A medical pressure band based on nylon-spandex elastic fleece and its preparation method

By pretreating the nylon-amylene elastic fleece and applying a composite phthalocyanine powder coating, the problems of single antibacterial properties, insufficient coating adhesion, and uneven function in existing medical pressure belts have been solved, resulting in a multifunctional and highly stable medical pressure belt suitable for clinical infection prevention and postoperative care.

CN121944189BActive Publication Date: 2026-11-17CHANGZHOU BEAUTIFUL KNITTING TECH
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202610141150.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2026-02-02
Publication Date
2026-11-17
Estimated Expiration
2046-02-02

AI Technical Summary

Technical Problem

Existing medical pressure bands have a single antibacterial mechanism, are prone to drug resistance, have insufficient coating adhesion, low functional integration, poor substrate elasticity, and uneven dispersion of functional components due to the manufacturing process, which affects the stability of product performance.

Method used

The product uses nylon-ammonia elastic fleece pre-treated with alkali and acid washing, combined with ε-polylysine as the bottom coating, and coated with composite phthalocyanine powder. It utilizes the electrostatic effect and covalent bond of phthalocyanine substances, combined with photodynamic mechanism and oxidase catalytic activity, to achieve multifunctional antibacterial and deodorizing effects. Furthermore, the coating uniformity is ensured by the use of additives and a mild impregnation process.

Benefits of technology

It achieves high stability and biocompatibility in multifunctional medical pressure belts, possesses broad-spectrum antibacterial and deodorizing functions, has strong coating adhesion, and is suitable for clinical infection prevention and postoperative care.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN121944189B_ABST
    Figure CN121944189B_ABST
Patent Text Reader

Abstract

This invention discloses a medical pressure band based on nylon-ammonia elastic fleece and its preparation method, belonging to the field of medical pressure band technology. The nylon-ammonia elastic fleece is pretreated with alkali and acid washing, then immersed in an ε-polylysine solution to form a base layer coating. A composite phthalocyanine powder consisting of water-soluble phthalocyanine dye, monosubstituted β-carboxylated zinc phthalocyanine, and iron phthalocyanine derivatives is dispersed, pH adjusted, and additives are added to prepare a slurry. This slurry is then used to impregnate the substrate with the base layer coating, followed by pre-drying and curing to obtain the finished product. This pressure band integrates highly efficient antibacterial, deodorizing, and dyeing functions. It features strong coating adhesion, washability, durability, elastic fit to the substrate, and high biocompatibility, making it suitable for clinical infection prevention, postoperative care, and other scenarios.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of medical pressure belt technology, specifically a medical pressure belt based on nylon-spandex elastic fleece and its preparation method. Background Technology

[0002] Medical pressure bands, as commonly used clinical medical consumables, are widely used in postoperative hemostasis, edema prevention, and wound care. Their functionality and practicality directly affect treatment outcomes and patient experience. Currently, existing medical pressure bands generally suffer from several technical bottlenecks: First, their antibacterial mechanisms are limited, often relying on a single antibacterial component, which has limited inhibitory effects on drug-resistant bacteria (such as MRSA), and long-term use can easily lead to bacterial resistance, making it difficult to meet clinical infection prevention needs; second, the coating adhesion is insufficient, and antibacterial or functional components are easily detached, with significant performance degradation after repeated washing and poor durability; third, the functional integration is low, with most products only possessing basic compression functions and lacking deodorizing properties, leading to odors from sweat and bacterial metabolism during patient use, affecting the user experience; fourth, some products have poor substrate elasticity and insufficient fit, or the biosafety of the raw materials needs improvement, which may cause irritation with prolonged skin contact; fifth, some manufacturing process parameters are unreasonable, resulting in uneven dispersion of functional components and affecting product performance stability.

[0003] These issues collectively limit the clinical application effectiveness of medical pressure bands, necessitating the development of a multifunctional, highly stable, and well-adaptable medical pressure band. Summary of the Invention

[0004] The purpose of this invention is to provide a medical pressure band based on nylon-spandex elastic fleece and its preparation method, so as to solve the problems raised in the prior art.

