A Visual Servo-Based Method and System for Positioning Injection Molding Control of Puncture-Proof Safety Shoes

By acquiring information on the fixation and thermal contact status of the puncture-resistant insert using visual servo technology, and dynamically adjusting the injection speed and exhaust valve control, the problem of insert misalignment during the injection molding process of puncture-resistant safety shoes is solved, thereby improving the injection molding quality and the stability of the puncture-resistant insert.

CN122851918BActive Publication Date: 2026-11-10DELTA PLUS CHINA CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202611327911.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2026-08-31
Publication Date
2026-11-10
Estimated Expiration
2046-08-31

AI Technical Summary

Technical Problem

Existing technologies cannot effectively identify and predict changes in the thermal contact and fixation states of puncture-resistant inserts in different areas during the injection molding process of puncture-resistant safety shoes. This causes the inserts to shift during the injection molding process, affecting the effectiveness of the protected coverage area.

Method used

A vision-servo-based control method is adopted to dynamically adjust the injection speed and the opening and closing of the vent valve by acquiring information on the fixed state and thermal contact state of each area of ​​the puncture-resistant sheet, identify the unstable areas of injection molding and actively intervene to ensure the stability of the puncture-resistant sheet during the injection molding process.

Benefits of technology

It enables dynamic control of the puncture-resistant sheet during injection molding, avoiding the limitations of relying solely on physical fixation or post-injection warning, and improving the positional accuracy of the puncture-resistant sheet and the injection molding quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122851918B_ABST
    Figure CN122851918B_ABST
Patent Text Reader

Abstract

This invention relates to the field of intelligent control technology, specifically a vision-servo-based method and system for positioning and injection molding control of puncture-resistant safety shoes. The method includes: acquiring the distribution of fixed points in the puncture-resistant patch area, sole structural parameters, and temperature data after mold closure; calculating the region's fixed constraint transmission state, initial anti-offset force, effective heat exposure, and remaining anti-offset force; then calculating the melt offset force based on the melt arrival time, pressure difference across the region, region area, and melt flow direction to obtain the region's anti-offset margin and determine the risk of injection molding instability. For injection molding instability areas, the method determines the target low-speed injection speed, speed switching position, and vent valve opening and closing time, achieving segmented injection and venting coordinated control. This invention can reduce the risk of edge displacement and edge lifting of the puncture-resistant patch during the encapsulation process, improving the encapsulation positioning accuracy and molding stability of the safety shoe.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of intelligent control technology, and is a method and system for controlling the alignment of puncture-resistant safety shoes during injection molding based on visual servoing. Background Technology

[0002] Puncture-resistant safety shoes typically use insert injection molding to achieve integrated molding with the sole substrate. Since the puncture-resistant insert is a large-sized, thin-walled, curved insert, its positional displacement during the injection molding process directly affects the effective protective coverage area of ​​the safety shoe. Therefore, preventing insert displacement is a crucial technical issue in this field.

[0003] Existing technologies mainly develop along two routes: one is visual pre-positioning combined with physical fixing structures (such as suction cups, magnets, locking pins, etc.) to fix inserts in the mold; the other is to monitor the melt pressure field and flow field through sensors during injection molding to provide early warning of insert displacement risks. However, the above technical solutions share a common premise: that the constraint capability of the insert remains constant throughout the injection molding process after it is placed in the mold and constrained by the fixing mechanism. But in actual injection molding, the thermal contact state between the anti-puncture sheet and different areas of the mold is not uniform. The fixing coverage, contact area, and heating rate of different areas vary significantly. The sheet softens and its interfacial friction characteristics change due to heat conduction before the melt arrives, causing the actual constraint effect of the same fixing structure on each area to continuously decrease. Existing technologies rely on passive responses such as physical locking or warning after force is applied, which cannot actively identify unstable areas and predict their attenuation trend before the melt fills the mold, making dynamic control difficult. Summary of the Invention

[0004] To overcome the problems existing in the prior art, a vision servo-based method and system for puncture-resistant safety shoe alignment injection molding control is proposed.

[0005] To achieve the above objectives, the present invention provides a vision-servo-based method for puncture-resistant safety shoe alignment injection molding control, comprising: Obtain information on the fixation status and thermal contact status of each area of ​​the puncture-resistant patch; Based on the fixed state information and the thermal contact state information, the anti-displacement level of each region during mold closing and the initial stage of injection molding and its decay trend with heating time are determined, and key protection areas are determined based on the anti-displacement level and the decay trend. The melt arrival state and pressure application state of each region during the melt filling process are obtained. Based on the melt arrival state and pressure application state and the anti-displacement level of each region, the injection molding instability region is determined. Based on the injection molding instability region, control the switching of injection speed and the opening and closing of the vent valve; Based on the actual offset state of the puncture-resistant sheet after molding, the switching of the injection speed and the opening and closing of the vent valve in subsequent injection cycles are corrected.

[0006] Preferably, obtaining the fixation status information and thermal contact status information of each area of ​​the puncture-resistant patch includes: The fixed area, fixed point distribution, and edge contour position of the puncture-resistant patch are collected. The fixed coverage rate of each area is determined based on the fixed area and fixed point distribution. The edge position deviation of each area is determined based on the comparison result between the edge contour position and the preset reference contour. After mold closing, the surface temperature of each area of ​​the puncture-resistant sheet and the temperature of the corresponding mold area are collected. Based on the continuously collected temperature data, the temperature difference between the mold and the heating rate of the sheet are determined.

[0007] Preferably, the anti-displacement level of each region during mold closing and the initial stage of injection molding and its decay trend with heating time are determined based on the fixed state information and the thermal contact state information, and the key protection areas are determined based on the anti-displacement level and the decay trend, including: Based on the fixed coverage, fixed point distribution, edge position deviation, mold temperature difference and sheet heating rate, the pre-established anti-offset calibration relationship is invoked to determine the anti-offset level and allowable offset threshold of each region in the mold closing and early injection molding stages. The anti-displacement rating of each region is updated according to the heating rate during the injection molding process, and the decay of the anti-displacement capability of each region with heating time is obtained. Areas with an anti-offset level lower than a preset level are identified as key protection areas.

[0008] Preferably, the melt arrival state and pressure application state of each region during the melt filling process are obtained, and the injection molding instability region is determined by matching the melt arrival state and pressure application state with the anti-displacement level of each region. Based on the injection port location, local cavity thickness, and preset injection process, determine the flow path of the melt extending to each edge of the puncture-resistant sheet; Collect the injection pressure curve and screw position curve of the injection molding machine, and combine them with the temperature detection points or pressure detection points set at the corresponding positions of the mold to determine the arrival time of the melt to each edge of the anti-puncture sheet; The arrival time difference of the melt is determined based on the arrival time of different edges, and the pressure change state of the melt before and after reaching the key protection area is determined based on the injection pressure curve; The melt arrival time difference and the pressure change state are matched with the anti-displacement level of each region, and the region that meets the risk judgment condition is identified as the injection molding instability region.

[0009] Preferably, controlling the switching of injection speed according to the injection molding instability region includes: Based on the arrival time of the melt in the injection instability zone and the corresponding screw position, the switching position of the injection speed is determined so that the melt fills the key protection zone at a target speed that matches the anti-deflection level of the key protection zone.

