A process for preparing nuts using electrospun nanofibers loaded with microcapsule powder
By using electrospun nanofibers to load microencapsulated powder, the problem of oxidative rancidity of nuts during storage was solved, achieving stable loading and oxidation inhibition of microencapsulated powder, and extending the shelf life of nuts.
Patent Information
- Application Number
- CN202611541424.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-01
- Publication Date
- 2026-11-10
AI Technical Summary
Nuts are susceptible to oxidative rancidity during storage, transportation, and sales due to factors such as oxygen, moisture, light, and temperature. This results in a short shelf life, unstable loading of functional microcapsule powder, easy migration and oxidation loss, and affects product quality.
The process for preparing nuts using electrospun nanofibers loaded with microcapsule powder involves dispersing functional microcapsule powder in the electrospinning solution of a carrier skeleton material, and then using electrospinning to deposit the spun jet onto the surface of the nut matrix, forming a stable nanofiber-loaded microcapsule powder functional layer. This solves the problems of short shelf life, unstable functional component loading, and easy migration and oxidation loss during shelf life in existing nuts.
It improves the loading stability of microencapsulated powder, delays the oxidative rancidity of nuts, and extends shelf life. After 18 months of storage at room temperature, the surface retention rate of microencapsulated powder reaches 88.4%-93.0%, effectively reducing the migration and loss of functional components. After 90 days of accelerated storage at 40℃, the peroxide value and acid value of the product still meet the qualified standards.
Smart Images

Figure CN123058367A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of microencapsulated powder processing, specifically to a nut preparation process using electrospun nanofibers loaded with microencapsulated powder. Background Technology
[0002] Nuts are rich in unsaturated fatty acids, protein, minerals, and various vitamins. With their crunchy texture, they are a popular snack and an important source of dietary nutrition. As public health awareness continues to rise, consumers are no longer satisfied with simply consuming nuts. They are demanding higher levels of nutritional fortification, functional specialization, and suitability for specific groups. The market demand for targeted functional nut products continues to grow, particularly among children, pregnant women, the elderly, fitness enthusiasts, and consumers seeking sleep improvement or mental stimulation. However, nuts are high in unsaturated fatty acids, making them susceptible to oxidative rancidity during storage, transportation, and sales due to factors such as oxygen, moisture, light, and temperature. This results in a sour taste and shortened shelf life. Furthermore, if functional microencapsulated powders are directly applied to the nut surface, issues such as insufficient adhesion, easy delamination and powder loss, uneven distribution of functional components, and migration and oxidation loss during shelf life further impact product quality and shelf life.
[0003] The prior art CN118830612A discloses a defatted nut, its preparation method, and defatted nut food products. It reduces the oil content of nuts by defatting the nut raw materials to solve the problems of high oil content, easy oxidation and rancidity, and short shelf life of nuts. However, its treatment focuses on defatting and quality control inside the nuts, which may affect the original nutrition, flavor, and crisp texture of the nuts. It does not involve loading functional microcapsule powder onto the surface of the nut kernel to form a stable coating, nor does it involve constructing an electrospun nanofiber loaded microcapsule powder layer on the surface of the nuts to block the migration and oxidation loss of functional components. The prior art CN109123562A discloses a process for preparing Sacha indica nuts, which involves drying the Sacha indica fruit, mixing it with salt and flavorings, steaming it in a steamer, and then drying it until it cracks, resulting in Sacha indica nuts with intact shells, crisp kernels, and a light fragrance. However, it mainly addresses the issue of improving the flavor and texture of Sacha indica nuts, without addressing the issue of extending the shelf life of nuts through surface functional coatings, or the issue of compounding various functional oils / functional ingredients with nut substrates, or the issue of stable loading of functional microcapsule powder on the surface of nuts.
[0004] Therefore, there is an urgent need for a nut preparation process that, without using additional barrier materials or changing the original preparation process of microcapsule powder, uses electrospun nanofibers to load microcapsule powder onto the surface of nuts to form a stable functional layer, improves the adhesion between microcapsule powder and nut matrix, inhibits the migration and oxidation loss of functional components, thereby effectively extending the shelf life of nuts while maintaining the original flavor and texture of nuts. Summary of the Invention
[0005] To address the problem that existing nuts, rich in unsaturated fatty acids, are susceptible to oxidative rancidity due to factors such as oxygen, moisture, light, and temperature during storage, transportation, and sales, resulting in a short shelf life, this invention proposes a nut preparation process using electrospun nanofibers loaded with microcapsule powder. This process involves dispersing functional microcapsule powder in an electrospinning solution on a carrier skeleton material, and then using electrospinning to deposit the spun jet onto the nut substrate surface. After neutralization with a fixative solution, rinsing, drying, and packaging, a stable nanofiber-loaded microcapsule powder functional layer is formed on the nut surface. This solves the problems of short shelf life, unstable functional component loading, and easy migration and oxidation loss during shelf life in existing nuts.
[0006] This invention proposes a process for preparing nuts using electrospun nanofibers loaded with microcapsule powder, comprising the following steps: S1. Raw material sorting: Select nut raw materials, and after washing, drying and morphological processing, obtain nut matrix; S2. Preparation of microencapsulated powder: The functional core material and wall material are emulsified, homogenized and dried to obtain microencapsulated powder; S3. Preparation of electrospinning solution: Dissolve the carrier skeleton material in an acidic mixed solvent and stir to obtain an electrospinning base solution; S4. Electrospinning loading: Add the microcapsule powder obtained in step S2 to the electrospinning base liquid obtained in step S3, stir or ultrasonically disperse evenly to obtain an electrospinning liquid containing microcapsule powder; place the nut matrix obtained in step S1 on a receiving device, and use electrospinning process to deposit the spinning jet on the surface of the nut matrix to obtain a nut with nanofiber loaded microcapsule powder on the surface. S5. Post-processing: The product obtained in step S4 is neutralized with a fixing solution, rinsed and dried. S6. Molding and Packaging: The product obtained in step S5 is packaged to obtain the finished nut product with electrospun nanofiber loaded microcapsule powder.
