A manufacturing process of a variable thickness scroll spring

By welding and grinding a segmented variable thickness structure onto a steel strip, the problems of torque mismatch and stress concentration of the coil spring on the variable thickness strip are solved, thereby improving the adaptability and safety of the coil spring.

CN123060385APending Publication Date: 2026-11-10HENAN JIANGHUA MEASURE TOOLS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611377294.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-07
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

When existing constant-thickness coil springs are used on variable-thickness tapes, problems such as improper torque matching, stress concentration, and winding jamming occur, resulting in unstable tape rebound speed, unsmooth feel, and inability to adapt to spatial changes.

Method used

A segmented variable thickness structure is formed on the steel strip using welding and grinding processes, including a welded thickening section, a ground thinning section, and a thickness transition section, to ensure torque matching and uniform stress distribution. The gradual transition is achieved through CNC grinding and pulse precision spot welding.

Benefits of technology

It achieves adaptive matching of spring torque with variable thickness tape, avoids stress concentration, improves safety and smoothness of use, reduces production costs and adapts to tapes of different specifications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123060385A_ABST
    Figure CN123060385A_ABST
Patent Text Reader

Abstract

The present application relates to the technical field of steel tape accessory processing, and provides a manufacturing process of a variable-thickness spiral spring, which takes a spring steel strip with equal thickness as a base material, forms a thickened section by welding spring steel sheets at a movable traction end area, and / or forms a thinned section by grinding at a fixed end area, and forms a thickness transition section by gradual grinding between different thickness sections, and finally winds and forms a variable-thickness spiral spring with segmented variable thickness. The segmented variable-thickness structure makes the spring torque self-adaptively match the thickness change law of a variable-thickness tape, and the winding is smooth, the rebound speed is slowed down, and there is no stress concentration. The present application adopts the welding thickening and grinding thinning process, has low processing difficulty, high yield, and low cost, and is suitable for batch industrial production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of steel tape measure accessory processing technology, and more specifically, to a manufacturing process for a variable thickness spiral spring. Background Technology

[0002] Standard measuring tape springs are made of steel strips of uniform thickness and cross-section. The springs themselves have consistent stiffness along the length direction, making them suitable for standard measuring tapes of uniform thickness.

[0003] The variable thickness measuring tapes currently available on the market have a thicker and more rigid front end (the protruding end) to ensure they do not bend during suspended measurements; the tape tail (the inside of the measuring tape casing) is thinner to reduce the minimum winding radius and decrease the volume of the measuring tape casing.

[0004] The application of existing constant-thickness coil springs to variable-thickness tapes has obvious drawbacks:

[0005] 1. When the measuring tape extends too far, the thin section of the measuring tape is pulled back by the coil spring. If the initial torque of the coil spring is too large, the measuring tape will rebound too quickly and may injure the user's hand. When the thick section of the measuring tape enters the housing, the remaining torque of the coil spring is insufficient, which may cause the measuring tape to fail to retract properly or become stuck.

[0006] 2. Variations in the thickness of the tape result in uneven outer diameters when the tape is coiled and stacked. This leads to uneven stress distribution on the springs with uniform stiffness. Over time, repeated expansion and contraction can cause localized stress concentration in the springs, resulting in fatigue fracture.

[0007] 3. When the tape measure with varying thickness is wound up, the radial space occupied changes dynamically. The coil spring with uniform thickness cannot adapt to the changes in space, which can easily cause friction and jamming between the tape measure and the coil spring, affecting the feel of pulling the tape measure.

[0008] Therefore, there is an urgent need to design a special measuring tape spring and its manufacturing process that can match the characteristics of tapes with varying thicknesses, and to solve problems such as torque matching, stress concentration, and winding jamming. Summary of the Invention

[0009] To overcome the shortcomings mentioned above, this invention aims to provide a manufacturing process for a variable thickness spiral spring, which can solve the aforementioned problems.

[0010] A manufacturing process for a variable thickness spiral spring includes the following steps:

[0011] A spring steel strip of uniform thickness is provided as the base material, wherein the thickness of the base material is 0.10-0.13 mm or 0.15-0.18 mm;

[0012] A movable traction end region and a fixed end region are defined on the substrate;

[0013] In the active traction end region, a welded thickened section is formed by locally thickening the substrate surface by welding a thin spring steel sheet; and / or in the fixed end region, a ground thinned section is formed by grinding and thinning the end of the substrate.

[0014] Between the welded thickening section and the original thickness section of the substrate, and / or between the grinding thinning section and the original thickness section of the substrate, a thickness transition section is formed by gradual grinding to make the thickness of the coil spring transition smoothly.

