A monitoring method and device for high-temperature life testing of lead-acid batteries
By using non-contact displacement sensors and real surface temperature monitoring, combined with internal resistance measurement, an electromechanical coupling damage index is constructed, which solves the problem of inaccurate temperature and internal resistance measurements in high-temperature life testing of lead-acid batteries, and achieves early warning and improved safety.
Patent Information
- Application Number
- CN202611321991.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-28
- Publication Date
- 2026-11-10
AI Technical Summary
Existing high-temperature life testing methods for lead-acid batteries suffer from problems such as inaccurate surface temperature measurement, susceptibility to interference in AC internal resistance measurement, and a lack of comprehensive evaluation models, resulting in the inability to provide early warnings and posing safety hazards.
A non-contact displacement sensor is used to monitor the deformation of the battery casing. Combined with the actual surface temperature and internal resistance measurement, an electromechanical coupling damage index is constructed, and early warning is achieved through a comprehensive hazard warning value.
It enables accurate assessment of battery health status during high-temperature life testing, avoiding safety accidents such as damage to testing equipment and fires, and improving testing safety and reliability.
Smart Images

Figure CN123066596A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of battery testing, and in particular relates to a monitoring method and monitoring device for high-temperature life testing of lead-acid batteries. Background Technology
[0002] Lead-acid batteries remain important in backup power, energy storage systems, and some power transmission applications due to their high safety, low cost, and wide temperature adaptability. High-temperature life testing is an essential verification step to assess the reliability of lead-acid batteries under extreme operating conditions. However, during long-term charge-discharge cycles at high temperatures, side reactions inevitably occur inside the battery, such as grid corrosion, active material shedding, and gas evolution and water loss. These side reactions are often accompanied by mechanical expansion (bulging) of the battery casing and intense heat generation.
[0003] Existing methods for monitoring the high-temperature life of lead-acid batteries often have the following drawbacks:
[0004] First, traditional surface temperature measurement usually involves directly attaching thermocouples or temperature probes to the surface of the battery casing. When the battery bulges outward, the pre-tight fit between the probe and the casing is disrupted, and the contact thermal resistance undergoes a drastic and nonlinear dynamic change, resulting in serious hysteresis and distortion in the measured apparent temperature.
[0005] Secondly, AC internal resistance is an important parameter characterizing the health status of a battery. However, in high-temperature testing, the measured internal resistance value is easily affected by the additional resistance of the measurement circuit and the cross interference of the real-time temperature fluctuations. Traditional methods are difficult to dynamically strip and normalize it to the reference temperature, resulting in inaccurate electrochemical degradation assessment.
[0006] Finally, existing monitoring methods usually treat temperature, internal resistance, or external deformation in isolation, lacking a comprehensive evaluation model that deeply couples thermodynamic acceleration effects, electrochemical internal resistance evolution, and shell mechanical deformation energy. When the battery is close to the edge of thermal runaway, it often has to rely on a single temperature hard threshold for post-event disconnection, which cannot achieve early warning and is very likely to cause damage to test equipment or even serious safety accidents such as fires. Summary of the Invention
[0007] To address the shortcomings of existing technologies, this invention provides a monitoring method and device for high-temperature life testing of lead-acid batteries, thus solving the aforementioned problems.
[0008] To achieve the above objectives, the present invention provides the following technical solution: a monitoring method for high-temperature life testing of lead-acid batteries, comprising:
[0009] S10. Obtain the apparent measurement temperature of the temperature probe, the real-time signed normal displacement of the battery casing of the non-contact displacement sensor, and the ambient temperature, compensate for probe contact and thermal errors, and obtain the true surface temperature.
[0010] S20. Under the preset state of charge, resting time and AC excitation, obtain the apparent AC internal resistance, remove the additional resistance of the measurement circuit and convert it to the calibrated reference temperature in combination with the real surface temperature to obtain the reference working condition equivalent internal resistance.
[0011] S30. Calculate the electrochemical degradation component based on the change of equivalent internal resistance, extract the positive displacement to obtain the positive outward bulging displacement, combine the temperature-corrected stiffness to calculate the shell's equivalent deformation energy and mechanical degradation component, couple the two to obtain the instantaneous damage state quantity, and update it to the electromechanical coupling equivalent cumulative damage index.
[0012] S40. Calculate the smooth deterioration rate of the index based on the window regression slope, and calculate the Arrhenius excess thermal acceleration. Normalize and sum the two with the electromechanical coupling equivalent cumulative damage index to obtain the comprehensive risk warning value.
[0013] S50. Calculate the smooth temperature rise rate of the actual surface temperature. When the comprehensive hazard warning value, the actual surface temperature, or the temperature rise rate of any of them reaches the corresponding preset threshold, cut off the charging and discharging circuit and lock the safety interruption state.
[0014] Based on the above technical solutions, the present invention also provides the following optional technical solutions:
[0015] Further technical solution: In S10, the calculation process of the real-time signed normal displacement and actual surface temperature of the battery casing includes:
[0016] The calculation process for the real-time signed normal displacement and true surface temperature of the battery casing includes:
[0017] The real-time signed normal displacement is constructed based on the deviation between the real-time ranging value and the initial reference ranging value of the non-contact displacement sensor. Geometric constraints are imposed by introducing a displacement direction conversion coefficient bound to the sensor installation direction, and the trend of the measured surface of the battery casing moving towards the probe along the outer normal is uniformly mapped as a positive displacement.
[0018] The real-time contact force between the temperature probe and the battery casing is obtained by mapping the pre-compression deformation of the probe and the real-time signed normal displacement scaled by the displacement transfer coefficient.
[0019] An equivalent contact thermal conductivity is constructed between the probe and the battery casing. This equivalent contact thermal conductivity is composed of the base contact thermal conductivity under the reference state and the contact mechanical compensation term. The contact mechanical compensation term is driven by the real-time contact force and modulated by the nonlinear heat transfer relationship through the nonlinear index of the contact thermal conductivity.
[0020] The true surface temperature is extracted from the apparent measured temperature based on the lumped dynamic thermal equilibrium relationship. The extraction process includes compensating for dynamic thermal inertia error terms and environmental heat dissipation error terms in the apparent measured temperature. The dynamic thermal inertia error term is jointly constrained by the lumped heat capacity of the temperature probe, the rate of change of the apparent measured temperature, and the equivalent contact thermal conductivity. The environmental heat dissipation error term is driven by the temperature difference between the apparent measured temperature and the ambient temperature, and is jointly constrained by the equivalent heat transfer constant and equivalent contact thermal conductivity of the temperature probe dissipating heat to the environment.
[0021] In the calculation, a strictly positive physical boundary constraint is applied to the mechanical compression of the probe to eliminate contact thermal conductivity singularities and thermal break failures that may occur in the contact thermodynamic calculation.
[0022] A further technical solution: The apparent temperature change rate is obtained by performing discrete-time least squares linear regression within a set temperature sliding time window. The rate of change corresponds to the slope of the first-order linear regression, and its value is obtained by normalizing the ratio of the time-temperature covariance within the sliding window to the time variance within the same window.
[0023] Further technical solution: In step S20, the calculation process of the equivalent internal resistance under the reference operating condition includes:
[0024] The fixed additional resistance of the measuring leads and the real-time contact additional resistance between the test fixture and the terminal are stripped from the acquired apparent AC internal resistance to obtain the measurement circuit compensation internal resistance; and a minimum effective internal resistance lower bound constraint is applied in the stripping operation to prevent negative resistance physical distortion caused by contact resistance fluctuations.
[0025] An exponential thermal compensation mapping relationship is constructed to map the internal resistance of the measurement loop to a unified calibration reference temperature to obtain the equivalent internal resistance under reference operating conditions. The thermal compensation mapping relationship is driven by the deviation of the actual surface temperature from the calibration reference temperature and is modulated by the internal resistance temperature correction coefficient of the battery system.
[0026] Further technical solution: In S30, the calculation process of the shell's equivalent deformation energy includes:
[0027] A non-negative truncation operator is applied to the real-time signed normal displacement to extract the positive outward bulging displacement, thus shielding the interference of the battery casing's inward shrinkage on the mechanical degradation assessment.
[0028] An equivalent stiffness of the shell penalized by the temperature softening effect is constructed. This stiffness is based on the benchmark equivalent stiffness at the reference temperature. A degradation reduction term dominated by the product of the actual temperature rise and the temperature softening correction coefficient is introduced. In the reduction calculation, a minimum effective equivalent stiffness lower bound constraint is applied to the shell equivalent stiffness to prevent the stiffness matrix from becoming singular at extreme high temperatures, which would lead to divergence in the deformation energy calculation.
[0029] Based on the physical constitutive relation of secondary strain energy, the equivalent deformation energy of the battery casing under the current boundary constraints is calculated by multiplying the temperature-corrected equivalent stiffness of the casing with the square of the positive outward bulging displacement.
[0030] Further technical solution: In step S30, the calculation process of the electromechanical coupling equivalent cumulative damage index includes:
[0031] The positive relative drift of the equivalent internal resistance under the reference operating condition relative to the initial reference operating condition reference internal resistance is defined as the electrochemical degradation component, and a zero-point bottoming constraint is applied to filter out internal resistance recovery artifacts:
[0032] The ratio of the shell's equivalent deformation energy to the structure's critical equivalent deformation energy is defined as the mechanical degradation component.
[0033] A multidimensional geometric coupling mechanism is constructed, which multiplies the electrochemical degradation component, which has been subjected to exponential sensitivity modulation by the electrochemical degradation sensitivity index and the mechanical degradation sensitivity index, with the mechanical degradation component, and maps the instantaneous damage state quantity after stripping the steady-state reference.
[0034] A Markov state update equation in the discrete time domain is established, and the damage index of the previous time step is iteratively accumulated according to the damage increment of the current sampling period. The damage increment is driven by the instantaneous damage state quantity and is transformed by rate scaling through the damage accumulation reference time constant and the sampling time interval, thereby outputting the electromechanical coupling equivalent cumulative damage index.
[0035] Further technical solution: In S40, the smoothing deterioration rate is obtained by performing discrete-time least squares linear regression on the electromechanical coupling equivalent cumulative damage index within a set damage sliding time window; its rate corresponds to the slope of the first-order linear regression, and its value is obtained by performing a ratio normalization operation on the time-damage covariance within the sliding window and the time variance within the same window.
[0036] Further technical solution: In step S40, the calculation process of the comprehensive risk warning value includes:
[0037] Based on the thermodynamic reaction kinetic constitutive model, the reciprocal difference between the actual surface temperature and the calibrated reference temperature is used as the driving potential. Under the constraint of the ratio of apparent activation energy to ideal gas constant, the exponential acceleration factor of the thermodynamic reaction is calculated, and the excess part is extracted to obtain the Arrhenius excess thermal acceleration.
[0038] A bounded rational fractional mapping function is constructed to nonlinearly map the electromechanical coupling equivalent cumulative damage exponent, the positive cutoff of the smooth deterioration rate, and the Arrhenius excess thermal acceleration to a dimensionless probability space of zero to one, generating the cumulative damage normalization, damage rate normalization, and excess thermal acceleration normalization. For the mapping of the rate term, a dimensionality elimination process is performed by introducing a characteristic time constant of the danger rate evaluation.
[0039] Based on the principle of convex combination weighted synthesis, the three normalized quantities are linearly summed and projected using a group of strictly non-negative weight coefficients with a sum of one, thereby outputting the comprehensive risk warning value that dynamically converges to the interval between zero and one.
[0040] Further technical solution: In S50, the security interruption control logic includes:
[0041] The smooth temperature rise rate is extracted by performing discrete-time least squares linear regression on the real surface temperature within a set surface temperature sliding time window.
[0042] The triggering condition for cutting off the charging and discharging circuit of the test battery is configured as a logical OR relationship of three independent parallel physical boundary conditions, specifically including: the comprehensive hazard warning value continuously exceeding the comprehensive hazard safety threshold in multiple consecutive samplings to achieve noise filtering; or the actual surface temperature instantaneously breaking down the temperature hard threshold set by the safety procedure; or the smooth temperature rise rate instantaneously breaking down the temperature rise rate hard threshold characterizing the critical slope of thermal runaway.
[0043] After the circuit is cut off, a safety interrupt latch state is triggered. The latch control is only released when the system receives a manual reset command and all three monitored variables spontaneously fall back below their respective reset safety thresholds.
[0044] A monitoring device for high-temperature life testing of lead-acid batteries, employing the aforementioned monitoring method for high-temperature life testing of lead-acid batteries.
[0045] This invention provides a monitoring method and device for high-temperature life testing of lead-acid batteries, which has the following advantages compared with the prior art:
[0046] 1. This invention introduces a non-contact displacement sensor to synchronously monitor the normal deformation of the battery casing, establishes a dynamic mapping relationship between displacement and real-time contact force of the probe, and then performs adaptive depth compensation for changes in probe contact thermal conductivity, system dynamic thermal inertia and environmental heat dissipation errors. This mechanism eliminates the temperature measurement discontinuity and distortion caused by battery swelling, and achieves high-precision restoration of the true surface temperature of the battery under extreme conditions.
[0047] 2. This invention breaks through the limitations of traditional single-dimensional life assessment. Based on eliminating interference from the measurement circuit and performing precise temperature normalization, it not only quantifies the equivalent internal resistance drift that characterizes electrochemical degradation, but also calculates the equivalent deformation energy of the shell using the positive displacement feature and the stiffness model corrected by temperature softening. It deeply geometrically couples mechanical degradation with electrochemical degradation. This coupled damage index can more scientifically and comprehensively reflect the true health status of the battery during the accelerated aging process at high temperatures.
[0048] 3. This invention comprehensively considers the total cumulative damage, the rate of damage deterioration, and the Arrhenius excess thermal acceleration, and constructs a bounded normalized comprehensive hazard warning system. Combined with the actual surface temperature and its smooth temperature rise rate, it forms a multi-level interruption logic that integrates trend prediction and physical limit defense. It can accurately lock in and cut off dangerous circuits before the battery experiences substantial thermal runaway, greatly improving the operational safety of the high-temperature life test bench. Attached Figure Description
[0049] Figure 1 This is a schematic diagram of the overall process of the monitoring method of the present invention.
[0050] Figure 2 This is a diagram illustrating the actual surface temperature compensation and reconstruction mechanism.
[0051] Figure 3 The logic diagram for calculating the equivalent cumulative damage of electromechanical coupling is shown.
[0052] Figure 4 This is a diagram of the logic framework for multi-level safety interrupt control. Detailed Implementation
[0053] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the invention.
[0054] The specific implementation of the present invention will be described in detail below with reference to specific embodiments.
[0055] Please see Figure 1 as well as Figure 4 A monitoring method for high-temperature life testing of lead-acid batteries, provided in one embodiment of the present invention, includes:
[0056] S10. Obtain the apparent measurement temperature of the temperature probe, the real-time signed normal displacement of the battery casing of the non-contact displacement sensor, and the ambient temperature, compensate for probe contact and thermal errors, and obtain the true surface temperature.
[0057] S20. Under the preset state of charge, resting time and AC excitation, obtain the apparent AC internal resistance, remove the additional resistance of the measurement circuit and convert it to the calibrated reference temperature in combination with the real surface temperature to obtain the reference working condition equivalent internal resistance.
[0058] S30. Calculate the electrochemical degradation component based on the change of equivalent internal resistance, extract the positive displacement to obtain the positive outward bulging displacement, combine the temperature-corrected stiffness to calculate the shell's equivalent deformation energy and mechanical degradation component, couple the two to obtain the instantaneous damage state quantity, and update it to the electromechanical coupling equivalent cumulative damage index.
[0059] S40. Calculate the smooth deterioration rate of the index based on the window regression slope, and calculate the Arrhenius excess thermal acceleration. Normalize and sum the two with the electromechanical coupling equivalent cumulative damage index to obtain the comprehensive risk warning value.