[0010] Preferably, controlling the opening and closing of the vent valve according to the injection molding instability region includes: Based on the arrival time of the melt at each edge of the anti-puncture sheet, the opening time of the vent valve connected to the injection molding instability area is determined, so that the vent channel is in the venting state before the melt covers the anti-puncture sheet, and the corresponding vent valve is closed after the melt reaches the vent channel inlet.

[0011] Preferably, correcting the switching of the injection speed and the opening and closing of the vent valve in subsequent injection cycles based on the actual offset state of the puncture-resistant sheet after molding includes: After injection molding is completed, the actual edge contour of the puncture-proof piece in the molded product is obtained by visual inspection. The actual edge contour is compared with the preset target contour to determine the actual offset of each area of ​​the puncture-proof piece. When the actual offset meets the correction conditions, the switching position of the injection speed is adjusted according to the offset area, and the opening time of the exhaust valve is adjusted according to the edge lifting state.

[0012] Preferably, defining the area that meets the risk assessment criteria as the injection molding instability area includes: when the melt arrival time difference and pressure change state of a certain area meet the risk assessment criteria corresponding to the anti-displacement level of that area, the area is defined as the injection molding instability area, and the displacement direction or edge lifting direction of the anti-puncture sheet is determined according to the melt flow direction and edge position relationship.

[0013] Preferably, determining the key protection area as the area with a displacement resistance level lower than the preset level includes: determining the area with a displacement resistance level lower than the preset level and whose displacement resistance decay rate with heating time meets the preset condition as the priority protection area.

[0014] In addition, the present invention provides a vision-servo-based puncture-resistant safety shoe alignment injection molding control system, comprising: The data acquisition module is used to acquire the fixation status information and thermal contact status information of each area of ​​the puncture-resistant patch; The constraint calculation module is used to calculate the transmission state of the fixed constraint to each region of the puncture-resistant sheet based on the fixed state information. The heat calculation module is used to calculate the remaining anti-displacement state of each area of ​​the puncture-resistant sheet after being heated, based on the heat contact state information. The flow determination module is used to determine the arrival status of the melt in each region during the melt filling process; The risk assessment module is used to determine the injection molding instability region based on the transmission state of the fixed constraint, the remaining anti-offset state, and the melt arrival state. The collaborative control module is used to control the switching of injection speed and the opening and closing of the vent valve according to the injection molding instability region.

[0015] Compared with the prior art, the technical effects of the present invention are as follows: 1. Existing technologies assume that the constraint state of the insert remains constant throughout the injection molding process after it is placed in the mold, focusing only on the positioning accuracy before mold entry or the force monitoring after mold entry. This invention collects the fixed coverage and thermal contact state of each zone of the puncture-resistant insert through S1, and combines it with the anti-displacement assessment through S2. This allows for the identification of key protection areas with the lowest and fastest attenuation of anti-displacement capability before melt injection, enabling subsequent control to shift from passive response to active intervention.

[0016] 2. This invention identifies injection molding instability areas and their offset directions, and uses S4 to coordinate the injection speed switching position and the vent valve opening sequence, ensuring that the pressure build-up process when the melt reaches the key protection area is adapted to the current anti-offset capability of that area. This invention's active matching mechanism effectively avoids the limitations of relying solely on physical fixation or post-event warnings. Attached Figure Description

[0017] To more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings used in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort. Wherein: Figure 1 This is a flowchart illustrating the puncture-resistant safety shoe alignment injection control method based on visual servoing of the present invention. Figure 2 This is a schematic diagram of the structure of the vision servo-based puncture-resistant safety shoe alignment injection molding control system of the present invention. Detailed Implementation

[0018] To make the above-mentioned objects, features and advantages of the present invention more apparent and understandable, the specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings.

[0019] Many specific details are set forth in the following description in order to provide a full understanding of the invention. However, the invention may also be practiced in other ways different from those described herein, and those skilled in the art can make similar extensions without departing from the spirit of the invention. Therefore, the invention is not limited to the specific embodiments disclosed below.

[0020] Example 1: This invention relates to a vision-servo-based method for puncture-resistant safety shoe positioning and injection molding control, applied during the injection molding process of shoe soles. The puncture-resistant sheet is pre-positioned within the mold cavity and fixed in place by fixed points located in the shoe sole structure area. This invention determines the injection speed switching position and the opening and closing time of the vent valve by analyzing the transmission state of the fixed point constraints in each area of ​​the puncture-resistant sheet, the thermal contact state of the areas after mold closing, and the regional action state during melt filling.

[0021] The puncture-resistant patch is divided into multiple zones according to its outline. ,in, The regions are numbered. Each region contains at least one edge segment and its adjacent regions extending inward, allowing edge offset, edge lift, and local translation to be analyzed within the respective regions.

[0022] like Figure 1 As shown, the specific steps include the following: S1: Obtain the distribution of fixing points, edge positioning status and structural features of the sole area where the fixing points are located after the anti-puncture patch is fixed in the pre-fixation stage, and collect the thermal contact status of each area of ​​the anti-puncture patch after the mold is closed. S2: Based on the structural characteristics of the sole area where the fixing point is located, determine the degree of transfer of the fixing constraint to each area of ​​the puncture-resistant piece, and combine the cumulative heating process of each area during mold closing and the initial stage of injection molding to determine the remaining anti-displacement ability and allowable displacement threshold of each area as time decays. S3: Based on the flow path of the melt extending to each area of ​​the anti-puncture sheet, the arrival time, and the change in injection pressure, the filling effect generated when the melt reaches each area is matched with the remaining anti-displacement capability at the corresponding time to determine the injection molding instability area, instability risk level, weak anti-displacement time window, and possible displacement direction. S4: Based on the injection molding instability area, instability risk level, and weak anti-displacement time window, determine the switching position of the segmented injection speed and the opening and closing time of the mold exhaust valve, and coordinate and control the pressure building process and gas discharge process when the melt approaches and covers the anti-puncture sheet.

[0023] The following provides further examples of the alignment injection molding control method for puncture-resistant safety shoes proposed in this invention: S11: Establish the coordinate relationship between the puncture-resistant patch area and the fixed point coordinates; Specifically, after the anti-puncture piece is fixed in the preliminary stage, the reference surface of the mold cavity and the reference positioning part are used as the mold coordinate system to obtain the target outline, actual outline, position coordinates of each fixed point, and the fixing method corresponding to each fixed point.

[0024] The target contour of the puncture-resistant patch is divided into multiple edge segments at preset arc length intervals. Based on each edge segment, a preset analysis width is extended into the interior of the puncture-resistant patch to form multiple regions. .

[0025] Adjacent areas should preferably share a boundary at the edge transition to maintain the continuity of the outline area division.

[0026] For each region Record the following positional relationships: area of ​​the puncture-resistant patch region. The geometric center of the puncture-resistant patch area and the outward normal unit vector of the edge segment of the area. The normal unit vector of the puncture-resistant sheet surface Fixed point numbers within and adjacent areas of the region, number Calculated location from a fixed point within the region distance , No. Minimum distance from each fixed point to the edge of the puncture-resistant patch Minimum design distance from the edge of the puncture-resistant plate to the finished edge of the sole. .

