Semiconductor devices and their fabrication methods, semiconductor packaging structures, electronic devices
By doping the drift layer of a silicon carbide substrate with aluminum and nitrogen, the problem of reduced carrier lifetime in silicon carbide semiconductor devices was solved, the breakdown voltage and dynamic performance of the devices were improved, the on-resistance was reduced, and the overall performance of the devices was enhanced.
Patent Information
- Application Number
- CN202510599600.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-09
- Publication Date
- 2026-11-10
AI Technical Summary
Silicon carbide semiconductor devices experience reduced carrier lifetime under high voltage, leading to decreased device performance and shortened short-circuit withstand time. Existing treatment methods are either costly or ineffective.
Aluminum and nitrogen are co-doped in the drift layer of a silicon carbide substrate. Nitrogen fills carbon vacancies, and the compensation effect of aluminum and nitrogen maintains a low net doping concentration, thereby optimizing the breakdown voltage and on-resistance and improving the electric field distribution.
It improves carrier lifetime, enhances device breakdown voltage and dynamic performance, reduces on-resistance, and improves overall device performance.
Smart Images

Figure CN123075979A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of semiconductor technology, and in particular to a semiconductor device and its fabrication method, a semiconductor packaging structure, and an electronic device. Background Technology
[0002] With the development of technology, silicon carbide (SiC) semiconductor materials, due to their physical properties such as wide bandgap, high critical electric field strength, high electron saturation migration rate, and high thermal conductivity, have broad application prospects in the fields of high voltage, high power, high frequency, and high temperature resistant electronic power devices.
[0003] In high-voltage power devices, carbon vacancy defects are formed during the homoepitaxial growth of silicon carbide (SiC), introducing deep-level defects. These deep-level defects become recombination centers for charge carriers, reducing the carrier lifetime of the SiC epitaxial layer and hindering effective conduction modulation. Low carrier lifetime is highly detrimental to high-voltage power devices, significantly increasing on-state resistance and power consumption. Furthermore, SiC power devices exhibit poorer short-circuit robustness compared to silicon devices, with their short-circuit withstand time further shortened under high voltage.
[0004] Therefore, how to increase carrier lifetime and improve the performance of silicon carbide power devices is an urgent problem to be solved. Summary of the Invention
[0005] This application provides a semiconductor device and its fabrication method, a semiconductor packaging structure, and an electronic device, which can increase the carrier lifetime in the silicon carbide epitaxial layer and improve the performance of silicon carbide power devices.
[0006] In a first aspect, embodiments of this application provide a semiconductor device, the device comprising a silicon carbide substrate and a buffer layer and a first drift layer stacked on the silicon carbide substrate; the first drift layer is doped with aluminum and nitrogen; the first drift layer includes a first doped region and a second doped region stacked on top of each other, wherein the doping concentration of nitrogen in the first doped region is greater than or equal to the doping concentration of nitrogen in the second doped region, the doping concentration of aluminum in the first doped region is greater than or equal to the doping concentration of aluminum in the second doped region, and the net doping concentration of the first doped region and the second doped region are the same.
[0007] In current silicon carbide power devices, carbon vacancy defects are formed during the homoepitaxial growth process, resulting in deep-level defects that reduce carrier lifetime and affect device performance. To address this, this application provides a semiconductor device in which a first drift layer stacked on a silicon carbide substrate is co-doped with aluminum and nitrogen. Nitrogen can fill carbon vacancies in the silicon carbide material, reducing deep-level defects and improving carrier lifetime. Furthermore, by simultaneously introducing aluminum and nitrogen into the drift layer, the compensation effect of aluminum and nitrogen allows for the introduction of more nitrogen to fill carbon vacancies while maintaining a low net doping concentration in the first drift layer (i.e., the nitrogen doping concentration minus the aluminum doping concentration). Moreover, when the aluminum and nitrogen doping concentrations in the first doping region are greater than those in the second doping region, this alternating light and heavy doping can synergistically optimize breakdown voltage and on-resistance, improve electric field distribution, and enhance dynamic performance. For example, the first doped region and the second doped region can also be periodically stacked, which is not specifically limited in this application.
[0008] In some possible implementations, the ratio of aluminum doping concentration to nitrogen doping concentration in any doped region of the first drift layer is greater than or equal to 0.1 and less than 1.
[0009] In this embodiment, the nitrogen doping concentration in the first drift layer is greater than the aluminum doping concentration, so that the first drift layer is N-type doped. Furthermore, the ratio of aluminum doping concentration to nitrogen doping concentration is greater than or equal to 0.1 and less than 1, which ensures that the doped first drift layer maintains a low net doping concentration, widens the depletion region, and improves the device's breakdown voltage. Additionally, by controlling the compensation degree, the resistivity of the drift layer can be precisely adjusted, avoiding the problem of excessively high on-resistance in pure N-type doping (where the nitrogen doping ratio is too high).
[0010] In some possible implementations, the thickness of the first drift layer in the direction perpendicular to the substrate is greater than 0.1 micrometers and less than or equal to 200 micrometers.