[0060] S50. Calculate the smooth temperature rise rate of the actual surface temperature. When the comprehensive hazard warning value, the actual surface temperature, or the temperature rise rate of any of them reaches the corresponding preset threshold, cut off the charging and discharging circuit and lock the safety interruption state.
[0061] The following example will provide a more detailed explanation of the above technical solution:
[0062] In a high-temperature life test scenario for a lead-acid battery, the test bench subjectes the battery to prolonged high-temperature charge-discharge cycles. During the test, it is necessary to monitor the battery's health status in real time and issue safety warnings.
[0063] First, in S10, the system continuously acquires the apparent measured temperature of the temperature probe, the real-time signed normal displacement of the battery casing from the non-contact displacement sensor, and the ambient temperature inside the test chamber. For example, the temperature probe might measure a battery surface temperature of 330K, the non-contact displacement sensor might measure an outward expansion of 0.5 mm in the casing, and the ambient temperature might be 325K. To obtain a more accurate true surface temperature, the system uses the displacement data to correct for changes in the contact thermal resistance between the probe and the casing based on a preset compensation model, and considers the thermal inertia of the probe itself, thereby correcting the apparent measured temperature to be closer to the actual true surface temperature, such as 332K.
[0064] Next, in S20, after the battery is in a preset state of charge and has been left to rest for a certain period of time, the system applies an AC excitation to obtain the apparent AC internal resistance. For example, if the measured apparent AC internal resistance is 1.5 milliohms, the system first removes the additional resistance from the measuring leads and test fixtures, for example, a total additional resistance of 0.2 milliohms, resulting in a compensated internal resistance of 1.3 milliohms for the measuring circuit. Subsequently, combining the actual surface temperature (332K) obtained in S10 and the preset calibration reference temperature (e.g., 298K), the system uses an internal resistance temperature correction factor to convert this compensated internal resistance to the equivalent internal resistance at the calibration reference temperature, for example, obtaining a reference operating condition equivalent internal resistance of 1.0 milliohms. This equivalent internal resistance can more accurately reflect the electrochemical state of the battery.
[0065] Subsequently, in S30, the system uses this data to calculate the battery's damage state. Assuming the battery's initial reference internal resistance is 0.8 milliohms, the electrochemical degradation component is calculated based on the change in the current reference equivalent internal resistance (1.0 milliohms). Simultaneously, the system extracts the positive outward bulging displacement (e.g., 0.5 mm) from the real-time signed normal displacement obtained from a non-contact displacement sensor. This is combined with the current actual surface temperature (332 K) to correct the shell's equivalent stiffness, as high temperatures may cause material softening and reduced stiffness. Using the corrected shell equivalent stiffness and the positive outward bulging displacement, the shell's equivalent deformation energy is calculated. Based on this deformation energy, the mechanical degradation component is calculated. Finally, the system couples the electrochemical and mechanical degradation components to obtain an instantaneous damage state quantity, which is then accumulated and updated into an electromechanical coupling equivalent cumulative damage index. This index comprehensively reflects the degree of battery degradation in both electrochemical and mechanical aspects.
[0066] Furthermore, in S40, the system uses historical data of the electromechanical coupling equivalent cumulative damage index and performs first-order linear regression with a sliding time window to calculate the smooth deterioration rate of the index, reflecting the trend of battery damage. Simultaneously, based on the actual surface temperature (332K) and the calibration reference temperature (298K), the system uses the Arrhenius equation to calculate the Arrhenius excess thermal acceleration, quantifying the accelerating effect of high temperature on battery aging. Subsequently, the system normalizes the electromechanical coupling equivalent cumulative damage index, the smooth deterioration rate, and the Arrhenius excess thermal acceleration, and performs a weighted summation to finally obtain a comprehensive hazard warning value; for example, this warning value might be 0.6.
[0067] Finally, in S50, the system continuously calculates the smoothed temperature rise rate of the actual surface temperature. For example, the current temperature rise rate is 0.05 Kelvin per second. The system compares the comprehensive hazard warning value (0.6), the actual surface temperature (332K), and its smoothed temperature rise rate (0.05 Kelvin per second) with preset corresponding thresholds. Assuming the preset comprehensive hazard threshold is 0.7, the temperature hard threshold is 340K, and the temperature rise rate hard threshold is 0.1 Kelvin per second. If any indicator reaches or exceeds its threshold, for example, if the comprehensive hazard warning value continues to rise and reaches 0.7, the system will immediately control the test bench to cut off the battery's charging and discharging circuit and lock the safety interruption state. This locked state will remain until manually reset and all safety conditions (such as temperature, temperature rise rate, and hazard level all being below the reset threshold) are met. Through this method, the system can provide timely warnings and intervention when the battery shows early signs of degradation or potential hazards, thus preventing accidents.
[0068] Based on the above examples, the technical concept of this embodiment demonstrates a significant technical contribution. Traditional monitoring methods suffer from unstable contact between the temperature probe and the casing when the battery undergoes external deformation, leading to severe lag and distortion in the measured apparent temperature. This embodiment, through S10, introduces a non-contact displacement sensor to acquire the real-time signed normal displacement of the battery casing and uses this displacement data to compensate for probe contact and thermal errors, thereby obtaining the true surface temperature. This method overcomes the accuracy problem of traditional temperature measurements under dynamic deformation and provides more reliable thermal state information.
[0069] Furthermore, in existing technologies, the measured AC internal resistance is easily affected by the cross-interference of the additional resistance in the measurement circuit and real-time temperature fluctuations during high-temperature testing, leading to inaccurate electrochemical degradation assessments. In this embodiment, in S20, not only is the additional resistance in the measurement circuit removed, but the internal resistance is also converted to the calibration reference temperature using the actual surface temperature to obtain the equivalent internal resistance under reference operating conditions. This processing method effectively eliminates the interference of temperature and the measurement circuit on the internal resistance measurement, making the calculation of the electrochemical degradation component more accurate and avoiding the inaccuracies of traditional methods.
[0070] More importantly, existing monitoring methods typically treat temperature, internal resistance, or external deformation in isolation, lacking a comprehensive evaluation model that deeply couples thermodynamic acceleration effects, electrochemical internal resistance evolution, and shell mechanical deformation energy, thus failing to achieve early warning. In S30, this embodiment innovatively couples the electrochemical degradation component and the mechanical degradation component to obtain an instantaneous damage state quantity, which is then accumulated and updated into an electromechanical coupling equivalent cumulative damage index. Further, in S40, the smoothing deterioration rate of this index is integrated with the Arrhenius excess thermal acceleration quantity to jointly construct a comprehensive hazard warning value. This warning value comprehensively considers the battery's cumulative damage, damage deterioration trend, and high-temperature thermal acceleration effect, achieving deep fusion of multi-physics information. By performing multiple threshold judgments based on this comprehensive hazard warning value, the actual surface temperature, and its temperature rise rate in S50, this embodiment can achieve early warning and proactive intervention for potential battery hazards, rather than relying solely on a single hard temperature threshold for post-event shutdown. This comprehensive evaluation model significantly improves the safety and reliability of high-temperature life testing, effectively preventing serious safety accidents such as damage to testing equipment or even fires.
[0071] Preferably, the method for obtaining the actual surface temperature in S10 is as follows:
[0072] The calculation process for the real-time signed normal displacement and true surface temperature of the battery casing includes:
[0073] The real-time signed normal displacement is constructed based on the deviation between the real-time ranging value and the initial reference ranging value of the non-contact displacement sensor. Geometric constraints are imposed by introducing a displacement direction conversion coefficient bound to the sensor installation direction, and the trend of the measured surface of the battery casing moving towards the probe along the outer normal is uniformly mapped as a positive displacement.
[0074] The real-time contact force between the temperature probe and the battery casing is obtained by mapping the pre-compression deformation of the probe and the real-time signed normal displacement scaled by the displacement transfer coefficient.
[0075] An equivalent contact thermal conductivity is constructed between the probe and the battery casing. This equivalent contact thermal conductivity is composed of the base contact thermal conductivity under the reference state and the contact mechanical compensation term. The contact mechanical compensation term is driven by the real-time contact force and modulated by the nonlinear heat transfer relationship through the nonlinear index of the contact thermal conductivity.
[0076] The true surface temperature is extracted from the apparent measured temperature based on the lumped dynamic thermal equilibrium relationship. The extraction process includes compensating for dynamic thermal inertia error terms and environmental heat dissipation error terms in the apparent measured temperature. The dynamic thermal inertia error term is jointly constrained by the lumped heat capacity of the temperature probe, the rate of change of the apparent measured temperature, and the equivalent contact thermal conductivity. The environmental heat dissipation error term is driven by the temperature difference between the apparent measured temperature and the ambient temperature, and is jointly constrained by the equivalent heat transfer constant and equivalent contact thermal conductivity of the temperature probe dissipating heat to the environment.
[0077] In the calculation, a strictly positive physical boundary constraint is applied to the mechanical compression of the probe to eliminate contact thermal conductivity singularities and thermal break failures that may occur in the contact thermodynamic calculation.
[0078] Specifically, the real-time signed normal displacement of the battery casing is calculated based on the real-time ranging value of the non-contact displacement sensor:
[0079]
[0080] in, for Real-time signed normal displacement (in meters) of the measured surface of the battery casing relative to the initial reference position. for Real-time distance measurement value (in meters) output by a non-contact displacement sensor. To initialize the reference distance measurement value (in meters) output by the non-contact displacement sensor in the reference state. The displacement direction conversion coefficient is determined based on the installation direction of the non-contact displacement sensor and satisfies... The displacement direction conversion coefficient When configured to move the measured surface of the battery casing along its outer normal direction toward the temperature probe, it satisfies And when the measured surface of the battery casing moves in a direction opposite to its outer normal, it satisfies ;
[0081] The real-time contact force between the temperature probe and the battery casing is calculated based on the real-time signed normal displacement.
[0082]
[0083] The equivalent contact thermal conductivity between the temperature probe and the battery casing is calculated based on the real-time contact force.
[0084]
[0085] Calculate the true surface temperature based on the equivalent contact thermal conductivity and the lumped dynamic thermal equilibrium relationship:
[0086]
[0087] in, for Real-time contact force between the temperature probe and the battery casing (in Newtons). The spring constant (in Newtons per meter) for the preload spring of the temperature probe. This represents the pre-compression deformation (in meters) of the temperature probe under initial calibration conditions. The transfer coefficient of the battery casing's signed normal displacement to the temperature probe spring compression displacement, and satisfying the following conditions: , for Equivalent contact thermal conductivity between the temperature probe and the battery casing (in watts per Kelvin). The baseline contact thermal conductivity (in watts per Kelvin) is initialized under reference conditions. For contact thermal conductivity-contact force calibration coefficient, For contact thermal conductivity nonlinearity index and satisfying 0, for The actual surface temperature of the battery casing at any given time (in Kelvin). for The apparent measured temperature (in Kelvin) output by the temperature probe at any given time. This is the lumped heat capacity of the temperature probe (in joules per Kelvin). The apparent rate of temperature change (in Kelvin per second) after smoothing. The equivalent heat transfer constant (in watts per Kelvin) is the heat dissipation from the temperature probe to the test chamber environment. for The ambient temperature inside the test chamber is constantly monitored (in Kelvin), and the calculation process for the actual surface temperature satisfies the following: , , ;
[0088] Furthermore, the apparent temperature change rate is obtained by performing discrete-time least squares linear regression within a set temperature sliding time window. The rate of change corresponds to the slope of the first-order linear regression, and its value is obtained by normalizing the ratio of the time-temperature covariance within the sliding window to the time variance within the same window.
[0089] Specifically, the apparent rate of temperature change It is obtained by the slope of a first-order linear regression within the temperature sliding time window;
[0090] For the current sampling time Within the corresponding temperature sliding time window The formula for calculating the apparent rate of temperature change at each temperature sampling point is:
[0091]
[0092]
[0093]
[0094] in, This represents the number of sampling points within the temperature sliding time window. For the first The sampling time (in seconds) corresponding to each temperature sampling point. This is the average value (in seconds) of the sampling time within the temperature sliding time window. For the first Apparent measured temperature (in Kelvin) at each temperature sampling point. The average value (in Kelvin) of the apparent measured temperature within the temperature sliding time window.
[0095] First, the real-time signed normal displacement of the battery casing is calculated based on the real-time ranging value obtained by the non-contact displacement sensor. This technique aims to accurately quantify the minute deformation of the battery casing surface relative to its initial reference position, using the ranging value acquired in real time by the non-contact displacement sensor. Reference distance value under initial reference state Perform the difference calculation and combine it with the displacement direction conversion coefficient. This allows us to obtain directional displacement. Displacement direction conversion coefficient. The setting ensures the physical meaning of the displacement direction. For example, when the battery casing expands towards the temperature probe, the displacement is defined as a positive value, and vice versa. This accurate displacement measurement is the basis for subsequent calculation of the contact force and contact thermal conductivity between the probe and the casing. It can be implemented by acquiring real-time ranging data through non-contact sensors such as laser displacement sensors and ultrasonic displacement sensors, and then having the above formulas executed by embedded processors or host computer software.
[0096] Next, the real-time contact force between the temperature probe and the battery casing is calculated based on the real-time signed normal displacement. This technique is used to quantify the interaction force between the temperature probe and the battery casing surface, and the contact force is one of the key factors affecting contact thermal conductivity. This is achieved by calculating the real-time signed normal displacement of the battery casing. This is converted into the compression deformation of the temperature probe preload spring, combined with the spring's elastic coefficient. and displacement transfer coefficient It can accurately calculate the real-time contact force. Displacement transfer coefficient The calculation takes into account the efficiency of displacement transmission from the battery casing to the probe spring. This ensures that the contact force can dynamically reflect the influence of the battery casing deformation on the probe pressure. This can be achieved by the control unit or data processing module performing real-time calculations based on preset spring parameters and transmission coefficients after the data acquisition system receives the displacement data.
[0097] Subsequently, the equivalent contact thermal conductivity between the temperature probe and the battery casing is calculated based on the real-time contact force. This technique aims to characterize the efficiency of heat transfer between the temperature probe and the battery casing. Equivalent contact thermal conductivity It is a key parameter in the calculation of real surface temperature, directly reflecting the thermal resistance characteristics of the contact interface. This is achieved through basic contact thermal conductivity... Contact thermal conductivity-contact force calibration factor Nonlinear index of contact thermal conductivity and real-time contact force A nonlinear relationship model between contact thermal conductivity and contact force can be established. This model can dynamically correct the contact thermal conductivity to more accurately reflect the actual heat transfer conditions. This can be achieved by having the data processing unit perform table lookup or formula calculation based on pre-calibrated parameters after the real-time contact force calculation is completed.
[0098] Furthermore, the true surface temperature is calculated based on the equivalent contact thermal conductivity and the lumped dynamic thermal equilibrium relationship, aiming to obtain the true surface temperature of the battery casing by compensating for probe contact and thermal errors. This calculation is based on the lumped dynamic thermal equilibrium relationship and comprehensively considers the apparent temperature measured by the temperature probe. Its rate of change Lumped heat capacity of the probe The equivalent heat transfer constant between the probe and the environment Ambient temperature and the equivalent contact thermal conductivity between the probe and the battery casing This thermal balance model effectively eliminates measurement errors caused by the probe's own thermal inertia, heat exchange with the environment, and thermal resistance in contact with the battery casing, thus obtaining a temperature closer to the actual battery surface. This can be achieved by a main control unit or dedicated signal processor acquiring various input data in real time and iterating or directly calculating based on the aforementioned thermal balance equation.
