Nickel-based superalloy ultimate tensile strength prediction model, modeling method, device and system
By establishing the ultimate tensile strength prediction model of nickel-based high-temperature alloy, combined with grain boundary, solid solution and γ' precipitation strengthening model, the problem of ultimate tensile strength prediction in additive manufacturing is solved, and the entire temperature range is achieved The high-efficiency component design improves the processing efficiency of nickel-based high-temperature alloys.
Patent Information
- Application Number
- CN202411222139.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-02
- Publication Date
- 2024-12-06
AI Technical Summary
The prior art is difficult to effectively predict the ultimate tensile strength of nickel-based high-temperature alloys in the additive manufacturing process, resulting in low component design efficiency, complex processing technology and low efficiency.
A nickel-based high-temperature alloy ultimate tensile strength prediction model was established. By introducing temperature variables and parameters, combining grain boundary strengthening, solid solution strengthening and γ' precipitation strengthening models, a yield strength model suitable for the full temperature range was established, and through Empirical formulas for the relationship between ultimate tensile strength and yield strength, and construct an ultimate tensile strength model for the full temperature range.
It improves the efficiency of nickel-based high-temperature alloy composition design, can accurately predict the ultimate tensile strength of nickel-based high-temperature alloy from room temperature to 1300K, supports the composition design of additive manufacturing, and improves processing efficiency and material utilization.
Smart Images

Figure CN119092019A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of mechanical technology of alloy composition design, and in particular to a nickel-based high-temperature alloy ultimate tensile strength prediction model, a nickel-based high-temperature alloy ultimate tensile strength modeling method, a nickel-based high-temperature alloy ultimate tensile strength modeling device and a nickel-based high-temperature alloy ultimate tensile strength modeling system. Background Art
[0002] Nickel-based superalloys are widely used in hot-end components such as gas turbines and aircraft engines because they can maintain good strength, creep resistance, fatigue resistance, oxidation resistance and corrosion resistance in high temperature environments. The unique performance comes from the unique microstructure, which includes multi-modal size distribution of L12 precipitates γ' and face-centered cubic (FCC) matrix γ. The excellent yield strength of nickel-based superalloys mainly comes from grain boundary strengthening, solid solution strengthening and γ' precipitation strengthening. Many researchers have studied these three strengthening methods and established relatively good models.
[0003] Due to the extremely complex use environment of the engine, the geometric morphology of parts made of nickel-based high-temperature alloys is also more complex. Although investment casting, as a traditional processing method, can be used for precision casting, the processing process is relatively complicated, the processing efficiency is relatively low, and there are certain limitations for the production of parts with complex shapes. Laser powder bed melting technology, as one of the additive manufacturing technologies, can process complex geometric shapes, can achieve fewer processing processes, has higher processing freedom and more efficient material utilization. However, considering the high temperature gradient, high cooling rate and cyclic heating-cooling process characteristics of laser powder bed melting technology, the microstructure of nickel-based high-temperature alloys formed by additive manufacturing will be different from that of nickel-based high-temperature alloys formed by traditional processes. Therefore, for the design of nickel-based high-temperature alloy composition in additive manufacturing, it is necessary to model the ultimate tensile strength of nickel-based high-temperature alloys for additive manufacturing forming processes.
[0004] Therefore, there is an urgent need for a new ultimate tensile strength model that can be applied to the composition design of nickel-based high-temperature alloys over the entire temperature range to improve the efficiency of the composition design of nickel-based high-temperature alloys. Summary of the invention
[0005] Therefore, in order to overcome at least some of the defects and shortcomings existing in the prior art, embodiments of the present invention provide a nickel-based high-temperature alloy ultimate tensile strength prediction model, a nickel-based high-temperature alloy ultimate tensile strength modeling method, a nickel-based high-temperature alloy ultimate tensile strength modeling device and a nickel-based high-temperature alloy ultimate tensile strength modeling system.
[0006] Specifically, on the one hand, an embodiment of the present invention provides a prediction model for the ultimate tensile strength of a nickel-based high-temperature alloy, characterized in that it includes: the calculation expression of the prediction model is:
[0007]
[0008] Where T is temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f γ′ is the volume fraction of γ' phase.