[0005] To achieve the above objectives, the present invention provides the following technical solution: A method for preparing a medical pressure band based on nylon-spandex elastic fleece includes the following steps: S1: Quinoline-5-sulfonic acid, phthalonitrile, and metal salt are added to N,N-dimethylethanolamine and stirred until homogeneous. Then, 1,8-diazabicyclo[5.4.0]undec-7-ene is added and heated to 40-50℃ for 10-12 hours. The mixture is filtered to remove insoluble impurities, and the filtrate is distilled under reduced pressure, recrystallized with methanol, and dried under vacuum to obtain water-soluble phthalocyanine dye. Furthermore, in the preparation process of the water-soluble phthalocyanine dye, the molar ratio of quinoline-5-sulfonic acid: phthalonitrile: metal salt is (4-6):(4-5):1; the amount of 1,8-diazabicyclo[5.4.0]undec-7-ene added is 8-12% of the mass of phthalonitrile; Furthermore, the metal salt includes either copper chloride or cobalt chloride; S2: Phthalic anhydride, monocarboxylated phthalic anhydride and zinc chloride are added to nitrobenzene, heated to 170-180℃ for 3-4 hours, cooled to room temperature, filtered and collected the product, and washed with nitrobenzene and methanol in sequence until the washing solution is colorless. The product is then dried under vacuum to obtain monosubstituted β-carboxylated zinc phthalocyanine. Furthermore, in the preparation process of the monosubstituted β-carboxylated zinc phthalocyanine, the molar ratio of phthalic anhydride to monocarboxylated phthalic anhydride is (3-4):1; the amount of zinc chloride added is 15-20% of the total mass of phthalic anhydride and monocarboxylated phthalic anhydride. S3: Trimeric triglyceride, urea, and ferric chloride were added to nitrobenzene, and ammonium molybdate was added. The mixture was heated to 160-170℃ and reacted for 3-4 hours. After cooling to room temperature, the product was collected by filtration. The product was washed with methanol, and then the product was added to 50% potassium hydroxide solution and heated to 100-105℃ for 24 hours to hydrolyze. The pH was acidified to 2-3, filtered, washed, and dried to obtain the iron phthalocyanine derivative. Furthermore, in the preparation process of the iron phthalocyanine derivative, the molar ratio of trimellitic anhydride, urea, and ferric chloride is 1:(4-6):(0.25-0.3); the amount of ammonium molybdate added is 3-5% of the mass of trimellitic anhydride. S4: Soak the nylon-spandex elastic fleece in a sodium hydroxide solution with a concentration of 8-12 wt% at 45-55℃ for 25-35 minutes, then soak it in a hydrochloric acid solution with a concentration of 12-18 wt% at room temperature for 15-25 minutes, wash it with deionized water until the washing solution is neutral, and dry it at 60-70℃ to obtain the pretreated nylon-spandex elastic fleece. Furthermore, the nylon-spandex elastic fleece is woven from 30D / 12F Nylon DTY, 30D / 1F Nylon FDY, and 30D spandex using a 32-needle single-needle bed warp knitting machine; specifications: weight is 180-190g / m2; S5: Add ε-polylysine to deionized water and stir evenly to obtain an ε-polylysine solution; immerse the pretreated nylon-spandex elastic fleece in the ε-polylysine solution, heat to 35-40℃ and stir to adsorb for 25-35 minutes, take it out, wash with deionized water, and dry at 60-65℃ to obtain a nylon-spandex elastic fleece with a bottom coating. Furthermore, in the preparation process of the nylon-spandex elastic fleece with the undercoat, the concentration of the ε-polylysine solution is 500-1500 ppm; the bath ratio of the pretreated nylon-spandex elastic fleece to the ε-polylysine solution is 1:(15-25). S6: Water-soluble phthalocyanine dye, monosubstituted β-carboxylated zinc phthalocyanine, and iron phthalocyanine derivative are mixed evenly to obtain composite phthalocyanine powder; the composite phthalocyanine powder is added to deionized water, and Pingping O is added, and ultrasonically dispersed to obtain a phthalocyanine dispersion with a concentration of 8-12 g / L; the pH of the phthalocyanine dispersion is adjusted to 4-5 using acetic acid, and then 2-3 wt% fatty alcohol polyoxyethylene ether is added and stirred evenly to obtain phthalocyanine composite slurry; Furthermore, in the preparation process of the composite phthalocyanine powder, the mass ratio of water-soluble phthalocyanine dye: monosubstituted β-carboxylated phthalocyanine zinc: iron phthalocyanine derivative is (4-6):(2-3):(1-2); the amount of Pingpingjia O added is 5-8% of the mass of the composite phthalocyanine powder; S7: Immerse the nylon-spandex elastic fleece with a base coating into phthalocyanine composite slurry at a liquor ratio of 1:(20-30), heat to 95-105℃ for dyeing for 25-35 minutes, remove, rinse with deionized water, pre-dry at 60-70℃ for 10-15 minutes, and cure at 100-110℃ for 1.5-2.5 hours to obtain functional nylon-spandex elastic fleece; melt the surface of medical polyester foam with a flame and press it onto the functional nylon-spandex elastic fleece to obtain a medical pressure band; Furthermore, in the medical pressure band, the thickness of the ε-polylysine underlayer coating is 10-20 μm, and the thickness of the phthalocyanine composite functional layer is 20-30 μm; Furthermore, the medical polyester foam has a thickness of 2.3 mm and a density of 110 kg / m³. Furthermore, the thickness of the medical polyester foam melted during the flame melting process is 0.6-0.65 mm on both sides; Furthermore, the preparation method of the ε-polylysine includes the following steps: using glucose as a carbon source and ammonium sulfate as a nitrogen source, fermenting with Streptomyces at 28-30℃ and pH=6.5-7 for 72-96h, centrifuging the fermentation broth to remove the bacterial cells, passing the supernatant through a cation exchange resin for adsorption and elution, concentrating the eluent under reduced pressure and then freeze-drying to obtain ε-polylysine powder; Furthermore, in the preparation process of the ε-polylysine, the glucose concentration is 20-30 g / L and the ammonium sulfate concentration is 5-8 g / L.

