A fluidized bed calcination system and calcination method for polymethylsilsesquioxane

By using a fluidized bed system and airflow design, the problems of uneven temperature, adhesion, and safety hazards in the calcination of polymethylsilsesquioxane were solved, achieving efficient and safe production of silica microspheres.

CN123102289APending Publication Date: 2026-11-17HEFEI CEMENT RESEARCH AND DESIGN INSTITUTE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611492529.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-23
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing methods for calcining polymethylsilsesquioxanes suffer from uneven temperature distribution, material adhesion, safety hazards, and limited production capacity.

Method used

A fluidized bed system is adopted, in which the heated main airflow is provided by the first air supply device and the secondary airflow is provided by the second air supply device, so as to realize the fluidized state heating of the particles. Combined with the variable cross-section reaction chamber design and sensor monitoring, temperature uniformity and safety are ensured.

Benefits of technology

This technology enables efficient and safe production of silica microspheres, avoiding the risks of material adhesion and flash fire, and improving production capacity and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123102289A_ABST
    Figure CN123102289A_ABST
Patent Text Reader

Abstract

This invention provides a fluidized bed calcination system and method for polymethylsilsesquioxane, relating to the technical field of organosilicon material calcination equipment. The system includes: a first air supply device for providing the main airflow; an air heating device for heating the main airflow; a fluidized bed including a reaction chamber, the cross-sectional area of ​​which gradually increases from the bottom to the center and gradually decreases from the center to the reaction outlet; a perforated plate located at the bottom of the fluidized bed, having a plurality of vertically penetrating through holes; and a second air supply device with two second air outlets, one of which communicates with some of the through holes on the perforated plate, and the other communicating with the reaction chamber, the connection point being located on the side wall of the fluidized bed near the perforated plate. This invention allows particles to be uniformly heated in a fluidized state, avoiding material caking and localized accumulation of combustible gases that could lead to flashover. After calcination, well-dispersed silica microspheres are obtained without secondary processing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of organosilicon calcination equipment technology, and more specifically, to a fluidized bed calcination system and calcination method for polymethylsilsesquioxane. Background Technology

[0002] Polymethylsilsesquioxanes are a class of organosilicon polymers whose molecular structure contains both silicon-carbon bonds and silicon-oxygen-silicon networks, thus possessing both the processability of organic materials and the thermal stability of inorganic materials. Under controlled pyrolysis conditions, polymethylsilsesquioxanes can be converted into high-purity amorphous silica microspheres. These microspheres can be used as low-refractive-index fillers in optically transparent composite materials, low-dielectric-constant precursors for semiconductor packaging, and catalyst supports. The conversion from polymethylsilsesquioxanes to silica microspheres requires calcination.

[0003] Currently, in industry, pusher kilns or box-type resistance furnaces are commonly used to calcine polymethylsilsesquioxane. The specific operation involves spreading polymethylsilsesquioxane powder evenly in a ceramic sagger, then pushing the sagger containing the powder into a furnace chamber preheated to the target temperature. The powder is slowly heated by radiation and conduction from the furnace walls, held at that temperature for several hours, and then naturally cooled, causing the polymethylsilsesquioxane to pyrolyze and transform into silica microspheres.

[0004] In this static, flat-laying calcination method, heat is conducted layer by layer from the outside of the sagger to the center of the material. The temperature rise in the center of the material is significantly delayed, and the temperature distribution inside the sagger is uneven. The low heat transfer efficiency severely limits production capacity. Moreover, the statically laid polymethyl silsesquioxane particles soften when heated and stick together. After cooling, they form clumps, which must undergo secondary processing such as crushing and sieving to obtain well-dispersed silica microspheres. This not only increases energy consumption and labor costs but may also introduce impurities or damage the particle morphology. At the same time, polymethyl silsesquioxane releases flammable gases such as methane during pyrolysis. Once a local high-temperature area appears inside the accumulated material, flammable gases can easily accumulate in that area. When the concentration reaches the explosive limit, flash combustion is very likely to occur. The additional heat released by flash combustion will accelerate the pyrolysis of the surrounding materials, forming a positive feedback loop, which will ultimately lead to uncontrolled temperature rise and product quality deterioration. Summary of the Invention

[0005] The present invention aims to solve the problems of poor calcination effect and low safety of existing polymethylsilsesquioxanes.

[0006] To address the aforementioned problems, in a first aspect, the present invention provides a fluidized bed calcination system for polymethylsilsesquioxane, comprising: The first air supply equipment is used to provide the main airflow and has a main air outlet. An air heating device for heating the main airflow to a first temperature, having a first sub-inlet end and a first sub-outlet end, wherein the first sub-inlet end is connected to the main outlet end; A fluidized bed includes a reaction chamber having a reaction inlet and a reaction outlet, the reaction outlet being higher than the reaction inlet, and the cross-sectional area of ​​the reaction chamber along the horizontal plane gradually increasing from the bottom to the middle and gradually decreasing from the middle to the reaction outlet. A porous plate, used to fill polymethylsilsesquioxane particles, is located at the bottom of the fluidized bed and communicates with the reaction chamber. It has a plurality of through holes that run vertically through it. The second air supply device, used to provide secondary airflow, has two second air outlets, one of which is connected to a portion of the through holes on the porous plate, and the other is connected to the reaction chamber, with the connection point located on the side wall of the fluidized bed near the porous plate.

