Process method for synthesizing hydroquinone by taking nitrobenzene as raw material

A two-step nitrobenzene-based hydroquinone synthesis process addresses inefficiencies in existing methods by using a catalyst system to directly utilize intermediate products, achieving high purity and reducing environmental impact and costs.

CN119080585APending Publication Date: 2024-12-06YUMEN HAIDING CHEMICAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411214556.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-01
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

Existing hydroquinone synthesis methods face issues such as high pollution, low conversion rates, high energy consumption, and difficulty in separating by-products, necessitating the development of a more efficient and environmentally friendly process.

Method used

A two-step reaction process using nitrobenzene as a raw material, involving a catalyst system with Pt/Ni/Pd/Cu loaded activated carbon and phase transfer catalysts, reduces intermediate product purification steps by directly utilizing the first-step product in the second-step hydrolysis, optimizing reaction conditions and extraction methods.

Benefits of technology

The process achieves high purity products with improved raw material utilization, reduced wastewater generation, and lower energy consumption, making it suitable for industrial applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119080585A_ABST
    Figure CN119080585A_ABST
Patent Text Reader

Abstract

The invention discloses a process method for synthesizing hydroquinone by taking nitrobenzene as a raw material, and relates to the technical field of chemical synthesis processes, and the process method comprises the following steps: S1, uniformly mixing nitrobenzene, sulfuric acid, deionized water, a catalyst and a phase transfer catalyst through a stirrer; s2, replacing gas in the reaction kettle with nitrogen until the oxygen content is less than or equal to 0.5%, raising the temperature and pressure of the reaction kettle to 50-99 DEG C, raising the pressure to 0.1-3 MPa, and introducing hydrogen at the pressure of 0.1-3 MPa; s3, keeping the temperature and the pressure, reacting for 1-24 hours, stopping introducing hydrogen, reducing the pressure to normal pressure, replacing with nitrogen, cooling, filtering the material while the material is hot, taking the filtered filtrate as a crude product of p-aminophenol for later use, and drying the filter residue to serve as a catalyst for later use; the process method provided by the invention has the advantages of low raw material price, high selectivity of the hydroquinone product, good stability, simple process flow, small fixed asset investment limit and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of chemical synthesis technology, in particular to a process for synthesizing hydroquinone by taking nitrobenzene as a raw material. Background Art

[0002] Hydroquinone is an important raw material for rubber, medicine, dyes, pesticides and fine chemicals. It is mainly used in the preparation of black-and-white developers for photographic films, the production of anthraquinone dyes and azo dyes, catalysts for synthetic gas desulfurization processes, antioxidants for rubber and plastics, monomer inhibitors, stabilizers and antioxidants for food and paint varnishes, and petroleum anticoagulants.

[0003] The application field of hydroquinone is still gradually expanding. There are many methods for its synthesis. So far, there are more than 10 methods, among which the aniline oxidation method, phenol hydroxylation method, diazotization method, hydrogen peroxide oxidation phenol method, etc. have been industrialized. The aniline oxidation method has a mature process and low raw material cost, but the process is cumbersome and the "three wastes" pollution is particularly serious. It has been eliminated abroad and will be gradually eliminated in China in the future; the raw materials of the phenol hydroxylation method are simple and easy to obtain.

[0004] The "three wastes" have less pollution, but the conversion rate of phenol is low, resulting in a large circulation of phenol, high energy consumption, and low equipment utilization. The conversion rate and reaction selectivity directly depend on the choice of catalyst. Although the conversion rate is high for the preparation of p-aminophenol by diazotization hydrolysis, the production process of this process is long, and the diazotization reaction needs to be carried out at low temperature. Overheating can easily cause production accidents, and it is also one of the key chemical processes announced by the state. In recent years, the method of producing hydroquinone by hydrogen peroxide oxidation of phenol has developed rapidly. Most of the products of this method are catechol, and the yield of hydroquinone is not particularly stable. There are many resorcinol and other by-products, and the product structure is close, which makes it difficult to separate. Therefore, it is urgent to expand other process methods to meet market demand.