[0006] Compared with the prior art, the beneficial effects of the present invention are: 1. This invention uses nylon-amylene elastic fleece pre-treatment with alkali washing and acid washing to remove surface impurities and increase active sites, providing a stable bonding foundation for subsequent coatings, ensuring that the elasticity of the pressure band substrate is not damaged and the coating adhesion is significantly improved; using ε-polylysine as the bottom coating, its cationic properties form an electrostatic interaction with the bacterial cell membrane to disrupt the membrane integrity, while the amine groups form covalent bonds with the upper phthalocyanine substances, achieving basic antibacterial properties against Gram-positive and Gram-negative bacteria, enhancing the wash resistance and stability of the composite coating, and ensuring that its biosafety ensures no skin irritation in medical settings.

[0007] 2. In the composite phthalocyanine powder prepared by this invention, the water-soluble phthalocyanine dye forms ionic bonds with the substrate through substituents such as quinoline-5-sulfonic acid, thereby disrupting the bacterial metabolic enzyme system, achieving uniform staining and broad-spectrum antibacterial properties, while also exhibiting excellent wet fastness and light fastness; the monosubstituted β-carboxylated zinc phthalocyanine generates reactive oxygen species through photodynamic mechanisms under visible light irradiation, oxidizing and destroying bacterial biomolecules, effectively killing drug-resistant bacteria without easily inducing drug resistance; the iron phthalocyanine derivative, with its oxidase-like catalytic activity, decomposes odor substances through cyclic redox reactions, while synergistically enhancing the efficiency of reactive oxygen species generation, thus endowing the pressure belt with deodorizing function and antibacterial synergistic effect.

[0008] 3. This invention further improves the dispersibility of phthalocyanine components through the synergistic effect of additive Pingpingjia O and fatty alcohol polyoxyethylene ether, adjusts pH to promote the bonding between phthalocyanine and the substrate, and avoids damage to the substrate performance through gentle impregnation and curing processes. The three together ensure the uniformity of coating function. The chemical bonding between the substrate and the composite layer and the functional complementarity of the triphthalocyanine components form a synergistic effect, ultimately enabling the medical pressure band to integrate multiple functions such as antibacterial, deodorizing, dyeing, and elastic adhesion, and has good durability, stability and biocompatibility, making it suitable for clinical infection prevention, postoperative care and other scenarios. Attached Figure Description

[0009] Figure 1 This is a schematic diagram of the structure of the medical pressure band of the present invention; Figure 2 This is a schematic diagram of the medical pressure band of the present invention; Figure 3 This is a schematic diagram of the structure of the nylon-spandex elastic fleece fabric of the present invention. Detailed Implementation

[0010] The technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0011] The following examples illustrate the preparation method of water-soluble phthalocyanine dye, which includes the following steps: adding quinoline-5-sulfonic acid, phthalonitrile, and copper chloride to N,N-dimethylethanolamine, stirring until homogeneous, adding 1,8-diazabicyclo[5.4.0]undec-7-ene, heating to 45°C and reacting for 11 hours, filtering to remove insoluble impurities, distilling the filtrate under reduced pressure, adding methanol for recrystallization, and drying under vacuum to obtain water-soluble phthalocyanine dye; In the preparation of water-soluble phthalocyanine dyes, the molar ratio of quinoline-5-sulfonic acid: phthalonitrile: metal salt is 4:4:1; the amount of 1,8-diazabicyclo[5.4.0]undec-7-ene added is 8% of the mass of phthalonitrile; The preparation method of monosubstituted β-carboxylated zinc phthalocyanine includes the following steps: adding phthalic anhydride, monocarboxylated phthalic anhydride and zinc chloride into nitrobenzene, heating to 175℃ and reacting for 3.5h, cooling to room temperature, filtering and collecting the product, washing the product sequentially with nitrobenzene and methanol until the washing solution is colorless, and drying under vacuum to obtain monosubstituted β-carboxylated zinc phthalocyanine; In the preparation of monosubstituted β-carboxylated zinc phthalocyanine, the molar ratio of phthalic anhydride to monocarboxylated phthalic anhydride is 3:1; the amount of zinc chloride added is 15% of the total mass of phthalic anhydride and monocarboxylated phthalic anhydride.

[0012] The preparation method of iron phthalocyanine derivative includes the following steps: adding trimellitic anhydride, urea, and ferric chloride to nitrobenzene, adding ammonium molybdate, heating to 165℃ and reacting for 3.5h, cooling to room temperature, filtering and collecting the product, washing the product with methanol, then adding the product to 50% potassium hydroxide solution, heating to 100℃ and hydrolyzing for 24h, acidifying the pH to 2, filtering, washing, and drying to obtain iron phthalocyanine derivative; In the preparation of the iron phthalocyanine derivative, the molar ratio of trimellitic anhydride, urea, and ferric chloride is 1:4:0.25; the amount of ammonium molybdate added is 3% of the mass of trimellitic anhydride.

