A method for segmented gradient cooling of weld seams in iron spray cans

By using a segmented gradient cooling method to independently cool the weld seams of the iron spray tank body, the temperature gradient problem between the weld center and the heat-affected zone was solved, which improved the uniformity of weld microstructure and crack resistance, extended fatigue life, and increased production efficiency.

CN123103265APending Publication Date: 2026-11-17GUANGZHOU HENGYU IRON-PRINTTING & CAN MAKING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611494336.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-23
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing cooling methods cannot effectively control the temperature gradient of the weld seam of the iron spray tank body, resulting in inconsistent microstructure and properties between the weld center and the heat-affected zone, as well as residual stress concentration, which affects the crack resistance and fatigue life of the weld seam.

Method used

A segmented gradient cooling method is adopted, including a rapid cooling section, a slow cooling section, and a temperature equalization section, to independently cool the weld center and the heat-affected zone. By setting different cooling rates and temperature trajectories, and combining air mist mixed spray, compressed air, and low-intensity airflow cooling, precise temperature control of the weld is achieved.

Benefits of technology

It effectively solves the temperature gradient problem between the center of thin-walled welds and the heat-affected zone, improves the consistency of weld microstructure and crack resistance, extends fatigue life, and improves production efficiency and cooling quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123103265A_ABST
    Figure CN123103265A_ABST
Patent Text Reader

Abstract

This invention belongs to the field of welding technology. It relates to a segmented gradient cooling method for the weld seam of an iron spray can, comprising the following steps: S1: Setting the cooling temperature trajectory, based on the continuous cooling transition curve of the iron material; S2: Setting segmented gradient cooling; S3: Zoned cooling control, dividing the weld seam into multiple cooling zones along its length, and within each cooling zone, dividing the weld seam into a central region and a heat-affected zone along its cross-sectional direction. Each cooling zone independently executes a rapid cooling section, a slow cooling section, and a homogenization section. In the rapid cooling section, a first cooling temperature is applied to the central region of the weld seam, and a second cooling temperature lower than the first cooling temperature is applied to the heat-affected zone. The second cooling temperature is 50% to 70% of the first cooling temperature. This invention solves the problem that existing cooling methods cannot effectively avoid welding deformation and thermal stress concentration in thin-walled structures.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of welding technology, and specifically relates to a method for segmented gradient cooling of the weld seam of an iron spray can. Background Technology

[0002] Spray cans, as a common packaging container, are widely used in cosmetics, pharmaceuticals, daily chemicals, food, and other fields. Iron spray cans hold an important position in the market due to their good mechanical strength, barrier properties, and cost advantages. The can body is typically made of thin-walled metal sheets through stamping, welding, and other processes. The wall thickness is usually only 0.15mm to 0.35mm, and the quality of the welds directly affects the can's sealing performance, pressure resistance, and safety during use.

[0003] Currently, the main welding methods for iron spray can bodies include resistance welding and laser welding. During the welding process, the temperature in the weld area rises rapidly, reaching 800℃~1200℃, forming a molten pool. After welding, how to quickly and effectively cool the weld while ensuring the weld microstructure and residual stress control are key issues affecting product quality.

[0004] Currently, weld cooling methods typically employ compressed air or inert gas to purge and cool the weld. While this method provides good cooling uniformity, the cooling rate is relatively low, usually between 10°C / s and 30°C / s. This makes it impossible to achieve rapid cooling in the high-temperature range of 600°C to 800°C, resulting in insufficient grain refinement. Furthermore, due to the small heat capacity and rapid heat dissipation of thin-walled structures, precise temperature control is difficult to achieve.

[0005] Meanwhile, the walls of iron spray cans are only 0.15mm to 0.35mm thick, constituting a thin-walled structure. During cooling, a significant temperature gradient, typically 100℃ to 150℃, exists between the weld center and the heat-affected zone. This temperature gradient leads to rapid cooling at the weld center, easily forming fine grains, while the heat-affected zone cools slowly, resulting in coarse grains. This causes inconsistencies in their mechanical properties. Furthermore, the thermal stress generated by the temperature gradient concentrates at the weld boundary, easily leading to stress corrosion cracking and fatigue crack initiation. Existing cooling methods neglect the temperature gradient issue between the thin-walled weld center and the heat-affected zone, employing a uniform cooling strategy. This fails to effectively control the uniformity of temperature distribution, resulting in inconsistent microstructure and residual stress concentration, severely impacting the weld's crack resistance and fatigue life. Summary of the Invention

[0006] To address the aforementioned problems in the prior art, this invention provides a segmented gradient cooling method for the weld seams of an iron spray can, which solves the problem that existing cooling methods cannot effectively prevent welding deformation and thermal stress concentration in thin-walled structures.

