A method for precision machining and surface strengthening of glass products under zero carbon emission guidance

By acquiring the power grid frequency deviation signal and dielectric loss tangent value for heat pump compressor frequency compensation, combined with potential regulation and electric field-assisted depolarization, zero carbon emission processing of glass products is achieved, solving the problems of high energy consumption, large carbon emissions and poor quality consistency, and providing uniform thermal state and static electricity elimination effect.

CN123106019APending Publication Date: 2026-11-17江苏通达家居用品有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611343140.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-01
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

The existing glass product processing process suffers from high energy consumption, large carbon emissions, and poor consistency in processing quality.

Method used

By acquiring the real-time frequency deviation signal of the power grid and the dielectric loss tangent of the glass products, active disturbance compensation of the power supply frequency of the heat pump compressor is performed. Combined with the DC bias potential regulation of the heat pump circulating water circuit and the pulse electric field-assisted depolarization, and the eddy current heating compensation and electromagnetic stirring are used to perform plasma corona discharge treatment on the glass surface. The power of the heat pump system on both the hot and cold sides is adjusted in real time to achieve zero carbon emission processing of glass products.

Benefits of technology

It achieves reduced energy consumption and zero carbon emissions in the glass product processing process, improves the consistency of processing quality, provides a uniform thermal state basis, and avoids the problems of repeated static electricity accumulation and water temperature stratification.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123106019A_ABST
    Figure CN123106019A_ABST
Patent Text Reader

Abstract

This invention discloses a method for precision machining and surface strengthening of glass products under zero-carbon emission guidance, belonging to the field of glass product processing technology. The method includes: acquiring the power grid frequency deviation signal and the dielectric loss tangent of the glass; actively compensating for the preheated glass substrate through perturbation; adjusting the DC bias potential and using pulsed electric field-assisted depolarization based on the surface charge accumulation potential to obtain an activated glass substrate; performing eddy current heating compensation and electromagnetic stirring in a hot water tank based on the volume resistivity change curve to obtain a strengthened glass semi-finished product; performing thermoelectric power generation and surface plasma corona discharge based on the required compressive stress layer depth to obtain a strengthened glass preform with controllable compressive stress layer; and performing real-time redistribution of electric power on both hot and cold sides and terminal curing with residual power fed back to the power grid based on the falling ball impact strength feedback to obtain a zero-carbon emission finished glass product. This invention solves the problems of high energy consumption, large carbon emissions, and poor quality consistency in existing glass processing methods.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of glass product processing technology, and in particular to a method for precision processing and surface strengthening of glass products under zero carbon emission guidance. Background Technology

[0002] In recent years, the precision machining and surface strengthening of glass products typically involve multiple processes, including preheating, depolarization, strengthening, surface treatment, and final curing. Each process has strict requirements for parameters such as temperature field uniformity, surface electrostatic potential, and compressive stress layer depth. Currently, the process water heating for these processes mainly relies on natural gas boilers for hot water combustion and heat exchange. The preheating process uses a constant-temperature hot water circulation heating method, surface electrostatic elimination uses passive neutralization with ion fans, strengthening treatment uses independent heat treatment equipment, and hot water storage tanks use mechanical stirring to eliminate water temperature stratification. The heating and cooling power of the heat pump system operates in a fixed distribution mode. The control systems for these processes are independent of each other, and the setting of process parameters largely depends on the operator's experience, lacking a closed-loop control mechanism based on the real-time status of the glass products.

[0003] However, the aforementioned existing technologies have at least the following drawbacks: First, natural gas boiler heating consumes a large amount of fossil energy, producing significant carbon dioxide emissions, which does not meet the requirements of green manufacturing oriented towards zero carbon emissions. Furthermore, the boiler's thermal efficiency is relatively low, and energy utilization efficiency needs improvement. Second, during the preheating process, the constant-temperature hot water experiences temperature gradient attenuation as it is conducted from the pipeline to the glass surface, resulting in uneven distribution of the internal thermal field along the glass thickness direction, affecting the uniformity of subsequent strengthening treatments. Simultaneously, existing electrostatic elimination methods can only treat static electricity on the glass surface and cannot simultaneously eliminate residual polarization charges accumulated within the glass bulk phase due to the pyroelectric effect, leading to repeated accumulation of static electricity in subsequent processes and affecting processing yield. Third, water temperature stratification in the hot water storage tank leads to unstable heat release, and mechanical stirring increases additional energy consumption. The control of the compressive stress layer depth relies on separate heat treatment equipment, making online electrical adjustment based on the actual glass condition during processing impossible. The heat pump system has a fixed power distribution on both the hot and cold sides, making dynamic adjustment based on finished product strength feedback impossible, and the compressor's deceleration braking energy is not recovered, resulting in energy waste. The combined effects of these issues result in high energy consumption and large carbon emissions in glass product processing, and make it difficult to guarantee consistent processing quality. Summary of the Invention

[0004] The technical problem solved by this invention is that existing glass product processing processes suffer from high energy consumption, large carbon emissions, and poor consistency in processing quality.

[0005] To solve the above-mentioned technical problems, the present invention provides the following technical solution: As a preferred embodiment of the zero-carbon emission guided precision machining and surface strengthening method for glass products described in this invention, wherein: By acquiring the real-time frequency deviation signal of the power grid and the dielectric loss tangent of the glass product, active disturbance compensation of the power supply frequency of the heat pump compressor is performed to obtain the preheated glass substrate. Based on the surface charge accumulation potential of the preheated glass substrate, the DC bias potential of the heat pump circulating water circuit is regulated and pulsed electric field-assisted depolarization is performed to obtain an activated glass substrate. Based on the real-time volume resistivity change curve of the activated glass matrix, eddy current heating compensation and electromagnetic stirring are combined in the hot water storage tank during off-peak hours to obtain a reinforced glass semi-finished product. Based on the required compressive stress layer depth of the semi-finished reinforced glass, thermoelectric power generation driven by waste heat from the exhaust side of the heat pump compressor and plasma corona discharge treatment on the glass surface are carried out to obtain a reinforced glass preform with controllable compressive stress layer depth. Based on the real-time impact strength feedback value of the reinforced glass preform, the real-time redistribution of the electric power on both the hot and cold sides of the heat pump system and the terminal curing of the surplus power fed back to the power grid are carried out to obtain zero-carbon emission finished glass.