[0007] Furthermore, the carrier skeleton material in step S3 is composed of a polysaccharide mixture and a polymer.
[0008] Furthermore, the polysaccharide mixture is selected from one or more of pullulan, sodium alginate, starch, pectin, gellan gum, inulin, konjac glucomannan, xanthan gum, guar gum, sodium carboxymethyl cellulose, and β-glucan.
[0009] Furthermore, the polymer is selected from one or more of chitosan, hyaluronic acid, and polyvinyl alcohol.
[0010] Furthermore, the nut ingredients in step S1 include any one of the following: walnuts, almonds, cashews, hazelnuts, peanuts, pine nuts, pistachios, macadamia nuts, pecans, and almonds.
[0011] Furthermore, the morphological processing in step S1 includes one or more of the following: peeling or not peeling, whole grains or half grains, opening or punching.
[0012] Further, in step S2, the functional core material is one or more of oils, vitamins, polyphenols, flavonoids, plant extracts, medium-chain triglycerides, and amino acids; the wall material includes one or more of gum arabic, maltodextrin, β-cyclodextrin, and gelatin.
[0013] Furthermore, in step S2, the mass ratio of the functional core material to the wall material is 1:(1-10), and the solid content of the microcapsule powder is 10-40%.
[0014] Furthermore, the conditions for the electrospinning process in step S4 are: voltage 10-30kV, receiving distance 10-25cm, flow rate 0.1-2mL / h, temperature 20-35℃, and relative humidity 30-60%.
[0015] In another aspect, the present invention proposes a nut containing microcapsule powder loaded with electrospun nanofibers prepared by the above-described preparation process.
[0016] The beneficial effects of the embodiments of the present invention are as follows: (1) Improve the stability of microcapsule powder loading: With the help of the nanofiber network structure formed by electrospinning, the microcapsule powder is anchored on the surface of the nut matrix, overcoming the defects of poor adhesion, easy powder loss and uneven distribution of functional components in the traditional direct spraying process. The surface retention rate of microcapsule powder can reach 88.4%-93.0% after 18 months of storage at room temperature, effectively reducing the migration and loss of functional components.
[0017] (2) Delaying oxidative rancidity of nuts and extending shelf life: The nanofiber coating can block the intrusion of oxygen and moisture and inhibit the oxidation of unsaturated fatty acids inside the nuts. After 90 days of accelerated storage at 40℃, the peroxide value and acid value of the product still meet the qualified standards. It can be stably stored at room temperature for 18 months, which significantly solves the problem of easy spoilage of nuts. Attached Figure Description
[0018] Figure 1 This is a flowchart of the preparation process of the carrier skeleton spinning solution in Example 1 of the present invention.
[0019] Figure 2 This is a bar chart showing the peroxide value of each group in the experimental examples of this invention. Detailed Implementation
[0020] The technical solution of the present invention will be clearly and completely described below with reference to the embodiments. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.
[0021] Example 1 Nuts loaded with microcapsule powder by electrospun nanofibers S1. Raw Material Sorting: Select fresh, mold-free, and insect-free walnut kernels, remove the skin, and keep the kernels whole. Wash twice with deionized water, and dry in a 45℃ hot air drying oven until the moisture content is ≤3%, to obtain the walnut matrix for later use.
[0022] S2. Preparation of microcapsule powder: S201. Weigh 3.038g of flaxseed oil and 0.338g of vitamin E at a mass ratio of 9:1, mix them evenly, and obtain 3.375g of functional core material.
[0023] S202. Weigh 3.375g of gum arabic and 6.750g of maltodextrin at a mass ratio of 1:2, add 54.000g of deionized water, stir at 50℃ and 400r / min until completely dissolved, adjust the solid content of the system to 20%, and obtain the wall material solution.
[0024] S203. Add the functional core material to the wall material solution and emulsify it at a high speed of 8000 r / min for 5 min to obtain the primary emulsion.
[0025] S204. Homogenize the colostrum twice at 30 MPa to obtain a homogenized emulsion.
[0026] S205. The homogenized emulsion is spray-dried with an inlet air temperature of 180℃, an outlet air temperature of 80℃, a feed rate of 5-10 mL / min, and an atomization pressure of 0.3 MPa.
[0027] S206. Collect the microcapsule powder, pass it through an 80-100 mesh sieve, and store it in a sealed, light-proof, and dry place.
[0028] S3. Preparation of carrier skeleton spinning solution, the preparation process is as follows: Figure 1 As shown S301. Polysaccharide compound: Weigh 15g pullulan polysaccharide, 10g sodium alginate and 5g pectin, place them in a stirring device, stir at room temperature and low speed of 100r / min for 10min, mix thoroughly to obtain a fine polysaccharide mixture without lumps.
[0029] S302. Preparation of acidic mixed solvent: Accurately weigh food-grade glacial acetic acid, food-grade lactic acid, and deionized water according to a mass ratio of 6.0:1.4:3.7. Specifically: 540.5g glacial acetic acid, 126.1g lactic acid, and 333.4g deionized water, totaling 1000g. Add the two organic acids sequentially to the deionized water and stir at room temperature for 60 minutes to ensure the solvent system is completely homogeneous and free from stratification.
[0030] S303, Preparation of electrospinning solution: Add 30g of the above polysaccharide mixture and 60g of low-molecular-weight chitosan to 1000g of acidic mixed solvent, set the temperature to 48℃ and the stirring speed to 550r / min, and stir at a constant temperature for 6h to allow the polymer materials to fully swell and dissolve, forming a highly stable spinning solution.
[0031] S304. Preparation of electrospinning solution containing microcapsule powder: Add 13.5g of the microcapsule powder obtained in step S2 to the above spinning solution. The amount of microcapsule powder added accounts for 15% of the total mass of the polysaccharide mixture and low-molecular-weight chitosan. First, ultrasonically disperse for 15min, then stir at 550r / min for 30min to uniformly disperse the microcapsule powder, thus obtaining the electrospinning solution containing microcapsule powder.
