A method for soldering a semiconductor multi-channel cleaning head

By employing chamfering and step design, Teflon coating, and oxidation treatment welding methods, the welding problem of semiconductor multi-channel cleaning heads has been solved, achieving the effects of no flow channel deformation, good sealing, uniform flow, and long service life, thus meeting the high precision requirements of semiconductor cleaning processes.

CN123104079APending Publication Date: 2026-11-17SUZHOU KSC PRECISE MACHINERY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611403990.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-10
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing semiconductor multi-channel cleaning heads are prone to generating flash, burrs, and flow channel deformation during the soldering process, resulting in cross-contamination, uneven flow, poor sealing, and short service life, making it difficult to meet the high cleanliness and high precision requirements of semiconductor cleaning processes.

Method used

Using KYNAR 740 plastic as the main material, the welding depth and sealing are controlled by chamfering and process step design, combined with Teflon coating and anodized heating plate and mold. Welding temperature and time are optimized, hot plate welding is performed, and vacuum testing is carried out to ensure sealing and flow uniformity.

Benefits of technology

It achieves non-deformation of the flow channel in the multi-channel cleaning head, good sealing performance, long service life, and uniform flow rate, meeting the high precision requirements of semiconductor cleaning processes and providing a process basis for mass production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123104079A_ABST
    Figure CN123104079A_ABST
Patent Text Reader

Abstract

This invention relates to the field of semiconductor manufacturing equipment technology and discloses a method for welding a semiconductor multi-channel cleaning head, comprising the following steps: S1: Preparing raw materials, using KYNAR 740 plastic as the main material of the cleaning head; S2: Chamfering and step processing, processing chamfers around the bonding area to be welded to allow excess material to overflow during welding, and processing a process step at the welding point to facilitate control of the weld penetration; S3: Preparing the welding equipment, the welding machine uses upper and lower mold heating plates, the heating plate material is 45# steel, and the surface is treated with Teflon coating. This invention achieves precise control of the weld penetration through the process step, good coaxiality of the multi-channels, and uniform flow rate in each channel, meeting the high precision requirements of semiconductor cleaning processes. The chamfer and annular overflow groove design allows excess molten material to overflow in an orderly manner, avoiding flash and burrs, resulting in a dense weld without pores and a high pass rate in airtightness testing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor manufacturing equipment technology, specifically to a semiconductor multi-channel cleaning head welding method. Background Technology

[0002] Semiconductor multi-channel cleaning heads are core components of wafer cleaning equipment. They contain multiple independent chemical / deionized water channels for precise cleaning of the wafer surface. These cleaning heads are typically made of corrosion-resistant plastics (such as PVDF and PFA), and multiple plastic components are joined together using a welding process.

[0003] In existing technologies, the plastic welding of semiconductor multi-channel cleaning heads mainly employs conventional hot plate welding or ultrasonic welding methods. However, conventional welding processes have the following drawbacks: burrs and flash are easily generated during welding, leading to channel deformation and blockage; cross-contamination occurs between multiple channels due to welding deformation, resulting in uneven flow rates across channels, which cannot meet the requirements of high cleanliness and high-precision flow consistency in semiconductor cleaning processes; furthermore, the welding seal is poor, the service life is short, and it is difficult to adapt to the frequent chemical exchange and high-temperature cleaning environments in semiconductor manufacturing. Therefore, a welding method for semiconductor multi-channel cleaning heads is proposed. Summary of the Invention

[0004] (a) Technical problems to be solved

[0005] To address the shortcomings of existing technologies, this invention provides a semiconductor multi-channel cleaning head welding method that enables simultaneous welding of multiple channels, ensures no deformation of the flow channels, improves sealing performance and service life, and lays the technological foundation for subsequent mass production.

