A dodecyl polyoxyethylene (5) amine oxide with low residual amine content and high hard water resistance, its preparation method and application

By using pre-hydration treatment, segmented oxidation and enzyme catalysis, the problems of insufficient oxidation of tertiary amine and residual hydrogen peroxide in the preparation of dodecyl polyoxyethylene (5) amine oxide were solved, and amine oxide with low residual amine and high hard water resistance was prepared, which improved the stability and compounding performance of the product.

CN123106480APending Publication Date: 2026-11-17HT FINE CHEM CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611341363.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-01
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing technologies have problems in the preparation of dodecyl polyoxyethylene (5) amine oxide, such as insufficient oxidation of tertiary amine, high residual tertiary amine content, increased hydrogen peroxide residue, and decreased stability and compounding performance of the product under high hard water conditions. These problems are particularly difficult to control at high conversion rates.

Method used

By pre-hydration treatment, staged addition of hydrogen peroxide and catalyst, and a coordination catalytic composition combining tungstate, phosphoric acid and polyhydroxy coordination components, residual hydrogen peroxide is decomposed by catalase catalysis, and purified using porous adsorption materials, avoiding the use of sulfite reducing agents, and controlling residual peroxides and pigments in the product.

Benefits of technology

The preparation of dodecyl polyoxyethylene (5) amine oxide with low free amine, low residual hydrogen peroxide, low color and high hard water adaptability was achieved, which improved the transparency stability and foam retention performance of the product under high hard water conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

This invention discloses a dodecyl polyoxyethylene (5) amine oxide with low residual amine and high hard water resistance, its preparation method, and its application. The method involves pre-hydrating the dodecyl polyoxyethylene (5) tertiary amine and forming a coordination catalyst using tungstate, a phosphoric acid-containing component, and a polyhydroxy coordination component. Hydrogen peroxide is divided into first, second, and third oxidant portions for gradient oxidation. After the tertiary amine conversion reaches over 98.5%, the reaction temperature and pH are adjusted, a reactivation adjusting solution is added, and the third oxidant portion is added at a low feeding rate for final deep oxidation. After the reaction, residual peroxides are decomposed using catalase and purified using porous adsorption materials. This method can reduce the residual free tertiary amine and hydrogen peroxide during the oxidation of polyether tertiary amines, reduce the introduction of salt post-treatment agents, and the resulting polyether amine oxide exhibits good low-temperature stability, hard water transparency, foam retention, and compound thickening stability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of fine chemical and surfactant synthesis technology, specifically relating to a dodecyl polyoxyethylene (5) amine oxide and its preparation method and application. Background Technology

[0002] Dodecyl polyoxyethylene (5) amine oxide is a nonionic / ampholy surfactant obtained by oxidizing a dodecyl polyoxyethylene ether tertiary amine containing about 5 oxyethylene units as a nitrogen-containing precursor to form an N→O structure. Compared with conventional dodecyl dimethyl amine oxide, the polyoxyethylene chain can improve hydrophilicity, low-temperature solubility, and compatibility with anionic and nonionic surfactants.

[0003] However, the introduction of polyoxyethylene chains also causes the tertiary amine oxidation process to exhibit mass transfer and microenvironment characteristics different from those of ordinary aliphatic tertiary amines. A hydrogen-bonded solvation layer forms between the polyether chains and water, and local association may occur at higher raw material concentrations, affecting the effective collision between the tertiary amine nitrogen centers and peroxides. In the later stages of the reaction with high conversion rates, the residual tertiary amine concentration decreases, and simply extending the reaction time or increasing the amount of hydrogen peroxide can easily lead to increased peroxide residue, darker color, and the risk of side reactions.

[0004] Existing technologies typically improve the conversion rate of tertiary amines by adding excess hydrogen peroxide and then using reducing agents such as sulfites to eliminate residual peroxides after the reaction. However, this method is prone to introducing inorganic ions such as sulfates and sulfites, and it fails to address the problem of the residual tertiary amine being difficult to further oxidize during the high-conversion stage. Therefore, there is a need for a method that can simultaneously control the oxidation microenvironment of polyether tertiary amines, improve the final oxidation efficiency, and reduce the salt load in the post-treatment process. Summary of the Invention

[0005] This invention addresses the problems existing in the preparation of polyether amine oxides by oxidation of dodecyl polyoxyethylene ether tertiary amines, such as insufficient oxidation of tertiary amines, high residual free tertiary amines after the reaction, easy increase in hydrogen peroxide residue after increasing the amount of hydrogen peroxide to improve the conversion rate of tertiary amines, easy introduction of inorganic salts into the product when using sulfite reducing agents for post-treatment, and decreased transparency stability, foam retention performance and compound thickening performance of the obtained amine oxides under high hardness water conditions. It provides a dodecyl polyoxyethylene (5) amine oxide with low residual amine and high hard water resistance, as well as its preparation method and application.

[0006] This invention further addresses the structural characteristics of dodecyl polyoxyethylene (5) tertiary amine, which distinguish it from ordinary dodecyl dimethyl tertiary amine, by controlling its oxidation process. The dodecyl polyoxyethylene (5) tertiary amine molecule simultaneously contains long-chain alkyl groups, polyoxyethylene segments, and tertiary amine groups. In an aqueous reaction medium, the polyoxyethylene segments can form strong hydrogen bonds with water molecules. At higher raw material concentrations, molecules may also associate to varying degrees, altering the local solvation state around the tertiary amine groups and the diffusion state of hydrogen peroxide towards the vicinity of the tertiary amine groups. Therefore, simply increasing the reaction temperature, extending the reaction time, or increasing the excess hydrogen peroxide coefficient cannot simultaneously solve the problems of deep tertiary amine conversion, residual hydrogen peroxide control, and product color stability.

[0007] Based on the above understanding, the present invention first pre-hydrates the dodecyl polyoxyethylene (5) tertiary amine to make the polyoxyethylene segments form a relatively uniform hydration state before entering the oxidation reaction; then, a coordination catalytic composition is formed by using tungstate, phosphoric acid-containing components and polyhydroxy coordination components, and hydrogen peroxide is added in stages according to the pre-stage induced oxidation, the middle stage main oxidation and the post-stage deep oxidation; when the conversion rate of tertiary amine reaches a high level, instead of simply extending the heat preservation time, the acid-base state and catalytic coordination environment at the end of the reaction are changed by adding a reactivation conditioning liquid, and the instantaneous addition rate of hydrogen peroxide at the end is reduced, so that the remaining low concentration of tertiary amine can further undergo N-oxidation reaction.

[0008] After oxidation, the present invention further employs catalase to catalyze the decomposition of residual hydrogen peroxide and uses porous adsorption materials for purification, thereby controlling residual peroxides, pigments and trace catalytic components in the product without using sulfite-based chemical reducing agents.

[0009] Therefore, the present invention does not adjust a single reaction parameter, but continuously controls the dodecyl polyoxyethylene (5) tertiary amine from the pre-reaction hydration state, oxidant supply state, catalytic environment, high conversion rate final reaction state to the post-reaction purification process, thereby obtaining dodecyl polyoxyethylene (5) amine oxide with low free amine, low residual hydrogen peroxide, low color, low temperature stability and high hard water adaptability.

[0010] To achieve the above objectives, the present invention provides a method for preparing dodecyl polyoxyethylene (5) amine oxide with low residual amine and high hard water resistance, comprising the following steps:

[0011] Prehydration treatment of S1, dodecyl polyoxyethylene (5) tertiary amine

[0012] Dodecyl polyoxyethylene (5) tertiary amine was mixed with the first portion of deionized water to obtain a mixture containing 55-75% by mass of dodecyl polyoxyethylene (5) tertiary amine. The mixture was stirred at 45-60°C for 20-60 min. The pH of the mixture was then adjusted to 6.8-7.8 using an acidic regulator, and the mixture was stirred for another 10-30 min to obtain a prehydrated tertiary amine solution.

[0013] Preferably, the average EO addition number of the dodecyl polyoxyethylene (5) tertiary amine is 4.5 to 5.5; more preferably 4.8 to 5.2; and even more preferably 5.0.

[0014] Preferably, the mass percentage of dodecyl polyoxyethylene (5) tertiary amine in the prehydrated tertiary amine solution is 60-70%, more preferably 62-68%.

[0015] Preferably, the prehydration temperature is 48–58°C, more preferably 50–55°C; the prehydration time is 30–50 min, more preferably 35–45 min.

[0016] As a preferred value of the present invention, the prehydration temperature is 53°C and the prehydration time is 40 min.

[0017] The acid regulator may be selected from one or more of citric acid, lactic acid, gluconic acid, and phosphoric acid; citric acid is preferred.

[0018] The present invention incorporates the aforementioned pre-hydration step, rather than simply diluting the raw materials with water. The dodecyl polyoxyethylene (5) tertiary amine contains multiple ether oxygen atoms, which can act as hydrogen bond acceptors to form a solvation reaction with water molecules. By controlling the concentration, temperature, and processing time of the tertiary amine before formal oxidation, the polyoxyethylene segments can be pre-formed into a relatively uniform hydration state, reducing mass transfer differences caused by local association in high-concentration polyether tertiary amines, and allowing the subsequently added catalytic components and hydrogen peroxide to be more uniformly dispersed in the reaction medium.

[0019] When the prehydration temperature is below 45°C, the movement of polyether segments and the establishment of hydration equilibrium are slow; when it is above 60°C, the functional distinction between the prehydration step and the subsequent oxidation reaction is weakened, and the possibility of color change due to prolonged residence of the material at higher temperatures is increased. Therefore, the present invention preferably uses a prehydration temperature range of 45–60°C.

[0020] S2, Preparation of Coordination Catalyst Solution

[0021] Tungstate, phosphoric acid-containing component and polyhydroxy coordination component are added to the second part of deionized water at a mass ratio of 1:(0.20~0.80):(0.10~0.60) and stirred at 40~55℃ for 10~30 min to obtain coordination catalytic solution.

[0022] The tungstate can be at least one of sodium tungstate, potassium tungstate, and ammonium tungstate, preferably sodium tungstate.

[0023] The phosphoric acid component can be one or more of phosphoric acid, sodium dihydrogen phosphate, and potassium dihydrogen phosphate, preferably phosphoric acid.

[0024] The polyhydroxy coordination component may be one or more of gluconic acid, sodium gluconate, sorbitol, and glycerol, preferably gluconic acid and / or sodium gluconate.

[0025] Preferably, the mass ratio of tungstate, phosphoric acid component, and polyhydroxy coordination component is 1:(0.30-0.60):(0.20-0.40).

[0026] As a preferred point value, the mass ratio of sodium tungstate, phosphoric acid, and gluconic acid is 1:0.40:0.27.

[0027] Preferably, the amount of tungstate added is 0.05 to 0.30 parts based on 100 parts by weight of dodecyl polyoxyethylene (5) tertiary amine, and more preferably 0.10 to 0.22 parts.

[0028] This invention does not involve directly adding a single tungstate to the reaction solution. Instead, the tungstate is first pre-contaminated with a phosphoric acid-containing component and a polyhydroxy coordination component in an aqueous phase. The phosphoric acid-containing component is used to adjust the acid-base balance and condensation state around the tungstate, while the polyhydroxy coordination component interacts with oxygen-containing metal species in the reaction medium through hydroxyl and carboxyl groups, ensuring that the catalytically active component has a good dispersion state before entering the high-concentration polyether tertiary amine medium.

[0029] Therefore, the three components described in this invention are not simply a random mixture of conventional catalysts, but are used in conjunction with the aforementioned pre-hydrated tertiary amine solution to allow the catalytically active components to enter the polyether tertiary amine medium that has already undergone hydration treatment, thereby reducing the possibility of excessively high local catalyst concentrations and rapid decomposition of local peroxides.

[0030] S3, first stage and second stage oxidation

[0031] Add the coordination catalyst obtained in step S2 to the prehydrated tertiary amine solution obtained in step S1, stir evenly, and then heat to 65-72℃.

[0032] The total amount of hydrogen peroxide added was determined according to the molar ratio of oxidizable tertiary amine groups to effective hydrogen peroxide in dodecyl polyoxyethylene (5) tertiary amine being 1:(1.01~1.08).

[0033] The hydrogen peroxide is divided into a first oxidant portion, a second oxidant portion, and a third oxidant portion according to the effective molar amount of H2O2, and the molar ratio of the three portions is (15-25):(60-75):(8-18); preferably (18-22):(65-70):(10-14); more preferably 20:68:12.

[0034] First, the first oxidant is added within 20–40 min, allowing the reaction system to gradually transition from a pre-hydrated state to a tertiary amine N-oxidation state; then, the second oxidant is added within 60–120 min, and the reaction temperature is controlled at 68–74 °C.

[0035] The amount of the first oxidant is lower than that of the second oxidant, in order to avoid the formation of an excessively high instantaneous hydrogen peroxide concentration when the tertiary amine concentration is high in the early stage of the reaction.

[0036] The second oxidant component undertakes the main N-oxidation reaction of the tertiary amine. As the second oxidant component is continuously added, the dodecyl polyoxyethylene (5) tertiary amine is gradually converted into the corresponding amine oxide.

[0037] After the second oxidant is added, it is preferable to control the reaction temperature at 70-78°C and continue to maintain the temperature for 30-90 minutes to achieve a tertiary amine conversion rate of over 98.5%.

[0038] S4, Reactivation of residual amine in the high-conversion stage and deep oxidation in the third stage

[0039] Once the tertiary amine conversion rate reaches 98.5% or higher, the reaction system temperature is adjusted to 62–70°C, and a reactivation adjustment solution is added to the reaction system to adjust the pH of the reaction system to 6.2–7.0. The reactivation adjustment solution preferably contains citric acid and gluconic acid; the mass ratio of citric acid to gluconic acid is 1:(0.5–2.0), preferably 1:(0.8–1.2), and more preferably 1:1.

[0040] The amount of reactivation conditioning liquid added is preferably 0.02 to 0.15% of the mass of dodecyl polyoxyethylene (5) tertiary amine, more preferably 0.05 to 0.12%; after adding the reactivation conditioning liquid, the third oxidant portion is added to the reaction system at 20 to 50% of the average feeding rate of the second oxidant portion, preferably 30 to 40%, more preferably 35%.

[0041] After the third oxidant is added, continue to keep warm at 62-70℃ for 30-90 min.

[0042] As the conversion rate of tertiary amine gradually approaches complete conversion, the concentration of unreacted tertiary amine in the system decreases significantly. Continuing to maintain the hydrogen peroxide supply rate during the main oxidation stage at this point can easily lead to an excessively high instantaneous effective concentration of hydrogen peroxide relative to the residual tertiary amine. By adjusting the pH and catalytic coordination state at the end of the reaction using a reactivation conditioning solution and reducing the addition rate of the third oxidant, the supply rate of the oxidant is better matched to the consumption rate of the low-concentration residual tertiary amine.

[0043] Therefore, this step can further reduce the residue of free tertiary amines without excessively increasing the total excess coefficient of hydrogen peroxide.

[0044] S5, Enzymatic decomposition of residual hydrogen peroxide

[0045] After completing the third stage of deep oxidation, the reaction solution is cooled to 38–48°C, preferably 40–45°C; catalase is added, with the amount of catalase added being 20–200 U / g of reaction solution, preferably 50–120 U / g of reaction solution, based on enzyme activity; the mixture is stirred at 38–48°C for 20–60 min to reduce the residual hydrogen peroxide content to below 0.05% by mass; as the optimal point, the amount of catalase used is 80 U / g of reaction solution, the treatment temperature is 43°C, and the treatment time is 40 min.

[0046] Catalase can catalyze the decomposition of hydrogen peroxide into water and oxygen. Therefore, compared with chemical reduction treatments such as sodium bisulfite and sodium sulfite, it is not necessary to consume peroxides by adding reducing inorganic salts, thereby reducing the impact of post-treatment processes on the ionic composition of the product.

[0047] This treatment is particularly advantageous for the high hard water resistance applications required by this invention. This is because introducing additional inorganic ions during the post-treatment stage alters the product's Ca content. 2+ Mg 2+ The presence of an ionic environment may affect the transparency and viscosity stability of the compound when combined with anionic surfactants.

[0048] S6, porous adsorption purification

[0049] After catalase treatment, 0.05–0.30% (by mass) of porous adsorbent material is added to the reaction solution, and the mixture is stirred at 35–50°C for 15–45 min. The porous adsorbent material can be selected from one or more of activated carbon, diatomaceous earth, and cross-linked porous adsorbent resin. