Preparation method of stable nanogold sol

CN119457107APending Publication Date: 2025-02-18SUZHOU XINGHAN NEW MATERIAL TECH CO LTD

Patent Information

Application Number
CN202411594837.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-11-10
Publication Date
2025-02-18

Smart Images

  • Figure CN119457107A_ABST
    Figure CN119457107A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation method of stable nanogold sol, which comprises the following steps: mixing a reducing agent solution, a stabilizer solution and deionized water to obtain a mixed solution A; mixing a chloroauric acid solution, a stabilizer solution and deionized water to obtain a mixed solution B; if a high-concentration and large-system mixed solution is prepared, the mixed solution A is subjected to heating treatment and a chloroauric acid solution is added for reaction, otherwise, the mixed solution B can be subjected to heating treatment and a reducing agent solution is added for reaction, and the mixed solution A can be subjected to heating treatment and a chloroauric acid solution is added for reaction; after the reaction is finished, cooling is conducted, nanogold sol is obtained, and the obtained nanogold sol is stored; according to the concentration of the prepared mixed solvent and the size of the system, the reagent adding sequence in the preparation process is changed, and the particle size, the morphology, the dispersity and the stability of the nanogold sol are regulated and controlled.
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Method for preparing fluorescence nano gold sol by using PVP (Poly Vinyl Pyrrolidone) through reduction modification under hydrothermal condition

    CN102990082A

  • Preparing technology of gold nanoparticles

    CN105081344A

  • Preparation method for gold nanoparticles

    CN105689732A

  • Synthesis of colloidal precious metal nanoparticles with controlled size and morphology

    CN106794448A

  • Preparation method of gold nanoparticle sol and composite optical film thereof

    CN115740478A

Cited By

  • Preparation method of high-sphericity gold powder

    CN121491357A

  • Preparation method of high sphericity gold powder

    CN121491357B