[0007] The objective of this invention can be achieved through the following technical solution: a method for segmented gradient cooling of the weld seam of an iron spray can, comprising the following steps: S1: Cooling temperature trajectory setting, based on the continuous cooling transformation curve of ferrous materials to set the cooling temperature trajectory; S2: Segmented gradient cooling setting, the cooling temperature trajectory includes a rapid cooling section, a slow cooling section and a uniform temperature section, the rapid cooling section is to reduce the welding completion temperature to a first target temperature at a first cooling rate, the slow cooling section is to reduce the temperature from the first target temperature to a second target temperature at a second cooling rate, the second cooling rate is less than the first cooling rate, and the uniform temperature section is to maintain the temperature near a third target temperature for a predetermined time. S3: Zoned cooling control. The weld is divided into multiple cooling zones along the length of the weld. Within each cooling zone, the weld is divided into a central region and a heat-affected zone along the cross-sectional direction of the weld. Each cooling zone independently performs a rapid cooling section, a slow cooling section, and a temperature equalization section. In the rapid cooling section, a first cooling temperature is applied to the central region of the weld, and a second cooling temperature lower than the first cooling temperature is applied to the heat-affected zone. The second cooling temperature is 50% to 70% of the first cooling temperature.

[0008] As a preferred embodiment of the present invention, the number of cooling zones is ≥3, and three adjacent zones are simultaneously in the rapid cooling section, the slow cooling section, and the uniform temperature section.

[0009] As a preferred embodiment of the present invention, the length L of the cooling partition is determined according to the following formula: L = v × t; Where v is the welding speed and t is the duration of a single cooling stage.

[0010] As a preferred embodiment of the present invention, the first target temperature is 500℃~750℃, the second target temperature is 250℃~450℃, and the third target temperature is 100℃~180℃.

[0011] As a preferred embodiment of the present invention, the first cooling rate is 50℃ / s to 200℃ / s, the second cooling rate is 5℃ / s to 30℃ / s, and the predetermined time of the temperature equalization section is 2s to 10s.

[0012] As a preferred embodiment of the present invention, the width of the weld center region is 40% to 60% of the weld width, and the heat-affected zone is located on both sides of the weld center region, with the width of the heat-affected zone being 20% ​​to 30% of the weld width.

[0013] As a preferred embodiment of the present invention, the rapid cooling section employs air-mist mixed spray cooling, the slow cooling section employs compressed air cooling, and the temperature equalization section employs low-intensity airflow cooling.

[0014] As a preferred embodiment of the present invention, in step S3, the temperature gradient difference between the weld center region and the heat-affected zone is 50°C to 80°C.

[0015] As a preferred technical solution of the present invention, in step S3, the weld temperature of each cooling zone is collected in real time by a temperature sensor, the actual temperature is compared with the cooling temperature trajectory, and the cooling medium parameters of each cooling zone are adjusted according to the comparison result.

[0016] As a preferred embodiment of the present invention, the temperature sensor is an infrared thermometer, and the temperature sensors are arranged in each cooling zone along the length of the weld, with at least two temperature sensors arranged in each cooling zone.

[0017] The beneficial effects of this invention are as follows: by using a three-stage gradient cooling based on the CCT curve, the weld is divided into zones and cooled independently, which solves the problem that existing cooling methods ignore the temperature gradient between the center of the thin-walled weld and the heat-affected zone, resulting in inconsistent microstructure and residual stress concentration, which seriously affects the crack resistance and fatigue life of the weld. Attached Figure Description

[0018] To facilitate understanding by those skilled in the art, the present invention will be further described below with reference to the accompanying drawings.

[0019] Figure 1 This is a flowchart of the cooling method of the present invention. Detailed Implementation

[0020] To further illustrate the technical means and effects of the present invention in achieving its intended purpose, the following detailed description of the specific implementation methods, structures, features, and effects of the present invention, in conjunction with the accompanying drawings and preferred embodiments, is provided.