[0007] The fluidized bed calcination system for polymethylsilsesquioxane provided by this invention has, but is not limited to, the following beneficial effects compared to the prior art: The heated main airflow is introduced into the fluidized bed through the first air supply equipment and the air heating equipment, so that the polymethylsilsesquioxane particles packed on the porous plate are in a fluidized state and are uniformly heated in the fluidized bed. The particles are in full contact with the hot airflow, resulting in high heat transfer efficiency and uniform temperature distribution in the bed. The particles do not stick together or clump together in the fluidized state. After calcination, there is no need for secondary treatment such as crushing and sieving to obtain well-dispersed silica microspheres. Secondary airflow is introduced into the fluidized bed through some through holes in the perforated plate and near the perforated plate on the sidewall of the fluidized bed by the second air supply device. This creates instantaneous disturbance to the bed, which can eliminate particle accumulation on the surface of the perforated plate and at the corners of the sidewalls, and avoid uneven calcination of locally accumulated materials. At the same time, the continuous flow of the main airflow can carry the combustible gas generated by pyrolysis out of the fluidized bed in a timely manner, preventing the local accumulation of combustible gas in the bed and causing flash combustion. The cross-sectional area of ​​the reaction chamber gradually increases from the bottom to the middle and gradually decreases from the middle to the reaction outlet. This results in a higher air velocity at the bottom of the bed to support the particles, and a gradually decreasing air velocity in the middle and upper parts. The particles form an internal circulation in the bed, which can prevent a large number of ultrafine particles from being carried away by the airflow, thus balancing fluidization quality and product yield.

[0008] Furthermore, the fluidized bed has a plurality of lateral air inlet nozzles around its sidewall, and one of the second air outlets of the second air supply device is connected to the sidewall of the fluidized bed through the lateral air inlet nozzles.

[0009] Furthermore, the number of through holes communicating with the second air outlet end accounts for 5%-10% of the total number of through holes.

[0010] Furthermore, the sidewalls constituting the reaction chamber are formed from bottom to top into a first part, a second part, and a third part, wherein the acute angle formed between the first part sidewall and the horizontal plane is smaller than the acute angle formed between the second part sidewall and the horizontal plane.

[0011] Furthermore, the acute angle formed by the first sidewall and the horizontal plane is 73°, the acute angle formed by the second sidewall and the horizontal plane is 83°, and the acute angle formed by the third sidewall and the horizontal plane is 50°.

[0012] Furthermore, the reaction outlet is connected to a first dust collector bag, which is used to block polymethylsilsesquioxane particles in the airflow.

[0013] Furthermore, the fluidized bed calcination system for polymethylsilsesquioxane also includes: A temperature sensor is installed inside the fluidized bed to detect the temperature inside the fluidized bed; An oxygen concentration sensor is installed inside the fluidized bed to detect the oxygen concentration inside the fluidized bed; A deflagration sensor is installed inside the fluidized bed to detect the pressure inside the fluidized bed.

[0014] Secondly, the present invention also provides a fluidized bed calcination method for polymethylsilsesquioxane, based on the above-described fluidized bed calcination system for polymethylsilsesquioxane, comprising the following steps: filling polymethylsilsesquioxane particles into the fluidized bed; The heated main airflow is introduced into the fluidized bed through the first air supply device and the air heating device, so that at least a portion of the polymethylsilsesquioxane particles are in a fluidized state. The secondary airflow is introduced into the fluidized bed through the second air supply device.

[0015] Furthermore, the polymethylsilsesquioxane particles are heated in segments according to temperature ranges, and different heating rates and gas-solid ratios are matched. The temperature ranges include a first temperature range of 0-360℃, a second temperature range of 360-470℃, and a third temperature range of 470-1000℃.

[0016] Furthermore, the heating rate is 10℃ / s and the gas-solid ratio is 0.5Nm³ / s / kg in the first temperature range; the heating rate is 4℃ / s and the gas-solid ratio is 0.625Nm³ / s / kg in the second temperature range; and the heating rate is 5℃ / s and the gas-solid ratio is 0.75Nm³ / s / kg in the third temperature range. Attached Figure Description

[0017] Figure 1 This is a schematic diagram of the system structure of the present invention; Figure 2This is a schematic diagram of the sensor arrangement within the system of the present invention; Figure 3 This is a schematic diagram of the through-hole arrangement of a perforated plate according to an embodiment of the present invention, wherein the solid through-holes are through-holes that communicate with the second air supply device; Figure 4 This is a schematic diagram of the side air intake nozzle in this invention.

[0018] Explanation of reference numerals in the attached figures: 1. First air supply equipment; 2. Air heating equipment; 3. Second air supply equipment; 4. Side air inlet nozzle; 5. Perforated plate; 6. Fluidized bed; 7. Reaction chamber; 8. First dust collector bag; 9. Oxygen concentration sensor; 10. Temperature sensor; 11. Deflagration sensor. Detailed Implementation

[0019] To make the objectives, technical solutions, and advantages of this application clearer, the technical solutions in the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. It should be understood that the described embodiments are only a part of the embodiments of this application, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments described in this application without creative effort will fall within the scope of protection of this application.