[0099] Among them, the apparent temperature change rate Obtained by the slope of a first-order linear regression within a temperature sliding time window, this technique is used to acquire the instantaneous change trend of the apparent temperature measured by the temperature probe, and is an important component of the dynamic thermal balance term in the calculation of real surface temperature. By performing first-order linear regression on each temperature sampling point, a smooth temperature change rate can be obtained. The linear regression method can effectively filter out measurement noise and provide a stable and reliable temperature change trend. The accuracy of this rate directly affects the dynamic response and precision of the actual surface temperature calculation. This can be achieved by having the data acquisition system maintain a sliding time window at each sampling moment and using digital signal processing algorithms (such as the least squares method) to calculate the slope of the data within the window in real time.
[0100] This application's solution establishes a complete physical chain, from battery casing displacement to contact force, then to contact thermal conductivity, and finally to the calculation of the actual surface temperature using a dynamic thermal balance model. This enables precise compensation for errors in the contact thermal resistance and thermal inertia of the temperature probe. This method not only provides more accurate battery surface temperature data than traditional direct measurement but also provides high-precision input for subsequent steps such as internal resistance temperature normalization, mechanical degradation component calculation, and comprehensive hazard warning, significantly improving the reliability and effectiveness of the entire high-temperature life testing and monitoring method.
[0101] The following is a concrete example. In practical applications, a high-precision laser displacement sensor can be used as the non-contact displacement sensor, capable of measuring distance changes on the battery casing surface in real time with micron-level accuracy. This sensor is mounted directly above the battery casing, adjacent to a temperature probe. The temperature probe can be a type K thermocouple with a pre-tensioned spring, its probe in close contact with the battery casing surface. When the battery casing undergoes slight expansion or contraction due to internal chemical reactions or temperature changes, the laser displacement sensor outputs the distance measurement value in real time. An embedded microcontroller, such as a unit based on an ARM Cortex-M series processor, can periodically sample... , and Data. The microcontroller first uses pre-stored reference ranging values. and the calibrated displacement direction conversion coefficient The real-time signed normal displacement was calculated. Next, the calibrated spring constant is used... Pre-compressed deformation and displacement transfer coefficient Calculate the real-time contact force Subsequently, based on the fundamental contact thermal conductivity in the contact thermal conductivity-contact force model... Calibration coefficient and nonlinear exponent The equivalent contact thermal conductivity was calculated. Simultaneously, the microcontroller maintains a temperature sliding time window, tracking historical apparent temperature measurements. The data were subjected to first-order linear regression to obtain the apparent rate of temperature change. Finally, all these parameters, including the lumped heat capacity of the probe, will be considered. and equivalent heat transfer constant Substituting into the dynamic thermal balance equation, the actual surface temperature of the battery casing is calculated in real time. The entire calculation process can be completed within each sampling period, ensuring the real-time nature and accuracy of the temperature data.
[0102] Through the above technical solution, this application overcomes the contact thermal resistance and thermal inertia errors inherent in traditional temperature measurement methods during high-temperature life testing. By accurately measuring the minute deformation of the battery casing and dynamically calculating the contact force and equivalent contact thermal conductance between the probe and the casing based on a physical model, combined with the probe's own dynamic thermal equilibrium relationship, accurate acquisition of the true surface temperature of the battery casing is achieved. This precise temperature data is crucial for subsequent internal resistance temperature normalization processing, eliminating the interference of temperature fluctuations on internal resistance measurement and allowing changes in internal resistance to more accurately reflect the electrochemical degradation state of the battery. Simultaneously, accurate true surface temperature is also the basis for calculating the equivalent stiffness temperature correction of the casing and subsequently assessing the mechanical degradation component, ensuring the reliability of electromechanical coupling damage assessment. Ultimately, by providing high-precision true surface temperature and its rate of change, this solution significantly improves the overall accuracy and timely warning of the high-temperature life testing monitoring method for lead-acid batteries, effectively avoiding misjudgments or omissions caused by inaccurate temperature measurements, thereby ensuring the safety of the testing process and the validity of the data.
[0103] Preferably, in step S20, the calculation process of the equivalent internal resistance under the reference operating condition includes:
[0104] The fixed additional resistance of the measuring leads and the real-time contact additional resistance between the test fixture and the terminal are stripped from the acquired apparent AC internal resistance to obtain the measurement circuit compensation internal resistance; and a minimum effective internal resistance lower bound constraint is applied in the stripping operation to prevent negative resistance physical distortion caused by contact resistance fluctuations.
[0105] An exponential thermal compensation mapping relationship is constructed to map the internal resistance of the measurement loop to a unified calibration reference temperature to obtain the equivalent internal resistance under reference conditions. The thermal compensation mapping relationship is driven by the deviation of the actual surface temperature from the calibration reference temperature and is modulated by the internal resistance temperature correction coefficient of the battery system.
[0106] Specifically, the equivalent internal resistance under the reference operating condition is obtained as follows:
[0107] By removing the additional resistance of the measurement circuit from the apparent AC internal resistance, the compensated internal resistance of the measurement circuit is obtained:
[0108]
[0109] The internal resistance of the measurement circuit is normalized to the reference temperature based on the actual surface temperature to obtain the equivalent internal resistance under the reference operating condition:
[0110]
[0111] in, for The internal resistance of the measurement circuit after removing the additional resistor in the measurement circuit (in ohms). The minimum effective internal resistance is set (in ohms). for Apparent AC internal resistance (in ohms) collected at all times. The fixed additional resistance (in ohms) formed by the measuring wires and acquisition channels. Additional resistance (in ohms) is added to the real-time contact formed between the test fixture and the battery terminal. for The equivalent internal resistance (in ohms) of the reference operating condition after being converted to the calibrated reference temperature. This is the internal resistance temperature correction factor (in reciprocal of Kelvin). for The actual surface temperature of the battery casing at any given time (in Kelvin). For calibration reference temperature (unit: Kelvin).
[0112] This application first examines the apparent internal resistance... The additional resistance of the measurement circuit is removed to obtain purer information about the battery's internal resistance. The additional resistance of the measurement circuit includes the fixed additional resistance formed by the measurement leads and the acquisition channel. Additional resistance to real-time contact formed between the test fixture and the battery terminals These additional resistances are inherent sources of error in the measurement system; they are superimposed on the battery's true internal resistance, resulting in an apparent AC internal resistance. The value is too high. The purpose of removing these additional resistors is to obtain an internal resistance value that is closer to the actual electrochemical state of the battery, i.e., the measurement circuit compensates for the internal resistance. Removing the additional resistor can be achieved in several ways, such as fixing the additional resistor. Precise calibration can be performed before testing by short-circuiting the measurement circuit or connecting a known standard resistor; while real-time contact with the additional resistor... Additional sensors (such as pressure sensors) can be used to monitor the contact state in real time, and estimation and compensation can be performed in conjunction with a pre-established contact resistance model, or separation can be achieved through multi-frequency impedance spectroscopy analysis. Simultaneously, a minimum effective internal resistance is set. This can effectively avoid the occurrence of physically meaningless negative internal resistance during the calculation process.
[0113] Based on this, this application further considers the actual surface temperature Compensation for internal resistance of the measurement circuit Normalize to the reference temperature to obtain the equivalent internal resistance under the reference operating condition. The internal resistance of a battery is significantly sensitive to temperature, and internal resistance values measured at different temperatures are not directly comparable. The measurement circuit should be compensated for the internal resistance. Normalized to calibration reference temperature This normalization process aims to eliminate the influence of temperature on internal resistance measurements, allowing internal resistance values obtained at different test temperatures to be compared and analyzed under a unified benchmark, thus more accurately reflecting the degree of electrochemical degradation of the battery. This normalization typically utilizes an internal resistance temperature correction factor. The current actual surface temperature is expressed using an exponential relationship. Internal resistance conversion to the calibration reference temperature Alternatively, an internal resistance-temperature lookup table or a polynomial fitting model based on a large amount of experimental data can be established, according to the real-time surface temperature. Interpolation or calculation is performed to achieve temperature normalization of the internal resistance.
[0114] The solution in this application systematically addresses the apparent internal resistance of the AC circuit. Interference factors were considered to ensure the obtained equivalent internal resistance under the reference operating condition. It can accurately reflect the true electrochemical state of a lead-acid battery. Firstly, by analyzing the apparent AC internal resistance... Subtract the fixed additional resistance formed by the measuring wires and the acquisition channel. Additional resistance to real-time contact formed between the test fixture and the battery terminals This effectively eliminates errors introduced by the measurement system itself. This step ensures that the measurement loop compensates for internal resistance. The temperature primarily originates from the battery itself, rather than from external connections. Subsequently, given the strong temperature dependence of the battery's internal resistance, this solution utilizes the aforementioned method to accurately obtain the true surface temperature. Compensation for internal resistance of the measurement circuit Perform reference temperature normalization. This is done using the internal resistance temperature correction factor. Will Converted to the preset calibration reference temperature equivalent value This dual correction mechanism, which first removes the additional resistance of the measurement circuit and then performs temperature normalization, ensures that the final equivalent internal resistance of the reference operating condition is obtained. This eliminates interference from variations in the measurement environment and conditions, providing a comparable and reliable indicator of battery electrochemical state under a unified benchmark. This is crucial for the subsequent accurate calculation of electrochemical degradation components. This is crucial, thus significantly improving the accuracy and reliability of the entire high-temperature life test monitoring method.
[0115] The following is a specific example to illustrate this. In practical applications, the fixed additional resistance formed by the measuring wires and the acquisition channel... Calibration can be achieved by short-circuiting the two ends of the measuring leads after the test bench is set up, and then measuring the impedance value using a high-precision impedance tester. For example, the impedance value can be measured... The resistance is 0.0005 ohms. This refers to the additional resistance of the real-time contact formed between the test fixture and the battery terminals. A dynamic compensation method can be used, for example, by integrating a miniature pressure sensor onto the test fixture to monitor the pressure of the fixture on the battery terminals in real time, and to estimate and compensate in real time based on the pressure-contact resistance relationship curve established experimentally beforehand. For example, when the pressure decreases, The minimum effective internal resistance may increase. This can be set to a very small positive value, such as 0.00001 ohms, to ensure the physical reasonableness of the calculation results. For reference temperature normalization, the internal resistance temperature correction factor... The internal resistance of the lead-acid battery under test can be measured in a laboratory at multiple stable temperature points (e.g., 20℃, 30℃, 40℃), and then the measurement data can be subjected to exponential fitting to obtain the internal resistance. Values, for example, can be obtained for Calibration reference temperature It can be set to 25℃ (i.e., 298.15 Kelvin), which is a commonly used industry benchmark temperature for battery performance evaluation. Actual surface temperature. This information is then obtained in real-time and accurately using the methods described above. Through these specific parameters and methods, the system can calculate the accurate equivalent internal resistance under the reference operating condition in real time. This provides reliable data for assessing the health status of batteries.
[0116] Through the above technical solution, this application can effectively solve the problems of additional resistance interference and temperature sensitivity in apparent AC internal resistance measurement. Specifically, it removes the additional resistance of the measurement circuit. and It can eliminate errors introduced by the measurement system itself, enabling the measurement loop to compensate for internal resistance. This more accurately reflects the electrochemical characteristics of the battery itself. Simultaneously, the actual surface temperature obtained based on the above method... Normalizing the internal resistance to a reference temperature eliminates the impact of ambient temperature fluctuations on internal resistance measurements. This provides a unified comparison benchmark for internal resistance data obtained at different times and temperatures, enabling accurate tracking of battery electrochemical degradation trends. Therefore, this solution provides a highly accurate and physically meaningful equivalent internal resistance under reference operating conditions. This provides a solid foundation for subsequent calculations of electrochemical degradation components, significantly improves the accuracy and reliability of the entire high-temperature life test monitoring method for lead-acid batteries, avoids misjudgments or omissions caused by measurement errors and temperature effects, and thus improves the accuracy of battery life prediction and safety warning.
[0117] Preferably, the electromechanical coupling equivalent cumulative damage index is obtained as follows:
[0118] Calculate the equivalent deformation energy of the shell: Apply a non-negative truncation operator to the real-time signed normal displacement to extract the positive outward bulging displacement, thus shielding the interference of the inward shrinkage of the battery shell on the mechanical degradation assessment;
[0119] An equivalent stiffness of the shell penalized by the temperature softening effect is constructed. This stiffness is based on the benchmark equivalent stiffness at the reference temperature. A degradation reduction term dominated by the product of the actual temperature rise and the temperature softening correction coefficient is introduced. In the reduction calculation, a minimum effective equivalent stiffness lower bound constraint is applied to the shell equivalent stiffness to prevent the stiffness matrix from becoming singular at extreme high temperatures, which would lead to divergence in the deformation energy calculation.
[0120] Based on the physical constitutive relation of secondary strain energy, the equivalent deformation energy of the battery shell under the current boundary constraints is calculated by multiplying the temperature-corrected shell equivalent stiffness with the square of the positive outward bulging displacement.
[0121] Specifically, the positive part of the real-time signed normal displacement is extracted to obtain the positive outward bulging displacement:
[0122]
[0123] The positive part operator is defined as follows:
[0124]
[0125] The equivalent stiffness of the shell is corrected based on the actual surface temperature.
[0126]
[0127] The equivalent deformation energy of the shell is calculated based on the temperature-corrected equivalent stiffness and the positive outward bulge displacement:
[0128]
[0129] in, for The positive outward displacement (in meters) of the measured surface of the battery casing bulging outward along the outer normal direction at any given moment. Time-directed outward bulging displacement , for The equivalent stiffness of the shell after temperature correction at any time (in Newtons per meter). The minimum effective equivalent stiffness (in Newtons per meter). To calibrate the shell's equivalent stiffness (in Newtons per meter) at the reference temperature. This is the temperature softening correction factor for the equivalent stiffness of the shell (in reciprocal of Kelvin). for The actual surface temperature at any given time (in Kelvin). For calibrating reference temperature (in Kelvin). for The equivalent deformation energy (in joules) of the measured area of the battery casing under preset boundary constraints at any given time.
[0130] Furthermore, the positive relative drift of the equivalent internal resistance under the reference operating condition relative to the reference internal resistance under the initial reference operating condition is defined as the electrochemical degradation component, and a zero-point bottoming constraint is applied to filter out internal resistance recovery artifacts.
[0131] The ratio of the shell's equivalent deformation energy to the structure's critical equivalent deformation energy is defined as the mechanical degradation component.
[0132] A multidimensional geometric coupling mechanism is constructed, which multiplies the electrochemical degradation component, which has been subjected to exponential sensitivity modulation by the electrochemical degradation sensitivity index and the mechanical degradation sensitivity index, with the mechanical degradation component, and maps the instantaneous damage state quantity after stripping the steady-state reference.
[0133] A Markov state update equation in the discrete time domain is established, and the damage index of the previous time step is iteratively accumulated according to the damage increment of the current sampling period. The damage increment is driven by the instantaneous damage state quantity and is transformed by rate scaling through the damage accumulation reference time constant and the sampling time interval, thereby outputting the electromechanical coupling equivalent cumulative damage index.
[0134] Specifically, the formula for calculating the electrochemical degradation component is as follows:
[0135]
[0136] The formula for calculating the mechanical degradation component is:
[0137]
[0138] The formula for calculating the instantaneous damage state quantity is:
[0139]
[0140] The electromechanical coupling equivalent cumulative damage index is updated according to discrete time:
[0141]
[0142] And it satisfies the initial conditions:
[0143]
[0144] in, Sampling time Electrochemical degradation component, Sampling time The equivalent internal resistance under reference operating conditions (in ohms). The initial reference internal resistance (in ohms) under the initial calibration condition. Sampling time Mechanical degradation component, Sampling time The shell's equivalent deformation energy (in joules). The critical equivalent deformation energy (in joules). Sampling time The instantaneous damage state quantity, It is the electrochemical degradation sensitivity index and satisfies , The mechanical degradation sensitivity index and satisfying , Sampling time The electromechanical coupling equivalent cumulative damage index, The sampling time interval (in seconds) between two consecutive damage updates. The reference time constant for damage accumulation (in seconds).
