A Diammonium Phosphate Production Process Based on Waste Acid from Titanium Chemical Industry

By treating titanium chemical wastewater and waste acid with a two-stage series cation adsorption resin column to produce diammonium phosphate, the impact of cationic impurities on the quality and production efficiency of phosphoric acid and diammonium phosphate products in the resource utilization of titanium chemical wastewater has been solved, achieving efficient resource utilization and improved product purity.

CN122853335BActive Publication Date: 2026-11-10INNER MONGOLIA DADI YUNTIAN CHEM CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202611374668.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2026-09-07
Publication Date
2026-11-10
Estimated Expiration
2046-09-07

AI Technical Summary

Technical Problem

Existing technologies cannot effectively reduce the adverse effects of cationic impurities on the quality and production efficiency of phosphoric acid and diammonium phosphate products while simultaneously utilizing waste acid and wastewater from titanium chemical industries.

Method used

A two-stage series cation adsorption resin column was used to pretreat titanium chemical wastewater and waste acid. The pretreated titanium chemical wastewater and waste acid were then reacted with phosphate rock to produce dilute phosphoric acid and diammonium phosphate. A cation adsorption resin column with a specific composition was used. The resin consisted of monosubstituted and disubstituted products. Macroporous cross-linked copolymer microspheres were prepared by suspension copolymerization and then hydrolyzed with hydrochloric acid to obtain the cation adsorption resin.

Benefits of technology

It significantly improves the purity of diammonium phosphate products, reduces the loss of effective phosphorus, increases the proportion of water-soluble phosphorus, ensures product quality and production efficiency, and realizes the resource utilization of titanium chemical wastewater and the simultaneous improvement of product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122853335B_ABST
    Figure CN122853335B_ABST
Patent Text Reader

Abstract

This invention belongs to the field of waste acid and wastewater treatment technology, and relates to a diammonium phosphate production process based on titanium chemical waste acid wastewater, including the following steps: S1. After sedimentation, the titanium chemical wastewater is microfiltered and then passed through a two-stage series-connected cation adsorption resin column to obtain pretreated titanium chemical wastewater; after sedimentation, the titanium chemical waste acid is microfiltered and then passed through a two-stage series-connected cation adsorption resin column, and then mixed with industrial sulfuric acid to obtain pretreated titanium chemical waste acid; S2. Phosphate rock is prepared into a slurry using the pretreated titanium chemical wastewater; S3. The slurry is heated and then the pretreated titanium chemical waste acid is added. After continuous reaction, it is filtered to obtain dilute phosphoric acid; S4. The dilute phosphoric acid is concentrated, heated, and ammonified by introducing ammonia gas to obtain diammonium phosphate slurry, which is then granulated and dried to obtain diammonium phosphate. This invention can significantly improve the purity of diammonium phosphate products, while improving product quality and production efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of waste acid and wastewater treatment technology, and in particular to a diammonium phosphate production process based on waste acid and wastewater from titanium chemical industry. Background Technology

[0002] In the sulfuric acid process for titanium dioxide production, when titanium ore is acidified and hydrolyzed with concentrated sulfuric acid to prepare metatitanic acid, hydrolytic waste acid with a sulfuric acid concentration of 20%-25% and containing various metal ions is generated; the metatitanic acid washing process generates washing wastewater with a sulfuric acid content of 3%-8%.

[0003] To achieve resource recycling, current production processes typically mix hydrolysis waste acid with industrial sulfuric acid to create sulfuric acid with a concentration of approximately 65%, which is then transported to the phosphate chemical system for the acidolysis of phosphate rock to produce phosphoric acid. Washing wastewater is then introduced into the phosphate chemical system for phosphate rock slurry preparation. However, residual metallic cations such as titanium, iron, aluminum, and magnesium in this waste acid and wastewater subsequently enter the phosphate chemical system.

