amount that is saturated with respect to the amount of the sample infiltrated into the reference electrode arrangement portion S1c, and as a result, the potential of the reference electrode 32 can be stabilized. Therefore, as long as there is an amount of KCl that can prepare saturated KCl, the coating amount is not limited thereto.

[0067] <Permeation of Sample>

[0068] Will refer to Figure 3A and Figure 3B The penetration of the sample into the micro-channel device M1 will be described. Figure 3A It is a top view of the micro-channel device M1 on which various electrodes are formed. Figure 3B A cross section taken along the dashed line D2 is shown.

[0069] When the micro-channel device M1 is used, the sample is distributed to the distribution part S1d. Then, the distributed sample flows along the channel due to the capillary phenomenon and penetrates in the direction of the arrow A1 and the direction of the arrow A2. Figure 3BAs shown, the ion selective membrane 21 does not fill the porous substrate S1 in the thickness direction, so that the sample can penetrate into the working electrode arrangement portion S1b. The reference electrode 32 is filled in the thickness direction of the paper, and the sample that has penetrated into the reference electrode 32 continues to penetrate into the reference electrode arrangement portion S1c, while dissolving the electrolyte layer 41 coated on the surface of the reference electrode 32, and is maintained around the reference electrode 32 in a state where the concentration of Cl is saturated.

[0070] Thus, as described above, regardless of the sample, the reference electrode 32 stably exhibits a potential in a KCl saturated state, while the working electrode 31 indicates a potential generated by the Nernst response of the ion selective membrane 21 according to the Na ion concentration of the sample. Thus, the potential difference between the reference electrode 32 and the working electrode 31 of the microchannel device M1 is measured, and the Na ion concentration of the sample can be detected by the ion electrode method using the following formula (2).

[0071] E-E0=2.303×(RT / nF)×log(f×c)···(2)

[0072] E: electrode potential of the working electrode

[0073] E0: electrode potential of the reference electrode

[0074] R: Gas constant (8.314 JK -1 mol -1 )

[0075] T: measured temperature expressed in absolute temperature

[0076] n: valence of the ion to be measured

[0077] F: Faraday constant (9.649×10 -4 Cmol -1 )

[0078] f: activity coefficient

[0079] c: molar concentration of the ion

[0080] As described above, when the ion selective membrane 21 is coated in such a manner as not to completely bury the porous substrate S1 in the thickness direction and then the working electrode 31 is coated thereon, the contact area between the ion selective membrane 21 and the sample can be increased without increasing the area or perimeter of the ion selective membrane 21, so that the measurement is stable. In comparison, Fig. 6A and Figure 6B FIG. 2 shows a conventional configuration example in which a working electrode 31 is formed and then covered with an ion selective membrane 21. Fig. 6A and Figure 6BIn the configuration of the embodiment, the ion selective membrane 21 completely buries the porous substrate S1 in the thickness direction, so that the sample distributed to S1d penetrates only to the portion indicated by the arrow A3, and the sample and the ion selective membrane 21 contact each other only at the interface of S1e, so that the contact area is small. Therefore, with the configuration of this embodiment, the contact area between the ion selective membrane 21 and the sample can be increased compared with the existing configuration.

[0081] The contact between the ion selective membrane 21 and the working electrode 31 is a solid contact without using an internal liquid therebetween, so that bubbles do not adhere to the surface of the base electrode, and measurement can be performed stably. In addition, since the ion selective membrane 21 and the working electrode 31 are constructed on a single porous substrate, a thin film construction can be achieved compared to the case where the ion selective membrane is formed on a first porous substrate and the working electrode is formed on a second porous substrate disposed on the ion selective membrane.

[0082] [Example 2]

[0083] As for the micro-flow channel device M2 according to the present embodiment, only the differences from the micro-flow channel device M1 of Embodiment 1 will be described, the same reference numerals denote the same components, and the description of the same parts will be omitted.

[0084] <Flow path>

[0085] Will refer to Figure 4A and Figure 4B The flow path of the micro-flow path device M2 will be described. Figure 4A The top view of the micro-channel device M2 before various electrodes are formed is schematically shown. Figure 4B A cross section taken along the dashed line D3 is shown.

[0086] In the microfluidic device M2, not only the flow path wall 11 is similar to the flow path wall of the microfluidic device M1, but also the flow path wall 12 is formed in the working electrode arrangement part S1b. The flow path wall 12 has a checkerboard pattern of 500 μm squares, and the hydrophobic resin is printed by electrophotography similar to that of Example 1, and can be easily printed by changing the image pattern. Compared with the flow path wall 11, by reducing the printing concentration of the hydrophobic resin, it is possible to perform adjustment so that the porous substrate S1 is not buried in the thickness direction. The phrase "checkerboard pattern of 500 μm squares" means that, as Figure 4A As shown, one side where the flow path wall is formed at the position of the 500 μm square and one side where the flow path wall is not formed at the position of the 500 μm square are alternately arranged.