[0006] (II) Technical Solution

[0007] To achieve the above objectives, the present invention provides the following technical solution: A method for soldering a semiconductor multi-channel cleaning head includes the following steps: S1: Prepare raw materials, including KYNAR 740 plastic as the main material for the cleaning head; S2: Beveling and step processing. Chamfering is processed around the bonding area to be welded to allow excess material to overflow during welding. A process step is processed at the welding point to facilitate control of the weld penetration. S3: Welding equipment preparation. The welding machine uses upper and lower mold heating plates. The heating plate material is 45# steel with Teflon coating. The fixed mold is made of 6061 aluminum alloy with natural oxidation treatment. The worktable is made of 45# steel with nickel plating. S4: Hot plate welding. Place the PVDF plastic parts to be welded in a fixed mold. Heat the upper and lower mold heating plates to a temperature of 240±5℃ for 10-15 seconds to fully melt the welding surface. Then remove the heating plates, butt the two parts together and apply pressure. The bonding time should be no less than 5 minutes to allow the welding interface to cool and solidify fully. S5: Inspection and verification. After welding, the multi-channel cleaning head is subjected to vacuum testing to verify that the sealing performance of each channel meets the requirements.

[0008] As a further embodiment of the present invention, in step S2, a 1.5×45° chamfer is processed around the bonding area to be welded to allow excess residue to overflow during welding, and a process step with a height of 0.6mm is processed at the welding area to control the welding penetration depth to 0.6mm.

[0009] Furthermore, the 1.5×45° chamfer in S2 is continuously provided around the bonding surface to form an annular overflow groove.

[0010] Based on the aforementioned scheme, the height of the 0.6mm process step in S2 is matched with the welding penetration depth to ensure that the flow channel size accuracy is controlled within ±0.05mm after welding.

[0011] Furthermore, the Teflon coating thickness of the heating plate in S3 is 20-50 μm to prevent PVDF material from adhering to the surface of the heating plate at high temperatures.

[0012] As a further embodiment of the present invention, the 6061 aluminum alloy used to fix the mold in S3 undergoes a natural oxidation treatment, resulting in a dense aluminum oxide film on its surface, which improves the wear resistance and corrosion resistance of the mold.

[0013] Based on the aforementioned scheme, the nickel plating layer thickness of the worktable in S3 is 10-30μm to improve the hardness and corrosion resistance of the worktable surface.

[0014] Furthermore, in step S5, the multi-channel cleaning head after welding is subjected to vacuum testing. The vacuum level reaches above -0.095MPa, and there is no leakage after holding the pressure for 30 minutes. The sealing performance of each channel meets the requirements. After flow testing, the flow deviation of each channel is less than ±3%, which meets the requirements of semiconductor cleaning process.

[0015] Three (Beneficial Effects)

[0016] Compared with the prior art, the present invention provides a semiconductor multi-channel cleaning head welding method, which has the following beneficial effects: 1. In this invention, the welding penetration depth is precisely controlled by the process steps, the multi-channel coaxiality is good, and the flow rate of each channel is uniform, thus meeting the high precision requirements of the semiconductor cleaning process.

[0017] 2. In this invention, the chamfer and annular overflow groove design allow excess molten material to overflow in an orderly manner, avoiding the generation of flash and burrs, resulting in dense welding without air holes and a high pass rate for air tightness testing.

[0018] 3. In this invention, the optimized welding temperature and time parameters enable the welding interface to fully fuse, resulting in excellent high and low temperature resistance, resistance to cracking and detachment, and significantly extending the service life of the cleaning head. Furthermore, the standardized welding parameters and mold design lay the technological foundation for subsequent mass production, ensuring good product consistency. Attached Figure Description

[0019] Figure 1 This is a schematic diagram of the steps in the semiconductor multi-channel cleaning head welding method proposed in this invention. Detailed Implementation