[0009] On the other hand, an embodiment of the present invention provides a prediction model, modeling method, device and system for the ultimate tensile strength of a nickel-based high-temperature alloy. The modeling method comprises: step 1: establishing a yield strength model for the composition design of a nickel-based high-temperature alloy according to the grain boundary strengthening contribution, solid solution strengthening contribution and γ' precipitation strengthening contribution models; step 2: introducing temperature variables and parameters, and establishing a yield strength model applicable to the entire temperature range according to the yield strength model; step 3: establishing an empirical formula for the relationship between ultimate tensile strength and yield strength; step 4: establishing an ultimate tensile strength model for the entire temperature range according to the yield strength model and the empirical formula for the relationship between ultimate tensile strength and yield strength; step 5: obtaining the coefficients of the new ultimate tensile strength model according to the ultimate tensile strength data in the composition design of the nickel-based high-temperature alloy; step 6: obtaining the ultimate tensile strength model formula of the nickel-based high-temperature alloy according to the coefficients and the new ultimate tensile strength model.
[0010] In a specific embodiment of the present invention, the step 5 specifically includes: step 5.1: obtaining the ultimate tensile strength data and alloy composition data of nickel-based high-temperature alloys with different compositions at different temperatures; step 5.2: calculating the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase and the volume fraction of the γ' strengthening phase in the nickel-based high-temperature alloy at different temperatures based on the alloy composition data; step 5.3: obtaining the coefficient based on the temperature, the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase, the volume fraction of the γ' strengthening phase and the ultimate tensile strength data.
[0011] In a specific embodiment of the present invention, the ultimate tensile strength model formula of the nickel-based high-temperature alloy is:
[0012]
[0013] Where T is temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f′ is the volume fraction of γ' phase.
[0014] γ
[0015] In a specific embodiment of the present invention, the yield strength model formula in step 1 is:
[0016]
[0017] Among them, σ 0 is the increase in basic yield strength, σ GB The increase in yield strength due to grain boundary strengthening, σ ss The increase in yield strength due to solid solution strengthening, σ γ′ The yield strength increase contributed by γ' precipitation strengthening, k is the Hall-Page constant, d is the average grain size, and f is γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, M is the Taylor factor, G is the shear model, b is the Burgers vector length, r w 、r s and r o are the radius of the precipitate phase through which the dislocation passes by the weak pair coupling mechanism, the strong pair coupling mechanism and the Orowan mechanism, respectively, APB is the reverse boundary energy, f γ′ is the volume fraction of γ' phase.
[0018] In a specific embodiment of the present invention, the yield strength model applicable to the full temperature range in step 2 is:
[0019]
[0020] Where T is temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f γ′ is the volume fraction of γ' phase.
[0021] In a specific embodiment of the present invention, the empirical formula for the relationship between the ultimate tensile strength and the yield strength in step 3 is:
[0022] σ UTS =C 0 *σ YS
[0023] Among them, σ UTS is the ultimate tensile strength, σ YS is the yield strength, C 0 is an empirical constant.
[0024] In a specific embodiment of the present invention, the new ultimate tensile strength model applicable to the full temperature range in step 4 is:
[0025]
[0026] Among them, a, o, b, p, c, q, k, g, j and h are the coefficients to be fitted, T is the temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f γ′ is the volume fraction of γ' phase.
[0027] On the other hand, an embodiment of the present invention also provides a nickel-based high-temperature alloy ultimate tensile strength modeling device, including: a data acquisition module, used to obtain ultimate tensile strength data and alloy composition data of nickel-based high-temperature alloys with different compositions at different temperatures; a thermodynamic calculation module, used to calculate the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase and the volume fraction of the γ' strengthening phase in the nickel-based high-temperature alloy at different temperatures according to the alloy composition data; a model optimization module, based on the grain boundary strengthening contribution, solid solution strengthening contribution and γ' precipitation strengthening contribution models, and introducing temperature variables and parameters, to establish a yield strength model; then the yield strength model and the empirical formula of the relationship between ultimate tensile strength and yield strength are combined to establish an ultimate tensile strength model for use in the nickel-based high-temperature alloy composition design, and the ultimate tensile strength model formula of the nickel-based high-temperature alloy is obtained.
