A method for preparing highly stable, high-acid-density carbon-based solid acids by ultrasound-assisted phosphoric acid co-activation.

By employing an ultrasound-assisted phosphoric acid co-activation method, a highly stable sulfonic acid group was constructed in a carbon-based solid acid catalyst. This solved the problems of insufficient pore connectivity and proximity of acidic sites, resulting in a carbon-based solid acid catalyst with high acid density and high stability, thereby improving the conversion rate and cycle stability of the esterification reaction.

CN123102391APending Publication Date: 2026-11-17KUNMING UNIV OF SCI & TECH +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202611496698.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-24
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing carbon-based solid acid catalysts have narrow pores and insufficient connectivity, making it difficult to access acidic sites. This results in low acid density and poor stability, which makes it difficult to meet the mass transfer requirements of macromolecular esterification reactions.

Method used

An ultrasonic-assisted phosphoric acid synergistic activation method was adopted, which utilizes the ultrasonic cavitation effect to promote the penetration of phosphoric acid molecules into the pores of a carbon support, constructing phosphorus-containing functional groups such as COP, P=O, and P-OH as chemical anchors, and forming POS bonds through thermal sulfonation to achieve highly stable chemical anchoring of sulfonic acid groups.

Benefits of technology

It significantly improves the acid density and stability of carbon-based solid acids, enhances the activity and cycle stability of catalysts, maintains the esterification reaction conversion rate above 70%, and solves the problem of easy sulfonic acid group removal.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123102391A_ABST
    Figure CN123102391A_ABST
Patent Text Reader

Abstract

This invention relates to a method for preparing highly stable, high-acid-density carbon-based solid acids through ultrasound-assisted phosphoric acid synergistic activation, belonging to the technical field of solid acid catalytic materials. In this invention, a carbon support is added to a phosphoric acid solution and mixed uniformly to obtain a mixture. This mixture is then subjected to ultrasound-assisted phosphoric acid synergistic activation at 25-60°C for 1.5-3 hours. Solid-liquid separation is performed, and the solid is washed and dried to constant weight to obtain a modified carbon support. The synergistic effect of ultrasonic cavitation and phosphoric acid enhances the diffusion of phosphoric acid into the pores, and phosphorus-containing anchoring sites such as C-O-P, P=O, and P-OH are constructed on the surface of the carbon support. Subsequently, without high-temperature carbonization or reactivation, and without metal loading, the modified carbon support is directly mixed uniformly with sulfuric acid and hot-sulfonated at 150-170°C for 2-4 hours. After cooling to room temperature, it is washed with deionized water until neutral and dried to obtain a carbon-based solid acid catalyst. When used in the esterification reaction of oleic acid and methanol, the oleic acid conversion rate of the carbon-based solid acid catalyst is not less than 80%, and the oleic acid conversion rate after five reuses is not less than 70%.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a method for preparing highly stable, high-acid-density carbon-based solid acids by ultrasound-assisted phosphoric acid co-activation, belonging to the field of solid acid catalytic materials technology. Background Technology

[0002] Traditional liquid acid catalysts (such as sulfuric acid) are widely used in acid-catalyzed reactions such as esterification and hydrolysis. However, liquid acids typically suffer from problems such as strong corrosiveness to equipment, difficulty in separating them from the products after the reaction, difficulty in direct recycling, and high costs for waste acid treatment. Solid acid catalysts can be separated from the reaction system through filtration, centrifugation, and other methods. Among them, carbon-based solid acids have become important candidate materials to replace traditional liquid acids due to their diverse carbon sources, tunable surface chemistry, and ease of separation and recovery.

[0003] Currently, carbon-based solid acids are mainly prepared using direct sulfonation, carbonization-sulfonation, or hydrothermal carbonization-sulfonation methods. However, untreated carbon supports often have narrow pores, insufficient connectivity, or sites located inside the particles, making some acidic sites difficult for reactants to access. Therefore, existing processes still fall short in simultaneously improving total acid density and the accessibility of acidic sites, especially in meeting the mass transfer and catalytic requirements of larger organic molecules such as free fatty acid esterification.