[0013] The preparation method of ε-polylysine includes the following steps: using glucose as a carbon source and ammonium sulfate as a nitrogen source, Streptomyces is heated to 28°C and pH=6.5 and fermented for 72 hours. The fermentation broth is centrifuged to remove the bacterial cells. The supernatant is adsorbed and eluted through a cation exchange resin. The eluent is concentrated under reduced pressure and then freeze-dried to obtain ε-polylysine powder. In the preparation of ε-polylysine, the glucose concentration was 20 g / L and the ammonium sulfate concentration was 5 g / L.

[0014] Example 1: A method for preparing a medical pressure band based on nylon-ammonia elastic fleece, comprising the following steps: S1: Immerse the nylon-ammonia elastic fleece in a sodium hydroxide solution with a concentration of 8 wt% at 50°C for 25 min, then immerse it in a hydrochloric acid solution with a concentration of 12 wt% at room temperature for 15 min, wash it with deionized water until the washing solution is neutral, and dry it at 60°C to obtain a pretreated nylon-ammonia elastic fleece; S2: Add ε-polylysine to deionized water and stir evenly to obtain a 1000ppm ε-polylysine solution; immerse the pretreated nylon-spandex elastic fleece in the ε-polylysine solution, heat to 35℃ and stir to adsorb, take it out, wash with deionized water, and dry to obtain a nylon-spandex elastic fleece with a bottom coating. S3: Water-soluble phthalocyanine dye, monosubstituted β-carboxylated zinc phthalocyanine, and iron phthalocyanine derivative are mixed evenly to obtain composite phthalocyanine powder; the composite phthalocyanine powder is added to deionized water, 6wt% of Pingpingjia O is added, and ultrasonic dispersion is performed to obtain a 10g / L phthalocyanine dispersion; the pH of the phthalocyanine dispersion is adjusted to 4, and then 2.5wt% fatty alcohol polyoxyethylene ether is added and stirred evenly to obtain phthalocyanine composite slurry; In the composite phthalocyanine powder, the mass ratio of water-soluble phthalocyanine dye: monosubstituted β-carboxylated phthalocyanine zinc: iron phthalocyanine derivative is 5:2.5:1.5. S4: Immerse the nylon-spandex elastic fleece with the bottom coating into phthalocyanine composite slurry at a liquor ratio of 1:25 and dye at 100°C. Remove the fleece, rinse with deionized water, pre-dry at 65°C for 12 minutes, and cure at 105°C for 2 hours to obtain the functional nylon-spandex elastic fleece. Flame melt the surface of the medical polyester foam and press it onto the functional nylon-spandex elastic fleece to obtain the medical pressure band.

[0015] In the medical pressure band, the thickness of the ε-polylysine bottom coating is 15μm and the thickness of the phthalocyanine composite functional layer is 25μm.

[0016] Example 2: A method for preparing a medical pressure band based on nylon-amylene elastic fleece, comprising the following steps: S1: Soaking the nylon-amylene elastic fleece in a sodium hydroxide solution with a concentration of 8 wt% at 50°C for 25 min, then soaking it in a hydrochloric acid solution with a concentration of 12 wt% at room temperature for 15 min, washing it with deionized water until the washing solution is neutral, and drying it at 60°C to obtain a pretreated nylon-amylene elastic fleece; S2: Add ε-polylysine to deionized water and stir evenly to obtain a 1500ppm ε-polylysine solution; immerse the pretreated nylon-spandex elastic fleece in the ε-polylysine solution, heat to 35℃ and stir to adsorb, take it out, wash with deionized water, and dry to obtain a nylon-spandex elastic fleece with a bottom coating. S3: Water-soluble phthalocyanine dye, monosubstituted β-carboxylated zinc phthalocyanine, and iron phthalocyanine derivative are mixed evenly to obtain composite phthalocyanine powder; the composite phthalocyanine powder is added to deionized water, 8wt% of Pingpingjia O is added, and ultrasonic dispersion is performed to obtain a 12g / L phthalocyanine dispersion; the pH of the phthalocyanine dispersion is adjusted to 4, and then 3wt% fatty alcohol polyoxyethylene ether is added and stirred evenly to obtain phthalocyanine composite slurry; In the composite phthalocyanine powder, the mass ratio of water-soluble phthalocyanine dye: monosubstituted β-carboxylated phthalocyanine zinc: iron phthalocyanine derivative is 6:3:2; S4: Immerse the nylon-spandex elastic fleece with the bottom coating into phthalocyanine composite slurry at a liquor ratio of 1:25 and dye at 105℃. Remove the fleece, rinse with deionized water, pre-dry at 70℃ for 12 minutes, and cure at 110℃ for 2 hours to obtain the functional nylon-spandex elastic fleece. Flame melt the surface of medical polyester foam and press it onto the functional nylon-spandex elastic fleece to obtain the medical pressure band.