[0011] In this embodiment, the thickness of the first drift layer can be determined based on the electrical performance and requirements of the device. For example, it can be between 0.1 and 1 micrometer. A larger thickness results in a slower switching speed, while a smaller thickness makes the device more susceptible to breakdown. Therefore, it can be flexibly adjusted according to the electrical performance and requirements of the device, and this embodiment does not impose specific limitations on this.
[0012] In some possible implementations, the net doping concentration of the first drift layer is 1 × 10⁻⁶. 14 cm -3 Up to 1×10 17cm -3 between.
[0013] In this embodiment, the net doping concentration of the first drift layer is 1×10⁻⁶. 14 cm -3 Up to 1×10 17 cm -3 Between 1×10⁻⁶. That is, the net doping concentration of both the first and second doped regions is between 1×10⁻⁶. 14 cm -3 Up to 1×10 17 cm -3 The first drift layer is kept lightly doped, allowing it to withstand high voltage, expand the depletion region of the device, and improve the breakdown voltage. The net doping concentration can be modulated directly by adjusting the flow rates of the aluminum and nitrogen dopant source gases, without introducing changes to other epitaxial process parameters, thus avoiding any impact on epitaxial process control, especially defect density control.
[0014] In some possible implementations, the device further includes a second drift layer disposed between the buffer layer and the first drift layer, wherein the doping concentration in the second drift layer is the same as the net doping concentration in the first drift layer.
[0015] In this embodiment of the application, the semiconductor device further includes a second drift layer with the same net doping concentration as the first drift layer. This multilayer drift layer structure can further improve the breakdown voltage of the device and improve device performance.
[0016] In some possible implementations, the device further includes a collector layer disposed between the silicon carbide substrate and the buffer layer.
[0017] In this embodiment, the semiconductor device can be applied to bipolar power devices, and a collector layer can be provided between the substrate and the buffer layer to connect the voltage, which increases the flexibility of the semiconductor device.
[0018] In some possible implementations, the aforementioned semiconductor device is a unipolar power device or a bipolar power device.
[0019] In the embodiments of this application, the semiconductor device can be a unipolar power device, such as a Schottky barrier diode (SBD), a metal-oxide-semiconductor field-effect transistor (MOSFET), and a junction field-effect transistor (JFET). It can also be a bipolar power device, such as a bipolar junction transistor (BJT), an insulated-gate bipolar transistor (IGBT), and a gate turn-off thyristor (GTO).
[0020] Secondly, embodiments of this application provide a method for fabricating a semiconductor device. The method includes: providing a silicon carbide substrate; forming a buffer layer and a first drift layer on the silicon carbide substrate, wherein the first drift layer is doped with aluminum and nitrogen; the first drift layer includes a first doped region and a second doped region stacked thereon, wherein the nitrogen doping concentration in the first doped region is greater than or equal to the nitrogen doping concentration in the second doped region, the aluminum doping concentration in the first doped region is greater than or equal to the aluminum doping concentration in the second doped region, and the net doping concentrations of the first doped region and the second doped region are the same.
[0021] In this embodiment, the co-doping of aluminum and nitrogen allows nitrogen to fill carbon vacancies, reducing deep-level defects and improving carrier lifetime. Simultaneously, the compensation effect of aluminum and nitrogen maintains a low net doping concentration. Furthermore, this alternating light and heavy doping can synergistically optimize breakdown voltage and on-resistance, improve electric field distribution, and enhance dynamic performance. Most importantly, the co-doping of aluminum and nitrogen can be directly achieved by changing the flow rate of the doping source gas, without introducing changes to other epitaxial process parameters. This avoids impacting epitaxial process control, especially defect density control. Moreover, this method does not introduce additional post-processing, thus saving costs and improving production efficiency.
[0022] Thirdly, embodiments of this application provide a semiconductor packaging structure, which includes a packaging substrate and any one of the semiconductor devices provided in the first aspect, wherein the packaging substrate is electrically connected to the semiconductor device.
[0023] Fourthly, embodiments of this application provide an electronic device, which includes a circuit board and the semiconductor packaging structure provided in the third aspect, wherein the circuit board is electrically connected to the semiconductor packaging structure.
[0024] It should be understood that the method for preparing the semiconductor device provided in the second aspect of this application and the electronic device provided in the third aspect are consistent with the technical solution of the first aspect of this application. Their specific contents and beneficial effects can be referred to the semiconductor device provided in the first aspect above, and will not be repeated here. Attached Figure Description
[0025] To more clearly illustrate the technical solutions in the embodiments of this application or the background art, the accompanying drawings used in the embodiments of this application or the background art will be described below.
[0026] Figure 1 This is a schematic diagram of the structure of a semiconductor device provided in an embodiment of this application.
[0027] Figure 2 This is a schematic diagram of the doping concentration of a semiconductor device provided in an embodiment of this application.
[0028] Figure 3 This is a schematic diagram of the doping concentration of another semiconductor device provided in an embodiment of this application.
[0029] Figure 4 This is a schematic diagram of another semiconductor device provided in an embodiment of this application.