[0020] Unless otherwise defined, all technical and scientific terms used in this application have the same meaning as commonly understood by one of ordinary skill in the art to which this application pertains; the terminology used in the specification of this application is for the purpose of describing specific embodiments only and is not intended to limit this application; the terms "comprising," "including," "having," "containing," etc., in the specification, claims, and accompanying drawings of this application are open-ended terms. Therefore, "comprising," "including," or "having" refers to, for example, a method or apparatus having one or more steps or elements, but is not limited to having only these one or more elements. The terms "first," "second," etc., in the specification, claims, or accompanying drawings of this application are used to distinguish different objects, not to describe a specific order or hierarchy. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, a feature defined with "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this application, unless otherwise stated, "a plurality of" means two or more.

[0021] In the description of this invention, it should be understood that the terms "upper", "lower", "left", "right", "front", "rear", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention.

[0022] In the description of this application, it should be noted that, unless otherwise expressly specified and limited, the terms "installation," "connection," "linking," and "attachment" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal communication between two components. Those skilled in the art can understand the specific meaning of the above terms in this application according to the specific circumstances.

[0023] It should be emphasized that when the term "comprising / including" is used in this specification, it is used to explicitly indicate the presence of the stated feature, integer, step, or component, but does not exclude the presence or addition of one or more other features, integers, steps, parts, or groups of features, integers, steps, or parts.

[0024] In this application, the term "and / or" is merely a description of the relationship between related objects, indicating that three relationships can exist. For example, A and / or B can represent: A existing alone, A and B existing simultaneously, or B existing alone. Additionally, in this application, the character " / " generally indicates that the preceding and following related objects have an "or" relationship.

[0025] See Figures 1-4An embodiment of the present invention provides a fluidized bed calcination system for polymethylsilsesquioxane, comprising a first air supply device 1, an air heating device 2, a fluidized bed 6, a perforated plate 5, and a second air supply device 3. The first air supply device 1 provides the main airflow and has a main air outlet. The air heating device 2 heats the main airflow to a first temperature and has a first sub-inlet and a first sub-outlet, the first sub-inlet being connected to the main air outlet. The fluidized bed 6 includes a reaction chamber 61 with a reaction inlet and a reaction outlet, the reaction outlet being higher than the reaction inlet. The cross-sectional area of ​​the fluidized bed 61 along the horizontal plane gradually increases from the bottom to the middle and gradually decreases from the middle to the reaction outlet. The porous plate 5 is used to fill polymethylsilsesquioxane particles. The porous plate 5 is located at the bottom of the fluidized bed 6 and is connected to the reaction chamber 61. The porous plate 5 has a plurality of through holes that run vertically through it. The second air supply device 3 is used to provide secondary airflow. The second air supply device 3 has two second air outlets. One of the second air outlets is connected to a portion of the through holes on the porous plate 5, and the other second air outlet is connected to the reaction chamber 61. The connection point is located on the side wall of the fluidized bed 6 near the porous plate 5.

[0026] In this embodiment, the first air supply device 1 can be, for example, a variable frequency fan. The variable frequency fan delivers ambient temperature air and its air volume can be adjusted. The variable frequency fan does not involve the delivery of high-temperature airflow, and the system only needs to be equipped with an ambient temperature fan. The air heating device 2 can be, for example, an air resistance wire heating device. The air resistance wire heating device is equipped with a plurality of resistance wires. The surface area of ​​the resistance wires in contact with the air is large, which can quickly heat the air to the same temperature as the resistance wires. The temperature of the resistance wires can be controlled by current. The temperature adjustment range of the resistance wires can be, for example, 20℃-1000℃. The first temperature can be the temperature that matches the current calcination stage. Using resistance wire heating instead of chemical combustion methods such as natural gas or coal powder can ensure that the oxygen concentration in the heated airflow is consistent with the oxygen concentration in the air, ensuring that polymethylsilsesquioxane can fully capture oxygen atoms during the calcination process.

[0027] The change in the cross-sectional area of ​​the reaction chamber 61 results in a high airflow velocity at the bottom of the reaction chamber 61 and a low airflow velocity in the middle and upper parts. The through holes on the perforated plate 5 are connected vertically, allowing airflow to enter the top of the perforated plate 5 from the bottom through the through holes. The inner diameter of the through holes can be larger than the minimum outer diameter of the polymethylsilsesquioxane particles. In the initial stage, a weak airflow can be introduced into the fluidized bed 6 through the first air supply device 1 to prevent the polymethylsilsesquioxane particles from falling. Secondly, after calcination, because the calcined polymethylsilsesquioxane particles have a certain degree of stickiness, a sticky arch bridge structure will be formed between the particles, so they will not fall down from the perforated plate 5. The second air supply device 3 can be, for example, a pulse blower, which outputs a pulsed airflow at room temperature. Of the two second air outlets, one of the second air outlets, which is connected to the upper part of the through hole of the perforated plate 5, can be connected to the bottom of the through hole via a pipe. The airflow generated by the first air supply device 1 cannot enter the through hole. Only the airflow generated by the second air supply device 3 enters the through hole via a pipe and then enters the reaction chamber 61. The other second air outlet can be further divided into two branches. Both branches are connected to the reaction chamber 61 from the side wall of the fluidized bed 6, which is close to the upper part of the perforated plate 5. Ultrafine particles are very likely to accumulate at the angle between the perforated plate 5 and the side wall.

[0028] The fluidized bed calcination system for polymethylsilsesquioxane can be used for the fluidized bed calcination of ultrafine polymethylsilsesquioxane particles to prepare high-purity amorphous silica microspheres. This system can be applied in the field of organosilicon material calcination equipment technology, specifically in scenarios such as the calcination preparation of low-refractive-index fillers for optically transparent composite materials, the calcination preparation of low-dielectric-constant material precursors for semiconductor packaging, and the calcination preparation of silica microspheres for catalyst supports; no specific limitations are imposed.

