Solid wood veneer fitting method

Through the combination mechanism of the prototyping board and the storage bag, the synergistic effect of rope and roller is used to solve the gaps and wrinkles when fitting the decorative surface of solid wood furniture, achieving efficient and excellent quality fitting effect, reducing manual operation .

CN119077884AActive Publication Date: 2024-12-06ZUOYOU FURNITURE (HUIZHOU) CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202411363051.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-27
Publication Date
2024-12-06
Estimated Expiration
2044-09-27

AI Technical Summary

Technical Problem

During the processing of solid wood furniture, the flexible finish sheets cannot be fully aligned when fit for a long time, resulting in gaps and wrinkles, and cannot meet product quality standards.

Method used

Using a combination mechanism of profiling plates, storage bags, ropes, rollers and elastic fillers, the process edges are fixed with glue and pins, and the wood is gradually pulled to fit the finish to ensure the decoration. Flat surface fits.

Benefits of technology

Achieve high-quality fit between wood and finish, avoid hollowing and wrinkling, improve fit efficiency and quality, and reduce manual operation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119077884A_ABST
    Figure CN119077884A_ABST
Patent Text Reader

Abstract

The invention discloses a solid wood veneer fitting method, which relates to the field of furniture, and comprises the following steps of: 1, molding a profile modeling plate according to the appearance of a veneer and wood; secondly, the containing bag is shaped according to the appearance of the profiling plate; thirdly, rollers are installed, and the profiling plate, the fixing strips and the containing bag are connected; fourthly, one end of the veneer is fixed to a profiling plate, and the profiling plate is fixed; fifthly, the wood is evenly coated with glue, one end of the wood is sleeved with the rope, and the wood is attached to one end of the veneer; sixthly, the pins are detached, the wood and the veneer are pulled at a constant speed, and the rest parts of the wood and the veneer penetrate through the ropes; and 7, after fitting is completed, the process edge of the veneer is cut off. And the wood and the veneer are pre-attached, the wood is pulled at a uniform speed, so that the rest parts of the veneer are attached to the wood, and the veneer attaching quality is guaranteed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of furniture, and in particular to a method for laminating solid wood veneers. Background Art

[0002] In order to improve the appearance of solid wood furniture, some parts need to be designed. When processing wooden columns with concave arcs and arc-shaped protrusions, the flexible facing sheet needs to be attached to the wooden column after milling. When attaching extra-long facing sheets, neither the wood nor the facing sheet can be placed inside the equipment. When attaching the wooden column and the facing sheet in sections, the rest of the flexible facing sheet will droop on the platform, and the facing sheet needs to be manually lifted to align the facing sheet with the wooden column. Affected by the concave arcs and arc-shaped protrusions on the surface of the wooden column, there will be a gap between the wooden column and the facing sheet, resulting in poor bonding, hollowing of the finished product and wrinkling of the facing sheet in many places, which does not meet the product quality standards. Summary of the invention

[0003] The object of the present invention is to provide a method for laminating solid wood veneer to solve the problems raised in the above background technology.

[0004] To achieve the above object, the present invention adopts the following technical solution: a method for laminating solid wood veneer, comprising the following steps: Step 1: Shape the profiling board according to the veneer and the appearance of the wood. After the profiling board is hardened and shaped, remove the profiling board and the veneer; Step 2: Place the profiling plate into the containing bag, shape the containing bag according to the appearance of the profiling plate, and after the containing bag is hardened and shaped, take out the profiling plate, fill the containing bag with elastic filling material, and then seal it; Step 3: Determine the number of rollers according to the specifications of the wood to be laminated, pass the rope through each roller, pass both ends of the rope through the profiling board and bind them, install the profiling board to the fixing bar, and install the fixing bar to the middle of the receiving bag; Step 4: Fix the process edge of one end of the facing to the profiling board through pins, and clamp and fix the profiling board; Step 5: Apply glue evenly to the part of the wood to be bonded with the veneer. After the glue is applied, put one end of the wood into the rope so that the craft edge of the veneer is clamped between the roller on the rope and the surface of the wood that does not need to be bonded with the veneer. Adjust the position of the wood so that the wood and the end of the veneer are aligned, and bond the wood to one end of the veneer. Step 6: Remove the pins, pull the end of the wood and the veneer at a constant speed, and pass the rest of the wood and the veneer through the bag and the rope; Step 7: After lamination, cut off the process edge of the veneer; The solid wood veneer laminating method relies on the laminating mechanism described below for laminating: the solid wood veneer laminating mechanism includes: ropes, rollers, a containing bag, elastic filling materials, fixed strips and contour plates, the ropes are penetrated by a plurality of rollers, the rollers, the containing bag, fixed strips and contour plates are arranged in sequence along a straight line, the fixed strips are fixed to the middle of the outer surface of the containing bag, the elastic filling materials are filled in the containing bag, both ends of the contour plates are detachably arranged on the fixed strips, both ends of the ropes are penetrated by thermoplastic plates, the two ends of the ropes are detachably connected to each other, and the contour plates are thermoplastic plates.

