Capacitor preparation method

A novel capacitor embedding process with protective deposition and selective etching addresses the challenges of high aspect ratio holes in HsRAM, ensuring uniformity and preventing short circuits, thus enhancing capacitor quality and efficiency.

CN119095477APending Publication Date: 2024-12-06温州核芯智存科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311124400.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-09-01
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The high aspect ratio of embedded holes in high-temperature state memory (HsRAM) processes necessitates maskless dry etching, which thins the film layer and risks short circuits between electrode plates, while thickened electrode film deposition fails to address uniformity issues.

Method used

A new capacitor embedding process involving sequential deposition of materials, a protective layer, and selective etching to avoid dry etching impacts, using protective deposition and plasma etching with specific precursors to ensure uniformity and prevent short circuits.

Benefits of technology

The process enhances capacitor quality by avoiding damage to inner layers, preventing short circuits, and improving efficiency by centralized etching, reducing cross-contamination risks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119095477A_ABST
    Figure CN119095477A_ABST
Patent Text Reader

Abstract

The invention discloses a capacitor preparation method. The method comprises the following steps: sequentially depositing capacitor materials on a substrate to generate a stack layer; laying a protective layer on the top of the stacking layer; sequentially removing the capacitor material on the stacking layer except the area covered by the protective layer; and depositing a dielectric layer on the base material, and polishing the dielectric layer to be parallel to the protective layer. The protection layer is added to serve as a mask protection plate for etching the capacitor layer, damage to a film layer in a cell hole caused by mask-free etching in the prior art is avoided, the etched capacitor is completely wrapped by the dielectric layer, the problem of short circuit is avoided, and the yield of the capacitor is improved. The etching processes of the four layers of capacitor materials are intensively carried out, so that the problems of cross contamination possibly caused by the manufacturing process, low efficiency and high potential quality hazard of capacitors are solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of high-temperature storage devices, and in particular to a capacitor preparation method. Background Art

[0002] High-stable memory is a new type of memory based on logic chips, using High-K ferroelectric materials as capacitor dielectrics and using the polarity of ferroelectric materials to achieve storage functions. Its capacitor structure adopts an embedded method, and the materials required for ferroelectric capacitors are embedded in the top winding layer to form embedded capacitors. The embedded holes engraved by our company based on the high-temperature state memory (HsRAM) process have a very high depth-to-width ratio, and it is impossible to use a masked photolithography scheme when etching the wafer surface, so it can only be etched using a maskless dry etching scheme. However, during the dry etching process, the maskless scheme will not only etch the wafer surface, but also thin the film layer in the embedded hole, affecting the chip function. The existing technology uses thickened electrode film deposition thickness to avoid damage, but this approach cannot solve the problem of poor uniformity of the film layer, and excessive etching of the high-dielectric capacitor layer in the middle will cause a short circuit between the upper and lower electrode plates, causing major risks. Therefore, a new capacitor embedding process is designed to change the logic of depositing electrical materials and increase the method of protective deposition to avoid the impact of dry etching on the capacitance in the hole, improve the efficiency of the entire process, eliminate potential risks, and improve the quality of capacitors. Summary of the invention

[0003] The purpose of this section is to summarize some aspects of the embodiments of the present invention and briefly introduce some preferred embodiments. Some simplifications or omissions may be made in this section and the abstract of the specification and the title of the invention of this application to avoid blurring the purpose of this section, the abstract of the specification and the title of the invention, and such simplifications or omissions cannot be used to limit the scope of the present invention.

[0004] In view of the above and / or the existing technologies, the embedded holes engraved based on the high temperature state memory (HsRAM) process have an extremely high aspect ratio, and it is impossible to use a masked photolithography scheme when etching the wafer surface, so only a maskless dry etching scheme can be used for etching. However, during the dry etching process, the maskless scheme not only etches the wafer surface, but also thins the film layer inside the embedded hole, affecting the chip function. The existing technology uses thickened electrode film deposition thickness to avoid damage, but this approach cannot solve the problem of poor uniformity of the film layer, and excessive etching of the high dielectric constant layer in the middle will cause a short circuit between the upper and lower electrode plates, causing a major risk. The present invention is proposed.

[0005] Therefore, the technical problem to be solved by the present invention is to design a new capacitor embedding process, which can change the logic of depositing electrical materials and increase the method of protective deposition to avoid the impact of dry etching on the capacitance in the hole, thereby improving the efficiency of the entire process, eliminating potential risks and improving the quality of the capacitor.