[0004] In the phosphate chemical system, phosphate rock and sulfuric acid are acid-hydrolyzed and filtered to produce dilute phosphoric acid. After concentration, the dilute phosphoric acid reacts with liquid ammonia to produce products such as diammonium phosphate and monoammonium phosphate. When waste acid and wastewater from titanium chemical plants are introduced, the metal cations in them enter the phosphoric acid system during the acid-hydrolyzed process. High-valence cations form complexes and colloidal phosphate precipitates in the phosphoric acid medium, and are further oxidized and transformed during ammoniation, concentration, granulation, and drying. This results in a significant decrease in the purity of phosphoric acid, and the diammonium phosphate product exhibits abnormal color, even turning black or mottled. At the same time, it causes problems such as increased consumption of available phosphorus, decreased water-soluble phosphorus ratio, increased slurry viscosity, and equipment scaling, seriously affecting the quality of diammonium phosphate products and production efficiency.

[0005] In an effort to improve product quality, existing technologies have attempted to increase the amount of additives to improve product quality. However, this has not only failed to improve the abnormal purity of phosphoric acid, but has also led to a significant increase in the reaction time between the additives and phosphoric acid, resulting in a worse product quality than before and failing to achieve the expected results.

[0006] While theoretically chemical precipitation, membrane separation, and ion adsorption methods can be used to treat cationic impurities in waste acid wastewater, chemical precipitation in strong acid systems suffers from problems such as high consumption of precipitant, excessive sludge production, and easy introduction of new impurities. Membrane separation in high acid, high salt systems containing colloidal particles has poor long-term operational stability, short lifespan, and high cost.

[0007] Therefore, how to effectively reduce the adverse effects of cationic impurities on the quality and production efficiency of phosphoric acid and diammonium phosphate products while maintaining the resource utilization of waste acid and wastewater from titanium chemical industry has become a technical problem that urgently needs to be solved in this field. Summary of the Invention

[0008] The technical problem to be solved by this invention is that the existing technology has the disadvantage of not being able to simultaneously realize the resource utilization of waste acid wastewater from titanium chemical industry and ensure the quality of diammonium phosphate products. To this end, we propose a diammonium phosphate production process based on waste acid wastewater from titanium chemical industry.

[0009] To achieve the above objectives, this application adopts the following technical solution: a diammonium phosphate production process based on titanium chemical waste acid, comprising the following steps: S1. After sedimentation, the titanium chemical wastewater is microfiltered and then passed through two-stage cation adsorption resin columns in series to obtain pretreated titanium chemical wastewater. The waste acid from titanium chemical industry is settled and then microfiltered, then passed through a two-stage series of cation adsorption resin columns, and finally mixed with industrial sulfuric acid to obtain pretreated waste acid from titanium chemical industry. S2. Phosphate rock is prepared into a slurry by pretreating titanium chemical wastewater; S3. After heating the slurry, pretreated titanium chemical waste acid is added, and after continuous reaction, it is filtered to obtain dilute phosphoric acid. S4. After concentrating dilute phosphoric acid, heating it and introducing ammonia gas for ammoniation, diammonium phosphate slurry is obtained, which is then granulated and dried to obtain diammonium phosphate.

[0010] Preferably, the cation adsorption resin column is prepared by the following steps: (1) 4-Chloromethylstyrene reacts with diethyl aminomethylphosphonate to generate a bicomponent functional monomer consisting of a monosubstituted product and a disubstituted product; (2) A suspension copolymerization of two-component functional monomers, styrene and divinylbenzene was carried out to prepare macroporous crosslinked copolymer microspheres; (3) The macroporous cross-linked copolymer microspheres were hydrolyzed with hydrochloric acid and then washed to obtain a cationic adsorption resin; (4) The cation adsorption resin column is prepared by wet packing of the cation adsorption resin column.

[0011] Preferably, the specific method of step (1) is as follows: in a reactor, diethyl aminomethylphosphonate, organic solvent and acid-binding agent are added, the temperature is raised to 60-80°C and 4-chloromethylstyrene is slowly added dropwise. After the addition is completed, the reaction is kept at the temperature for 8-12 hours. After filtration, washing and vacuum evaporation to remove the solvent, the bicomponent functional monomer is obtained. The organic solvent is selected from acetonitrile, tetrahydrofuran, or N,N-dimethylformamide; The acid-binding agent is selected from either potassium carbonate or sodium carbonate; The molar ratio of 4-chloromethylstyrene and diethyl aminomethylphosphonate is 1:(0.5-1.0). The bicomponent functional monomer is composed of a monosubstituted product and a disubstituted product, with a molar ratio of (70-95):(5-30). The monosubstituted product has the structure shown in Formula A, and the disubstituted product has the structure shown in Formula B: , .