[0145] Among them, positive outward bulging displacement Used to quantify the outward expansion deformation of the battery casing, its function is to accurately capture the mechanical deformation caused by internal pressure or material expansion during high temperatures and charge-discharge cycles. This is crucial for assessing the structural integrity and mechanical damage of the battery. This displacement can be obtained through real-time signed normal displacement acquired by a non-contact displacement sensor. This is achieved by applying a positive part operator, which retains only the positive values and ignores the inward contraction displacement, thus focusing on the outward bulging phenomenon that could lead to mechanical failure. Shell equivalent stiffness. This stiffness characterizes the battery casing's resistance to deformation. Its function is to correlate the casing's deformation with the mechanical load it bears, forming the basis for calculating the casing's equivalent deformation energy. This stiffness can be determined based on the actual surface temperature. Corrections are made because the stiffness of battery casing materials typically decreases with increasing temperature; this is achieved by introducing a temperature softening correction factor. This allows for a more accurate reflection of the actual mechanical properties of the shell at high temperatures. Shell equivalent deformation energy This refers to the energy stored in the battery casing due to deformation. It directly reflects the level of mechanical stress the battery casing experiences, and its function is to provide a quantitative indicator of mechanical damage. When the deformation energy reaches a certain level, it means that the battery casing may face the risk of structural damage. This energy can be measured using the temperature-corrected equivalent stiffness of the casing. and positive outward bulging displacement It is calculated as half the product of the squares. Electrochemical degradation component. The internal resistance is used to quantify the degree of degradation in battery electrochemical performance, primarily reflected by changes in internal resistance. Its role is to provide information on the decline in the battery's internal electrochemical activity and ion transport capacity, making it an important indicator for assessing battery capacity decay and power reduction. This component can be obtained from the equivalent internal resistance under reference operating conditions at the current moment. With initial reference internal resistance The relative change is used for calculation, and its value is ensured to be not less than zero. Mechanical degradation component The degree of degradation in battery structural integrity is primarily reflected by the equivalent deformation energy of the casing. Its function is to provide information about damage to the external physical structure of the battery, such as casing cracking or seal failure. This component can be expressed through the equivalent deformation energy of the casing. With respect to the preset critical equivalent deformation energy The ratio is used for calculation. Instantaneous damage state quantity. It is a comprehensive index of the overall damage level of the battery at a certain sampling moment. Its function is to effectively couple the two different types of damage, electrochemical degradation and mechanical degradation, to form a unified instantaneous damage measure. This state quantity can be obtained through the electrochemical degradation component. and mechanical degradation components The calculation is performed using a nonlinear product form, which incorporates an electrochemical degradation sensitivity index. and mechanical degradation sensitivity index This is used to adjust the contribution weights of the two degradation components to the overall damage. Electromechanical coupling equivalent cumulative damage index. It is a comprehensive quantification of the cumulative damage a battery has experienced from its initial state to the present moment. Its purpose is to provide a continuously and dynamically updated battery health status indicator, comprehensively reflecting the overall degradation trend of the battery during high-temperature life testing. This index measures the instantaneous damage state... at discrete time step This is achieved through cumulative updates within the system, and a damage accumulation reference time constant is introduced. This is used to adjust the accumulation rate; initially, the index is set to zero.
[0146] This application's solution organically combines the electrochemical and mechanical degradation of the battery to form a unified electromechanical coupling equivalent cumulative damage index, thus solving the problem that traditional methods struggle to comprehensively assess the overall degradation state of the battery. Specifically, based on the battery's true surface temperature, real-time signed normal displacement, and equivalent internal resistance under reference operating conditions, firstly, by extracting the positive part of the real-time signed normal displacement, the outward expansion mechanical deformation of the battery casing can be accurately captured, which is crucial for identifying potential structural damage. Simultaneously, considering the changes in material mechanical properties under high-temperature environments, a temperature correction is applied to the casing's equivalent stiffness, ensuring that the subsequently calculated equivalent deformation energy of the casing more accurately reflects the mechanical stress state of the battery casing at actual operating temperatures. Secondly, the electrochemical degradation component (based on internal resistance changes) and the mechanical degradation component (based on casing deformation energy) are nonlinearly coupled. This coupling method fully reflects the interaction and accelerating effect between the two degradation mechanisms. For example, casing expansion may lead to internal structural damage, thereby affecting electrochemical performance; conversely, the intensification of electrochemical reactions may also generate gas, causing casing expansion. The instantaneous damage state variables calculated in this way can more comprehensively reflect the overall damage level of the battery at a given moment. Finally, through discrete-time cumulative updates, the instantaneous damage state variables are integrated into an electromechanical coupling equivalent cumulative damage index. This index not only considers the damage at the current moment but also includes the cumulative effect of historical damage, thus providing a continuous, dynamic, and comprehensive battery health status assessment indicator. This electromechanical coupling assessment method enables a deeper and more accurate understanding of the degradation process of lead-acid batteries in high-temperature life testing, providing a solid foundation for subsequent hazard warnings.
[0147] As a specific implementation method, the above-mentioned technical means can be implemented with reference to the following example. In a battery high-temperature life testing system, a data acquisition and processing unit can be configured. This unit can be an embedded controller or an industrial computer. This unit continuously receives real-time data from a non-contact displacement sensor, a temperature probe, and an AC internal resistance acquisition module. When a real-time signed normal displacement is received... At that time, the processing unit will perform a conditional judgment; if If the value is greater than zero, then assign it to the positive outward bulging displacement. ,otherwise It is set to zero. Meanwhile, the processing unit will adjust the actual surface temperature based on the real-time data. Combined with the pre-calibrated reference stiffness Temperature softening correction factor and minimum effective stiffness The equivalent stiffness of the shell at the current moment is calculated using the formula. Subsequently, using the calculated... and The equivalent deformation energy of the shell was calculated. In terms of electrochemistry, the processing unit will obtain the equivalent internal resistance under reference operating conditions. And compared with the initial reference operating condition internal resistance recorded during initialization. By comparison, the electrochemical degradation component was calculated. Mechanical degradation component Then through With respect to the preset critical equivalent deformation energy The ratio is obtained. Once and Once the calculation is complete, the processing unit will utilize the preset electrochemical degradation sensitivity index. and mechanical degradation sensitivity index The instantaneous damage state quantity is calculated using a nonlinear coupling formula. Finally, the processing unit will perform sampling at fixed time intervals. ,Will Equivalent cumulative damage index of electromechanical coupling added to the previous moment Above, and divided by the damage accumulation reference time constant. This allows for the updating of the current electromechanical coupling equivalent cumulative damage index. The entire calculation process is executed in a loop within the data acquisition and processing unit to ensure real-time updates of the damage index.
[0148] Through the above technical solution, this application integrates the complex electrochemical and mechanical degradation phenomena of lead-acid batteries during high-temperature life testing into a unified, physically meaningful electromechanical coupling equivalent cumulative damage index. This allows the assessment of battery health status to no longer be limited to a single dimension, but to comprehensively and accurately reflect the overall degree of battery degradation. Obtaining this index significantly improves the predictive ability of battery failure risks, providing more reliable and refined data support for safety monitoring and early warning in high-temperature life testing, thereby effectively avoiding potential safety hazards or test interruptions caused by insufficient assessment of a single parameter.
[0149] Preferably, the method for obtaining the comprehensive risk warning value is as follows:
[0150] Obtaining the smooth deterioration rate: The smooth deterioration rate is obtained by performing discrete-time least squares linear regression on the electromechanical coupling equivalent cumulative damage index within a set damage sliding time window; its rate corresponds to the slope of the first-order linear regression, and its value is obtained by normalizing the ratio of the time-damage covariance within the sliding window to the time variance within the same window.
[0151] Specifically, the duration is... The damage sliding time window is used to perform a first-order linear regression on the electromechanical coupling equivalent cumulative damage index, and the slope of the first-order linear regression is used as the smoothing deterioration rate:
[0152]
[0153]
[0154]
[0155] in, Sampling time The electromechanical coupling equivalent cumulative damage exponent smooth deterioration rate (in reciprocal of seconds). The duration of the damage sliding time window (in seconds). The number of sampling points within the damage sliding time window. Within the damage sliding time window, the first The sampling time (in seconds) corresponding to each sampling point. This represents the average sampling time (in seconds) within the damage sliding time window. For the first The electromechanical coupling equivalent cumulative damage index at each sampling point This represents the average value of the electromechanical coupling equivalent cumulative damage index within the damage sliding time window;
[0156] Furthermore, based on the thermodynamic reaction kinetic constitutive model, the reciprocal difference between the real surface temperature and the calibrated reference temperature is used as the driving potential, and under the constraint of the ratio of apparent activation energy to ideal gas constant, the exponential acceleration factor of the thermodynamic reaction is calculated, and its excess part is extracted to obtain the Arrhenius excess thermal acceleration.
[0157] A bounded rational fractional mapping function is constructed to nonlinearly map the electromechanical coupling equivalent cumulative damage exponent, the positive cutoff of the smooth deterioration rate, and the Arrhenius excess thermal acceleration to a dimensionless probability space of zero to one, thereby generating the cumulative damage normalization, damage rate normalization, and excess thermal acceleration normalization; wherein, for the mapping of the rate term, a dimensional elimination process is performed by introducing a characteristic time constant of the danger rate evaluation.
[0158] Based on the principle of convex combination weighted synthesis, the three normalized quantities are linearly summed and projected using a group of strictly non-negative weight coefficients with a sum of one, thereby outputting the comprehensive risk warning value that dynamically converges to the interval between zero and one.
[0159] Specifically, the Arrhenius thermal acceleration factor relative to the calibration reference temperature is calculated:
[0160]
[0161] Calculate the normalized cumulative damage, normalized damage rate, and normalized excess thermal acceleration separately:
[0162]
[0163]
[0164]
[0165] The comprehensive hazard warning value is calculated based on the cumulative damage normalization, damage rate normalization, and excess thermal acceleration normalization:
[0166]
[0167] in, for Arrhenius thermal acceleration factor relative to the calibration reference temperature. The apparent activation energy (in joules per mole) is obtained by calibration through the high-temperature side reaction test of lead-acid batteries. is the ideal gas constant (unit: joules per mole Kelvin). For calibrating reference temperature (in Kelvin). for The actual surface temperature at any given time (in Kelvin). To accumulate damage normalization, This is a normalized value for the damage rate. To accelerate the normalization of excess heat, The time constant (in seconds) is used to evaluate the rate of danger. This is a comprehensive risk warning value, and , The cumulative damage evaluation coefficient, The coefficient for evaluating the rate of damage deterioration. The coefficient for evaluating excess thermal acceleration. , , Both are not less than zero and .
[0168] Damage sliding time window is a data processing technique used to extract local trend information from continuous data streams. It involves defining a fixed-length time period or number of sampling points, analyzing the data within that window, and then sliding the window forward over time, repeating the analysis process. First-order linear regression is a statistical method used to fit a linear relationship between data points; its slope represents the rate of change of the data over time. Here, the electromechanical coupling equivalent cumulative damage index is used. Using the input data, performing a first-order linear regression within a sliding time window effectively filters out instantaneous noise and fluctuations, resulting in a smooth and representative deterioration rate. This method can reveal the long-term trend and rate of change of damage accumulation, providing a dynamic basis for subsequent risk assessment. In addition to using the least squares method for first-order linear regression, the exponentially weighted moving average method can also be used to estimate the rate, or a Kalman filter can be used to estimate the state of the damage index and extract its rate of change.
[0169] Arrhenius thermal acceleration factor It is a dimensionless parameter derived from the Arrhenius equation, used to quantify the effect of temperature on the rate of chemical reactions or physical degradation processes. In battery degradation, increased temperature typically accelerates various side reactions and material degradation, thus shortening battery life. This factor addresses this by introducing the apparent activation energy. Ideal gas constant Calibration reference temperature and real-time surface temperature To accurately describe this accelerating effect, it correlates the degradation rate at actual operating temperatures with the degradation rate at a reference temperature, thereby accurately assessing the additional degradation risk caused by temperature increases in high-temperature testing environments. Besides direct calculation using the Arrhenius equation, it can also be queried using a pre-established temperature-acceleration factor lookup table, or approximated using a piecewise linear function within a specific temperature range.
[0170] Cumulative damage normalization Damage rate normalization and excess heat acceleration normalization It is the process of converting indices with different physical meanings and dimensions (cumulative damage index, damage deterioration rate, thermal acceleration factor) into a unified, bounded numerical range (e.g., between 0 and 1). The cumulative damage normalization quantity is... Reflects the relative extent of current cumulative damage; damage rate normalization. It reflects the relative degree of damage deterioration rate; normalized excess heat acceleration. This reflects the relative degree of thermal acceleration effect beyond the reference temperature. Normalization eliminates dimensional differences between different indicators, enabling effective weighted summation and thus constructing a comprehensive risk assessment index. Besides using the specific function form given in this application for normalization, other sigmoid functions (such as the sigmoid function) or linear mapping functions can be used to map the original values to the interval between 0 and 1.
[0171] Comprehensive risk warning value It is a normalized quantity of cumulative damage. Damage rate normalization and excess heat acceleration normalization A single index obtained through weighted summation is designed to provide a comprehensive and intuitive assessment of battery hazard levels. This is achieved by assigning appropriate evaluation coefficients to different normalization values. , , The weights of various risk factors in the final warning value can be adjusted according to actual application needs or battery characteristics, thus more flexibly reflecting the true dangerous state of the battery. This warning value is usually designed to be between 0 and 1, with a higher value indicating a higher degree of danger. In addition to simple linear weighted summation, fuzzy logic reasoning systems or neural network models can also be used to fuse these normalized quantities to generate a more complex comprehensive risk assessment.
[0172] Evaluation coefficient , , It is used to adjust the cumulative damage normalization. Damage rate normalization and excess heat acceleration normalization In the comprehensive risk warning value The parameters weighted in the calculation, all of which have coefficients that are not less than zero, and whose sum equals 1, ensure the accuracy of the comprehensive risk warning value. The rationality and interpretability of these coefficients can be ensured. By refining the calibration of these coefficients, the early warning system can more accurately reflect the true risk preference for specific battery types or application scenarios. For example, in applications sensitive to the rate of battery life degradation, the damage deterioration rate evaluation coefficient can be appropriately increased. The weight of the excess thermal acceleration evaluation coefficient can be increased under high temperature conditions. The weights. These coefficients can be obtained through statistical analysis of a large amount of experimental data, expert experience setting, or automatic optimization through optimization algorithms (such as genetic algorithms and particle swarm optimization algorithms).