[0006] Furthermore, by acquiring the real-time frequency deviation signal of the power grid and the dielectric loss tangent of the glass product, active disturbance compensation for the power supply frequency of the heat pump compressor is performed to obtain a preheated glass substrate, including: The real-time frequency of the power grid is acquired by a frequency transmitter and compared with the rated frequency to obtain the frequency deviation signal; Measure the dielectric loss tangent of the glass product to be processed under power frequency conditions; The frequency deviation signal and the dielectric loss tangent are superimposed by a PID controller and a dielectric loss tangent feedforward compensator to be converted into a power supply frequency offset command for the heat pump compressor inverter driver. The heat pump compressor adjusts the output hot water temperature according to the power supply frequency offset command to generate controlled micro-pulses in the hot water temperature. The controlled micro-pulsating hot water is conducted to the surface of the glass product through a circulation pipeline. The dielectric loss characteristics of the glass product are used to convert the micro-pulsating electrical energy into supplementary internal heat to compensate for the temperature drop during the hot water conduction process, thus obtaining a preheated glass substrate.

[0007] Further, the controlled micro-pulsating hot water is conducted to the surface of the glass product through a circulation pipeline. Utilizing the dielectric loss characteristics of the glass product, the micro-pulsating electrical energy is converted into supplementary internal heat to compensate for temperature attenuation during hot water conduction, resulting in a preheated glass substrate, comprising: The controlled micro-pulsating hot water is introduced into the circulation jacket of the glass product preheating station to allow the hot water to exchange heat with the surface of the glass product. Meanwhile, the glass product is connected as a dielectric to the pulsating electric field of the frequency converter driver of the heat pump compressor. Under the controlled micro-pulsation drive, the dipoles inside the glass product undergo forced orientation polarization, generating dielectric relaxation loss, and the micro-pulsating electrical energy is directly converted into the bulk heat inside the glass product. The internal heat and the surface heat conducted by hot water to the surface of the glass product form a complementary coupled thermal field in the thickness direction of the glass product. The internal heat decays from the inside of the glass product to the outside, and the surface heat decays from the surface of the glass product to the inside. The internal heat and the surface heat intersect and superimpose at the center line of the thickness of the glass product, canceling out the nonlinear distortion of the temperature gradient caused by their individual conduction. This makes the overall internal thermal field of the glass product symmetrically and uniformly distributed in the thickness direction, resulting in a preheated glass substrate.

[0008] Further, based on the surface charge accumulation potential of the preheated glass substrate, the DC bias potential of the heat pump circulating water circuit is regulated and pulsed electric field-assisted depolarization is performed to obtain an activated glass substrate, including: The surface charge accumulation potential of the preheated glass substrate is detected by an electrostatic potentiometer. The metal pipe section of the heat pump circulating water circuit is configured as a flowing electrode, and a potential regulation loop is established between the metal pipe section and the surface of the glass product. Based on the polarity and amplitude of the surface charge accumulation potential, a DC bias potential with the opposite polarity to the surface charge accumulation potential is applied to the heat pump circulating water based on the potential control loop, so that polar ions in the circulating water migrate to the surface of the glass product under the action of the DC bias electric field, neutralizing the surface charge accumulation. While applying a DC bias potential, a rectangular wave pulse electric field is superimposed on the heat pump circulating water. The rectangular wave pulse electric field generates an alternating polarization field inside the glass product, forcing the bound charges in the bulk phase of the glass product to undergo periodic relaxation oscillations and release residual polarization charges. The frequency of the rectangular wave pulse electric field is lower than the power frequency, the duty cycle is less than the constant amplitude state, and the amplitude is lower than the dielectric breakdown threshold of the glass product. The neutralizing effect of the DC bias potential and the depolarizing effect of the rectangular wave pulse electric field are superimposed in time and space, so that the electrostatic potential on the surface of the glass product and the residual polarization charge in the bulk phase are eliminated simultaneously, resulting in an activated glass matrix.

[0009] Furthermore, based on the polarity and amplitude of the surface charge accumulation potential, a DC bias potential with the opposite polarity to the surface charge accumulation potential is applied to the heat pump circulating water using a potential control loop. This causes polar ions in the circulating water to migrate to the surface of the glass product under the influence of the DC bias electric field, neutralizing the surface charge accumulation. This includes: After signal conditioning, the surface charge accumulation potential is used as the voltage reference signal of the potential control circuit, so that the potential control circuit outputs a DC bias voltage that is positively correlated with the amplitude of the surface charge accumulation potential but opposite in polarity. The DC bias voltage is applied between the metal pipe section of the heat pump circulating water circuit and the glass product to establish a potential difference between the circulating water and the surface of the glass product. Polar ions in the circulating water migrate directionally to the surface of the glass product under the drive of the potential difference, and undergo an electric neutralization reaction with the accumulated charge on the surface; The residual potential change on the surface of the glass product is monitored in real time during the neutralization process. When the residual potential approaches zero, the DC bias voltage is dynamically reduced until the residual potential is maintained within the target threshold range, thus completing the neutralization of the surface charge.

[0010] Furthermore, while applying a DC bias potential, a rectangular wave pulsed electric field is superimposed on the heat pump circulating water. This rectangular wave pulsed electric field generates an alternating polarization field within the glass product, forcing the bound charges within the bulk phase of the glass product to undergo periodic relaxation oscillations, releasing residual polarization charges. This includes: The rectangular wave pulse electric field is coupled to the heat pump circulating water, so that the circulating water conducts the rectangular wave pulse electric field to the surface of the glass product. The rectangular wave pulse electric field is coupled into the bulk phase of the glass product through the surface of the glass product, and an alternating polarization field is established inside the glass product. Under the drive of the alternating polarization field, the bound charges within the bulk phase of the glass product undergo relaxation motion with alternating directions as the polarity of the pulsed electric field changes. During the turn-off period of the rectangular wave pulse electric field, the released charge in the bulk phase of the glass product diffuses to the surface along the bulk resistance path, connects with the external channel established by the DC bias potential, and forms a charge discharge path from the bulk phase to the surface, releasing the residual polarization charge.

[0011] Furthermore, based on the real-time volume resistivity change curve of the activated glass substrate, eddy current heating compensation and electromagnetic stirring are performed in the hot water storage tank during off-peak electricity hours to obtain a reinforced glass semi-finished product, including: The volume resistivity of the activated glass substrate is detected in real time, a volume resistivity change curve is generated, and the target heat storage temperature of the hot water storage tank during off-peak electricity hours is determined based on the slope trend of the volume resistivity change curve. During off-peak hours, an AC current is applied to the excitation coil on the outer wall of the hot water storage tank, inducing eddy currents in the metal wall of the hot water storage tank. The Joule effect of the eddy currents is used to heat and compensate the water in the tank. The alternating magnetic field generated by the power frequency AC power interacts with the eddy current to produce a Lorentz force, which drives the water in the hot water storage tank to circulate. The constant-temperature process water, after being treated by the combined heating compensation and electromagnetic stirring, is transported to the strengthening station to strengthen the activated glass substrate, thereby obtaining a semi-finished strengthened glass product.