[0005] Preferably, the outer surface of the wood is parallel to the center line of the wood, and the moving direction of the profiling board and the wood after hardening and shaping is parallel to each other.

[0006] Preferably, the containing bag is a thermoplastic plastic bag, and the elastic filler is rubber particles.

[0007] Preferably, the rope is a metal rope or a plastic rope with plastic deformation capability, the rope is detachably provided with two limiting elements, and the rollers are arranged between the two limiting elements. The rope is formed by twisting steel wires.

[0008] Preferably, the roller comprises a cylinder and an elastic outer coating, the cylinder is rotatably arranged on the rope, the elastic outer coating is sleeved on the outer surface of the cylinder, and the difference between the outer diameter and the inner diameter of the roller is equal to the thickness of the process edge.

[0009] Preferably, both ends of the fixing strip are bent with clamping plates, and both ends of the contoured plate are detachably arranged on the fixing strip through the clamping plates, and the fixing strip is any one of a thermoplastic plate, a memory metal plate and a spring plate.

[0010] Preferably, through holes for the rope to pass through are evenly spaced at both upper and lower ends of the profiling plate, and pin holes for the pins to pass through are evenly spaced at both left and right ends of the profiling plate.

[0011] Preferably, the elastic outer covering layer is a rubber ring or a sponge ring.

[0012] Preferably, step one specifically includes the following steps: S1. Prepare in advance a wooden model with the same appearance as the wood to be laminated with the veneer, place the veneer with the craft edge retained on the wooden model, fix the craft edge of the veneer on the wooden model with pins, and then place the wooden model with the veneer fixed on a flat surface; S2. Place the profiling plate in 60-70°C hot water to soften it completely, and then take it out; S3, placing the completely softened profiling board on the veneer of the wooden model, and shaping the completely softened profiling board so that the profiling board completely fits the veneer; S4. After the profiling board is shaped, use a cold air blower to continuously cool the profiling board for 5 to 10 minutes. After the profiling board is hardened and shaped, remove the profiling board and the facing.

[0013] Preferably, step 2 specifically includes the following steps: S1. After the hardening and shaping is completed, the profiling board is evenly wrapped with a heat insulation tape, and the end of the heat insulation tape is pasted to the profiling board after ensuring that the heat insulation tape is away from the profiling board for a certain distance; S2. After the contour board is wrapped, put the contour board into the containing bag, make sure that the part of the contour board that is not attached to the thermal insulation tape is outside the containing bag, then put the containing bag with the bag opening facing upward in 60-70° C. hot water to completely soften the containing bag, and then take out the containing bag; S3, shaping the completely softened containing bag so that the containing bag completely fits the contour plate; S4. After the bag is shaped, a cold air machine is used to continuously cool the bag for 5 to 10 minutes. After the bag is hardened and shaped, the portion of the heat-insulating tape located outside the bag is grasped to pull out the profiling plate, and the elastic filler is filled into the bag and then sealed.

[0014] The beneficial effects of the present invention are as follows: the method pre-bonds one end of the wood and one end of the veneer, pulls the wood through the bonding mechanism at a uniform speed, moves the veneer between the containing bag and the wood, and bonds the remaining portion of the veneer with a longer length to the wood, thereby ensuring the bonding quality of the veneer.

[0015] The edge of the profiling board can be used to flatten the surface of the veneer sheet to avoid wrinkles on the veneer surface. And because the profiling board fits the contour of the finished product, the edge of the profiling board flattens the veneer sheet and trims the veneer sheet at the same time, making the veneer sheet further fit the wooden column to ensure the quality of the veneer fitting.

[0016] It can replace manual work to apply veneer to solid wood columns, save manpower, and improve work efficiency and quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] The accompanying drawings further illustrate the present invention, but the embodiments in the accompanying drawings do not constitute any limitation to the present invention.