[0032] S4. Electrospinning Loading: The walnut matrix obtained in step S1 is placed on a rotating drum receiving device at a speed of 20 r / min. The electrospinning equipment parameters are adjusted as follows: spinning voltage 22 kV, receiving distance 20 cm, original solution feed rate 1.2 mL / h, temperature 25 °C, and relative humidity 45%. All parameters fall within the range described in claim 9: voltage 10–30 kV, receiving distance 10–25 cm, flow rate 0.1–2 mL / h, temperature 20–35 °C, and relative humidity 30–60%. High-speed, stable spinning is performed for 30 min, during which the walnut matrix is turned twice to ensure uniform deposition of the spun jet on the surface of the walnut matrix, forming a dense primary nanofiber-loaded microcapsule powder coating layer.
[0033] S5, Post-processing The walnut matrix coated with nanofiber-loaded microcapsules obtained in step S4 was immersed in a 5% (w / w) food-grade sodium bicarbonate fixative for 90 min to completely neutralize the acidity of the system. It was then rinsed repeatedly with deionized water until the rinse water was neutral. The rinsed product was placed in a vacuum drying oven and dried at 45℃ and a vacuum of -0.08 MPa for 10 h to remove all moisture and residual solvent, yielding a high-strength, highly absorbent composite nanofiber-loaded microcapsule-coated walnut.
[0034] S6. Molding and Packaging: The product obtained in step S5 is packaged into aluminum foil bags, each containing 25-35g, to obtain the finished walnut product with electrospun nanofibers loaded with microcapsule powder.
[0035] Example 2 A process for preparing almonds with microcapsule powder loaded on electrospun nanofibers S1. Raw material sorting: Select fresh almond kernels, without removing the skin, keeping the kernels whole. After washing, dry at 50℃ until the moisture content is ≤3% to obtain almond matrix.
[0036] S2. Preparation of microcapsule powder: S201. Weigh 1.080g of tea polyphenols and 1.080g of grape seed extract at a mass ratio of 1:1, mix them evenly, and obtain 2.160g of functional core material.
[0037] S202. Weigh 4.320g of β-cyclodextrin and 4.320g of gelatin at a mass ratio of 1:1. First, swell the gelatin with a small amount of deionized water for 20-30 minutes, then mix it with β-cyclodextrin, add 32.400g of deionized water, and stir at 55℃ and 400r / min until completely dissolved. Adjust the solid content of the system to 25% to obtain the wall material solution.
[0038] S203. Add the functional core material to the wall material solution and emulsify it at a high speed of 8000 r / min for 5 min to obtain the primary emulsion.
[0039] S204. Homogenize the colostrum twice at 30 MPa to obtain a homogenized emulsion.
[0040] S205. The homogenized emulsion is spray-dried with an inlet air temperature of 175℃, an outlet air temperature of 80℃, a feed rate of 5-10 mL / min, and an atomization pressure of 0.3 MPa.
[0041] S206. Collect the microcapsule powder, pass it through an 80-100 mesh sieve, seal it, protect it from light, and store it in a dry place to obtain approximately 10.8g of microcapsule powder.
[0042] S3. Preparation of carrier skeleton spinning solution: S301, Polysaccharide Compound: Weigh 15g sodium alginate, 10g gellan gum, and 5g inulin, stir at low speed at room temperature for 10 minutes, mix evenly, total 30g.
[0043] S302. Preparation of acidic mixed solvent: Same as in Example 1, prepared according to glacial acetic acid: lactic acid: deionized water = 6.0:1.4:3.7, specifically 540.5g of glacial acetic acid, 126.1g of lactic acid, and 333.4g of deionized water, totaling 1000g, and stirred at room temperature for 60min until homogenized.
[0044] S303, Preparation of electrospinning solution: Add 30g of polysaccharide mixture and 60g of hyaluronic acid to 1000g of acidic mixed solvent, and stir at 48℃ and 550r / min for 6h to obtain the electrospinning solution.
[0045] S304. Preparation of electrospinning solution containing microcapsule powder: Add 10.8g of microcapsule powder obtained in step S2, accounting for 12% of the total mass of the polysaccharide mixture and hyaluronic acid. After ultrasonic dispersion for 15min, stir at 550r / min for 30min until uniformly mixed.
[0046] S4. Electrospinning load: Place the almond matrix on the receiving device. The electrospinning conditions are: voltage 22kV, receiving distance 20cm, flow rate 1.2mL / h, temperature 25℃, relative humidity 45%, and spinning time 40min.
[0047] S5. Post-treatment: Neutralize with 5% food-grade sodium bicarbonate fixative for 90 min, rinse with deionized water until neutral, and dry at 45℃ and vacuum degree -0.08MPa for 10 h.
[0048] S6. Molding and Packaging: Packaging into bags of 25-35g each to obtain almond products with electrospun nanofibers loaded with microcapsule powder.
[0049] Example 3 A process for preparing cashew nuts with microcapsule powder loaded on electrospun nanofibers S1. Raw material sorting: Select cashew kernels, remove the skin, and process in half. After washing and drying, cashew base is obtained.
[0050] S2. Preparation of microcapsule powder: S201. Weigh 1.350g of medium-chain triglyceride powder and 1.350g of vitamin D3 at a mass ratio of 1:1, mix them evenly, and obtain 2.700g of functional core material.
[0051] S202. Weigh 5.400g of gum arabic, 5.400g of maltodextrin, and 2.700g of gelatin in a mass ratio of 1:1:0.5. Add 37.800g of deionized water and stir at 50℃ and 350r / min until completely dissolved. Adjust the solid content of the system to 30% to obtain the wall material solution.
[0052] S203. Add the functional core material to the wall material solution and gently shear emulsify at 4000 r / min for 3 min to obtain the primary emulsion.
[0053] S204. Homogenize the colostrum once at 20 MPa to obtain a homogenized emulsion.
