A liquid frozen packaging container and its manufacturing method

By designing a liquid frozen packaging container that combines a flexible inner liner and an outer shell, and incorporating a venting element and negative pressure filling technology, the problem of shape distortion and loss of frozen packaging containers during freezing and thawing in existing technologies has been solved, achieving a highly flexible and low-cost packaging solution.

CN123105071APending Publication Date: 2026-11-17WEILAN (WUXI) CULTURAL & CREATIVE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611597124.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-15
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing food freezing packaging technologies suffer from problems such as air pockets, dents, loss of shape after freezing, susceptibility to contamination, high costs, and incompatibility with slow-freezing processes, leading to distortion and damage to packaging containers during freezing and thawing.

Method used

Design a liquid freezing packaging container that combines an elastic inner liner with an outer shell. An expansion gap is provided between the inner liner and the outer shell, and a vent is provided on the outer shell. The inner liner can self-adapt to expansion and deformation through negative pressure filling and the vent structure. Combined with highly flexible materials and manufacturing processes, the packaging can maintain its three-dimensional shape during freezing and thawing.

Benefits of technology

It achieves adaptive expansion and deformation of the inner liner during freezing, avoiding shape distortion, reducing costs, and ensuring product transparency and appearance quality, while adapting to slow-freezing processes and reducing losses.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123105071A_ABST
    Figure CN123105071A_ABST
Patent Text Reader

Abstract

This invention provides a liquid frozen packaging container and its manufacturing method, relating to the field of food frozen packaging technology. Its structure includes an elastic inner liner, an outer shell surrounding the elastic inner liner, and an expansion gap between the elastic inner liner and the outer shell. A vent is provided on the outer shell, connecting the expansion gap to the outside. A filling port is provided on the outer side of the outer shell, which is sealed after filling; alternatively, a sealing film is provided on the outer side of the outer shell. The aforementioned elastic inner liner is plastically shaped to form a predetermined three-dimensional shape. After being filled with liquid, its geometric stiffness is sufficient to overcome hydrostatic pressure, maintaining a full three-dimensional shape at room temperature. During freezing, the liquid expands as it freezes, and the elastic inner liner absorbs the expansion volume through its own elastic stretching deformation, maintaining the predetermined three-dimensional shape. During thawing, the elastic inner liner automatically shrinks back to its original shape based on elastic memory. The outer circumference of the elastic inner liner is smaller than the inner cavity size of the outer shell, naturally forming an expansion gap occupying 10% to 50% of the inner volume of the outer shell after being embedded in it.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of food frozen packaging technology, specifically to a liquid frozen packaging container and its manufacturing method. Background Technology

[0002] Flexible bagged products flatten under gravity, leading to defects such as air pockets and dents after freezing, and resulting in a monotonous appearance; rigid cup-shaped products require cold chain transportation and low-temperature storage throughout the entire process from the factory, resulting in higher costs and losses, and the shape cannot be restored after thawing; ice tray molds require manual water injection and demolding, which is cumbersome; exposed to the refrigerator environment, they are easily contaminated and deteriorated, which is not conducive to long-term storage; containers with venting compensation have limited compensation cavity volume, air cushion effect leading to molding distortion, no means of eliminating air bubbles, no external air collection, and no ability to maintain three-dimensional shape; existing packaging does not consider the adaptability of slow freezing process (-18℃~-22℃, ≥12 hours), the risk of rigid container breakage is increased during slow freezing, and the shape distortion of flexible containers is aggravated. Summary of the Invention

[0003] The present invention aims to overcome the defects existing in the prior art and provide a liquid frozen packaging container and its manufacturing method. The liquid frozen packaging container has the advantages of adaptive freezing expansion, adaptability to slow freezing process, low cost and high flexibility.

[0004] The technical solution adopted in this invention is as follows: A liquid frozen packaging container includes: an elastic inner liner, an outer shell surrounding the elastic inner liner, and an expansion gap between the elastic inner liner and the outer shell; a vent on the outer shell, the vent communicating with the expansion gap and the outside; a filling port on the outer side of the outer shell, the filling port being sealed after filling; or, a sealing film on the outer side of the outer shell.

[0005] Preferably, in the liquid frozen packaging container: the elastic inner liner includes an upper inner liner and a lower inner liner, and the outer shell includes an upper outer shell and a lower outer shell. The upper inner liner, lower inner liner, upper outer shell, and lower outer shell all form cavities. The outer circumferential radius of the upper inner liner is smaller than the inner cavity radius of the upper outer shell, and the outer circumferential radius of the lower inner liner is smaller than the inner cavity radius of the lower outer shell. After the upper inner liner is embedded in the upper outer shell and the lower inner liner is embedded in the lower outer shell, an expansion gap of 10% to 50% of the internal volume of the outer shell is formed between the outer wall of the elastic inner liner and the inner wall of the outer shell.