[0021] Please see Figure 1 This embodiment provides a segmented gradient cooling method for the weld seam of an iron spray can, including the following steps: S1: Cooling Temperature Trajectory Setting. Before cooling begins, a cooling temperature trajectory is first set based on the Continuous Cooling Transformation (CCT) curve of the ferrous material. The CCT curve reflects the temperature-time-structure relationship of the ferrous material's transformation from austenite to different microstructures (ferrite, pearlite, bainite, martensite, etc.) at different cooling rates. Specifically, the operator determines the corresponding phase transformation microstructure type and phase transformation temperature range at different cooling rates based on the CCT curve of the ferrous material used, and then sets a target cooling temperature trajectory that includes three continuous stages: a rapid cooling stage, a slow cooling stage, and a homogenization stage. This trajectory records the expected path of weld temperature change over time from the weld completion temperature to the end of cooling. S2: Segmented gradient cooling setting. After welding, the weld seam is subjected to gradient cooling in three stages: rapid cooling, slow cooling, and isothermal cooling, according to a preset cooling temperature trajectory. Rapid cooling stage: Immediately after welding, the weld seam is rapidly cooled at the first cooling rate, reducing the weld temperature from the welding completion temperature to the first target temperature. The core purpose of rapid cooling is to inhibit austenite grain growth through rapid cooling. The longer the weld metal remains at high temperatures, the more likely the grains will coarsen, thus deteriorating the weld's strength and toughness. Rapid cooling allows the weld metal to quickly pass through the austenite recrystallization temperature range, controlling the grain size within a small range and achieving fine-grain strengthening. Slow cooling stage: After the weld temperature drops to the first target temperature, the cooling rate is reduced to the second cooling rate, which is lower than the first cooling rate, allowing the weld temperature to slowly decrease from the first target temperature to the second target temperature. After the rapid cooling stage, the weld temperature has dropped to the sensitive temperature range where austenite gradually transforms into ferrite, pearlite, and bainite. If cooling continues at a high rate, the weld microstructure may transform into brittle and hard phases such as martensite, leading to weld embrittlement. Therefore, the slow cooling section reduces the cooling rate, allowing the weld microstructure to transform along the ideal path in the CCT curve, obtaining a microstructure dominated by fine-grained ferrite and pearlite, while avoiding the formation of brittle and hard phases such as martensite. Furthermore, reducing the cooling rate helps to decrease the temperature gradient between the weld and the base metal, reducing thermal stress concentration and preventing deformation or cracking of the thin-walled tank due to thermal stress. In the isothermal equalization section, once the weld temperature drops to the second target temperature, active cooling is stopped or the temperature is switched to a holding mode, maintaining the weld temperature near the third target temperature for a predetermined time. After the rapid cooling and slow cooling sections, some residual stress still exists inside the weld. This residual stress is caused by uneven temperature distribution and inconsistent phase transformation volume changes in different areas of the weld during the cooling process. The isothermal equalization section stops active cooling, maintaining the weld temperature in a lower temperature range for a period of time, promoting uniform temperature within the weld, allowing residual stress to be fully released and eliminated, and stabilizing the microstructure. S3: Zoned cooling control. The weld is divided into multiple cooling zones along its length. Within each cooling zone, the weld is further divided into a central region and a heat-affected zone (HAZ) along its cross-section. Each cooling zone independently executes a rapid cooling phase, a slow cooling phase, and a homogenization phase. In the rapid cooling phase, a first cooling temperature is applied to the central region, while a second cooling temperature, lower than the first, is applied to the HAZ. The second cooling temperature is 50%–70% of the first cooling temperature. Due to the thin-walled structure of the iron spray can, the temperature distribution and cooling requirements of different regions on the weld cross-section vary significantly. The central region of the weld is where the welding heat input is most concentrated and the temperature is highest, exhibiting the strongest tendency for grain growth. It requires the strongest cooling intensity for rapid cooling to refine the grains. The HAZ, adjacent to the central region, has a lower peak temperature than the weld center but higher than the base metal. Applying the same cooling intensity as the weld center would result in an excessively large temperature gradient between the HAZ and the base metal, leading to thermal stress concentration and welding deformation. Therefore, applying a lower cooling intensity to the heat-affected zone (HAZ) ensures sufficient cooling while controlling the temperature gradient along the weld cross-section within a reasonable range, preventing deformation or cracking of the thin-walled tank due to excessive temperature differences. Furthermore, dividing the weld into multiple cooling zones along its length and controlling them independently is crucial because the heat input, peak temperature, and cooling conditions differ between the initial, intermediate, and final welding sections as the welding heat source moves along the weld length. Independent control of each zone enables precise temperature regulation along the weld length.

[0022] By using a three-stage gradient cooling system based on the CCT curve, and simultaneously partitioning and cooling the weld independently, the problem of existing cooling methods neglecting the temperature gradient between the center of thin-walled welds and the heat-affected zone, leading to inconsistent microstructure and residual stress concentration, which seriously affects the crack resistance and fatigue life of the weld, is solved.

[0023] Different positions along the length of the weld are in different cooling stages at the same time: the position where welding has just been completed is in the rapid cooling section, the position where welding was completed slightly earlier is in the slow cooling section, and the position where welding was completed even earlier is in the isotherm section. Therefore, in order to ensure the continuity and integrity of the cooling process and significantly improve production efficiency and cooling quality, in this embodiment, during continuous welding, rapid cooling module, slow cooling module, and isotherm treatment module are arranged sequentially along the length of the weld. When the welding heat source moves forward, the weld section that has just been welded enters the range of action of the rapid cooling module and begins rapid cooling; after moving forward, this section enters the range of action of the slow cooling module and begins slow cooling; after moving forward again, it enters the range of action of the isotherm treatment module and begins isotherm treatment. In this way, the three adjacent zones are in the rapid cooling section, slow cooling section and uniform temperature section at the same time, respectively, realizing the continuous synchronous operation of the cooling process and the welding process. By setting up at least 3 cooling zones and making the three adjacent zones simultaneously in three different cooling stages, the continuous synchronous operation of the cooling process and the welding process is realized. Moreover, each zone works independently without interfering with each other, ensuring the independent controllability of different cooling stages, and greatly improving production efficiency and cooling quality.

[0024] To avoid uneven temperature distribution within each freezing zone, in this embodiment, the length L of the cooling zone is determined according to the following formula: L = v × t; Where v is the welding speed and t is the duration of a single cooling stage.

[0025] During welding, the heat source moves forward along the length of the weld at a welding speed v, and each point on the weld successively experiences the welding thermal cycle. The duration of a single cooling stage (such as a quenching stage) is t. During this time period, the distance the heat source moves is v × t, which corresponds exactly to the length of the weld that is simultaneously in the same cooling stage. Therefore, using L = v × t as the length of the cooling zone ensures that each cooling zone is synchronized with the movement of the welding heat source in time. When the heat source moves one zone length, that zone completes exactly one cooling stage, avoiding the situation where the cooling stages are misaligned or overlapped due to a mismatch between the zone length and the welding speed, resulting in inconsistent cooling effects.

[0026] Since the target temperature settings for each segment must be based on the phase transformation temperature range in the CCT curve of ferrous materials, the austenite-ferrite transformation temperature is typically between 750°C and 850°C, the austenite-pearlite transformation temperature is approximately 500°C to 750°C, the bainite transformation temperature is approximately 250°C to 550°C, and the martensite transformation temperature is typically between 250°C and 450°C, depending on the carbon content and alloying elements. Therefore, to avoid problems such as coarse grains, martensite embrittlement, or excessive residual stress caused by unreasonable temperature settings, this embodiment sets the first target temperature of the quenching segment to 500°C to 750°C. This is because above this temperature range, the weld metal is still in a high-temperature state of austenite or austenite + ferrite, with a significant tendency for grain growth, requiring rapid cooling through this range to suppress grain growth. The first target temperature is set at 500℃~750℃ to ensure that the rapid cooling section covers the sensitive temperature range for austenite recrystallization and grain growth, allowing the weld to be rapidly cooled to below a safe temperature before significant grain growth. The second target temperature for the slow cooling section is set at 250℃~450℃ because if the cooling rate is too fast within this range, austenite may transform into martensite, forming a brittle and hard structure. Setting the second target temperature at 250℃~450℃ ensures that the slow cooling section covers the sensitive temperature range for martensitic transformation. Within this range, slow cooling at a lower rate allows sufficient time for austenite to transform into ferrite, pearlite, or bainite, avoiding martensite formation. Simultaneously, 250℃~450℃ is also the temperature range where thermal stress is most concentrated; slow cooling helps reduce the temperature gradient and lower thermal stress. The third target temperature for the isotherm section is set at 100℃~180℃ because below this temperature range, the phase transformation of the weld is essentially complete, and residual stress becomes the main factor affecting weld performance. The uniform temperature treatment within the range of 100℃ to 180℃ can make the internal temperature of the weld more uniform and promote the release of residual stress, while avoiding the tempering of the structure or the degradation of performance caused by excessive temperature. By strictly following the phase transformation law of the CCT curve of ferrous materials when setting the target temperature of each segment, the precise matching between the cooling rate and the phase transformation requirements is ensured, avoiding problems such as coarse grains, martensite embrittlement or excessive residual stress caused by unreasonable temperature settings.