[0030] Figure 5 This is a schematic diagram of the structure of another semiconductor device provided in the embodiments of this application.
[0031] Figure 6 This is a schematic diagram of the doping concentration of another semiconductor device provided in the embodiments of this application.
[0032] Figure 7 This is a schematic diagram of the structure of another semiconductor device provided in the embodiments of this application.
[0033] Figure 8 This is a schematic diagram of the doping concentration of another semiconductor device provided in the embodiments of this application.
[0034] Figure 9 This is a schematic diagram of the structure of another semiconductor device provided in the embodiments of this application.
[0035] Figure 10 This is a comparative schematic diagram provided in an embodiment of this application.
[0036] Figure 11 This is a schematic diagram of a process for fabricating a semiconductor device provided in an embodiment of this application.
[0037] Figure label:
[0038] 101 Silicon carbide substrate, 102 Buffer layer, 103 First drift layer, 104 Second drift layer, 105 Collector layer;
[0039] 1031 is the first doped region, and 1032 is the doped region. Detailed Implementation
[0040] The embodiments of this application will now be described with reference to the accompanying drawings.
[0041] The terms "first" and "second," etc., in the specification, claims, and accompanying drawings of this application are used to distinguish different objects, not to describe a specific order. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover non-exclusive inclusion. For example, a process, method, system, product, or apparatus that includes a series of steps or units is not limited to the listed steps or units, but may optionally include steps or units not listed, or may optionally include other steps or units inherent to such processes, methods, products, or apparatus.
[0042] It should be understood that in this application, "at least one (item)" means one or more, and "more than" means two or more. "And / or" is used to describe the relationship between related objects, indicating that three relationships can exist. For example, "A and / or B" can represent three cases: only A exists, only B exists, and both A and B exist simultaneously, where A and B can be singular or plural. The character " / " generally indicates that the preceding and following related objects are in an "or" relationship. "At least one (item) of the following" or similar expressions refer to any combination of these items, including any combination of single or plural items. For example, at least one (item) of a, b, or c can represent: a, b, c, "a and b", "a and c", "b and c", or "a and b and c", where a, b, and c can be single or multiple.
[0043] For ease of description, embodiments of this application may use spatial relation terms such as "below," "below," "lower than," "below," "above," "upper," etc., to describe the relationship between an element or feature shown in the accompanying drawings and other elements or features. It will be understood that these spatial relation terms are intended to include orientations of the device in use or operation other than those depicted in the drawings. For example, if the device in the drawings is flipped, the orientation of an element described as "below," "below," or "below" other elements or features will change to "above" said other elements or features. Thus, the exemplary terms "below" and "below" can encompass both up and down directions. The device may also have other orientations (rotated 90 degrees or in other orientations), and therefore the spatial relation descriptors used herein should be interpreted accordingly. Furthermore, it will be understood that when a layer is referred to as being "between" two layers, it can be the only layer between the two layers, or there may be one or more layers in between.
[0044] In this document, the term "embodiment" means that a particular feature, structure, or characteristic described in connection with an embodiment may be included in at least one embodiment of this application. The appearance of this phrase in various places throughout the specification does not necessarily refer to the same embodiment, nor is it a separate or alternative embodiment mutually exclusive with other embodiments. It will be explicitly and implicitly understood by those skilled in the art that the embodiments described herein can be combined with other embodiments.
[0045] First, to facilitate understanding of the embodiments of this application, the following detailed analysis addresses the technical problems to be solved and the applicable application scenarios of the embodiments of this application.
[0046] With the development of technology, silicon carbide (SiC) semiconductor materials, due to their physical properties such as wide bandgap, high critical electric field strength, high electron saturation migration rate, and high thermal conductivity, have broad application prospects in the fields of high voltage, high power, high frequency, and high temperature resistant electronic power devices.
[0047] In high-voltage power devices, carbon vacancy defects are formed during the homoepitaxial growth of silicon carbide (SiC), introducing deep-level defects. These deep-level defects become recombination centers for charge carriers, reducing the carrier lifetime of the epitaxial layer and hindering effective conductance modulation. Low carrier lifetime is highly detrimental to high-voltage power devices, significantly increasing on-state resistance and power consumption. Furthermore, SiC power devices exhibit poorer short-circuit robustness compared to silicon devices; that is, under the same experimental conditions, SiC power devices have shorter short-circuit withstand times, which are further reduced under high voltage.
[0048] Currently, the main method used is to reduce the deep-level defect density and improve the carrier lifetime by performing post-processing on silicon carbide epitaxial wafers. Among these methods, there are two main approaches: carbon implantation combined with high-temperature annealing and long-term high-temperature oxidation combined with high-temperature annealing.
[0049] One method, carbon implantation combined with high-temperature annealing, involves implanting carbon ions into a silicon carbide epitaxial wafer and then annealing it in an inert atmosphere (such as Ar) to promote the occupancy of vacancies by implanted carbon atoms, restore lattice integrity, and eliminate implantation damage. However, high-energy carbon ion implantation can easily introduce new defects; furthermore, the effect is not ideal for thick silicon carbide epitaxy due to the limitation of carbon implantation depth.