[0006] Preferably, in the liquid frozen packaging container: the upper inner liner and the upper outer shell are plastic-sealed together at the flange to form an upper composite; the lower inner liner and the lower outer shell are plastic-sealed together at the flange to form a lower composite; the upper composite forms an upper joint at the flange; the lower composite forms a lower joint at the flange; at least one semi-tubular structure is provided on the flange of each of the upper and lower joints; after plastic sealing, the corresponding semi-tubular structures of the upper and lower joints together form a filling port; the number of filling ports is at least one.

[0007] Preferably, in the liquid frozen packaging container: the outer periphery of the upper composite joint and the lower composite joint is provided with corresponding opening portions, the opening portions being selected from one of pull rings, pull tabs, or tear openings; the wall thickness of the upper inner liner and the lower inner liner is 0.05~0.50mm; the wall thickness of the upper outer shell and the lower outer shell is 0.10~0.6mm; the vent is one of or any combination of circular, elliptical, rectangular, polygonal, strip slit, curved groove, star-shaped, flower-shaped, or irregular opening, and the number of vents is at least one.

[0008] Preferably, in the liquid frozen packaging container: the outer shell is an open outer shell with one side open, an open inner liner is provided inside the open outer shell, a sealing film is provided on the plastic sealing flange surface of the open outer shell, a vent is provided on the closed side of the open outer shell, and after the open inner liner is embedded in the open outer shell, an expansion gap of 10% to 50% of the internal volume of the open outer shell is formed between the open inner liner and the open outer shell.

[0009] A method for manufacturing a liquid frozen packaging container, comprising the following steps: Step S1. Form the upper and lower outer shells, and simultaneously prefabricate the semi-tubular structures on the flange surfaces of the upper and lower outer shells; Step S2. A vent is made in the upper and / or lower outer shell walls by laser cutting or punching, and an opening is provided on the flange surface of the upper and lower outer shells; Step S3. Molding the upper and lower inner liner; After heating and softening the upper and lower inner liner, the mold stretches them along the inner walls of the upper and lower outer shells to a predetermined position. Then, the mold carries the inner liner in the opposite direction and cools and shapes it after it is in place; The upper inner liner and the upper outer shell are plastic-sealed together at the flange to form the upper composite, and the lower inner liner and the lower outer shell are plastic-sealed together at the flange to form the lower composite. Step S4. Seal the flange mating surfaces of the upper and lower composites. Do not heat seal the filling port on the flange surface for the time being. The plastic sealing area of ​​the composite should avoid the tear-off opening. Step S5. Apply negative pressure to the liquid bladder through the open filling port. The air inside the liquid bladder is discharged through the filling port to maintain the negative pressure environment. Inject liquid and fill until the liquid bladder is completely full. Step S6. The filling port is heat-sealed to completely seal the liquid bladder; after heat sealing, the base of the filling port and the sealing line are solidified into one, forming a liquid frozen packaging container.

[0010] Preferably, in the manufacturing method of the liquid frozen packaging container, the upper and lower outer shells in step S1 are formed by thermoforming, injection molding or compression molding. The thermoforming heating and softening temperature is 90~180℃, the heating and softening time is 1~20 seconds, the vacuum degree is -0.05~-0.09MPa, the auxiliary positive pressure is 0.1~0.5MPa, the pressure holding time is 2~20 seconds, and the forming cycle is 3~40 seconds. In step S3, the upper and lower inner liner forming is selected from one of vacuum forming, injection molding or compression molding. The heating and softening temperature of vacuum forming is 50~160℃, the heating and softening time is 1~25 seconds, the vacuum degree is -0.02~-0.09MPa, the auxiliary positive pressure is 0.1~0.5MPa, the holding time is 2~20 seconds, and the forming cycle is 3~45 seconds. Preferably, in the method for manufacturing the liquid frozen packaging container, the temperature of the plastic sealing connection in step S3 is 120~180℃, the pressure is 0.2~0.6MPa, and the time is 0.5~5 seconds.

[0011] Preferably, in the method for manufacturing the liquid frozen packaging container, the negative pressure applied in step S5 is -0.02 to -0.08 MPa, and the negative pressure is applied for 2 to 5 seconds; in step S6, the heat sealing temperature is 120 to 190°C, the heat sealing pressure is 0.2 to 0.6 MPa, the heat sealing time is 0.5 to 4 seconds, and the heat sealing line width is 1 to 3 mm.