[0054] S205. Pre-freeze the homogenized emulsion to -40℃ and maintain for 4 hours, then freeze-dry it for 36-48 hours at a cold trap temperature of -55℃ and a vacuum degree of 10-20Pa until the moisture content is ≤5%.
[0055] S206. Collect the microcapsule powder, pass it through an 80-100 mesh sieve, and store it in a sealed, light-proof, and low-temperature environment.
[0056] S3. Preparation of carrier skeleton spinning solution: S301. Polysaccharide compound: Weigh 10g pullulan, 5g xanthan gum, 5g guar gum, and 10g sodium carboxymethyl cellulose, totaling 30g. Stir at low speed at room temperature for 10 minutes until homogeneous. All the above polysaccharides are selected from the range described in claim 3.
[0057] S302, Preparation of acidic mixed solvent: Same as in Example 1, 540.5g of glacial acetic acid, 126.1g of lactic acid, and 333.4g of deionized water, totaling 1000g, are stirred at room temperature for 60 minutes until homogeneous.
[0058] S303, Preparation of electrospinning solution: 30g of polysaccharide mixture and 60g of polymer (40g of low-molecular-weight chitosan and 20g of polyvinyl alcohol) were added to 1000g of acidic mixed solvent. The mixture was stirred at 48℃ and 550r / min for 6h to obtain the electrospinning solution.
[0059] S304. Preparation of electrospinning solution containing microcapsule powder: Add 16.2g of microcapsule powder obtained in step S2, accounting for 18% of the total mass of the polysaccharide mixture and polymer. After ultrasonic dispersion for 15min, stir at 550r / min for 30min until uniformly mixed.
[0060] S4. Electrospinning load: Place the cashew nut matrix on the receiving device. The electrospinning conditions are: voltage 22kV, receiving distance 20cm, flow rate 1.2mL / h, temperature 25℃, relative humidity 45%, and spinning time 45min.
[0061] S5. Post-treatment: Neutralize with 5% food-grade sodium bicarbonate fixative for 90 min, rinse with deionized water until neutral, and dry at 45℃ and vacuum degree -0.08MPa for 10 h.
[0062] S6. Molding and Packaging: Packaging, 25-35g per bag, to obtain cashew nut finished product with electrospun nanofiber loaded microcapsule powder.
[0063] Example 4 A process for preparing hazelnuts with electrospun nanofibers loaded with microcapsule powder S1. Raw material sorting: Select fresh hazelnut kernels, do not remove the skin, keep the kernels whole, wash twice with deionized water, and dry with hot air at 50℃ until the moisture content is ≤3% to obtain hazelnut matrix.
[0064] S2. Preparation of microcapsule powder: S201. Weigh 1.234g of conjugated linoleic acid and 0.309g of vitamin E at a mass ratio of 8:2, mix them evenly, and obtain 1.543g of functional core material.
[0065] S202. Weigh 4.629g of gum arabic and 4.629g of maltodextrin at a mass ratio of 1:1, add 61.200g of deionized water, stir at 50℃ and 400r / min until completely dissolved, adjust the solid content of the system to 15%, and obtain the wall material solution.
[0066] S203. Add the functional core material to the wall material solution and emulsify it at a high speed of 8000 r / min for 5 min to obtain the primary emulsion.
[0067] S204. Homogenize the colostrum twice at 30 MPa to obtain a homogenized emulsion.
[0068] S205. The homogenized emulsion is spray-dried with an inlet air temperature of 170℃, an outlet air temperature of 75℃, a feed rate of 5-10 mL / min, and an atomization pressure of 0.3 MPa.
[0069] S206. Collect the microcapsule powder, pass it through an 80-100 mesh sieve, and store it in a sealed, light-proof, and dry place.
[0070] S3. Preparation of electrospinning solution: Weigh 10g of starch, 10g of konjac glucomannan, and 10g of β-glucan, totaling 30g. Mix thoroughly at room temperature and low speed for 10min to obtain a polysaccharide mixture. Prepare 1000g of acidic mixed solvent according to the mass ratio of glacial acetic acid: lactic acid: deionized water = 6.0:1.4:3.7. Add 30g of the polysaccharide mixture and 60g of polymer (40g of low-molecular-weight chitosan and 20g of hyaluronic acid) to the solvent. Stir at 48℃ and 550r / min for 6h to obtain the electrospinning base solution. Add 10.8g of microcapsule powder obtained in step S2, accounting for 12% of the total mass of the polysaccharide mixture and polymer. Disperse ultrasonically for 15min, stir at 550r / min for 30min, and mix thoroughly.
[0071] S4. Electrospinning load: Place the hazelnut matrix on the receiving device. The electrospinning conditions are: voltage 15kV, receiving distance 12cm, flow rate 0.6mL / h, temperature 30℃, relative humidity 40%, spinning time 35min, during which the hazelnut matrix is turned over twice.
[0072] S5. Post-treatment: Neutralize with 5% food-grade sodium bicarbonate fixative for 90 min, rinse with deionized water until neutral, and dry at 45℃ and vacuum degree -0.08MPa for 10 h.
[0073] S6. Molding and Packaging: Packaging, 25-35g per bag, to obtain hazelnut finished product with electrospun nanofiber loaded microcapsule powder.
[0074] Example 5 A process for preparing open peanuts with electrospun nanofibers loaded with microcapsule powder S1. Raw material sorting: Select peanut kernels without removing the skin, open them up, wash them and dry them at 50℃ until the moisture content is ≤3% to obtain open peanut matrix.
[0075] S2. Preparation of microcapsule powder: S201. Weigh 3.000g of fish oil and 3.000g of green tea plant extract at a mass ratio of 1:1, mix them evenly, and obtain 6.000g of functional core material.
[0076] S202. Weigh 4.000g of gelatin and 8.000g of β-cyclodextrin at a mass ratio of 1:2. First, swell the gelatin with a small amount of deionized water for 20-30 minutes, then mix it with β-cyclodextrin and add 33.429g of deionized water. Stir at 55℃ and 400r / min until completely dissolved. Adjust the solid content of the system to 35% to obtain the wall material solution.