[0004] To improve the pore structure and surface chemical properties of carbon supports, existing technologies have gradually adopted chemical reagents such as phosphoric acid, potassium hydroxide, and zinc chloride to activate carbon-containing raw materials or carbon materials. Among these, phosphoric acid activation does not introduce metal activators, has a relatively mild treatment effect, and can affect the formation of pores in carbon materials and the composition of oxygen- and phosphorus-containing functional groups on the surface, thus becoming a commonly used method for carbon material modification. Existing technologies have disclosed technical routes that combine phosphoric acid treatment with subsequent thermal activation and sulfonation. For example, patent CN110846194A discloses using biomass such as wood flour as a carbon source, mixing and impregnating it with phosphoric acid and drying it, followed by incomplete carbonization and activation at 350–550 °C, and then sulfonation using concentrated sulfuric acid, fuming sulfuric acid, or chlorosulfonic acid. The phosphoric acid used in this method is mainly used to promote high-temperature carbonization and pore structure formation of biomass. The treated object is not a pre-formed carbon support, and it still requires high-temperature carbonization activation and subsequent sulfonation, resulting in numerous steps and high energy consumption. High-temperature treatment may also cause decomposition or rearrangement of some oxygen- and phosphorus-containing surface structures, making it difficult to synergistically regulate the pore accessibility and surface functional group composition of the carbon support before sulfonation. To compensate for insufficient mass transfer, existing processes usually require extended impregnation time or additional thermal activation steps, further increasing energy consumption and process complexity. Patent CN103771409A uses crop straw as raw material, first performing anaerobic carbonization at 700 °C, then treating with phosphoric acid, followed by washing, drying, molding, and heat treatment at 260 °C. It is mainly used to prepare molded biomass activated carbon and does not involve subsequent sulfonation or the construction of acidic sites on carbon-based solids. Patent CN106693961A discloses a method for low-temperature phosphoric acid impregnation of pre-formed activated carbon, specifically impregnation in 0.1–3 mol / L phosphoric acid at 20–40 °C for 12 h, followed by filtration, drying, and reactivation at 500 °C for 60 min under a nitrogen atmosphere, before loading with palladium active components. While this patent involves pre-formed activated carbon and low-temperature phosphoric acid impregnation, it requires reactivation at 500 °C and Pd loading after impregnation, meaning the final catalytic activity originates from Pd metal, rather than through sulfonation to construct –SO3H acidic sites. Furthermore, the phosphoric acid impregnation step does not involve ultrasound, and sulfonation is not performed directly after impregnation. Patent CN114471559A discloses a Cu / AC denitrification catalyst using coconut shell activated carbon as a support, where ultrasound is used for aqueous pretreatment before phosphoric acid treatment and for copper sulfate impregnation after phosphoric acid treatment. The phosphoric acid treatment step itself does not involve ultrasound, and the final active components are CuO and Cu2O. It is evident that none of the above technologies disclose a method for directly applying ultrasound during the low-temperature contact process between pre-formed activated carbon and phosphoric acid, and for directly sulfonating the carbon after treatment without intermediate high-temperature carbonization or reactivation. Summary of the Invention

[0005] To address the shortcomings of existing technologies, such as insufficient activation of carbon supports, low loading of sulfonic acid groups, and poor stability, this invention proposes a method for preparing highly stable, high-acid-density carbon-based solid acids through ultrasound-assisted phosphoric acid co-activation. Ultrasound is introduced into the low-temperature phosphoric acid pretreatment process. The extreme physical conditions generated by the ultrasonic cavitation effect drive the transport of phosphoric acid molecules into the pores of the carbon support and induce the reconstruction of the carbon support surface chemistry. This not only efficiently creates pores but also generates high-density phosphorus-containing functional groups (such as COP, P=O, P-OH) on the inner and outer surfaces of the pores as chemical anchors. Subsequently, without high-temperature carbonization or reactivation, and without metal loading, the modified carbon support is directly subjected to thermal sulfonation with sulfuric acid. Ultrasound-assisted phosphoric acid co-activation enables the high-stability chemical bonding and anchoring (POS bonds) of sulfonic acid groups (-SO3H) during thermal sulfonation, improving the problem of easy sulfonic acid group detachment in traditional methods.