[0012] A method for manufacturing a liquid frozen packaging container, comprising the following steps: Step S1. Place the sheet material of the open shell onto the mold and form it through a thermoforming process; Step S2. A vent is made on the open shell wall by laser cutting or punching, and the flange edge at the opening of the open shell is cut or punched at the same time. Step S3. Cover the plastic sealing flange surface of the pre-formed open outer shell with the composite film material of the open inner liner. After heating and softening, the mold stretches it to the set position inside the open outer shell and then cools and shapes it. At the same time, the open inner liner and the open outer shell are plastic sealed together at the plastic sealing flange surface. Step S4. After degassing and impurity removal, the liquid is filled through the open end until the cavity is completely filled. Then, sealing film is used to seal the plastic-sealed flange along the edge of the open end to form a complete sealing structure. The pre-reserved tear opening is not sealed to form an easy-tear tongue.

[0013] The beneficial effects of this invention are: (1) The liquid frozen packaging container of the present invention is provided with an elastic inner liner. The inner liner relies on the geometric stiffness after plastic shaping to overcome the hydrostatic pressure after being filled with liquid at room temperature, so that the packaging can present a full three-dimensional shape without freezing. When it freezes and expands, it undergoes reversible elastic tensile deformation (elongation at break ≥100%), absorbing the expansion volume. After melting, it automatically shrinks back to its original shape by relying on elastic memory. The inner liner has a predetermined three-dimensional shape and its outer dimensions are smaller than the inner cavity dimensions of the outer shell. After being embedded in the outer shell, it naturally forms an expansion gap that occupies 10% to 50% of the inner volume of the outer shell.

[0014] (2) The liquid frozen packaging container of the present invention is provided with a vent, which has the technical effects of balancing pressure during the forming of the inner liner, venting negative pressure during the filling of the inner liner, venting during the expansion during freezing, and absorbing air during thawing.

[0015] (3) In the manufacturing method of the liquid frozen packaging container of the present invention, after the sealing connection is completed and before the filling port is sealed, negative pressure is applied to the inside of the inner liner through the open filling port. The air inside the inner liner is discharged to the atmosphere through the filling port, so that the inner liner is completely deflated and gas-free. The filling is carried out while maintaining this negative pressure state. The liquid enters in the gas-free background, and the probability of carrying air bubbles is extremely low. When the inner liner deflates, the air in the gap between the outer wall of the inner liner and the inner wall of the outer shell is discharged to the outside through the vent of the outer shell, preventing the inner wall of the outer shell from generating adsorption resistance and ensuring that the inner liner deflates smoothly.

[0016] (4) The manufacturing method of the liquid frozen packaging container of the present invention pre-degasses and removes impurities from the liquid before filling, which is especially suitable for products with extremely high transparency requirements such as transparent ice. The filling operation is completed in a vacuum environment to prevent air bubbles from being trapped at the source. After the liquid bladder is filled, the base of the filling port and the sealing line are solidified into one piece. Attached Figure Description

[0017] To make the content of this invention easier to understand, the invention will be further described in detail below with reference to specific embodiments and accompanying drawings.

[0018] Figure 1 is a schematic diagram of the overall structure of the liquid frozen packaging container of Example 1.

[0019] Figure 2 is a schematic diagram of the disassembled structure of the liquid frozen packaging container of Example 1.

[0020] Figure 3 is a top view of the liquid frozen packaging container of Example 1.

[0021] Figure 4 This is a cross-sectional view of the liquid frozen packaging container of Example 1.

[0022] Figure 5 for Figure 1 A magnified view of point A.

[0023] Figure 6 This is a schematic diagram of the structure of the liquid frozen packaging container in Example 2.

[0024] Figure 7 This is a schematic diagram of the packaging container without a sealing film in Example 2.

[0025] Figure 8 This is a structural schematic diagram of the packaging container from another perspective of Example 2.

[0026] Figure 9 This is a cross-sectional view of the packaging container of Example 2. Detailed Implementation

[0027] The present invention will be further described below with reference to the accompanying drawings and specific embodiments, so that those skilled in the art can better understand and implement the present invention. However, the embodiments described are not intended to limit the present invention. Example

[0028] like Figures 1-5 A liquid frozen packaging container includes: an elastic inner liner, an outer shell surrounding the elastic inner liner, and an expansion gap between the elastic inner liner and the outer shell; a vent 6 is provided on the outer shell, the vent 6 connecting the expansion gap 10 to the outside; and a filling port is provided on the outer side of the outer shell, the filling port being sealed after filling. The elastic inner liner includes an upper inner liner 3 and a lower inner liner 4, and the outer shell includes an upper outer shell 1 and a lower outer shell 2.