[0027] Since the setting of the cooling rate of each stage directly determines the final metallographic structure of the weld, in order to ensure that the weld microstructure and residual stress can be precisely controlled, in this embodiment, the first cooling rate is set to 50℃ / s to 200℃ / s. This is because for ferrous materials, when the cooling rate is lower than 50℃ / s, the austenite grains stay in the high temperature range for a longer time, and the grains tend to coarsen, resulting in a decrease in weld strength and toughness. While when the cooling rate is higher than 200℃ / s, although the grain refinement effect is better, the excessively fast cooling will generate an excessive temperature gradient and thermal stress, which can lead to welding deformation or even cracking for thin-walled tanks. Therefore, a rapid cooling rate range of 50℃ / s to 200℃ / s can effectively refine the grains and control the thermal stress within the range that the thin-walled tank can withstand. The second cooling rate is set at 5℃ / s to 30℃ / s because in the slow cooling section, when the temperature drops from the first target temperature of 500℃ to 750℃ to the second target temperature of 250℃ to 450℃, if the cooling rate is higher than 30℃ / s, the weld structure will transform into brittle and hard phases such as martensite. If the cooling rate is lower than 5℃ / s, the cooling efficiency will be too low, affecting production efficiency and also leading to an increase in the pearlite lamellar spacing and coarsening of the structure. Therefore, a slow cooling rate range of 5℃ / s to 30℃ / s ensures that austenite has sufficient time to transform into the ideal ferrite and pearlite structure, while also avoiding the formation of martensite. Meanwhile, the predetermined time for the isothermal annealing section is set to 2 s to 10 s because in the temperature range of 100℃ to 180℃, the release of residual stress requires a certain amount of time. If the time is too short, less than 2 s, the residual stress will not be released sufficiently; if the time is too long, greater than 10 s, it will affect production efficiency and cause unnecessary tempering changes in the already stabilized structure. An isothermal annealing time of 2 s to 10 s is sufficient to make the internal temperature of the weld tend to be uniform and to fully release residual stress.

[0028] Due to significant differences in temperature distribution and cooling requirements across different regions of the weld cross-section, the weld center region exhibits the highest temperature and most complete melting during welding. This region shows the strongest tendency for grain growth and requires the strongest cooling intensity for rapid cooling to refine the grains. The heat-affected zone (HAZ), located on either side of the weld center, is the heat-affected but unmelted base metal region. Its peak temperature is lower than the weld center but higher than the base metal. Applying the same cooling intensity as the weld center would result in an excessively large temperature gradient between the HAZ and the base metal, leading to thermal stress concentration and welding deformation. Therefore, to avoid a large stability gradient between the weld center and the HAZ, which could cause stress corrosion cracking and fatigue cracking, this… In this embodiment, the width of the weld center region accounts for 40% to 60% of the total weld width. This range covers the core area of ​​the weld with the highest temperature and the greatest need for strong cooling, without excessively encroaching on the space of the heat-affected zone (HAZ). This ensures that the HAZ has sufficient width for a gradient transition. The width of the HAZ is 20% to 30% of the weld width, ensuring that the HAZ has sufficient width to achieve a smooth temperature transition from the weld center region to the base material. At the same time, the HAZ microstructure within this width range can be properly cooled and controlled, which ensures both the grain refinement effect in the weld center region and the control of the temperature gradient between the HAZ and the base material.