[0006] A method for preparing highly stable, high-acid-density carbon-based solid acids by ultrasound-assisted phosphoric acid co-activation includes the following specific steps: (1) The carbon support is added to the phosphoric acid solution and mixed evenly to obtain a mixture. The mixture is then activated by ultrasound-assisted phosphoric acid synergistic activation at a temperature of 25~60℃ for 1.5~3h. The solid and liquid are separated, and the solid is washed and dried to constant weight to obtain the modified carbon support. (2) Mix the modified carbon support with sulfuric acid evenly, heat sulfonate at 150~170℃ for 2~4 h, cool to room temperature, wash with deionized water until neutral, and dry to obtain carbon-based solid acid catalyst.

[0007] Preferably, in step (1), the mass concentration of the phosphoric acid solution is 8-25%, and the solid-liquid ratio of the carbon support to the phosphoric acid solution (g:L) is 1:2.5-4.

[0008] Preferably, in step (1), the ultrasonic frequency is 25~28kHz and the ultrasonic power density is 500~900W / L.

[0009] Preferably, in step (2), the sulfuric acid concentration is 4~6 mol / L, and the solid-liquid ratio of the modified carbon support to sulfuric acid is 1:8~10 g:L.

[0010] Preferably, the acid density of the carbon-based solid acid catalyst in step (2) is 3.0~3.5 mmol / g.

[0011] The mechanism of this invention for preparing highly stable, high-acid-density carbon-based solid acids through ultrasound-assisted phosphoric acid synergistic activation is as follows: On the one hand, ultrasound-assisted phosphoric acid synergistic activation breaks down dead zones and liquid film mass transfer resistance within the carbon support pores through physical cavitation, significantly increasing the specific surface area and accessible pore volume. On the other hand, ultrasound energy promotes the chemical reaction between phosphoric acid and the active sites at the carbon edges, stably and uniformly constructing phosphorus-containing functional groups, represented by COP, P=O, and P-OH, on the carbon framework surface and pore inner walls. These functional groups act as anchor points during subsequent thermal sulfonation, forming stable POS covalent bonds with -SO3H, thereby achieving highly dispersed, high-density, and chemically anchored sulfonic acid groups that resist detachment. This is fundamentally different from traditional methods where sulfonic acid groups mainly rely on weak physical adsorption or binding with unstable oxygen-containing groups. This synergistic mechanism is not a simple superposition of ultrasound physical treatment and phosphoric acid chemical modification, but rather involves constructing phosphorus-containing anchor points on pre-formed activated carbon through low-temperature ultrasound-phosphoric acid synergy, followed by direct thermal sulfonation to form POS bonds, thus significantly improving the stability of sulfonic acid groups while increasing acid density.

[0012] The beneficial effects of this invention are: (1) The present invention can improve the mass transfer conditions in the static impregnation process of phosphoric acid: the ultrasonic cavitation effect is introduced into the phosphoric acid activation process, and the micro-jet and shock wave generated by cavitation drive the phosphoric acid molecules to penetrate into the deep pores of the carbon support, thereby enhancing the regulation of the pore structure and surface chemical properties of the carbon support by phosphoric acid pretreatment. (2) This invention is not limited to simple pore structure regulation, but creatively utilizes ultrasound-phosphoric acid synergy to generate a large number of stable phosphorus-containing groups such as COP / P=O on carbon support as chemical anchors, thereby achieving high-stability chemical bonding anchoring (POS bond) of sulfonic acid groups and solving the problem of easy loss of sulfonic acid groups in catalytic reactions; (3) The ultrasonic pretreatment of the present invention is carried out under mild conditions of normal pressure and 25~60℃, and the hot sulfonation is carried out in a closed reaction vessel at 150~170℃, which can achieve an acid density of ≥3.0mmol / g, which is ≥15% higher than the conventional method; the catalyst exhibits excellent activity and cycle stability in the esterification reaction, and the conversion rate is not less than 70% after 5 cycles; (4) The optimal window effect of ultrasonic power density on synergistic activation effect (500~900 W / L) of the present invention; below this window, the activation is insufficient, and above this window, the carbon skeleton will collapse and the surface anchor point will be destroyed due to excessive cavitation, which provides a clear technical guidance for the precise control of the process. Attached Figure Description