[0005] In view of this, a process for synthesizing hydroquinone using nitrobenzene as a raw material is provided to overcome the above-mentioned problems, aiming at synthesizing hydroquinone from nitrobenzene through a two-step reaction, utilizing the material in the first step reaction, without the need to purify the reaction intermediate product, and directly utilizing the material in the previous step reaction to complete the second step of the hydrolysis process of p-aminophenol, thereby reducing the generation of production wastewater in the intermediate step and improving the utilization efficiency of the raw materials. Summary of the invention

[0006] The object of the present invention is to provide a method for controlling line losses in power transmission and distribution lines and substations, so as to solve the problems raised in the above-mentioned background technology.

[0007] In order to solve the above technical problems, the present invention provides a process for synthesizing hydroquinone using nitrobenzene as a raw material, comprising the following steps:

[0008] S1. Mix nitrobenzene, sulfuric acid, deionized water, catalyst and phase transfer catalyst uniformly by a stirrer;

[0009] S2. Replace the gas in the reactor with nitrogen until the oxygen content is ≤0.5%, raise the temperature and pressure of the reactor to 50°C to 99°C, raise the pressure to 0.1MPa to 3MPa, and introduce hydrogen to a pressure of 0.1MPa to 3MPa;

[0010] S3, maintaining the temperature and pressure for 1h to 24h, then stop introducing hydrogen, reduce the pressure to normal pressure and replace with nitrogen, cool and filter the material while hot, and use the filtrate after filtration as a crude product of p-aminophenol for standby use, and use the filter residue as a catalyst for standby use after drying;

[0011] S4, put the filtrate into the reactor, add a small amount of demulsifier, start the agitator to mix evenly;

[0012] S5, introducing nitrogen into the reactor to replace the oxygen content until the oxygen content is ≤0.5%, and raising the temperature and pressure;

[0013] S6, keep the reaction material warm for 1h to 24h, then cool it to 30℃ to 50℃ and discharge it;

[0014] S7, add activated carbon and hydrosulfite to the reaction solution in sequence, raise the temperature to 50°C to 99°C again, and reflux for 0.5h to 5h;

[0015] S8, filtering the material while hot, extracting the obtained filtrate with an extractant, and collecting the extract after multiple extractions;

[0016] S9. The extract is distilled and cooled at the top to obtain the extractant and the product aniline, and the product hydroquinone is obtained at the bottom of the still.

[0017] Furthermore, in S1, the mass ratio of nitrobenzene: sulfuric acid (98.3%): deionized water: catalyst: phase transfer catalyst is (based on nitrobenzene) 1: (0.5-5): (1-10): (0.004-0.1): (0.0001-0.1).

[0018] Further, in S1, the catalyst used is Pt / Ni / Pd / Cu loaded activated carbon as the catalyst; the activated carbon is activated by nitric acid, the mass fraction of nitric acid is 10-30%, the mass ratio of activated carbon to nitric acid is 1:1-1:9, the soaking time is 1-10h, and it is washed with deionized water to neutrality and then dried at 100℃-350℃ for use; then the dried activated carbon is impregnated with a mixed solution of H2PtCl6 / CuCl / H2O in the ratio of 1mL:1ml:100g-100ml:100ml:100g, the constant temperature is 40-95℃, the stirring time is 1-10h, and the filter residue is dried at 100-350℃ after filtration. The dried activated carbon catalyst is used as the base catalyst, and then H2PdCl4 / Ni(NO3)2 / H2O is prepared in the ratio of 1mL:1ml:100g-100m The dried activated carbon-based catalyst is impregnated with a mixed solution of l:100ml:100g, the constant temperature is 40-95°C, and the stirring time is 1-10h. After the impregnation is completed, the activated carbon catalyst is dried at 100-350°C for standby use.

[0019] Furthermore, in S1, the phase transfer catalyst is one or two of tetraethylammonium bromide, dodecyltrimethylammonium bromide, dodecyltrimethylammonium chloride, and hexadecyltrimethylammonium bromide, and the amount of the phase transfer catalyst added is 0.01% to 5% of the total volume, so that nitrobenzene and sulfuric acid form a homogeneous mixed solution.

[0020] Further, in S3, the temperature is lowered to 50°C and the reaction material is filtered.