[0077] S203. Add the functional core material to the wall material solution and emulsify it at a high speed of 8000 r / min for 5 min to obtain the primary emulsion.
[0078] S204. Homogenize the colostrum twice at 30 MPa to obtain a homogenized emulsion.
[0079] S205. Pre-freeze the homogenized emulsion to -40℃ and maintain for 4 hours, then freeze-dry it for 36-48 hours at a cold trap temperature of -55℃ and a vacuum degree of 10-20Pa until the moisture content is ≤5%.
[0080] S206. Collect the microcapsule powder, pass it through an 80-100 mesh sieve, and store it in a sealed, light-proof, and low-temperature environment.
[0081] S3. Preparation of electrospinning solution: Weigh 15g pullulan, 10g sodium alginate, and 5g gellan gum, totaling 30g, and mix thoroughly to obtain a polysaccharide mixture. Prepare 1000g of acidic mixed solvent according to the mass ratio of glacial acetic acid: lactic acid: deionized water = 6.0:1.4:3.7. Add 30g of the polysaccharide mixture and 60g of polyvinyl alcohol, and stir at 48℃ and 550r / min for 6h to obtain the electrospinning base solution. Add 18g of the microcapsule powder obtained in step S2, accounting for 20% of the total mass of the polysaccharide mixture and polyvinyl alcohol, and disperse ultrasonically before stirring thoroughly.
[0082] S4. Electrospinning load: Place the open peanut matrix on the receiving device. The electrospinning conditions are: voltage 28kV, receiving distance 23cm, flow rate 1.8mL / h, temperature 22℃, relative humidity 55%, spinning time 50min, during which the peanut is turned over twice.
[0083] S5. Post-treatment: Neutralize with 5% food-grade sodium bicarbonate fixative for 90 min, rinse with deionized water until neutral, and dry at 45℃ and vacuum degree -0.08MPa for 10 h.
[0084] S6. Molding and Packaging: Packaging, 25-35g per bag, to obtain open peanut products with electrospun nanofibers loaded with microcapsule powder.
[0085] Example 6 A process for preparing pine nuts using electrospun nanofibers loaded with microcapsule powder S1. Raw material sorting: Select pine nuts, remove the skin, keep the whole kernels, wash and dry at 45℃ until the moisture content is ≤3% to obtain pine nut matrix.
[0086] S2. Preparation of microcapsule powder: S201. Weigh 0.500g of bamboo leaf flavonoids and 0.500g of tea polyphenols at a mass ratio of 1:1, mix them evenly, and obtain 1.000g of functional core material.
[0087] S202. Weigh 5.333g of maltodextrin and 2.667g of gum arabic at a mass ratio of 2:1, add 66.000g of deionized water, stir at 50℃ and 400r / min until completely dissolved, adjust the solid content of the system to 12%, and obtain the wall material solution.
[0088] S203. Add the functional core material to the wall material solution and emulsify it at a high speed of 8000 r / min for 5 min to obtain the primary emulsion.
[0089] S204. Homogenize the colostrum twice at 25 MPa to obtain a homogenized emulsion.
[0090] S205. The homogenized emulsion is spray-dried with an inlet air temperature of 175℃, an outlet air temperature of 80℃, a feed rate of 5-10 mL / min, and an atomization pressure of 0.3 MPa.
[0091] S206. Collect the microcapsule powder, pass it through an 80-100 mesh sieve, and store it in a sealed, light-proof, and dry place.
[0092] S3. Preparation of electrospinning solution: Weigh 10g of inulin, 10g of pectin, and 10g of sodium carboxymethyl cellulose, totaling 30g, and mix them evenly to obtain a polysaccharide mixture. Prepare 1000g of acidic mixed solvent according to the mass ratio of glacial acetic acid: lactic acid: deionized water = 6.0:1.4:3.7. Add 30g of the polysaccharide mixture, 30g of low-molecular-weight chitosan, and 30g of polyvinyl alcohol, and stir at 48℃ and 550r / min for 6h to obtain the electrospinning base solution. Add 9g of the microcapsule powder obtained in step S2, accounting for 10% of the total mass of the skeleton material, and disperse it ultrasonically before stirring evenly.
[0093] S4. Electrospinning load: Place the pine nut matrix on the receiving device. The electrospinning conditions are: voltage 12kV, receiving distance 10cm, flow rate 0.2mL / h, temperature 35℃, relative humidity 30%, and spinning time 20min.
[0094] S5. Post-treatment: Neutralize with 5% food-grade sodium bicarbonate fixative for 90 min, rinse with deionized water until neutral, and dry at 45℃ and vacuum degree -0.08MPa for 10 h.
[0095] S6. Molding and Packaging: Packaging, 25-35g per bag, to obtain pine nut finished product with electrospun nanofiber loaded microcapsule powder.
[0096] Example 7 A process for preparing pistachio powder loaded with electrospun nanofibers S1. Raw material sorting: Select pistachio kernels, do not remove the skin, cut half of each kernel and open it, wash and dry until the moisture content is ≤3% to obtain pistachio matrix.
[0097] S2. Preparation of microcapsule powder: S201. Weigh 1.250g of L-theanine and 1.250g of vitamin C in a mass ratio of 1:1, mix them evenly, and obtain 2.500g of functional core material.
[0098] S202. Weigh 6.250g of β-cyclodextrin and 6.250g of gelatin at a mass ratio of 1:1. First, swell the gelatin with a small amount of deionized water for 20-30 minutes, then mix it with β-cyclodextrin, add 22.500g of deionized water, and stir at 55℃ and 400r / min until completely dissolved. Adjust the solid content of the system to 40% to obtain the wall material solution.
[0099] S203. Add the functional core material to the wall material solution and emulsify it at a high speed of 8000 r / min for 5 min to obtain the primary emulsion.
[0100] S204. Homogenize the colostrum twice at 25 MPa to obtain a homogenized emulsion.
[0101] S205. The homogenized emulsion is spray-dried with an inlet air temperature of 170℃, an outlet air temperature of 75℃, a feed rate of 5-10 mL / min, and an atomization pressure of 0.3 MPa.