[0015] A steel strip that has undergone thickness treatment is wound into a spiral spring with a segmented variable thickness structure along its length. The segmented variable thickness structure enables the spring torque to adaptively match the thickness variation of the matching variable thickness strip.

[0016] Furthermore, the processing of the welded thickened section includes:

[0017] Select spring steel sheets with a thickness of 0.02–0.04 mm;

[0018] The spring steel sheet is symmetrically attached to the upper and lower surfaces of the active traction end of the substrate;

[0019] Welding is performed using pulse precision spot welding technology, resulting in uniformly distributed weld spots with a spacing of 1–3 mm between them.

[0020] After welding, the entire welding area is finely ground and leveled to remove weld beads and burrs, so that the thickness of the thickened section reaches 0.15 to 0.18 mm.

[0021] Furthermore, the grinding and cutting of thin segments includes:

[0022] The fixed end of the substrate is subjected to double-sided uniform fine grinding to reduce its thickness. The grinding length is set according to the matching variable thickness tape, and the grinding length is equivalent to the thin section length of the matching variable thickness tape.

[0023] After grinding, the thickness of the fixed end is uniformly reduced to 0.11–0.13 mm;

[0024] The ground surface is smooth and flat, without local depressions or cracks.

[0025] Furthermore, the processing of the thickness transition section includes:

[0026] Gradual grinding is performed between the welded thickening section and the original thickness section of the substrate, or between the grinding thinning section and the original thickness section of the substrate, so that the thickness decreases uniformly without abrupt steps.

[0027] The gradual grinding process uses a CNC grinding machine or a grinding wheel machine with a contour template to control the feed rate of the grinding wheel to gradually change along the length of the steel strip, so that the thickness decreases uniformly.

[0028] Furthermore, when welding thickening and grinding thinning are used simultaneously, the movable traction end is welded thickened to 0.15-0.18 mm, the fixed end is ground thinned to 0.11-0.13 mm, the middle section retains the original thickness of the substrate and transitions smoothly, forming a gradient structure that is thick at the beginning and thin at the end;

[0029] The length of the welded thickening section is not less than the effective working length of the thick section of the matching variable thickness ruler belt, and the length of the grinding and thinning section is equivalent to the length of the thin section of the matching variable thickness ruler belt.

[0030] Furthermore, the overall width of the coil spring remains consistent, and the thickness is only changed by welding or grinding, resulting in a final coil spring thickness range of 0.10mm to 0.20mm.

[0031] Furthermore, it also includes surface treatment steps:

[0032] The completed coil springs are then subjected to a bluing and rust-preventing treatment.

[0033] Apply anti-corrosion and wear-resistant coatings to the welding and grinding areas for sealing and corrosion protection.

[0034] Compared with the prior art, the beneficial effects of the present invention are:

[0035] ① In this invention, the traditional high-difficulty integral gradient stamping process is abandoned, and welding and grinding modification processes are adopted. The equipment requirements are low, the processing error tolerance is high, the problem of integral stamping cracks and uneven thickness is solved, the production cost is greatly reduced, it is suitable for mass production, the process is simple, the mass production capability is strong, and the yield rate is high.

[0036] ② In this invention, the front welded thickened section provides sufficient retraction torque to ensure that the thick tape does not loosen when extended and retracts forcefully; the rear ground and thinned section reduces the residual torque at the end of the recovery, slows down the tape rebound speed, avoids high-speed rebound from injuring people, and makes the tape measure have uniform damping and a smooth feel throughout the entire pulling process.

[0037] ③ In this invention, the thickened section, transition section and thinned section are smoothly connected without abrupt changes in thickness or sharp corners in the structure, which avoids stress concentration caused by long-term reciprocating expansion and contraction, stabilizes the structure, reduces the probability of fatigue fracture of the coil spring, and extends the service life of the spring.

[0038] ④ In this invention, the welding thickness can be flexibly adjusted or the grinding and thinning length can be adjusted according to different specifications of variable thickness strips, without the need to change the mold, and the adaptability is stronger than that of traditional one-piece molded gradient coil springs.

[0039] ⑤ In this invention, the surface is flat after welding and ground, and the surface is smooth and burr-free after grinding. The coil spring will not rub or jam against the tape or the housing when it is wound up. Combined with the anti-corrosion coating, it is suitable for harsh working conditions such as humid and dusty construction sites. Attached Figure Description

[0040] The accompanying drawings are provided to further illustrate the invention and form part of the specification. They are used in conjunction with embodiments of the invention to explain the invention and do not constitute a limitation thereof. In the drawings:

[0041] Figure 1 This is a schematic diagram of the process flow for this technology;

[0042] Figure 2 This is a schematic diagram of a variable thickness coil spring.