[0020] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention. Example 1

[0021] Reference Figure 1 A method for soldering a semiconductor multi-channel cleaning head includes the following steps: S1: Prepare raw materials, prepare KYNAR 740 (PVDF) plastic as the main material of the cleaning head; S2: Beveling and step processing: A 1.5×45° chamfer is processed around the bonding area to be welded. The 1.5×45° chamfer is continuously set around the bonding surface to form an annular overflow groove for the overflow of excess material during welding. A process step with a height of 0.6mm is processed at the welding point to control the weld penetration depth to 0.6mm. The height of the 0.6mm process step matches the weld penetration depth to ensure that the flow channel size accuracy is controlled within ±0.05mm after welding. S3: Welding equipment preparation. The welding machine uses upper and lower mold heating plates. The heating plate material is 45# steel with Teflon (polytetrafluoroethylene) coating. The fixed mold is made of 6061 aluminum alloy with natural oxidation treatment. The worktable is made of 45# steel with nickel plating. S4: Hot plate welding. Place the PVDF plastic parts to be welded in a fixed mold. Heat the upper and lower mold heating plates to a temperature of 240±5℃ for 15 seconds to fully melt the welding surface. Then remove the heating plates, butt the two parts together and apply pressure. The bonding time should be no less than 5 minutes to allow the welding interface to cool and solidify fully. S5: Inspection and verification. After welding, the multi-channel cleaning head is subjected to vacuum testing to verify that the sealing performance of each channel meets the requirements. Example 2

[0022] Reference Figure 1 A method for soldering a semiconductor multi-channel cleaning head includes the following steps: S1: Prepare raw materials, prepare KYNAR 740 (PVDF) plastic as the main material of the cleaning head; S2: Beveling and step processing: A 1.5×45° chamfer is processed around the bonding area to be welded to allow excess material to overflow during welding. A process step with a height of 0.6mm is processed at the welding point to control the weld penetration depth to 0.6mm. S3: Welding equipment preparation. The welding machine uses upper and lower mold heating plates. The heating plates are made of 45# steel with a Teflon (polytetrafluoroethylene) coating. The Teflon coating thickness of the heating plates is 20-50μm to prevent PVDF material from adhering to the heating plate surface at high temperatures. The fixed mold is made of 6061 aluminum alloy with a natural anodizing treatment. The worktable is made of 45# steel with a nickel plating treatment. After the natural anodizing treatment, a dense aluminum oxide film is formed on the surface of the 6061 aluminum alloy of the fixed mold, which improves the wear resistance and corrosion resistance of the mold. The nickel plating layer thickness of the worktable is 10-30μm to improve the surface hardness and corrosion resistance of the worktable. S4: Hot plate welding. Place the PVDF plastic parts to be welded in a fixed mold. Heat the upper and lower mold heating plates to a temperature of 240±5℃ for 12 seconds to fully melt the welding surface. Then remove the heating plates, butt the two parts together and apply pressure. The bonding time should be no less than 5 minutes to allow the welding interface to cool and solidify fully. S5: Inspection and verification. After welding, the multi-channel cleaning head is subjected to vacuum testing to verify that the sealing performance of each channel meets the requirements. Example 3

[0023] Reference Figure 1 A method for soldering a semiconductor multi-channel cleaning head includes the following steps: S1: Prepare raw materials, prepare KYNAR 740 (PVDF) plastic as the main material of the cleaning head; S2: Beveling and step processing: A 1.5×45° chamfer is processed around the bonding area to be welded to allow excess material to overflow during welding. A process step with a height of 0.6mm is processed at the welding point to control the weld penetration depth to 0.6mm. S3: Welding equipment preparation. The welding machine uses upper and lower mold heating plates. The heating plates are made of 45# steel with a Teflon (polytetrafluoroethylene) coating. The Teflon coating thickness of the heating plates is 20-50μm to prevent PVDF material from adhering to the heating plate surface at high temperatures. The fixed mold is made of 6061 aluminum alloy with a natural anodizing treatment. The worktable is made of 45# steel with a nickel plating treatment. After the natural anodizing treatment, a dense aluminum oxide film is formed on the surface of the 6061 aluminum alloy of the fixed mold, which improves the wear resistance and corrosion resistance of the mold. The nickel plating layer thickness of the worktable is 10-30μm to improve the surface hardness and corrosion resistance of the worktable. S4: Hot plate welding. Place the PVDF plastic parts to be welded in a fixed mold. Heat the upper and lower mold heating plates to a temperature of 240±5℃ for 12 seconds to fully melt the welding surface. Then remove the heating plates, butt the two parts together and apply pressure. The bonding time should be no less than 5 minutes to allow the welding interface to cool and solidify fully. S5: Testing and verification. The multi-channel cleaning head after welding is vacuum tested. The vacuum degree reaches above -0.095MPa. There is no leakage after holding the pressure for 30 minutes. The sealing of each channel meets the requirements. After flow test, the flow deviation of each channel is less than ±3%, which meets the requirements of semiconductor cleaning process.