[0050] For high-temperature oxidation combined with high-temperature annealing, the silicon carbide surface needs to be oxidized at high temperatures for an extended period (several hours to tens of hours, or even 48 hours) in an oxygen or humid oxygen atmosphere. This oxidation process fills vacancies with oxygen atoms, and the diffusion and recombination of silicon and carbon during oxidation can repair near-surface lattice distortions, appropriately increasing carrier lifetime. However, this significantly increases time and economic costs. Furthermore, high-temperature oxidation may cause free carbon (C clusters) to precipitate from silicon carbide, forming new defect sources, and due to depth limitations, the results are not ideal.
[0051] To address this, and to fill carbon vacancy defects formed during homoepitaxial growth of silicon carbide, reduce deep-level defects, and improve carrier lifetime, this application provides a semiconductor device in which a first drift layer stacked on a silicon carbide substrate is co-doped with aluminum and nitrogen. Nitrogen can be used to fill carbon vacancies, reduce deep-level defects, and improve carrier lifetime. Furthermore, by simultaneously introducing aluminum and nitrogen into the drift layer, the compensation effect of aluminum and nitrogen allows for the introduction of more nitrogen to fill carbon vacancies while maintaining a low net doping concentration in the first drift layer (i.e., the nitrogen doping concentration minus the aluminum doping concentration). Due to the compensation effect, the more nitrogen doped, the more aluminum doped is required. However, excessive aluminum can also increase the on-state resistance of the device due to defects. Therefore, compared to maintaining a consistently high doping concentration of aluminum and nitrogen, the doping concentration of aluminum and nitrogen can be reduced in the second doping region while still ensuring sufficient nitrogen to fill carbon vacancies. Furthermore, this alternation of light and heavy doping can synergistically optimize breakdown voltage and on-resistance, improve electric field distribution, and enhance dynamic performance. The structural configuration of this semiconductor device can also be found in the description of the following embodiments.
[0052] Based on the technical problems mentioned above, and in order to facilitate understanding of the embodiments of this application, several semiconductor devices on which the embodiments of this application are based will be described below.
[0053] This application provides a semiconductor device including a silicon carbide substrate and a buffer layer and a first drift layer stacked on the silicon carbide substrate; the first drift layer is doped with aluminum and nitrogen; the first drift layer includes a first doped region and a second doped region stacked on top of each other, wherein the nitrogen doping concentration in the first doped region is greater than or equal to the nitrogen doping concentration in the second doped region, the aluminum doping concentration in the first doped region is greater than or equal to the aluminum doping concentration in the second doped region, and the net doping concentrations of the first doped region and the second doped region are the same.
[0054] Please refer to the attached document. Figure 1 , Figure 1 This is a schematic diagram of the structure of a semiconductor device provided in an embodiment of this application.
[0055] like Figure 1 As shown in (1) and (2), the semiconductor device includes a silicon carbide substrate 101 and a buffer layer 102 and a first drift layer 103 stacked on the silicon carbide substrate 101. The first drift layer 103 includes at least a first doped region 1031 and a second doped region 1032 stacked on top of each other.
[0056] The specific locations of the first doped region 1031 and the second doped region 1032 are not limited in this embodiment. For example, Figure 1 As shown in (1), the first doped region 1031 is disposed on the side of the buffer layer 102 away from the silicon carbide substrate 101, and the second doped region 1032 is disposed on the side of the first doped region 1031 away from the buffer layer 102; or, as shown in (1), Figure 1 As shown in (2), the second doped region 1032 is disposed on the side of the buffer layer 102 away from the silicon carbide substrate 101, and the first doped region 1031 is disposed on the side of the second doped region 1032 away from the buffer layer 102.
[0057] It should be noted that in the embodiments of this application and the following related embodiments, the plane parallel to the surface of the silicon carbide substrate 101 and parallel to the plane ... Figure 1 The left-right direction shown is the X-axis direction. The Y-axis direction is defined as the direction parallel to the surface of the silicon carbide substrate 101 and perpendicular to the X-axis direction, i.e., as shown... Figure 1 The front-back direction is shown. The Z-axis direction is defined as the direction perpendicular to the surface of the silicon carbide substrate 101, i.e., as shown... Figure 1 The vertical direction is shown. The X-axis, Y-axis, and Z-axis are all perpendicular to each other.
[0058] It should also be noted that the embodiments of this application only illustrate a portion of the structure of the semiconductor device, and the embodiments of this application do not impose specific limitations on the specific structure of the semiconductor device. For example, a barrier layer, a well layer, etc., may also be provided on the side of the first drift layer 103 away from the silicon carbide substrate 101 in the semiconductor device (the above structures are not illustrated).
[0059] The thickness of the buffer layer 102 in the direction perpendicular to the silicon carbide substrate 101 can be between 0.1 micrometers and 10 micrometers, and can be adaptively adjusted according to device requirements.