[0087] In the present embodiment, the printing concentration of the flow path wall 12 is set to 20% of the printing concentration of the flow path wall 11. Thus, the X-side plane of the working electrode arrangement portion S1b is partially covered with resin, and the flow path through which the sample penetrates remains on the Y-side plane on the back. Then, at the position of the flow path wall 12 forming the X-side plane, the pores of the porous substrate S1 are filled with a hydrophobic resin, so that the capillary phenomenon does not work and the liquid does not penetrate. On the other hand, the pores of the porous substrate S1 remain at the position on the X-side plane where the hydrophobic resin does not exist (the position where the flow path wall 12 is not formed), so such a position is used as the flow path through which the liquid penetrates. By changing the ratio of the area of ​​the flow path wall 12 (the total area of ​​the flow path wall 12) to the area of ​​the working electrode arrangement portion S1b (hereinafter, also referred to as the area ratio), the amount of liquid that penetrates into the porous substrate S1 from the X-side plane can be controlled. In the present embodiment, as Figure 4A As shown, a checkerboard pattern is adopted, and the area ratio of the flow path wall is 50%; however, the size and shape of each flow path wall 12 and the area ratio are not limited thereto and can be selected as needed according to various configurations. The size and shape of each flow path wall can be changed according to the position of the flow path wall (e.g., the distance from the distribution portion S1d).

[0088] In the following, reference will be made to Figure 5A and Figure 5B The formation of the ion selective membrane 22 will be described. Figure 5A It is a top view of the micro-channel device M2 after various electrodes and the like are formed. Figure 5B (a) shows a cross section taken along the dotted line D4. Figure 5B (b) shows Figure 5B A partial enlarged view of (a).

[0089] <Ion Selective Membrane>

[0090] The ion selective membrane 22 is made of the same material as the ion selective membrane 21, and is different from the ion selective membrane 21 only in the substrate to which the material forming the ion selective membrane is applied. The ion selective membrane 22 is applied to the flow path wall 12 by the same method as that of Example 1. At this time, since the ion selective membrane 22 penetrates into the porous substrate S1 only from the portion without resin in the flow path wall 12, the ion selective membrane 22 can be formed in a state where the porous substrate S1 reduces the amount of the ion selective membrane to be penetrated and leaves more flow paths in the thickness direction of the paper, compared with Example 1. Thus, after the sample is distributed into the distribution section S1d, the rate at which the sample penetrates into the working electrode arrangement section S1b increases, so that further rapid measurement can be performed.

[0091] In addition to the above, the working electrode 31, the reference electrode 32 and the electrolyte layer 41 were formed in the same manner as in Example 1 to obtain Figure 5A and Figure 5B The micro-channel device M2 shown. Then, by measuring the potential difference between the reference electrode 32 and the working electrode 31 after the sample is dispensed to the dispensing portion S1d, the Na ion concentration of the sample can be measured.

[0092] As described above, by pre-forming a flow path wall in a portion of the flow path in the region where the ion selective membrane is formed, the penetration of the ion selective membrane after coating into the porous substrate in the thickness direction in this region can be controlled, and measurement can be performed quickly by leaving the flow path wider.

[0093] If the area ratio of the flow path wall 12 is excessively increased, the contact area between the ion selective membrane 22 and the sample is reduced, so it is necessary to appropriately select the area ratio according to the size of the working electrode arrangement portion S1b, the thickness of the porous substrate, other desired measurement accuracy and rate, etc. The area ratio of the flow path wall 12 is not limited to the conditions of this embodiment.

[0094] The present invention is not limited to the above-described embodiments. Various changes or modifications are applicable without departing from the spirit and scope of the present invention. Therefore, the following claims are attached to show the scope of the present invention.

[0095] This application claims priority from Japanese Patent Application No. 2022-074918 filed on April 28, 2022, the entire contents of which are incorporated herein by reference.

[0096] Description of Reference Numerals

[0097] M1 Microfluidic Device

[0098] S1 Porous Substrate

[0099] S1b Working electrode arrangement part (area A)

[0100] S1c Reference electrode arrangement portion (region B)

[0101] S1d Distribution Department

[0102] 11 Flow path wall

[0103] 12 Flow path wall

[0104] 21, 22 Ion selective membrane

[0105] 31 Working electrode

[0106] 32 Reference electrode

[0107] 41 Electrolyte layer

Claims

1. A microfluidic device using a porous substrate, wherein: The microfluidic device has a flow path region using a porous body, The flow path region partially has a region A where a component having ion selectivity exists in the pores in the porous substrate, and in the region A, the component having ion selectivity exists in the pores on the plane X side of one side of the porous substrate, and the plane Y side of the other side of the porous substrate is a flow path where empty pores exist, The working electrode is disposed on the surface of the region A on the side of the plane X in such a manner as to at least partially overlap the ion-selective component, and The reference electrode is provided in a region B of the flow path region excluding the region A, and the region A and the region B are formed in the same porous substrate.

2. The microfluidic device according to claim 1, wherein: The working electrode is in full contact with the ion-selective membrane at the surface opposite to the plane X side of the porous substrate in the region A.

3. The microfluidic device according to claim 1 or 2, wherein: The region A has a portion at the surface of the plane X that uses the porous body to become a flow path and a portion that buries the porous body so as not to function as a flow path, and The ion-selective component is present so as to span between the portion serving as the flow path and the portion not serving as the flow path.

4. The microfluidic device according to claim 3, wherein: The portion in which the porous body is buried so as not to function as a flow path is a portion in which the porous body is buried with a hydrophobic resin so that the portion does not function as a flow path.

5. The microfluidic device according to claim 1 or 2, wherein: The region A and the region B are connected via a flow path.