[0024] In the description herein, it should be noted that relational terms such as "first" and "second" are used merely to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such process, method, article, or apparatus.

[0025] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

Claims

1. A method for soldering a semiconductor multi-channel cleaning head, characterized in that, Includes the following steps: S1: Prepare raw materials, including KYNAR 740 plastic as the main material for the cleaning head; S2: Beveling and step processing. Chamfering is processed around the bonding area to be welded to allow excess material to overflow during welding. A process step is processed at the welding point to facilitate control of the weld penetration. S3: Welding equipment preparation. The welding machine uses upper and lower mold heating plates. The heating plate material is 45# steel with Teflon coating. The fixed mold is made of 6061 aluminum alloy with natural oxidation treatment. The worktable is made of 45# steel with nickel plating. S4: Hot plate welding. Place the PVDF plastic parts to be welded in a fixed mold. Heat the upper and lower mold heating plates to a temperature of 240±5℃ for 10-15 seconds to fully melt the welding surface. Then remove the heating plates, butt the two parts together and apply pressure. The bonding time should be no less than 5 minutes to allow the welding interface to cool and solidify fully. S5: Inspection and verification. After welding, the multi-channel cleaning head is subjected to vacuum testing to verify that the sealing performance of each channel meets the requirements.

2. The semiconductor multi-channel cleaning head welding method according to claim 1, characterized in that, In step S2, a 1.5×45° chamfer is processed around the bonding area to be welded to allow excess material to overflow during welding. A process step with a height of 0.6mm is processed at the welding point to control the weld penetration depth to 0.6mm.

3. The semiconductor multi-channel cleaning head welding method according to claim 2, characterized in that, The 1.5×45° chamfer in S2 is continuously provided around the bonding surface to form an annular overflow groove.

4. The semiconductor multi-channel cleaning head welding method according to claim 2, characterized in that, The height of the 0.6mm process step in S2 matches the welding penetration depth, ensuring that the flow channel size accuracy is controlled within ±0.05mm after welding.

5. The semiconductor multi-channel cleaning head welding method according to claim 1, characterized in that, The Teflon coating thickness of the heating plate in S3 is 20-50 μm to prevent PVDF material from adhering to the surface of the heating plate at high temperatures.

6. The semiconductor multi-channel cleaning head welding method according to claim 5, characterized in that, The 6061 aluminum alloy used to fix the mold in S3 undergoes a natural oxidation treatment, resulting in a dense aluminum oxide film on its surface, which improves the mold's wear resistance and corrosion resistance.

7. The semiconductor multi-channel cleaning head welding method according to claim 6, characterized in that, The nickel plating layer on the worktable in S3 is 10-30 μm thick to improve the hardness and corrosion resistance of the worktable surface.

8. The semiconductor multi-channel cleaning head welding method according to claim 1, characterized in that, In step S5, the multi-channel cleaning head after welding is vacuumed and tested. The vacuum level reaches above -0.095MPa, and there is no leakage after holding the pressure for 30 minutes. The sealing performance of each channel meets the requirements. After flow test, the flow deviation of each channel is less than ±3%, which meets the requirements of semiconductor cleaning process.