[0006] In order to solve the above technical problems, the present invention provides the following technical solutions: a method for preparing a capacitor, comprising: sequentially depositing capacitor materials on a substrate to generate stacked layers;

[0007] Laying a protective layer on top of the stack;

[0008] Sequentially remove capacitor materials on the stacked layers except for the area covered by the protective layer;

[0009] A dielectric layer is deposited on the substrate and polished to be parallel to the protective layer.

[0010] As a preferred solution of a capacitor preparation method of the present invention, wherein: a substrate is arrayed with cell holes, and the stacked layers are deposited on the substrate surface and in the cell holes.

[0011] As a preferred solution of a capacitor preparation method of the present invention, wherein: the protective layer is formed by a protective material through a cutting process;

[0012] The specific cutting process is:

[0013] Depositing the protective material on the top of the stacking layer, and dividing it into the substrate surface stacking layer protection and the cell hole stacking layer protection;

[0014] A photoresist is coated on the cell hole stacking layer protection, and the photoresist can protect the cell hole stacking layer protection from the plasma etching of dry etching;

[0015] After the photoresist coating is completed, the substrate surface is etched by plasma to eliminate the stacked layer protection on the substrate surface, and the cell hole stacked layer protection is retained, thereby forming a protective layer.

[0016] As a preferred solution of a capacitor preparation method of the present invention, the capacitor material includes a barrier layer, a lower electrode layer, a High-k electrical material, and an upper electrode layer.

[0017] As a preferred solution of the capacitor preparation method of the present invention, the capacitor materials on the stacked layers except the area covered by the protective layer are removed in sequence by dry etching on the surface of the substrate.

[0018] As a preferred embodiment of a capacitor preparation method of the present invention, a dielectric layer is deposited on a substrate, and the dielectric layer is polished to be parallel to the protective layer, including:

[0019] Filling a dielectric layer on the surface of the substrate and the protective layer;

[0020] The dielectric layer above the protective layer is removed by grinding, and the dielectric layer on the surface of the substrate is deposited to be parallel to the protective layer.

[0021] As a preferred solution of a capacitor preparation method of the present invention, wherein: a plate line is deposited on the top of the plane formed by the protective layer and the dielectric layer, and the plate line connects each protective layer and the upper electrode layer.

[0022] As a preferred solution of a capacitor preparation method of the present invention, wherein: the ratio of the depth and width of the cell hole is greater than 10:1, and the cell hole diameter is 150nm;

[0023] The cell holes can be formed by dry etching through the substrate surface.

[0024] As a preferred solution of a capacitor preparation method of the present invention, wherein: the deposition method of capacitor materials is atomic layer deposition;

[0025] The barrier layer uses tantalum nitride as the film component with a thickness of 10nm;

[0026] The lower electrode layer uses titanium nitride as the capacitor lower electrode component with a thickness of 10nm;

[0027] High-k electrical materials use zirconium oxide and hafnium oxide as the dielectric components of capacitors with a thickness of 10nm;

[0028] The upper electrode layer uses titanium nitride as the capacitor upper electrode component with a thickness of 10nm.

[0029] As a preferred solution of a capacitor preparation method of the present invention, the protective layer and the plate line can be deposited by a PVD process;

[0030] The protective material and plate wire use titanium as the film component;

[0031] The thickness of the protective material is 500nm and the thickness of the board line is 300nm.

[0032] As a preferred solution of a capacitor preparation method of the present invention, the dielectric layer can be deposited by a PECVD process;

[0033] The dielectric layer is made of silicon dioxide and has a thickness of 500nm-1000nm. The dielectric layer covers the gaps between adjacent substrates and the gaps between adjacent protective layers.

[0034] The dielectric layer can be polished by CMP process.

[0035] As a preferred solution of a capacitor preparation method of the present invention, wherein: the plasma etching of the shaping process, the precursors are CL2 and CLL4, and the surface protection of the dry-etched substrate;

[0036] Dry etching of substrate surface includes:

[0037] Plasma etching was used, with CL2 and CCL4 as precursors, to dry-etch the upper electrode layer outside the area covered by the protective layer;

[0038] Use plasma etching, the precursor is CF4, and the High-K electrical material outside the area covered by the dry etching protective layer;

[0039] Plasma etching was used, with CL2 and CCL4 as precursors, and the lower electrode layer outside the area covered by the protective layer was dry-etched;

[0040] Plasma etching is used, the precursor is CF4, and the isolation layer outside the area covered by the dry etching protective layer is formed.