[0029] In this embodiment, the main airflow is provided by the first air supply device 1, and the main airflow is heated to a first temperature by the air heating device 2 and then introduced into the fluidized bed 6 from the bottom of the perforated plate 5. This allows the polymethylsilsesquioxane particles packed on the perforated plate 5 to be in a fluidized state and uniformly heated in the reaction chamber 61. The particles are in full contact with the hot airflow, resulting in high heat transfer efficiency and uniform temperature distribution in the bed. Furthermore, the particles do not stick together or clump in the fluidized state. After calcination, there is no need for secondary processing such as crushing or sieving to obtain well-dispersed silica microspheres. The cross-sectional area of ​​the reaction chamber 61 gradually increases from the bottom to the middle and gradually decreases from the middle to the reaction outlet. This allows for a higher air velocity at the bottom of the bed to support the particles, while the air velocity in the upper middle gradually decreases. The particles form an internal circulation in the bed, which can prevent a large number of ultrafine particles from being carried away by the airflow, thus balancing fluidization quality and product yield. The second air supply device 3 has one second air outlet that introduces secondary airflow into the reaction chamber 61 through some through holes on the perforated plate 5, and another second air outlet that introduces secondary airflow from the side wall of the fluidized bed 6 near the perforated plate 5. This can generate instantaneous disturbance to the bed, eliminate particle accumulation on the surface of the perforated plate 5 and at the angle between the perforated plate 5 and the side wall, and prevent uneven calcination of locally accumulated materials, which can lead to discolored materials and spread to other parts of the bed. At the same time, the continuously flowing main airflow can carry the combustible gas generated by pyrolysis out of the reaction chamber 61 in a timely manner, preventing the combustible gas from accumulating locally in the bed to the point of reaching the explosion limit and causing flash fire. Thus, it overcomes the problems of uneven temperature distribution, material caking, and flash fire hazards in the existing static calcination method, and improves the system's production capacity, safety, and product quality.

[0030] See Figure 1 , Figure 2 and Figure 4 Optionally, a plurality of lateral air inlet nozzles 4 are provided around the sidewall of the fluidized bed 6, and one of the second air outlets of the second air supply device 3 is connected to the sidewall of the fluidized bed 6 through the lateral air inlet nozzle 4.

[0031] In this embodiment, the lateral air inlet nozzle 4 can be, for example, a tapered nozzle, with its outlet facing the interior of the reaction chamber 61. A plurality of lateral air inlet nozzles 4 can be arranged in two layers on the sidewall of the fluidized bed 6. Each layer of lateral air inlet nozzles 4 can be evenly distributed around the sidewall of the fluidized bed 6, and the installation height of both layers of lateral air inlet nozzles 4 is close to the top of the perforated plate 5. One layer of lateral air inlet nozzles 4 can be connected to one branch of one of the second air outlets via a pipe, and the other layer of lateral air inlet nozzles 4 can be connected to another branch of the second air outlet via a pipe. The pulsed airflow is accelerated by the lateral air inlet nozzles 4 and then injected into the reaction chamber 61, which can directionally scour the particles near the sidewall.

[0032] In this embodiment, a plurality of lateral air inlet nozzles 4 are provided around the sidewall of the fluidized bed 6, which can make the secondary airflow uniformly sprayed into the reaction chamber 61 along the circumference of the sidewall; one of the second air outlets of the second air supply device 3 is connected to the sidewall of the fluidized bed 6 through the lateral air inlet nozzle 4, which can make the pulse airflow concentrate on scouring the angle area between the perforated plate 5 and the sidewall, specifically eliminating the accumulation of ultrafine particles that are very likely to occur in this angle area, and further reducing the fluidization dead angle in the bed.

[0033] Optionally, the number of through holes communicating with the second air outlet end accounts for 5%-10% of the total number of through holes.

[0034] In this embodiment, the proportion of the number of through holes connected to the second air outlet to the total number of through holes can be, for example, 7%. When this proportion is too low, the amount of pulsed airflow introduced through the through holes is insufficient, resulting in a weak disturbance effect on the particles above the porous plate 5, making it difficult to eliminate particle accumulation in the central region of the porous plate 5. When this proportion is too high, the pulsed airflow introduced through the through holes will interfere with the uniformity of the main airflow distribution on the porous plate 5, affecting the basic fluidization effect of the bed. Controlling the proportion between 5% and 10% can balance the pulsed disturbance effect with the basic fluidization effect.

[0035] In this embodiment, by limiting the number of through holes connected to the second outlet to be between 5% and 10% of the total number of through holes, it is possible to ensure that the main airflow is uniformly introduced through most of the through holes to maintain basic fluidization, while allowing the pulse airflow to be concentrated through a small number of through holes to form sufficient instantaneous disturbance intensity, thereby specifically eliminating the particle accumulation dead zone above the porous plate 5, especially in the central region of the porous plate 5.

[0036] See Figure 1 and Figure 2 Optionally, the sidewalls constituting the reaction chamber 61 are formed from bottom to top as a first part, a second part, and a third part, wherein the acute angle formed between the sidewall of the first part and the horizontal plane is smaller than the acute angle formed between the sidewall of the second part and the horizontal plane.

