Silicon carbide power device terminal, preparation method and chip
By forming the main junction region and field-limiting ring region on the N-type epitaxial layer of the silicon carbide power device, and forming a dense oxide layer by using a multi-step oxidation process, the problems of poor density of the oxide layer and high charge density are solved, and the device is improved Pressure resistance and reliability.
Patent Information
- Application Number
- CN202411488592.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-24
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-10-24
AI Technical Summary
The terminal oxide layer of existing silicon carbide power devices has poor density and high charge density, resulting in low voltage resistance of the device, affecting its reliability and performance.
The main junction area and the field-limited ring area are formed on the N-type epitaxial layer, and the terminal oxide layer is formed by performing high-temperature dry oxygen, annealing, low-temperature dry oxygen and low-temperature wet oxygen processes on some areas of the field-limited ring area and main junction area in turn. , the dense oxide layer is grown through a multi-step oxidation process to reduce the fixed charge in the oxide layer.
It effectively reduces the fixed charge in the oxide layer, improves the voltage withstandability and reliability of the device, and improves the long-term application performance of the device.
Smart Images

Figure CN119092405A_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of power devices, and in particular, relates to a silicon carbide power device terminal, a preparation method, and a chip. Background Art
[0002] As a wide bandgap semiconductor, silicon carbide power devices have obvious advantages in high voltage, high current, high temperature, radiation and other application fields due to their excellent characteristics of high critical electric field and high thermal conductivity. The withstand voltage characteristics of silicon carbide power devices are an important indicator to measure device performance and reliability. The withstand voltage of power devices can be attributed to the breakdown characteristics of the PN junction structure. Because the PN junction presents a curved junction and extends to the surface, an electric field concentration is formed, resulting in a lower withstand voltage of the power device than that of the planar junction. For this reason, terminal structures such as field plates, junction terminal extensions, and field limiting rings are introduced to improve the withstand voltage characteristics of the device. In addition to the influence of the curved junction, the oxide layer on the surface of the power device terminal is another important factor affecting the withstand voltage of the device; the charge in the oxide layer above the terminal of the silicon carbide power device will cause the shape of the PN junction space charge region to change, causing the device to have insufficient withstand voltage. Therefore, the defects and pinhole density in the oxide layer above the device terminal, especially the fixed charge, oxide layer trap charge, and oxide layer interface charge in the oxide layer are important factors affecting the reliability quality of silicon carbide power devices.
[0003] However, the current methods for manufacturing the terminal oxide layer of silicon carbide power devices mostly use chemical vapor deposition. The grown oxide layer has a loose structure and poor density, a high charge density in the oxide layer, and a poor interface state, which will reduce the device terminal's ability to withstand voltage, and may further degrade the device's performance and reliability, and may further lead to device failure. Summary of the invention
[0004] In order to solve the above technical problems, the embodiments of the present application provide a silicon carbide power device terminal and a preparation method and a chip, aiming to improve the reliability of the oxide layer of the silicon carbide power device terminal.
[0005] A first aspect of an embodiment of the present application provides a method for preparing a silicon carbide power device terminal, the method comprising: An N-type buffer layer and an N-type epitaxial layer are sequentially formed on the front side of the N-type substrate; forming a main junction region and a field limiting ring region on the N-type epitaxial layer; Forming a terminal oxide layer on the field limiting ring region and a part of the main junction region by sequentially adopting high temperature dry oxygen, annealing, low temperature dry oxygen and low temperature wet oxygen processes; forming a passivation layer on the terminal oxide layer; forming a front metal electrode on a portion of the main junction region; After the back side of the N-type substrate is thinned, a back side metal material is deposited to form a back side metal electrode.
[0006] In some embodiments, the forming of the terminal oxide layer on the field limiting ring region and a portion of the main junction region by sequentially using high temperature dry oxygen, annealing, low temperature dry oxygen and low temperature wet oxygen processes includes: Performing dry oxygen oxidation treatment on the field limiting ring region and a portion of the main junction region under a preset high temperature dry oxygen temperature condition to obtain a first thermal oxide layer; annealing the first thermal oxide layer under inert gas conditions; The annealed thermal oxide layer is further oxidized by a low temperature dry oxygen process to obtain a second thermal oxide layer; A low temperature wet oxygen process is used to continue oxidation treatment in the field limiting ring area and a part of the main junction area to obtain a third thermal oxide layer; the terminal oxide layer includes a first thermal oxide layer, a second thermal oxide layer and a third thermal oxide layer.