[0012] Furthermore, the volume resistivity of the activated glass substrate is detected in real time, a volume resistivity change curve is generated, and the target heat storage temperature of the hot water storage tank during off-peak electricity hours is determined based on the slope trend of the volume resistivity change curve, including: At the start of the off-peak electricity period, the initial volume resistivity of the activated glass substrate at the preheating temperature was collected; The activated glass substrate is heated to the strengthening temperature at a set heating rate, and the volume resistivity is continuously collected at set time intervals during the heating process to generate a volume resistivity change curve with time as the horizontal axis and volume resistivity as the vertical axis. The volume resistivity change curve is numerically differentiated to obtain the volume resistivity change rate at each sampling time. When the rate of change of the volume resistivity first changes from a negative value to a positive value, the temperature corresponding to that moment is recorded as the transition temperature; The aforementioned transition temperature is used as the target heat storage temperature of the hot water storage tank during off-peak electricity periods.

[0013] Furthermore, based on the required compressive stress layer depth of the aforementioned reinforced glass semi-finished product, thermoelectric power generation driven by waste heat from the exhaust side of the heat pump compressor and plasma corona discharge treatment on the glass surface are performed to obtain a reinforced glass preform with controllable compressive stress layer depth, including: A thermoelectric conversion plate is installed on the outer wall of the exhaust pipe of a heat pump compressor. The hot end of the thermoelectric conversion plate is attached to the outer wall of the exhaust pipe and the cold end is exposed to the ambient air. Direct current is generated by the temperature difference between the outer wall of the exhaust pipe and the external environment. The DC current is boosted and applied to a discharge electrode positioned above the tempered glass semi-finished product, generating a corona discharge between the discharge electrode and the glass surface. Adjust the output voltage of the thermoelectric converter to control the intensity of the corona discharge; The plasma generated by the corona discharge acts on the glass surface to strengthen it, resulting in a strengthened glass preform with controllable compressive stress layer depth.

[0014] Furthermore, based on the real-time falling ball impact strength feedback value of the strengthened glass preform, the real-time redistribution of the electrical power on both the hot and cold sides of the heat pump system and the terminal curing of the surplus electricity fed back to the power grid are performed to obtain zero-carbon emission finished glass, including: The impact strength of the reinforced glass preform when dropped by a ball is detected, and a real-time strength feedback value is generated. The deviation is obtained by comparing the real-time intensity feedback value with the target intensity value. Based on the deviation, the power distribution ratio between the hot and cold sides of the heat pump system is redistributed in real time. The regenerative electrical energy generated by the heat pump system during the real-time redistribution process is fed back to the plant's power grid. After the real-time redistribution and surplus power feedback to the power grid are completed, the reinforced glass preform is terminally cured to obtain zero-carbon emission finished glass.

[0015] Compared with the prior art, the beneficial effects of the present invention are as follows: 1. This invention actively compensates for the power supply frequency disturbance of the heat pump compressor by acquiring the real-time frequency deviation signal of the power grid and the dielectric loss tangent of the glass product. This causes controlled micro-pulsations in the hot water and utilizes the dielectric loss of the glass product to convert the micro-pulsated electrical energy into supplementary internal heat, achieving a symmetrical and uniform distribution of the internal thermal field along the glass thickness direction, thus improving preheating quality. Furthermore, by adjusting the DC bias potential of the heat pump circulating water circuit and using a rectangular wave pulse electric field to assist depolarization based on the accumulated charge potential on the surface of the preheated glass substrate, the surface electrostatic potential and residual polarization charge in the bulk phase are eliminated synchronously, avoiding repeated accumulation of static electricity during subsequent processing. Finally, by adjusting the real-time frequency deviation signal of the activated glass substrate and the dielectric loss tangent of the glass product, this invention further improves preheating quality. The resistivity variation curve determines the target heat storage temperature of the hot water tank during off-peak electricity hours. A single coil simultaneously achieves eddy current heating compensation and electromagnetic stirring, eliminating water temperature stratification and improving off-peak electricity thermal energy storage efficiency. Direct current is generated by thermoelectric power generation driven by waste heat from the exhaust side of the heat pump compressor. After being boosted, this power is used for corona discharge plasma treatment of the glass surface, achieving online electrical adjustment of the compressive stress layer depth. Real-time redistribution of the power on both the hot and cold sides of the heat pump system based on the real-time impact strength feedback value of the reinforced glass preform, along with feeding regenerated electricity back to the grid, achieves closed-loop control of processing quality and cascaded energy utilization. This invention solves the problems of high energy consumption, large carbon emissions, and poor processing quality consistency in existing glass product processing.

[0016] 2. This invention actively compensates for the power supply frequency disturbance of the heat pump compressor by acquiring the real-time frequency deviation signal of the power grid and the dielectric loss tangent of the glass product. This causes the hot water to generate controlled micro-pulsations, and the glass product is connected to the pulsating electric field as a dielectric. This causes the internal heat of the bulk phase and the surface conduction heat to converge and superimpose at the center line of the thickness of the glass product, canceling the nonlinear distortion of the temperature gradient generated when each is conducted separately. This makes the overall internal thermal field of the glass product symmetrical and uniformly distributed in the thickness direction, improving the preheating quality and providing a uniform thermal state basis for the strengthening process.

[0017] 3. This invention neutralizes the accumulated surface charge by applying a DC bias potential of opposite polarity to the circulating water of the heat pump based on the potential control loop of the preheated glass substrate surface charge accumulation potential. At the same time, a rectangular wave pulse electric field is superimposed to generate an alternating polarization field inside the glass product, causing the bound charges in the bulk phase to undergo periodic relaxation oscillations and diffuse to the surface along the bulk resistance path. This forms a charge discharge path by connecting with the external channel established by the DC bias potential, so that the surface electrostatic potential and the residual polarization charge in the bulk phase are eliminated simultaneously, avoiding the yield loss caused by repeated accumulation of static electricity during processing.