[0060] It is understood that the embodiments of this application and the following related embodiments are applicable to epitaxial structures formed of silicon carbide material, that is, by way of example, the substrate can be an N-type conductive SiC substrate. The buffer layer can be an N-type SiC epitaxial layer, and the doping element is N. The first drift layer can also be an N-type SiC epitaxial layer, and the embodiments of this application do not specifically limit this.
[0061] In addition, the first drift layer 103 is doped with aluminum and nitrogen; wherein, the nitrogen doping concentration in the first doped region 1031 of the first drift layer 103 is greater than or equal to the nitrogen doping concentration in the second doped region 1032, the aluminum doping concentration in the first doped region 1031 is greater than or equal to the aluminum doping concentration in the second doped region 1032, and the net doping concentrations of the first doped region 1031 and the second doped region 1032 are the same.
[0062] Here, the net doping concentration refers to the difference between the doping concentrations of aluminum and nitrogen. (Based on the above...) Figure 1 For example, please refer to the appendix for the structure shown in (2). Figure 2 , Figure 2 This is a schematic diagram illustrating the doping concentration of a semiconductor device provided in an embodiment of this application. For example... Figure 2 As shown, the buffer layer 102 is an N-type heavily doped N-type material. N * For example, it can be greater than 1×10 19 cm -3 The second doped region 1032 is doped with aluminum and nitrogen, with a net doping concentration of N. N-AL Nitrogen doping concentration N N Subtract aluminum doping concentration N AL It should be noted that in the embodiments of this application, both the buffer layer 102 and the first drift layer 103 are N-type doped. Therefore, in the first drift layer 103, the nitrogen doping concentration N N Greater than the aluminum doping concentration N AL .
[0063] like Figure 2As shown, the nitrogen doping concentration in the first doping region 1031 is greater than that in the second doping region 1032. Correspondingly, the aluminum doping concentration in the first doping region 1031 is greater than that in the second doping region 1032. Therefore, the net doping concentrations of the first doping region 1031 and the second doping region 1032 can be kept the same.
[0064] Additionally, please refer to the appendix. Figure 3 , Figure 3 This is a schematic diagram showing the doping concentration of another semiconductor device provided in an embodiment of this application. For example... Figure 3 As shown, the nitrogen doping concentration in the first doping region 1031 can be equal to the nitrogen doping concentration in the second doping region 1032. Correspondingly, the aluminum doping concentration in the first doping region 1031 can be equal to the aluminum doping concentration in the second doping region 1032. This ensures that the net doping concentrations of the first doping region 1031 and the second doping region 1032 are the same.
[0065] It should be noted that, considering the differences in doping process flow and equipment, the net doping concentrations mentioned in the above embodiments and the following related embodiments, when they are the same or consistent, can be considered to be approximately the same, not completely equal net doping concentrations. Due to the influence of various factors such as the doping process flow and process, the net doping concentrations of the first doping region 1031 and the second doping region 1032 can fluctuate reasonably within a certain range. This application embodiment does not make specific limitations on this.
[0066] In some embodiments, the ratio of the aluminum doping concentration to the nitrogen doping concentration in any doped region of the first drift layer is greater than or equal to 0.1 and less than 1.
[0067] Understandably, a high nitrogen doping concentration is required to fill sufficient carbon vacancies. However, to avoid excessively high nitrogen doping concentrations affecting device performance, the compensation effect of aluminum and nitrogen can be utilized in the first drift layer to maintain a low doping concentration. Therefore, the ratio of aluminum to nitrogen doping concentration in any doped region of the first drift layer 103 (e.g., the first doped region 1031 and the aforementioned second doped region 1032) can be greater than or equal to 0.1 and less than 1. This allows the doped first drift layer to maintain a low net doping concentration, widening the depletion region and improving the device's breakdown voltage. Furthermore, by controlling the compensation degree, the resistivity of the drift layer can be precisely adjusted, avoiding the problem of excessively high on-resistance in pure N-type doping (where the nitrogen doping ratio is too high).
[0068] In some embodiments, the net doping concentration of the first drift layer is 1×10⁻⁶. 14 cm-3 Up to 1×10 17 cm -3 between.
[0069] Understandably, maintaining a low net doping concentration in the first drift layer can improve the device's breakdown voltage. Therefore, the net doping concentration of the first drift layer can be maintained at 1×10⁻⁶. 14 cm -3 Up to 1×10 17 cm -3 Between. That is, the net doping concentration of both the first doped region 1031 and the second doped region 1032 is between 1×10. 14 cm -3 Up to 1×10 17 cm -3 Between these parameters, it can withstand high voltage, expand the depletion region of the device, and improve the breakdown voltage. The modulation of the net doping concentration can be directly achieved through the flow rate of the aluminum and nitrogen doping source gas streams, without introducing changes in other epitaxial process parameters, thus avoiding the impact on epitaxial process control, especially defect density control.
[0070] In some embodiments, the thickness of the first drift layer in the direction perpendicular to the substrate is greater than 0.1 micrometers and less than or equal to 200 micrometers.