[0028] On the other hand, an embodiment of the present invention further provides a nickel-based high-temperature alloy ultimate tensile strength modeling system, comprising: a processor and a memory connected to the processor, wherein the memory stores a computer program, and when the processor executes the computer program, the ultimate tensile strength modeling method of the nickel-based high-temperature alloy is executed as described above.
[0029] From the above, it can be seen that the ultimate tensile strength modeling method of the nickel-based high-temperature alloy provided in the embodiment of the present invention is based on the grain boundary strengthening contribution, solid solution strengthening contribution and γ' precipitation strengthening contribution models, and introduces temperature variables and parameters to establish a yield strength model applicable to the entire temperature range, and then establish an empirical formula for the relationship between the ultimate tensile strength and the yield strength; an ultimate tensile strength model for the entire temperature range is established based on the yield strength model and the empirical formula for the relationship between the ultimate tensile strength and the yield strength; the coefficients of the new ultimate tensile strength model are obtained based on the ultimate tensile strength data in the nickel-based high-temperature alloy composition design; the ultimate tensile strength model formula of the nickel-based high-temperature alloy is obtained based on the coefficients and the new ultimate tensile strength model. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.
[0031] Figure 1 A schematic flow chart of a method for modeling ultimate tensile strength of a nickel-based high-temperature alloy provided in accordance with the first embodiment of the present invention.
[0032] Figure 2 Another schematic flow chart of the method for modeling the ultimate tensile strength of nickel-based high-temperature alloys provided in the first embodiment of the present invention.
[0033] Figure 3 for Figure 1 Schematic diagram of the process of step 5 in .
[0034] Figure 4 The ultimate tensile strength modeling method of the nickel-based high-temperature alloy provided in an embodiment of the present invention has a predictive effect on the ultimate tensile strength.
[0035] Figure 5 A schematic structural diagram of a nickel-based high-temperature alloy ultimate tensile strength modeling device provided in accordance with the second embodiment of the present invention.
[0036] Figure 6 A schematic structural diagram of a nickel-based high-temperature alloy ultimate tensile strength modeling system provided in the third embodiment of the present invention.
[0037] Figure 7 A schematic structural diagram of a storage medium provided in a fourth embodiment of the present invention. DETAILED DESCRIPTION
[0038] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments described in the present invention, all other embodiments obtained by ordinary technicians in this field without creative work belong to the protection scope of the present invention.
[0039] In the embodiments of the present invention, the descriptions of "first", "second", etc. are only for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include at least one of the features.
[0040] [First embodiment]
[0041] The first embodiment of the present invention provides a prediction model for the ultimate tensile strength of a nickel-based high-temperature alloy, wherein the calculation expression of the prediction model is:
[0042]
[0043] Where T is temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f ′ is the volume fraction of γ' phase.
[0044] γ
[0045] See also Figure 1 The first embodiment of the present invention provides a method for modeling the ultimate tensile strength of a nickel-based high-temperature alloy, which may specifically include the following steps:
[0046] S10, step 1: establishing an ultimate tensile strength model for composition design of nickel-based high-temperature alloys based on grain boundary strengthening contribution, solid solution strengthening contribution and γ' precipitation strengthening contribution models;
[0047] S20, step 2: introducing temperature variables and parameters, and establishing a yield strength model applicable to the full temperature range according to the yield strength model;
[0048] S30, step 3: establishing an empirical formula for the relationship between ultimate tensile strength and yield strength;
[0049] S40, step 4: establishing an ultimate tensile strength model for the entire temperature range according to the yield strength model and an empirical formula for the relationship between the ultimate tensile strength and the yield strength;
[0050] S50, step 5: obtaining coefficients of the new ultimate tensile strength model according to the ultimate tensile data in the nickel-based high-temperature alloy composition design;
[0051] S60, step 6: obtaining an ultimate tensile strength model formula of the nickel-based high-temperature alloy according to the coefficient and the new ultimate tensile strength model.
[0052] Specifically, the ultimate tensile strength model formula of the nickel-based high-temperature alloy described in this embodiment is:
[0053]
[0054] Where T is temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f′ is the volume fraction of γ' phase.