[0018] 4. This invention utilizes the waste heat from the exhaust side of the heat pump compressor to drive a thermoelectric conversion plate to generate direct current. After being boosted, this current is applied to the discharge electrode to produce corona discharge, allowing plasma to act on the glass surface for strengthening treatment. This achieves online electrical adjustment of the compressive stress layer depth. Simultaneously, based on the real-time feedback value of the impact strength of the glass preform, the power of the heat pump system on both the hot and cold sides is redistributed in real time, and the regenerated electricity is fed back to the factory power grid, forming a closed-loop control of processing quality and cascaded utilization of energy. This eliminates the need to consume fossil fuels throughout the precision processing and surface strengthening of glass products, reducing energy consumption and carbon emissions while improving the consistency of processing quality. Attached Figure Description

[0019] Figure 1 This is a schematic diagram of the basic process of a zero-carbon emission guided precision machining and surface strengthening method for glass products, provided as an embodiment of the present invention. Detailed Implementation

[0020] To make the above-mentioned objects, features and advantages of the present invention more apparent and understandable, the specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Example 1

[0021] like Figure 1 As shown in the figure, this embodiment introduces a method for precision machining and surface strengthening of glass products under zero carbon emission guidance, including: Step 1: Obtain the real-time frequency deviation signal of the power grid and the dielectric loss tangent of the glass product, perform active disturbance compensation of the power supply frequency of the heat pump compressor, and obtain the preheated glass substrate.

[0022] This embodiment actively compensates for the power supply frequency disturbance of the heat pump compressor by acquiring the real-time frequency deviation signal of the power grid and the dielectric loss tangent of the glass product. This causes the hot water to generate controlled micro-pulsations, and the glass product is connected to the pulsating electric field as a dielectric. This causes the internal heat of the bulk phase and the surface conduction heat to converge and superimpose at the center line of the thickness of the glass product, canceling the nonlinear distortion of the temperature gradient caused by their individual conduction. This makes the overall internal thermal field of the glass product symmetrical and uniformly distributed in the thickness direction, providing a uniform thermal state basis for subsequent strengthening treatment.

[0023] Step 2: Based on the surface charge accumulation potential of the preheated glass substrate, the DC bias potential of the heat pump circulating water circuit is regulated and pulsed electric field-assisted depolarization is performed to obtain an activated glass substrate.

[0024] In this embodiment, a DC bias potential of opposite polarity is applied to neutralize the accumulated charge on the surface of the preheated glass substrate. At the same time, a rectangular wave pulse electric field is superimposed to cause the bound charge in the bulk phase to relax and oscillate and diffuse to the surface along the bulk resistance path. This forms a charge discharge path by connecting with the external channel established by the DC bias potential, so that the surface electrostatic potential and the residual polarization charge in the bulk phase are eliminated simultaneously, avoiding repeated accumulation of static electricity in subsequent processing.

[0025] Step 3: Based on the real-time volume resistivity change curve of the activated glass substrate, perform eddy current heating compensation and electromagnetic stirring synergistic treatment in the hot water storage tank during off-peak hours to obtain a reinforced glass semi-finished product.

[0026] This embodiment determines the target heat storage temperature of the hot water tank during off-peak hours by analyzing the slope of the real-time volume resistivity change curve of the activated glass substrate. This ensures that the heat storage temperature matches the physical properties of the glass itself. Furthermore, a single coil simultaneously achieves eddy current heating compensation and electromagnetic stirring, eliminating water temperature stratification in the tank and improving the thermal energy storage efficiency during off-peak hours.

[0027] Step 4: Based on the required compressive stress layer depth of the semi-finished reinforced glass, perform thermoelectric power generation driven by waste heat from the exhaust side of the heat pump compressor and plasma corona discharge treatment on the glass surface to obtain a reinforced glass preform with controllable compressive stress layer depth.

[0028] In this embodiment, the waste heat from the exhaust side of the heat pump compressor drives the thermoelectric conversion plate to generate direct current, which is then boosted and applied to the discharge electrode to generate corona discharge. This allows the plasma to act on the glass surface for strengthening treatment, achieving online electrical adjustment of the compressive stress layer depth without the need for an additional independent heat treatment power supply.

[0029] Step 5: Based on the real-time impact strength feedback value of the reinforced glass preform, perform real-time redistribution of the electric power on both the hot and cold sides of the heat pump system and terminal curing of the surplus power fed back to the power grid to obtain zero-carbon emission finished glass.

[0030] This embodiment redistributes the power of the heat pump system on both the hot and cold sides in real time based on the feedback value of the impact intensity of the dropped ball on the reinforced glass preform, and feeds the regenerated power back to the factory power grid, forming a closed-loop control of processing quality and cascade utilization of energy, thereby reducing energy consumption and improving the consistency of processing quality. Example 2

[0031] This embodiment describes the implementation steps of a method for precision machining and surface strengthening of glass products under zero carbon emission guidance, including: Step 1: Obtain the real-time frequency deviation signal of the power grid and the dielectric loss tangent of the glass product, perform active disturbance compensation of the power supply frequency of the heat pump compressor, and obtain the preheated glass substrate.

[0032] Step 1.1: Acquire the real-time frequency of the power grid using a frequency transmitter and compare it with the rated frequency to obtain the frequency deviation signal.

[0033] This embodiment acquires the real-time frequency of the power grid using a frequency transmitter and compares it with the rated frequency to obtain a frequency deviation signal, thus realizing real-time sensing of power grid frequency fluctuations.

[0034] Step 1.2: Measure the dielectric loss tangent of the glass product to be processed under power frequency conditions.

[0035] This embodiment measures the dielectric loss tangent of the glass product to be processed under power frequency conditions to provide a feedforward basis for subsequent frequency disturbance compensation.

[0036] Step 1.3: The frequency deviation signal and the dielectric loss tangent are superimposed by the PID controller and the dielectric loss tangent feedforward compensator to be converted into a power supply frequency offset command for the heat pump compressor inverter driver; the heat pump compressor adjusts the output hot water temperature according to the power supply frequency offset command to generate controlled micro-pulsations in the hot water temperature.

[0037] In this embodiment, the frequency deviation signal and dielectric loss tangent are superimposed by a PID controller and a feedforward compensator to be converted into a power supply frequency offset command. The heat pump compressor adjusts the output hot water temperature according to the command, so that the hot water temperature generates controlled micro-pulse, thereby realizing active disturbance compensation of the output hot water temperature of the heat pump.

[0038] Step 1.4: The controlled micro-pulsating hot water is conducted to the surface of the glass product through a circulation pipeline. The dielectric loss characteristics of the glass product are used to convert the micro-pulsating electrical energy into supplementary internal heat to compensate for the temperature drop during the hot water conduction process, thereby obtaining a preheated glass substrate.

[0039] In this embodiment, controlled micro-pulsating hot water is conducted to the surface of the glass product through a circulation pipeline. The dielectric loss characteristics of the glass product are used to convert the micro-pulsating electrical energy into supplementary internal heat to compensate for the temperature drop during the hot water conduction process, thereby obtaining a preheated glass substrate.

[0040] Step 1.4.1: The controlled micro-pulsating hot water is introduced into the circulation jacket of the glass product preheating station to allow the hot water to exchange heat with the surface of the glass product.