[0043] In the diagram: 1. Thickened section; 2. Transition section; 3. Thinned section. Detailed Implementation

[0044] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0045] The following three embodiments correspond to three implementation methods: welding-only thickening, grinding-only thinning, and composite processes. It should be understood that these three methods all belong to the same inventive concept of this invention, all using a spring steel strip of uniform thickness as the base material, forming a segmented variable thickness structure through local thickening or thinning, and setting thickness transition sections to ultimately achieve a match between the coil spring torque and the thickness variation law of the variable thickness strip. The embodiments can be referenced interchangeably, and the relevant process parameters can be adjusted according to actual needs. Specific Implementation

[0046] Example 1: Manufacturing process of welded thickened variable thickness spiral spring:

[0047] In this embodiment, standard uniform-thickness spring steel strip is used as the base material for the coil spring, with a base material thickness of 0.10–0.13 mm. First, the area of ​​the movable traction end is determined on the base material. At the movable traction end of the coil spring body, thin spring steel sheets with a thickness of 0.02–0.04 mm are symmetrically welded to the upper and lower surfaces of the base material using a pulse precision spot welding process. The weld spots are evenly distributed with a spacing of 1–3 mm. After welding, the welded area is finely ground and leveled to remove weld beads and burrs, increasing the overall thickness of the traction end to 0.15–0.18 mm, forming a high-torque welded thickened section. The length of the welded thickened section is not less than the effective working length of the matching variable-thickness strip section.

[0048] Then, the middle section of the coil spring is subjected to gradual grinding, so that the thickness gradually decreases from 0.18mm to 0.11mm, serving as a thickness transition section. The length of the transition section is determined based on the thickness difference and the working curvature of the coil spring, generally 50 to 200 times the thickness difference. Gradual grinding is performed using a CNC surface grinder or a grinding wheel machine with a contour template. The feed rate of the grinding wheel (CBN grinding wheel) is gradually changed along the length of the steel strip to ensure a uniform decrease in thickness and a smooth transition without abrupt steps. The fixed end of the coil spring is not welded, preserving the original structure of the base material.

[0049] After the thickness treatment is completed, the steel strip is wound into shape along the predetermined spiral direction to form a spiral spring.

[0050] The final product is a variable-thickness spiral spring with an increased active traction end and a fixed end that retains the original thickness of the base material. During assembly and use, the thickened section of the spiral spring is welded to the thicker section of the strain gauge. When the gauge extends significantly, the thickened section of the spring provides sufficient pull-back force to ensure that the gauge remains straight and stable during retraction. The middle transition section is adapted to the transition area between the thick and thin sections of the gauge, ensuring uniform force distribution without jamming.

[0051] Example 2: Manufacturing process of variable thickness spiral spring by grinding and thinning:

[0052] In this embodiment, a standard spring steel strip with a thickness of 0.15–0.18 mm is used as the base material. The fixed end of the coil spring body is uniformly thinned by precision grinding. The grinding length is equivalent to the length of the thin section of the matching variable thickness gauge strip. After grinding, the thickness of the fixed end is uniformly reduced to 0.11–0.13 mm, and the ground surface is smooth and flat, without local depressions or cracks. The grinding is carried out using a double-sided synchronous precision grinding machine, with the upper and lower grinding heads feeding synchronously. Coolant is used during the grinding process to prevent the steel strip from overheating and deforming. After grinding, a micrometer is used to check the thickness uniformity to ensure that the thickness tolerance is within ±0.005 mm.

[0053] The active traction end of the coil spring retains the original base material thickness, serving as a high-torque working section, with a natural and smooth transition in the middle section and no abrupt changes in thickness.

[0054] After the thickness treatment is completed, the steel strip is wound into shape along the predetermined spiral direction to form a spiral spring.

[0055] During use, when the tape is fully withdrawn and the thin section of the tape enters the housing, the working torque of the spring grinding section is greatly reduced, effectively slowing down the tape's retraction speed, preventing the tape from hitting the housing and injuring the user, and greatly improving safety.

[0056] Example 3: Manufacturing process of variable thickness spiral spring by welding thickening + grinding and thinning composite molding:

[0057] This embodiment combines the two processes described above. First, at the movable traction end of the coil spring, a double-sided welded spring steel sheet is used to thicken the section to 0.15–0.18 mm, forming a traction thickened section. The length of the welded thickened section is not less than the effective working length of the matching variable thickness tape thickened section. Then, at the fixed end of the coil spring, a double-sided fine grinding process is used to thin the section to 0.11–0.13 mm, forming a buffer thinning section. The length of the ground thinning section is equivalent to the length of the matching variable thickness tape thinned section. The middle section retains the original thickness of the base material and transitions smoothly, forming a gradual structure that is thicker at the beginning and thinner at the end. The length of the thickness transition section is determined according to the thickness difference and the working curvature of the coil spring, matching the structural characteristics of the variable thickness tape, which is thicker at the beginning and thinner at the end.