[0055] γ
[0056] Step 1: Based on the grain boundary strengthening contribution, solid solution strengthening contribution and γ' precipitation strengthening contribution models, establish the yield strength model formula for the composition design of nickel-based high-temperature alloys. Specifically, first list the grain boundary strengthening, solid solution strengthening and γ' precipitation strengthening formulas, as follows:
[0057]
[0058]
[0059]
[0060] where k is the Hall-Page constant, d is the average grain size, and f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, M is the Taylor factor, G is the shear model, b is the Burgers vector length, P w , P s and P o are the probabilities of dislocation passing through the γ' precipitate phase by weak pair coupling mechanism, strong pair coupling mechanism and Orowan mechanism, respectively, and r w 、r s and r o are the radius of the precipitate phase through which the dislocation passes by the weak pair coupling mechanism, the strong pair coupling mechanism and the Orowan mechanism, respectively, APB is the reverse boundary energy, f γ′ is the volume fraction of γ' phase.
[0061] The grain boundary strengthening, solid solution strengthening and γ' precipitation strengthening models are combined, that is, formulas (1), (2) and (3) are combined to establish the yield strength model formula for the composition design of nickel-based high-temperature alloys. The specific formula is:
[0062]
[0063] Among them, σ 0 is the increase in basic yield strength, σ GB The increase in yield strength due to grain boundary strengthening, σ ss The increase in yield strength due to solid solution strengthening, σ γ′ is the contribution model for γ' precipitation strengthening, k is the Hall-Page constant, d is the average grain size, and f is γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x iis the concentration of the ith atom, M is the Taylor factor, G is the shear model, b is the Burgers vector length, r w 、r s and r o are the radius of the precipitate phase through which the dislocation passes by the weak pair coupling mechanism, the strong pair coupling mechanism and the Orowan mechanism, respectively, APB is the reverse boundary energy, f γ′ is the volume fraction of γ' phase.
[0064] In this embodiment, the parameters that are insensitive to the composition can be replaced by constants, and then formula (4) can be expressed as follows:
[0065]
[0066] Where a, b and c are the coefficients to be fitted.
[0067] Further, step 2: introduce temperature variables and parameters, and establish a yield strength model applicable to the full temperature range according to the yield strength model formula, so as to expand the applicable temperature range of the model formula. The yield strength model applicable to the full temperature range is:
[0068]
[0069] Among them, a, o, b, p, c, q, k, g, j and h are the coefficients to be fitted, T is the temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f ′ is the volume fraction of γ' phase.
[0070] γ
[0071] Step 3: Establish an empirical formula for the relationship between ultimate tensile strength and yield strength. The specific formula is:
[0072] σ UTS =C 0 *σ YS (7)
[0073] Among them, σ UTS is the ultimate tensile strength, σ YS is the yield strength, C 0 is an empirical constant.
[0074] Further, step 4: combine the yield strength model formula and the empirical formula of the relationship between the ultimate tensile strength and the yield strength, that is, combine formulas (6) and (7) to establish a new ultimate tensile strength model applicable to the full temperature range. The specific formula is:
[0075]
[0076] Among them, a, o, b, p, c, q, k, g, j and h are the coefficients to be fitted, T is the temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f γ′ is the volume fraction of γ' phase.
[0077] See also Figure 3 Step 5: Obtain the coefficients of the new ultimate tensile strength model according to the ultimate tensile data in the nickel-based high-temperature alloy composition design, which specifically includes the following steps:
[0078] S51, step 5.1: obtaining ultimate tensile strength data and alloy composition data of nickel-based high-temperature alloys with different compositions at different temperatures;
[0079] S52, step 5.2: calculating the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase and the volume fraction of the γ' strengthening phase in the nickel-based high-temperature alloy at different temperatures according to the alloy composition data;
[0080] S53, step 5.3: obtaining the coefficient according to the temperature, the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase, the volume fraction of the γ' strengthening phase and the ultimate tensile strength data.