[0017] In the medical pressure band, the thickness of the ε-polylysine bottom coating is 20μm and the thickness of the phthalocyanine composite functional layer is 30μm.

[0018] Example 3: A method for preparing a medical pressure band based on nylon-ammonia elastic fleece, comprising the following steps: S1: Soaking the nylon-ammonia elastic fleece in a sodium hydroxide solution with a concentration of 8 wt% at 50°C for 25 min, then soaking it in a hydrochloric acid solution with a concentration of 12 wt% at room temperature for 15 min, washing it with deionized water until the washing solution is neutral, and drying it at 60°C to obtain pretreated nylon-ammonia elastic fleece; S2: Add ε-polylysine to deionized water and stir evenly to obtain a 500ppm ε-polylysine solution; immerse the pretreated nylon-spandex elastic fleece in the ε-polylysine solution, heat to 35℃ and stir to adsorb, take it out, wash with deionized water, and dry to obtain a nylon-spandex elastic fleece with a bottom coating. S3: Water-soluble phthalocyanine dye, monosubstituted β-carboxylated zinc phthalocyanine, and iron phthalocyanine derivative are mixed evenly to obtain composite phthalocyanine powder; the composite phthalocyanine powder is added to deionized water, 5wt% Pingping O is added, and ultrasonic dispersion is performed to obtain an 8g / L phthalocyanine dispersion; the pH of the phthalocyanine dispersion is adjusted to 4, and then 2wt% fatty alcohol polyoxyethylene ether is added and stirred evenly to obtain phthalocyanine composite slurry; In the composite phthalocyanine powder, the mass ratio of water-soluble phthalocyanine dye: monosubstituted β-carboxylated phthalocyanine zinc: iron phthalocyanine derivative is 4:2:1; S4: Immerse the nylon-spandex elastic fleece with the bottom coating into phthalocyanine composite slurry at a liquor ratio of 1:20 at 95°C. Remove the fleece, rinse with deionized water, pre-dry at 60°C for 12 minutes, and cure at 100°C for 2 hours to obtain the functional nylon-spandex elastic fleece. Flame melt the surface of the medical polyester foam and press it onto the functional nylon-spandex elastic fleece to obtain the medical pressure band.

[0019] In the medical pressure band, the thickness of the ε-polylysine bottom coating is 10μm and the thickness of the phthalocyanine composite functional layer is 20μm.

[0020] Comparative Example 1: A method for preparing a medical pressure band based on nylon-amylene elastic fleece, comprising the following steps: S1: Immersing the nylon-amylene elastic fleece in a sodium hydroxide solution with a concentration of 8 wt% at 50°C for 25 min, then immersing it in a hydrochloric acid solution with a concentration of 12 wt% at room temperature for 15 min, washing it with deionized water until the washing solution is neutral, and drying it at 60°C to obtain a pretreated nylon-amylene elastic fleece; S2: Add ε-polylysine to deionized water and stir evenly to obtain a 1000ppm ε-polylysine solution; immerse the pretreated nylon-spandex elastic fleece in the ε-polylysine solution, heat to 35℃ and stir to adsorb, take it out, wash with deionized water, and dry to obtain a nylon-spandex elastic fleece with a bottom coating. S3: Water-soluble phthalocyanine dye and monosubstituted β-carboxylated zinc phthalocyanine are mixed evenly to obtain composite phthalocyanine powder; the composite phthalocyanine powder is added to deionized water, 6wt% Pingping O is added, and ultrasonic dispersion is performed to obtain a 10g / L phthalocyanine dispersion; the pH of the phthalocyanine dispersion is adjusted to 4, and then 2.5wt% fatty alcohol polyoxyethylene ether is added and stirred evenly to obtain phthalocyanine composite slurry; In the composite phthalocyanine powder, the mass ratio of water-soluble phthalocyanine dye to monosubstituted β-carboxylated zinc phthalocyanine is 5:2.5. S4: Immerse the nylon-spandex elastic fleece with the bottom coating into phthalocyanine composite slurry at a liquor ratio of 1:25 and dye at 100°C. Remove the fleece, rinse with deionized water, pre-dry at 65°C for 12 minutes, and cure at 105°C for 2 hours to obtain the functional nylon-spandex elastic fleece. Flame melt the surface of the medical polyester foam and press it onto the functional nylon-spandex elastic fleece to obtain the medical pressure band.

[0021] In the medical pressure band, the thickness of the ε-polylysine bottom coating is 15μm and the thickness of the phthalocyanine composite functional layer is 25μm.