[0071] The thickness of the first drift layer 103 can be determined according to the electrical performance and requirements of the device. For example, it can be between 0.1 and 1 micrometer. A larger thickness results in a slower switching speed, while a smaller thickness makes the device more susceptible to breakdown. Therefore, it can be flexibly adjusted according to the electrical performance and requirements of the device; this embodiment does not impose specific limitations on this.
[0072] In addition, in some other embodiments, the first doped region 1031 and the second doped region 1032 of the first drift layer 103 can also be periodically repeated.
[0073] Based on the above Figure 1 For example, please refer to the attached diagram. Figure 4 , Figure 4 This is a schematic diagram of another semiconductor device provided in an embodiment of this application.
[0074] like Figure 4As shown in (1) and (2), the first doped region 1031 and the second doped region 1032 can be periodically repeated. This alternation of light and heavy doping in the first and second doped regions 1031 and 1032 can synergistically optimize breakdown voltage and on-resistance, improve electric field distribution, and enhance dynamic performance. It should be noted that the total thickness of the first drift layer 103 is greater than 0.1 micrometers and less than or equal to 200 micrometers. Therefore, the number of repetitions of the first doped region 1031 and the second doped region 1032 can be determined according to the circuit design requirements and fabrication process.
[0075] In some embodiments, the device further includes a second drift layer disposed between the buffer layer and the first drift layer, wherein the doping concentration in the second drift layer is the same as the net doping concentration in the first drift layer.
[0076] Based on the above Figure 1 For example, please refer to the attached diagram. Figure 5 , Figure 5 This is a schematic diagram of the structure of another semiconductor device provided in the embodiments of this application.
[0077] like Figure 5 As shown in (1) and (2), the semiconductor device also includes a second drift layer 104 with the same net doping concentration as the first drift layer 103, for example: in 1×10 14 cm -3 Up to 1×10 17 cm -3 The second drift layer 104 is N-type doped, and can be doped with only nitrogen, or with both aluminum and nitrogen. This embodiment does not specifically limit this. The second drift layer 104 is disposed between the buffer layer 102 and the first drift layer 103. This multi-layer drift layer structure can further improve the device's breakdown voltage and enhance device performance.
[0078] Please refer to the attached document. Figure 6 , Figure 6 This is a schematic diagram illustrating the doping concentration of another semiconductor device provided in an embodiment of this application. For example... Figure 6 As shown, based on the above Figure 4 In the structure shown in (2), the doping type of the second drift layer 104 is N-type, which can contain only nitrogen doping, but the nitrogen doping concentration is the same as the net doping concentration in the first drift layer.
[0079] It should be noted that if the doped regions of the first drift layer are periodically set, please refer to the appendix. Figure 7 and Figure 8 , Figure 7 This is a schematic diagram of the structure of another semiconductor device provided in the embodiments of this application. Figure 8 This is a schematic diagram illustrating the doping concentration of another semiconductor device provided in an embodiment of this application. For example... Figure 7 As shown above, Figure 5 Taking the structure shown in (2) as an example, a first doped region 1031 and a second doped region 1032 can be periodically set on the side of the second drift layer 104 away from the buffer layer 102. Figure 8 As shown, the second drift layer 104 is N-type doped, and can contain nitrogen doping, with the nitrogen doping concentration being the same as the net doping concentration in the first drift layer 103. Correspondingly, when the net doping concentration is the same, the aluminum and nitrogen doping concentrations in the first doped region 1031 and the second doped region 1032 of the first drift layer 103 are different.
[0080] In some other embodiments, the second drift layer 104 may also be disposed on the side of the first drift layer 103 away from the buffer layer 102, which is not specifically limited in this embodiment.
[0081] The thickness of the second drift layer 104 in the direction perpendicular to the silicon carbide substrate 101 can be between 0 micrometers and 200 micrometers, and can be adaptively adjusted according to device requirements. This application embodiment does not make specific limitations on this.
[0082] In some embodiments, the device further includes a collector layer disposed between the silicon carbide substrate and the buffer layer.
[0083] Figure 9 This is a schematic diagram of the structure of another semiconductor device provided in the embodiments of this application, such as... Figure 9 As shown above, Figure 5 Taking the structures shown in (1) and (2) as examples, this semiconductor device can be applied to bipolar power devices. Correspondingly, a collector layer 105 can also be provided between the silicon carbide substrate 101 and the buffer layer 102 to connect the voltage, which increases the flexibility of the semiconductor device.
[0084] In some embodiments, the semiconductor device described above is a unipolar power device or a bipolar power device.
[0085] It is understandable that the semiconductor device can be a unipolar power device, such as a Schottky Barrier Diode (SBD), a Metal Oxide Semiconductor Field Effect Transistor (MOSFET), and a Junction Field-Effect Transistor (JFET). The semiconductor device can also be a bipolar power device, such as a Bipolar Junction Transistor (BJT), an Insulated Gate Bipolar Transistor (IGBT), and a Gate Turn-Off Thyristor (GTO).