[0018] Figure 1 A schematic diagram of the structure provided by the present invention; Figure 2 A schematic diagram of the structure of a fixing bar provided in one embodiment of the present invention Figure 1 ; Figure 3 A schematic diagram of the structure of a fixing bar provided in one embodiment of the present invention Figure 2 ; Figure 4 A schematic structural diagram of a profiling plate provided in one embodiment of the present invention.

[0019] Reference numerals: contour plate 1, fixing strip 2, receiving bag 3, rope 4, roller 5 DETAILED DESCRIPTION

[0020] The specific implementation of the present invention is described in detail below in conjunction with the accompanying drawings. It should be understood that the specific implementation described here is only used to illustrate and explain the present invention, and is not used to limit the present invention.

[0021] It should be noted that, in the present invention, unless otherwise stated, when an element is referred to as being "fixed to" or "disposed on" another element, it may be directly on the other element or there may be an intermediate element at the same time. When an element is referred to as being "connected to" another element, it may be directly connected to the other element or there may be an intermediate element at the same time. The directional words used, such as "upper, lower, left, right" generally refer to the position of the element. Figure 1 "Inside and outside" refer to the inside and outside of a specific outline. "Far and near" refer to the far and near relative to a certain component.

[0022] A method for laminating a solid wood veneer provided by an embodiment of the present invention comprises the following steps: Step 1: Shape the profiling board 1 according to the veneer and the appearance of the wood. After the profiling board 1 is hardened and shaped, remove the profiling board 1 and the veneer; Step 2: Place the profiling plate 1 into the containing bag 3, shape the containing bag 3 according to the appearance of the profiling plate 1, and after the containing bag 3 is hardened and shaped, take out the profiling plate 1, fill the containing bag 3 with elastic filling material, and then seal it; Step 3: Determine the number of rollers 5 according to the specifications of the wood to be laminated, pass the rope 4 through each roller 5, pass both ends of the rope 4 through the profiling plate 1 and bind them, install the profiling plate 1 to the fixing strip 2, and install the fixing strip 2 to the middle of the receiving bag 3; Step 4: fix the process edge of one end of the facing to the profiling plate 1 by means of a pin, and clamp and fix the profiling plate 1; Step 5: Apply glue evenly to the part of the wood to be bonded with the veneer. After the glue is applied, insert one end of the wood into the rope 4 so that the craft edge of the veneer is clamped between the roller 5 on the rope 4 and the surface of the wood that does not need to be bonded with the veneer. Adjust the position of the wood so that the wood and the end of the veneer are aligned, and bond the wood to one end of the veneer. Step 6: Remove the pin, pull the end of the wood and the veneer at a constant speed, and pass the remaining parts of the wood and the veneer through the receiving bag 3 and the rope 4; Step 7: After lamination, cut off the process edge of the veneer; The method of laminating solid wood veneer depends on Figure 1-Figure 4The bonding is performed using the bonding mechanism shown in the figure: the solid wood veneer bonding mechanism includes: a rope 4, a roller 5, a receiving bag 3, an elastic filling material, a fixing strip 2 and a profiling plate 1, the rope 4 is penetrated by a plurality of rollers 5, the roller 5, the receiving bag 3, the fixing strip 2 and the profiling plate 1 are sequentially arranged along a straight line, the fixing strip 2 is fixed to the middle part of the outer surface of the receiving bag 3, the elastic filling material is filled in the receiving bag 3, both ends of the profiling plate 1 are detachably arranged on the fixing strip 2, both ends of the rope 4 are penetrated by the thermoplastic plate, the two ends of the rope 4 are detachably connected to each other, and the profiling plate 1 is a thermoplastic plate.

[0023] The outer surface of the wood is parallel to the center line of the wood, and the profiling board 1 after hardening and shaping is parallel to the moving direction of the wood.

[0024] The containing bag 3 is a thermoplastic plastic bag, and the elastic filler is rubber particles.

[0025] The rope 4 is a metal rope or a plastic rope with plastic deformation ability. The rope 4 is detachably provided with two limiting elements, and the roller 5 is arranged between the two limiting elements. The rope 4 is made of twisted steel wires. The rope 4 can also be made of a thermoplastic plastic rope. A clothespin can be used as a limiting element, and the roller 5 is limited by clamping a specific position on the rope 4 with the clothespin. Two permanent magnets can be used as limiting elements, and the two permanent magnets attract each other and clamp a specific position on the rope 4 to limit the roller 5. A knot can be directly tied on the rope 4 as a limiting element to limit the roller 5 between two rope sections.

[0026] The fixing plate is connected to the containing bag 3 by Velcro or double-sided tape.

[0027] The roller 5 includes a cylinder and an elastic outer coating. The cylinder is rotatably arranged on the rope 4. The elastic outer coating is sleeved on the outer surface of the cylinder. The difference between the outer diameter and the inner diameter of the roller 5 is equal to the thickness of the process edge.

[0028] Both ends of the fixing strip 2 are bent to provide clamping plates, and both ends of the profiling plate 1 are detachably arranged on the fixing strip 2 through the clamping plates. The fixing strip 2 is any one of a thermoplastic plate, a memory metal plate and a spring plate.

[0029] The upper and lower ends of the profiling plate 1 are evenly spaced apart with through holes for the rope 4 to pass through, and the left and right ends of the profiling plate 1 are evenly spaced apart with pin holes for the pins to pass through.

[0030] The elastic outer covering layer is a rubber ring or a sponge ring.

[0031] Step 1 specifically includes the following steps: S1. Prepare in advance a wooden model with the same appearance as the wood to be laminated with the veneer, place the veneer with the craft edge retained on the wooden model, fix the craft edge of the veneer on the wooden model with pins, and then place the wooden model with the veneer fixed on a flat surface; S2, placing the profiling plate 1 in 60-70°C hot water to soften it completely, and then taking it out; S3, placing the completely softened profiling board 1 on the facing surface of the wooden model, and shaping the completely softened profiling board 1 so that the profiling board 1 completely fits the facing surface; S4. After the profiling board 1 is shaped, a cold air blower is used to continuously cool the profiling board for 15 to 10 minutes. After the profiling board 1 is hardened and shaped, the profiling board 1 is removed and the facing is removed.

[0032] Step 2 specifically includes the following steps: S1, after the hardening and shaping is completed, the profiling board 1 is evenly wrapped with a heat-insulating tape, and the end of the heat-insulating tape is pasted to the profiling board 1 after ensuring that the heat-insulating tape is away from the profiling board 1 for a certain distance; S2. After the profiling board 1 is wrapped, the profiling board 1 is placed in the receiving bag 3, ensuring that the portion of the profiling board 1 that is not attached to the thermal insulation tape is located outside the receiving bag 3, and then the receiving bag 3 is placed in 60-70° C. hot water with the bag opening facing upward to completely soften the receiving bag 3, and then the receiving bag 3 is taken out; S3, shaping the completely softened containing bag 3 so that the containing bag 3 completely fits the contour plate 1; S4. After the containing bag 3 is shaped, a cold air machine is used to continuously cool the containing bag for 35 to 10 minutes. After the containing bag 3 is hardened and shaped, the portion of the thermal insulation tape located outside the containing bag 3 is grasped and the contour plate 1 is pulled out. The thermal insulation tape is removed from the contour plate 1, and the elastic filler is filled into the containing bag 3 and then sealed.

[0033] The technical features of the above-mentioned embodiments can be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above-mentioned embodiments are described. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which should be considered as the scope of this specification.

Claims

1. A method for laminating solid wood veneer, characterized in that: The following steps are involved: Step 1: Shape the profiling board according to the veneer and the appearance of the wood. After the profiling board is hardened and shaped, remove the profiling board and the veneer; Step 2: Place the profiling plate into the containing bag, shape the containing bag according to the appearance of the profiling plate, and after the containing bag is hardened and shaped, take out the profiling plate, fill the containing bag with elastic filling material, and then seal it; Step 3: Determine the number of rollers according to the specifications of the wood to be laminated, pass the rope through each roller, pass both ends of the rope through the profiling board and bind them, install the profiling board to the fixing bar, and install the fixing bar to the middle of the receiving bag; Step 4: Fix the process edge of one end of the facing to the profiling board through pins, and clamp and fix the profiling board; Step 5: Apply glue evenly to the part of the wood to be bonded with the veneer. After the glue is applied, put one end of the wood into the rope so that the craft edge of the veneer is clamped between the roller on the rope and the surface of the wood that does not need to be bonded with the veneer. Adjust the position of the wood so that the wood and the end of the veneer are aligned, and bond the wood to one end of the veneer. Step 6: Remove the pins, pull the end of the wood and the veneer at a constant speed, and pass the rest of the wood and the veneer through the bag and the rope; Step 7: After lamination, cut off the process edge of the veneer; The solid wood veneer laminating method relies on the laminating mechanism described below for laminating: the solid wood veneer laminating mechanism includes: ropes, rollers, a containing bag, elastic filling materials, fixed strips and contour plates, the ropes are penetrated by a plurality of rollers, the rollers, the containing bag, fixed strips and contour plates are arranged in sequence along a straight line, the fixed strips are fixed to the middle of the outer surface of the containing bag, the elastic filling materials are filled in the containing bag, both ends of the contour plates are detachably arranged on the fixed strips, both ends of the ropes are penetrated by thermoplastic plates, the two ends of the ropes are detachably connected to each other, and the contour plates are thermoplastic plates.

2. The solid wood veneer laminating method according to claim 1, characterized in that: The outer surface of the wood is parallel to the center line of the wood, and the moving direction of the profiling board and the wood after hardening and shaping is parallel to each other.

3. The method for attaching solid wood veneer according to claim 1, characterized in that: The containing bag is a thermoplastic plastic bag, and the elastic filler is rubber particles.

4. The method for attaching solid wood veneer according to claim 1, characterized in that: The rope is a metal rope or a plastic rope with plastic deformation capability. The rope is detachably provided with two limiting elements, and the rollers are arranged between the two limiting elements.

5. The method for attaching solid wood veneer according to claim 1, characterized in that: The roller comprises a cylinder and an elastic outer coating, the cylinder is rotatably arranged on the rope, the elastic outer coating is sleeved on the outer surface of the cylinder, and the difference between the outer diameter and the inner diameter of the roller is equal to the thickness of the process edge.

6. The method for attaching solid wood veneer according to claim 1, characterized in that: Both ends of the fixing strip are bent to provide clamping plates, and both ends of the profiling plate are detachably arranged on the fixing strip through the clamping plates. The fixing strip is any one of a thermoplastic plate, a memory metal plate and a spring plate.

7. The method for attaching solid wood veneer according to claim 1, characterized in that: The upper and lower ends of the profiling plate are evenly spaced to be provided with through holes for the rope to pass through, and the left and right ends of the profiling plate are evenly spaced to be provided with pin holes for the pin to pass through.

8. The method for attaching solid wood veneer according to claim 1, characterized in that: The elastic outer covering layer is a rubber ring or a sponge ring.

9. The method for attaching solid wood veneer according to claim 1, characterized in that: Step 1 specifically includes the following steps: S1. Prepare in advance a wooden model with the same appearance as the wood to be laminated with the veneer, place the veneer with the craft edge retained on the wooden model, fix the craft edge of the veneer on the wooden model with pins, and then place the wooden model with the veneer fixed on a flat surface; S2. Place the profiling plate in 60-70°C hot water to soften it completely, and then take it out; S3, placing the completely softened profiling board on the veneer of the wooden model, and shaping the completely softened profiling board so that the profiling board completely fits the veneer; S4. After the profiling board is shaped, use a cold air blower to continuously cool the profiling board for 5 to 10 minutes. After the profiling board is hardened and shaped, remove the profiling board and the facing.

10. The solid wood veneer laminating method according to claim 1, characterized in that: Step 2 specifically includes the following steps: S1. After the hardening and shaping is completed, the profiling board is evenly wrapped with a heat insulation tape, and the end of the heat insulation tape is pasted to the profiling board after ensuring that the heat insulation tape is away from the profiling board for a certain distance; S2. After the contour board is wrapped, put the contour board into the containing bag, make sure that the part of the contour board that is not attached to the thermal insulation tape is outside the containing bag, then put the containing bag with the bag opening facing upward in 60-70° C. hot water to completely soften the containing bag, and then take out the containing bag; S3, shaping the completely softened containing bag so that the containing bag completely fits the contour plate; S4. After the bag is shaped, a cold air machine is used to continuously cool the bag for 5 to 10 minutes. After the bag is hardened and shaped, the portion of the heat-insulating tape located outside the bag is grasped to pull out the profiling plate, and the elastic filler is filled into the bag and then sealed.

Citation Information

Patent Citations

  • Furniture manufacturing composite board surface veneer attachment machining technology

    CN111391057A

  • Veneer sticking equipment for wood processing

    CN111702882A

  • Wood veneer fitting device

    CN114474258A

  • Carrier film pasting jig