[0021] Furthermore, in S3, the filter residue is dried in a vacuum system at a temperature of 100°C to 350°C.

[0022] Furthermore, in S4, the demulsifier is one or two of polyoxyethylene polyoxypropylene octadecyl alcohol ether, polyoxyethylene polyoxypropylene polyether, polyoxyethylene polyoxypropylene polyether, polyacrylamide, and polyaluminum chloride, and the usage amount is 10ppm to 1000ppm.

[0023] Further, in S5, the molar ratio of sulfuric acid to p-aminophenol is detected to be 1:(0.5-5), sulfuric acid needs to be supplemented when the content of sulfuric acid is insufficient, and deionized water needs to be used to dilute the sulfuric acid when the content exceeds the specified molar ratio. Then, the gas in the reactor is replaced with nitrogen to an oxygen content of ≤0.5%, and the reactor is heated to 150°C-400°C and the pressure is increased to 1MPa-5MPa.

[0024] Furthermore, in S8, the extractant used is one of acetone, butanone, dichloromethane, 4-methyl-2-pentanone (MIBK), diisobutyl (methyl) ketone (DIBK) and the like, and the extractant is added to the reaction solution in multiple times for extraction.

[0025] Furthermore, in S9, the extract is distilled by pressurized, normal pressure and reduced pressure distillation, the distillation temperature is 60°C to 350°C, the extractant and the product aniline are recovered at the top of the distillation kettle, the product hydroquinone is obtained in the bottom of the distillation tower, the extractant is recycled, the purity of the aniline product is 91.5% to 97.2%, and the purity of the hydroquinone product is 94.4% to 99.

[0026] Compared with the prior art, the present invention has the following beneficial effects:

[0027] In the present invention, the raw material of nitrobenzene is widely available and inexpensive. The process route for synthesizing nitrobenzene through the reaction of nitrobenzene is the greenest, most environmentally friendly and safest synthesis process. The process route of the present invention reduces the refining step of the intermediate product p-aminophenol, and directly uses the material obtained after the first step of nitrobenzene hydrogenation to carry out the second step of hydrolysis reaction. Therefore, the utilization rate of the material is high, the waste is small, and the two products produced have high industrial added value. The process route of the present invention is a process synthesis route worthy of promotion. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] The accompanying drawings are part of the present invention and are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention, but do not constitute an improper limitation of the present invention. Obviously, the drawings described below are only some embodiments. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work. In the accompanying drawings:

[0029] Figure 1 The present invention is a flow chart of a process for synthesizing hydroquinone using nitrobenzene as a raw material.

[0030] It should be noted that these drawings and textual descriptions are not intended to limit the conceptual scope of the present invention in any way, but are intended to illustrate the concept of the present invention for those skilled in the art by referring to specific embodiments. DETAILED DESCRIPTION

[0031] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. The following embodiments are used to illustrate the present invention, but are not used to limit the scope of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0032] See also Figure 1 :

[0033] Preparation stage: Activate the commercially available Pt / Ni / Pd / Cu loaded activated carbon with nitric acid, the mass fraction of nitric acid used to activate the activated carbon is 10-30%, the mass ratio of activated carbon to nitric acid is 1:1-1:9, the soaking time is 1-10 hours, wash with deionized water and dry for use. Then, H2PtCl6 / CuCl / H2O is prepared into a mixed solution in the ratio of 1mL:1ml:100g~100ml:100ml:100g to impregnate the dried activated carbon, the constant temperature is 40~95℃, the stirring time is 1~10h, and the filter residue is dried after filtration. The dried activated carbon catalyst is used as the base catalyst, and then H2PdCl4 / Ni(NO3)2 / H2O is prepared into a mixed solution in the ratio of 1mL:1ml:100g~100ml:100ml:100g to impregnate the dried activated carbon base catalyst, the constant temperature is 40~95℃, the stirring time is 1~10h, and the activated carbon catalyst is dried for use after impregnation.

