Double-channel hot charging and direct conveying production line and plate blank transportation method
Through the dual-channel hot loading direct delivery line and slab transportation method, the use of hot loading rollers and cross-traffic vehicles to achieve synchronous transportation, solving the problems of low temperature and high energy consumption in the traditional slab transportation process, and improving the transportation speed and heat The direct delivery rate has improved economic and social benefits.
Patent Information
- Application Number
- CN202411135380.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-19
- Publication Date
- 2024-12-06
AI Technical Summary
In the traditional slab transfer process, the complex types of steel lead to different requirements for stack cold time, which leads to difficulty in direct delivery of hot loading and direct delivery of hot loading. The slab loading furnace is low, consumes a long time and has high energy consumption.
Using the dual-channel hot-mounted direct delivery line and slab transportation method, two channels are formed by the first and second feed rollers, which are not required to stack and need to stack and cool, respectively, and synchronously is achieved by using the hot-mounted rollers and cross-traffic vehicles. For transportation, set up laser targeting and temperature measurement devices to ensure accurate positioning and temperature control.
It improves the speed of blank transfer, improves the direct delivery rate of hot loading, reduces energy consumption, and improves economic and social benefits.
Smart Images

Figure CN119076651A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of steel production, and in particular to a dual-channel hot-charging direct-transportation production line and a slab transportation method. Background Art
[0002] Due to the variety of products produced by medium and thick plate and coil mills, each type of steel has different requirements for stack cooling time, which makes it difficult to organize hot charging and direct delivery. The traditional slab transfer process is to transport the billets produced in the continuous casting workshop to the hot rolling slab warehouse by vehicle. The transportation method is single, and it takes a long time from the billet leaving the continuous casting machine to loading and then transporting it to the hot rolling workshop, resulting in a low slab charging furnace temperature. Summary of the invention
[0003] The technical problem to be solved by the present invention is to overcome the shortcomings of the prior art and provide a dual-channel hot-loading direct delivery production line and a slab transportation method.
[0004] In order to solve the above technical problems, the technical solution of the present invention is as follows: A dual-channel hot-loading direct delivery production line, comprising: A first feeding roller, the feeding end of which is connected to the discharging end of the continuous casting machine; A second feeding roller conveyor, the axis of which coincides with the axis of the first feeding roller conveyor, the feeding direction of the second feeding roller conveyor is opposite to that of the first feeding roller conveyor, and the discharge end of the second feeding roller conveyor is adjacent to the discharge end of the first feeding roller conveyor; A first heating furnace is arranged on one side of the first feeding roller conveyor and is located at a discharge end of the first feeding roller conveyor; A second heating furnace is arranged on one side of the second feeding roller conveyor and is located at a discharge end of the second feeding roller conveyor; A cooling bed, arranged on one side of the first feeding roller conveyor; A slab storage is arranged on one side of the second feeding roller, and the slab storage and the cooling bed are located on the same side of the axis of the first feeding roller; The steel loader is used to transport the blanks on the first feeding roller and the second feeding roller to the first heating furnace and the second heating furnace respectively.
[0005] As a preferred solution of the dual-channel hot-loading direct delivery production line of the present invention, it also includes a cross-car assembly, which is located between the cooling bed and the slab warehouse and is used to transport the blanks on the cooling bed to the slab warehouse.
[0006] As a preferred solution of the dual-channel hot-loading direct delivery production line described in the present invention, it also includes a first crane and a second crane, the first crane is used to transport the blanks on the cooling bed to the cross-car assembly, and the second crane is used to transport the blanks in the slab warehouse to the second feeding roller.
[0007] As a preferred solution of the dual-channel hot-loading direct-feeding production line described in the present invention, first laser irradiation devices are provided on both sides of the first feeding roller.
[0008] As a preferred solution of the dual-channel hot-loading direct delivery production line described in the present invention, a second laser irradiation device and a third laser irradiation device are respectively provided at the inlet end of the first heating furnace and the inlet end of the second heating furnace.