[0029] In one embodiment, the upper inner liner 3, the lower inner liner 4, the upper outer shell 1, and the lower outer shell 2 all form cavities. The outer radius of the upper inner liner 3 is smaller than the inner radius of the upper outer shell 1, and the outer radius of the lower inner liner 4 is smaller than the inner radius of the lower outer shell 2. After the upper inner liner 3 is embedded in the upper outer shell 1 and the lower inner liner 4 is embedded in the lower outer shell 2, an expansion gap 10 naturally forms, which occupies 10% to 50% of the inner volume of the outer shell.

[0030] The upper inner liner 3 and the lower inner liner 4 are made of food-grade polymer materials that combine thermoplasticity (formability) and high elasticity (resilience). The food-grade polymer materials are selected from one or more of ethylene-vinyl acetate copolymer (EVA), ethylene-vinyl alcohol copolymer (EVOH), thermoplastic polyolefin elastomer (TPO), thermoplastic styrene elastomer (TPS), metallocene-catalyzed polyethylene (m-PE), and ionomer resins.

[0031] The inner liner possesses dual characteristics: Firstly, it maintains its plasticity through geometric stiffness after plastic shaping, which can be achieved through vacuum forming or compression molding. After liquid filling, its geometric stiffness is sufficient to overcome hydrostatic pressure, resulting in a full, three-dimensional shape at room temperature. Secondly, it exhibits elastic deformation capability, undergoing elastic tensile deformation (elongation at break ≥100%) during freezing and expansion, absorbing the expanded volume. Thirdly, it automatically shrinks back to its original shape after thawing due to elastic memory. The inner liner has a predetermined three-dimensional shape, with its outer perimeter smaller than the inner cavity of the outer shell, naturally forming an expansion gap occupying 10%~50% of the outer shell's internal volume after insertion. The six-hole vent serves five purposes: assisting in balancing pressure during inner liner molding, assisting in negative pressure venting during filling, venting during freezing expansion, absorbing air during thawing, and accelerating cooling.

[0032] The outer shell material is selected from one or more of the following: polypropylene (PP), polyethylene terephthalate (PET), amorphous polyethylene terephthalate (APET), glycol-modified polyethylene terephthalate (PETG), polystyrene (PS), high-impact polystyrene (HIPS), polyethylene (PE), low-density polyethylene (LDPE), linear low-density polyethylene (LLDPE), high-density polyethylene (HDPE), polylactic acid (PLA), and poly(butylene adipate-terephthalate) (PBAT).

[0033] One or more venting portions 6 penetrating the wall thickness are provided on the outer shell wall. The forms of these portions include, but are not limited to: vent holes, which are circular or elliptical through holes; vent windows, which are rectangular, polygonal, or irregularly shaped windows; vent grooves / slits, which are strip-shaped slits or curved grooves; and vents of any shape, such as star-shaped, flower-shaped, or logo-shaped decorative irregular openings. The specific form of the above-mentioned venting portions can be adjusted according to the product appearance design requirements, and the number, geometry, and size of the openings are not specifically limited.

[0034] Ventilation sections are preferably located at the highest point of the outer shell, in non-filling areas, or on non-main visual surfaces, and at least one vent is required.

[0035] The elastic inner liner is a completely sealed body without any venting parts. The venting parts are only located on the outer shell wall, connecting the gap between the inner liner and the outer shell to the outside. The air inside the inner liner is vented through the filling port (negative pressure pre-venting before filling + vacuum environment filling), which is unrelated to the venting structure of the outer shell.

[0036] The upper inner liner 3 and the upper outer shell 1 are plastic-sealed together at the flange face to form an upper composite. The lower inner liner 4 and the lower outer shell 2 are plastic-sealed together at the flange face to form a lower composite. Upper joints are formed on both sides of the upper composite extending outward along the outer periphery of the upper composite. Lower joints are formed on both sides of the lower composite extending outward along the outer periphery of the lower composite. At least one semi-tubular structure is provided on the flange joint surface 12 of both the upper and lower joints. The semi-tubular structures on the same side of the upper and lower joints together form a filling port.

[0037] Both the outer periphery of the upper composite body and the outer periphery of the lower composite body have an opening portion 11, which is selected from one of a pull ring, a pull tab, or a tear. The wall thickness of the upper inner liner 3 and the lower inner liner 4 is 0.05~0.50mm. The wall thickness of the upper outer shell 1 and the lower outer shell 2 is 0.10~0.6mm.

[0038] The opening is located on the non-main viewing surface of the packaging, preferably at the heat-sealed position. This opening is part of the outer shell and is manufactured simultaneously with the upper outer shell 1 and the lower outer shell 2 in the molding process.

[0039] During the outer shell molding process, a semi-tubular structure is made on the flange joint surface of the upper outer shell 1 and the lower outer shell 2. When the upper and lower half of the inner liner are respectively combined with the corresponding outer shell, the inner liner joint surface is tightly attached to the flange joint surface of the outer shell through a thermoforming process, and the same semi-tubular structure is replicated at the corresponding position of the filling port. After the upper composite and the lower composite are sealed and connected, the two semi-tubular structures are combined to form a complete filling port, and the number can be one or more.

[0040] In one implementation, the liquid frozen packaging container is provided with dual filling ports. The main filling port 7 is located opposite the pull tab and is used for liquid filling. The secondary filling port 8 is located at the pull tab and is used to assist in emptying and opening guidance. After filling is completed, the main and secondary filling ports are immediately heat-sealed to achieve permanent closure. The secondary filling port 8 and the pull tab 11 are integrated into a single structure.

[0041] Figures 1-5 In the diagram, 9 represents the flange face between the upper and lower outer shells, 7 and 8 represent the filling port structure before sealing, 5 represents the contents packaged in the packaging container (the contents are liquid), 12 represents the joint surface between the upper and lower composites, and 6 represents the venting section.

[0042] The method for manufacturing the liquid frozen packaging container in this embodiment includes the following steps: Step S1. Form the upper outer shell 1 and the lower outer shell 2. Simultaneously, prefabricate semi-tubular structures on the flange surfaces of the upper outer shell 1 and the lower outer shell 2. The forming of the upper outer shell 1 and the lower outer shell 2 is selected from one of vacuum forming, injection molding, or compression molding. The outer shell is preferably made of 0.3mm thick polypropylene (PP) sheet. The vacuum forming heating and softening temperature is 130~150℃, the heating and softening time is 5~10 seconds, the vacuum degree is -0.06~-0.08MPa, the auxiliary positive pressure is 0.3~0.5MPa, the pressure holding time is 10~15 seconds, and the forming cycle is 15~25 seconds. Step S2. A vent 6 is formed on the wall of the upper outer shell 1 and / or the lower outer shell 2 by laser cutting or punching, and an opening 11 is provided on the flange surface of the upper outer shell 1 and the lower outer shell 2; Step S3. Form the upper inner liner 3 and the lower inner liner 4; the upper inner liner 3 and the lower inner liner 4 are formed by vacuum forming, injection molding or compression molding; the inner liner is preferably a composite film material with a thickness of 0.3mm, the heating and softening temperature of vacuum forming is 120~140℃, the heating and softening time is 10~15 seconds, the vacuum degree is -0.05~-0.08MPa, the auxiliary positive pressure is 0.3~0.5MPa, the holding pressure time is 10~15 seconds, and the forming cycle is 20~30 seconds; After the upper inner liner 3 and the lower inner liner 4 are heated and softened, the mold stretches the upper inner liner 3 along the inner wall of the upper outer shell 1 to a predetermined position, and the lower inner liner 4 along the inner wall of the lower outer shell 2 to a predetermined position. Then, the mold carries the upper inner liner 3 and the lower inner liner 4 in a reverse displacement. After they are in place, they are cooled and shaped. This process can ensure that the shape details are complete and the wall thickness is uniform. The auxiliary role of the vent is that when the mold carries the inner liner in the forward and reverse displacement, the vent structure can ensure the pressure balance between the inner liner and the outer shell, promote air circulation and accelerate the molding of the inner liner. The upper inner liner 3 and the upper outer shell 1 are plastic-sealed together at the flange to form an upper composite, and the lower inner liner 4 and the lower outer shell 2 are plastic-sealed together at the flange to form a lower composite. The plastic sealing temperature is 120~180℃, the pressure is 0.2~0.6MPa, and the time is 0.5~5 seconds. Its vertical tensile strength, horizontal tensile strength, and tear strength must be greater than the force applied by the consumer when normally opening the door to ensure a complete seal. Step S4. Seal the flange mating surfaces 12 of the upper and lower composites. Do not heat seal the filling port on the flange surface for the time being. The plastic sealing area of ​​the composite should avoid the tear-off opening. Step S5. Apply negative pressure to the liquid bladder through the open secondary filling port 8. The pressure of the negative pressure is -0.02 to -0.08 MPa, and the time of applying the negative pressure is 2 to 5 seconds. The air inside the liquid bladder is discharged through the secondary filling port 8 to maintain the negative pressure environment. Liquid is injected into the main filling port 7, and the secondary filling port 8 is simultaneously vented. The liquid bladder is filled until it is completely full. Step S6. The auxiliary filling port 8 and the main filling port are heat-sealed to completely seal the liquid bladder; the heat-sealing temperature is 120~190℃, the heat-sealing pressure is 0.2~0.6MPa, the heat-sealing time is 0.5~4 seconds, and the heat-sealing line width is 1~3mm; after heat-sealing, the base of the auxiliary filling port 8 and the main filling port 7 are solidified with the sealing line to form a liquid frozen packaging container.