[0013] Figure 1 High-resolution X-ray photoelectron spectra of conventionally phosphoric acid pretreated carbon support PC-C and ultrasound-assisted phosphoric acid pretreated carbon support PC-U are shown. Figure 1(a) is the p 2p spectrum of PC-C. Figure 1 (b) is the P 2p spectrum of PC-U. Figure 1 (c) shows the O 1s spectrum of PC-C. Figure 1 (d) is the O 1s spectrum of PC-U; Figure 2 Fourier transform infrared spectra of samples with different pretreatments and sulfonation, where, Figure 2 (a) Fourier transform infrared spectra of the original carbon support AC, conventional phosphoric acid pretreated carbon support PC-C, and ultrasound-assisted phosphoric acid pretreated carbon support PC-U. Figure 2 (b) are Fourier transform infrared spectra of the original carbon support AC, carbon-based solid acid CBSA-C obtained by sulfonation after conventional phosphoric acid pretreatment, and carbon-based solid acid CBSA-U obtained by sulfonation after ultrasonic-assisted phosphoric acid pretreatment. Detailed Implementation

[0014] The present invention will be further described in detail below with reference to specific embodiments, but the scope of protection of the present invention is not limited to the content described.

[0015] Example 1: A method for preparing highly stable, high-acid-density carbon-based solid acids by ultrasound-assisted phosphoric acid co-activation, the specific steps of which are as follows: (1) Commercial wood-based activated carbon was added to a 10% phosphoric acid solution and mixed evenly to obtain a mixture (the solid-liquid ratio of commercial wood-based activated carbon to phosphoric acid solution was 1:3 g:L). The mixture was then subjected to ultrasonic-assisted phosphoric acid co-activation at 40℃ for 2.5 h. The solid and liquid were separated, and the solid was washed and dried to constant weight to obtain a modified carbon carrier. The ultrasonic frequency was 25 kHz and the ultrasonic power density was 720 W / L. (2) Mix the modified carbon support with sulfuric acid of 5 mol / L (the solid-liquid ratio of the modified carbon support to sulfuric acid is 1:10 g:L), heat sulfonate at 160℃ for 3 h, cool to room temperature, wash with deionized water until neutral, and dry to obtain carbon-based solid acid catalyst. The carbon-based solid acid catalyst in this embodiment has an acid density of 3.37 mmol / g and achieves a conversion rate of 89.2% in the oleic acid-methanol esterification reaction. After being recycled 5 times, the conversion rate is 78%.