[0086] It should be noted that the doping type of the silicon carbide substrate 101 in this embodiment of the application does not specifically limit the type of doping, and can be adaptively adjusted according to the type of device. For example, when it is a bipolar power device, the silicon carbide substrate 101 can be P-type doped; when it is a unipolar power device, the silicon carbide substrate 101 can be N-type doped.
[0087] Additionally, please refer to the appendix. Figure 10 , Figure 10 This is a comparative schematic diagram provided in an embodiment of this application, such as... Figure 10As shown in the diagram, a simplified illustration compares the changes in carrier lifetime in silicon carbide when aluminum and nitrogen are not co-doped in the first drift layer, and when aluminum and nitrogen are co-doped in the first drift layer, in the prior art. The carrier distribution diagram shows that before co-doping, high-lifetime carriers tend to concentrate in the central region of the silicon carbide epitaxial wafer, while the carrier lifetime in the peripheral region is generally lower, easily leading to uneven electric field distribution and affecting device performance. After co-doping, the distribution of high and low lifetime carriers is more uniform, resulting in a more uniform electric field distribution and improved device performance. The bar chart and distribution curve respectively statistically analyze the carrier lifetime and related proportions in silicon carbide before and after co-doping. Based on the above figures, in undoped silicon carbide, the average lifetime of charge carriers is approximately 428.58 ns, the median is approximately 462.38 ns, and the deviation is approximately 40.348% (the distribution of charge carriers with the same lifetime is relatively concentrated), with the lifetime range mostly concentrated between 154-600 ns. In codoped silicon carbide, the average lifetime of charge carriers is approximately 3004.6 ns (an improvement of about 7 times compared to before codoping), the median is approximately 2511.9 ns, and the deviation is approximately 82.647% (the distribution of charge carriers with the same lifetime is more dispersed, which is beneficial to improving device lifetime), with the lifetime range mostly concentrated between 794-5559 ns, and some charge carriers even have extremely high values of over 10000 ns.
[0088] It should be noted that the above Figure 10 The data shown is only a simple example. Since the doping concentrations of aluminum and nitrogen are different during co-doping, the data will also change. Therefore, this application does not impose specific limitations on this.
[0089] Therefore, this application provides a semiconductor device in which a first drift layer stacked on a silicon carbide substrate is co-doped with aluminum and nitrogen. Nitrogen can be used to fill carbon vacancies, reduce deep-level defects, and improve carrier lifetime. Furthermore, by simultaneously introducing aluminum and nitrogen into the drift layer, the compensation effect of aluminum and nitrogen allows for the introduction of more nitrogen to fill carbon vacancies while maintaining a low net doping concentration in the first drift layer (i.e., the nitrogen doping concentration minus the aluminum doping concentration). Moreover, when the aluminum and nitrogen doping concentrations in the first doping region are greater than those in the second doping region, this alternation of light and heavy doping can synergistically optimize breakdown voltage and on-resistance, improve electric field distribution, and enhance dynamic performance. Additionally, appropriately reducing the aluminum doping concentration in the second doping region can reduce the possibility of defects due to excessive aluminum, while the higher doping concentration in the first doping region ensures sufficient nitrogen to fill carbon vacancies, thereby reducing deep-level defects and improving carrier lifetime.
[0090] Secondly, this application provides a method for fabricating a semiconductor device, which can be used to manufacture the semiconductor device mentioned in the above embodiments.
[0091] The method includes: providing a silicon carbide substrate; forming a buffer layer and a first drift layer on the silicon carbide substrate, wherein the first drift layer is doped with aluminum and nitrogen; the first drift layer includes a first doped region and a second doped region stacked thereon, wherein the nitrogen doping concentration in the first doped region is greater than or equal to the nitrogen doping concentration in the second doped region, the aluminum doping concentration in the first doped region is greater than or equal to the aluminum doping concentration in the second doped region, and the net doping concentrations of the first doped region and the second doped region are the same.
[0092] Based on the above method and process, and the above Figure 1 For example, please refer to the appendix for the structure of the semiconductor device shown in (1). Figure 11 , Figure 11 This is a schematic diagram of a process for fabricating a semiconductor device provided in an embodiment of this application.
[0093] Among them, such as Figure 11 As shown:
[0094] Step S11: Provide a silicon carbide substrate.
[0095] The doping type of the silicon carbide substrate 101 can be selected according to the device requirements. Furthermore, after providing the substrate, the silicon carbide substrate can be chemically and mechanically polished and cleaned to eliminate surface scratches and remove surface contaminants.
[0096] Step S12: A buffer layer and a first drift layer are formed on a silicon carbide substrate.
[0097] A buffer layer 102 and a first drift layer 103 are epitaxially grown on a silicon carbide substrate using processes such as vapor deposition. During the growth of the first drift layer 103, different doping concentrations of aluminum and nitrogen can be achieved directly by changing the flow rate of the doping source gas. This forms a first doped region and a second doped region stacked on top of each other in the first drift layer. The nitrogen doping concentration in the first doped region is greater than or equal to the nitrogen doping concentration in the second doped region, and the aluminum doping concentration in the first doped region is greater than or equal to the aluminum doping concentration in the second doped region. Furthermore, the net doping concentrations of the first and second doped regions are the same.