[0041] In this embodiment, controlled micro-pulsating hot water is introduced into the circulating jacket of the glass product preheating station, so that the hot water exchanges heat with the surface of the glass product.

[0042] Step 1.4.2: Simultaneously, the glass product is connected as a dielectric to the pulsating electric field of the frequency converter driver of the heat pump compressor. Under the controlled micro-pulsation drive, the dipoles inside the glass product undergo forced orientation polarization, generating dielectric relaxation loss, and the micro-pulsating electrical energy is directly converted into the bulk internal heat of the glass product body.

[0043] In this embodiment, the glass product is used as a dielectric to be connected to the pulsating electric field of the frequency converter driver of the heat pump compressor. Under the controlled micro-pulsation drive, the dipoles inside the glass product undergo forced orientation polarization, generating dielectric relaxation loss, and the micro-pulsating electrical energy is directly converted into the bulk internal heat of the glass product.

[0044] Step 1.4.3: The bulk heat and the surface heat conducted by hot water to the surface of the glass product form a complementary coupled thermal field in the thickness direction of the glass product. The bulk heat attenuates from the inside of the glass product to the outside, and the surface heat attenuates from the surface of the glass product to the inside. The bulk heat and the surface heat intersect and superimpose at the center line of the thickness of the glass product, canceling out the nonlinear distortion of the temperature gradient generated when they are conducted individually. This makes the overall internal thermal field of the glass product symmetrically and uniformly distributed in the thickness direction, thus obtaining a preheated glass substrate.

[0045] In this embodiment, the internal heat of the bulk phase and the surface conduction heat conducted by hot water to the surface of the glass product form a complementary coupled thermal field in the thickness direction of the glass product. The internal heat of the bulk phase attenuates from the inside of the glass product to the outside, and the surface conduction heat attenuates from the surface of the glass product to the inside. The two converge and superimpose at the center line of the thickness of the glass product, canceling out the nonlinear distortion of the temperature gradient generated when they are conducted individually. This makes the overall internal thermal field of the glass product symmetrically and uniformly distributed in the thickness direction, resulting in a preheated glass substrate.

[0046] Step 2: Based on the surface charge accumulation potential of the preheated glass substrate, the DC bias potential of the heat pump circulating water circuit is regulated and pulsed electric field-assisted depolarization is performed to obtain an activated glass substrate.

[0047] Step 2.1: Detect the surface charge accumulation potential of the preheated glass substrate using an electrostatic potentiometer.

[0048] In this embodiment, the surface charge accumulation potential of the preheated glass substrate is detected by an electrostatic potentiometer, thereby realizing the real-time acquisition of the electrostatic state of the glass surface.

[0049] Step 2.2: Configure the metal pipe section of the heat pump circulating water circuit as a flowing electrode, and establish a potential regulation loop between the metal pipe section and the surface of the glass product.

[0050] In this embodiment, the metal pipe section of the heat pump circulating water circuit is configured as a flowing electrode, and an electrostatic control loop is established between the metal pipe section and the surface of the glass product, so that the heat pump circulating water can simultaneously serve as a heat carrier and an electrostatic control medium.

[0051] Step 2.3: Based on the polarity and amplitude of the surface charge accumulation potential, apply a DC bias potential with the opposite polarity to the surface charge accumulation potential to the heat pump circulating water using a potential control loop, so that the polar ions in the circulating water migrate to the surface of the glass product under the action of the DC bias electric field, thereby neutralizing the surface charge accumulation.

[0052] Step 2.3.1: After signal conditioning, the surface charge accumulation potential is used as the voltage reference signal of the potential control circuit, so that the potential control circuit outputs a DC bias voltage that is positively correlated with the amplitude of the surface charge accumulation potential but opposite in polarity.

[0053] Step 2.3.2: Apply the DC bias voltage between the metal pipe section of the heat pump circulating water circuit and the glass product to establish a potential difference between the circulating water and the surface of the glass product.

[0054] Step 2.3.3: Polar ions in the circulating water migrate directionally to the surface of the glass product under the drive of the potential difference, and undergo an electric neutralization reaction with the accumulated charge on the surface.

[0055] Step 2.3.4: Monitor the change in residual potential on the surface of the glass product in real time during the neutralization process. When the residual potential approaches zero potential, dynamically reduce the DC bias voltage until the residual potential is maintained within the target threshold range, thus completing the neutralization of surface charge.

[0056] In this embodiment, a DC bias voltage of opposite polarity is applied based on the polarity and amplitude of the surface charge accumulation potential, causing polar ions in the circulating water to migrate to the surface of the glass product to neutralize the surface charge. The DC bias voltage is dynamically reduced in real time by monitoring the changes in residual potential until the residual potential is maintained within the target threshold range, thus avoiding excessive neutralization that could lead to reverse polarity charging.

[0057] Step 2.4: While applying a DC bias potential, a rectangular wave pulse electric field is superimposed on the heat pump circulating water. The rectangular wave pulse electric field generates an alternating polarization field inside the glass product, forcing the bound charges in the bulk phase of the glass product to undergo periodic relaxation oscillations and release residual polarization charges. The frequency of the rectangular wave pulse electric field is lower than the power frequency, the duty cycle is less than the constant amplitude state, and the amplitude is lower than the dielectric breakdown threshold of the glass product.

[0058] Step 2.4.1: Couple the rectangular wave pulse electric field to the heat pump circulating water, so that the circulating water conducts the rectangular wave pulse electric field to the surface of the glass product.

[0059] Step 2.4.2: The rectangular wave pulse electric field is coupled into the bulk phase of the glass product through the surface of the glass product, and an alternating polarization field is established inside the glass product.

[0060] Step 2.4.3: Under the drive of the alternating polarization field, the bound charges in the bulk phase of the glass product undergo relaxation motion with alternating directions as the polarity of the pulsed electric field changes.

[0061] Step 2.4.4: During the turn-off period of the rectangular wave pulse electric field, the released charge in the bulk phase of the glass product diffuses to the surface along the bulk resistance path, connects with the external channel established by the DC bias potential, and forms a charge discharge path from the bulk phase to the surface, releasing the residual polarization charge.

[0062] In this embodiment, a rectangular wave pulse electric field is superimposed while a DC bias potential is applied, causing the bound charges in the bulk phase to relax and oscillate. During the pulse turn-off period, the charges diffuse along the bulk resistance path to the surface, connecting with the external channel established by the DC bias potential to form a charge discharge path, releasing residual polarized charges and achieving deep emptying of the bulk phase charges.

[0063] Step 2.5: The neutralizing effect of the DC bias potential and the depolarizing effect of the rectangular wave pulse electric field are superimposed in time and space, so that the electrostatic potential on the surface of the glass product and the residual polarization charge in the bulk phase are eliminated simultaneously, thus obtaining an activated glass matrix.