[0037] In this embodiment, the first, second, and third parts are connected sequentially from bottom to top. The corresponding areas of the first and second parts together constitute the part of the reaction chamber 61 where the cross-sectional area gradually increases from the bottom to the middle, and the corresponding area of ​​the third part constitutes the part of the reaction chamber 61 where the cross-sectional area gradually decreases from the middle to the reaction outlet. The connection point between the second and third parts corresponds to the middle position where the cross-sectional area of ​​the reaction chamber 61 is the largest. The acute angle formed by the sidewall of the first part and the horizontal plane is smaller than the acute angle formed by the sidewall of the second part and the horizontal plane, which allows the cross-sectional area of ​​the corresponding area of ​​the first part to increase rapidly with height, and the airflow velocity to decrease significantly in this area. The sidewall of the second part is closer to vertical, and the change in the cross-sectional area of ​​the corresponding area of ​​the second part tends to be gentle, and the decreasing trend of the airflow velocity is weakened. The sidewall of the third part contracts inward to form a constriction, and particles carried by the airflow to the upper part of the reaction chamber 61 can decelerate and fall back at the constriction.

[0038] In this embodiment, the sidewalls of the reaction chamber 61 are formed from bottom to top into a first part, a second part, and a third part, and the acute angle formed between the first part sidewall and the horizontal plane is smaller than the acute angle formed between the second part sidewall and the horizontal plane. This allows the airflow velocity in the bottom region of the reaction chamber 61 to be higher to support the particles, while the air velocity above the bottom gradually decreases according to the gradient. Under the action of gravity and airflow, the particles form a stable internal circulation in the bed, which can prevent a large number of ultrafine particles from being entrained and escaped by the airflow, and can also maintain the fluidization stability of the bed.

[0039] Optionally, the acute angle formed by the first sidewall and the horizontal plane is 73°, the acute angle formed by the second sidewall and the horizontal plane is 83°, and the acute angle formed by the third sidewall and the horizontal plane is 50°.

[0040] In this embodiment, when the acute angle formed between the first sidewall and the horizontal plane is too small, the airflow will separate near the first sidewall, forming a large low-speed zone at the sidewall, and more particles will accumulate on the sidewall, affecting the fluidization effect. When the angle is too large, the variable cross-section effect of the reaction chamber 61 is poor, the decreasing trend of airflow velocity is not obvious, and the internal circulation fluidization of particles cannot be achieved, resulting in a large circulating load and low output of the system. Setting the acute angle formed between the first sidewall and the horizontal plane to 73° and the acute angle formed between the second sidewall and the horizontal plane to 83° can ensure the effect of the variable cross-section on the airflow velocity adjustment while avoiding the formation of the low-speed zone on the sidewall. The acute angle formed between the third sidewall and the horizontal plane is 50°, which can form a clear constriction structure, so that the particles that are carried upward lose the support of the airflow in the corresponding area of ​​the third part and fall back to the bed.

[0041] In this embodiment, by setting the acute angle between the first sidewall and the horizontal plane to 73°, the acute angle between the second sidewall and the horizontal plane to 83°, and the acute angle between the third sidewall and the horizontal plane to 50°, the airflow velocity within the reaction chamber 61 can be varied according to a distribution that is high at the bottom, slow in the middle, and low at the top. This allows the particles to form a stable internal circulation within the bed, ensuring that over 90% of the particles remain within the fluidized bed 6 for internal circulation fluidization, further reducing particle entrainment and improving product yield. Only when the acute angle between the first sidewall and the horizontal plane is 73°, and the acute angle between the second sidewall and the horizontal plane is 50°... When the acute angle is 83° and the acute angle formed by the third sidewall and the horizontal plane is 50°, the gas velocity at the bottom of the reaction chamber 61 can be maintained above the critical fluidization gas velocity required to fluidize polymethylsilsesquioxane ultrafine particles, and the gas velocity in the middle and upper part can be reduced to below the terminal settling velocity of the particles. When the particles carried upward by the airflow reach the corresponding area of ​​the third part, they will lose the support of the airflow and fall back, thus closing the internal circulation. Any deviation from the angle will disrupt the above gas velocity distribution. When the angle is too large, the gas velocity attenuation is insufficient, and a large number of particles will be carried away by the airflow and escape. When the angle is too small, a low-speed zone will be formed near the sidewall, and the particles will accumulate on the sidewall.

[0042] See Figure 1 and Figure 2 Optionally, the reaction outlet is connected to a first dust collector bag 7, which is used to block polymethylsilsesquioxane particles in the airflow.

[0043] In this embodiment, although the variable cross-section structure of the fluidized bed 6 can retain more than 90% of the particles within the fluidized bed 6 for internal circulation fluidization, due to the extremely fine particle size of the polymethylsilsesquioxane particles, about 10% of the particles will still escape with the airflow. The first dust collector bag 7 can intercept these particles. The first dust collector bag 7 can be, for example, a high-silica uncoated dust collector bag, which is an existing mature product that can be directly selected by those skilled in the art. The first dust collector bag 7 does not use metal material, which can avoid the metal material damaging the high-purity silica medium of the calcined product. The electrical performance is excellent, and the high-silica material can withstand operating environments up to 1000℃. Furthermore, the first dust collector bag 7 can be equipped with a pulse cleaning device, which is used to periodically spray pulse airflow onto the first dust collector bag 7 to blow the particles accumulated on the first dust collector bag 7 back into the fluidized bed 6. The operating frequency of the pulse cleaning device can be higher than that of conventional bag dust collectors to avoid particle accumulation on the first dust collector bag 7. The pulse cleaning device is a device carried by the first dust collector bag 7 itself and is a different device from the second air supply device 3. The airflow of the two is independent of each other.

[0044] In this embodiment, a first dust collector bag 7 is connected to the reaction outlet, which can block and collect polymethylsilsesquioxane particles that escape with the airflow, prevent product particles from being lost with the airflow, improve raw material utilization, and prevent ultrafine particles from being directly discharged into subsequent equipment or the atmosphere.

[0045] See Figure 1 and Figure 2 Optionally, the fluidized bed calcination system for polymethylsilsesquioxane further includes a temperature sensor 9, an oxygen concentration sensor 8, and a deflagration sensor 10; wherein, the temperature sensor 9 is disposed within the fluidized bed 6 and is used to detect the temperature within the fluidized bed 6; the oxygen concentration sensor 8 is disposed within the fluidized bed 6 and is used to detect the oxygen concentration within the fluidized bed 6; and the deflagration sensor 10 is disposed within the fluidized bed 6 and is used to detect the pressure within the fluidized bed 6.

[0046] In this embodiment, the oxygen concentration sensor 8 can be arranged in layers at different heights within the reaction chamber 61, for example, in three layers, to monitor the oxygen concentration at different heights within the reaction chamber 61. The oxygen concentration within the reaction chamber 61 can always be controlled to be greater than 15%, ensuring that oxygen atoms can be fully captured during the calcination of polymethylsilsesquioxane. The temperature sensor 9 can detect the temperature inside the bed in real time, and the operator or control system can adjust the heating power of the air heating device 2 according to the detection value of the temperature sensor 9. The deflagration sensor 10 is used to detect the pressure inside the reaction chamber 61. The pyrolysis of polymethylsilsesquioxane will produce a large amount of... If the temperature rise is not properly controlled, combustible gases such as methane, hydrogen, and carbon monoxide may produce a large amount of combustible gas in a short period of time, which may cause deflagration. When deflagration occurs, the combustible gas burns rapidly in the bed, the gas volume expands instantaneously, and the pressure in the reaction chamber 61 will rise sharply in a very short time. The deflagration sensor 10 can detect the pressure change in the reaction chamber 61 to determine whether deflagration has occurred in the bed. Once the deflagration sensor 10 detects deflagration and alarms, the air heating device 2 can be cooled down to below 400°C and the gas flow rate into the reaction chamber 61 can be increased to dilute the concentration of combustible gas in the bed and suppress pyrolysis positive feedback.

[0047] In this embodiment, a temperature sensor 9 is installed inside the fluidized bed 6 to obtain the bed temperature in real time, providing feedback for the control of the heating process; an oxygen concentration sensor 8 is installed inside the fluidized bed 6 to monitor the oxygen concentration inside the bed, ensuring the oxidizing atmosphere required for calcination; and a deflagration sensor 10 is installed inside the fluidized bed 6 to detect the pressure inside the bed and promptly detect deflagration and trigger response. The installation of these three types of sensors helps to maintain the stability of the fluidization and heating environment, ensuring the safe conduct of the calcination process.

[0048] See Figure 1 and Figure 2 An embodiment of the present invention provides a fluidized bed calcination method for polymethylsilsesquioxane, based on the above-mentioned fluidized bed calcination system for polymethylsilsesquioxane, comprising the following steps: filling polymethylsilsesquioxane particles into a fluidized bed 6; introducing a heated main airflow into the fluidized bed 6 through a first air supply device 1 and an air heating device 2, so that at least a portion of the polymethylsilsesquioxane particles are in a fluidized state; and introducing a secondary airflow into the fluidized bed 6 through a second air supply device 3.

[0049] In this embodiment, during filling, polymethylsilsesquioxane particles can be pre-filled into the fluidized bed 6 and positioned above the perforated plate 5. When the heated main airflow is introduced, the temperature of the air heating device 2 can continuously rise, and the airflow temperature will also continuously rise. After the airflow enters the reaction chamber 61 through the through holes of the perforated plate 5, it fluidizes and heats the polymethylsilsesquioxane particles, gradually fluidizing and calcining the particles. At this time, most of the polymethylsilsesquioxane particles can be in a fluidized state. When the secondary airflow is introduced, the second air supply device 3 can output a pulsed airflow, causing the bed to be momentarily disturbed, so that a small number of polymethylsilsesquioxane particles that are gathered on the sides and bottom of the fluidized bed 6 can also be in a fluidized state.

[0050] In one specific embodiment, the first air supply device 1 can transport ambient temperature air to the air heating device 2 via a pipeline. The heated air continues forward through the pipeline and enters the fluidized bed 6 through the through holes on the perforated plate 5 to fluidize and heat the pre-filled polymethylsilsesquioxane particles. A small number of particles entrained by the airflow are intercepted by the first dust collector bag 7 at the reaction outlet. The high-temperature airflow exiting the first dust collector bag 7 can enter the wet particle drying device through the outlet pipeline to dry other wet particle materials that need to be dried, so as to make full use of the heat generated by the system. This high-temperature airflow must not be used for drying polymethylsilsesquioxane. After passing through the wet particle drying device, the airflow temperature can be reduced to below 100°C. To meet environmental protection requirements, the low-temperature bag filter can filter the airflow and finally discharge the airflow into the atmosphere. Thus, the heat of the system is fully utilized, and the discharged airflow meets environmental protection requirements.