[0102] S206. Collect the microcapsule powder, pass it through an 80-100 mesh sieve, and store it in a sealed, light-proof, and dry place.
[0103] S3. Preparation of electrospinning solution: Weigh 10g xanthan gum, 10g guar gum, and 10g β-glucan, totaling 30g, and mix thoroughly to obtain a polysaccharide mixture. Prepare 1000g of acidic mixed solvent according to the mass ratio of glacial acetic acid: lactic acid: deionized water = 6.0:1.4:3.7. Add 30g of the polysaccharide mixture and 60g of hyaluronic acid, and stir at 48℃ and 550r / min for 6h to obtain the electrospinning base solution. Add 15g of the microcapsule powder obtained in step S2, accounting for 16.7% of the total mass of the skeleton material, and disperse ultrasonically before stirring thoroughly.
[0104] S4. Electrospinning load: Place the pistachio matrix on the receiving device. The electrospinning conditions are: voltage 25kV, receiving distance 16cm, flow rate 1.0mL / h, temperature 20℃, relative humidity 60%, and spinning time 40min.
[0105] S5. Post-treatment: Neutralize with 5% food-grade sodium bicarbonate fixative for 90 min, rinse with deionized water until neutral, and dry at 45℃ and vacuum degree -0.08MPa for 10 h.
[0106] S6. Molding and Packaging: Packaging, 25-35g per bag, to obtain pistachio finished product with microcapsule powder loaded by electrospun nanofibers.
[0107] Example 8 A process for preparing macadamia nuts with microcapsule powder loaded on electrospun nanofibers S1. Raw material sorting: Select macadamia nuts, do not remove the skin, keep the whole nuts, wash them and dry them at 50℃ until the moisture content is ≤3% to obtain macadamia nut matrix.
[0108] S2. Preparation of microcapsule powder: S201. Weigh 0.218g of medium-chain triglyceride powder and 0.436g of plant extract at a mass ratio of 1:2, mix them evenly, and obtain 0.654g of functional core material.
[0109] S202. Weigh 3.273g of gum arabic and 3.273g of gelatin at a mass ratio of 1:1. First, swell the gelatin with a small amount of deionized water for 20-30 minutes, then mix it with gum arabic and add 64.800g of deionized water. Stir at 50℃ and 350r / min until completely dissolved. Adjust the solid content of the system to 10% to obtain the wall material solution.
[0110] S203. Add the functional core material to the wall material solution and gently shear emulsify at 4000 r / min for 3 min to obtain the primary emulsion.
[0111] S204. Homogenize the colostrum once at 20 MPa to obtain a homogenized emulsion.
[0112] S205. Pre-freeze the homogenized emulsion to -40℃ and maintain for 4 hours, then freeze-dry it for 36-48 hours at a cold trap temperature of -55℃ and a vacuum degree of 10-20Pa until the moisture content is ≤5%.
[0113] S206. Collect the microcapsule powder, pass it through an 80-100 mesh sieve, and store it in a sealed, light-proof, and low-temperature environment.
[0114] S3. Preparation of electrospinning solution: Weigh 10g of konjac glucomannan, 10g of sodium alginate, and 10g of starch, totaling 30g, and mix them evenly to obtain a polysaccharide mixture. Prepare 1000g of acidic mixed solvent according to the mass ratio of glacial acetic acid: lactic acid: deionized water = 6.0:1.4:3.7. Add 30g of the polysaccharide mixture and 60g of low-molecular-weight chitosan, and stir at 48℃ and 550r / min for 6h to obtain the electrospinning base solution. Add 7.2g of the microcapsule powder obtained in step S2, accounting for 8% of the total mass of the skeleton material, and disperse it ultrasonically before stirring evenly.
[0115] S4. Electrospinning load: Place the macadamia nut matrix on the receiving device. The electrospinning conditions are: voltage 30kV, receiving distance 25cm, flow rate 2.0mL / h, temperature 28℃, relative humidity 50%, and spinning time 60min.
[0116] S5. Post-treatment: Neutralize with 5% food-grade sodium bicarbonate fixative for 90 min, rinse with deionized water until neutral, and dry at 45℃ and vacuum degree -0.08MPa for 10 h.
[0117] S6. Molding and Packaging: Packaging, 25-35g per bag, to obtain the finished macadamia nut product with microcapsule powder loaded by electrospun nanofibers.
[0118] Example 9 A process for preparing pecan fruit microcapsule powder loaded with electrospun nanofibers S1. Raw material sorting: Select pecan kernels, do not remove the skin, make holes, wash and dry to a moisture content of ≤3% to obtain pecan matrix.
[0119] S2. Preparation of microcapsule powder: S201. Weigh 4.500g of walnut oil and 4.500g of soy isoflavones in a 1:1 mass ratio, mix them evenly, and obtain 9.000g of functional core material.
[0120] S202. Weigh 4.500g of maltodextrin and 4.500g of β-cyclodextrin at a mass ratio of 1:1, add 46.286g of deionized water, stir at 50℃ and 400r / min until completely dissolved, adjust the solid content of the system to 28%, and obtain the wall material solution.
[0121] S203. Add the functional core material to the wall material solution and emulsify it at a high speed of 8000 r / min for 5 min to obtain the primary emulsion.
[0122] S204. Homogenize the colostrum twice at 30 MPa to obtain a homogenized emulsion.
[0123] S205. The homogenized emulsion is spray-dried with an inlet air temperature of 180℃, an outlet air temperature of 80℃, a feed rate of 5-10 mL / min, and an atomization pressure of 0.3 MPa.
[0124] S206. Collect the microcapsule powder, pass it through an 80-100 mesh sieve, and store it in a sealed, light-proof, and dry place.
[0125] S3. Preparation of electrospinning solution: Weigh 10g pullulan, 10g gellan gum, and 10g inulin, totaling 30g, and mix thoroughly to obtain a polysaccharide mixture. Prepare 1000g of acidic mixed solvent according to the mass ratio of glacial acetic acid: lactic acid: deionized water = 6.0:1.4:3.7. Add 30g of the polysaccharide mixture, 30g of polyvinyl alcohol, and 30g of hyaluronic acid, and stir at 48℃ and 550r / min for 6h to obtain the electrospinning base solution. Add 18g of the microcapsule powder obtained in step S2, accounting for 20% of the total mass of the skeleton material, and disperse ultrasonically before stirring thoroughly.
[0126] S4. Electrospinning load: The pecan matrix is placed on the receiving device. The electrospinning conditions are: voltage 20kV, receiving distance 18cm, flow rate 0.9mL / h, temperature 32℃, relative humidity 45%, and spinning time 45min.
[0127] S5. Post-treatment: Neutralize with 5% food-grade sodium bicarbonate fixative for 90 min, rinse with deionized water until neutral, and dry at 45℃ and vacuum degree -0.08MPa for 10 h.
[0128] S6. Molding and Packaging: Packaging, 25-35g per bag, to obtain the finished pecan product with electrospun nanofibers loaded with microcapsule powder.
[0129] Example 10 A process for preparing almonds with microcapsule powder loaded on electrospun nanofibers S1. Raw material sorting: Select almonds, remove skin, process in half, wash and dry at 45℃ until moisture content is ≤3% to obtain almond matrix.
[0130] S2. Preparation of microcapsule powder: S201. Weigh out 0.500g of vitamin E, 0.500g of tea polyphenols, and 0.500g of L-tryptophan in a mass ratio of 1:1:1, mix them evenly, and obtain 1.500g of functional core material.
[0131] S202. Weigh 5.250g of gelatin and 5.250g of gum arabic at a mass ratio of 1:1. First, swell the gelatin with a small amount of deionized water for 20-30 minutes, then mix it with the gum arabic and add 42.545g of deionized water. Stir at 50℃ and 400r / min until completely dissolved. Adjust the solid content of the system to 22% to obtain the wall material solution.
[0132] S203. Add the functional core material to the wall material solution and emulsify it at a high speed of 8000 r / min for 5 min to obtain the primary emulsion.
[0133] S204. Homogenize the colostrum twice at 30 MPa to obtain a homogenized emulsion.
[0134] S205. The homogenized emulsion is spray-dried with an inlet air temperature of 170℃, an outlet air temperature of 75℃, a feed rate of 5-10 mL / min, and an atomization pressure of 0.3 MPa.
[0135] S206. Collect the microcapsule powder, pass it through an 80-100 mesh sieve, and store it in a sealed, light-proof, and dry place.
[0136] S3. Preparation of electrospinning solution: Weigh 10g of sodium carboxymethyl cellulose, 10g of xanthan gum, and 10g of pectin, totaling 30g, and mix them evenly to obtain a polysaccharide mixture. Prepare 1000g of acidic mixed solvent according to the mass ratio of glacial acetic acid: lactic acid: deionized water = 6.0:1.4:3.7. Add 30g of the polysaccharide mixture, 20g of low-molecular-weight chitosan, 20g of hyaluronic acid, and 20g of polyvinyl alcohol. Stir at 48℃ and 550r / min for 6h to obtain the electrospinning base solution. Add 12g of the microcapsule powder obtained in step S2, accounting for 13.3% of the total mass of the skeleton material. Disperse by ultrasonication and stir evenly.
[0137] S4. Electrospinning load: Place the almond matrix on the receiving device. The electrospinning conditions are: voltage 16kV, receiving distance 14cm, flow rate 0.4mL / h, temperature 26℃, relative humidity 38%, and spinning time 30min.
[0138] S5. Post-treatment: Neutralize with 5% food-grade sodium bicarbonate fixative for 90 min, rinse with deionized water until neutral, and dry at 45℃ and vacuum degree -0.08MPa for 10 h.
[0139] S6. Molding and Packaging: Packaging, 25-35g per bag, to obtain almond finished product with microcapsule powder loaded by electrospun nanofibers.
[0140] Comparative Example 1 A walnut preparation process using direct spraying of microcapsule powder S1. Raw material sorting: Same as in Example 1, to obtain walnut matrix.
[0141] S2. Preparation of microencapsulated powder: Same as in Example 1, to obtain microencapsulated powder.
[0142] S3. Preparation of spraying liquid: Add the microcapsule powder obtained in Example 1 to deionized water to prepare a microcapsule powder suspension with a mass concentration of 10%, add 0.5% sodium carboxymethyl cellulose as a thickener, and stir evenly.
[0143] S4. Spraying Load: Place the walnut substrate obtained in step S1 into a spraying device and spray the suspension obtained in step S3 evenly. The amount of spraying should be enough to completely wet the surface of the walnut. After spraying, dry with hot air at 45℃ until the moisture content is ≤3%.
[0144] S5. Post-treatment: No fixative neutralization is performed; the product is directly vacuum dried at 45°C for 10 hours.
[0145] S6. Shaping and Packaging: Packaging to obtain walnut products with direct microcapsule powder coating.
[0146] The difference from Example 1: Electrospun nanofibers were not used for loading, and the microcapsule powder adhered to the walnut surface only by a thickener.
[0147] Comparative Example 2 A process for preparing walnuts coated only with electrospun nanofibers S1. Raw material sorting: Same as in Example 1, to obtain walnut matrix.
[0148] S2. Microcapsule powder preparation: Same as in Example 1, obtain microcapsule powder for later use, but do not add spinning solution subsequently.
[0149] S3. Preparation of electrospinning solution: Same as in Example 1, but without adding microcapsule powder, only prepare carrier skeleton spinning solution.
[0150] S4. Electrospinning loading: The walnut matrix is placed on the receiving device, and the same electrospinning conditions as in Example 1 are used to deposit pure nanofibers on the surface of the walnut matrix.
[0151] S5. Post-processing: Same as in Example 1.
[0152] S6. Shaping and Packaging: Packaging to obtain walnut products with only the surface coated with nanofibers.