[0064] This embodiment achieves a synergistic superposition of the neutralizing effect of the DC bias potential and the depolarizing effect of the rectangular wave pulse electric field in time and space, thereby simultaneously eliminating the electrostatic potential on the surface of the glass product and the residual polarization charge in the bulk phase, resulting in an activated glass matrix. This avoids repeated accumulation of static electricity during subsequent processing, eliminates the need for additional independent static elimination and depolarization equipment, and reduces equipment costs.

[0065] Step 3: Based on the real-time volume resistivity change curve of the activated glass substrate, perform eddy current heating compensation and electromagnetic stirring synergistic treatment in the hot water storage tank during off-peak hours to obtain a reinforced glass semi-finished product.

[0066] Step 3.1: Real-time detection of the volume resistivity of the activated glass substrate, generation of a volume resistivity change curve, and determination of the target heat storage temperature of the hot water storage tank during off-peak electricity periods based on the slope trend of the volume resistivity change curve.

[0067] Step 3.1.1: At the beginning of the off-peak electricity period, the initial volume resistivity of the activated glass substrate at the preheating temperature is collected.

[0068] Step 3.1.2: Heat the activated glass substrate to the strengthening temperature at a set heating rate, and continuously collect the volume resistivity at set time intervals during the heating process to generate a volume resistivity change curve with time as the horizontal axis and volume resistivity as the vertical axis.

[0069] Step 3.1.3: Perform numerical differentiation on the volume resistivity change curve to obtain the volume resistivity change rate at each sampling time.

[0070] Step 3.1.4: When the rate of change of the volume resistivity first changes from a negative value to a positive value, record the temperature corresponding to that moment as the transition temperature.

[0071] Step 3.1.5: Use the aforementioned transition temperature as the target heat storage temperature of the hot water storage tank during off-peak electricity periods.

[0072] This embodiment generates a volume resistivity change curve by real-time detection of the volume resistivity of the activated glass substrate, and obtains the volume resistivity change rate at each sampling time by differentiating its value. When the change rate first changes from a negative value to a positive value, the temperature corresponding to that time is recorded as the transition temperature. The transition temperature is used as the target heat storage temperature of the hot water storage tank during off-peak electricity periods, so that the heat storage temperature matches the physical properties of the glass itself.

[0073] Step 3.2: During off-peak hours, power frequency AC current is passed through the excitation coil on the outer wall of the hot water storage tank to induce eddy currents in the metal wall of the hot water storage tank. The Joule effect of the eddy currents is used to heat and compensate the water in the tank.

[0074] In this embodiment, during off-peak hours, an industrial frequency alternating current is applied to the excitation coil on the outer wall of the hot water storage tank, inducing eddy currents in the metal wall of the hot water storage tank. The Joule effect of the eddy currents is used to heat and compensate the water in the tank.

[0075] Step 3.3: The alternating magnetic field generated by the power frequency AC power interacts with the eddy current to produce Lorentz force, which drives the water in the hot water storage tank to circulate.

[0076] This embodiment utilizes the interaction between the alternating magnetic field generated by the power frequency AC and the eddy current to produce Lorentz force, which drives the water circulation in the hot water storage tank without the need for an additional independent mechanical stirring device.

[0077] Step 3.4: The constant-temperature process water, after being treated by the combined heating compensation and electromagnetic stirring, is transported to the strengthening station to strengthen the activated glass substrate, thereby obtaining a strengthened glass semi-finished product.

[0078] In this embodiment, constant-temperature process water that has undergone combined heating compensation and electromagnetic stirring is transported to the strengthening station to strengthen the activated glass substrate, thereby obtaining a semi-finished strengthened glass product.

[0079] Step 4: Based on the required compressive stress layer depth of the semi-finished reinforced glass, perform thermoelectric power generation driven by waste heat from the exhaust side of the heat pump compressor and plasma corona discharge treatment on the glass surface to obtain a reinforced glass preform with controllable compressive stress layer depth.

[0080] Step 4.1: Install a thermoelectric conversion plate on the outer wall of the exhaust pipe of the heat pump compressor. The hot end of the thermoelectric conversion plate is attached to the outer wall of the exhaust pipe, and the cold end is exposed to the ambient air. Direct current is generated by the temperature difference between the outer wall of the exhaust pipe and the external environment.

[0081] In this embodiment, a thermoelectric conversion plate is installed on the outer wall of the exhaust pipe of the heat pump compressor. The hot end is attached to the outer wall of the exhaust pipe, and the cold end is exposed to the ambient air. Direct current is generated by the temperature difference between the outer wall of the exhaust pipe and the external environment, so that the power source can be obtained without external power supply.

[0082] Step 4.2: The DC current is boosted and applied to the discharge electrode located above the tempered glass semi-finished product, generating corona discharge between the discharge electrode and the glass surface.

[0083] In this embodiment, the DC voltage is boosted and applied to the discharge electrode located above the tempered glass semi-finished product, generating a corona discharge between the discharge electrode and the glass surface.

[0084] Step 4.3: Adjust the output voltage of the thermoelectric converter to control the intensity of the corona discharge.

[0085] This embodiment controls the intensity of corona discharge by adjusting the output voltage of the thermoelectric converter, thereby achieving online electrical adjustment of the compressive stress layer depth.

[0086] Step 4.4: The plasma generated by the corona discharge acts on the glass surface to strengthen the glass surface and obtain a strengthened glass preform with controllable compressive stress layer depth.

[0087] Step 5: Based on the real-time falling ball impact strength feedback value of the reinforced glass preform, perform real-time redistribution of the electric power on both the hot and cold sides of the heat pump system and terminal curing of the surplus power fed back to the power grid to obtain zero-carbon emission finished glass.

[0088] Step 5.1: Detect the drop ball impact strength of the reinforced glass preform and generate a real-time strength feedback value.

[0089] This embodiment detects the impact strength of a falling ball on a reinforced glass preform and generates a real-time strength feedback value, thus achieving a real-time quantitative evaluation of the strengthening effect.

[0090] Step 5.2: Compare the real-time intensity feedback value with the target intensity value to obtain the deviation.

[0091] This embodiment compares the real-time intensity feedback value with the target intensity value to obtain the deviation, providing a control basis for power adjustment.

[0092] Step 5.3: Based on the deviation, real-time redistribution of the electrical power distribution ratio on both the hot and cold sides of the heat pump system.

[0093] This embodiment redistributes the power distribution ratio between the hot and cold sides of the heat pump system in real time based on the deviation, and uses the processing quality deviation as the direct input for heat pump power regulation, replacing the traditional control mode based on temperature or pressure, and realizing closed-loop control of processing quality.