[0051] In this embodiment, by filling polymethylsilsesquioxane particles into a fluidized bed 6 and introducing a heated main airflow into the fluidized bed 6 through a first air supply device 1 and an air heating device 2, the particles can be uniformly heated in a fluidized state. The heat is directly transferred to the particles by the airflow, resulting in high heat transfer efficiency and uniform temperature distribution within the bed. This overcomes the problems of delayed temperature rise at the center of the material and limited production capacity in static calcination in a sagger. By introducing a secondary airflow into the fluidized bed 6 through a second air supply device 3, the polymethylsilsesquioxane particles are kept in a fluidized state. The particles continue to move during calcination without sticking together or caking. After calcination, well-dispersed silica microspheres can be obtained without secondary crushing and sieving. At the same time, the continuously flowing airflow carries away the combustible gases generated by pyrolysis in a timely manner, preventing the local accumulation of combustible gases in the bed from causing flashover and uncontrolled temperature rise. The safety of the method and the quality of the product are both improved.

[0052] Optionally, the polymethylsilsesquioxane particles are heated in segments according to temperature ranges, and different heating rates and gas-solid ratios are matched. The temperature ranges include a first temperature range of 0-360℃, a second temperature range of 360-470℃, and a third temperature range of 470-1000℃.

[0053] In this embodiment, the pyrolysis process of polymethylsilsesquioxane differs across different temperature ranges: in the first temperature range of 0-360℃, the particles are mainly in the preheating and pyrolysis stage, with a relatively small release of pyrolysis gases; in the second temperature range of 360-470℃, the polymethylsilsesquioxane main chain breaks down significantly, resulting in the concentrated release of combustible gases such as methane, and a lower heating rate can prevent the explosive release of combustible gases; in the third temperature range of 470-1000℃, the remaining groups undergo further oxidation and condensation, allowing for a relatively higher heating rate to ensure calcination efficiency; as the temperature changes, the interaction forces between particles change, and the dispersion and flowability of the particle group change accordingly. Dynamically setting the gas-solid ratio based on the state of the material at different temperatures can ensure continuous fluidization within each temperature range; precise heating division can accelerate calcination efficiency while meeting the calcination temperature requirements at different stages, preventing excessively long calcination times due to the limitation of the minimum heating rate.

[0054] In this embodiment, by heating the polymethylsilsesquioxane particles in segments according to temperature ranges and matching different heating rates and gas-solid ratios, the heating process can be matched with the pyrolysis kinetics of polymethylsilsesquioxane, corresponding to the release rate of pyrolysis gases in each temperature range. This avoids the explosive accumulation of combustible gases such as methane in a short time, prevents particle structure rupture and local overheating sintering, and ensures that the bed remains continuously and stably fluidized in each temperature range, taking into account calcination efficiency and the microstructural integrity and whiteness of the product.

[0055] Optionally, the heating rate is 10℃ / s and the gas-solid ratio is 0.5Nm³ / s / kg in the first temperature range; the heating rate is 4℃ / s and the gas-solid ratio is 0.625Nm³ / s / kg in the second temperature range; and the heating rate is 5℃ / s and the gas-solid ratio is 0.75Nm³ / s / kg in the third temperature range.

[0056] In this embodiment, a heating rate of 10℃ / s and a gas-solid ratio of 0.5 Nm³ / s / kg can be used in the first temperature range. At this stage, the amount of pyrolysis gas released is small, and a higher heating rate can shorten the preheating time, while a smaller gas-solid ratio can reduce the disturbance of the airflow to the bed. In the second temperature range, a heating rate of 4℃ / s and a gas-solid ratio of 0.625 Nm³ / s / kg can be used. Lowering the heating rate can slow down the release rate of combustible gases, while increasing the gas-solid ratio can promptly carry out the concentrated release of combustible gases and maintain bed fluidization. In the third temperature range, a heating rate of 5℃ / s and a gas-solid ratio of 0.75 Nm³ / s / kg can be used. At this stage, the particles gradually become denser, and further increasing the gas-solid ratio can adapt to changes in the flowability of the particle group.

[0057] In one specific embodiment, an air flow sensor can be installed in the system to monitor airflow. The airflow rate of the first air supply device 1 is Q1, and the airflow rate after being heated and expanded by the air heating device 2 is Q2. The gas generated by the pyrolysis and combustion of polymethylsilsesquioxane after fluidized calcination is mixed with the airflow rate of Q2, increasing the airflow rate to Q3. Q3 is greater than Q2, and Q2 is greater than Q1. The operator or control system can adjust the gas-solid ratio according to the monitoring value of the air flow sensor.

[0058] In comparison, Supplementary Experiment 1 used a two-stage heating method: a heating rate of 10℃ / s and a gas-solid ratio of 0.5 Nm³ / s / kg in the 0-400℃ stage, and a heating rate of 4℃ / s and a gas-solid ratio of 0.5 Nm³ / s / kg in the 400-1000℃ stage. The experimental results showed poor fluidization at the bottom and a large amount of material accumulation. Supplementary Experiment 2 also used a two-stage heating method: a heating rate of 10℃ / s and a gas-solid ratio of 1.5 Nm³ / s / kg in the 0-400℃ stage, and a heating rate of 4℃ / s and a gas-solid ratio of 1.5 Nm³ / s / kg in the 400-1000℃ stage. The experimental results showed that all the powder was blown away, and very little material remained inside the equipment. When the heating stage was coarse and the gas flow rate was fixed, the material calcination was unqualified, and either all the material was blown away or the fluidization effect was poor.