[0098] This co-doping modulation method eliminates the need to introduce changes in other epitaxial process parameters. Furthermore, the modulation of the doping concentration and ratio of aluminum and nitrogen can be achieved by changing the flow rate of the doping source gas, avoiding the impact on epitaxial process control, especially defect density control. In addition, this modulated co-doped structure is nested in a conventional SiC epitaxial drift layer, without introducing additional post-processing, thus saving costs and improving production efficiency.
[0099] In addition, a collector layer can be formed in advance according to device requirements before forming a buffer layer, and a second drift layer can be formed in advance according to device requirements before forming a first drift layer; or a barrier layer, a well layer, or other structures can be formed after forming the first drift layer according to device requirements. This application does not make specific limitations on these embodiments.
[0100] It should be noted that the above refers to Figure 11 The specific fabrication process of the semiconductor device shown is merely an exemplary method, and the embodiments of this application do not specifically limit the specific fabrication process.
[0101] It should also be noted that the above Figures 1-9 The specific fabrication processes for each semiconductor device shown can also be referred to the above. Figure 11 The embodiments shown are not repeated here.
[0102] This application also provides a semiconductor packaging structure, which includes a packaging substrate and the semiconductor device involved in the above embodiments, wherein the packaging substrate is electrically connected to the semiconductor device.
[0103] This application also provides an electronic device, which includes a circuit board and the semiconductor packaging structure involved in the above embodiments, wherein the circuit board is electrically connected to the semiconductor packaging structure.
[0104] It should be understood that the semiconductor device fabrication method, packaging structure, and electronic device provided in this application can be consistent with the semiconductor device technical solution provided in this application, and their specific contents and beneficial effects can be referred to the above. Figures 1-4 The semiconductor devices mentioned in the illustrated embodiments will not be described in detail here.
[0105] It should be noted that, for the sake of simplicity, the foregoing method embodiments are all described as a series of actions. However, those skilled in the art should understand that this application is not limited to the described order of actions, as some steps may be performed in other orders or simultaneously according to this application. Furthermore, those skilled in the art should also understand that the embodiments described in the specification are preferred embodiments, and the actions and modules involved are not necessarily essential to this application.
[0106] The above-described embodiments are only used to illustrate the technical solutions of this application, and are not intended to limit them. Although this application has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of this application.
Claims
1. A semiconductor device, characterized in that, The device includes a silicon carbide substrate and a buffer layer and a first drift layer stacked on the silicon carbide substrate; the first drift layer is doped with aluminum and nitrogen. The first drift layer includes a first doped region and a second doped region stacked together, wherein the nitrogen doping concentration in the first doped region is greater than or equal to the nitrogen doping concentration in the second doped region, the aluminum doping concentration in the first doped region is greater than or equal to the aluminum doping concentration in the second doped region, and the net doping concentrations of the first doped region and the second doped region are the same.
2. The apparatus according to claim 1, characterized in that, The ratio of aluminum doping concentration to nitrogen doping concentration in any doped region of the first drift layer is greater than or equal to 0.1 and less than 1.
3. The apparatus according to claim 1 or 2, characterized in that, In the direction perpendicular to the substrate, the thickness of the first drift layer is greater than 0.1 micrometers and less than or equal to 200 micrometers.
4. The apparatus according to any one of claims 1-3, characterized in that, The net doping concentration of the first drift layer is 1×10 14 cm -3 Up to 1×10 17 cm -3 between.
5. The apparatus according to any one of claims 1-4, characterized in that, The device further includes a second drift layer disposed between the buffer layer and the first drift layer, wherein the doping concentration in the second drift layer is the same as the net doping concentration in the first drift layer.
6. The apparatus according to any one of claims 1-5, characterized in that, The device further includes a collector layer disposed between the silicon carbide substrate and the buffer layer.
7. The apparatus according to any one of claims 1-6, characterized in that, The semiconductor device is a unipolar power device or a bipolar power device.
8. A method for fabricating a semiconductor device, characterized in that, The method includes: Provide silicon carbide substrates; A buffer layer and a first drift layer are formed on the silicon carbide substrate, wherein the first drift layer is doped with aluminum and nitrogen; the first drift layer includes a first doped region and a second doped region stacked together, wherein the nitrogen doping concentration in the first doped region is greater than or equal to the nitrogen doping concentration in the second doped region, the aluminum doping concentration in the first doped region is greater than or equal to the aluminum doping concentration in the second doped region, and the net doping concentrations of the first doped region and the second doped region are the same.
9. A semiconductor packaging structure, characterized in that, It includes a packaging substrate and a semiconductor device as described in any one of claims 1-7, wherein the packaging substrate is electrically connected to the semiconductor device.
10. An electronic device, characterized in that, It includes a circuit board and a semiconductor package structure as described in claim 9 above, wherein the circuit board is electrically connected to the semiconductor package structure.