[0009] As a preferred solution of the dual-channel hot-loading direct-feeding production line described in the present invention, a first temperature measuring device is provided on one side of the first feeding roller, and a second temperature measuring device is provided on one side of the second feeding roller.
[0010] The present invention also provides a slab transportation method, which is based on the above-mentioned dual-channel hot charging direct delivery production line, comprising: Step S101: Determine whether the blank needs to be subjected to stack cooling treatment, if yes, proceed to step S102, if no, proceed to step S103; Step S102: conveying the blank to the first temperature measuring device through the first feeding roller to measure the temperature and determine the charging temperature, then conveying the blank to the inlet end of the first heating furnace through the first feeding roller, and loading the blank with steel through the steel loader after positioning is completed; Step S103: The blank is conveyed to the cooling bed through the first feeding roller, and then the second crane is used to lift the blank to the cross-car assembly, and the cross-car assembly conveys the blank to the slab warehouse. After the blank is cooled to below 550°C, the second crane lifts the blank to the second feeding roller, and conveys it to the second temperature measuring device through the second feeding roller for temperature measurement to determine the charging temperature. Then, the second feeding roller conveys the blank to the entrance of the second heating furnace, and after positioning, it is loaded with steel through the steel loader.
[0011] The beneficial effects of the present invention are: The present invention forms a first channel and a second channel for billet transportation for billets that do not require stack cooling and billets that require stack cooling, respectively, solving the problems of long traditional slab transportation process, low furnace loading temperature, and high energy consumption. The hot charging roller and the cross-over car realize dual-path synchronous transportation, which improves the transportation speed of billets, increases the hot charging direct delivery rate, reduces energy consumption, and improves economic and social benefits. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative labor.
[0013] Figure 1 This is a schematic diagram of the structure of the dual-channel hot-loading direct-delivery production line provided by the present invention; Among them: 1. continuous casting machine; 2. billet; 3. first feeding roller; 4. first laser shooting device; 5. cooling bed; 6. first crane; 7. straddle car assembly; 8. second crane; 9. slab warehouse; 10. steel loader; 11. second laser shooting device; 12. third laser shooting device; 13. first heating furnace; 14. second heating furnace; 15. second feeding roller; 16. first temperature measuring device; 17. second temperature measuring device. DETAILED DESCRIPTION
[0014] In order to make the content of the present invention more clearly understood, the present invention is further described in detail below according to specific implementation modes and in combination with the accompanying drawings.
[0015] Figure 1 Schematic diagram of the dual-channel hot charging direct delivery production line provided in this application. The device includes a first feeding roller 3, a second feeding roller 15, a first heating furnace 13, a second heating furnace 14, a cooling bed 5, a slab warehouse 9 and a steel loader 10. Among them, two different feeding channels are formed for the two types of billets 2 that require stack cooling and those that do not require stack cooling.
[0016] For details, see Figure 1 , the feeding end of the first feeding roller 3 is connected to the discharging end of the continuous casting machine 1. The axis of the second feeding roller 15 coincides with the axis of the first feeding roller 3, that is, the first feeding roller 3 and the second feeding roller 15 are located on the same horizontal line. The feeding direction of the first feeding roller 3 is opposite, and the discharging end of the second feeding roller 15 is adjacent to the discharging end of the first feeding roller 3. Among them, the conveying direction of the billet 2 on the first feeding roller 3 is from right to left, and the conveying direction of the billet 2 on the second feeding roller 15 is from left to right.
[0017] The first heating furnace 13 and the second heating furnace 14 are respectively arranged on one side of the first feeding roller 3 and the second feeding roller 15. Figure 1From the top view of the dual-channel hot charging direct delivery production line, the first heating furnace 13 is located below the first feeding roller 3 and is close to the discharge end of the first feeding roller 3. The second heating furnace 14 is located below the second feeding roller 15 and is close to the discharge end of the second feeding roller 15. The cooling bed 5 is located above the first feeding roller 3. The slab warehouse 9 is located above the second feeding roller 15. The steel loader 10 is arranged at the entrance end of the two heating furnaces, and is used to transport the blank 2 on the feeding roller to the corresponding heating furnace.