[0059] In this embodiment, by using a heating rate of 10℃ / s and a gas-solid ratio of 0.5 Nm³ / s / kg in the first temperature range, a heating rate of 4℃ / s and a gas-solid ratio of 0.625 Nm³ / s / kg in the second temperature range, and a heating rate of 5℃ / s and a gas-solid ratio of 0.75 Nm³ / s / kg in the third temperature range, the heating rate and gas-solid ratio at each stage can be matched with the release rate of pyrolysis gases and the fluidization state of the material at that stage. This avoids the explosive accumulation of combustible gases such as methane that could cause flash combustion, while also avoiding material accumulation due to an excessively low gas-solid ratio and particle entrainment due to an excessively high gas-solid ratio. The calcined silica microspheres have good sphericity, and the silica purity can reach approximately 99.999%.

[0060] While the present invention has been disclosed above, its scope of protection is not limited thereto. Those skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention, and all such changes and modifications will fall within the scope of protection of the present invention.

Claims

1. A fluidized bed calcination system for polymethylsilsesquioxane, characterized in that, include: The first air supply device (1) is used to provide the main airflow and has a main air outlet. An air heating device (2) is used to heat the main airflow to a first temperature, and has a first sub-inlet end and a first sub-outlet end, wherein the first sub-inlet end is connected to the main outlet end; The fluidized bed (6) includes a reaction chamber (61) having a reaction inlet and a reaction outlet, the reaction outlet being higher than the reaction inlet, and the cross-sectional area of ​​the reaction chamber (61) along the horizontal plane gradually increasing from the bottom to the middle and gradually decreasing from the middle to the reaction outlet; A porous plate (5) is used to fill polymethylsilsesquioxane particles. It is located at the bottom of the fluidized bed (6) and is connected to the reaction chamber (61). It has a plurality of through holes that run vertically through it. The second air supply device (3) is used to provide secondary airflow and has two second air outlets, one of which is connected to a portion of the through holes on the porous plate (5) and the other is connected to the reaction chamber (61), with the connection point located on the side wall of the fluidized bed (6) near the porous plate (5).

2. The fluidized bed calcination system for polymethylsilsesquioxane according to claim 1, characterized in that, The fluidized bed (6) has a plurality of lateral air inlet nozzles (4) around its sidewall. One of the second air outlets of the second air supply device (3) is connected to the sidewall of the fluidized bed (6) through the lateral air inlet nozzles (4).

3. The fluidized bed calcination system for polymethylsilsesquioxane according to claim 1, characterized in that, The number of through holes communicating with the second air outlet is between 5% and 10% of the total number of through holes.

4. The fluidized bed calcination system for polymethylsilsesquioxane according to claim 1, characterized in that, The sidewalls constituting the reaction chamber (61) are formed from bottom to top as a first part, a second part and a third part, wherein the acute angle formed between the sidewall of the first part and the horizontal plane is smaller than the acute angle formed between the sidewall of the second part and the horizontal plane.

5. The fluidized bed calcination system for polymethylsilsesquioxane according to claim 4, characterized in that, The acute angle formed by the first sidewall and the horizontal plane is 73°, the acute angle formed by the second sidewall and the horizontal plane is 83°, and the acute angle formed by the third sidewall and the horizontal plane is 50°.

6. The fluidized bed calcination system for polymethylsilsesquioxane according to claim 1, characterized in that, The reaction outlet is connected to a first dust collector bag (7), which is used to block polymethylsilsesquioxane particles in the airflow.

7. The fluidized bed calcination system for polymethylsilsesquioxane according to claim 1, characterized in that, The fluidized bed calcination system for polymethylsilsesquioxane also includes: A temperature sensor (9) is installed inside the fluidized bed (6) to detect the temperature inside the fluidized bed (6); An oxygen concentration sensor (8) is installed in the fluidized bed (6) to detect the oxygen concentration in the fluidized bed (6); A deflagration sensor (10) is installed in the fluidized bed (6) to detect the pressure inside the fluidized bed (6).

8. A fluidized bed calcination method for polymethylsilsesquioxane, based on the fluidized bed calcination system for polymethylsilsesquioxane according to any one of claims 1-7, characterized in that, The steps include: filling polymethylsilsesquioxane particles into the fluidized bed (6); Heated main airflow is introduced into the fluidized bed (6) through the first air supply device (1) and the air heating device (2) so that at least a portion of the polymethylsilsesquioxane particles are in a fluidized state; The secondary airflow is introduced into the fluidized bed (6) through the second air supply device (3).

9. The fluidized bed calcination method for polymethylsilsesquioxane according to claim 8, characterized in that, The polymethylsilsesquioxane particles are heated in segments according to temperature ranges, and different heating rates and gas-solid ratios are matched. The temperature ranges include a first temperature range of 0-360℃, a second temperature range of 360-470℃, and a third temperature range of 470-1000℃.

10. The fluidized bed calcination method for polymethylsilsesquioxane according to claim 9, characterized in that, The heating rate is 10℃ / s and the gas-solid ratio is 0.5Nm³ / s / kg in the first temperature range; the heating rate is 4℃ / s and the gas-solid ratio is 0.625Nm³ / s / kg in the second temperature range; and the heating rate is 5℃ / s and the gas-solid ratio is 0.75Nm³ / s / kg in the third temperature range.