[0027] The actual contour of the puncture-resistant piece is compared with the target contour to obtain the initial positional deviation before mold closure. It should be noted that the initial position deviation Used to correct for the allowable offset that can continue to occur in this area during injection molding; the outward normal unit vector Used for S33 to calculate the component of melt pressure in the outward displacement direction at the edge; the surface normal unit vector The area used to identify the edge lifting direction of the puncture-resistant patch Used for calculating melt displacement force in S33.

[0028] S12: Obtain the structural features of the sole structure area where the fixed point is located; It should be noted that S12 is used to obtain the sole structure conditions on which the fixed-point constraint is transferred to the puncture-resistant patch area.

[0029] Regarding the first At a fixed point, the thickness of the sole substrate at the location of the fixed point is obtained. and the local curvature of the puncture-resistant patch .

[0030] It should be noted that the thickness of the sole base material... Used to characterize the support capacity of the material surrounding the anchor point for the puncture-resistant patch; local curvature Used to characterize the directional change of fixed constraints as they are transmitted along the contour of the puncture-resistant patch; support distance It is used to characterize the spatial conditions under which a puncture-resistant sheet undergoes local deformation after being subjected to the action of a melt.

[0031] For each region Based on the structural characteristics of the area or adjacent fixed points, regional structural support data is obtained, including the average thickness of the substrate in the area. Average support distance in the region and regional average local curvature .

[0032] At the same time, the distribution status of fixed points within the area is determined, including single-point constraint status, adjacent two-point continuous constraint status, and multi-point enclosure constraint status.

[0033] In this embodiment, the curvature is expressed as an absolute value, in meters. The thickness of the sole substrate at the fixed point is also considered. and local curvature Used for calculating the fixed constraint transfer coefficient in S21; average substrate thickness in the region. Average support distance in the region and regional average local curvature Used for calculating the structural support coefficient in S22.

[0034] S13: Obtain regional thermal contact data after mold closure, and form a regional temperature change curve from the moment mold closure is completed to the moment pressure holding begins; It should be noted that the regional thermal contact data is used to characterize the thermal contact process of each region of the puncture-resistant sheet before the arrival of the melt.

[0035] When the mold completes closing, the moment of mold closure is recorded as... Temperature sensors located near the mold cavity wall or puncture-resistant sheet are used to collect the temperature at each detection location after the mold is closed.

[0036] For the puncture-resistant patch area equipped with temperature sensors, the temperature readings from each sensor within that area are weighted and averaged according to their respective coverage areas to obtain the area temperature. .

[0037] For the puncture-resistant patch area without a temperature sensor, the area temperature is obtained by inverse distance-weighted interpolation based on the distance from the geometric center of the area to the adjacent temperature sensor. When interpolating, at least three adjacent temperature sensors should be selected, and the interpolation result should be limited to the maximum and minimum values ​​detected by the selected temperature sensors.

[0038] Update the region temperature according to the preset sampling period. This forms a temperature change curve for the region from the moment the mold is closed to the moment the pressure holding begins.

[0039] S2: Calculate the remaining anti-displacement capability of each region of the puncture-resistant sheet based on the fixed constraint transfer and regional thermal contact process; Specifically, based on the distribution of fixed points, the structural characteristics of the sole, and the regional temperature data after mold closing, the initial anti-displacement force of each puncture-resistant plate area at the initial moment of mold closing and the remaining anti-displacement force after heating are calculated, and the allowable displacement is output. (Steps S21-S22), Remaining Anti-Offset Force (Steps S23-S25) and the time window for resisting displacement weakness (Step S26).

[0040] S21: Determine the constraint transfer coefficient of the fixed point to each area of ​​the puncture-resistant patch; It should be noted that S21 is used to characterize the degree of effective constraint of each fixed point on different areas of the puncture-resistant patch.

[0041] For the puncture-resistant patch area Any calculation position within Get the location and the first Distance between fixed points And obtain the distance from the fixing point to the edge of the puncture-resistant patch. Thickness of the sole substrate at the location of the fixing point and local curvature .

[0042] Determine the constraint transfer length at the fixing point based on the distance from the fixing point to the edge of the puncture-resistant patch: ; in, The maximum effective constraint transfer length at the fixed point. For example, the edge distance conversion factor is used. and Determined through a fixed-point pull-out test.

[0043] Furthermore, the fixed-point pull-out test used the same puncture-resistant sheet material and fixed-point structure as the actual product. The specimen size was a rectangular test plate scaled down proportionally to the actual puncture-resistant sheet (250mm in length, 150mm in width, and the same thickness as the actual sheet), with the fixed point located at the geometric center of the test plate. During the test, the test plate was placed flat on a support platform, which was set to correspond to the actual state of the mold support surface, constraining only the displacement in the thickness direction of the test plate, not the in-plane displacement. The test loading speed was 5mm / min, and the load was applied using a universal testing machine.

[0044] At a fixed point distance of In the sample, starting from directly above the fixed point, along the length of the sample plate... Loading points were set at various points, each at a distance of mm. A tensile load was applied perpendicular to the surface of the test plate at each loading point, and the displacement of the loading point was recorded until the specified offset was achieved. The corresponding load value at time Among them, the specified offset amount The allowable offset of the puncture-resistant sheet is taken as 75%-80% to simulate the critical state before instability is triggered during injection molding. In this embodiment, it is taken as... mm. The test was repeated 5 times at each measuring point, and the average value was taken as the load value at that point. The spacing between the measuring points ensured that the indenter at the loading point would not interfere with the fixed structure.

[0045] by The load value measured at a point mm (close to the fixed point) is used as the reference load for that fixed point. Plot the load values. With distance The decay curve is obtained using an exponential decay model. Fit the measured data, using only the measured data during fitting. Measurement data within the specified range are used to eliminate the interference of edge effects on constraint transmission. When the measured data does not contain a load exactly equal to... When measuring points, calculations are performed using curve fitting interpolation. Time corresponding The value is determined as the effective constraint transfer length of the fixed point. .

[0046] For different fixed point distances The samples (prepared in this embodiment) are respectively Samples with four fixed point distances (mm) covering the common fixed point layout range of puncture-resistant sheets were obtained according to the above method. Value. Establish and The correspondence was fitted using linear regression. (Forced to pass through the origin), the slope obtained from the fitting is the proportionality coefficient. The correlation coefficient of the fitting results The value should not be lower than 0.90; otherwise, the number of samples should be increased or the sample size range adjusted, and the test repeated. Preferably, The empirical value is 0.60-0.85, and in this embodiment, it is preferred. .

[0047] Effective constraint transfer length in each region In the subsequent S21 In the calculation, the actual distance measured by S1 is further compared. Combined, it is used to determine the actual constraint coverage of each fixed point on each area of ​​the puncture-resistant patch. Take all of the above Measured under the conditions The maximum value is used to truncate excessively long or short constraint transfer lengths in the S21 formula, avoiding the adverse effects of extreme values ​​on the calculation results.