[0029] To precisely control the cooling rate at each stage, in this embodiment, the rapid cooling stage needs to achieve a high cooling rate of 50℃ / s to 200℃ / s. The aerosol spray atomizes liquid water and mixes it with compressed air before spraying it onto the weld surface. It utilizes the latent heat of vaporization of water and the convective heat transfer of air to achieve efficient cooling. By adjusting the spray pressure and water volume, the cooling rate can be precisely controlled. Compared with simple air cooling, the aerosol spray has a higher cooling efficiency and can meet the rapid cooling requirements of the rapid cooling stage. The slow cooling stage needs to achieve a medium cooling rate of 5℃ / s to 30℃ / s. The compressed air removes the heat from the weld through convective heat transfer, resulting in a moderate and easily controllable cooling rate. Compared to spray cooling, compressed air contains no liquid medium, thus avoiding the drastic temperature drop caused by liquid vaporization. The cooling process is smoother and gentler, suitable for the temperature control requirements of the slow cooling stage. By adjusting the flow rate and pressure of the compressed air, the cooling rate of the slow cooling stage can be precisely controlled. The isolating temperature stage requires maintaining a predetermined temperature range of 100℃ to 180℃ for a predetermined time. The low-intensity airflow has weak cooling capacity, allowing the weld temperature to change slowly or remain relatively stable near the third target temperature, providing sufficient time for residual stress release. By using different types of cooling media in each cooling stage, the advantages of each medium's cooling characteristics are fully utilized, thereby achieving precise control of the cooling rate at each stage.

[0030] Because the temperature gradient difference between the weld center region and the heat-affected zone is a key indicator for measuring the uniformity of temperature distribution in the cross-sectional direction, in order to avoid excessive temperature gradients causing significant welding deformation and thermal stress concentration in thin-walled tanks, in this embodiment, in step S3, the temperature gradient difference between the weld center region and the heat-affected zone is 50℃~80℃. If the temperature gradient difference is less than 50℃, it means that the difference in cooling intensity between the weld center region and the heat-affected zone is too small, resulting in the heat-affected zone bearing excessively high cooling intensity, causing a large temperature gradient between the heat-affected zone and the base material, which leads to welding deformation. If the temperature gradient difference is greater than 80℃, it means that the temperature difference between the weld center region and the heat-affected zone is too large, and the thermal stress concentration in the cross-sectional direction of the weld increases significantly, which can easily lead to cracking or permanent deformation in thin-walled tanks.

[0031] In the actual welding cooling process, there are various uncontrollable disturbances. For example, the welding heat input may change due to power grid fluctuations, the ambient temperature may vary with workshop conditions, and the initial temperature of the weld may deviate due to slight fluctuations in welding speed. Therefore, in order to ensure the consistency of the weld metallographic structure and product quality, in this embodiment, in step S3, the weld temperature of each cooling zone is collected in real time by a temperature sensor. The actual temperature is compared with the cooling temperature trajectory, and the cooling medium parameters of each cooling zone are adjusted according to the comparison results. The control system can calculate the temperature deviation in real time by collecting the weld temperature of each cooling zone in real time by a temperature sensor and comparing the actual temperature with the preset cooling temperature trajectory point by point. According to the comparison results, the control system dynamically adjusts the cooling medium parameters of each cooling zone so that the actual cooling curve of each zone tracks the preset target temperature trajectory. Through real-time temperature monitoring and dynamic adjustment, closed-loop intelligent control of the cooling process is realized; it effectively copes with disturbances such as welding heat input fluctuations and ambient temperature changes, ensures the consistency of cooling effect between batches, and enables the actual cooling curve of each cooling zone to accurately track the preset target temperature trajectory, thus ensuring the stability of the weld metallographic structure.

[0032] To accurately capture real-time temperature changes in the weld, this embodiment uses infrared thermometers as the temperature sensors. Temperature sensors are arranged along the weld length in each cooling zone, with at least two sensors in each zone. This arrangement of sensors along the weld length allows for the acquisition of actual temperature distribution data within each zone. Each cooling zone has at least two temperature sensors: one located in the weld center area and the other in the heat-affected zone (HAZ). The temperature data from both sensors allows for simultaneous monitoring of temperature changes in both the weld center area and the HAZ within the zone. This provides real-time data support for differentiated cooling of the weld center area and HAZ in zoned cooling control. By using infrared thermometers, real-time capture of weld surface temperature changes is possible without affecting the application of the cooling medium or the movement of the weld. Compared to contact-based temperature measurement methods such as thermocouples, infrared thermometers do not damage the thin-walled tank surface due to contact and do not exhibit hysteresis due to the thermal inertia of the sensing element.