[0034] Conduct a gas tightness test on the reactor with nitrogen in advance to confirm that there are no leaks;

[0035] After the above preparation stage is completed, the following implementation method is followed, including:

[0036] Embodiment 1:

[0037] Raw material ratio:

[0038] Nitrobenzene: 100g;

[0039] Sulfuric acid: 50g;

[0040] Deionized water: 500g;

[0041] Catalyst (Pt / Ni / Pd / Cu supported activated carbon): 0.05 g;

[0042] Phase transfer catalyst (tetraethylammonium bromide): 0.5 g (calculated as 0.5% of the total volume);

[0043] Catalyst preparation:

[0044] Activation of activated carbon: Use 20% nitric acid by mass, the mass ratio of activated carbon to nitric acid is 1:5, soak for 5 hours, wash to neutrality, and dry at 200°C.

[0045] Impregnation: first impregnate with H2PtCl6 / CuCl / H2O (10mL:10mL:100g), keep the temperature at 60℃, stir for 5h, and dry; then impregnate with H2PdCl4 / Ni(NO3)2 / H2O (10mL:10mL:100g), and treat under the same conditions.

[0046] Reaction conditions:

[0047] Replacement gas: Replace with nitrogen until the oxygen content is ≤ 0.5%.

[0048] Temperature and pressure increase: temperature to 70℃, pressure to 1MPa.

[0049] Introduce hydrogen: maintain the pressure at 1 MPa.

[0050] Reaction time: 10h.

[0051] Subsequent processing:

[0052] Demulsifier: Polyoxyethylene polyoxypropylene octadecyl alcohol ether, dosage is 100ppm.

[0053] Sulfuric acid adjustment: Check and adjust the molar ratio of sulfuric acid to p-aminophenol to 1:2.

[0054] Temperature and pressure increase: temperature increased to 250°C, pressure increased to 3MPa.

[0055] Insulation time: 8h.

[0056] Extraction: Use dichloromethane as the extractant and extract multiple times.

[0057] Distillation: atmospheric distillation is adopted, and the distillation temperature is 150°C, and the extractant and the product aniline are recovered to obtain hydroquinone.

[0058] Effect:

[0059] The product has high purity, with aniline product purity of 95% and hydroquinone product purity of 97%.

[0060] The catalyst has high efficiency, short reaction time and low energy consumption.

[0061] By optimizing the process route of the present invention, the conversion rate of hydroquinone calculated with nitrobenzene is 53.8%, and the selectivity is 98.7%.

[0062] Embodiment 2:

[0063] Raw material ratio:

[0064] Nitrobenzene: 100g;

[0065] Sulfuric acid: 30g;

[0066] Deionized water: 800g;

[0067] Catalyst (Pt / Ni / Pd / Cu supported activated carbon): 0.03 g;

[0068] Phase transfer catalyst (dodecyltrimethylammonium bromide): 0.3 g (

[0069] Calculated as 0.3% of the total volume);

[0070] Catalyst preparation:

[0071] Activation of activated carbon: Use 15% nitric acid by mass, the mass ratio of activated carbon to nitric acid is 1:3, soak for 8 hours, wash to neutrality, and dry at 150°C.

[0072] Impregnation: first impregnate with H2PtCl6 / CuCl / H2O (5mL:5mL:100g), keep constant temperature at 70℃, stir for 8h, and dry; then impregnate with H2PdCl4 / Ni(NO3)2 / H2O (5mL:5mL:100g), and treat under the same conditions.

[0073] Reaction conditions:

[0074] Replacement gas: Replace with nitrogen until the oxygen content is ≤ 0.5%.

[0075] Temperature and pressure increase: temperature to 80℃, pressure to 2MPa.

[0076] Introduce hydrogen: maintain the pressure at 2MPa.

[0077] Reaction time: 15h.

[0078] Subsequent processing:

[0079] Demulsifier: Polyoxyethylene polyoxypropylene polyether, dosage is 500ppm.

[0080] Sulfuric acid adjustment: Check and adjust the molar ratio of sulfuric acid to p-aminophenol to 1:3.

[0081] Temperature and pressure increase: temperature increased to 300°C, pressure increased to 4MPa.

[0082] Insulation time: 12h.

[0083] Extraction: Use MI BK as the extraction agent and extract multiple times.

[0084] Distillation: Use vacuum distillation at a distillation temperature of 200°C to recover the extractant and product aniline to obtain hydroquinone.