[0048] The location of the fixed point is determined based on the distance between the fixed point and the calculated position, the thickness of the sole substrate, and the local curvature. The local constraint transfer coefficients for the th Calculate the position of each fixed point. The local fixed constraint transfer coefficient is: ; in, The coefficient representing the influence of substrate thickness was determined through a fixed-point pull-out test, with a typical value range of 0.2-0.6. The curvature influence coefficient is determined by fitting a fixed-point pull-out test, with a typical value range of 0.2-0.8m.

[0049] In another preferred embodiment, and The calibration method is as follows: prepare substrates with different thicknesses ( mm) and different curvatures ( The samples were subjected to pull-out tests, and the results were recorded for each sample at the same distance. Effective constraint transfer length Substituting the measured data into the above formula, the least squares method is used to fit the result. and The optimal value. The fitting requirement is set to... Otherwise, increase the number of samples or adjust the sample parameter range and repeat the test.

[0050] and These are the lower and upper limits of the base material thickness within the current shoe sole structure range. At that time, the thickness correction item is taken When the puncture-resistant patch has a planar structure, .

[0051] For multiple fixed points within the same area, the area constraint transfer coefficient is determined according to the coverage state of the fixed constraints: ; In the formula: ; It should be noted that, by... Limited to to Between these points, the composite result from multiple fixed points can still represent the coverage ratio of the fixed constraints in the region.

[0052] For example, in actual calculations, the region Discretize into several grid cells, and calculate at the center of each cell. Then, a weighted average is calculated, with the grid size not exceeding 1mm × 1mm.

[0053] S22: Determine the initial anti-displacement capability and allowable displacement threshold of the area based on the sole structure; It should be noted that this step is used to convert the fixed constraint state and the regional structural support state into the initial resistance to offset of the region.

[0054] The average substrate thickness in the region obtained from S1 Regional support distance and local curvature Determine the regional structural support coefficient: ; in, Based on the thickness of the base material of the shoe sole, As the baseline support distance, The curvature influence coefficient is expressed in meters (m) and is determined through static loading tests. Its typical value range is 0.2-0.8 m.

[0055] For example, , , This was determined through static loading tests on similar shoe sole structures. In another embodiment, the detailed method of the static loading test is as follows: A monotonically increasing load was applied along the outward normal direction at the edge of each section of the specimen, with a loading rate of 0.5 mm / min. The offset of each section when it reached the specified value was recorded. Load value at time Set the offset Consistent with S21, the allowable offset is taken as 75%-80%, and in this embodiment, it is taken as 1.5mm. In this embodiment, the statistical median value of the thickness of each zone of the puncture-resistant sheet is taken. mm. Preparation of different support distances ( A sample (mm) was prepared, maintaining a thickness of... and curvature Unchanged, according to Calculate the structural support coefficient of each specimen (wherein) Reference sample , (the corresponding load value at that time), through fitting get .

[0056] Preparation of different curvatures ( () of the sample, maintaining thickness and support distance Without changing the thickness and support distance terms, and incorporating them into the known quantities, the results are obtained through fitting. get ,in Each fitting step requires a correlation coefficient. Otherwise, increase the number of samples and repeat the test. After substituting the fitted parameters back into the formula, each sample... The relative error between the predicted value and the measured value should be within ±10%.

[0057] When the puncture-resistant patch has a planar structure The curvature correction term is 1; when When the support distance correction term is 1, the value of the term is 1.

[0058] Based on the regional fixed constraint transfer coefficient and structural support coefficient, determine the regional anti-displacement capability at the initial moment of formwork closure: ; in, The reference offset resistance is measured under both the reference fixed state and the reference structural support state, and the unit is Newton; Based on the minimum design distance from the edge of the puncture-resistant plate to the target boundary of the sole. Specified minimum coverage width and initial position deviation before mold closure Determine the allowable offset for the region: ; In the formula, , , and The units are all meters, where the specified minimum coverage width is... The minimum coverage width of the puncture-resistant patch is determined according to the product design requirements. For example, in this embodiment, it is determined according to the minimum coverage width requirement of the effective protection area of ​​the safety shoe standard (such as ISO 20344), which is usually 5mm-10mm.

[0059] area Simultaneously, a directional constraint state is formed. Specifically, based on the distribution of fixed points in the region relative to the region's center and edge segments, the constraint strength of the region in the edge normal direction, edge tangential direction, and direction perpendicular to the plane of the anti-puncture sheet is determined. This directional constraint state is used in S34 to determine the main offset direction under the action of the melt.

[0060] S23: Determine the initial state of regional thermal decay and thermal response parameters; It should be noted that S23 is used to determine the moment when thermal decay begins in each region and its thermal response rate; Specifically, the thermal attenuation initiation temperature of the puncture-resistant sheet material under fixed conditions is obtained. .

[0061] Thermal decay onset temperature The temperature is determined by a constant-temperature tensile test, specifically the lowest test temperature at which the specimen's resistance to displacement begins to continuously decrease relative to its resistance at room temperature. For example, in a constant-temperature tensile test, the temperature at which the specimen's resistance to displacement decreases by more than 5% compared to 23°C after being held at a constant temperature for 30 seconds, and the subsequent continuous decrease does not recover, is used as the temperature at which the resistance to displacement decreases. .

[0062] Based on the regional contact temperature variation curve obtained from S1 Determine the regional thermal activation temperature: ; when When the condition is met for the first time, the region is identified as entering the state of thermal decay.

[0063] Regional thermal response time constant The temperature was determined through a heating test with the same substrate thickness, contact structure, and mold temperature conditions as the actual shoe sole area, measured in seconds. In the heating test, firstly, when the sample temperature change did not exceed ±0.5℃ within 60 seconds, it was considered to have reached the final stable temperature rise. Then, starting from the start of the heating, the time elapsed until the sample temperature first reached 63.2% of the final stable temperature rise was recorded; this time was used as the thermal response time constant for that area. .

[0064] S24: Calculate the effective cumulative heat received by the region; specifically, for the region At any moment Effective cumulative heat received: ; in: For the region Deadline The effective cumulative heat received; For a moment The thermal activation temperature; is the regional thermal response time constant.

[0065] Through this calculation, the region forms an increasing effective cumulative heat under continuous thermal contact conditions; as the regional contact temperature gradually decreases, the earlier thermal effects continue to decay according to the regional thermal response time constant.

[0066] For each region, update at a preset sampling period. In another embodiment, during discrete computation, a trapezoidal integral is used, and the overheating amount at each sampling point is recorded. The effective heat exposure at the current moment is updated to... ,in The sampling period.

[0067] S25: Calculate the remaining mitigation capability of each region, specifically, based on the initial mitigation capability obtained in S22. The effective cumulative heat received by S24 Determine the amount of attenuation in the region's resistance to migration: ; in, For the region The reference cumulative heat received when the preset anti-offset capability attenuation level is reached.

[0068] Then the region at time The remaining offset resistance is: ; in, This refers to the region's ability to maintain its basic stability under current sole support conditions.

[0069] and The minimum residual resistance to displacement is determined based on the puncture-resistant plate material, the regional fixed constraint transfer coefficient, the structural support coefficient, and the directional constraint state. More specifically, it is determined based on the minimum residual resistance to displacement. The preferred method is to determine the load through a high-temperature isothermal loading test, specifically the load measured when the sample reaches a specified offset at the specified maximum molding temperature and the longest heating time.

[0070] Based on the above, S25 forms the area. Remaining anti-displacement capability curve from the moment of mold closure to the moment of pressure holding. .

[0071] S26: Determine the time window for regional vulnerability to migration, specifically based on the region's allowable migration threshold. Read the load value corresponding to the allowable offset from the area static load-displacement calibration curve, and determine this load value as the minimum offset resistance requirement for the area. .

[0072] The regional static load-displacement calibration curve adopts the same as that of the region. The calibration curve was measured using specimens with the same distribution of fixed points (consistent number and relative positions of fixed points), substrate thickness, support distance, and local curvature. The specific method for obtaining the calibration curve is as follows: The specimen is heated to the melt arrival temperature of the region (obtained from S32) according to the actual heating rate of that region during the injection molding process (calculated from the temperature data in S13; in this embodiment, approximately 8℃ / s for the arch area and approximately 7℃ / s for the heel area). Then, a monotonically increasing load is applied at a rate of 0.5 mm / min, and the load-displacement curve is recorded until the displacement exceeds the allowable offset. The value is up to twice the value of the load; where the horizontal axis of the curve represents displacement in meters, and the vertical axis represents load in Newtons.

[0073] When the remaining resistance to displacement in the region satisfies the following formula, the moment when the remaining resistance to displacement satisfies the following condition is defined as the weak state of resistance to displacement: ; The time window for obtaining the region's weak resistance to migration is: ; S3: Determine the risk of injection molding instability based on the melt filling process and the remaining anti-displacement capability of the area; S31: Determine the main flow path of the melt to each puncture-resistant sheet area; In this step, the simulation analysis of the melt flow path and the correction of the first trial production are both achieved using injection flow simulation technology known in the field. Specifically, the injection port position, flow channel structure, cavity geometry model, local thickness distribution of the cavity, and preset injection speed curve are obtained.

[0074] According to the injection port to each area The candidate paths for the melt to advance into each region are determined by the changes in cavity channel length, local cavity thickness, and flow channel cross-section.

[0075] For each region, the candidate path with the earliest expected arrival time is selected as the main flow path; Record the length of the main flow path and the flow direction when the melt approaches the region. Locations where adjacent melt fronts may converge and exhaust channels connected to this area.

[0076] The main flow path is first obtained through injection molding flow simulation and then corrected by the actual arrival sequence detected by cavity pressure or temperature sensors during the first trial production. The correction factor is the weighted average of the ratios of the actual arrival time and the simulated arrival time. When the deviation between the actual arrival time and the simulated arrival time exceeds 20%, the simulation model is recalibrated.

[0077] For example, in this embodiment, the arch region is used. For example, the injection molding flow simulation used the viscosity curve of this batch of PU material at 210℃, with the injection speed set to 25 cm³ / s. The simulation results showed that there were two candidate paths in the arch region: path A had a cavity channel length of 82 mm and an estimated arrival time of 4.8 s; path B had a channel length of 76 mm, but due to a section of cross-sectional contraction, its estimated arrival time was 5.3 s. The time difference between the two was 0.5 s, which just met the judgment boundary for simultaneous arrival. Therefore, the flow directions of both paths were recorded simultaneously.

[0078] S32: Determine the actual arrival time of the melt in each region and the corresponding screw position; During the injection molding process, injection pressure, screw position, cavity pressure, and cavity temperature are collected simultaneously.

[0079] For areas equipped with pressure or temperature sensors, the moment when the increment of the detection signal relative to the pre-filling reference value reaches a preset threshold and remains there for at least a preset confirmation time is defined as the moment the melt arrives. For areas without sensors, the inter-regional transmission time obtained from the simulation is adjusted according to the ratio of the actual arrival time of the upstream area to the upstream arrival time of the current injection, thereby determining the arrival time of that area.

[0080] At the moment the melt arrives The corresponding screw position is read from the synchronously acquired screw position curve. .

[0081] S33: Determine the effective offset driving force when the melt reaches the region; When the melt reaches the puncture-resistant plate area Then, obtain the upstream cavity pressure in the region. Downstream cavity pressure The unit vector of the main melt flow direction recorded by S31 .

[0082] The pressure difference across the region is: ; The directional component of the melt flow direction normal to the region edge is: ; In the formula, and All are unit vectors.

[0083] The force of regional melt displacement is: ; The unit is Newton.

[0084] The upstream and downstream cavity pressures of the region are preferentially measured using cavity pressure sensors located upstream and downstream of the region, respectively. When no corresponding sensors are installed, the flow simulation results corrected by the pressure data from the first round of trial production are used.

[0085] For areas where the melt impacts the surface of the puncture-resistant sheet in the normal direction and may cause edge lifting, the formula above will be used... Replace with The displacement force of the melt in the lifting direction is calculated by using the pressure difference formed by the melt on both sides of the puncture-resistant sheet.

[0086] S34: Determine the regional instability margin, offset direction, and instability risk level; For the region The remaining anti-offset capability in S2 is invoked at the moment the melt arrives: ; Determine the regional instability margin: ,in, This indicates the margin of resistance to displacement in the region at the moment the melt arrives.

[0087] The regional risk status is determined based on the instability margin and the allowable offset threshold: when Greater than the preset safety margin When the predicted offset is less than the allowed offset threshold, it is determined to be a stable region; when ,or When, it is identified as an area of ​​interest; it should be noted that when Furthermore, when this area is identified as an area of ​​interest, it is elevated to an injection molding instability area to reflect the direct correspondence between the arrival time of the melt and the thermal decay state of the area.

[0088] when If the value is less than 0, or if the predicted offset reaches the allowable offset threshold, it is identified as an injection molding instability region.

[0089] Preset safety margin The minimum anti-displacement margin for each region in the qualified test specimens is determined, with the unit being Newtons. In another embodiment, for example, multiple qualified test specimens can be taken, and the anti-displacement margin for each region at the moment of melt arrival can be calculated. 80% of the minimum margin among all qualified specimens is taken as the safety margin. .

[0090] In addition, the main offset direction depends on the melt flow direction. Outer normal of the region edge The angle relationship is determined as follows: when and When the directions are consistent, the offset direction is an outward shift along the edge normal to the region edge; when When the offset direction is consistent with the tangential direction of the region edge, the offset direction is a tangential slip along the edge direction; when Along the normal direction of the puncture-resistant patch surface When the direction has a component, the offset direction is edge lifting.

[0091] S4: Coordinate and control the injection speed and vent valve timing based on the risk of injection molding instability; S41: Identify key protection areas and injection control zones; The injection molding instability areas identified in S3 are designated as key protection areas. In particular, when multiple injection molding instability areas exist, protection is implemented based on the arrival time of the melt. Arranged from earliest to latest; when the arrival times of the melts are the same, according to the anti-displacement margin. Arranged from smallest to largest.

[0092] For each key protected area, the arrival time of the melt is recorded. Corresponding screw position Weak time window against migration and the rate of pressure rise.

[0093] Based on the response time required for the injection system to switch from the current speed to the target low speed. The starting point of the injection control range is determined by the displacement of the screw within the response time.

[0094] The screw position corresponding to the start of the injection control zone is: ,in The screw speed before speed switching (absolute value); The safety margin displacement (which can be 0.5mm-1mm) is intended to ensure that the actual speed switching is completed before the melt arrives.

[0095] The endpoint of the injection control zone is the screw position corresponding to when the melt completes the coverage of the key protection area. It is determined by the sensor detection signal at the downstream edge of the zone or by the moment when the zone is completely filled in the injection flow simulation.

[0096] For example, the response time of the injection system The time taken from the time the controller issues a speed switching command to the actual injection speed entering the target speed allowable deviation range is measured by switching the speed under no-load or standard load conditions on the injection molding machine.

[0097] S42: Determine the target low-speed injection rate for key protected areas; During the initial trial production or process calibration phase, injection was performed at multiple injection speed levels. The pressure rise rate and melt displacement force corresponding to each key protected area were recorded to establish the injection speed... Rate of pressure rise Force of melt displacement The calibration data table.

[0098] During calibration, a fixed injection rate is maintained. Record the cavity pressure difference in the key protected area at this speed when the melt arrives. Calculated according to S33 ,Establish and The correspondence is as follows, and in particular, linear interpolation is used between adjacent calibration speeds.

[0099] For key protection areas The following conditions will be met ( The highest calibrated injection speed is determined as the target low-speed injection speed. ; When there is no calibrated injection speed that meets the above conditions, select the lowest injection speed at which the injection molding equipment can maintain continuous and stable filling, and list the corresponding area as a structural correction area that requires adjustment of the fixed point position or increase of the number of fixed points.

[0100] S43: Determine the injection speed switching location; Based on the location of the screw corresponding to the key protection area Screw speed before switching and injection system response time Calculate the speed switching advance displacement: ; As the screw position increases during the injection process, the speed switching position is... When the screw position decreases during the injection process, the speed switching position is as follows: This is designed to ensure that the speed switching position is located before the melt reaches the key protection area.

[0101] Specifically, when the injection control zones of multiple key protection areas overlap, the target low-speed injection speed with the smallest value within the overlapping zone is taken as the execution speed of that zone.

[0102] S44: Determine the opening and closing times of the exhaust valve; For each key protected area, identify the exhaust channels and exhaust valves connected to that area, and obtain the effective volume of the exhaust channels. Measured average volumetric flow rate of the exhaust valve under the set pressure difference and exhaust valve response time .

[0103] The time required for the exhaust channel to complete one effective exhaust cycle is: ; The exhaust valve opens at the following time: ; in, The arrival time of the melt at the venting channel inlet is taken as the arrival time of the melt in the area closest to the puncture-resistant sheet area of ​​the venting channel inlet; in particular, if the channel serves multiple areas at the same time, the earliest arrival time is taken.

[0104] It should be noted that the measured average volumetric flow rate of the exhaust valve... The test was conducted under the same initial mold pressure and vent valve opening as in actual production. In particular, when a vent channel is connected to multiple key protected areas, the earliest melt arrival time is used to determine the vent valve opening time.

[0105] The arrival status of the melt is determined by a pressure sensor or temperature sensor installed at the inlet of the exhaust channel. When the pressure at the inlet of the exhaust channel reaches the preset closing pressure, or the temperature at the inlet of the exhaust channel reaches the melt arrival temperature threshold, the corresponding exhaust valve is closed.

[0106] In another embodiment, the preset sealing pressure and melt arrival temperature threshold are obtained through the first round of trial production: a pressure sensor is set at the inlet of the exhaust channel to record the pressure peak when the melt just arrives at the inlet but has not yet entered the valve body, and 80% of the peak value is taken as the sealing pressure threshold; the temperature threshold is taken as 50% of the temperature rise when the melt arrives.

[0107] S45: Performs coordinated control of segmented injection and venting; After injection begins, the controller reads the screw position, injection pressure, cavity pressure, cavity temperature, and venting channel detection signals in real time.

[0108] Before the screw reaches the first speed switching position, fill at the preset initial injection speed.

[0109] Screw reaches speed switching position At that time, switch the injection speed to the corresponding target low-speed injection speed. .

[0110] In cases where injection control zones for multiple key protected areas overlap, the injection should be performed at the minimum target speed within the overlapping zone.

[0111] When the exhaust valve opens When the exhaust valve is activated, the corresponding exhaust valve is opened; when the exhaust channel inlet detection signal reaches the closing condition specified in S44, the corresponding exhaust valve is closed.

[0112] During the coverage of key protected areas, the cavity pressure rise rate is calculated in real time and compared with the allowable pressure rise rate corresponding to the target speed in the S42 calibration data table; when the actual rate is higher than the allowable rate, the injection speed is switched to the next lower stable speed level in the calibration data table.

[0113] After completing the covering of all key protection areas, the remaining part of the cavity is filled according to the preset subsequent filling speed. After reaching the pressure holding switching conditions, the pressure holding stage is entered.

[0114] Furthermore, the subsequent filling speed adopts the process setting value, and the pressure holding switching condition is that the screw position reaches 98% of the calculated filling volume or the cavity pressure reaches the set peak value.

[0115] Complete the injection molding of the puncture-resistant safety shoes.

[0116] Example 2: To facilitate understanding of the principle behind this invention for identifying weak areas in puncture-resistant panels, in another preferred embodiment, the steel midsole of a size 40 safety shoe is used as the subject. Following the method described in Embodiment 1, it is divided into four regions: medial forefoot (A), lateral forefoot (B), arch (C), and heel (D). After molding, the temperature changes and the decay process of residual offset resistance in each region are continuously monitored to verify whether the differences in thermal contact states in different regions after molding do indeed lead to different decay rates of offset resistance, and whether such differences are sufficient to affect the identification results of weak areas.

[0117] A puncture-resistant steel midsole with a thickness of 2.0 mm was selected and divided into four areas as described in Example 1: medial forefoot A, lateral forefoot B, arch C, and heel D.

[0118] The closing time is denoted as Temperature data for each region was recorded with a sampling period of 0.5 seconds, and the remaining anti-displacement force for each region was calculated according to the methods described in S21-S25. The mold temperature is set to 160℃, and the initial temperature of the puncture-resistant sheet is 25℃.

[0119] The measured temperatures and corresponding residual offset force data for each region are as follows:

[0120] Temperature data shows that the arch area (C) heated up the fastest, reaching 95℃ in 5 seconds, while the forefoot areas (A and B) reached 82℃ and 78℃ respectively, and the heel area (D) reached 73℃. This is because the contact area between the arch support plate and the mold support surface is small, and the support distance is large (i.e., a high degree of suspension), resulting in poor heat conduction from the mold to the plate. Heat tends to accumulate more easily inside the plate and is harder to dissipate through the contact surface to the mold. The forefoot area has sufficient contact, and heat is continuously conducted to the mold, resulting in a relatively slower temperature rise. Although the heel area has a larger contact area, the curvature of this area changes significantly, and the thermal resistance between the plate and the mold is uneven.

[0121] The residual anti-displacement force data show that the attenuation is most significant in the arch region (C), decreasing from an initial value of 360N to 240N after 30 seconds, a drop of 33.3%, with the steepest attenuation trend occurring in the first 15 seconds. The heel region (D) is next, decreasing from 440N to 368N after 30 seconds, a drop of 16.4%. The medial forefoot region (A) and lateral forefoot region (B), due to their higher fixation coverage and better structural support, show relatively slower attenuation, with decreases of only 18.3% and 14.6%, respectively.

[0122] This experimental example demonstrates that if a holistic assessment is used instead of zoned thermal contact state detection, the rapid decay in the arch area will be averaged out by other areas, masking the weak points. However, by using the methods described in S1 to S2 of this invention, the arch area C, due to its lowest fixed coverage and fastest heating rate, is accurately identified as the key protection area.

[0123] Example 3: After identifying the arch region C as a key protection area in the aforementioned embodiments, this experimental example further examines the actual impact of injection speed on the instability risk of this area. By varying the injection speed under the same conditions, the cavity pressure difference, offset force, and final edge displacement of the arch region C at different speeds are measured to verify whether the control strategy of reducing the injection speed in the key protection area in S4 is indeed effective, and to determine the minimum speed that meets safety requirements.

[0124] In this embodiment, with the mold temperature, material batch, and fixing method remaining constant, filling tests were conducted at three injection speeds: 20 cm³ / s, 25 cm³ / s, and 30 cm³ / s. The area of ​​region C... Direction coefficient .

[0125] Record the cavity pressure difference when the melt reaches region C. Calculate the melt displacement force according to the method described in S33. .

[0126] Meanwhile, the data table from Experiment Example 2 above shows the remaining resistance to displacement at 15s after the melt arrives. Based on this, the offset margin is calculated. .

[0127] After demolding, the actual outward displacement of the edge of area C is measured by visual inspection. The allowable offset for this area is 2.0mm, as detailed below:

[0128] As shown in the table above, when the injection speed increases from 20 cm³ / s to 30 cm³ / s, the cavity pressure difference increases from 1.12 MPa to 1.82 MPa (an increase of 62.5%), and the offset force increases from 219 N to 356 N (an increase of 62.5%), which is higher than the increase in injection speed. In the physical mechanism of injection molding, the melt must overcome flow resistance when filling the cavity. The higher the injection speed, the greater the pressure gradient at the melt front, the greater the pressure difference on both sides of the puncture-resistant sheet, and the greater the force driving the sheet offset.

[0129] Under conditions of 25 cm³ / s, the allowance is -21 N, and the measured offset is 2.2 mm, exceeding the allowable offset of 2.0 mm, making the product unqualified. Under conditions of 20 cm³ / s, the allowance is +50 N, and the measured offset is only 1.1 mm, making the product qualified. When the allowance changes from -21 N to +50 N, the measured offset decreases from 2.2 mm to 1.1 mm, a reduction of 50%, indicating a clear correspondence between the offset tolerance allowance and the offset.

[0130] This experimental example verifies the rationality of the target velocity selection method described in S42: using the remaining anti-deflection force As a matching benchmark, selection is made through calibration to meet the requirements. (Right now The maximum speed is 20 cm³ / s, at which the product is qualified and the loss of production efficiency is minimal. At the same time, the above also explains the necessity that the speed switching position in S43 must precede the arrival position of the melt. If the speed is reduced after the melt has reached the arch area and generated a high-pressure impact, the pressure peak has already formed, and deviation will be unavoidable, significantly reducing the injection molding quality.

[0131] Example 4: The vision-servo-based puncture-resistant safety shoe alignment injection molding control system of this invention, as shown in the embodiment of the invention... Figure 2 As shown, it includes the following modules: The data acquisition module is used to establish the positional relationship between the puncture-resistant patch area and the fixed point, and to obtain the area of ​​the puncture-resistant patch area, the outward normal unit vector of the area edge segment, the normal unit vector of the puncture-resistant patch surface, the position of the fixed point, the distance from the fixed point to the calculated position within the area, the minimum distance from the fixed point to the edge of the puncture-resistant patch, the minimum design distance from the edge of the puncture-resistant patch to the finished shoe sole boundary, the initial position deviation before mold closing, the thickness of the shoe sole substrate, the effective support distance, the local curvature, and the area temperature data after mold closing.

[0132] The constraint calculation module is used to calculate the local and regional fixed constraint transfer coefficients of the fixed point to each puncture-resistant patch area based on the distance from the fixed point to the calculated position within the area, the minimum distance from the fixed point to the edge of the puncture-resistant patch, the thickness of the sole substrate at the fixed point location, and the local curvature. It also calculates the regional structural support coefficient, initial anti-offset force, and allowable offset based on the average sole substrate thickness, effective support distance, and local curvature of the area.

[0133] The heat calculation module is used to determine the regional overheating amount and the moment when the region enters the heat decay state based on the regional temperature data and the thermal decay initiation temperature; calculate the effective heat exposure amount based on the overheating amount and the regional thermal response time constant; calculate the regional residual offset force based on the effective heat exposure amount, the reference heat exposure amount, the initial offset resistance force, and the minimum residual offset resistance force; and determine the minimum offset resistance force and the offset weakness time window based on the allowable offset amount and the regional static load-displacement calibration curve.

[0134] The flow determination module is used to determine the main flow path of the melt reaching each anti-puncture plate area, the confluence position of adjacent melt fronts, and the connecting venting channel based on the injection port location, flow channel structure, mold cavity geometry model, cavity thickness distribution, and preset injection speed curve; and to determine the melt arrival time and corresponding screw position of the melt reaching each anti-puncture plate area based on cavity pressure, cavity temperature, screw position, and modified flow simulation results.

[0135] The risk assessment module is used to calculate the melt offset force in the outward movement direction of the edge based on the upstream cavity pressure, downstream cavity pressure, area of ​​the region, and the directional component between the melt flow direction and the unit normal vector of the region edge. For regions with edge lifting risk, it calculates the melt offset force in the edge lifting direction based on the pressure difference of the melt on both sides of the anti-puncture sheet and the unit normal vector of the anti-puncture sheet surface. It also calculates the anti-offset margin based on the remaining anti-offset force and melt offset force at the melt arrival time, and determines the stable region, the region of concern, and the injection molding instability region by combining the anti-offset weak time window.

[0136] The collaborative control module identifies injection molding instability areas as key protection zones and determines the injection control range based on melt arrival time, corresponding screw position, weak anti-displacement time window, anti-displacement margin, and injection system response time. It determines the target low-speed injection speed based on calibration data between injection speed, pressure rise rate, and melt displacement force. It determines the speed switching position based on the screw position and speed switching advance displacement in the target area. It determines the vent valve opening time based on the effective volume of the vent channel, the measured average volumetric flow rate of the vent valve, the vent valve response time, and the melt arrival time at the vent channel inlet, and determines the vent valve closing conditions based on the vent channel inlet pressure or temperature. During the coverage of the key protection zone, it implements real-time speed reduction control based on the actual pressure rise rate.

[0137] Example 5: This embodiment provides an electronic device, including: a processor and a memory, wherein the memory stores a computer program that can be called by the processor; The processor executes the aforementioned visual servo-based puncture-resistant safety shoe alignment injection control method by calling the computer program stored in memory.