[0041] The beneficial effects of the present invention are as follows: by adding a protective layer as a mask protection plate for etching the capacitor layer, damage to the inner membrane layer of the cell hole caused by maskless etching in the prior art is avoided, and the capacitor after etching is completely wrapped by the dielectric layer, avoiding the short circuit problem, and the etching process of the four-layer capacitor material is carried out in a centralized manner, avoiding the cross-contamination problem that may be caused by the process and the problem of low efficiency and high quality risks of the capacitor. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for describing the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative labor. Among them:

[0043] Figure 1 A schematic diagram of a capacitor hierarchical structure of a capacitor manufacturing method according to an embodiment of the present invention;

[0044] Figure 2 A schematic diagram of a preliminary substrate hole making process flow of a capacitor preparation method according to an embodiment of the present invention;

[0045] Figure 3 A schematic diagram of a process flow of a partition layer in a capacitor material in a capacitor preparation method according to an embodiment of the present invention;

[0046] Figure 4 A schematic diagram of the process flow of the lower electrode layer in the capacitor material of a capacitor preparation method according to an embodiment of the present invention;

[0047] Figure 5 A schematic diagram of a process flow of a High-K electrical material in a capacitor material in a capacitor preparation method according to an embodiment of the present invention;

[0048] Figure 6A schematic diagram of the process flow of an upper electrode layer in a capacitor material in a capacitor preparation method according to an embodiment of the present invention;

[0049] Figure 7 A schematic diagram of a protective material process flow of a capacitor preparation method according to an embodiment of the present invention;

[0050] Figure 8 A schematic diagram of a protective material deposition process flow of a capacitor preparation method according to an embodiment of the present invention;

[0051] Fig. 9 A schematic diagram of a process flow of a protective material being cut in a capacitor manufacturing method according to an embodiment of the present invention;

[0052] Fig.10 A schematic diagram of a process flow of dry etching on a substrate surface in a capacitor preparation method according to an embodiment of the present invention;

[0053] Fig.11 A schematic diagram of a process flow of dry etching on a substrate surface in a capacitor preparation method according to an embodiment of the present invention;

[0054] Fig.12 A schematic diagram of a process flow of dry etching on a substrate surface in a capacitor preparation method according to an embodiment of the present invention;

[0055] Fig.13 A schematic diagram of a process flow of dry etching on a substrate surface in a capacitor preparation method according to an embodiment of the present invention;

[0056] Fig.14 A schematic diagram of a dielectric layer deposition process flow of a capacitor preparation method according to an embodiment of the present invention;

[0057] Fig.15 A schematic diagram of a process flow of polishing a dielectric layer of a capacitor manufacturing method according to an embodiment of the present invention;

[0058] Fig.16 A schematic diagram of a plate line deposition process flow of a capacitor manufacturing method according to an embodiment of the present invention;

[0059] Fig.17 A schematic diagram of a plate line preparation process flow of a capacitor preparation method according to an embodiment of the present invention; DETAILED DESCRIPTION

[0060] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific implementation methods of the present invention are described in detail below in conjunction with the accompanying drawings.

[0061] In the following description, many specific details are set forth to facilitate a full understanding of the present invention, but the present invention may also be implemented in other ways different from those described herein, and those skilled in the art may make similar generalizations without violating the connotation of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.

[0062] Secondly, the present invention is described in detail with reference to schematic diagrams. When describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional diagrams showing the device structure will not be partially enlarged according to the general scale, and the schematic diagrams are only examples, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional dimensions of length, width and depth should be included.

[0063] Furthermore, the term "one embodiment" or "embodiment" as used herein refers to a specific feature, structure, or characteristic that may be included in at least one implementation of the present invention. The term "in one embodiment" that appears in different places in this specification does not necessarily refer to the same embodiment, nor does it refer to a separate or selective embodiment that is mutually exclusive with other embodiments.