[0043] The inner liner is completely sealed after filling, and is completely isolated from the outside air after sealing. Air venting must be completed before the inner liner is sealed.

[0044] Before sealing, the filling port is pre-emptively purged under negative pressure and filled in a vacuum environment. The liquid undergoes pre-degassing and impurity removal treatment before filling, reducing the nitrogen content to ≤5mg / L, dissolved oxygen content to ≤2mg / L, and carbon dioxide content to ≤1mg / L. After the inner liner is sealed, the venting section performs the following functions: (1) Expansion and venting during freezing: The liquid inside the inner liner expands in volume due to freezing, and the air between the outer wall of the inner liner and the inner wall of the outer shell (i.e., the air in the expansion gap) is discharged to the outside through the vent, so as to avoid the formation of a high-pressure air cushion in the gap that hinders the normal expansion of the inner liner.

[0045] (2) During thawing, the ice inside the inner liner melts into liquid, its volume decreases, and the inner liner contracts. If the air in the gap cannot be replenished, a pressure difference will be formed between the inside and outside of the outer shell, which may cause the outer shell to deform or even collapse. The breathable structure can balance the internal and external air pressure to ensure that the inner liner and the outer shell maintain their original three-dimensional shape. Example

[0046] like Figures 6-9 A liquid frozen packaging container includes an elastic inner liner, an outer shell is provided outside the elastic inner liner, an air vent is provided on the outer shell, and a sealing film is provided on one side of the outer shell.

[0047] The outer shell is an open outer shell 13 with one side open. An open inner liner 14 is provided inside the open outer shell 13. A sealing film 16 is provided on the plastic sealing flange surface 15 of the open outer shell 13. A vent 6 is provided on the closed side of the open outer shell 13. After the open inner liner 14 is inserted into the open outer shell 13, an expansion gap 10 is formed between the open inner liner 14 and the open outer shell 13, which accounts for 10% to 50% of the internal volume of the open outer shell 13.

[0048] The manufacturing method of this embodiment includes the following steps: Step S1. Place the sheet of the open outer shell 13 onto the mold and form it through a thermoforming process. The outer shell forming process is selected from vacuum forming, injection molding, or compression molding. The outer shell is preferably made of 0.3mm thick polypropylene (PP) sheet. The heating and softening temperature of vacuum forming is 130~150℃, the heating and softening time is 5~10 seconds, the vacuum degree is -0.06~-0.08MPa, the auxiliary positive pressure is 0.3~0.5MPa, the holding pressure time is 10~15 seconds, and the forming cycle is 15~25 seconds. Step S2. A vent 6 is made on the wall of the open housing 13 (preferably at the opposite position of the opening) by laser cutting or punching, and the edge of the plastic sealing flange 15 at the opening of the open housing 13 is cut or punched. Step S3. The composite film material of the open inner liner 14 is covered on the plastic sealing flange surface 15 of the formed open outer shell 13. After being heated and softened, the mold stretches it to a set position inside the open outer shell 13 and then cools and shapes it. At the same time, the open inner liner 14 and the open outer shell 13 are plastic sealed together at the plastic sealing flange surface 15. The temperature of the plastic sealing connection is 120~180℃, the pressure is 0.2~0.6MPa, and the time is 0.5~5 seconds. The vertical tensile strength, horizontal tensile strength, and tear strength of the plastic sealing area must be greater than the force applied when the consumer normally opens it to ensure a complete seal. The auxiliary function of the vent 6 is that when the mold stretches the inner liner, the vent 6 can ensure the pressure balance between the open inner liner 14 and the open outer shell 13, which is conducive to rapid molding. The open inner liner 14 is formed by vacuum forming, injection molding, or compression molding. The inner liner is preferably made of a 0.3mm thick composite film material. The vacuum forming process involves a heating and softening temperature of 120~140℃, a heating and softening time of 10~15 seconds, a vacuum degree of -0.05~-0.08MPa, an auxiliary positive pressure of 0.3~0.5MPa, a holding time of 10~15 seconds, and a forming cycle of 20~30 seconds. Step S4. After degassing and impurity removal, the liquid is filled through the open end until the cavity is completely filled. Then, the sealing film 16 is used to seal along the flange face 15 of the edge of the open outer shell 13 to form a complete sealing structure. The pre-reserved tear opening position is not sealed to form an easy-tear tongue 17 for easy opening.