[0085] Effect:

[0086] The product has high purity, with the purity of aniline product being 96% and that of hydroquinone product being 98%.

[0087] The reaction conditions are mild, the operation is simple, and it is suitable for industrial production.

[0088] By optimizing the process route of the present invention, the conversion rate of hydroquinone calculated with nitrobenzene is 63.5%, and the selectivity of hydroquinone is 99%.

[0089] Embodiment three:

[0090] Raw material ratio:

[0091] Nitrobenzene: 100g;

[0092] Sulfuric acid: 70g;

[0093] Deionized water: 400g;

[0094] Catalyst (Pt / Ni / Pd / Cu supported activated carbon): 0.02 g;

[0095] Phase transfer catalyst (tetrabutylammonium bromide): 0.2 g (calculated as 0.2% of the total volume);

[0096] Catalyst preparation:

[0097] Activation of activated carbon: Use 10% nitric acid with a mass ratio of activated carbon to nitric acid of 1:4, soak for 4 hours, wash to neutrality, and dry at 100°C.

[0098] Impregnation: first impregnate with H2PtCl6 / CuCl / H2O (8mL:8mL:100g), keep the temperature at 50℃, stir for 3h, and dry; then impregnate with H2PdCl4 / Ni(NO3)2 / H2O (8mL:8mL:100g) and treat under the same conditions.

[0099] Reaction conditions:

[0100] Replacement gas: Replace with nitrogen until the oxygen content is ≤1%.

[0101] Temperature and pressure increase: temperature to 60℃, pressure to 0.5MPa.

[0102] Introduce hydrogen: maintain the pressure at 0.5 MPa.

[0103] Reaction time: 18h.

[0104] Subsequent processing:

[0105] Demulsifier: Polyoxyethylene polyoxypropylene ether, dosage is 300ppm.

[0106] Sulfuric acid adjustment: Check and adjust the molar ratio of sulfuric acid to p-aminophenol to 1:1.5.

[0107] Temperature and pressure increase: temperature increased to 200°C, pressure increased to 2MPa.

[0108] Insulation time: 6h.

[0109] Extraction: Use ethyl acetate as the extractant and extract multiple times.

[0110] Distillation: Use vacuum distillation at a distillation temperature of 100°C to recover the extractant and product aniline to obtain hydroquinone.

[0111] Effect:

[0112] The product purity is relatively low, with the purity of aniline product being 90% and the purity of hydroquinone product being 93%.

[0113] The catalyst efficiency is low, the reaction time is long, and the energy consumption is high.

[0114] By optimizing the process route of the present invention, the conversion rate of hydroquinone calculated with nitrobenzene is 59.2%, and the selectivity is 98.3%.

[0115] Compare:

[0116] Compared with Example 2, the product purity of Example 3 is lower, the reaction conditions are not mild enough, and the catalyst efficiency is also lower, resulting in higher production costs and lower production efficiency. Therefore, Example 3 is not as good as Example 2; similarly, Example 1 is not as good as Example 2.

[0117] Best embodiment:

[0118] Embodiment 2 is the best embodiment because it not only has high product purity, but also has relatively mild reaction conditions, is easy to operate, and is more suitable for large-scale industrial production. In addition, the catalyst efficiency in Embodiment 2 is also high, that is, the conversion rate and selectivity of hydroquinone are high, which helps to reduce production costs and improve production efficiency.

[0119] Summarize:

[0120] Two-step reaction synthesis process:

[0121] In the first step of the reaction, nitrobenzene, sulfuric acid, deionized water, catalyst, and phase transfer catalyst are added to the reactor, stirred evenly, and then nitrogen replacement, hydrogen introduction, temperature and pressure increase, etc. are performed. After a period of reaction, hydrogen introduction is stopped, the pressure is reduced, nitrogen replacement is performed, the temperature is lowered, and filtration is performed. The filtrate is used as a crude p-aminophenol product for standby use, and the filter residue is dried and recycled as a catalyst.