[0018] Preferably, a cross-car assembly 7 is provided between the cooling bed 5 and the slab warehouse 9. The cross-car assembly 7 is used to transport the blank 2 on the cooling bed 5 to the slab warehouse 9.
[0019] According to whether the steel type will produce hot-charging cracks, the billet 2 can be divided into two categories: those that need stack cooling and those that do not need stack cooling. For the billet 2 that does not need stack cooling, it is transferred to the first heating furnace 13 through the first channel. Specifically: after the continuous casting machine 1 pulls out the billet 2, it is cut and directly transported to the front of the first heating furnace 13 by the first feeding roller 3. After positioning in front of the first heating furnace 13, it is loaded into the furnace by the steel loader 10. For the billet 2 that needs stack cooling, it is transferred to the second heating furnace 14 through the second channel. Specifically: after the continuous casting machine 1 pulls out the billet 2, it is cut and transported to the front of the cooling bed 5 along the first feeding roller 3, and the billet 2 is transported to the cooling bed 5 by a conveying device such as a sprocket, cooled on the cooling bed 5, and then transported to the cold cargo position of the slab warehouse 9 by the equipped cross-car to wait for loading. When the billet 2 reaches the stack cooling condition, the billet 2 is hoisted to the second feeding roller 15 by a crane and transported to the front of the second heating furnace 14. After being positioned in front of the second heating furnace 14 , the steel is loaded by the steel loader 10 .
[0020] Preferably, a first laser irradiation device 4 is provided on both sides of the first feeding roller 3. The first laser irradiation device 4 includes a laser emitting end and a laser receiving end. The laser emitting end and the laser receiving end are relatively arranged on both sides of the first feeding roller 3. When the first feeding roller 3 conveys the blank 2, the first laser irradiation device 4 can measure the length of the blank 2.
[0021] At the same time, a second laser irradiation device 11 is provided on both sides of the entrance end of the first heating furnace 13, and a third laser irradiation device 12 is provided on both sides of the entrance end of the second heating furnace 14. When the steel loader 10 loads the billet 2 into the heating furnace, the corresponding laser irradiation device can collect the width information of the billet 2.
[0022] In addition, a first temperature measuring device 16 is provided on one side of the first feeding roller 3, and a second temperature measuring device 17 is provided on one side of the second feeding roller 15. When the first feeding roller 3 is conveying the blank 2, the first temperature measuring device 16 can collect the temperature information of the blank 2 thereon. When the second feeding roller 15 is conveying the blank 2, the second temperature measuring device 17 can collect the temperature information of the blank 2 thereon.
[0023] The present application also provides a slab transportation method, which is based on the above-mentioned dual-channel hot-loading direct delivery production line. The method comprises the following steps: Step S101: Determine whether the blank 2 needs to be subjected to stack cooling treatment. If so, proceed to step S102; if not, proceed to step S103.
[0024] Specifically, depending on whether hot-charging cracks will occur in the steel type, the blank 2 can be divided into two categories: needing stack cooling and not needing stack cooling.
[0025] Step S102: The blank 2 is conveyed to the first temperature measuring device 16 by the first feeding roller 3 for temperature measurement to determine the charging temperature, and then the blank 2 is conveyed to the entrance end of the first heating furnace 13 by the first feeding roller 3. After positioning is completed, the blank 2 is loaded with steel by the steel loader 10.
[0026] Specifically, after the continuous casting machine 1 pulls out the billet 2, it is cut and directly transported to the front of the first heating furnace 13 by the first feeding roller 3. The first laser beam device 4 and the first temperature measuring device 16 arranged on both sides of the first feeding roller 3 respectively collect the length and temperature information of the billet 2. After positioning in front of the first heating furnace 13, the steel loader 10 loads the furnace. While loading steel, the second laser beam device 11 in front of the furnace collects the width information of the billet 2.