[0007] In some embodiments, the preset high temperature dry oxygen temperature condition includes: Dry oxygen temperature of 1050℃-1150℃.
[0008] In some embodiments, the annealing conditions include: Argon atmosphere, annealing temperature of 1050°C - 1150°C and annealing time of 25-35 minutes.
[0009] In some embodiments, the conditions of the low temperature dry oxygen process include: Dry oxygen temperature of 900℃-950℃.
[0010] In some embodiments, the conditions of the low temperature wet oxygen process include: Wet oxygen temperature of 900℃-950℃.
[0011] In some embodiments, forming a passivation layer on the terminal oxide layer comprises: An insulating material is used to form a passivation layer on the front side of the terminal oxide layer.
[0012] In some embodiments, forming a front metal electrode on a portion of the main junction region includes: Using metal materials to deposit metal materials on the main junction and the front side of the active area to form a front metal layer; The front metal layer is annealed at a preset annealing temperature, annealing time and annealing atmosphere to form the front metal electrode.
[0013] A second aspect of the embodiments of the present application further provides a silicon carbide power device terminal, wherein the silicon carbide power device terminal is prepared by the preparation method described in any one of the above embodiments.
[0014] A third aspect of the embodiments of the present application further provides a chip, comprising a silicon carbide power device terminal prepared by the preparation method described in any of the above embodiments.
[0015] The beneficial effects of the embodiments of the present application are as follows: a main junction region and a field limiting ring region are formed on an N-type epitaxial layer, and a terminal oxide layer is formed by sequentially using high-temperature dry oxygen, annealing, low-temperature dry oxygen, and low-temperature wet oxygen processes on partial regions of the field limiting ring region and the main junction region. Among them, the first part of the terminal oxide layer is grown by a high-temperature dry oxygen oxidation method, the first part is annealed in an inert gas environment while the temperature remains constant, and then the second component of the terminal oxide layer is grown by a low-temperature dry oxygen process under low-temperature conditions by adjusting the oxidation temperature, and finally the third component of the terminal oxide layer is grown by low-temperature wet oxygen, so that a denser oxide layer can be grown on the one hand, which effectively reduces the fixed charge in the oxide layer, reduces the number of positive charges in the terminal oxide layer, and improves the reliability of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 A schematic diagram of a process for preparing a silicon carbide power device terminal provided in an embodiment of the present application; Figure 2 A schematic diagram of the structure of a silicon carbide power device terminal prepared by the preparation method provided in an embodiment of the present application; Figure 3 This is a schematic flow chart of step S300 in the method for preparing a silicon carbide power device terminal provided in an embodiment of the present application. DETAILED DESCRIPTION
[0017] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0018] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it can be directly on the other element or indirectly on the other element. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.
[0019] It should be understood that the orientation or position relationship indicated by terms such as "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0020] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, "plurality" means one or more, unless otherwise clearly and specifically defined.
[0021] The existing methods for manufacturing the terminal oxide layer of silicon carbide power devices mostly use chemical vapor deposition. The grown oxide layer has a loose structure and poor density, a high charge density in the oxide layer, and a poor interface state, which will reduce the device terminal's ability to withstand voltage, and may further degrade the device's performance and reliability, and may further lead to device failure.
[0022] In order to solve the above technical problems, the present invention provides a method for preparing a silicon carbide power device terminal. Figure 1 As shown, a method for preparing a silicon carbide power device terminal in this embodiment includes steps S100 to S600.
[0023] In step S100 , an N-type buffer layer 120 and an N-type epitaxial layer 130 are sequentially formed on the front surface of an N-type substrate 110 .