[0173] The solution in this application is to use the electromechanical coupling of the battery as an equivalent cumulative damage index. Using this as the core input, and incorporating dynamic trends and environmental acceleration effects, a multi-dimensional and comprehensive hazard assessment system was constructed. Firstly, to overcome the interference of instantaneous damage index fluctuations on risk assessment, a damage sliding time window was used to assess the electromechanical coupling equivalent cumulative damage index. Perform first-order linear regression to extract the smoothing deterioration rate. This rate indicator reflects the speed of battery degradation, providing crucial dynamic information for early warning systems. Secondly, considering that the degradation process of lead-acid batteries is significantly accelerated at high temperatures, this application introduces the Arrhenius thermal acceleration factor based on the Arrhenius equation. This factor can quantify the real-time surface temperature. This accelerates the battery degradation rate, thus incorporating the impact of ambient temperature into the risk assessment. This application further incorporates the cumulative damage index. Smoothing deterioration rate and Arrhenius thermal acceleration factor Converted to cumulative damage normalization respectively Damage rate normalization and excess heat acceleration normalization These normalized quantities are all mapped to a uniform interval of 0 to 1, ensuring their comparability in subsequent weighted summation. Finally, a weighted summation of these three normalized quantities is performed, and a cumulative damage evaluation coefficient is introduced. Damage deterioration rate evaluation coefficient and excess thermal acceleration evaluation coefficient A comprehensive risk warning value was obtained. This weighted fusion mechanism allows the system to be flexibly configured according to the importance of different risk factors. For example, in scenarios sensitive to rapid degradation, the damage rate can be given a higher weight. Through this mechanism, the proposed solution can comprehensively assess the dangerous state of the battery from three key dimensions: cumulative damage level, damage development speed, and environmental thermal acceleration effect. This provides more accurate, timely, and forward-looking early warning information than a single damage index, effectively avoiding misjudgments or omissions caused by the lag or one-sidedness of a single indicator, and significantly improving the safety and reliability of the high-temperature life test process.
[0174] The following is a concrete example. In practical applications, a high-performance digital signal processor (DSP) or embedded microcontroller (e.g., based on the ARM Cortex-M series) can be used to perform the above calculation process. This processor periodically obtains the latest electromechanical coupling equivalent cumulative damage index from the data acquisition module. and true surface temperature For smoothing the rate of deterioration For computation, the processor can maintain a circular buffer to store the most recent... Each sampling time Values and their corresponding sampling times When the new When a value arrives, the oldest data is replaced, and then the processor uses the data in the buffer to perform a first-order linear regression algorithm (e.g., based on least squares) to calculate the current slope as... At the same time, the processor will... Value, combined with pre-stored apparent activation energy Ideal gas constant and calibration reference temperature The Arrhenius thermal acceleration factor was calculated. Then, the processor will , and Substituting each into the corresponding normalization formula, we obtain... , and Finally, the processor compares these normalized values with pre-calibrated evaluation coefficients. , , (For example, by conducting statistical analysis or setting expert experience on a large amount of battery failure data, it can be determined that...) , , The weighted summation is performed to calculate the comprehensive risk warning value in real time. The entire calculation process can be completed within each sampling period, ensuring the real-time nature and effectiveness of the early warning values.
[0175] Through the above technical solution, this application overcomes the limitations of relying solely on the electromechanical coupling equivalent cumulative damage index for risk assessment. This solution not only considers the current degree of battery degradation but also introduces the dynamic impact of degradation trends (smoothing deterioration rate) and environmental factors (Arrhenius thermal acceleration factor) on risk. By normalizing and weightedly fusing this multi-dimensional information, a comprehensive hazard warning value is generated. This enables a more comprehensive and timely identification of potential failure risks during high-temperature life testing of lead-acid batteries, avoiding misjudgments caused by the lag or bias of a single indicator. Especially in high-temperature environments, this solution can effectively capture the accelerated degradation effect caused by temperature increases, thereby providing more proactive safety warnings and significantly improving the safety, reliability, and efficiency of the testing process.
[0176] Preferably, in S50, the security interruption control logic includes:
[0177] The smooth temperature rise rate is extracted by performing discrete-time least squares linear regression on the real surface temperature within a set surface temperature sliding time window.
[0178] The triggering condition for cutting off the charging and discharging circuit of the test battery is configured as a logical OR relationship of three independent parallel physical boundary conditions, specifically including: the comprehensive hazard warning value continuously exceeding the comprehensive hazard safety threshold in multiple consecutive samplings to achieve noise filtering; or the actual surface temperature instantaneously breaking down the temperature hard threshold set by the safety procedure; or the smooth temperature rise rate instantaneously breaking down the temperature rise rate hard threshold characterizing the critical slope of thermal runaway.
[0179] After the circuit is cut off, a safety interrupt latch state is triggered. The latch control is only released when the system receives a manual reset command and all three monitored variables spontaneously fall back to their respective reset safety thresholds.
[0180] Specifically, in S50, a duration of [duration missing] is used. A sliding time window for surface temperature is used to perform a first-order linear regression on the actual surface temperature, and the slope of the first-order linear regression is used as the smoothed temperature rise rate of the actual surface temperature.
[0181]
[0182]
[0183]
[0184] in, Sampling time The true surface temperature smooth temperature rise rate (in Kelvin per second). This is the duration of the surface temperature sliding time window (in seconds). This represents the number of sampling points within the surface temperature sliding time window. The first time within the surface temperature sliding time window The sampling time (in seconds) corresponding to each sampling point. This is the average value (in seconds) of the sampling time within the surface temperature sliding time window. For the first The actual surface temperature (in Kelvin) at each sampling point. This represents the average value of the actual surface temperature within the surface temperature sliding time window (in Kelvin).
[0185] In continuous Each sampling time satisfies Or at any sampling time, the following conditions are met. Or at any sampling time, the following conditions are met. At that time, the control test bench disconnects the charging and discharging circuits of the test battery;
[0186] in, The number of consecutive samples required to confirm the overall risk level exceeding the limit, and meeting the following requirements. , The comprehensive risk level safety threshold and meets the following requirements , This is the temperature hard threshold (in Kelvin). The temperature rise rate hard threshold (in Kelvin per second);
[0187] After the test bench disconnects the charging and discharging circuit, it remains in a safe interruption latch state until a manual reset command is received, provided that the actual surface temperature is lower than the preset reset temperature, the actual surface temperature smooth temperature rise rate is lower than the preset reset temperature rise rate threshold, and the comprehensive hazard warning value is lower than the preset reset hazard threshold.
[0188] The smooth temperature rise rate of the actual surface temperature is obtained by using a time period of... The technique employs a sliding time window for surface temperature, performing a first-order linear regression on the actual surface temperature and using the slope of the first-order linear regression as the smoothed temperature rise rate of the actual surface temperature. This technique aims to obtain the trend of actual surface temperature changes over time, i.e., the temperature rise rate, by processing the data. Since the original temperature data may contain instantaneous fluctuations or noise, directly calculating the instantaneous rate may not be stable enough. Therefore, using a sliding time window and first-order linear regression can effectively smooth the temperature data, resulting in a more representative and stable temperature rise rate. The introduction of the sliding time window allows the calculation to continuously track the latest temperature change trend, while the first-order linear regression fits the data points within the window using the least squares method. Its slope directly reflects the average rate of temperature change, thus filtering out high-frequency noise and providing a reliable smoothed temperature rise rate. For example, a fixed-size buffer can be set in the data acquisition module or host computer software. Each time new actual surface temperature data is acquired, the oldest data point is removed, and the new data point is added. Then, linear regression calculations are performed on the data in the buffer. Another approach is to utilize the mathematical processing unit built into a digital signal processor (DSP) or microcontroller (MCU) to execute the linear regression algorithm within the sliding window in real time to meet real-time requirements.
[0189] When any of the comprehensive hazard warning value, the actual surface temperature, or its rate of temperature rise reaches a corresponding preset threshold, the charging and discharging circuit is cut off and a safety interruption state is locked. This technical feature defines three independent and unaffected triggering conditions for immediate safety measures to be taken once a potential hazard is detected during the high-temperature life test of lead-acid batteries. The first condition is that the comprehensive hazard warning value continuously exceeds a certain threshold. The first condition is that the sampling time continuously exceeds a preset threshold, which avoids false triggering caused by instantaneous fluctuations and improves the robustness of the system. The second condition is that the actual surface temperature reaches the absolute upper limit, which directly addresses the potential overheating risk of the battery and provides a hard safety barrier. The third condition is that the smooth temperature rise rate of the actual surface temperature exceeds a preset threshold, which can serve as an early warning signal, intervening in time when the temperature has not yet reached the absolute upper limit but has shown a rapid upward trend to prevent thermal runaway. These conditions can be monitored and judged in real time by the test bench's control system. For example, the control system can be configured with multiple independent logic judgment modules, each responsible for monitoring one condition. Once any module judges that the condition is met, a safety interrupt is triggered.
[0190] After the test bench disconnects the charge / discharge circuit, it maintains a safety interruption latched state until a manual reset command is received, provided that the actual surface temperature is below the preset reset temperature, the smooth temperature rise rate of the actual surface temperature is below the preset reset temperature rise rate threshold, and the comprehensive hazard warning value is below the preset reset hazard threshold. This technical feature describes the direct intervention measures taken by the system after detecting a dangerous situation. Disconnecting the charge / discharge circuit is the most direct means to prevent further battery deterioration or danger. By physically disconnecting the power supply from the battery, energy input and output can be stopped immediately. Latching the safety interruption state ensures that the system will not automatically resume operation without manual intervention after a safety interruption is triggered, thus avoiding potential secondary hazards. For example, disconnecting the charge / discharge circuit can be achieved by controlling a high-power relay or solid-state contactor, which will immediately disconnect the circuit upon receiving a control signal. The latching of the safety interruption state can be achieved by setting a non-automatically reset flag in the control software or by designing a self-locking circuit at the hardware level, which can only be released after specific reset conditions are met and a manual command is received. This technical feature specifies stringent conditions for releasing the safety interruption latch, aiming to ensure that testing can only be restarted after both the battery and the test environment have returned to a safe state. These include three necessary conditions: First, a manual reset command must be received, emphasizing the importance of human verification; second, the actual surface temperature must be lower than the preset reset temperature, ensuring the battery body has been sufficiently cooled; and finally, the smooth temperature rise rate of the actual surface temperature and the comprehensive hazard warning value must also be lower than their respective preset reset thresholds, further confirming the stability of the battery state and the elimination of risk. Only when all three conditions are met simultaneously will the system allow the latch to be released. For example, the control system can integrate a human-machine interface through which the operator issues a reset command. After receiving the command, the system will check the outputs of the temperature sensor and risk assessment module in real time. Only when all safety indicators meet the reset requirements will the latch be released, allowing the charge / discharge circuit to reclose.
[0191] This application's solution, during the continuous monitoring of lead-acid battery high-temperature life test, not only conducts macro-risk assessment based on the electromechanical coupling equivalent cumulative damage index and comprehensive hazard warning value, but also further introduces direct, real-time monitoring of the battery's actual surface temperature and its smooth temperature rise rate. By employing a sliding time window to perform first-order linear regression on the actual surface temperature data, the smooth temperature rise rate of the battery can be accurately and stably calculated, effectively filtering out instantaneous noise and thus capturing the true trend of temperature changes. Regarding the safety judgment mechanism, this solution constructs a multi-layered protection system. When the comprehensive hazard warning value continuously exceeds a certain threshold... When a sampling time consistently exceeds a preset threshold, it indicates that the overall degradation risk of the battery has reached an unacceptable level, requiring intervention. Simultaneously, to address sudden or localized thermal risks, this solution also independently monitors the absolute value of the actual surface temperature. Once it reaches a preset temperature hard threshold, a safety interruption is immediately triggered regardless of the overall risk. Furthermore, for potential precursors to thermal runaway, this solution utilizes a calculated smooth temperature rise rate. Once this rate exceeds a preset temperature rise rate hard threshold, safety protection is immediately activated. This allows the system to respond to rapid temperature rise trends before the temperature reaches a dangerous absolute value, enabling earlier warning and intervention. Once any of the above safety conditions are triggered, the test bench immediately disconnects the battery's charging and discharging circuits and maintains the safety interruption state through a latching mechanism. This latching mechanism ensures that the system will not automatically resume operation until the danger is eliminated, thus avoiding secondary risks caused by misoperation or system instability. The safety interruption state is only lifted, allowing the test to restart, after the operator issues a clear manual reset command and the system confirms that the battery's actual surface temperature, smooth temperature rise rate, and overall danger warning value have all fallen below their respective preset safety reset thresholds. This rigorous reset logic ensures the safety and controllability of the testing process, effectively preventing the risk of thermal runaway of the battery in high-temperature testing environments and protecting the safety of testing equipment and personnel.
[0192] The following is a concrete example. In a high-temperature life test bench for lead-acid batteries, the control system continuously acquires the battery's actual surface temperature. To calculate the smooth temperature rise rate of the actual surface temperature, the control system can be configured with a microcontroller that internally maintains a circular buffer to store the most recent temperature data. A real surface temperature sampling point. For example, when When set to 60 and with a sampling period of 1 second, this buffer will store temperature data from the past minute. Whenever a new actual surface temperature is available... Upon entering the buffer, the oldest data point is removed, and then the microcontroller executes a first-order linear regression algorithm to calculate the smoothed temperature rise rate of the true surface temperature at the current moment. Simultaneously, the control system monitors three key parameters in real time: the comprehensive hazard warning value calculated using the above method. Real-time collected actual surface temperature And the smoothed temperature rise rate of the actual surface temperature just calculated. The system has preset corresponding safety thresholds, such as the comprehensive risk level safety threshold. Temperature hard threshold and temperature rise rate hard threshold The system will immediately trigger a safety interruption when it detects any of the following conditions: Comprehensive hazard warning value. In continuous Each sampling time (e.g.) All are greater than or equal to True surface temperature At any sampling time, greater than or equal to ; Smooth temperature rise rate of real surface temperature At any sampling time, greater than or equal to Once any condition is met, the control system immediately sends a disconnect command to the power relay connected to the charging / discharging circuit, opening the relay contacts and physically cutting off the battery's charging / discharging circuit. Simultaneously, a safety latch module within the control system is activated. This module sets a non-auto-reset flag and illuminates the "Safety Interruption" indicator on the test bench. In the safety interruption state, the charging / discharging circuit will not automatically close even if the external environment returns to normal. The safety latch module will only release its latch when the tester issues a "reset" command via the human-machine interface on the test bench, and the control system simultaneously confirms that the following three conditions are met: actual surface temperature... Below the preset reset temperature; smooth temperature rise rate based on actual surface temperature. Below the preset reset temperature rise rate threshold; comprehensive hazard warning value The threshold for reset risk is lower than the preset threshold. Only when all conditions are met will the system allow the power relay to close again and resume testing.
[0193] Through the above technical solution, this application significantly improves the safety and reliability of the monitoring method for high-temperature life testing of lead-acid batteries. By introducing the smooth temperature rise rate of the actual surface temperature as an independent monitoring indicator, the system can identify abnormal heating trends that may exist inside the battery earlier, thus intervening before the temperature reaches the critical value and effectively avoiding thermal runaway. Simultaneously, by combining the comprehensive hazard warning value, the absolute value of the actual surface temperature, and its temperature rise rate as conditions for triggering a safety interruption, a multi-layered and comprehensive safety assurance system is constructed. This not only addresses the long-term risks caused by overall battery degradation but also responds promptly to emergencies such as sudden local overheating or rapid temperature rise, greatly reducing the risk of battery damage or safety accidents during testing. Furthermore, the strict latching mechanism and multi-condition reset strategy ensure that the system will not be accidentally restored in an unsafe state after a safety interruption, further protecting the safety of the testing equipment and operators, enabling high-temperature life testing to be conducted in a more controllable and safer environment.
[0194] Preferably, before S10, an initialization calibration step is included. The initialization calibration and model parameter calibration are used to determine the fixed parameters and model-related parameters used in the calculation of the actual surface temperature, the calculation of the equivalent internal resistance under the reference working condition, the calculation of the equivalent deformation energy of the shell, the calculation of the equivalent cumulative damage of electromechanical coupling, and the calculation of the comprehensive hazard warning.
[0195] For lead-acid batteries with the same model, rated capacity, casing material and structure, temperature probe structure, test fixture structure, and main high-temperature life test conditions, after parameter calibration, the obtained parameters are stored in the corresponding battery model parameter table of the test bench controller or host computer, and directly called in the subsequent high-temperature life test of the same model of lead-acid battery; when the battery model, casing structure, temperature probe, test fixture, or main test conditions change in a way that affects the corresponding parameters, the affected parameters are recalibrated.