[0027] Step S103: The blank 2 is conveyed to the cooling bed 5 by the first feeding roller 3, and then the second crane 8 is used to lift the blank 2 to the cross-car assembly 7, and the cross-car assembly 7 conveys the blank 2 to the slab warehouse 9. After the blank is cooled to below 550°C, the second crane 8 lifts the blank 2 to the second feeding roller 15, and conveys it to the second temperature measuring device 17 by the second feeding roller 15 for temperature measurement to determine the charging temperature. Then, the blank 2 is conveyed to the entrance of the second heating furnace 14 by the second feeding roller 15, and after positioning is completed, it is loaded with steel by the steel loader 10.
[0028] Specifically, after the continuous casting machine 1 pulls out the billet 2, it is cut and transported to the cooling bed 5 along the first feeding roller 3, cooled on the cooling bed 5, and then transported to the billet 2 warehouse by the first crane 6 and the cross-car assembly 7 to wait for loading into the furnace. When the billet 2 reaches the stack cooling condition, the second crane 8 is used to lift the billet 2 to the second feeding roller 15. The third laser shooting device 12 and the second temperature measuring device 17 equipped on the second feeding roller 15 respectively collect the length and temperature information of the billet 2. The billet 2 is transported by the second feeding roller 15 to the front of the second heating furnace 14. After being positioned in front of the second heating furnace 14, the steel is loaded by the steel adding machine 10. At the same time, the third laser shooting device 12 in front of the furnace will collect the width information of the billet 2.
[0029] The above-mentioned slab transportation method is described below through specific embodiments.
[0030] Example 1: In this example, a continuous casting machine 1 pulls out a billet 2 that does not require stacking and cooling, and the steel grade of the billet 2 is Q245R. It is transported by the first feeding roller 3, and after passing through the first laser shooting device 4, the length of the billet 2 is measured to be 8164mm. It continues to be transported along the first feeding roller 3 to the first temperature measuring device 16 to collect the temperature of the billet 2, and the charging temperature is measured to be 622℃. After the collection is completed, it is transported to the front of the first heating furnace 13, and after positioning is completed, the steel loader 10 is used to load the steel, and the second laser shooting device 11 in front of the furnace measures the width of the billet 2 to be 3003mm, completing the charging of the direct-sent billet 2. The specific parameters are shown in Table 1.
[0031]
[0032] Table 1 Embodiment 2: In this embodiment, a billet 2 that needs to be stacked and cooled is pulled out by the continuous casting machine 1. The steel grade of the billet 2 is LR-A36 and is transported by the first feeding roller 3. After the first laser shooting device 4, the length of the billet 2 is measured to be 17131mm, and then it is transported to the cooling bed 5. When the billet 2 is transported to the end of the cooling bed 5, the first crane 6 is used to lift the billet 2 to the cross-car assembly 7, and the cross-car assembly 7 transports the billet 2 to the slab warehouse 9. After the billet 2 is stacked and cooled to below 550°C, the second crane 8 is used to transport the billet 2 to the second feeding roller 15, and the second feeding roller 15 is transported to the second temperature measuring device 17 to collect the temperature of the billet 2, which is 444°C. Then the billet 2 is transported to the second heating furnace 14. After positioning is completed, the steel loader 10 is used to load the steel, and the third laser shooting device 12 in front of the furnace measures the width of the billet 2 to be 3100mm, completing the loading of the direct-sent billet 2 into the furnace. The specific parameters are shown in Table 2.
[0033]
[0034] Table 2 Therefore, the technical solution of this application solves the problems of long traditional slab transfer process, low furnace loading temperature and high energy consumption. The hot charging roller and the cross-cart realize the synchronous transfer of dual paths, which improves the transfer speed of the slab, increases the hot charging direct delivery rate, reduces energy consumption, and improves economic and social benefits.
[0035] In addition to the above embodiments, the present invention may also have other implementation modes; any technical solutions formed by equivalent replacement or equivalent transformation shall fall within the protection scope required by the present invention.