[0024] In this embodiment, combined with Figure 2 As shown, an N-type buffer layer 120 with a lower doping concentration can be formed on the front side of the N-type substrate 110, or the N-type doped N-type substrate 110 with the N-type buffer layer 120 can be directly selected as an electrode of the device, and a lower N-type doped N-type epitaxial layer 130 with a certain thickness can be epitaxially grown on the N-type buffer layer 120, wherein the back side of the N-type substrate 110 is used to deposit metal materials for use as electrodes.
[0025] In some embodiments, the N-type substrate 110 may be an N-type single crystal substrate material.
[0026] In some embodiments, the resistivity of the N-type substrate 110 in this embodiment may be 0.015 ohm·cm-0.25 ohm·cm.
[0027] In some embodiments, the N-type substrate 110 may be an N-type silicon carbide substrate.
[0028] In some embodiments, the thickness of the N-type buffer layer 120 is 0.5 micrometers to 1 micrometers.
[0029] In some embodiments, the concentration of the N-type buffer layer 120 is 0.9E18 / cm 3 -1.1E18 / cm 3 The doping ions of the N-type buffer layer 120 are all nitrogen ions, and the N-type buffer layer 120 can serve as a polarity terminal of the silicon carbide power device.
[0030] In some embodiments, the thickness of the N-type epitaxial layer 130 may be 5 micrometers to 20 micrometers, and the doping ions of the N-type epitaxial layer 130 are nitrogen ions.
[0031] In some embodiments, the concentration of the N-type epitaxial layer 130 may be 5E15 / cm 3 -9E15 / cm 3 .
[0032] In step S200 , a main junction region 150 and a field limiting ring region 140 are formed on the N-type epitaxial layer 130 .
[0033] In this embodiment, an ion implantation window can be formed on the front side of the N-type epitaxial layer 130 by photolithography or etching process, P-type doping ions can be implanted into the set ion implantation window, and the main junction region 150 and the field limiting ring region 140 of the device terminal can be formed by high temperature annealing activation treatment.
[0034] In some embodiments, the concentration of the main junction region 150 and the field limiting ring region 140 may be 1E16 / cm 3 -1E19 / cm 3 .
[0035] In some embodiments, the annealing temperature after implanting the P-type dopant ions may be 1750° C.-1800° C.
[0036] In some embodiments, aluminum ions may be used as implanted ions in the main junction region 150 and the field limiting ring region 140, with an implantation dose of 4.6E13 cm -2 To 8.8E14cm -2 The implantation energy is between 30 KeV and 550 KeV to form the main junction region 150 and the field limiting ring region 140 of the device terminal, and the depth of the main junction region 150 and the field limiting ring region 140 is between 0.6 microns and 0.8 microns.
[0037] In some embodiments, in combination Figure 2As shown, the field limiting ring region 140 may include a plurality of P-type doped sub-regions 141 , and the width of the main junction region 150 is greater than the width of the P-type doped sub-regions 141 in the field limiting ring region 140 .
[0038] In some embodiments, the distance between the first P-type doped sub-region 141 in the field limiting ring region 140 and the main junction region 150 is less than a preset distance, which may be 1.1 microns or 1.2 microns.
[0039] In some embodiments, among the multiple P-type doped sub-regions 141 in the field limiting ring region 140, the spacing between adjacent P-type doped sub-regions 141 is related to the first distance, and the first distance is the distance between the corresponding P-type doped sub-region 141 and the main junction region 150. The larger the first distance, the larger the spacing between the corresponding P-type doped sub-region 141 and its adjacent P-type doped sub-region 141, so that the electric field distribution in the N-type epitaxial layer 130 can be adjusted to match the doping concentration of the N-type epitaxial layer 130, thereby improving the reliability of the device.
[0040] In some embodiments, the width of the P-type doped sub-region 141 is related to the first distance, which is the distance between the corresponding P-type doped sub-region 141 and the main junction region 150. The larger the first distance, the larger the width of the corresponding P-type doped sub-region 141, so that the electric field distribution in the N-type epitaxial layer 130 can be adjusted to match the doping concentration of the N-type epitaxial layer 130, thereby improving the reliability of the device.