[0081] The coefficients are fitted by applying the above formula (8) to the design of the composition of the nickel-based superalloy as an example. The nickel-based superalloy in this embodiment may be, for example, an additively manufactured nickel-based superalloy. Of course, this embodiment is not limited thereto. Specifically, the ultimate tensile strength data of the nickel-based superalloys with different compositions at different temperatures are obtained, and the alloy composition data, temperature and ultimate tensile strength data are recorded in detail. For example, the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase and the volume fraction of the γ' strengthening phase at the corresponding temperature can be obtained according to the alloy composition data at different temperatures. For example, the corresponding thermodynamic database and alloy composition data can be imported in succession through the high-throughput module in the thermodynamic software, and then the volume fraction of each phase and the concentration of each solute atom in each phase at different temperatures are calculated. The Result Analysis module in the thermodynamic software is used to batch process the calculation results to obtain the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase and the volume fraction of the γ' strengthening phase at the corresponding temperature. According to the above-obtained temperature, the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase and the volume fraction of the γ' strengthening phase and the yield strength data, the coefficients are fitted by combining the global optimization algorithm and the local optimization algorithm. Specifically, for example, each optimization can firstly perform a differential evolution algorithm, and then further optimize with the L-BFGS-B algorithm, and select the best result in multiple runs. In this way, better results can be provided. The yield strength model formula of the nickel-based high-temperature alloy finally obtained is:
[0082]
[0083] Where T is temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f ′ is the volume fraction of γ' phase.
[0084] γ
[0085] In summary, the present invention can predict the ultimate tensile strength of nickel-based high-temperature alloys at room temperature to 1300K according to the alloy composition, providing favorable support for the composition design of nickel-based high-temperature alloys for additive manufacturing.
[0086] [Second embodiment]
[0087] See also Figure 5 The second embodiment of the present invention provides a nickel-based high-temperature alloy ultimate tensile strength modeling device 10, which may specifically include: a data acquisition module 100, a thermodynamic module 200 and a model optimization module 300.
[0088] The data acquisition module 100 is used to obtain the ultimate tensile strength data and alloy composition data of nickel-based high-temperature alloys with different compositions at different temperatures;
[0089] Thermodynamic calculation module 200, used for calculating the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase and the volume fraction of the γ' strengthening phase in the nickel-based high-temperature alloy at different temperatures according to the alloy composition data;
[0090] The model optimization module 300 establishes a yield strength model based on the grain boundary strengthening contribution, solid solution strengthening contribution and γ' precipitation strengthening contribution models, and introduces temperature variables and parameters; then combines the yield strength model with the empirical formula of ultimate tensile strength and yield strength to establish an ultimate tensile strength model for nickel-based high-temperature alloy composition design applicable to the entire temperature range; obtains coefficients of the new ultimate tensile strength model based on ultimate tensile data in the nickel-based high-temperature alloy composition design; obtains the ultimate tensile strength model formula of the nickel-based high-temperature alloy based on the coefficients and the new ultimate tensile strength model, and obtains the ultimate tensile strength model formula of the nickel-based high-temperature alloy.
[0091] The specific working process and technical effects of the various modules in the nickel-based high-temperature alloy ultimate tensile strength modeling device 10 in this embodiment refer to the description of the first embodiment mentioned above.
[0092] [Third embodiment]
[0093] See also Figure 6 The third embodiment of the present invention provides a nickel-based high-temperature alloy ultimate tensile strength modeling system 20. The nickel-based high-temperature alloy ultimate tensile strength modeling system 20 includes a processor 400 and a memory 500 connected to the processor 400. The memory 500 may be, for example, a non-volatile storage cavity, and a computer program 510 is stored in the memory 500. The processor 400 may be, for example, an embedded processor. When the processor 400 executes the computer program 510, the nickel-based high-temperature alloy ultimate tensile strength modeling method in the first embodiment is executed.
[0094] The specific working process and technical effects of the nickel-based high-temperature alloy ultimate tensile strength modeling system 20 in this embodiment refer to the description of the first embodiment mentioned above.
[0095] [Fourth embodiment]
[0096] See also Figure 7 The fourth embodiment of the present invention provides a storage medium 30 storing a computer program 510.
[0097] The storage medium 30 is, for example, a non-volatile memory, such as: magnetic media (such as hard disks, floppy disks, and tapes), optical media (such as CDROM disks and DVDs), magneto-optical media (such as optical disks), and hardware devices (such as read-only memory (ROM), random access memory (RAM), flash memory, etc.) specially constructed to store and execute the computer program 510. The storage medium 30 stores the computer program 510, and the computer program 510 can be executed by the processor of the device where the storage medium 30 is located. The storage medium 30 can be executed by one or more processors or processing devices to execute the computer program 510 to implement the nickel-based high-temperature alloy ultimate tensile strength modeling method in the aforementioned first embodiment.