[0016] Comparative Example 1: The difference between this comparative example and Example 1 is that step (1) does not introduce ultrasonic assistance, but directly activates the product in phosphoric acid solution; The comparative carbon-based solid acid catalyst has an acid density of 2.73 mmol / g and achieves a conversion rate of 79.5% in the oleic acid-methanol esterification reaction. After being recycled 5 times, the conversion rate is 68%. High-resolution X-ray photoelectron spectra of the conventional phosphoric acid pretreated carbon support PC-C and the ultrasound-assisted phosphoric acid pretreated carbon support PC-U of Example 1 are shown below. Figure 1 ,in, Figure 1 (a) is the p 2p spectrum of PC-C. Figure 1 (b) is the P 2p spectrum of PC-U. Figure 1 (c) shows the O 1s spectrum of PC-C. Figure 1 (d) shows the O 1s spectrum of PC-U; the peak areas of components in PC-U belonging to phosphorus-containing anchoring structures such as COP and P=O increased significantly, proving that ultrasound-assisted activation promoted the generation of more chemical anchors; Fourier transform infrared spectra of samples with different pretreatments and sulfonation are shown below. Figure 2 ,in, Figure 2 (a) Fourier transform infrared spectra of the original carbon support AC, conventional phosphoric acid pretreated carbon support PC-C, and ultrasound-assisted phosphoric acid pretreated carbon support PC-U. Figure 2 (b) Fourier transform infrared spectra of the original carbon support AC, the carbon-based solid acid CBSA-C obtained by sulfonation after conventional phosphoric acid pretreatment, and the carbon-based solid acid CBSA-U obtained by sulfonation after ultrasound-assisted phosphoric acid pretreatment; the carbon-based solid acid (CBSA-U) obtained by sulfonation after ultrasound synergistic activation is shown in the spectrum at 1180 cm⁻¹. -1 The absorption peaks nearby (attributed to the symmetric stretching vibration of the POS bond) are much stronger than those of the conventional sample (CBSA-C), directly confirming that the sulfonic acid group is stably anchored to the carbon support through chemical bonding. After introducing ultrasound assistance, the total acid density of the catalyst increased from 2.73 mmol / g to 3.37 mmol / g, an increase of 23.4%; from Figure 1 and 2 It can be seen that the improvement is not solely due to the increase in physical specific surface area (BET from 979.2 m²). 2 ·g -1 Increased to 1039.5 m 2 ·g -1 More importantly, it stems from a significant increase in the number of chemical anchor points; peak fitting results of XPS P 2p spectra show that after ultrasonic synergistic activation, the relative content of phosphorus-containing groups such as COP and P=O on the carbon support surface increases significantly; these groups react with -SO3H during thermal sulfonation to form stable POS covalent bonds (at 1180 cm⁻¹ in FTIR). -1 (The absorption peak is significantly enhanced). This chemically anchored structure is the fundamental reason why the activity (oleic acid conversion rate) of the solid acid catalyst can still be maintained at more than 78% after 5 cycles of use, while conventional samples can only maintain about 68%.

[0017] Comparative Example 2: The difference between this comparative example and Example 1 is that deionized water was used instead of the phosphoric acid solution in step (1) to obtain the comparative catalyst (denoted as CBSA-1); the acid density of the solid acid catalyst in this comparative example is only 2.19 mmol·g. -1 This indicates that the ability of simple low-temperature hydrothermal pretreatment to introduce acidic groups is extremely limited.

[0018] Comparative Example 3: The difference between this comparative example and Example 1 is that the ultrasonic power density is 1200 W / L; The acid density of the solid acid catalyst in this comparative example drops sharply to 2.18 mmol·g. -1 Therefore, excessively high ultrasonic power density can lead to excessive cavitation effect. The strong shock waves and shear forces generated may destroy the phosphorus-containing chemical anchors already formed on the carbon support surface or cause partial collapse of the microporous structure of the carbon skeleton, thereby reducing the effective anchoring points of sulfonic acid groups.

[0019] Example 2: A method for preparing highly stable, high-acid-density carbon-based solid acids by ultrasound-assisted phosphoric acid co-activation, the specific steps of which are as follows: (1) Coconut shell activated carbon was added to a 20% phosphoric acid solution and mixed evenly to obtain a mixture (the solid-liquid ratio of coconut shell activated carbon to phosphoric acid solution was 1:2.5 g:L). The mixture was then subjected to ultrasonic-assisted phosphoric acid co-activation at 60℃ for 2 hours. The solid and liquid were separated, and the solid was washed and dried to constant weight to obtain the modified carbon carrier. The ultrasonic frequency was 28kHz and the ultrasonic power density was 900W / L. (2) Mix the modified carbon support with sulfuric acid of 4 mol / L (the solid-liquid ratio of the modified carbon support to sulfuric acid is 1:9 g:L), heat sulfonate at 170℃ for 2.5 h, cool to room temperature, wash with deionized water until neutral, and dry to obtain carbon-based solid acid catalyst. The carbon-based solid acid catalyst in this embodiment has an acid density of 3.02 mmol / g and achieves a conversion rate of 86.3% in the oleic acid-methanol esterification reaction. After being recycled 5 times, the conversion rate is 75.2%.