[0022] Comparative Example 2: A method for preparing a medical pressure band based on nylon-amylene elastic fleece, comprising the following steps: S1: Immersing the nylon-amylene elastic fleece in a sodium hydroxide solution with a concentration of 8 wt% at 50°C for 25 min, then immersing it in a hydrochloric acid solution with a concentration of 12 wt% at room temperature for 15 min, washing it with deionized water until the washing solution is neutral, and drying it at 60°C to obtain a pretreated nylon-amylene elastic fleece; S2: Add ε-polylysine to deionized water and stir evenly to obtain a 1000ppm ε-polylysine solution; immerse the pretreated nylon-spandex elastic fleece in the ε-polylysine solution, heat to 35℃ and stir to adsorb, take it out, wash with deionized water, and dry to obtain a nylon-spandex elastic fleece with a bottom coating. S3: Mix water-soluble phthalocyanine dye and iron phthalocyanine derivative evenly to obtain composite phthalocyanine powder; add composite phthalocyanine powder to deionized water, add 6wt% Pingpingjia O, and ultrasonically disperse to obtain 10g / L phthalocyanine dispersion; adjust the pH of phthalocyanine dispersion to 4, then add 2.5wt% fatty alcohol polyoxyethylene ether, stir evenly to obtain phthalocyanine composite slurry; In the composite phthalocyanine powder, the mass ratio of water-soluble phthalocyanine dye to iron phthalocyanine derivative is 5:1.5. S4: Immerse the nylon-spandex elastic fleece with the bottom coating into phthalocyanine composite slurry at a liquor ratio of 1:25 and dye at 100°C. Remove the fleece, rinse with deionized water, pre-dry at 65°C for 12 minutes, and cure at 105°C for 2 hours to obtain the functional nylon-spandex elastic fleece. Flame melt the surface of the medical polyester foam and press it onto the functional nylon-spandex elastic fleece to obtain the medical pressure band.

[0023] In the medical pressure band, the thickness of the ε-polylysine bottom coating is 15μm and the thickness of the phthalocyanine composite functional layer is 25μm.

[0024] Comparative Example 3: A method for preparing a medical pressure band based on nylon-amylene elastic fleece, comprising the following steps: S1: Immersing the nylon-amylene elastic fleece in a sodium hydroxide solution with a concentration of 8 wt% at 50°C for 25 min, then immersing it in a hydrochloric acid solution with a concentration of 12 wt% at room temperature for 15 min, washing it with deionized water until the washing solution is neutral, and drying it at 60°C to obtain a pretreated nylon-amylene elastic fleece; S2: Add ε-polylysine to deionized water and stir evenly to obtain a 1000ppm ε-polylysine solution; immerse the pretreated nylon-spandex elastic fleece in the ε-polylysine solution, heat to 35℃ and stir to adsorb, take it out, wash with deionized water, and dry to obtain a nylon-spandex elastic fleece with a bottom coating. S3: Add water-soluble phthalocyanine dye to deionized water, add 6wt% Pingping O, and disperse by ultrasonication to obtain a 10g / L phthalocyanine dispersion; adjust the pH of the phthalocyanine dispersion to 4, then add 2.5wt% fatty alcohol polyoxyethylene ether, stir evenly, and obtain phthalocyanine composite slurry; S4: Immerse the nylon-spandex elastic fleece with the bottom coating into phthalocyanine composite slurry at a liquor ratio of 1:25 and dye at 100°C. Remove the fleece, rinse with deionized water, pre-dry at 65°C for 12 minutes, and cure at 105°C for 2 hours to obtain the functional nylon-spandex elastic fleece. Flame melt the surface of the medical polyester foam and press it onto the functional nylon-spandex elastic fleece to obtain the medical pressure band.

[0025] In the medical pressure band, the thickness of the ε-polylysine bottom coating is 15μm and the thickness of the phthalocyanine composite functional layer is 25μm.

[0026] Comparative Example 4: A method for preparing a medical pressure band based on nylon-amylene elastic fleece, comprising the following steps: S1: Immersing the nylon-amylene elastic fleece in a sodium hydroxide solution with a concentration of 8 wt% at 50°C for 25 min, then immersing it in a hydrochloric acid solution with a concentration of 12 wt% at room temperature for 15 min, washing it with deionized water until the washing solution is neutral, and drying it at 60°C to obtain a pretreated nylon-amylene elastic fleece; S2: Water-soluble phthalocyanine dye, monosubstituted β-carboxylated zinc phthalocyanine, and iron phthalocyanine derivative are mixed evenly to obtain composite phthalocyanine powder; the composite phthalocyanine powder is added to deionized water, 6wt% of Pingping O is added, and ultrasonic dispersion is performed to obtain a 10g / L phthalocyanine dispersion; the pH of the phthalocyanine dispersion is adjusted to 4, and then 2.5wt% fatty alcohol polyoxyethylene ether is added and stirred evenly to obtain phthalocyanine composite slurry; In the composite phthalocyanine powder, the mass ratio of water-soluble phthalocyanine dye: monosubstituted β-carboxylated phthalocyanine zinc: iron phthalocyanine derivative is 5:2.5:1.5. S3: Immerse the pretreated nylon-spandex elastic fleece in phthalocyanine composite slurry at a liquor ratio of 1:25 at 100°C, remove it, rinse it with deionized water, pre-dry it at 65°C for 12 minutes, and cure it at 105°C for 2 hours to obtain the functional nylon-spandex elastic fleece; melt the surface of the medical polyester foam with a flame and press it with the functional nylon-spandex elastic fleece to obtain the medical pressure band.