Claims
1. A dual-channel hot-loading direct delivery production line, Features: include: A first feeding roller (3), the feeding end of which is connected to the discharging end of the continuous casting machine (1); A second feeding roller (15), the axis of which coincides with the axis of the first feeding roller (3), the feeding direction of the second feeding roller (15) is opposite to that of the first feeding roller (3), and the discharge end of the second feeding roller (15) is adjacent to the discharge end of the first feeding roller (3); A first heating furnace (13) is arranged on one side of the first feeding roller conveyor (3) and is located at the discharge end of the first feeding roller conveyor (3); A second heating furnace (14) is arranged on one side of the second feeding roller conveyor (15) and is located at the discharge end of the second feeding roller conveyor (15); A cooling bed (5) is arranged on one side of the first feeding roller conveyor (3); A slab storage (9) is arranged on one side of the second feeding roller conveyor (15), and the slab storage (9) and the cooling bed (5) are located on the same side of the axis of the first feeding roller conveyor (3); The steel loader (10) is used to transport the blanks (2) on the first feeding roller (3) and the second feeding roller (15) to the first heating furnace (13) and the second heating furnace (14) respectively.
2. According to the dual-channel hot-loading direct delivery production line of claim 1, Features: It also comprises a cross-car assembly (7), which is located between the cooling bed (5) and the slab warehouse (9) and is used to transport the blanks (2) on the cooling bed (5) to the slab warehouse (9).
3. According to claim 2, the dual-channel hot-loading direct delivery production line, Features: It also comprises a first crane (6) and a second crane (8), wherein the first crane (6) is used to transport the blank (2) on the cooling bed (5) to the cross-car assembly (7), and the second crane (8) is used to transport the blank (2) in the slab warehouse (9) to the second feeding roller (15).
4. According to claim 3, the dual-channel hot-loading direct delivery production line, Features: First laser irradiation devices (4) are arranged on both sides of the first feeding roller conveyor (3).
5. According to claim 4, the dual-channel hot-loading direct delivery production line, Features: A second laser irradiation device (11) and a third laser irradiation device (12) are respectively provided at the inlet end of the first heating furnace (13) and the inlet end of the second heating furnace (14).
6. According to claim 5, the dual-channel hot-loading direct delivery production line, Features: A first temperature measuring device (16) is provided on one side of the first feeding roller conveyor (3), and a second temperature measuring device (17) is provided on one side of the second feeding roller conveyor (15).
7. A slab transportation method, based on the dual-channel hot-loading direct delivery production line according to claim 6, Features: include: Step S101: Determine whether the blank (2) needs to be subjected to stack cooling treatment. If so, proceed to step S102; if not, proceed to step S103; Step S102: The blank (2) is conveyed to the first temperature measuring device (16) by the first feeding roller (3) for temperature measurement to determine the furnace charging temperature, and then the blank (2) is conveyed to the inlet end of the first heating furnace (13) by the first feeding roller (3). After positioning is completed, the blank (2) is loaded with steel by the steel loader (10); Step S103: The blank (2) is transported to the cooling bed (5) by the first feeding roller (3), and then the second crane (8) is used to lift the blank (2) to the cross-car assembly (7), and the cross-car assembly (7) transports the blank (2) to the slab warehouse (9). After being stacked and cooled to below 550° C., the second crane (8) lifts the blank (2) to the second feeding roller (15), and then the blank is transported to the second temperature measuring device (17) by the second feeding roller (15) for temperature measurement to determine the charging temperature. Then, the blank (2) is transported to the inlet end of the second heating furnace (14) by the second feeding roller (15), and after positioning is completed, it is loaded with steel by the steel loader (10).
Citation Information
Patent Citations
Hot rolled strip steel production system based on mixed heating and method
CN112108519A
Slab yard and heating furnace layout for thick plate cold blank and hot blank split charging and charging method through same
CN112575175A
Slab cast-rolling system and method for improving production efficiency of cast-rolling interface
CN114406019A
Multifunctional high-strength steel plate strip heat treatment production system and method