[0122] In the second step, the filtrate from the first step is put into the reactor, and after adding the demulsifier, nitrogen replacement, temperature and pressure are performed again. Then, the reaction liquid is kept warm and discharged, and activated carbon and hydrosulfite are added to the reaction liquid in sequence, and the temperature is raised and refluxed. Then, the filtrate is filtered while hot, and the filtrate is extracted with an extractant. After multiple extractions, the extract is collected. Finally, the extract is distilled, and the extractant and product aniline are obtained by cooling at the top, and the product hydroquinone is obtained at the bottom of the distillation kettle.

[0123] Direct use of intermediate products: In traditional processes, it is usually necessary to purify the intermediate products of the reaction, which not only increases the complexity of the process flow, but also consumes a lot of resources and energy, and produces a lot of wastewater. However, this process directly uses the materials from the first step reaction for the second step of the hydrolysis process of p-aminophenol, without the need to purify the intermediate products, which greatly simplifies the process flow.

[0124] Reduce production wastewater:

[0125] Omitting the refining process: Since there is no need to purify the intermediate products, the large amount of wastewater generated in the traditional refining process is avoided. This is an important environmental improvement for chemical production and meets the development requirements of modern green chemical industry.

[0126] Reduce environmental pressure: Reducing the generation of wastewater in intermediate steps will help reduce the cost and pressure of enterprises in wastewater treatment, while also reducing pollution to the environment, with good social and ecological benefits.

[0127] Improve the efficiency of raw material utilization:

[0128] Full utilization of materials: Directly use the materials from the previous step for the next step, so that the raw materials are fully utilized in the entire process. There is no loss in the refining process of intermediate products, which improves the utilization rate of raw materials and reduces production costs.

[0129] Optimal allocation of resources: This efficient way of utilizing raw materials realizes the optimal allocation of resources, making limited resources more valuable. At the same time, it also improves the economic benefits and market competitiveness of enterprises.

[0130] In summary, the process of synthesizing hydroquinone from nitrobenzene through a two-step reaction has the advantages of reducing wastewater generation and improving raw material utilization efficiency, providing a new efficient, environmentally friendly and economical method for the synthesis of hydroquinone, which has broad application prospects.

[0131] The above description is only a preferred embodiment of the present invention, and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technician familiar with this patent can make some changes or modifications to equivalent embodiments of equivalent changes by using the technical content suggested above without departing from the scope of the technical solution of the present invention. The implementation scheme in the above embodiment can also be further combined or replaced. However, any simple modification, equivalent change and modification made to the above embodiment based on the technical essence of the present invention without departing from the content of the technical solution of the present invention still falls within the scope of the solution of the present invention.

Claims

1. A process for synthesizing hydroquinone using nitrobenzene as a raw material, characterized in that: The following steps are involved: S1. Mix nitrobenzene, sulfuric acid, deionized water, catalyst and phase transfer catalyst uniformly by a stirrer; S2. Replace the gas in the reactor with nitrogen until the oxygen content is ≤0.5%, raise the temperature and pressure of the reactor to 50°C to 99°C, raise the pressure to 0.1MPa to 3MPa, and introduce hydrogen to a pressure of 0.1MPa to 3MPa; S3, maintaining the temperature and pressure for 1h to 24h, then stop introducing hydrogen, reduce the pressure to normal pressure and replace with nitrogen, cool and filter the material while hot, and use the filtrate after filtration as a crude product of p-aminophenol for standby use, and use the filter residue as a catalyst for standby use after drying; S4, put the filtrate into the reactor, add a small amount of demulsifier, start the agitator to mix evenly; S5, introducing nitrogen into the reactor to replace the oxygen content until the oxygen content is ≤0.5%, and raising the temperature and pressure; S6, keep the reaction material warm for 1h to 24h, then cool it to 30℃ to 50℃ and discharge it; S7, add activated carbon and hydrosulfite to the reaction solution in sequence, and heat to 50°C to 99°C again, with a reflux time of 0.5h to 5h; S8, filtering the material while hot, extracting the obtained filtrate with an extractant, and collecting the extract after multiple extractions; S9. The extract is distilled and cooled at the top to obtain the extractant and the product aniline, and the product hydroquinone is obtained at the bottom of the still.