[0033] The above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention in any way. Although the present invention has been disclosed above with reference to preferred embodiments, it is not intended to limit the present invention. Any person skilled in the art can make some modifications or alterations to the above-disclosed technical content to create equivalent embodiments without departing from the scope of the present invention. Any simple modifications, equivalent changes and alterations made to the above embodiments based on the technical essence of the present invention without departing from the scope of the present invention shall still fall within the scope of the present invention.

Claims

1. A method for segmented gradient cooling of the weld seams of an iron spray can, characterized in that, Includes the following steps: S1: Cooling temperature trajectory setting, based on the continuous cooling transformation curve of ferrous materials to set the cooling temperature trajectory; S2: Segmented gradient cooling setting, the cooling temperature trajectory includes a rapid cooling section, a slow cooling section and a uniform temperature section, the rapid cooling section is to reduce the welding completion temperature to a first target temperature at a first cooling rate, the slow cooling section is to reduce the temperature from the first target temperature to a second target temperature at a second cooling rate, the second cooling rate is less than the first cooling rate, and the uniform temperature section is to maintain the temperature near a third target temperature for a predetermined time. S3: Zoned cooling control. The weld is divided into multiple cooling zones along the length of the weld. Within each cooling zone, the weld is divided into a central region and a heat-affected zone along the cross-sectional direction of the weld. Each cooling zone independently performs a rapid cooling section, a slow cooling section, and a temperature equalization section. In the rapid cooling section, a first cooling temperature is applied to the central region of the weld, and a second cooling temperature lower than the first cooling temperature is applied to the heat-affected zone. The second cooling temperature is 50% to 70% of the first cooling temperature.

2. The method for segmented gradient cooling of the weld seam of an iron spray can according to claim 1, characterized in that: The number of cooling zones is ≥3, and three adjacent zones are simultaneously in the rapid cooling section, the slow cooling section, and the uniform temperature section.

3. The method for segmented gradient cooling of the weld seam of an iron spray can according to claim 1, characterized in that: The length L of the cooling zone is determined according to the following formula: L = v × t; Where v is the welding speed and t is the duration of a single cooling stage.

4. The method for segmented gradient cooling of the weld seam of an iron spray can according to claim 1, characterized in that: The first target temperature is 500℃~750℃, the second target temperature is 250℃~450℃, and the third target temperature is 100℃~180℃.

5. The method for segmented gradient cooling of the weld seam of an iron spray can according to claim 1, characterized in that: The first cooling rate is 50℃ / s to 200℃ / s, the second cooling rate is 5℃ / s to 30℃ / s, and the predetermined time for the temperature equalization section is 2s to 10s.

6. The method for segmented gradient cooling of the weld seam of an iron spray can according to claim 1, characterized in that: The width of the weld center region is 40% to 60% of the weld width, and the heat-affected zone is located on both sides of the weld center region, with the width of the heat-affected zone being 20% ​​to 30% of the weld width.

7. The method for segmented gradient cooling of the weld seam of an iron spray can according to claim 1, characterized in that: The rapid cooling section uses a mixture of air and mist for cooling, the slow cooling section uses compressed air for cooling, and the temperature equalization section uses low-intensity airflow for cooling.

8. The method for segmented gradient cooling of the weld seam of an iron spray can according to claim 1, characterized in that: In step S3, the temperature gradient difference between the weld center region and the heat-affected zone is 50℃~80℃.

9. The method for segmented gradient cooling of the weld seam of an iron spray can according to claim 1, characterized in that: In step S3, the weld temperature of each cooling zone is collected in real time by a temperature sensor, the actual temperature is compared with the cooling temperature trajectory, and the cooling medium parameters of each cooling zone are adjusted according to the comparison results.

10. A method for segmented gradient cooling of the weld seam of an iron spray can according to claim 9, characterized in that: The temperature sensor is an infrared thermometer, and the temperature sensors are arranged along the length of the weld in each cooling zone, with at least two temperature sensors arranged in each cooling zone.