[0058] After the thickness treatment is completed, the steel strip is wound into shape along the predetermined spiral direction to form a spiral spring.

[0059] After processing, the entire coil of spring is bluing for rust prevention. The welded and ground areas are specifically coated with an anti-corrosion and wear-resistant coating to prevent rust and wear in the processed areas. This composite process results in excellent torque matching, a smooth pulling feel without jamming or rapid rebound, and compatibility with most variable thickness tape measuring tapes.

[0060] Finally, it should be noted that the above descriptions are merely preferred embodiments of the present invention and are not intended to limit the present invention. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art can still modify the technical solutions described in the foregoing embodiments or make equivalent substitutions for some of the technical features. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.

Claims

1. A manufacturing process for a variable thickness spiral spring, characterized in that, Includes the following steps: A spring steel strip of uniform thickness is provided as the base material, wherein the thickness of the base material is 0.10-0.13 mm or 0.15-0.18 mm; A movable traction end region and a fixed end region are defined on the substrate; In the active traction end region, a welded thickened section is formed by locally thickening the substrate surface by welding a thin spring steel sheet; and / or in the fixed end region, a ground thinned section is formed by grinding and thinning the end of the substrate. Between the welded thickening section and the original thickness section of the substrate, and / or between the grinding thinning section and the original thickness section of the substrate, a thickness transition section is formed by gradual grinding to make the thickness of the coil spring transition smoothly. A steel strip that has undergone thickness treatment is wound into a spiral spring with a segmented variable thickness structure along its length. The segmented variable thickness structure enables the spring torque to adaptively match the thickness variation of the matching variable thickness strip.

2. The manufacturing process of a variable thickness spiral spring according to claim 1, characterized in that, The processing of the welded thickened section includes: Select spring steel sheets with a thickness of 0.02–0.04 mm; The spring steel sheet is symmetrically attached to the upper and lower surfaces of the active traction end of the substrate; Welding is performed using pulse precision spot welding technology, resulting in uniformly distributed weld spots with a spacing of 1–3 mm between them. After welding, the entire welding area is finely ground and leveled to remove weld beads and burrs, so that the thickness of the thickened section reaches 0.15 to 0.18 mm.

3. The manufacturing process of a variable thickness spiral spring according to claim 1, characterized in that, The grinding and thinning process includes: The fixed end of the substrate is subjected to double-sided uniform fine grinding to reduce its thickness. The grinding length is set according to the matching variable thickness tape, and the grinding length is equivalent to the thin section length of the matching variable thickness tape. After grinding, the thickness of the fixed end is uniformly reduced to 0.11–0.13 mm; The ground surface is smooth and flat, without local depressions or cracks.

4. The manufacturing process of a variable thickness spiral spring according to claim 1, characterized in that, The processing of the thickness transition section includes: Gradual grinding is performed between the welded thickening section and the original thickness section of the substrate, or between the grinding thinning section and the original thickness section of the substrate, so that the thickness decreases uniformly without abrupt steps. The gradual grinding process uses a CNC grinding machine or a grinding wheel machine with a contour template to control the feed rate of the grinding wheel to gradually change along the length of the steel strip, so that the thickness decreases uniformly.

5. The manufacturing process of a variable thickness spiral spring according to claim 1, characterized in that, When welding thickening and grinding thinning are used simultaneously, the movable traction end is welded thickened to 0.15-0.18 mm, the fixed end is ground thinned to 0.11-0.13 mm, the middle section retains the original thickness of the substrate and transitions smoothly, forming a gradient structure that is thick at the beginning and thin at the end. The length of the welded thickening section is not less than the effective working length of the thick section of the matching variable thickness ruler belt, and the length of the grinding and thinning section is equivalent to the length of the thin section of the matching variable thickness ruler belt.

6. The manufacturing process of a variable thickness spiral spring according to claim 1, characterized in that, The overall width of the coil spring remains consistent, and the thickness is only changed by welding or grinding, resulting in a final coil spring thickness range of 0.10mm to 0.20mm.

7. The manufacturing process of a variable thickness spiral spring according to claim 1, characterized in that, It also includes surface treatment steps: The completed coil springs are then subjected to a bluing and rust-preventing treatment. Apply anti-corrosion and wear-resistant coatings to the welding and grinding areas for sealing and corrosion protection.