[0020] Example 3: A method for preparing highly stable, high-acid-density carbon-based solid acids by ultrasound-assisted phosphoric acid co-activation, the specific steps of which are as follows: (1) Coconut shell activated carbon was added to a phosphoric acid solution with a mass concentration of 8% and mixed evenly to obtain a mixture (the solid-liquid ratio of coconut shell activated carbon to phosphoric acid solution was 1:4 g:L). The mixture was then subjected to ultrasonic-assisted phosphoric acid co-activation at 25℃ for 3 hours. The solid and liquid were separated, and the solid was washed and dried to constant weight to obtain a modified carbon carrier. The ultrasonic frequency was 25kHz and the ultrasonic power density was 600W / L. (2) Mix the modified carbon support with sulfuric acid of 6 mol / L (the solid-liquid ratio of the modified carbon support to sulfuric acid is 1:8 g:L), heat-sulfonate at 150℃ for 4 h, cool to room temperature, wash with deionized water until neutral, and dry to obtain carbon-based solid acid catalyst. The carbon-based solid acid catalyst in this embodiment has an acid density of 3.43 mmol / g and achieves a conversion rate of 89.95% in the oleic acid-methanol esterification reaction. After being recycled 5 times, the conversion rate is 83.2%.

[0021] The specific embodiments of the present invention have been described in detail above. However, the present invention is not limited to the above embodiments. Within the scope of knowledge possessed by those skilled in the art, various changes can be made without departing from the spirit of the present invention.

Claims

1. A method for preparing highly stable, high-acid-density carbon-based solid acids by ultrasound-assisted phosphoric acid co-activation, characterized in that, The specific steps are as follows: (1) The carbon support is added to the phosphoric acid solution and mixed evenly to obtain a mixture. The mixture is then activated by ultrasound-assisted phosphoric acid synergistic activation at a temperature of 25~60℃ for 1.5~3h. The solid and liquid are separated, and the solid is washed and dried to constant weight to obtain the modified carbon support. (2) Mix the modified carbon support with sulfuric acid evenly, heat sulfonate at 150~170℃ for 2~4 h, cool to room temperature, wash with deionized water until neutral, and dry to obtain carbon-based solid acid catalyst.

2. The method for preparing highly stable, high-acid-density carbon-based solid acids by ultrasound-assisted phosphoric acid co-activation according to claim 1, characterized in that: Step (1) The mass concentration of the phosphoric acid solution is 8~25%, and the solid-liquid ratio of the carbon support to the phosphoric acid solution is 1:2.5~4 g:L.

3. The method for preparing highly stable, high-acid-density carbon-based solid acids by ultrasound-assisted phosphoric acid co-activation according to claim 1, characterized in that: Step (1) The ultrasonic frequency is 25~28kHz and the ultrasonic power density is 500~900W / L.

4. The method for preparing highly stable, high-acid-density carbon-based solid acids by ultrasound-assisted phosphoric acid co-activation according to claim 1, characterized in that: Step (2) The sulfuric acid concentration is 4~6 mol / L, and the solid-liquid ratio of the modified carbon support to sulfuric acid is 1:8~10 g:L.

5. The method for preparing highly stable, high-acid-density carbon-based solid acids by ultrasound-assisted phosphoric acid co-activation according to claim 1, characterized in that: Step (2) The acid density of the carbon-based solid acid catalyst is 3.0~3.5 mmol / g.

Citation Information

Patent Citations

  • Preparation method for molded biomass active carbon with crop straw as raw material

    CN103771409A

  • Palladium-carbon catalyst and preparation method and application thereof

    CN106693961A

  • Method for improving Baijiu quality by carbon-based solid acid

    CN110846194A

  • CO-SCR denitration anti-Zn poisoning Cu / AC catalyst and preparation method and application thereof

    CN114471559A