[0041] In some embodiments, the width of the P-type doped sub-region 141 and the spacing between adjacent P-type doped sub-regions 141 may change simultaneously with the first distance. When the first distance gradually increases, the spacing between the corresponding P-type doped sub-region 141 and its adjacent P-type doped sub-region 141 becomes larger.
[0042] In some embodiments, the width of the P-type doped sub-region 141 and the spacing between adjacent P-type doped sub-regions 141 may be gradually changed according to a certain region. In a first preset region close to the main junction region 150, the width of the P-type doped sub-region 141 and the spacing between adjacent P-type doped sub-regions 141 are equal, in a second preset region close to the first preset region, the width of the P-type doped sub-region 141 and the spacing between adjacent P-type doped sub-regions 141 are equal, in a third preset region close to the second preset region, the width of the P-type doped sub-region 141 and the spacing between adjacent P-type doped sub-regions 141 are equal, and so on. The spacing between adjacent P-type doped sub-regions 141 in the second preset region is greater than the spacing between adjacent P-type doped sub-regions 141 in the first preset region, and the spacing between adjacent P-type doped sub-regions 141 in the third preset region is greater than the spacing between adjacent P-type doped sub-regions 141 in the second preset region.
[0043] In some embodiments, the intervals between adjacent P-type doped sub-regions 141 are equal.
[0044] In step S300 , a terminal oxide layer 160 is formed on a portion of the field limiting ring region 140 and the main junction region 150 by sequentially adopting high temperature dry oxygen, annealing, low temperature dry oxygen and low temperature wet oxygen processes.
[0045] In this embodiment, by using a high-temperature dry oxygen process to form the first part of the terminal oxide layer 160 on the field limiting ring area 140 and the partial area of the main junction area 150, and then annealing, the dangling bonds and twisted bonds between the interface of silicon dioxide and silicon carbide can be recrystallized to restore the lattice defects at the interface. The second part of the terminal oxide layer 160 is formed by a low-temperature dry oxygen process, and the third part of the terminal oxide layer 160 is formed by a low-temperature wet oxygen process. Through the process, on the one hand, a denser oxide layer is grown, the oxide layer has voids, and the carbon clustering at the interface between the oxide layer and silicon carbide or the carbon in the oxide layer is significantly reduced, which effectively reduces the fixed charge in the oxide layer; the number of positive charges in the oxide layer is reduced, which suppresses the positive charges in the oxide layer at the device terminal affecting the device withstand voltage, increasing the leakage of the device, and causing the device electrical performance to deteriorate or reliability failure. Related problems such as failure, improve the long-term application reliability of the device.
[0046] In some embodiments, the high temperature dry oxygen in step S300 means that pure oxygen is introduced under high temperature conditions to oxidize the field limiting ring region 140 and a portion of the main junction region 150 , wherein the high temperature dry oxygen condition means that water vapor is not mixed in the oxygen.
[0047] In some embodiments, the low temperature dry oxygen in step S300 means that pure oxygen is introduced under low temperature conditions to oxidize the field limiting ring region 140 and a portion of the main junction region 150 , wherein the low temperature dry oxygen condition means that water vapor is not mixed in the oxygen.
[0048] In some embodiments, the temperature of the low-temperature dry oxygen process in step S300 is lower than the temperature of the high-temperature dry oxygen process.
[0049] In some embodiments, the low temperature wet oxygen in step S300 means that oxygen is introduced under low temperature conditions to oxidize a portion of the field limiting ring region 140 and the main junction region 150 , wherein the low temperature wet oxygen condition means that a certain proportion of water vapor is mixed into the oxygen.
[0050] In some embodiments, the temperature of the low temperature wet oxygen process and the low temperature dry oxygen process in step S300 may be the same.
[0051] In step S400 , a passivation layer 220 is formed on the terminal oxide layer 160 .
[0052] In this embodiment, the passivation layer 220 may be formed on the terminal oxide layer 160 by a plasma enhanced chemical vapor deposition (PECVD) process.
[0053] In step S500 , a front metal electrode 210 is formed on a portion of the main junction region 150 .