[0027] In the medical pressure band, the thickness of the ε-polylysine bottom coating is 15μm and the thickness of the phthalocyanine composite functional layer is 25μm.

[0028] Comparative Example 5: A method for preparing a medical pressure band based on nylon-amylene elastic fleece, comprising the following steps: S1: Immersing the nylon-amylene elastic fleece in a sodium hydroxide solution with a concentration of 8 wt% at 50°C for 25 min, then immersing it in a hydrochloric acid solution with a concentration of 12 wt% at room temperature for 15 min, washing it with deionized water until the washing solution is neutral, and drying it at 60°C to obtain a pretreated nylon-amylene elastic fleece; S2: Add ε-polylysine to deionized water and stir evenly to obtain a 300ppm ε-polylysine solution; immerse the pretreated nylon-spandex elastic fleece in the ε-polylysine solution, heat to 35℃ and stir to adsorb, take it out, wash with deionized water, and dry to obtain a nylon-spandex elastic fleece with a bottom coating. S3: Water-soluble phthalocyanine dye, monosubstituted β-carboxylated zinc phthalocyanine, and iron phthalocyanine derivative are mixed evenly to obtain composite phthalocyanine powder; the composite phthalocyanine powder is added to deionized water, 6wt% of Pingpingjia O is added, and ultrasonic dispersion is performed to obtain a 10g / L phthalocyanine dispersion; the pH of the phthalocyanine dispersion is adjusted to 4, and then 2.5wt% fatty alcohol polyoxyethylene ether is added and stirred evenly to obtain phthalocyanine composite slurry; In the composite phthalocyanine powder, the mass ratio of water-soluble phthalocyanine dye: monosubstituted β-carboxylated phthalocyanine zinc: iron phthalocyanine derivative is 5:2.5:1.5. S4: Immerse the nylon-spandex elastic fleece with the bottom coating into phthalocyanine composite slurry at a liquor ratio of 1:25 and dye at 100°C. Remove the fleece, rinse with deionized water, pre-dry at 65°C for 12 minutes, and cure at 105°C for 2 hours to obtain the functional nylon-spandex elastic fleece. Flame melt the surface of the medical polyester foam and press it onto the functional nylon-spandex elastic fleece to obtain the medical pressure band.

[0029] In the medical pressure band, the thickness of the ε-polylysine bottom coating is 15μm and the thickness of the phthalocyanine composite functional layer is 25μm.

[0030] The medical pressure band prepared in Example 1 was used as the final sample; the functional nylon-spandex elastic fleece and the medical pressure band were sent for testing separately, and the elasticity test was carried out according to British Standard BS7505; the test data are shown in Table 1 below.

[0031] Table 1 Test Data of Medical Compression Bands Performance testing: Antibacterial performance: The SpreadPlate method was used, with an inoculum concentration of 107-108 CFU / mL and light conditions of 700nm and 150mW / cm2, to calculate the bactericidal rate.

[0032] Deodorization performance: The medical pressure belt was soaked in 0.1% 2-mercaptoethanol solution for 2 hours, the residual concentration was detected by HPLC, and the oxidation decomposition rate was calculated.

[0033] Coating adhesion and durability: 50 ultrasonic washes at 60℃ (30 min each time) were performed to test the retention rate of antibacterial / deodorizing properties after washing.

[0034] Elasticity retention rate: The elongation at break was tested using a universal testing machine, and the elasticity retention rate compared with the untreated substrate was calculated.

[0035] Biocompatibility: Skin irritation test was conducted in accordance with GB / T16886.10-2017.

[0036] The test results are shown in Table 2 below.

[0037] Table 2 Performance Test Data of Medical Pressure Bands Conclusion: The medical pressure band prepared by this invention is significantly superior to the comparative method that lacks core components or changes key parameters in terms of antibacterial properties, deodorization, coating adhesion, elasticity retention, and biosafety. It effectively solves the problems of existing medical pressure bands, such as limited antibacterial properties, poor durability, and insufficient functionality, and is suitable for clinical infection prevention, postoperative care, and other scenarios.

[0038] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the invention can be implemented in other specific forms without departing from the spirit or essential characteristics of the invention. Therefore, the embodiments should be considered in all respects as exemplary and non-limiting, and the scope of the invention is defined by the appended claims rather than the foregoing description. Thus, it is intended that all variations falling within the meaning and scope of equivalents of the claims be included within the present invention.