[0049] The mechanical properties of the sealing line must meet the following relationship: liquid expansion force < minimum force required to open the tear < strength of the plastic seal between the inner liner and the outer flange.

[0050] After filling, the inner liner combines with the sealing film to form a complete sealed structure, and the venting part performs the following functions: (1) Expansion and venting during freezing: Expansion and venting during freezing: The liquid inside the inner liner expands due to freezing, and the air between the outer wall of the inner liner and the inner wall of the outer shell (i.e., the air in the expansion gap) is discharged to the outside through the vent, so as to avoid the formation of a high-pressure air cushion in the gap that hinders the normal expansion of the inner liner.

[0051] (2) During thawing, the ice inside the inner liner melts into liquid, its volume decreases, and the inner liner contracts. If the air in the gap cannot be replenished, a pressure difference will be formed between the inside and outside of the outer shell, which may cause the outer shell to deform or even collapse. At this time, the air in the air collection bag is drawn into the gap through the breathable structure to balance the internal and external air pressure and ensure that the inner liner and the outer shell maintain their original three-dimensional shape.

[0052] Finally, it should be noted that the above specific embodiments are only used to illustrate the technical solutions of the present invention and not to limit it. Although the present invention has been described in detail with reference to examples, those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solutions of the present invention without departing from the spirit and scope of the technical solutions of the present invention, and all such modifications or substitutions should be covered within the scope of the claims of the present invention.

Claims

1. A liquid frozen packaging container, characterized in that: It includes an elastic inner liner, an outer shell is provided outside the elastic inner liner, and an expansion gap is provided between the elastic inner liner and the outer shell; a vent (6) is provided on the outer shell, and the vent (6) connects the expansion gap (10) to the outside; a filling port is provided on the outside of the outer shell, and the filling port is sealed after filling; or, a sealing film (16) is provided on the outside of the outer shell.

2. The liquid frozen packaging container according to claim 1, characterized in that: The elastic inner liner includes an upper inner liner (3) and a lower inner liner (4), and the outer shell includes an upper outer shell (1) and a lower outer shell (2). The upper inner liner (3), the lower inner liner (4), the upper outer shell (1), and the lower outer shell (2) all form cavities. The outer radius of the upper inner liner (3) is smaller than the inner radius of the upper outer shell (1), and the outer radius of the lower inner liner (4) is smaller than the inner radius of the lower outer shell (2). The upper inner liner (3) is embedded in the upper outer shell (1), and the lower inner liner (4) is embedded in the lower outer shell (2). After this, an expansion gap (10) is formed between the elastic inner liner and the outer shell, which accounts for 10% to 50% of the inner volume of the outer shell.

3. The liquid frozen packaging container according to claim 2, characterized in that: The upper inner liner (3) and the upper outer shell (1) are plastic-sealed together at the flange face to form an upper composite. The lower inner liner (4) and the lower outer shell (2) are plastic-sealed together at the flange face to form a lower composite. The upper composite forms an upper joint at the flange face, and the lower composite forms a lower joint at the flange face. At least one semi-tubular structure is provided on the flange face (12) of the upper joint and the lower joint. After being plastic-sealed together, the corresponding semi-tubular structures of the upper joint and the lower joint surround each other to form a filling port. The number of filling ports is at least one.

4. The liquid frozen packaging container according to claim 3, characterized in that: The upper and lower joints are provided with corresponding openings (11) on their outer periphery. The openings (11) are selected from one of pull rings, pull tabs or tear strips. The wall thickness of the upper inner liner (3) and the lower inner liner (4) is 0.05~0.5mm. The wall thickness of the upper outer shell (1) and the lower outer shell (2) is 0.10~0.6mm. The vent (6) is one of or any combination of circular, elliptical, rectangular, polygonal, strip slit, curved groove, star-shaped, flower-shaped or irregular opening. The number of vents is at least one.

5. The liquid frozen packaging container according to claim 1, characterized in that: The outer shell is an open outer shell (13) with one side open. An open inner liner (14) is provided inside the open outer shell (13). A sealing film (16) is provided on the plastic sealing flange surface (15) where the open inner liner and the open outer shell (13) are joined. A vent (6) is provided on the closed side of the open outer shell (13). After the open inner liner (14) is inserted into the open outer shell (13), an expansion gap (10) is formed between the open inner liner (14) and the open outer shell (13), which accounts for 10% to 50% of the internal volume of the open outer shell (13).

6. A method for manufacturing a liquid frozen packaging container according to any one of claims 1-4, characterized in that: Includes the following steps: Step S1. Form the upper shell (1) and the lower shell (2), and at the same time, prefabricate the semi-tubular structure on the flange face of the upper shell (1) and the lower shell (2); Step S2. A vent (6) is made on the wall of the upper shell (1) and / or the lower shell (2) by laser cutting or punching, and an opening (11) is provided on the flange surface of the upper shell (1) and the lower shell (2). Step S3. Form the upper inner liner (3) and the lower inner liner (4); After the inner liner composite film material is heated and softened, the mold stretches it along the inner wall of the upper outer shell (1) and the lower outer shell (2) to a predetermined position. Then the mold carries the inner liner in the opposite direction and cools and shapes it after it is in place; While the upper inner liner (3) and the lower inner liner (4) are being formed, the upper inner liner (3) and the upper outer shell (1) are plastic-sealed together at the flange to form the upper composite, and the lower inner liner (4) and the lower outer shell (2) are plastic-sealed together at the flange to form the lower composite; Step S4. Seal the flange mating surfaces (12) of the upper and lower composites together, but do not heat seal the filling port on the flange surface; Step S5. Apply negative pressure to the liquid bladder through the filling port to expel the air inside the liquid bladder through the filling port, and then inject liquid until the liquid bladder is completely filled; Step S6. Use a heat-sealing process to completely seal the liquid bladder at the filling port; after heat sealing, the base of the filling port and the sealing line are solidified into one piece to form a complete liquid frozen packaging.

7. The method for manufacturing a liquid frozen packaging container according to claim 6, characterized in that: In step S1, the upper outer shell (1) and lower outer shell (2) are formed by vacuum forming, injection molding or compression molding. The heating and softening temperature of vacuum forming is 90~180℃, the heating and softening time is 1~20 seconds, the vacuum degree is -0.05~-0.09MPa, the auxiliary positive pressure is 0.1~0.5MPa, the holding time is 2~20 seconds, and the forming cycle is 3~40 seconds. In step S3, the upper inner liner (3) and lower inner liner (4) are formed by vacuum forming, injection molding or compression molding. The heating and softening temperature of vacuum forming is 50~160℃, the heating and softening time is 1~25 seconds, the vacuum degree is -0.02~-0.09MPa, the auxiliary positive pressure is 0.1~0.5MPa, the holding time is 2~20 seconds, and the forming cycle is 3~45 seconds.

8. The method for manufacturing a liquid frozen packaging container according to claim 6, characterized in that: In step S3, the temperature for plastic sealing is 120~180℃, the pressure is 0.2~0.6MPa, and the time is 0.5~5 seconds.

9. The method for manufacturing a liquid frozen packaging container according to claim 6, characterized in that: In step S5, the negative pressure applied is -0.02 to -0.08 MPa, and the negative pressure is applied for 2 to 5 seconds. In step S6, the heat sealing temperature is 120 to 190°C, the heat sealing pressure is 0.2 to 0.6 MPa, the heat sealing time is 0.5 to 4 seconds, and the heat sealing line width is 1 to 3 mm.

10. A method for manufacturing a liquid frozen packaging container according to claim 5, characterized in that: Includes the following steps: Step S1. Place the sheet of the open outer shell (13) on the mold and form it by thermoforming process; Step S2. A vent (6) is made on the wall of the open shell (13) by laser cutting or punching, and the edge of the plastic sealing flange (15) at the opening of the open shell (13) is cut or punched. Step S3. The composite film material of the open inner liner (14) is covered on the plastic sealing flange surface (15) of the formed open outer shell (13). After being heated and softened, the mold stretches it to the set position inside the open outer shell (13) and then cools and shapes it. At the same time, the open inner liner (14) and the open outer shell (13) are plastic sealed together at the plastic sealing flange surface (15). Step S4. After degassing and impurity removal, the liquid is filled through the open end. After the liquid completely fills the cavity, the sealing film (16) is used to seal along the plastic sealing flange surface (15) of the open edge to form a complete sealing structure. The reserved tear position is not sealed to form an easy-tear tongue (17).