[0094] Step 5.4: Feed the regenerated electricity generated by the heat pump system during the real-time redistribution process back to the plant's power grid.

[0095] This embodiment feeds the regenerated electricity generated by the heat pump system during real-time redistribution back to the plant's power grid, enabling the compressor's deceleration braking energy to be recovered and utilized, avoiding energy waste, and realizing energy cascade utilization.

[0096] Step 5.5: After the real-time redistribution and surplus power feedback to the power grid are completed, the reinforced glass preform is terminally cured to obtain zero-carbon emission finished glass.

[0097] In this embodiment, after real-time redistribution and surplus power feedback to the power grid are completed, the reinforced glass preform is terminally cured to obtain zero-carbon emission finished glass. This means that the entire processing does not require the consumption of fossil energy, thus reducing energy consumption and carbon emissions.

[0098] Those skilled in the art will understand that embodiments of the present invention can be provided as methods, systems, or computer program products. Therefore, the present invention can take the form of a completely hardware embodiment, a completely software embodiment, or an embodiment combining software and hardware aspects. Furthermore, the present invention can take the form of a computer program product implemented on one or more computer-usable storage media containing computer-usable program code. It should be noted that the above embodiments are merely illustrative of the technical solutions of the present invention and are not intended to limit it. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solutions of the present invention without departing from the spirit and scope of the technical solutions of the present invention, and all such modifications and substitutions should be covered within the scope of the claims of the present invention.

Claims

1. A method for precision machining and surface strengthening of glass products under zero carbon emission guidance, characterized in that, include: By acquiring the real-time frequency deviation signal of the power grid and the dielectric loss tangent of the glass product, active disturbance compensation of the power supply frequency of the heat pump compressor is performed to obtain the preheated glass substrate. Based on the surface charge accumulation potential of the preheated glass substrate, the DC bias potential of the heat pump circulating water circuit is regulated and pulsed electric field-assisted depolarization is performed to obtain an activated glass substrate. Based on the real-time volume resistivity change curve of the activated glass matrix, eddy current heating compensation and electromagnetic stirring are combined in the hot water storage tank during off-peak hours to obtain a reinforced glass semi-finished product. Based on the required compressive stress layer depth of the semi-finished reinforced glass, thermoelectric power generation driven by waste heat from the exhaust side of the heat pump compressor and plasma corona discharge treatment on the glass surface are carried out to obtain a reinforced glass preform with controllable compressive stress layer depth. Based on the real-time impact strength feedback value of the reinforced glass preform, the real-time redistribution of the electric power on both the hot and cold sides of the heat pump system and the terminal curing of the surplus power fed back to the power grid are carried out to obtain zero-carbon emission finished glass.

2. The method for precision machining and surface strengthening of glass products under zero carbon emission guidance as described in claim 1, characterized in that, By acquiring the real-time frequency deviation signal of the power grid and the dielectric loss tangent of the glass product, active disturbance compensation for the power supply frequency of the heat pump compressor is performed to obtain the preheated glass substrate, including: The real-time frequency of the power grid is acquired by a frequency transmitter and compared with the rated frequency to obtain the frequency deviation signal; Measure the dielectric loss tangent of the glass product to be processed under power frequency conditions; The frequency deviation signal and the dielectric loss tangent are superimposed by a PID controller and a dielectric loss tangent feedforward compensator to be converted into a power supply frequency offset command for the heat pump compressor inverter driver. The heat pump compressor adjusts the output hot water temperature according to the power supply frequency offset command to generate controlled micro-pulses in the hot water temperature. The controlled micro-pulsating hot water is conducted to the surface of the glass product through a circulation pipeline. The dielectric loss characteristics of the glass product are used to convert the micro-pulsating electrical energy into supplementary internal heat to compensate for the temperature drop during the hot water conduction process, thus obtaining a preheated glass substrate.

3. The method for precision machining and surface strengthening of glass products under zero carbon emission guidance as described in claim 2, characterized in that, The controlled micro-pulsating hot water is conducted to the surface of the glass product through a circulation pipeline. Utilizing the dielectric loss characteristics of the glass product, the micro-pulsating electrical energy is converted into supplementary internal heat to compensate for temperature attenuation during hot water conduction, resulting in a preheated glass substrate, comprising: The controlled micro-pulsating hot water is introduced into the circulation jacket of the glass product preheating station to allow the hot water to exchange heat with the surface of the glass product. Meanwhile, the glass product is connected as a dielectric to the pulsating electric field of the frequency converter driver of the heat pump compressor. Under the controlled micro-pulsation drive, the dipoles inside the glass product undergo forced orientation polarization, generating dielectric relaxation loss, and the micro-pulsating electrical energy is directly converted into the bulk heat inside the glass product. The internal heat and the surface heat conducted by hot water to the surface of the glass product form a complementary coupled thermal field in the thickness direction of the glass product. The internal heat decays from the inside of the glass product to the outside, and the surface heat decays from the surface of the glass product to the inside. The internal heat and the surface heat intersect and superimpose at the center line of the thickness of the glass product, canceling out the nonlinear distortion of the temperature gradient caused by their individual conduction. This makes the overall internal thermal field of the glass product symmetrically and uniformly distributed in the thickness direction, resulting in a preheated glass substrate.

4. The method for precision machining and surface strengthening of glass products under zero carbon emission guidance as described in claim 3, characterized in that, Based on the surface charge accumulation potential of the preheated glass substrate, DC bias potential regulation and pulsed electric field-assisted depolarization of the heat pump circulating water circuit are performed to obtain an activated glass substrate, including: The surface charge accumulation potential of the preheated glass substrate is detected by an electrostatic potentiometer. The metal pipe section of the heat pump circulating water circuit is configured as a flowing electrode, and a potential regulation loop is established between the metal pipe section and the surface of the glass product. Based on the polarity and amplitude of the surface charge accumulation potential, a DC bias potential with the opposite polarity to the surface charge accumulation potential is applied to the heat pump circulating water based on the potential control loop, so that polar ions in the circulating water migrate to the surface of the glass product under the action of the DC bias electric field, neutralizing the surface charge accumulation. While applying a DC bias potential, a rectangular wave pulse electric field is superimposed on the heat pump circulating water. The rectangular wave pulse electric field generates an alternating polarization field inside the glass product, forcing the bound charges in the bulk phase of the glass product to undergo periodic relaxation oscillations and release residual polarization charges. The frequency of the rectangular wave pulse electric field is lower than the power frequency, the duty cycle is less than the constant amplitude state, and the amplitude is lower than the dielectric breakdown threshold of the glass product. The neutralizing effect of the DC bias potential and the depolarizing effect of the rectangular wave pulse electric field are superimposed in time and space, so that the electrostatic potential on the surface of the glass product and the residual polarization charge in the bulk phase are eliminated simultaneously, resulting in an activated glass matrix.