[0153] The difference from Example 1: The electrospinning solution does not contain microcapsule powder and has no functional component loading on the surface.
[0154] Comparative Example 3 A process for preparing walnuts by electrospinning using only polysaccharides as carriers S1. Raw material sorting: Same as in Example 1.
[0155] S2. Preparation of microcapsule powder: Same as in Example 1.
[0156] S3. Preparation of electrospinning solution: Weigh 15g pullulan, 10g sodium alginate, and 5g pectin, totaling 30g, and dissolve them in 1000g of acidic mixed solvent. Do not add low-molecular-weight chitosan. Stir at 48℃ and 550r / min for 6h, then add 13.5g of microcapsule powder and disperse evenly.
[0157] S4, Electrospinning load: Same as in Example 1.
[0158] S5. Post-processing: Same as in Example 1.
[0159] S6. Shaping and Packaging: Packaging to obtain electrospun walnut products with polysaccharides as the carrier.
[0160] The difference from Example 1: The carrier skeleton material contains only a mixture of polysaccharides and no polymers.
[0161] Test case S1. Accelerated Storage Test: Test conditions: 40℃±1℃, relative humidity 75%±5%, protected from light, sealed in aluminum foil bags. Samples were taken at 0, 15, 30, 45, 60, and 90 days. Shelf life endpoint determination: peroxide value ≤20 meq / kg, acid value ≤1.5 mg KOH / g, sensory score ≥6.0. Results are shown in Table 1.
[0162] S2, 18-month test at room temperature, results are shown in Table 2. The peroxide value bar charts for each group are shown below. Figure 2 As shown.
[0163] Table 1 Results of accelerated storage at 40℃ for 90 days
[0164] Table 2 Results after 18 months at 25℃ and 60% relative humidity.
[0165] S3. Results: As shown in Table 1, all examples still met the shelf-life endpoint requirements after 90 days of accelerated treatment at 40℃; the blank group and comparative examples 1-3 were all unqualified. As shown in Table 2, the sensory scores of all examples were greater than 6 points after 18 months at 25℃ and 60% relative humidity, and the peroxide value, acid value, and microcapsule powder surface retention rate were all qualified.
[0166] In summary, this invention utilizes a nanofiber network constructed by electrospinning to firmly anchor microencapsulated powder onto the surface of nuts without altering the original microencapsulated powder preparation process, thus preserving the original flavor and crisp texture of the nuts. It not only enhances the nutritional functions of nuts but also effectively inhibits the oxidative rancidity of nut oils, significantly extending the product's shelf life. It is suitable for the functional processing of various nuts such as walnuts, almonds, cashews, and hazelnuts, and has promising prospects for industrial application in the food industry.
[0167] Although embodiments of the present invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and variations can be made to these embodiments without departing from the principles and spirit of the present invention. All equivalent changes and improvements made within the scope of the present invention should still fall within the patent coverage of the present invention.
Claims
1. A process for preparing nuts using electrospun nanofibers loaded with microcapsule powder, characterized in that, Includes the following steps: S1. Raw material sorting: Select nut raw materials, and after washing, drying and morphological processing, obtain nut matrix; S2. Preparation of microencapsulated powder: The functional core material and wall material are emulsified, homogenized and dried to obtain microencapsulated powder; S3. Preparation of electrospinning solution: Dissolve the carrier skeleton material in an acidic mixed solvent and stir to obtain an electrospinning base solution; S4. Electrospinning loading: Add the microcapsule powder obtained in step S2 to the electrospinning base liquid obtained in step S3, stir or ultrasonically disperse evenly to obtain an electrospinning liquid containing microcapsule powder; place the nut matrix obtained in step S1 on a receiving device, and use electrospinning process to deposit the spinning jet on the surface of the nut matrix to obtain a nut with nanofiber loaded microcapsule powder on the surface. S5. Post-processing: The product obtained in step S4 is neutralized with a fixing solution, rinsed and dried. S6. Molding and Packaging: The product obtained in step S5 is packaged to obtain the finished nut product with electrospun nanofiber loaded microcapsule powder.
2. The preparation process according to claim 1, characterized in that, The carrier skeleton material in step S3 is composed of a polysaccharide mixture and a polymer.
3. The preparation process according to claim 2, characterized in that, The polysaccharide mixture is selected from one or more of pullulan, sodium alginate, starch, pectin, gellan gum, inulin, konjac glucomannan, xanthan gum, guar gum, sodium carboxymethyl cellulose, and β-glucan.
4. The preparation process according to claim 2, characterized in that, The polymer is selected from one or more of chitosan, hyaluronic acid, and polyvinyl alcohol.
5. The preparation process according to claim 1, characterized in that, The nut ingredients in step S1 include any one of the following: walnuts, almonds, cashews, hazelnuts, peanuts, pine nuts, pistachios, macadamia nuts, pecans, and almonds.
6. The preparation process according to claim 1, characterized in that, The morphological processing in step S1 includes one or more of the following: peeling or not peeling, whole grains or half grains, opening or punching.
7. The preparation process according to claim 1, characterized in that, In step S2, the functional core material is one or more of the following: oils, vitamins, polyphenols, flavonoids, plant extracts, medium-chain triglycerides, and amino acids; the wall material includes one or more of the following: gum arabic, maltodextrin, β-cyclodextrin, and gelatin.
8. The preparation process according to claim 1, characterized in that, In step S2, the mass ratio of the functional core material to the wall material is 1:(1-10), and the solid content of the microcapsule powder is 10-40%.
9. The preparation process according to claim 1, characterized in that, The conditions for the electrospinning process in step S4 are: voltage 10-30kV, receiving distance 10-25cm, flow rate 0.1-2mL / h, temperature 20-35℃, and relative humidity 30-60%.
10. A nut containing electrospun nanofibers loaded with microcapsule powder prepared by any one of the preparation processes described in any one of claims 1 to 9.
Citation Information
Patent Citations
Preparation technology of sacha inchi nut
CN109123562A
Degreased nut, preparation method thereof and degreased nut food
CN118830612A