[0138] The electronic device can vary considerably depending on its configuration or performance. It may include one or more Central Processing Units (CPUs) and one or more memories, wherein the memory stores at least one computer program, which is loaded and executed by the processor to implement the vision-servoing-based puncture-resistant safety shoe alignment injection control method provided in the above-described embodiment. The electronic device may also include other components for implementing its functions; for example, it may have wired or wireless network interfaces and input / output interfaces for data input and output. Details will not be elaborated upon in this embodiment.

[0139] Example 6: This embodiment proposes a computer-readable storage medium on which an erasable and rewritable computer program is stored. When the computer program runs on the computer device, it causes the computer device to execute the above-described visual servo-based puncture-resistant safety shoe alignment injection control method of the present invention.

[0140] For example, computer-readable storage media can be read-only memory (ROM), random access memory (RAM), compact disc read-only memory (CD-ROM), magnetic tape, floppy disk, and optical data storage devices.

[0141] It should be understood that in the various embodiments of this application, the order of the above-mentioned processes does not imply the order of execution. The execution order of each process should be determined by its function and internal logic, and should not constitute any limitation on the implementation process of the embodiments of this application.

[0142] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely illustrative of the principles of the invention. Various changes and modifications can be made to the invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the claimed invention.

Claims

1. A method for puncture-resistant safety shoe alignment injection molding control based on visual servoing, characterized in that, include: Obtain the fixation status information and thermal contact status information of each area of ​​the puncture-resistant patch, including: The fixed area, fixed point distribution, and edge contour position of the puncture-resistant patch are collected. The fixed coverage rate of each area is determined based on the fixed area and fixed point distribution. The edge position deviation of each area is determined based on the comparison result between the edge contour position and the preset reference contour. After mold closing, the surface temperature of each area of ​​the anti-puncture sheet and the temperature of the corresponding mold area are collected. Based on the continuously collected temperature data, the temperature difference of the mold sheet and the heating rate of the sheet are determined. Based on the fixed state information and the thermal contact state information, the anti-displacement level of each region during mold closing and the initial stage of injection molding and its decay trend with heating time are determined, and key protection areas are determined based on the anti-displacement level and the decay trend. Specifically, it includes: Based on the fixed coverage, fixed point distribution, edge position deviation, mold temperature difference and sheet heating rate, the pre-established anti-offset calibration relationship is invoked to determine the anti-offset level and allowable offset threshold of each region in the mold closing and early injection molding stages. The anti-displacement rating of each region is updated according to the heating rate during the injection molding process, and the decay of the anti-displacement capability of each region with heating time is obtained. Areas with a displacement resistance level lower than a preset level are identified as key protection areas; The melt arrival state and pressure application state of each region during the melt filling process are obtained. Based on the melt arrival state and pressure application state and the anti-displacement level of each region, the injection molding instability region is determined. Based on the injection molding instability region, control the switching of injection speed and the opening and closing of the vent valve; Based on the actual offset state of the puncture-resistant sheet after molding, the switching of the injection speed and the opening and closing of the vent valve in subsequent injection cycles are corrected.

2. The method for puncture-resistant safety shoe alignment injection molding control based on visual servoing according to claim 1, characterized in that, The melt arrival state and pressure application state of each region during the melt filling process are obtained. Based on the melt arrival state and pressure application state and the displacement resistance level of each region, the injection molding instability regions are determined, including: Based on the injection port location, local cavity thickness, and preset injection process, determine the flow path of the melt extending to each edge of the puncture-resistant sheet; Collect the injection pressure curve and screw position curve of the injection molding machine, and combine them with the temperature detection points or pressure detection points set at the corresponding positions of the mold to determine the arrival time of the melt to each edge of the anti-puncture sheet; The arrival time difference of the melt is determined based on the arrival time of different edges, and the pressure change state of the melt before and after reaching the key protection area is determined based on the injection pressure curve; The melt arrival time difference and the pressure change state are matched with the anti-displacement level of each region, and the region that meets the risk judgment condition is identified as the injection molding instability region.

3. The method for puncture-resistant safety shoe alignment injection molding control based on visual servoing according to claim 1, characterized in that, Controlling the injection speed switching based on the injection instability region includes: Based on the arrival time of the melt in the injection instability zone and the corresponding screw position, the switching position of the injection speed is determined so that the melt fills the key protection zone at a target speed that matches the anti-deflection level of the key protection zone.

4. The method for puncture-resistant safety shoe alignment injection molding control based on visual servoing according to claim 1, characterized in that, Controlling the opening and closing of the vent valve according to the injection molding instability region includes: Based on the arrival time of the melt at each edge of the anti-puncture sheet, the opening time of the vent valve connected to the injection molding instability area is determined, so that the vent channel is in the venting state before the melt covers the anti-puncture sheet, and the corresponding vent valve is closed after the melt reaches the vent channel inlet.

5. The method for puncture-resistant safety shoe alignment injection molding control based on visual servoing according to claim 1, characterized in that, The adjustment of the injection speed switching and the opening and closing of the vent valve in subsequent injection cycles based on the actual offset state of the puncture-resistant sheet after molding includes: After injection molding is completed, the actual edge contour of the puncture-proof piece in the molded product is obtained by visual inspection. The actual edge contour is compared with the preset target contour to determine the actual offset of each area of ​​the puncture-proof piece. When the actual offset meets the correction conditions, the switching position of the injection speed is adjusted according to the offset area, and the opening time of the exhaust valve is adjusted according to the edge lifting state.

6. The method for puncture-resistant safety shoe alignment injection molding control based on visual servoing according to claim 2, characterized in that, The area that meets the risk assessment criteria is identified as an injection molding instability area. This includes: when the melt arrival time difference and pressure change state of a certain area meet the risk assessment criteria corresponding to the anti-displacement level of that area, the area is identified as an injection molding instability area, and the displacement direction or edge lifting direction of the anti-puncture sheet is determined according to the melt flow direction and edge position relationship.

7. The method for puncture-resistant safety shoe alignment injection molding control based on visual servoing according to claim 1, characterized in that, Determining areas with a displacement resistance level lower than a preset level as key protection areas includes: determining areas with a displacement resistance level lower than a preset level and whose displacement resistance decay rate with heating time meets a preset condition as priority protection areas.

8. A vision-servo-based puncture-resistant safety shoe alignment injection molding control system, used to implement the vision-servo-based puncture-resistant safety shoe alignment injection molding control method as described in any one of claims 1-7, characterized in that, Includes the following modules: The data acquisition module is used to acquire the fixation status information and thermal contact status information of each area of ​​the puncture-resistant patch; The constraint calculation module is used to calculate the transmission state of the fixed constraint to each region of the puncture-resistant sheet based on the fixed state information. The heat calculation module is used to calculate the remaining anti-displacement state of each area of ​​the puncture-resistant sheet after being heated, based on the heat contact state information. The flow determination module is used to determine the arrival status of the melt in each region during the melt filling process; The risk assessment module is used to determine the injection molding instability region based on the transmission state of the fixed constraint, the remaining anti-offset state, and the melt arrival state. The collaborative control module is used to control the switching of injection speed and the opening and closing of the vent valve according to the injection molding instability region.

Citation Information

Patent Citations

  • Injection molding machine control method and system based on visual algorithm, medium and program product

    CN120245356A

  • Injection mold insert monitoring system based on multi-source sensor

    CN121375043A