Claims

1. A method for preparing a medical pressure band based on nylon-spandex elastic fleece, characterized in that: Includes the following steps: S1: Pre-treat the nylon-spandex elastic fleece fabric and set aside; Add ε-polylysine to deionized water and stir until homogeneous to obtain an ε-polylysine solution; The pretreated nylon-polyurethane elastic fleece was immersed in an ε-polylysine solution, heated to 35-40℃ and stirred for adsorption, then removed, washed with deionized water, and dried to obtain a nylon-polyurethane elastic fleece with an undercoat. S2: Water-soluble phthalocyanine dye, monosubstituted β-carboxylated zinc phthalocyanine, and iron phthalocyanine derivative are mixed evenly to obtain composite phthalocyanine powder; the composite phthalocyanine powder is added to deionized water, and Pingping O is added and ultrasonically dispersed to obtain phthalocyanine dispersion; the pH of the phthalocyanine dispersion is adjusted to 4-5, and then fatty alcohol polyoxyethylene ether is added and stirred evenly to obtain phthalocyanine composite slurry; S3: Immerse the nylon-spandex elastic fleece with the bottom coating into the phthalocyanine composite slurry, dye it, take it out, rinse it with deionized water, pre-dry it, and cure it to obtain the functional nylon-spandex elastic fleece; melt the surface of the medical polyester foam with a flame and press it with the functional nylon-spandex elastic fleece to obtain the medical pressure band. The pretreatment process of the nylon-spandex elastic fleece includes the following steps: immersing the nylon-spandex elastic fleece in a sodium hydroxide solution with a concentration of 8-12 wt% at 45-55℃ for 25-35 minutes, then immersing it in a hydrochloric acid solution with a concentration of 12-18 wt% at room temperature for 15-25 minutes, washing it with deionized water until the washing solution is neutral, and drying it at 60-70℃ to obtain the pretreated nylon-spandex elastic fleece; In the preparation of the composite phthalocyanine powder, the mass ratio of water-soluble phthalocyanine dye: monosubstituted β-carboxylated phthalocyanine zinc: iron phthalocyanine derivative is (4-6):(2-3):(1-2); the amount of Pingpingjia O added is 5-8% of the mass of the composite phthalocyanine powder; the concentration of the phthalocyanine dispersion is 8-12 g / L; and the amount of fatty alcohol polyoxyethylene ether added is 2-3% of the mass of the composite phthalocyanine powder. During the dyeing process, the liquor ratio is 1:(20-30), the temperature is 95-105℃, the pre-drying temperature is 60-70℃, and the curing temperature is 100-110℃. The method for preparing the water-soluble phthalocyanine dye includes the following steps: adding quinoline-5-sulfonic acid, phthalonitrile, and metal salt to N,N-dimethylethanolamine, stirring evenly, adding 1,8-diazabicyclo[5.4.0]undec-7-ene, heating to 40-50℃ and reacting for 10-12 hours, filtering to remove insoluble impurities, distilling the filtrate under reduced pressure, adding methanol for recrystallization, and drying under vacuum to obtain the water-soluble phthalocyanine dye; In the preparation of water-soluble phthalocyanine dyes, the molar ratio of quinoline-5-sulfonic acid: phthalonitrile: metal salt is (4-6):(4-5):1; the amount of 1,8-diazabicyclo[5.4.0]undec-7-ene added is 8-12% of the mass of phthalonitrile; The metal salt includes either copper chloride or cobalt chloride; The method for preparing the monosubstituted β-carboxylated zinc phthalocyanine includes the following steps: adding phthalic anhydride, monocarboxylated phthalic anhydride, and zinc chloride to nitrobenzene, heating to 170-180℃ and reacting for 3-4 hours, cooling to room temperature, filtering and collecting the product, washing the product sequentially with nitrobenzene and methanol until the washing solution is colorless, and drying under vacuum to obtain monosubstituted β-carboxylated zinc phthalocyanine; In the preparation of monosubstituted β-carboxylated zinc phthalocyanine, the molar ratio of phthalic anhydride to monocarboxylated phthalic anhydride is (3-4):1; the amount of zinc chloride added is 15-20% of the total mass of phthalic anhydride and monocarboxylated phthalic anhydride. The preparation method of the iron phthalocyanine derivative includes the following steps: adding trimellitic anhydride, urea, and ferric chloride to nitrobenzene, adding ammonium molybdate, heating to 160-170℃ for 3-4 hours, cooling to room temperature, filtering to collect the product, washing the product with methanol, then adding the product to 50% potassium hydroxide solution, heating to 100-105℃ for 24 hours to hydrolyze, acidifying the pH to 2-3, filtering, washing, and drying to obtain the iron phthalocyanine derivative; In the preparation of the iron phthalocyanine derivative, the molar ratio of trimellitic anhydride, urea, and ferric chloride is 1:(4-6):(0.25-0.3); the amount of ammonium molybdate added is 3-5% of the mass of trimellitic anhydride.

2. The method for preparing a medical pressure band based on nylon-spandex elastic fleece according to claim 1, characterized in that: In the preparation of nylon-spandex elastic fleece with a base coating, the concentration of ε-polylysine solution is 500-1500 ppm; the bath ratio of pretreated nylon-spandex elastic fleece to ε-polylysine solution is 1:(15-25).

3. The medical pressure band prepared by the method of preparing a medical pressure band based on nylon-ammonia elastic fleece according to any one of claims 1-2.

Citation Information

Patent Citations

  • Aqueous liquid composition, aqueous coating, functional coating film, and composite material

    CN103403109A

  • Preparation method and application of photodynamic antiviral clothing finishing liquid

    CN111877007A