5. The method for precision machining and surface strengthening of glass products under zero carbon emission guidance as described in claim 4, characterized in that, Based on the polarity and amplitude of the surface charge accumulation potential, a DC bias potential with the opposite polarity to the surface charge accumulation potential is applied to the heat pump circulating water using a potential control loop. This causes polar ions in the circulating water to migrate to the surface of the glass product under the influence of the DC bias electric field, neutralizing the surface charge accumulation. This includes: After signal conditioning, the surface charge accumulation potential is used as the voltage reference signal of the potential control circuit, so that the potential control circuit outputs a DC bias voltage that is positively correlated with the amplitude of the surface charge accumulation potential but opposite in polarity. The DC bias voltage is applied between the metal pipe section of the heat pump circulating water circuit and the glass product to establish a potential difference between the circulating water and the surface of the glass product. Polar ions in the circulating water migrate directionally to the surface of the glass product under the drive of the potential difference, and undergo an electric neutralization reaction with the accumulated charge on the surface; The residual potential change on the surface of the glass product is monitored in real time during the neutralization process. When the residual potential approaches zero, the DC bias voltage is dynamically reduced until the residual potential is maintained within the target threshold range, thus completing the neutralization of the surface charge.

6. The method for precision machining and surface strengthening of glass products under zero carbon emission guidance as described in claim 4, characterized in that, While applying a DC bias potential, a rectangular wave pulsed electric field is superimposed on the circulating water of the heat pump. This rectangular wave pulsed electric field generates an alternating polarization field inside the glass product, forcing the bound charges within the bulk phase of the glass product to undergo periodic relaxation oscillations, releasing residual polarization charges, including: The rectangular wave pulse electric field is coupled to the heat pump circulating water, so that the circulating water conducts the rectangular wave pulse electric field to the surface of the glass product. The rectangular wave pulse electric field is coupled into the bulk phase of the glass product through the surface of the glass product, and an alternating polarization field is established inside the glass product. Under the drive of the alternating polarization field, the bound charges within the bulk phase of the glass product undergo relaxation motion with alternating directions as the polarity of the pulsed electric field changes. During the turn-off period of the rectangular wave pulse electric field, the released charge in the bulk phase of the glass product diffuses to the surface along the bulk resistance path, connects with the external channel established by the DC bias potential, and forms a charge discharge path from the bulk phase to the surface, releasing the residual polarization charge.

7. The method for precision machining and surface strengthening of glass products under zero carbon emission guidance as described in claim 6, characterized in that, Based on the real-time volume resistivity change curve of the activated glass matrix, eddy current heating compensation and electromagnetic stirring are performed in the hot water storage tank during off-peak electricity hours to obtain a reinforced glass semi-finished product, including: The volume resistivity of the activated glass substrate is detected in real time, a volume resistivity change curve is generated, and the target heat storage temperature of the hot water storage tank during off-peak electricity hours is determined based on the slope trend of the volume resistivity change curve. During off-peak hours, an AC current is applied to the excitation coil on the outer wall of the hot water storage tank, inducing eddy currents in the metal wall of the hot water storage tank. The Joule effect of the eddy currents is used to heat and compensate the water in the tank. The alternating magnetic field generated by the power frequency AC power interacts with the eddy current to produce a Lorentz force, which drives the water in the hot water storage tank to circulate. The constant-temperature process water, after being treated by the combined heating compensation and electromagnetic stirring, is transported to the strengthening station to strengthen the activated glass substrate, thereby obtaining a semi-finished strengthened glass product.

8. The method for precision machining and surface strengthening of glass products under zero carbon emission guidance as described in claim 7, characterized in that, The volume resistivity of the activated glass substrate is detected in real time, a volume resistivity change curve is generated, and the target heat storage temperature of the hot water storage tank during off-peak electricity hours is determined based on the slope trend of the volume resistivity change curve, including: At the start of the off-peak electricity period, the initial volume resistivity of the activated glass substrate at the preheating temperature was collected; The activated glass substrate is heated to the strengthening temperature at a set heating rate, and the volume resistivity is continuously collected at set time intervals during the heating process to generate a volume resistivity change curve with time as the horizontal axis and volume resistivity as the vertical axis. The volume resistivity change curve is numerically differentiated to obtain the volume resistivity change rate at each sampling time. When the rate of change of the volume resistivity first changes from a negative value to a positive value, the temperature corresponding to that moment is recorded as the transition temperature; The aforementioned transition temperature is used as the target heat storage temperature of the hot water storage tank during off-peak electricity periods.

9. The method for precision machining and surface strengthening of glass products under zero carbon emission guidance as described in claim 8, characterized in that, Based on the required compressive stress layer depth of the semi-finished reinforced glass, thermoelectric power generation driven by waste heat from the exhaust side of a heat pump compressor and plasma corona discharge treatment on the glass surface are performed to obtain a reinforced glass preform with controllable compressive stress layer depth, including: A thermoelectric conversion plate is installed on the outer wall of the exhaust pipe of a heat pump compressor. The hot end of the thermoelectric conversion plate is attached to the outer wall of the exhaust pipe and the cold end is exposed to the ambient air. Direct current is generated by the temperature difference between the outer wall of the exhaust pipe and the external environment. The DC current is boosted and applied to a discharge electrode positioned above the tempered glass semi-finished product, generating a corona discharge between the discharge electrode and the glass surface. Adjust the output voltage of the thermoelectric converter to control the intensity of the corona discharge; The plasma generated by the corona discharge acts on the glass surface to strengthen it, resulting in a strengthened glass preform with controllable compressive stress layer depth.

10. The method for precision machining and surface strengthening of glass products under zero carbon emission guidance as described in claim 9, characterized in that, Based on the real-time falling ball impact strength feedback value of the strengthened glass preform, the real-time redistribution of the electrical power on both the hot and cold sides of the heat pump system and the terminal curing of the surplus power fed back to the power grid are performed to obtain zero-carbon emission finished glass, including: The impact strength of the reinforced glass preform when dropped by a ball is detected, and a real-time strength feedback value is generated. The deviation is obtained by comparing the real-time intensity feedback value with the target intensity value. Based on the deviation, the power distribution ratio between the hot and cold sides of the heat pump system is redistributed in real time. The regenerative electrical energy generated by the heat pump system during the real-time redistribution process is fed back to the plant's power grid. After the real-time redistribution and surplus power feedback to the power grid are completed, the reinforced glass preform is terminally cured to obtain zero-carbon emission finished glass.