[0054] In this embodiment, a front metal material is deposited on a portion of the main junction region 150 , and the deposited front metal material is patterned through photolithography and etching processes.
[0055] In some embodiments, a metal aluminum layer may be formed on a portion of the main junction region 150 by a sputtering or evaporation process.
[0056] In some embodiments, the material of the front metal electrode 210 may be one or more metals including titanium, nickel, silver, and aluminum.
[0057] In some embodiments, a metal electrode window can be formed in a partial area on the main junction region 150 through photolithography and etching processes, and the front metal electrode 210 can be obtained by annealing the front-deposited metal layer at a preset annealing temperature, preset annealing time, and annealing atmosphere.
[0058] In some embodiments, the preset annealing temperature may be 400° C.-450° C., the preset annealing time may be 45 minutes-60 minutes, and the annealing atmosphere may be nitrogen.
[0059] In step S600 , after the back side of the N-type substrate 110 is thinned, a back side metal material is deposited to form a back side metal electrode 230 .
[0060] In this embodiment, after the back side of the N-type substrate 110 is thinned, a back side metal material is deposited, and the back side metal is annealed at a preset annealing time and annealing atmosphere to form a back side metal electrode 230 .
[0061] In some embodiments, the thickness of the back metal electrode 230 is 0.1 micrometers to 1.8 micrometers.
[0062] In some embodiments, the thickness of the back side of the N-type substrate 110 after thinning is 150 micrometers to 175 micrometers.
[0063] In some embodiments, the material of the back metal electrode 230 can be one or more metals including titanium, nickel, silver, and aluminum.
[0064] In some embodiments, in combination Figure 3 As shown, step S300 includes steps S310 to S340.
[0065] In step S310 , a dry oxygen oxidation treatment is performed on a portion of the field limiting ring region 140 and the main junction region 150 under a preset high temperature dry oxygen temperature condition to obtain a first thermal oxide layer.
[0066] In this embodiment, after the dry oxygen oxidation process in step S310, a first thermal oxide layer can be grown on the main junction and the front of the field limiting ring by high-temperature dry oxygen oxidation. The first thermal oxide layer has a dense structure, good uniformity, and strong pressure resistance.
[0067] In some embodiments, the temperature of the dry oxygen oxidation process in step S310 may be 1050° C.-1150° C.
[0068] In step S320, the first thermal oxide layer is annealed under an inert gas condition.
[0069] In this embodiment, after the annealing treatment in step S320, the dangling bonds and twisted bonds at the interface between silicon dioxide and silicon carbide can be recrystallized, thereby restoring the lattice defects at the interface.
[0070] In some embodiments, the annealing temperature of the annealing treatment in step S320 is 1050° C.-1150° C., the predetermined annealing time is 25 minutes-35 minutes, and the inert gas of the annealing treatment in step S320 may be argon gas.
[0071] In step S330, the thermal oxide layer after annealing is further oxidized by a low temperature dry oxygen process to obtain a second thermal oxide layer.
[0072] In this embodiment, the low-temperature dry oxygen process in step S330 can effectively reduce the number of dangling bonds caused by carbon clusters at the interface between the oxide layer and silicon carbide. In addition to reducing the charge distribution in the depletion layer at the terminal of the silicon carbide device due to the presence of the interface state, thereby effectively suppressing the device's withstand voltage characteristics, it can also reduce the free carbon elements in the oxide layer, thereby achieving the purpose of improving the quality of the oxide layer.
[0073] In some embodiments, the temperature of the low temperature dry oxygen process in step S330 is 900° C.-950° C.
[0074] In step S340 , a low temperature wet oxygen process is used to continue oxidation treatment on a portion of the field limiting ring region 140 and the main junction region 150 to obtain a third thermal oxide layer.
[0075] In the present embodiment, the terminal oxide layer 160 includes a first thermal oxide layer, a second thermal oxide layer and a third thermal oxide layer. The low-temperature wet oxygen process in step S340 can form a wet oxygen oxidation atmosphere by forming a mixed gas of oxygen and water vapor. After the third low-temperature wet oxygen oxidation process in step S340, a complete terminal oxide layer 160 of the silicon carbide device is formed, in the form of oxygen carrying water vapor for oxidation, reducing the fixed positive charge of the oxide layer, and eliminating the influence of its induced charge on the terminal surface on the PN junction withstand voltage. In the present embodiment, after the third low-temperature wet oxygen oxidation process in step S340, the fixed charge density in the oxide layer is reduced, so that the charge induced by the charge in the oxide layer on the terminal surface of the device affects the surface electric field of the device, thereby effectively improving the condition of reducing the withstand voltage of the device, and the reliability of the silicon carbide power device is effectively improved and enhanced.
[0076] In some embodiments, the wet oxygen oxidation temperature of the low temperature wet oxygen process in step S340 is 900° C.-950° C.
[0077] In some embodiments, the preset high temperature dry oxygen temperature condition includes: a dry oxygen temperature of 1050°C-1150°C.
[0078] In some embodiments, the annealing process conditions include: an argon atmosphere, an annealing temperature of 1050° C.-1150° C., and an annealing time of 25-35 minutes.
[0079] In some embodiments, the temperature in the low temperature dry oxygen process and the low temperature wet oxygen process is the same.
[0080] In some embodiments, the conditions of the low temperature dry oxygen process include: a dry oxygen temperature of 900° C.-950° C.
[0081] In some embodiments, the conditions of the low temperature wet oxygen process include: a wet oxygen temperature of 900° C.-950° C.
[0082] In some embodiments, forming the passivation layer 220 on the terminal oxide layer 160 includes: forming the passivation layer 220 on the front side of the terminal oxide layer 160 using an insulating material.
[0083] In some embodiments, in step S500 , a front metal electrode 210 is formed on a portion of the main junction region 150 , including step S510 and step S520 .
[0084] In step S510, a metal material is deposited on the main junction and the front side of the active region to form a front side metal layer.
[0085] In step S520 , the front metal layer is annealed at a preset annealing temperature, annealing time, and annealing atmosphere to form the front metal electrode 210 .
[0086] In some embodiments, the thickness of the front metal electrode 210 is 0.15 micrometers to 4.0 micrometers. An embodiment of the present application further provides a silicon carbide power device terminal, which is prepared by the preparation method of any one of the above embodiments.
[0087] An embodiment of the present application further provides a chip. The chip in this embodiment includes a silicon carbide power device terminal prepared by the preparation method of any of the above embodiments.
[0088] In this embodiment, the chip includes a chip substrate, and one or more silicon carbide power device terminals are arranged on the substrate. The silicon carbide power device terminal can be prepared by the preparation method in any of the above embodiments, or the silicon carbide power device terminal in any of the above embodiments can be arranged on the chip substrate.
[0089] In a specific application embodiment, other related semiconductor devices may be integrated on the chip substrate and form an integrated circuit with the silicon carbide power device terminal in any of the above embodiments.
[0090] In a specific application embodiment, the chip may be a switch chip or a driver chip.
[0091] The beneficial effects of the embodiments of the present application are as follows: a main junction region and a field limiting ring region are formed on an N-type epitaxial layer, and a terminal oxide layer is formed by sequentially using high-temperature dry oxygen, annealing, low-temperature dry oxygen, and low-temperature wet oxygen processes on partial regions of the field limiting ring region and the main junction region. Among them, the first part of the terminal oxide layer is grown by a high-temperature dry oxygen oxidation method, the first part is annealed in an inert gas environment while the temperature remains constant, and then the second component of the terminal oxide layer is grown by a low-temperature dry oxygen process under low-temperature conditions by adjusting the oxidation temperature, and finally the third component of the terminal oxide layer is grown by low-temperature wet oxygen, so that a denser oxide layer can be grown on the one hand, which effectively reduces the fixed charge in the oxide layer, reduces the number of positive charges in the terminal oxide layer, and improves the reliability of the device.
[0092] Those skilled in the art can clearly understand that for the convenience and simplicity of description, only the division of the above-mentioned doping regions and devices is used as an example for illustration. In actual applications, the above-mentioned functions can be assigned to different doping regions and devices as needed, that is, the internal structure of the device is divided into different doping regions to complete all or part of the functions described above. The doping regions and devices in the embodiments can be integrated into one unit, or each unit can exist physically separately, or two or more units can be integrated into one unit.
[0093] In addition, the specific names of the doping regions and devices are only for the convenience of distinguishing each other and are not used to limit the scope of protection of the present application.
[0094] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described or recorded in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.
[0095] In addition, each doping region in each embodiment of the present application may be integrated into one unit, or each unit may exist physically separately, or two or more units may be integrated into one unit.
[0096] The above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. These modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application, and should all be included in the protection scope of the present application.
Claims
1. A method for preparing a silicon carbide power device terminal, characterized in that: The preparation method comprises: An N-type buffer layer and an N-type epitaxial layer are sequentially formed on the front side of the N-type substrate; forming a main junction region and a field limiting ring region on the N-type epitaxial layer; Forming a terminal oxide layer on the field limiting ring region and a part of the main junction region by sequentially adopting high temperature dry oxygen, annealing, low temperature dry oxygen and low temperature wet oxygen processes; forming a passivation layer on the terminal oxide layer; forming a front metal electrode on a portion of the main junction region; After the back side of the N-type substrate is thinned, a back side metal material is deposited to form a back side metal electrode.
2. The preparation method according to claim 1, characterized in that The step of sequentially forming a terminal oxide layer on the field limiting ring region and a portion of the main junction region by using high temperature dry oxygen, annealing, low temperature dry oxygen and low temperature wet oxygen processes includes: Performing dry oxygen oxidation treatment on the field limiting ring region and a portion of the main junction region under a preset high temperature dry oxygen temperature condition to obtain a first thermal oxide layer; annealing the first thermal oxide layer under inert gas conditions; The annealed thermal oxide layer is further oxidized by a low temperature dry oxygen process to obtain a second thermal oxide layer; A low temperature wet oxygen process is used to continue oxidation treatment in the field limiting ring area and a part of the main junction area to obtain a third thermal oxide layer; the terminal oxide layer includes a first thermal oxide layer, a second thermal oxide layer and a third thermal oxide layer.
3. The preparation method according to claim 2, characterized in that: The preset high temperature dry oxygen temperature conditions include: Dry oxygen temperature of 1050℃-1150℃.
4. The preparation method according to claim 2, characterized in that: The conditions of the annealing treatment include: Argon atmosphere, annealing temperature of 1050°C - 1150°C and annealing time of 25-35 minutes.
5. The preparation method according to claim 2, characterized in that: The conditions of the low temperature dry oxygen process include: Dry oxygen temperature of 900℃-950℃.
6. The preparation method according to claim 2, characterized in that: The conditions of the low temperature wet oxygen process include: Wet oxygen temperature of 900℃-950℃.
7. The preparation method according to any one of claims 1 to 6, characterized in that: The forming of a passivation layer on the terminal oxide layer comprises: An insulating material is used to form a passivation layer on the front side of the terminal oxide layer.
8. The preparation method according to any one of claims 1 to 6, characterized in that: Forming a front metal electrode on a partial area of the main junction region, comprising: Using metal materials to deposit metal materials on the main junction and the front side of the active area to form a front metal layer; The front metal layer is annealed at a preset annealing temperature, annealing time and annealing atmosphere to form the front metal electrode.
9. A silicon carbide power device terminal, characterized in that: The silicon carbide power device terminal is prepared by the preparation method according to any one of claims 1-8.
10. A chip, characterized in that: It comprises a silicon carbide power device terminal prepared by the preparation method according to any one of claims 1 to 8.
Citation Information
Patent Citations
Low-on-resistance SiC IGBT and manufacturing method thereof
CN104241348A
A SiC power device terminal and a manufacturing method thereof
CN109087940A
Reinforcement process method for improving gate oxide reverse breakdown of anti-radiation VDMOS
CN111293169A
Preparation method of silicon carbide power device, and silicon carbide power device
CN112002648A
Semiconductor power device and manufacturing method thereof
CN113629130A