[0196] Initialize the calibration of the reference distance measurement values:
[0197] Place the test battery, which has not been charged or discharged, in a constant temperature test chamber to stabilize the ambient temperature of the test chamber at the calibrated reference temperature. The battery was then allowed to stand until it reached thermal equilibrium and mechanical stress stability. Under these conditions, multiple stable ranging values were continuously acquired from the non-contact displacement sensor, and the initial reference ranging value was determined according to the following formula: In the formula, This is used to initialize the reference distance value output by the non-contact displacement sensor under the reference state, in meters (m). For the first The distance measurement value corresponding to each stable sampling point is in meters; The total number of stable sampling points used in the calculation of the baseline ranging value; This refers to the sequence number of the stable ranging sampling point. Using the average of multiple stable ranging values as the reference ranging value can reduce the impact of random noise from the displacement sensor on the initial zero point.
[0198] Calibration of displacement direction conversion coefficient:
[0199] The displacement direction conversion coefficient satisfy: In the formula, The displacement direction conversion coefficient is determined based on the installation direction of the non-contact displacement sensor; -1 and +1 are used to adapt to different installation directions where the distance measurement value of the non-contact displacement sensor increases or decreases with the bulging movement of the battery casing. Maintaining the above initialization state, a known small displacement is artificially applied to the measured surface of the battery casing along its actual outer normal direction. The change in the distance measurement value of the non-contact displacement sensor is read, and the value is selected based on the aforementioned real-time signed normal displacement calculation relationship. The symbol is such that when the measured surface of the battery casing bulges outward along the outer normal direction, it satisfies the following: In the formula, for The real-time signed normal displacement of the measured surface of the battery casing relative to the initial reference position, in meters; This is the current sampling time, in seconds. The following condition applies when the measured surface of the battery casing moves in the direction opposite to its outer normal: In the formula, Still indicate The real-time signed normal displacement of the battery casing is measured in meters; a negative value indicates that the measured surface moves in the opposite direction to the outward bulge.
[0200] Calibration of the spring constant of the temperature probe preload spring:
[0201] Temperature probe preload spring coefficient The force-displacement calibration test was used. A temperature probe was installed in a high-precision micro-material testing machine or a precision displacement loading mechanism. Multiple known compressive displacements were sequentially applied within the linear elastic working range of the temperature probe's preload spring, and the reaction force corresponding to each compressive displacement was recorded simultaneously. First, the average value of each compressive displacement was calculated: In the formula, The arithmetic mean of the compressive displacements corresponding to all valid calibration points, in meters; For the first The spring compression displacement corresponding to each calibration point is expressed in meters. This represents the number of effective calibration points for the spring force-displacement test. Further calculation of the average reaction force at each calibration point is then performed. In the formula, The arithmetic mean of the reaction forces at all valid calibration points, in Newtons (N); For the first The spring reaction force measured at each calibration point, in Newtons; This represents the number of effective calibration points for the spring force-displacement test. The spring constant of the temperature probe preload spring is determined using the slope of a least-squares linear regression. .
[0202] Calibration of pre-compressed deformation:
[0203] The temperature probe is mounted on a high-precision micromaterial testing machine and slowly brought closer to the surface of a standard battery casing. When the contact force sensor output first stably exceeds the zero-point noise range, this position is determined as the initial contact position of the temperature probe. The probe is then moved further until it reaches the standard mechanical limit position specified by the test bench. The pre-compression deformation is determined according to the following formula: In the formula, The pre-compression deformation of the temperature probe under initial calibration conditions, in meters; This represents the travel position of the testing machine when the temperature probe is in the standard mechanical limit position, in meters. This is the travel distance at which the temperature probe just makes contact with the surface of the standard battery casing, expressed in meters.
[0204] Calibration of displacement transfer coefficient:
[0205] The real-time contact force between the aforementioned temperature probe and the battery casing will continue to be calculated according to the original model: When calibrating the displacement transfer coefficient, with the temperature probe in the standard installation position, a material testing machine is used to simulate the outward bulging of the battery casing, and multiple known normal displacement increments are applied sequentially. And simultaneously record the corresponding contact force increment. The average value of the normal displacement increment is: In the formula, This is the average of the normal displacement increments of all valid calibration points, in meters. For the first Each calibration point simulates the normal displacement increment generated by the outer bulge of the shell, in meters; The number of effective external drum displacement calibration points; This is the calibration point number. The average value of the corresponding contact force increment is: In the formula, This is the average value of the contact force increments at all valid calibration points, in Newtons. For the first The contact force increment corresponding to each normal displacement increment is expressed in Newtons. The number of valid calibration points; The calibration point number is used. The slope of the fit between the normal displacement increment and the contact force increment is obtained through least squares linear regression: In the formula, Let be the slope of the least-squares fit between the normal displacement increment and the contact force increment, in Newtons per meter. Based on the aforementioned contact force model: In the formula, The slope of the aforementioned force-displacement increment regression is expressed in N / m. The spring constant of the temperature probe preload spring is expressed in N / m. Let be the displacement transfer coefficient. Therefore: In the formula, This is the displacement transfer coefficient obtained from the final calibration.
[0206] Calibration of basic contact thermal conductivity, contact thermal conductivity-contact force calibration factor, and contact thermal conductivity nonlinearity index:
[0207] The equivalent contact thermal conductivity between the temperature probe and the battery casing continues to use the original model: A steady-state heat transfer calibration bench was constructed, consisting of a standard heat source, a temperature probe, a standard shell specimen, a mechanical loading mechanism, and a heat flux meter. With the temperature probe in its initial pre-compression state, a stable heat flux was applied through the standard heat source. After the system enters thermal steady state, measure the steady-state temperature difference between the temperature probe and the interface between the standard shell. The basic contact thermal conductivity is determined according to the following formula: In the formula, Based on basic contact thermal conductivity, the unit is W / K; The steady-state heat flux through the probe to the shell contact interface under the initial basic contact force condition is expressed in watts. This represents the steady-state temperature difference across the contact interface under this condition, expressed in Kelvin. Subsequently, multiple different contact forces are applied sequentially. And the steady-state heat transfer test was repeated under each contact force. The equivalent contact thermal conductivity corresponding to each contact force is: In the formula, For the first The equivalent contact thermal conductivity corresponding to each contact force calibration point is expressed in W / K. For the first The steady-state heat flux through the contact interface under contact force conditions, expressed in watts; The steady-state temperature difference between the two sides of the contact interface under this condition is expressed in Kelvin. This is the contact force calibration point number. Based on this, the following is established: In the formula, For the first A contact force calibration value, in Newtons; This represents the measured equivalent contact thermal conductivity corresponding to the contact force, in W / K. The total number of effective contact force calibration points participating in the nonlinear fitting of the contact thermal conduction-contact force relationship. Establish the nonlinear least squares objective function: In the formula, The objective function for the residual sum of squares calibrated for the parameters of the contact thermal conductivity model; The contact thermal conductivity-contact force calibration coefficient to be calibrated; The contact thermal conductivity nonlinearity index to be calibrated; For the first Measured equivalent contact thermal conductivity at each calibration point; The basic contact thermal conductivity has been determined; For the first Contact force at each calibration point; The number of valid calibration points; This refers to the calibration point number. The final parameters are determined according to the following formula: In the formula, The contact thermal conductivity-contact force calibration coefficient that minimizes the objective function of the residual sum of squares; This is the corresponding contact thermal conductivity nonlinearity index; This represents the combination of parameters that minimizes the objective function. Let be the aforementioned nonlinear least squares objective function. The parameter solution process satisfies: The aforementioned positive constraint is used to ensure that the contact thermal conductivity maintains a trend that conforms to the physical laws of contact heat transfer as the effective contact force increases.
[0208] Calibration of the lumped heat capacity of the temperature probe and the equivalent heat transfer constant of the environment:
[0209] Temperature probe lumped heat capacity It can be determined by the effective mass of the temperature probe's sensing end and the material's specific heat capacity at constant pressure: In the formula, The total heat capacity of the temperature probe is expressed in joules per Kelvin (J / K). The effective mass of the temperature probe's sensing end participating in the transient thermal response is expressed in kilograms (kg). This refers to the specific heat capacity at constant pressure of the corresponding material, expressed in joules per kilogram Kelvin. When the temperature probe's sensing end contains multiple main materials, the total lumped heat capacity can be determined according to the following formula: In the formula, This is the lumped heat capacity of the temperature probe, expressed in J / K. For the first The mass of the effective material, expressed in kg; For the first The specific heat capacity at constant pressure of the material, in units of ; The number of effective material types participating in the thermal response; This refers to the material serial number. The total heat capacity of the temperature probe can also be directly calibrated using a differential scanning calorimeter. Furthermore, the temperature probe is suspended in an environment where the temperature is constant. The temperature probe is placed inside the test chamber, ensuring that its measuring tip does not contact any solid surface. The temperature probe is then heated to its initial temperature using a standard heat source. The standard heat source was then removed, allowing the temperature probe to cool naturally within the test chamber. Under the aforementioned suspended boundary conditions, the temperature response of the temperature probe during natural cooling satisfies: In the formula, During the natural cooling process The apparent measured temperature output by the temperature probe at any given time, in Kelvin; The test chamber is used to measure the stable ambient temperature, measured in Kelvin. The initial apparent temperature measured by the instantaneous temperature probe after removing the standard heat source, in Kelvin; The equivalent heat transfer constant for heat dissipation from the temperature probe to the test chamber environment, expressed in W / K; This is the lumped heat capacity of the temperature probe, expressed in J / K. This represents the cooling time, expressed in seconds, calculated from the removal of the standard heat source. Take the natural logarithm of both sides of the above natural cooling relationship: In the formula, for The apparent temperature is measured by a time-lapse temperature probe. The ambient temperature of the test chamber; The equivalent heat transfer constant of the environment to be calibrated; The lumped heat capacity of the temperature probe has been determined; Cooling time; The initial temperature of the temperature probe at the moment natural cooling begins. For the first... Definition of each cooling sampling point: In the formula, For the first Logarithmic temperature difference corresponding to each cooling sampling point; For the first The apparent temperature measured by the temperature probe at each sampling time is in K; The ambient temperature is expressed in Kelvin (K). For the first The sampling time corresponding to each cooling sampling point is given in seconds. The slope is calculated using least squares linear regression.
[0210]
[0211] In the formula, The slope of the fitted straight line representing the logarithmic temperature difference over time is given by units of... ; For the first Sampling time for each cooling sampling point; This is the average of all cooling sampling times, in seconds; For the first The logarithmic temperature difference corresponding to each sampling point; This is the average of all logarithmic temperature differences; The number of effective sampling points participating in the linear fitting of the cooling process; This represents the sampling point number. According to the natural cooling model: In the formula, The slope of the logarithmic temperature difference-time fitted line, in units of .therefore: In the formula, The final calibrated equivalent heat transfer constant is given in W / K. After completing the above parameter calibration, the actual surface temperature will still be determined using the original model. .
[0212] Calibration of fixed additional resistance and pressure-contact resistance relationship:
[0213] Fixed additional resistance formed by measuring wires and acquisition channels Calibration was performed using a four-wire Kelvin connection. Without connecting the test battery, a low-resistance standard shorting piece was used to directly short-circuit the positive and negative test leads and the clamp terminals. Impedance measurements were performed using the same AC excitation frequency and amplitude as in the formal test. Multiple short-circuit impedance measurements were collected consecutively. In the formula, The fixed additional resistance formed by the measuring wires and the acquisition channel is measured in ohms (Ω). For the first The impedance value measured under substandard short-circuit conditions is expressed in ohms. To fix the additional resistance, repeat the measurement a certain number of times; This is the sequence number for repeated measurements. Furthermore, the real-time contact resistance between the test fixture and the battery terminals is determined using a pressure-contact resistance calibration method. Using the same fixture, battery terminal material, contact area, and contact surface treatment as the formal test, multiple clamping force calibration points are set within the normal clamping force range of the test fixture: In the formula, For the first The clamping force corresponding to each clamping force calibration point is expressed in Newtons. This represents the total number of clamping force calibration points. This is the index of the clamping force calibration point. Preferably, it satisfies: This constraint is used to ensure that the pressure-contact resistance relationship has a sufficient number of experimental data points. In the... Repeated measurements were performed at each clamping force calibration point using the four-wire Kelvin method. The secondary contact resistance, and its average additional contact resistance are: In the formula, For the first The average additional contact resistance corresponding to each clamping force condition is expressed in ohms. For the first Under the first clamping force condition, the first The additional contact resistance measured this time, in ohms; The number of repeated measurements for each clamping force calibration point; This is the sequence number of the repeated measurements. Therefore, the following is established: In the formula, For the first Each clamping force calibration value is in Newtons; The average contact resistance corresponding to this clamping force is expressed in ohms; c is the total number of clamping force calibration points. During formal testing, when the real-time clamping force satisfies: In the formula, for The real-time clamping force applied by the clamp to the battery terminals is constantly tested and measured in Newtons. and These are the two adjacent calibrated clamping forces on either side of the current real-time clamping force, both in Newtons. The real-time contact resistance is determined using piecewise linear interpolation. In the formula, for The real-time contact resistance between the fixture and the battery terminal is constantly tested, in ohms. and These are the average additional contact resistances corresponding to two adjacent clamping force calibration points, in ohms; after completing the above calibration, the internal resistance of the measurement circuit compensation continues to be calculated according to the original model: In the formula, for The internal resistance of the measurement circuit after removing the additional resistor from the measurement circuit is compensated, in ohms. This is the preset minimum effective internal resistance, in ohms. for The apparent AC internal resistance obtained at any time, in ohms; The fixed additional resistance formed by the measuring wires and the acquisition channel is measured in ohms. Additional resistance to the real-time contact formed between the test fixture and the battery terminal, measured in ohms; This indicates that the larger value is taken to prevent non-physical negative internal resistance from being generated by additional resistor compensation.
[0214] Calibration of internal resistance temperature correction factor and initial reference operating condition reference internal resistance:
[0215] Internal resistance temperature correction factor The internal resistance was determined using a multi-temperature steady-state internal resistance test combined with log-linear least squares regression. The lead-acid battery under test was placed at multiple stable temperature steps while in its initial calibration state and before substantial aging. After thermal equilibrium is reached, the corresponding measurement circuit compensation internal resistance is obtained. The original temperature-internal resistance relationship remains unchanged: In the formula, For the first The internal resistance of the measurement loop corresponding to each stable temperature step is expressed in ohms. The initial reference reference internal resistance at the calibration reference temperature under initialization conditions, in ohms; This is the internal resistance temperature correction factor, expressed as the reciprocal of Kelvin, i.e. ; For the first The absolute temperature corresponding to each stable temperature step is expressed in K. To calibrate the reference temperature, the unit is K. Take the natural logarithm of both sides of the above relationship: , This is the initial reference operating condition internal resistance. Definition: In the formula, For the first The temperature deviation of each temperature step relative to the calibrated reference temperature, expressed in Kelvin (K). Further definition: In the formula, For the first The natural logarithmic value of the internal resistance of the measurement loop compensation corresponding to each temperature step. Therefore, the above relationship can be written as: In the formula, To fit the intercept of the straight line; To fit the slope of the straight line, in units of .in: .at the same time: Multiple temperature steps The average value is: In the formula, This is the average temperature deviation across all temperature steps, expressed in K. This refers to the number of effective temperature steps involved in calibrating the internal resistance temperature correction factor. The corresponding... The average value is: The slope of the least squares fit is: .therefore: During the formal testing process, the equivalent internal resistance under the reference operating condition will continue to use the original formula: Under the initial calibration state, the following conditions must be met: In the formula, Initialization time The corresponding actual surface temperature of the battery casing, in Kelvin (K). Therefore: In the formula, The initial reference internal resistance under initial calibration conditions, in ohms; The equivalent internal resistance of the reference operating condition after conversion to the calibrated reference temperature at the initialization time is expressed in ohms. The internal resistance of the measurement loop at the initialization moment is compensated, and the unit is ohms.