[0064] Example 1

[0065] Reference Figure 1 , this embodiment provides a capacitor preparation method, comprising,

[0066] Capacitor materials are sequentially deposited on the substrate 100 to generate a stacked layer 200. The main component of the stacked layer 200 is four layers of capacitor materials stacked sequentially, and the four stacking methods are all deposited to generate thin films to achieve a stacking effect. The stacked layer 200 is essentially a capacitor body, which is used to store or release charges in the deep hole;

[0067] A protective layer 300 is laid on the top of the stacked layer 200. The protective layer 300 (Top plate) is designed to protect the stacked layer 200 in the cell hole. Its function is to resist the plasma bombardment during photolithography that affects the capacitor material in the cell hole. At the same time, the protective layer 300 also serves as an extension of the capacitor upper electrode in the same storage array, and is connected by aluminum plate wires to achieve unified driving;

[0068] The capacitor materials of the stacked layers 200 except the area covered by the protective layer 300 are removed in sequence. The area covered by the protective layer 300 is from the cell hole to the top of the upper opening. After filling the entire deep hole, a film of a certain thickness is formed at the opening. Due to the special composition of the protective layer 300, when the wafer surface is dry-etched, the capacitor materials in the cell hole are protected from any influence to avoid damage to the chip effect. The wafer surface area outside the cell hole will naturally be hit by the ions of the dry etching and will be completely eliminated.

[0069] A dielectric layer 400 is deposited on the substrate 100 and polished to be parallel to the protective layer 300. The dielectric layer 400 is used to completely isolate the capacitors from each other and wrap the sides of the capacitors to form insulation to prevent short circuits between the capacitors. The dielectric layer 400 needs to be polished to a horizontal thickness parallel to the protective layer 300 through a chemical mechanical polishing process so as to expose the protective layer 300 for connection with the board line.

[0070] The comparison between the existing technology and our capacitor generation method before the board line preparation and connection is as follows:

[0071] Existing technology: cell hole preparation - barrier layer deposition (tantalum nitride) - lower electrode deposition (titanium nitride 15nm) - lower electrode etching (maskless) - high dielectric material deposition (zirconium oxide / hafnium) - electrical material etching (maskless) - upper electrode deposition (titanium nitride 15nm) - upper electrode etching (maskless) - board line preparation

[0072] Our technology: cell hole preparation - barrier layer deposition (tantalum nitride) - bottom electrode deposition (titanium nitride 10nm) - High-K electrode deposition (zirconium oxide / hafnium) - top electrode deposition (titanium nitride 10nm) - protective layer 300 (Topplate) deposition - cutting process - substrate surface dry etching (TTiN, high-k, TaN) - dielectric layer 400 deposition - dielectric layer 400 polishing (CMP) - board line preparation

[0073] When the plate line is connected to the protective layer 300, the capacitor embedding process is completed. It can be clearly seen that compared with the prior art method of one deposition, one etching, and multiple cycles, multiple depositions, multiple etchings after protection are safer and more efficient, and capacitor quality problems are less likely to occur. The etched capacitor is completely wrapped by the dielectric layer 400 to avoid short circuit problems. The etching process of the four-layer capacitor material is concentrated to avoid cross contamination problems that may be caused by the process and the problem of low efficiency and high capacitor quality risks.

[0074] Example 2

[0075] Reference Figure 1 — Figure 6, which is the second embodiment of the present invention. This embodiment is based on the previous embodiment, and is different from the previous embodiment in that: in addition to the substrate surface 101, the substrate 100 is also arrayed with cell holes 102. The cell holes 102 serve as the embedding space of the capacitor and are arranged on the dielectric layer 400 of the array area (Array area) by dry etching, that is, the top of the substrate 100. The composition of the substrate 100 is a combination layer of silicon oxide and silicon nitride with a thickness of 1200nm. The aperture of the cell hole 102 determines the size and effect of the capacitor, and also determines the improvement point of the capacitor process in our technology.

[0076] The stacked layer 200 is deposited on the substrate surface 101 and in the cell hole 102. In the prior art, all the capacitor materials contained in the stacked layer 200 are formed by depositing once and etching once, and this process is repeated. However, such a process will also cause etching to the capacitor material in the cell hole 102 when the cell hole 102 has a high depth-width ratio and requires maskless dry etching. In the process implementation scheme of the High-K ferroelectric material high-temperature state memory, if the High-K layer is etched too much, it is very likely to cause a short circuit between the upper and lower electrodes, forming a potential risk;

[0077] So based on this point, the capacitor material of our capacitor process is deposited in multiple layers at one time without etching. The stacked layer 200 is a stack of capacitor materials and is spread flat on every part of the substrate surface 101, including the embedded area of ​​the cell hole 102, which is also covered with the stacked layer 200. It is necessary to distinguish the stacked layer 200 in the cell hole 102 from the stacked layer 200 on the substrate surface 101 to adapt to the improvement of the capacitor process.