2. A process for synthesizing hydroquinone using nitrobenzene as a raw material as claimed in claim 1, characterized in that: In S1, the mass ratio of nitrobenzene: sulfuric acid (98.3%): deionized water: catalyst: phase transfer catalyst is (based on nitrobenzene) 1: (0.5-5): (1-10): (0.004-0.1): (0.0001-0.1).

3. A process for synthesizing hydroquinone using nitrobenzene as a raw material as claimed in claim 1, characterized in that: In S1, Pt / Ni / Pd / Cu-supported activated carbon was used as the catalyst; Activated carbon is activated by nitric acid, the mass fraction of nitric acid is 10-30%, the mass ratio of activated carbon to nitric acid is 1:1-1:9, the soaking time is 1-10h, washed with deionized water to neutrality and dried at 100℃-350℃ for standby use; then H2PtCl 6 / CuCl / H2O is prepared into a mixed solution in the ratio of 1mL:1ml:100g~100ml:100ml:100g to impregnate the dried activated carbon, the constant temperature is 40~95℃, the stirring time is 1~10h, and the filter residue is dried at 100~350℃ after filtration. The dried activated carbon catalyst is used as the base catalyst, and then H2PdCl4 / Ni(NO3)2 / H2O is prepared into a mixed solution in the ratio of 1mL:1ml:100g~100ml:100ml:100g to impregnate the dried activated carbon base catalyst, the constant temperature is 40~95℃, the stirring time is 1~10h, and after impregnation, the activated carbon catalyst is dried at 100~350℃ for use.

4. A process for synthesizing hydroquinone using nitrobenzene as a raw material as claimed in claim 1, characterized in that: In S1, the phase transfer catalyst is one or two of tetraethylammonium bromide, dodecyltrimethylammonium bromide, dodecyltrimethylammonium chloride, and hexadecyltrimethylammonium bromide, and the added amount of the phase transfer catalyst is added at a ratio of 0.01% to 5% of the total volume, so that nitrobenzene and sulfuric acid form a homogeneous mixed solution.

5. A process for synthesizing hydroquinone using nitrobenzene as a raw material as claimed in claim 1, characterized in that: In S3, the temperature is lowered to 50°C and the reaction material is filtered.

6. A process for synthesizing hydroquinone using nitrobenzene as a raw material as claimed in claim 1, characterized in that: In S3, the filter residue is dried in a vacuum system at a temperature of 100°C to 350°C.

7. A process for synthesizing hydroquinone using nitrobenzene as a raw material as claimed in claim 1, characterized in that: In S4, the demulsifier is one or two of polyoxyethylene polyoxypropylene octadecyl alcohol ether, polyoxyethylene polyoxypropylene polyether, polyoxyethylene polyoxypropylene polyether, polyacrylamide, and polyaluminum chloride, and the dosage is 10ppm to 1000ppm.

8. A process for synthesizing hydroquinone using nitrobenzene as a raw material as claimed in claim 1, characterized in that: In S5, the molar ratio of sulfuric acid to p-aminophenol is detected to be 1:(0.5-5). When the sulfuric acid content is insufficient, sulfuric acid needs to be supplemented. When the sulfuric acid exceeds the specified molar ratio, it needs to be diluted with deionized water. Then, the gas in the reactor is replaced with nitrogen to an oxygen content of ≤0.5%. The reactor is heated to 150° C.-400° C. and the pressure is increased to 1 MPa-5 MPa.

9. A process for synthesizing hydroquinone using nitrobenzene as a raw material as claimed in claim 1, characterized in that: In S8, the extractant used is one of acetone, butanone, dichloromethane, 4-methyl-2-pentanone (MIBK), diisobutyl (methyl) ketone (DIBK) and the like, and the extractant is added to the reaction solution in multiple times for extraction.

10. The process for synthesizing hydroquinone using nitrobenzene as a raw material as claimed in claim 1, characterized in that: In the above S9, the extract is distilled by pressurized, normal pressure and reduced pressure distillation, the distillation temperature is 60°C to 350°C, the extractant and the product aniline are recovered at the top of the distillation kettle, the product hydroquinone is obtained in the bottom of the distillation tower, the extractant is recycled, the purity of the aniline product is 91.5% to 97.2%, and the purity of the hydroquinone product is 94.4% to 99%.