[0216] Calibration of shell reference equivalent stiffness and temperature softening correction factor:
[0217] Prepare several casing specimens with the same casing material, thickness, geometry, and boundary constraints as the test battery. Test at the reference calibration temperature. A universal testing machine was used to apply a normal load to the test area of the shell, and multiple sets of load-displacement data were obtained in the linear elastic stage. The average normal displacement is: In the formula, This represents the average normal displacement of each effective loading point during the linear elastic stage, in meters. For the first The normal displacement corresponding to each loading point, in meters; This represents the number of effective loading points in the linear elastic stage. The average normal load is: In the formula, The average value of the normal load at all effective loading points, in Newtons; For the first The normal load corresponding to each loading point is expressed in Newtons. This represents the number of effective loading points. The shell reference equivalent stiffness at the calibration reference temperature is: In the formula, For calibrating reference temperature The shell's baseline equivalent stiffness is given, in N / m. The original shell equivalent stiffness temperature correction model remains unchanged: In the formula, for The equivalent stiffness of the shell after temperature correction at any time, in N / m; The minimum effective equivalent stiffness is expressed in N / m. The reference equivalent stiffness of the shell at the calibrated reference temperature is expressed in N / m. This is the temperature softening correction factor for the equivalent stiffness of the shell, in units of... ; for Real-time battery casing surface temperature, in Kelvin (K). The reference temperature is measured in Kelvin (K). This is achieved across multiple stable high-temperature steps. Repeated force-displacement tests were conducted on the lower shell to obtain the corresponding equivalent stiffness. ,definition: In the formula, For the first The temperature difference between each temperature step and the calibrated reference temperature is expressed in K. For the first The absolute temperature corresponding to each stable temperature step (the temperature value of the shell specimen after reaching thermal equilibrium under preset temperature conditions), in K; The reference temperature is measured in Kelvin (K).
[0218] Further definition: In the formula, For the first Each temperature step corresponds to the ratio between the shell's equivalent stiffness and the reference equivalent stiffness; For the first The measured equivalent stiffness of the shell at each temperature step is expressed in N / m.
[0219] Based on the original temperature correction model: In the formula, For the first Normalized shell stiffness at a high-temperature calibration point; This is the softening correction factor for the temperature to be calibrated, in units of... ; The corresponding temperature deviation is expressed in Kelvin (K). The temperature softening correction factor is obtained according to the following formula:
[0220]
[0221] In the formula, The final calibrated shell equivalent stiffness temperature softening correction factor, in units of... ; For the first The temperature difference between the calibrated temperature and the reference temperature; To correspond to the normalized shell stiffness; The number of effective temperature calibration points participating in the temperature softening fitting.
[0222] Calibrating the minimum effective equivalent stiffness and critical equivalent deformation energy:
[0223] Multiple shell specimens were placed in a preset extreme high-temperature softening state, and small-load normal loading tests were conducted without structural failure. The residual equivalent stiffness of each shell specimen was obtained. In the formula, For the first The residual equivalent stiffness of each shell specimen under extreme high temperature softening state is expressed in N / m. This refers to the number of shell specimens participating in the extreme softening stiffness test. The minimum effective equivalent stiffness is determined conservatively as follows: In the formula, The minimum effective equivalent stiffness is expressed in N / m. to These represent the residual equivalent stiffness of each shell specimen measured under extreme high-temperature softening conditions.
[0224] The critical equivalent deformation energy is calibrated by destructive hydrostatic test, pneumatic test or ultimate mechanical loading test.
[0225] Under the same or equivalent boundary constraints as the formal test, the load is gradually increased until the shell first exhibits irreversible plastic yielding, microcracks, seal failure, or other predetermined structural failure states. For the first... For each shell specimen, the strain energy absorbed before failure was calculated using discrete load-displacement data and a trapezoidal summation method. In the formula, The critical equivalent deformation energy is the first occurrence of the preset structural failure in the j-th shell specimen, in joules (J). and Each of the adjacent numbers The and the first Normal load at each loading point, in Newtons; and These represent the normal displacements of the corresponding loading points, in meters. To achieve the predetermined number of effective load-displacement intervals before structural failure, for multiple shell specimens, the final critical equivalent deformation energy can be conservatively determined as follows: In the formula, The critical equivalent deformation energy used for subsequent mechanical degradation component calculations, in joules; For the first The critical equivalent deformation energy measured for a shell specimen; This represents the minimum critical deformation energy among all effective shell specimens. The equivalent deformation energy of the shell still uses the original model: In the formula, for The equivalent deformation energy of the battery casing under the current boundary constraints at any given moment is expressed in joules. for The equivalent stiffness of the shell after temperature correction at any time, in N / m; for The positive outward bulge displacement of the battery casing along the outer normal direction at any given moment is measured in meters. This positive outward bulge displacement is still calculated using the original formula: .
[0226] Damage model and definitions of parameters to be calibrated:
[0227] The electrochemical degradation component continues to use the original model: In the formula, Sampling time The corresponding electrochemical degradation component; Sampling time The corresponding reference operating condition equivalent internal resistance, in ohms; The initial reference internal resistance under initial calibration conditions, in ohms; For the first Each damage calculation sampling time.
[0228] The mechanical degradation component continues to use the original model: In the formula, Sampling time The corresponding mechanical degradation component; Sampling time The corresponding equivalent deformation energy of the shell, in joules; The critical equivalent deformation energy is obtained through destructive shell testing, and the unit is joules.
[0229] The instantaneous damage state quantity still follows the original formula: And satisfy: In the formula, The electrochemical degradation sensitivity index; This is the mechanical degradation sensitivity index; both parameters are limited to positive values to ensure that the instantaneous damage state quantity does not decrease in the opposite direction when the corresponding degradation component increases.
[0230] The electromechanical coupling equivalent cumulative damage index continues to use the original discrete update model: Its initial conditions remain the same: , The electromechanical coupling equivalent cumulative damage index at the initialization moment; This indicates the start time for damage accumulation calculation; 0 indicates that the cumulative damage baseline is initialized to zero at the start of the test.
[0231] Determination of the true cumulative damage:
[0232] The actual cumulative damage amount described in this application is used as a sensitivity index for electrochemical degradation. Mechanical deterioration sensitivity index and damage accumulation reference time constant It provides offline calibration targets and instantaneous physical quantities that need to be directly measured by individual sensors during informal online monitoring.
[0233] For the Only the battery is calibrated, and its initial actual capacity is obtained under uniform capacity testing conditions before the start of the full life test. And determine the corresponding termination capacity according to the preset lifespan termination criterion. During the full lifespan test, capacity testing is performed at preset intervals, at specific times. Obtain actual capacity .
[0234] The actual cumulative damage is calculated using the following formula: In the formula, For the first Only calibrate the battery at the calibration time The actual cumulative damage amount; For the first Only the initial actual capacity before the start of battery testing is calibrated, in ampere-hours (Ah). For the first Only the battery is calibrated at the time. The actual capacity measured under the unified capacity testing conditions is expressed in Ah. For the first Only the termination capacity corresponding to the preset end-of-life condition of the battery is specified, in Ah; For the first The time corresponding to each lifetime calibration node; A bounded truncation operator for the interval from zero to one. The bounded truncation operator is defined as: In the formula, This is the original calculated value before bounded truncation. When: In the formula, This represents the current actual capacity. This represents the initial actual capacity; their equality indicates that no lifetime loss, as characterized by capacity decay, has yet occurred. At this point: In the formula, This represents the actual cumulative damage; 0 indicates the initial lifetime state. When: In the formula, This represents the current actual capacity. This represents the end-of-life capacity; if both are equal, it indicates that the battery has reached the preset end-of-life condition. At this point: In the formula, The value represents the actual cumulative damage; 1 indicates that the preset end-of-life state has been reached. The joint calibration of the electrochemical degradation sensitivity index, mechanical degradation sensitivity index, and damage accumulation reference time constant is crucial for the first... Only the battery is calibrated, in the first Each capacity damage calibration node expands the original discrete damage update model from its initial state to obtain the model's calculated cumulative damage amount: In the formula, For the first Only the battery is calibrated in the first The model calculates the cumulative damage for each calibration node; For the first Only the battery is calibrated in the first The electrochemical degradation component corresponding to each sampling time; To correspond to the mechanical degradation component; The electrochemical degradation sensitivity index is to be calibrated; The mechanical degradation sensitivity index to be calibrated; The time interval between adjacent damage sampling times, in seconds; Here, represents the cumulative reference time constant for the damage to be calibrated, in seconds. It should be noted that the above formula is based on the original discrete recursive relationship... The equivalent expansion under the given conditions does not change the original electromechanical coupling equivalent cumulative damage model. The objective function for calculating the sum of squared residuals between the damage quantity and the actual cumulative damage quantity is established as follows: In the formula, The objective function is the sum of squared residuals jointly calibrated for the damage model parameters; The reference time constant for the cumulative damage to be calibrated; The electrochemical degradation sensitivity index is to be calibrated; The mechanical degradation sensitivity index to be calibrated; The number of lead-acid batteries of the same model participating in the joint calibration; For the first Only the number of effective capacity impairment calibration nodes included in the battery is calibrated; The cumulative damage amount calculated by the model; This represents the actual cumulative damage amount obtained through actual capacity decay; To calibrate the battery serial number; The lifetime calibration node number is determined. Finally, the three parameters are determined jointly according to the following formula: In the formula, The final calibrated reference time constant for damage accumulation, in seconds; The final calibrated electrochemical degradation sensitivity index; The final calibrated mechanical degradation sensitivity index; The objective function is jointly calibrated for the aforementioned parameters; This indicates the search for a combination of parameters that minimizes the objective function. The parameters satisfy: In the formula, This is the reference time constant for damage accumulation; The electrochemical degradation sensitivity index; The mechanical degradation sensitivity index is defined; all three parameters are constrained to positive values. The solution can be obtained using the trust region reflection algorithm, Gauss-Newton algorithm, or other nonlinear least squares algorithms capable of handling positive constraints. After calibration, [the following steps will be taken]. , and It is stored in the parameter table of the same model battery and can be directly called during formal online testing.
[0235] Calibration of apparent activation energy:
[0236] Apparent activation energy Calibration was performed using high-temperature side reaction tests at multiple stable temperatures. While maintaining consistency in the test battery's state of charge, charge / discharge regime, and other key test conditions, calibration was conducted at multiple stable temperatures. The high-temperature side reaction calibration test was then conducted. The standardized capacity loss rate under a given temperature condition is defined as: In the formula, For the first Standardized capacity loss rate under a given temperature condition, in units of ; For the first The actual capacity measured at the beginning of each temperature calibration cycle, in Ah; The actual capacity measured at the end of the temperature calibration cycle, in Ah; For the first The duration of each high-temperature calibration cycle is in seconds. This represents the temperature calibration point number. The capacity loss rate is related to the absolute temperature using the Arrhenius relation: In the formula, For temperature Standardized capacity loss rate, in units of ; The Arrhenius apparent frequency factor, its unit is... Consistent; The apparent activation energy to be calibrated is expressed in joules per mole (J / mol). The ideal gas constant is expressed in joules per mole Kelvin, i.e. ; For the first The absolute temperature of each calibration test is given in Kelvin. Both ends are taken as the natural logarithm. In the formula, For the first Standardized capacity loss rate under a given temperature condition; It is the apparent frequency factor; It is the apparent activation energy; It is the ideal gas constant; Absolute temperature. Definition: In the formula, For the first The reciprocal of the absolute temperature of each temperature calibration point, in units of ; For the first An absolute temperature calibration value, in Kelvin (K). Definition: In the formula, For the first The natural logarithm of the standardized capacity loss rate corresponds to each calibration temperature; To correspond to the standardized capacity loss rate, the least squares method is used to obtain... about The fitted slope: In the formula, for about The least squares fit slope, in units of K; For the first The reciprocal of the calibration temperature; This is the average of the reciprocals of all temperatures; For the first The natural logarithm of the standardized capacity loss rate; For all The average value; To determine the number of effective high-temperature side reaction calibration temperature points; This refers to the calibration temperature point number. Based on: In the formula, represents the slope of the Arrhenius linear fit, in k; Apparent activation energy, expressed in J / mol; is the ideal gas constant, with units of . .therefore: In the formula, The apparent activation energy obtained from the final calibration is expressed in J / mol. The slope of the aforementioned least squares fit is expressed in K. is the ideal gas constant, with units of . In the formal calculations, the Arrhenius thermal acceleration factor continues to follow the original formula: .
[0237] Determination of the time constant for damage sliding window and hazard rate assessment characteristics:
[0238] The smooth deterioration rate of the electromechanical coupling equivalent cumulative damage index continues to be calculated using the original least squares linear regression method within the damage sliding time window: In the formula, The current sampling time The corresponding electromechanical coupling equivalent cumulative damage exponent smooth deterioration rate, in units of ; This represents the number of valid sampling points contained within the damage sliding time window. Within the damage sliding time window, the first The sampling time corresponding to each sampling point is in seconds; This is the average of all sampling times within the damage sliding time window, in seconds; For the first The electromechanical coupling equivalent cumulative damage index corresponding to each sampling time; This represents the average value of the electromechanical coupling equivalent cumulative damage index within the damage sliding time window. This represents the sampling point number within the sliding window. Where: In the formula, This represents the average sampling time within the damage sliding time window, in seconds. For the first The sampling time corresponding to each damage sampling point is in seconds; This represents the number of sampling points within the damage sliding time window. This refers to the sampling point number. And: In the formula, This represents the average value of the electromechanical coupling equivalent cumulative damage index within the damage sliding time window; For the first The electromechanical coupling equivalent cumulative damage index corresponding to each damage sampling point; This represents the number of sampling points within the damage sliding time window. The damage rate normalization still uses the original model: Extract samples of positively smoothed degradation rates during the critical deterioration phase in the later stages of battery life from data of calibrated batteries of the same model that have completed full-life testing. Preferably, the actual cumulative damage amount satisfies: In the formula, This represents the actual cumulative damage corresponding to the current lifespan stage; 0.8 is the example critical stage starting value used to define the remaining 20% of the lifespan stage. The historical calibration sampling time must also satisfy: In the formula, The smoothed deterioration rate at the current historical sampling moment, in units of A value greater than 0 indicates that the electromechanical coupling equivalent cumulative damage index is increasing. The median of the positive deterioration rates across all hazardous stages is taken as the reference hazardous deterioration rate. In the formula, For reference to the rate of danger deterioration, the unit is... ; For the first The smoothed deterioration rate corresponding to each historical sample of a dangerous stage, in units of ; This represents the statistical median of the rates for all valid hazardous stages. To correspond to historical sampling times, the intermediate response value of the damage rate normalization corresponding to the reference hazard deterioration rate is specified as follows: In the formula, is the damage rate normalization factor, dimensionless; 0.5 represents the intermediate response position of the bounded normalization function. Substituting into the original model: In the formula, 0.5 is the preset intermediate response value; The time constant for evaluating the hazard rate to be determined is in seconds. For reference to the rate of danger deterioration, the unit is... Therefore, we can conclude that: In the formula, The time constant for the final determined hazard rate evaluation characteristics, in seconds; The reference hazard deterioration rate (e.g., average value) is determined from historical full-life test data, in units of... .