[0098] In addition, it can be understood that the aforementioned embodiments are only exemplary descriptions of the present invention. Under the premise that the technical features do not conflict, the structures do not contradict, and the purpose of the present invention is not violated, the technical solutions of the various embodiments can be arbitrarily combined and used in combination.
[0099] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A prediction model for the ultimate tensile strength of nickel-based superalloys. It is characterized in that include: The calculation expression of the prediction model is: Where T is temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f γ′ is the volume fraction of γ' phase.
2. A method for modeling the ultimate tensile strength of nickel-based superalloys, It is characterized in that include: Step 1: Based on the grain boundary strengthening contribution, solid solution strengthening contribution and γ' precipitation strengthening contribution models, a yield strength model for the composition design of nickel-based high-temperature alloys is established; Step 2: Introduce temperature variables and parameters, and establish a yield strength model applicable to the full temperature range according to the yield strength model; Step 3: Establish an empirical formula for the relationship between ultimate tensile strength and yield strength; Step 4: Establish an ultimate tensile strength model for the entire temperature range based on the yield strength model and the empirical formula for the relationship between ultimate tensile strength and yield strength; Step 5: Obtaining coefficients of the new ultimate tensile strength model according to the ultimate tensile data in the nickel-based high-temperature alloy composition design; Step 6: Obtain an ultimate tensile strength model formula of the nickel-based high-temperature alloy according to the coefficient and the new ultimate tensile strength model.
3. The method for modeling the ultimate tensile strength of a nickel-based high-temperature alloy as claimed in claim 2, It is characterized in that The step 5 specifically includes: Step 5.1: Obtain the ultimate tensile strength data and alloy composition data of nickel-based high-temperature alloys with different compositions at different temperatures; Step 5.2: Calculate the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase and the volume fraction of the γ' strengthening phase in the nickel-based high-temperature alloy at different temperatures according to the alloy composition data; Step 5.3: Obtaining the coefficient according to the temperature, the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase, the volume fraction of the γ' strengthening phase and the ultimate tensile strength data.
4. The method for modeling the ultimate tensile strength of a nickel-based high-temperature alloy according to claim 2, It is characterized in that The ultimate tensile strength model formula of the nickel-based high-temperature alloy is: Where T is temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f γ′ is the volume fraction of γ' phase.
5. The method for modeling the ultimate tensile strength of a nickel-based high-temperature alloy according to claim 2, It is characterized in that The empirical formula for the relationship between ultimate tensile strength and yield strength in step 3 is: s UTS =C 0 *s YS Among them, σ UTS is the ultimate tensile strength, σ YS is the yield strength, C 0 is an empirical constant.
6. The modeling method according to claim 2, It is characterized in that The new ultimate tensile strength model applicable to the full temperature range in step 4 is: Among them, a, o, b, p, c, q, k, g, j and h are the coefficients to be fitted, T is the temperature, f γ is the volume fraction of γ phase, β i is the solid solution strengthening coefficient of the ith atom, x i is the concentration of the ith atom, f γ′ is the volume fraction of γ' phase.
7. A nickel-based superalloy ultimate tensile strength modeling device, It is characterized in that include: A data acquisition module is used to obtain the ultimate tensile strength data and alloy composition data of nickel-based high-temperature alloys with different compositions at different temperatures; A thermodynamic calculation module is used to calculate the volume fraction of the γ matrix phase, the concentration of each solute atom in the γ matrix phase and the volume fraction of the γ' strengthening phase in the nickel-based high-temperature alloy at different temperatures according to the alloy composition data; The model optimization module establishes a yield strength model based on the grain boundary strengthening contribution, solid solution strengthening contribution and γ' precipitation strengthening contribution models, and introduces temperature variables and parameters; then the yield strength model is combined with the empirical formula of ultimate tensile strength and yield strength to establish an ultimate tensile strength model for the composition design of nickel-based high-temperature alloys, and the ultimate tensile strength model formula of the nickel-based high-temperature alloy is obtained.
8. A nickel-based superalloy ultimate tensile strength modeling system, It is characterized in that include: A processor and a memory connected to the processor, wherein the memory stores a computer program, and when the processor executes the computer program, the method for modeling the ultimate tensile strength of a nickel-based high-temperature alloy as claimed in any one of claims 2 to 6 is executed.
Citation Information
Cited By