[0012] The cationic adsorption resin column of the present invention comprises a two-component functional monomer consisting of a monosubstituted product and a disubstituted product. The monosubstituted product serves as a functional monomer to provide chelation sites, while the disubstituted product serves as a cross-linking functional monomer, allowing the cross-linking points to simultaneously carry phosphonic acid groups. The two can be directly suspended and copolymerized without separation, which simplifies the resin preparation process, reduces production costs, and achieves simultaneous control of adsorption capacity and framework mechanical strength. The resulting resin has a uniform functional group density and a regular cross-linking network, exhibiting higher effective capacity utilization and faster adsorption effect in strong acid systems.

[0013] Preferably, the specific method of step (2) is as follows: a two-component functional monomer, styrene, divinylbenzene, pore-forming agent and initiator are mixed to form an oil phase, polyvinyl alcohol, sodium chloride and deionized water are mixed to form an aqueous phase, the oil phase is added to the aqueous phase, and the mixture is stirred and heated to 60-80℃ under nitrogen protection for 18-24 hours. After filtration, washing and sieving, the macroporous crosslinked copolymer microspheres are obtained. The pore-forming agent is selected from at least one of toluene, n-heptane, or 2-ethylhexanol; The initiator is selected from azobisisobutyronitrile or benzoyl peroxide; The mass ratio of the two-component functional monomer, styrene, divinylbenzene, porogen, and initiator in the oil phase is (30-60):(10-30):(5-15):(60-150):(0.5-1.5). The mass ratio of polyvinyl alcohol, sodium chloride, and deionized water in the aqueous phase is (0.5-2):(5-20):(300-500). The mass ratio of the oil phase to the water phase is 1:(2-4); The average particle size of the macroporous crosslinked copolymer microspheres is 0.3-1.25 mm.

[0014] Preferably, the specific method of step (3) is as follows: In a reactor, macroporous cross-linked copolymer microspheres and concentrated hydrochloric acid are added, and after reflux reaction for 18-24 hours, the mixture is washed with water until neutral to obtain the cation adsorption resin; The mass concentration of the concentrated hydrochloric acid is 30%-40%; The mass ratio of the macroporous crosslinked copolymer microspheres to concentrated hydrochloric acid is 1:(3-10).

[0015] Preferably, the specific method of step (4) is as follows: the resin and water are mixed into a slurry at a volume ratio of 1:(1-2), and slowly added into the adsorption column from the top of the column to obtain the cation adsorption resin column; The height-to-diameter ratio of the cation adsorption resin column is 3-6:1.

[0016] The cation adsorption resin column of the present invention is prepared by wet packing of a cation adsorption resin having a macroporous cross-linked polystyrene-divinylbenzene framework and containing aminomethylene phosphonic acid groups. The resin framework and carbon-phosphorus bonds are resistant to strong acids and can operate stably for a long time in waste acid systems with sulfuric acid concentration of 20%-30%. The aminomethylene phosphonic acid groups have a selective chelating effect on high-valence cations, taking into account both high adsorption capacity and high selectivity. The macroporous structure is conducive to the mass transfer of ions in high-viscosity strong acid systems, so that the prepared cation adsorption resin column has excellent acid resistance, high selective chelating ability and high adsorption capacity.

[0017] Preferably, in step S1, the sulfuric acid concentration in the titanium chemical wastewater is 3%-8%, the sulfuric acid concentration in the titanium chemical waste acid is 20%-30%, and the sulfuric acid concentration in the industrial sulfuric acid is 90%-98%. The suspended solids content of the filtrate after microfiltration treatment of titanium chemical wastewater and titanium chemical waste acid is ≤5mg / L; The adsorption temperature of the cation adsorption resin column is 25-60℃, the space velocity is 3-8 BV / h, and it adsorbs Fe from the water. 3+ ≤50mg / L, total iron removal rate ≥90%; The mass concentration of the pretreated titanium chemical waste acid is 55%-75%.

[0018] Preferably, in step S2, the amount of pretreated titanium chemical wastewater added is 30%-80% of the mass of phosphate rock; In step S3, the heating temperature of the slurry is 80-90℃, and the reaction time is 6-8h. The amount of pretreated titanium chemical waste acid added is 70-110% of the slurry mass.

[0019] Preferably, in step S4, the dilute phosphoric acid is concentrated to a mass concentration of 40-50%. The ammoniation temperature is 110-120℃, and ammonia gas is introduced to neutralize the pH to 7.5-8.5.

[0020] Preferably, the diammonium phosphate contains ≥90% water-soluble phosphorus, ≤2.0% moisture, and ≥90% particle size of 1-4mm.

[0021] The technical effects and advantages of this invention are as follows: (1) The diammonium phosphate production process based on titanium chemical waste acid wastewater provided by the present invention pre-treats the titanium chemical waste acid wastewater with a cation adsorption resin column before producing diammonium phosphate. This effectively removes cationic impurities such as titanium, iron, aluminum, and magnesium in the waste acid wastewater before it enters the phosphate rock acid hydrolysis process, thus avoiding the formation of colored complexes and colloidal precipitates during the ammoniation, concentration, and drying processes. This significantly improves the purity of the diammonium phosphate product, while reducing effective phosphorus loss and increasing the proportion of water-soluble phosphorus, thereby improving product quality and production efficiency.

[0022] (2) In the diammonium phosphate production process based on titanium chemical waste acid wastewater provided by the present invention, the titanium chemical waste acid wastewater is treated by two-stage series cation adsorption resin columns, and the total iron removal rate reaches more than 90%. Moreover, no improvement additives are needed during the treatment process, which fundamentally avoids the problems of prolonged reaction time and poor product quality caused by additives. It effectively weakens the influence of key cations and ensures the quality of products as well as the continuity and stability of production.

[0023] (3) In the diammonium phosphate production process based on titanium chemical waste acid wastewater provided by the present invention, the cation adsorption resin column is prepared by wet packing of a cation adsorption resin with a macroporous cross-linked polystyrene-divinylbenzene skeleton and containing aminomethylene phosphonic acid groups; the resin skeleton and carbon-phosphorus bonds are resistant to strong acids and can operate stably for a long time in a waste acid system with a sulfuric acid concentration of 20%-30%; the aminomethylene phosphonic acid groups have a selective chelating effect on high-valence cations, taking into account both high adsorption capacity and high selectivity, and the macroporous structure is conducive to the mass transfer of ions in a high-viscosity strong acid system, so that the prepared cation adsorption resin column has excellent acid resistance, high selective chelating ability and high adsorption capacity.

[0024] (4) In the diammonium phosphate production process based on titanium chemical waste acid wastewater provided by the present invention, the two-component functional monomer of the cation adsorption resin column is composed of monosubstituted products and disubstituted products. The monosubstituted products provide chelation sites as functional monomers, and the disubstituted products carry phosphonic acid groups at the crosslinking points as crosslinking functional monomers. The two can be directly suspended and copolymerized without separation, which simplifies the resin preparation process, reduces production costs, and realizes the synchronous control of adsorption capacity and skeleton mechanical strength. The resulting resin has uniform functional group density and regular crosslinking network, and exhibits higher effective capacity utilization and faster adsorption effect in strong acid system.

[0025] (5) The diammonium phosphate production process based on titanium chemical waste acid wastewater provided by the present invention organically combines cation adsorption pretreatment with phosphate rock slurry preparation, acid hydrolysis, filtration, concentration, ammonia introduction and granulation drying. While ensuring the purity and quality of diammonium phosphate products, it realizes the recycling of titanium chemical waste acid wastewater, reduces the consumption of fresh sulfuric acid and process water, and comprehensively reduces the negative impact of key factors on product quality and production efficiency. It meets the development requirements of green chemical industry and has significant economic and environmental benefits. Attached Figure Description

[0026] The disclosure of this invention is illustrated with reference to the accompanying drawings. It should be understood that the drawings are for illustrative purposes only and are not intended to limit the scope of protection of this invention.

[0027] Figure 1 This is a flowchart of the diammonium phosphate production process based on titanium chemical waste acid wastewater of the present invention; Figure 2 The infrared spectrum of the monosubstituted product of this invention; Figure 3 The infrared spectrum of the disubstituted product of this invention is shown. Detailed Implementation

[0028] It is readily understood that, based on the technical solution of this invention, those skilled in the art can propose various interchangeable structural methods and implementations without altering the essential spirit of the invention. Therefore, the following detailed embodiments and accompanying drawings are merely illustrative examples of the technical solution of this invention and should not be considered as the entirety of the invention or as limitations or restrictions on the technical solution of this invention.

[0029] In the specific embodiments of the present invention, the commercially available aminophosphonic acid chelating resin is D412 macroporous aminophosphonic acid chelating resin purchased from Shandong Shoucheng Chemical Co., Ltd.; the CAS number of 4-chloromethylstyrene is 1592-20-7; the CAS number of (aminomethyl)phosphonate diethyl ester is 50917-72-1; and the remaining reagents and equipment are conventional reagents and equipment in this technical field.

[0030] Preparation of bicomponent functional monomers (1) In a 2000mL three-necked flask equipped with a stirrer, thermometer and nitrogen inlet, add 0.8mol of diethyl aminomethylphosphonate, 0.7mol of anhydrous potassium carbonate and 800mL of acetonitrile, stir under nitrogen protection to form a suspension, and heat to 60℃. (2) Dissolve 1.0 mol of 4-chloromethylstyrene in 200 mL of acetonitrile and slowly add it dropwise to the above suspension over 2 hours. After the addition is complete, keep the mixture at 70 °C for 6 hours and then at 80 °C for 2 hours. (3) After the reaction is complete, filter to remove inorganic salts, wash the filtrate three times with water to remove free amine hydrochloride, and evaporate acetonitrile under reduced pressure to obtain a pale yellow oily liquid, which is the two-component functional monomer; GC-MS analysis showed that the molar ratio of the monosubstituted product to the disubstituted product was 80:20.

[0031] The infrared spectrum of the monosubstituted product is as follows: Figure 2 As shown, the infrared spectrum of the disubstituted product is as follows: Figure 3 As shown.

[0032] Example 1 Diammonium phosphate based on titanium chemical waste acid wastewater is prepared by the following steps: I. Preparation of cationic adsorption resin (1) According to the formulation in Table 1, the two-component functional monomer, styrene, divinylbenzene, pore-forming agent and initiator are mixed to prepare the oil phase; polyvinyl alcohol, sodium chloride and deionized water are mixed to prepare the aqueous phase; the oil phase is added to the aqueous phase, and the mixture is stirred and heated to 70°C for 18 h under nitrogen protection. After the reaction is completed, the mixture is filtered, washed with hot water, extracted with ethanol by Soxhlet extraction for 12 h, dried, and sieved to obtain 0.3-1.25 mm fractions to obtain macroporous crosslinked copolymer microspheres; Table 1 Suspension copolymer formulation

[0033] (2) Take 30g of macroporous cross-linked copolymer microspheres, add 150mL of concentrated hydrochloric acid with a mass concentration of 37%, reflux for 18h, wash with water until neutral, convert to H+ form with 1mol / L sulfuric acid, drain, and obtain cation adsorption resin. (3) The cation adsorption resin and water are mixed into a slurry at a volume ratio of 1:1.5. The slurry is slowly added from the top of the column into an adsorption column with a height-to-diameter ratio of 5:1 and 1 / 3 column volume of water has been pre-filled. The resin is submerged throughout the column while the material is added. After filling, the column is backwashed with water. The bed expansion rate is 40%. After backwashing for 15 minutes, the cation adsorption resin column is obtained.

[0034] II. Diammonium Phosphate Production Process Based on Waste Acid from Titanium Chemical Industry Take sulfuric acid with a mass concentration of 5%, total iron of 4.5 g / L, and Al... 3+ 1.2 g / L, Mg 2+ The titanium chemical wastewater has a concentration of 0.8 g / L and a sulfuric acid concentration of 25%, with a total iron concentration of 20 g / L and an Al concentration of 10 g / L. 3+ 3 g / L, Mg 2+ 2g / L, Ti 4+ 0.6 g / L titanium chemical waste acid is prepared for future use; S1. Titanium chemical wastewater was settled and then microfiltered until the suspended solids content was ≤5mg / L. The wastewater was then passed through a two-stage cation adsorption resin column at 40℃ and a space velocity of 5BV / h to obtain pretreated titanium chemical wastewater. The effluent contained Fe... 3+ The concentration was 32 mg / L, with a total iron removal rate of 96%. Titanium chemical waste acid was settled and then microfiltered until the suspended solids content was ≤5mg / L. It was then passed through a two-stage cation adsorption resin column at 40℃ and a space velocity of 5BV / h. Finally, it was mixed with 93% industrial sulfuric acid at a mass ratio to achieve a sulfuric acid concentration of 65%, thus obtaining pretreated titanium chemical waste acid. The effluent contained Fe... 3+ The concentration was 38 mg / L, with a total iron removal rate of 95%. S2. Mix 1000g of phosphate rock powder (grinding to pass through a 100-mesh sieve with a mass ratio of ≥90%) with 500g of pretreated titanium chemical wastewater, stir and adjust the slurry for 1 hour to obtain a slurry with a solid volume ratio of 40%. S3. Heat the slurry until the temperature reaches 80°C. Add 1350g of pretreated titanium chemical waste acid at a uniform rate. Maintain the temperature at 85°C and continue the reaction for 8 hours. After the reaction is completed, filter the filter cake at 70°C. Wash the filter cake with pretreated titanium chemical waste water in a three-stage countercurrent process. Combine the washing liquid with the filtrate to obtain dilute phosphoric acid. S4. Dilute phosphoric acid is vacuum concentrated to a mass concentration of 46% based on P2O5, heated to 115℃, and ammonia gas is introduced to neutralize the pH to 7.8 to obtain diammonium phosphate slurry. The slurry is then granulated and dried to obtain diammonium phosphate.

[0035] Example 2 The process is basically the same as in Example 1, except that in step (1), the two-component functional monomer is changed to 35g, styrene to 25g, divinylbenzene to 8g, and the pore-forming agent is changed to 35g toluene, 15g n-heptane, and 20g 2-ethylhexanol.

[0036] Example 3 The process is basically the same as in Example 1, except that in step (1), the two-component functional monomer is changed to 30g, styrene to 28g, and divinylbenzene to 12g; and in step S1, the adsorption temperature is changed to 60℃ and the space velocity is changed to 8BV / h.

[0037] Comparative Example 1 The process is basically the same as in Example 1, except that in step S1, no cation adsorption resin column is set up, and 25% titanium chemical waste acid is directly mixed with 93% industrial sulfuric acid to a concentration of 65%, and the titanium chemical wastewater is directly used for slurry preparation.

[0038] Comparative Example 2 The process is basically the same as in Example 1, except that step S1 is omitted, and 93% industrial sulfuric acid and process water are used instead of pretreated titanium chemical waste acid and pretreated titanium chemical wastewater.

[0039] Comparative Example 3 The process is basically the same as in Example 1, except that a commercially available aminophosphonic acid chelating resin is used instead of the cation adsorption resin column prepared in Example 1.

[0040] Comparative Example 4 The process is basically the same as in Example 1, except that the monosubstituted product purified by column chromatography is used instead of the two-component functional monomer.

[0041] Performance testing 1. Resin performance testing: The resins prepared in Examples 1-3 and Comparative Examples 3-4 were tested. The phosphorus content was determined by elemental analysis; the phosphonic acid exchange capacity was determined by acid-base titration; and the specific surface area and average pore size were determined by a specific surface area analyzer.

[0042] The test results are shown in Table 1 below:

[0043] 2. Resin Adsorption Capacity Test: The resins of Examples 1-3 and Comparative Examples 3-4 were placed in a solution of sulfuric acid with a mass concentration of 20% and Fe... 3+ 2g / L, Mg 2+ 2g / L, Ca 2+ In a simulated solution with a concentration of 0.5 g / L, the solution was shaken at 25 °C for 24 h. The equilibrium concentrations of each ion were determined by ICP-OES, and the Fe was calculated. 3+ Saturated adsorption capacity and selectivity coefficients α(Fe / Mg) and α(Fe / Ca).

[0044] The test results are shown in Table 2 below:

[0045] A comparison of the test results of Examples 1-3 and Comparative Examples 3-4 shows that in the diammonium phosphate production process based on titanium chemical waste acid provided by the present invention, the cation adsorption resin column obtained by copolymerization of two-component functional monomers has a higher density of functional groups and a more developed pore structure. Its specific structure has a stronger selective chelating effect on high-valence cations, exhibiting higher adsorption capacity and selectivity in strong acid systems. This indicates that after the disubstituted product participates in copolymerization as a cross-linked functional monomer, the phosphonic acid groups carried by the cross-linking nodes work synergistically with the suspended chelating arms to further improve the selectivity of the resin for key cations. The above effects cannot be achieved by using only the monosubstituted product.

[0046] 3. Diammonium phosphate product testing: According to the standard GB / T 10205-2009, the percentage of water-soluble phosphorus in Examples 1-3 and Comparative Examples 1-2, the moisture content and particle size were determined, and the appearance and color were observed.

[0047] The test results are shown in Table 3 below:

[0048] A comparison of the test results of Examples 1-3 and Comparative Examples 1-2 shows that in the diammonium phosphate production process based on titanium chemical waste acid wastewater provided by the present invention, cationic impurities in the titanium chemical waste acid wastewater consume available phosphorus and cause product coloring. After reducing cationic impurities from the source through adsorption pretreatment, the purity and quality of the product are significantly improved. This demonstrates that while achieving full recycling of titanium chemical waste acid wastewater, the present invention does not adversely affect the quality of diammonium phosphate products, thus achieving simultaneous protection of resource utilization and product quality.

[0049] The technical scope of this invention is not limited to the content described above. Those skilled in the art can make various modifications and variations to the above embodiments without departing from the technical concept of this invention, and all such modifications and variations should fall within the protection scope of this invention.

Claims

1. A process for producing diammonium phosphate based on waste acid from titanium chemical industry, characterized in that, Includes the following steps: S1. After sedimentation, the titanium chemical wastewater is microfiltered and then passed through two-stage cation adsorption resin columns in series to obtain pretreated titanium chemical wastewater. The waste acid from titanium chemical industry is settled and then microfiltered, then passed through a two-stage series of cation adsorption resin columns, and finally mixed with industrial sulfuric acid to obtain pretreated waste acid from titanium chemical industry. S2. Phosphate rock is prepared into a slurry by pretreating titanium chemical wastewater; S3. After heating the slurry, pretreated titanium chemical waste acid is added, and after continuous reaction, it is filtered to obtain dilute phosphoric acid. S4. After concentrating dilute phosphoric acid, heating it and introducing ammonia gas for ammoniation, diammonium phosphate slurry is obtained, which is then granulated and dried to obtain diammonium phosphate. The cation adsorption resin column is prepared by the following steps: (1) 4-Chloromethylstyrene reacts with diethyl aminomethylphosphonate to generate a bicomponent functional monomer consisting of a monosubstituted product and a disubstituted product; (2) A suspension copolymerization of two-component functional monomers, styrene and divinylbenzene was carried out to prepare macroporous crosslinked copolymer microspheres; (3) The macroporous cross-linked copolymer microspheres were hydrolyzed with hydrochloric acid and then washed to obtain a cationic adsorption resin; (4) The cation adsorption resin column is prepared by wet packing of the cation adsorption resin; The specific method of step (1) is as follows: In a reactor, diethyl aminomethylphosphonate, organic solvent and acid-binding agent are added, the temperature is raised to 60-80℃ and 4-chloromethylstyrene is slowly added dropwise. After the addition is completed, the reaction is kept at the temperature for 8-12 hours. After filtration, washing and depressurization to remove the solvent, the bicomponent functional monomer is obtained. The organic solvent is selected from acetonitrile, tetrahydrofuran, or N,N-dimethylformamide; The acid-binding agent is selected from either potassium carbonate or sodium carbonate; The molar ratio of 4-chloromethylstyrene and diethyl aminomethylphosphonate is 1:(0.5-1.0). The bicomponent functional monomer is composed of a monosubstituted product and a disubstituted product, with a molar ratio of (70-95):(5-30). The monosubstituted product has the structure shown in Formula A, and the disubstituted product has the structure shown in Formula B: , ; The specific method of step (2) is as follows: the two-component functional monomer, styrene, divinylbenzene, pore-forming agent and initiator are mixed to form an oil phase, polyvinyl alcohol, sodium chloride and deionized water are mixed to form an aqueous phase, the oil phase is added to the aqueous phase, and the mixture is stirred and heated to 60-80℃ under nitrogen protection for 18-24 hours. After filtration, washing and sieving, the macroporous crosslinked copolymer microspheres are obtained. The pore-forming agent is selected from at least one of toluene, n-heptane, or 2-ethylhexanol; The initiator is selected from azobisisobutyronitrile or benzoyl peroxide; The mass ratio of the two-component functional monomer, styrene, divinylbenzene, porogen, and initiator in the oil phase is (30-60):(10-30):(5-15):(60-150):(0.5-1.5). The mass ratio of polyvinyl alcohol, sodium chloride, and deionized water in the aqueous phase is (0.5-2):(5-20):(300-500). The mass ratio of the oil phase to the water phase is 1:(2-4); The macroporous crosslinked copolymer microspheres have an average particle size of 0.3-1.25 mm; The specific method of step (3) is as follows: In a reactor, macroporous cross-linked copolymer microspheres and concentrated hydrochloric acid are added, and after reflux reaction for 18-24 hours, the mixture is washed with water until neutral to obtain the cation adsorption resin. The mass concentration of the concentrated hydrochloric acid is 30%-40%; The mass ratio of the macroporous cross-linked copolymer microspheres to concentrated hydrochloric acid is 1:(3-10). The specific method of step (4) is as follows: the resin and water are mixed into a slurry at a volume ratio of 1:(1-2), and slowly added into the adsorption column from the top of the column to obtain the cation adsorption resin column. The height-to-diameter ratio of the cation adsorption resin column is 3-6:

1.

2. The diammonium phosphate production process based on titanium chemical waste acid wastewater according to claim 1, characterized in that, In step S1, the sulfuric acid concentration in the titanium chemical wastewater is 3%-8%, the sulfuric acid concentration in the titanium chemical waste acid is 20%-30%, and the sulfuric acid concentration in the industrial sulfuric acid is 90%-98%. The suspended solids content of the filtrate after microfiltration treatment of titanium chemical wastewater and titanium chemical waste acid is ≤5mg / L; The adsorption temperature of the cation adsorption resin column is 25-60℃, the space velocity is 3-8 BV / h, and it adsorbs Fe from the water. 3+ ≤50mg / L, total iron removal rate ≥90%; The mass concentration of the pretreated titanium chemical waste acid is 55%-75%.

3. The diammonium phosphate production process based on titanium chemical waste acid wastewater according to claim 1, characterized in that, In step S2, the amount of pretreated titanium chemical wastewater added is 30%-80% of the mass of phosphate rock; In step S3, the heating temperature of the slurry is 80-90℃, and the reaction time is 6-8h. The amount of pretreated titanium chemical waste acid added is 70-110% of the slurry mass.

4. The diammonium phosphate production process based on titanium chemical waste acid wastewater according to claim 1, characterized in that, In step S4, the dilute phosphoric acid is concentrated to a mass concentration of 40-50%. The ammoniation temperature is 110-120℃, and ammonia gas is introduced to neutralize the pH to 7.5-8.

5.

5. The diammonium phosphate production process based on titanium chemical waste acid wastewater according to claim 1, characterized in that, The diammonium phosphate contains ≥90% water-soluble phosphorus, ≤2.0% moisture, and ≥90% particle size of 1-4mm.

Citation Information

Patent Citations

  • Adsorption resin for o-phenylenediamine wastewater treatment and preparation method thereof

    CN122321837A

  • Method for recycling high-cod nickel-cobalt-lithium-magnesium wastewater and use thereof

    WO2024192575A1