[0239] Calibration of the comprehensive risk assessment coefficient:
[0240] The normalized cumulative damage continues to be calculated using the original formula: The normalized excess heat acceleration continues to use the original formula: The overall risk warning value will continue to use the original formula: The three evaluation coefficients satisfy: In the formula, , and These are the cumulative damage evaluation coefficient, the damage deterioration rate evaluation coefficient, and the excess thermal acceleration evaluation coefficient, respectively; the non-negativity constraint is used to prevent a reverse risk contribution when any risk factor increases. Simultaneously satisfying: For the first For calibrated batteries that have completed full lifecycle high-temperature life testing, the proportion of lifecycle progress corresponding to historical sampling moments is defined as the target hazard level benchmark: In the formula, For the first Only calibrate the battery at the historical sampling time. The corresponding target hazard level benchmark; The cumulative test time, in seconds, is the time from the start of the battery's full life test to the current historical calibration node. For the first Only the total effective time, in seconds, is specified from the start of the test until the battery reaches the preset critical failure or end-of-life conditions. To calibrate the battery serial number; This is used to assign the historical node sequence number. The corresponding historical time points are calculated synchronously. , and Establish the objective function for evaluating coefficient calibration: In the formula, The objective function for the sum of squared residuals calibrated by the comprehensive risk assessment coefficients; The number of historical full-life batteries of the same model used in the evaluation coefficient calibration; For the first Only the number of valid calibration nodes included in the historically calibrated battery; For the first Only the battery in the first The target hazard benchmark corresponding to each historical calibration node; This corresponds to the normalized amount of cumulative damage; This is the normalized value corresponding to the damage rate; To correspond to the normalized amount of excess thermal acceleration; , and There are three evaluation coefficients to be calibrated; To calibrate the battery serial number; Assign historical node numbers. Finally, obtain three evaluation coefficients according to the following formula: In the formula, The cumulative damage evaluation coefficient obtained from the final calibration; The final calibrated evaluation coefficient for the rate of damage deterioration; The final calibrated excess thermal acceleration evaluation coefficient; The objective function is the sum of squared residuals of the evaluation coefficients; This represents the combination of evaluation coefficients that minimizes the objective function. During the solution process, the aforementioned non-negativity constraints and the sum-to-1 constraint must continue to be satisfied. The solution can be obtained using a least-squares optimization algorithm with equality and inequality constraints, or the interior-point method.
[0241] Determining the reset temperature:
[0242] After confirming that the test battery is in a normal, stable, high-temperature test state, continuously acquire... A sample of real surface temperatures. The average real surface temperature under normal steady-state conditions is: In the formula, The average surface temperature during the normal and stable testing phase is expressed in Kelvin (K). For the first The actual surface temperature corresponding to each steady-state sampling moment, in K; This represents the number of temperature samples used in the statistics under normal, stable conditions. The standard deviation of the true surface temperature is: In the formula, The sample standard deviation of the true surface temperature under normal and stable test conditions is expressed in K. For the first The true surface temperature in a stable state; This represents the average actual surface temperature during the normal and stable testing phase. This represents the number of temperature samples included in the statistics under normal steady-state conditions. Temperature reset hysteresis is selected. In the formula, The temperature hysteresis amount set between the temperature safety trigger threshold and the reset threshold, in K; The standard deviation of the true surface temperature under normal steady-state conditions is expressed in Kelvin; the coefficient 3 indicates that at least three times the steady-state statistical fluctuation is used as the minimum hysteresis margin. The reset temperature is determined according to the following formula: In the formula, Reset temperature, in Kelvin (K). The temperature hard threshold in the safety interrupt logic, in K; This represents the temperature reset hysteresis, expressed in K.
[0243] Determination of the reset temperature rise rate threshold:
[0244] The actual surface temperature smoothing rate of rise continues to be calculated using a first-order linear regression within the aforementioned surface temperature sliding time window: In the formula, The current sampling time The corresponding smooth temperature rise rate of the actual surface temperature, in K / s; This represents the number of sampling points included within the surface temperature sliding time window. For the first The sampling time corresponding to each temperature sampling point is in seconds; This is the average value of all sampling times within the surface temperature sliding time window, in seconds; For the first The actual surface temperature corresponding to each sampling point, in K; This represents the average of all real surface temperatures within the surface temperature sliding time window, in Kelvin (K). This represents the current calculation time. Multiple smooth temperature rise rate samples were obtained under normal, stable operating conditions, and their average values were calculated. In the formula, The average smooth temperature rise rate of the real surface temperature under normal steady-state conditions, in K / s; For the first The smoothed temperature rise rate corresponding to each steady-state sampling point is expressed in K / s. This represents the number of valid steady-state samples used for statistical analysis. The corresponding standard deviation is: In the formula, The sample standard deviation of the smoothed temperature rise rate under normal steady-state conditions is expressed in K / s. For the first A sample with a smooth temperature rise rate; The average value of the smoothed temperature rise rate; This represents the number of valid samples.
[0245] Temperature rise rate reset hysteresis satisfies: In the formula, This is the temperature rise rate reset hysteresis, in K / s; The standard deviation of the smoothed temperature rise rate under normal steady-state conditions is given in K / s. The reset temperature rise rate threshold is: In the formula, This is the reset temperature rise rate threshold, in K / s. This is the hard threshold for the rate of temperature rise in the safety interrupt logic, measured in K / s. This represents the reset hysteresis of the temperature rise rate, expressed in K / s.
[0246] Determination of the repositioning risk threshold:
[0247] Under normal and stable testing conditions, continuously acquire comprehensive risk warning values. The average value is: In the formula This represents the average value of the comprehensive risk warning value under normal and stable conditions. For the first The comprehensive risk warning value at each stable state sampling time; This represents the number of valid steady-state samples used in hazard statistics. Its standard deviation is: In the formula, This represents the sample standard deviation of the comprehensive risk warning value under normal and stable conditions. For the first A sample of comprehensive risk levels in a stable state; This represents the average overall risk level. The effective sample size. The hazard reset hysteresis satisfies: In the formula, The hysteresis is calculated based on the overall risk level. This represents the standard deviation of the overall hazard warning value under normal and stable conditions. The reset hazard threshold is determined according to the following formula: In the formula, To reset the risk threshold; The overall risk level is the safety threshold. This represents the hysteresis amount for risk level reset.
[0248] Therefore, the following should be satisfied: , Temperature hard threshold These are physical constants and do not require experimental calibration.
[0249] A monitoring device for high-temperature life testing of lead-acid batteries, employing the aforementioned monitoring method for high-temperature life testing of lead-acid batteries.
[0250] It should be noted that, in this document, relational terms such as "first" and "second" are used only to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus.
[0251] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.
Claims
1. A monitoring method for high-temperature life testing of lead-acid batteries, characterized in that, include: S10. Obtain the apparent measurement temperature of the temperature probe, the real-time signed normal displacement of the battery casing of the non-contact displacement sensor, and the ambient temperature, compensate for probe contact and thermal errors, and obtain the true surface temperature. S20. Under the preset state of charge, resting time and AC excitation, obtain the apparent AC internal resistance, remove the additional resistance of the measurement circuit and convert it to the calibrated reference temperature in combination with the real surface temperature to obtain the reference working condition equivalent internal resistance. S30. Calculate the electrochemical degradation component based on the change of equivalent internal resistance, extract the positive displacement to obtain the positive outward bulging displacement, combine the temperature-corrected stiffness to calculate the shell's equivalent deformation energy and mechanical degradation component, couple the two to obtain the instantaneous damage state quantity, and update it to the electromechanical coupling equivalent cumulative damage index. S40. Calculate the smooth deterioration rate of the index based on the window regression slope, and calculate the Arrhenius excess thermal acceleration. Normalize and sum the two with the electromechanical coupling equivalent cumulative damage index to obtain the comprehensive risk warning value. S50. Calculate the smooth temperature rise rate of the actual surface temperature. When the comprehensive hazard warning value, the actual surface temperature, or the temperature rise rate of any of them reaches the corresponding preset threshold, cut off the charging and discharging circuit and lock the safety interruption state.
2. The monitoring method for high-temperature life testing of lead-acid batteries according to claim 1, characterized in that, In step S10, the calculation process for the real-time signed normal displacement and actual surface temperature of the battery casing includes: The calculation process for the real-time signed normal displacement and true surface temperature of the battery casing includes: The real-time signed normal displacement is constructed based on the deviation between the real-time ranging value and the initial reference ranging value of the non-contact displacement sensor. Geometric constraints are imposed by introducing a displacement direction conversion coefficient bound to the sensor installation direction, and the trend of the measured surface of the battery casing moving towards the probe along the outer normal is uniformly mapped as a positive displacement. The real-time contact force between the temperature probe and the battery casing is obtained by mapping the pre-compression deformation of the probe and the real-time signed normal displacement scaled by the displacement transfer coefficient. An equivalent contact thermal conductivity is constructed between the probe and the battery casing. This equivalent contact thermal conductivity is composed of the base contact thermal conductivity under the reference state and the contact mechanical compensation term. The contact mechanical compensation term is driven by the real-time contact force and modulated by the nonlinear heat transfer relationship through the nonlinear index of the contact thermal conductivity. The true surface temperature is extracted from the apparent measured temperature based on the lumped dynamic thermal equilibrium relationship. The extraction process includes compensating for dynamic thermal inertia error terms and environmental heat dissipation error terms in the apparent measured temperature. The dynamic thermal inertia error term is jointly constrained by the lumped heat capacity of the temperature probe, the rate of change of the apparent measured temperature, and the equivalent contact thermal conductivity. The environmental heat dissipation error term is driven by the temperature difference between the apparent measured temperature and the ambient temperature, and is jointly constrained by the equivalent heat transfer constant and equivalent contact thermal conductivity of the temperature probe dissipating heat to the environment. In the calculation, a strictly positive physical boundary constraint is applied to the mechanical compression of the probe to eliminate contact thermal conductivity singularities and thermal break failures that may occur in the contact thermodynamic calculation.
3. The monitoring method for high-temperature life testing of lead-acid batteries according to claim 2, characterized in that, The apparent rate of temperature change is obtained by performing discrete-time least squares linear regression within a set temperature sliding time window. The rate of change corresponds to the slope of the first-order linear regression, which is obtained by normalizing the ratio of the time-temperature covariance within the sliding window to the time variance within the same window.
4. The monitoring method for high-temperature life testing of lead-acid batteries according to claim 3, characterized in that, In step S20, the calculation process of the equivalent internal resistance under the reference operating condition includes: The fixed additional resistance of the measuring leads and the real-time contact additional resistance between the test fixture and the terminal are stripped from the acquired apparent AC internal resistance to obtain the measurement circuit compensation internal resistance; and a minimum effective internal resistance lower bound constraint is applied in the stripping operation to prevent negative resistance physical distortion caused by contact resistance fluctuations. An exponential thermal compensation mapping relationship is constructed to map the internal resistance of the measurement loop to a unified calibration reference temperature to obtain the equivalent internal resistance under reference operating conditions. The thermal compensation mapping relationship is driven by the deviation of the actual surface temperature from the calibration reference temperature and is modulated by the internal resistance temperature correction coefficient of the battery system.
5. The monitoring method for high-temperature life testing of lead-acid batteries according to claim 4, characterized in that, In step S30, the calculation process for the equivalent deformation energy of the shell includes: A non-negative truncation operator is applied to the real-time signed normal displacement to extract the positive outward bulging displacement, thus shielding the interference of the battery casing's inward shrinkage on the mechanical degradation assessment. An equivalent stiffness of the shell penalized by the temperature softening effect is constructed. This stiffness is based on the benchmark equivalent stiffness at the reference temperature. A degradation reduction term dominated by the product of the actual temperature rise and the temperature softening correction coefficient is introduced. In the reduction calculation, a minimum effective equivalent stiffness lower bound constraint is applied to the shell equivalent stiffness to prevent the stiffness matrix from becoming singular at extreme high temperatures, which would lead to divergence in the deformation energy calculation. Based on the physical constitutive relation of secondary strain energy, the equivalent deformation energy of the battery casing under the current boundary constraints is calculated by multiplying the temperature-corrected equivalent stiffness of the casing with the square of the positive outward bulging displacement.
6. The monitoring method for high-temperature life testing of lead-acid batteries according to claim 5, characterized in that, In step S30, the calculation process of the electromechanical coupling equivalent cumulative damage index includes: The positive relative drift of the equivalent internal resistance under the reference operating condition relative to the initial reference operating condition reference internal resistance is defined as the electrochemical degradation component, and a zero-point bottoming constraint is applied to filter out internal resistance recovery artifacts: The ratio of the shell's equivalent deformation energy to the structure's critical equivalent deformation energy is defined as the mechanical degradation component. A multidimensional geometric coupling mechanism is constructed, which multiplies the electrochemical degradation component, which has been subjected to exponential sensitivity modulation by the electrochemical degradation sensitivity index and the mechanical degradation sensitivity index, with the mechanical degradation component, and maps the instantaneous damage state quantity after stripping the steady-state reference. A Markov state update equation in the discrete time domain is established, and the damage index of the previous time step is iteratively accumulated according to the damage increment of the current sampling period. The damage increment is driven by the instantaneous damage state quantity and is transformed by rate scaling through the damage accumulation reference time constant and the sampling time interval, thereby outputting the electromechanical coupling equivalent cumulative damage index.
7. The monitoring method for high-temperature life testing of lead-acid batteries according to claim 6, characterized in that, In S40, the smoothing deterioration rate is obtained by performing discrete-time least squares linear regression on the electromechanical coupling equivalent cumulative damage index within a set damage sliding time window; its rate corresponds to the slope of the first-order linear regression, and its value is obtained by performing a ratio normalization operation on the time-damage covariance within the sliding window and the time variance within the same window.
8. The monitoring method for high-temperature life testing of lead-acid batteries according to claim 7, characterized in that, In step S40, the calculation process of the comprehensive risk warning value includes: Based on the thermodynamic reaction kinetic constitutive model, the reciprocal difference between the actual surface temperature and the calibrated reference temperature is used as the driving potential. Under the constraint of the ratio of apparent activation energy to ideal gas constant, the exponential acceleration factor of the thermodynamic reaction is calculated, and the excess part is extracted to obtain the Arrhenius excess thermal acceleration. A bounded rational fractional mapping function is constructed to nonlinearly map the electromechanical coupling equivalent cumulative damage exponent, the positive cutoff of the smooth deterioration rate, and the Arrhenius excess thermal acceleration to a dimensionless probability space of zero to one, generating the cumulative damage normalization, damage rate normalization, and excess thermal acceleration normalization. For the mapping of the rate term, a dimensionality elimination process is performed by introducing a characteristic time constant of the danger rate evaluation. Based on the principle of convex combination weighted synthesis, the three normalized quantities are linearly summed and projected using a group of strictly non-negative weight coefficients with a sum of one, thereby outputting the comprehensive risk warning value that dynamically converges to the interval between zero and one.
9. The monitoring method for high-temperature life testing of lead-acid batteries according to claim 8, characterized in that, In S50, the security interruption control logic includes The smooth temperature rise rate is extracted by performing discrete-time least squares linear regression on the real surface temperature within a set surface temperature sliding time window. The triggering condition for cutting off the charging and discharging circuit of the test battery is configured as a logical OR relationship of three independent parallel physical boundary conditions, specifically including: the comprehensive hazard warning value continuously exceeding the comprehensive hazard safety threshold in multiple consecutive samplings to achieve noise filtering; or the actual surface temperature instantaneously breaking down the temperature hard threshold set by the safety procedure; or the smooth temperature rise rate instantaneously breaking down the temperature rise rate hard threshold characterizing the critical slope of thermal runaway. After the circuit is cut off, a safety interrupt latch state is triggered. The latch control is only released when the system receives a manual reset command and all three monitored variables spontaneously fall back below their respective reset safety thresholds.
10. A monitoring device for high-temperature life testing of lead-acid batteries, characterized in that, The monitoring method for high-temperature life testing of lead-acid batteries as described in any one of claims 1-9 is adopted.