[0078] Example 3

[0079] Reference Figure 7 — Fig. 9 , which is the second embodiment of the present invention, is based on the previous embodiment, and is different from the previous embodiment in that: the protective layer 300 is formed by a protective material through a shaving process, and the protective material is similar to the capacitor material. Only after the protective material undergoes a series of treatments can a complete and functional protective layer 300 be formed, and the treatment method is the shaving process;

[0080] The profiling process is equivalent to a combined process of photolithography and etching, but the etching object selected in the profiling process is different from the existing technology. This difference also brings about improvements to the entire process after photolithography and development.

[0081] The protective material is deposited on the top of the stacking layer 200 and is divided into the substrate surface stacking layer protection and the cell hole stacking layer protection, which also corresponds to the above-mentioned stacking layer 200 being divided into the substrate surface 101 part and the cell hole 102 part. The ultimate purpose of the shaping process is mainly to remove the substrate surface stacking layer protection;

[0082] Therefore, according to the photolithography process, photoresist is first coated on the entire protective material, and then the required photoresist area is reserved through a mask to form a photoresist that only exists on the cell hole stacking layer protection. In this way, the photoresist can protect the cell hole stacking layer protection from the plasma etching of dry etching;

[0083] After the photoresist coating is completed, the substrate surface 101 is etched by plasma. Since the stacked layer protection on the substrate surface is not covered by the photoresist, the stacked layer protection on the substrate surface is completely etched, and the cell hole stacked layer protection is retained, thereby forming a protection layer 300;

[0084] That is to say, the protection layer 300 only refers to the protection material (thin film) deposited on the cell hole stacking layer.

[0085] Example 4

[0086] Reference Figure 1 and Fig. 9 — Fig.13 , which is the second embodiment of the present invention, is based on the previous embodiment, and is different from the previous embodiment in that: the capacitor material includes a blocking layer 201, a lower electrode layer 202, a High-K electrical material 202, and an upper electrode layer 201. In the prior art, High-K is generally used in the transistor part of a 1t1c storage unit as a High-K matalgate process, a technology used to solve the problem of MOS tube size below 45nm. As a high dielectric material in DRAM, it is an unprecedented attempt to use its polarity to realize storage function;

[0087] Furthermore, in order to ensure the integrity of the capacitor, the capacitor is constructed by laying the capacitor material. The barrier layer isolates the metal material through the characteristics of its material to prevent metal particles from diffusing in the dielectric layer 400. Compared with the existing technology, in addition to the bold use of High-K materials, overcoming the technical difficulties brought by high-dielectric ferroelectric High-K materials is the value of the entire capacitor process.

[0088] Example 5

[0089] Reference Fig. 9 — Fig.13, which is the second embodiment of the present invention, is based on the previous embodiment, and is different from the previous embodiment in that: by dry etching the substrate surface 101, the capacitor materials on the stacking layer 200 except the area covered by the protective layer 300 are removed in sequence, and the protective layer 300 above the stacking layer 200 only exists at the top of the cell hole 102, that is, the dry etching of the substrate surface 101 refers to the removal and dry etching of the stacking layer 200 on the substrate surface 101 outside the cell hole 102, and will not involve any stacking layer 200 in the cell hole 102, and the main reason why the cell hole 102 will not be affected is because of the intervention of the protective layer 300;

[0090] According to the above description of the stacking layer 200 and the protective material, it can be understood that the cell hole 102 is now filled with the stacking layer 200 and the protective layer 300, and only the stacking layer 200 exists on the substrate surface 101, so the substrate surface 101 will be fully affected by the etching, and the stacking layer 200 will be completely removed. The specific removal requires some confirmed steps and methods, which is also the specific content of "dry etching of the substrate surface 101".

[0091] Example 6

[0092] Reference Fig.14 — Fig.17 , which is the second embodiment of the present invention, is based on the previous embodiment, and is different from the previous embodiment in that: a dielectric layer 400 is deposited on the substrate 100, and the dielectric layer 400 is polished to be parallel to the protective layer 300. This action includes:

[0093] After the substrate surface 101 is dry-etched, there is no other substance on the substrate surface 101, the stacked layer 200 in the cell hole 102 is intact, and the protective layer 300 is still provided on the top. On this basis, the dielectric layer 400 is filled on the substrate surface 101 and the protective layer 300. Since the substrate surface 101 and the protective layer 300 are not on the same horizontal plane, the first filling result of the dielectric layer 400 is not a complete plane, and the dielectric layer 400 is uneven.

[0094] The uneven dielectric layer 400 will affect the connection between the electrode plate and the plate line, so it is necessary to remove the raised part, that is, the dielectric layer 400 above the protective layer 300, by grinding, and then deposit the dielectric layer 400 on the substrate surface 101 to be parallel to the protective layer 300. This completes the stacking and flattening of the entire dielectric layer 400, and allows the top surface of the protective layer 300 to be exposed for easy wiring.

[0095] Example 7

[0096] Reference Figure 5, which is the second embodiment of the present invention. This embodiment is based on the previous embodiment, and is different from the previous embodiment in that: a plate line is deposited on the top of the plane formed by the protective layer 300 and the dielectric layer 400, and the plate line is used to realize the unified driving of each upper electrode plate line in the entire storage array. The plate line is also laid by deposition, and each protective layer 300 and the upper electrode layer 201 are formed and connected on the plane by photolithography and wet etching.

[0097] Example 8

[0098] Reference Fig.16 — Fig.17 , which is the third embodiment of the present invention, is based on the previous embodiment, and is different from the previous embodiment in that: the depth and width ratio of the cell hole 102 is greater than 10:1, and the diameter of the cell hole 102 is 150nm. Compared with the diameter of 150nm, this aspect ratio is quite difficult to process, and the cell hole 102 needs to be formed by dry etching through the substrate surface 101. The traditional photolithography and wet etching process is not suitable for such a large aspect ratio.

[0099] As a memory with embedded capacitors, the width of the cell hole 102 determines the density of the storage unit. The smaller the width, the more capacitors can be arranged, but the difficulty of preparation will also increase relatively. The depth of the cell hole 102 determines the area of ​​the upper and lower capacitors. [Capacitance formula: C = εA / d, (ε is the dielectric capacitance constant, determined by the material itself), A represents the parallel plate area, d represents the parallel plate spacing, that is, the dielectric thickness], so in the preparation process of the cell hole 102, the deeper the depth, the greater the depth-to-width ratio of the upper and lower electrodes, the greater the capacitance, and the greater the difficulty of preparation;

[0100] However, the aspect ratio of our cell hole 102 is relatively high (greater than 10:1), so the difficulty of preparation is also relatively high. According to the mask lithography scheme commonly used in the prior art, the photoresist in the hole cannot be completely removed during the yellow light process, resulting in abnormal coating of titanium nitride and High-K materials. Therefore, only a maskless dry etching method can be used to form the cell hole 102.

[0101] Example 9

[0102] Reference Figure 1 — Figure 6 , which is the second embodiment of the present invention, is based on the previous embodiment, and is different from the previous embodiment in that: the deposition method of the capacitor material can adopt atomic layer deposition, and the atomic layer deposition is to form a new atomic film by replacing particles between the bottom layer of deposition and the new layer of deposition, so the upper and lower atomic films are related, and the components used for deposition of each layer of capacitor material and the thickness of the deposition are clearly specified;

[0103] The bottom barrier layer uses tantalum nitride as the film component with a thickness of 10nm;

[0104] The following lower electrode layer 202 uses titanium nitride as the capacitor lower electrode component, with a thickness of 10nm;

[0105] The middle and most important High-K material 202 uses zirconium oxide and hafnium oxide as the dielectric components of the capacitor, with a thickness of 10nm;

[0106] The top electrode layer 201 uses titanium nitride as the capacitor top electrode component and has a thickness of 10 nm.

[0107] Each layer will react with each other, so the composition needs to be determined, and the thickness is also determined based on the capacitance.

[0108] Example 10

[0109] Reference Figure 7 — Fig.16 , which is the second embodiment of the present invention. This embodiment is based on the previous embodiment, and is different from the previous embodiment in that: the protective layer 300 and the plate line can be deposited by a PVD process, also known as physical vapor deposition. This deposition method is to deposit physically in a vacuum environment. Here, the protective plate and the plate line are deposited by a physical magnetron sputtering method, which uses plasma Ar+ to bombard a metal titanium target to deposit a titanium film on the substrate 100;

[0110] Therefore, the main component of the protective material and the plate line is titanium, which is used as a film component;

[0111] The thickness of protective material is 500nm, and the thickness of plate line is 300nm;

[0112] Because the protection layer 300 is used as a shielding layer for subsequent etching of the capacitor film layer, it requires a higher strength, so the thickness is relatively high.

[0113] Embodiment 11

[0114] Reference Fig.14 — Fig.15 , which is the second embodiment of the present invention. This embodiment is based on the previous embodiment, and is different from the previous embodiment in that: the deposition method of the dielectric layer 400 can adopt the PECVD process, also known as plasma enhanced chemical vapor deposition. This deposition method uses glow discharge to produce chemical deposition, excites gas, and generates low-temperature plasma, and then forms a solid film by epitaxy. Because the laying object of the dielectric layer 400 is the entire substrate 100 and the gaps between the substrates 100, this chemical deposition method is required to meet the overall coverage deposition requirements;

[0115] The dielectric layer 400 is made of silicon dioxide and has a thickness of 500nm-1000nm. The thickness of 500nm is located in the small gap on the substrate 100, and the thickness of 1000nm is located in the gap between the substrates 100 and the substrates 100. The dielectric layer 400 wraps the gap between adjacent substrates 100 and the gap between adjacent protective layers 300 to achieve the barrier effect, avoiding the occurrence of short circuits or other problems caused by the crossing of lines;

[0116] The dielectric layer 400 may be polished by a CMP process, also known as a chemical mechanical polishing process, which is mainly used for the final flatness processing of the silicon surface.

[0117] Example 12

[0118] Reference Fig. 9 — Fig.13 , which is the second embodiment of the present invention, and is based on the previous embodiment, and is different from the previous embodiment in that: the plasma etching of the shaping process, the precursors are CL2 and CLL4, and the surface 101 of the dry-etched substrate is protected;

[0119] The substrate surface 101 is dry-etched, i.e., plasma-etched, and its main content is to erode the capacitor material by acting as a precursor of the etching gas, including:

[0120] Plasma etching is used, with precursors of CL2 and CCL4, to dry-etch the upper electrode layer 201 outside the area covered by the protective layer 300;

[0121] Plasma etching is used, the precursor is CF4, and the High-K electrical material 202 outside the area covered by the protective layer 300 is dry-etched;

[0122] Plasma etching is used, with precursors of CL2 and CCL4, to dry-etch the lower electrode layer 202 outside the area covered by the protective layer 300;

[0123] Plasma etching is used, with CF4 as the precursor, to dry-etch the isolation layer 201 outside the area covered by the protective layer 300.

[0124] Each layer of capacitor material is corroded by a specific precursor and deposited by a specific atomic layer. Since the laying and corrosion of the capacitor material are processed centrally after the protective layer 300 is deposited, both the preparation efficiency and the preparation safety are greatly improved compared to the existing technology.

[0125] Importantly, it should be noted that the construction and arrangement of the present application shown in a plurality of different exemplary embodiments are only exemplary. Although only a few embodiments are described in detail in this disclosure, it should be readily understood by those who refer to this disclosure that many modifications are possible (e.g., the size, scale, structure, shape and proportion of various elements, and parameter values ​​(e.g., temperature, pressure, etc.), installation arrangement, use of materials, color, directional changes, etc.) without substantially departing from the novel teachings and advantages of the subject matter described in the application. For example, the element shown as integrally formed can be composed of multiple parts or elements, the position of the element can be inverted or otherwise changed, and the nature or number or position of the discrete element can be changed or changed. Therefore, all such modifications are intended to be included in the scope of the present invention. The order or sequence of any process or method steps can be changed or reordered according to alternative embodiments. In the claims, any "device plus function" clause is intended to cover the structure of performing the function described herein, and is not only structurally equivalent but also equivalent structure. Without departing from the scope of the present invention, other replacements, modifications, changes and omissions can be made in the design, operating conditions and arrangement of the exemplary embodiments. Therefore, the invention is not limited to a specific embodiment, but extends to several modifications still falling within the scope of the appended claims.

[0126] Additionally, in order to provide a concise description of exemplary embodiments, all features of an actual embodiment (ie, those features that are not relevant to the best mode presently contemplated for carrying out the invention or those that are not relevant to implementing the invention) may not be described.

[0127] It will be appreciated that in the development of any actual implementation, as in any engineering or design project, numerous implementation-specific decisions may be made. Such a development effort may be complex and time-consuming, but will be a routine task of design, fabrication, and production for those of ordinary skill having the benefit of this disclosure without undue experimentation.

[0128] It should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solutions of the present invention may be modified or replaced by equivalents without departing from the spirit and scope of the technical solutions of the present invention, which should all be included in the scope of the claims of the present invention.

Claims

1. A method for preparing a capacitor, characterized in that: include, Depositing capacitor materials in sequence on a substrate (100) to form a stacked layer (200); Laying a protective layer (300) on top of the stacked layer (200); sequentially removing the capacitor material on the stacked layers (200) except for the area covered by the protective layer (300); A dielectric layer (400) is deposited on the substrate (100), and the dielectric layer (400) is polished until it is parallel to the protective layer (300).

2. The capacitor preparation method according to claim 1, characterized in that: The substrate (100) is arrayed with cell holes (102), and the stacked layer (200) is deposited on the substrate surface (101) and in the cell holes (102).

3. The capacitor preparation method according to claim 2, characterized in that: The protective layer (300) is formed from the protective material through a cutting process; The cutting process is specifically as follows: Depositing the protective material on the top of the stacked layer (200) and dividing it into a substrate surface stacked layer protection and a cell hole stacked layer protection; Coating a photoresist on the cell hole stacking layer protection, the photoresist can protect the cell hole stacking layer protection from being affected by dry etching plasma etching; After the photoresist coating is completed, the substrate surface (101) is etched with plasma to remove the stacked layer protection on the substrate surface, and the cell hole stacked layer protection is retained, thereby forming the protection layer (300).

4. The capacitor preparation method according to claim 3, characterized in that: The capacitor material comprises a barrier layer (201), a lower electrode layer (202), a High-K electrical material (203), and an upper electrode layer (204).

5. The capacitor preparation method according to claim 3, characterized in that: By dry etching the surface of the substrate, the capacitor material on the stacked layer (200) except the area covered by the protective layer (300) is removed in sequence.

6. The capacitor preparation method according to claim 6, characterized in that: The step of depositing a dielectric layer (400) on the substrate (100) and polishing the dielectric layer (400) to be parallel to the protective layer (300) comprises: Filling the dielectric layer (400) on the substrate surface (101) and the protective layer (300); The dielectric layer (400) above the protective layer (300) is removed by grinding, and the dielectric layer (400) on the substrate surface (101) is deposited to be parallel to the protective layer (300).

7. The capacitor preparation method according to claim 6, characterized in that: A plate line is deposited on the top of the plane formed by the protective layer (300) and the dielectric layer (400), and the plate line connects each of the protective layers (300) and the upper electrode layer (204).

8. The capacitor preparation method according to claim 2, characterized in that: The ratio of the depth to the width of the cell hole (102) is greater than 10:1, and the diameter of the cell hole (102) is 150 nm; The cell holes (102) can be formed by drilling through the substrate surface (101) through dry etching.

9. The capacitor preparation method according to claim 4, characterized in that: The deposition method of the capacitor material is atomic layer deposition; The barrier layer uses tantalum nitride as a film component with a thickness of 20nm; The lower electrode layer (202) uses titanium nitride as the capacitor lower electrode component, with a thickness of 20 nm; The High-K electrical material (203) uses zirconium oxide and hafnium oxide as dielectric components of the capacitor, and has a thickness of 20 nm; The upper electrode layer (204) uses titanium nitride as the capacitor upper electrode component and has a thickness of 20 nm.

10. The capacitor preparation method according to claim 7, characterized in that: The protective layer (300) and the plate line can be deposited using a PVD process; The protective material and the plate wire use titanium as a film component; The thickness of the protective material is 500nm, and the thickness of the plate line is 300nm.

11. The capacitor preparation method according to claim 8, characterized in that: The dielectric layer (400) may be deposited using a PECVD process; The dielectric layer (400) is made of silicon dioxide and has a thickness of 500nm-2000nm. The dielectric layer (400) covers the gaps between adjacent substrates (100) and the gaps between adjacent protective layers (300); The dielectric layer (400) may be polished using a CMP process.

12. The capacitor preparation method according to claim 9, characterized in that: The plasma etching of the cutting process, the precursors are CL2 and CLL4, and the surface protection of the substrate is dry-etched; The substrate surface dry etching comprises: Using plasma etching, with precursors of CL2 and CCL4, to dry-etch the upper electrode layer (204) outside the area covered by the protective layer (300); Using plasma etching, with CF4 as the precursor, to dry-etch the High-K electrical material (203) outside the area covered by the protective layer (300); Using plasma etching, with precursors of CL2 and CCL4, to dry-etch the lower electrode layer (202) outside the area covered by the protective layer (300); Plasma etching is used, with CF4 as the precursor, to dry-etch the isolation layer (201) outside the area covered by the protective layer (300).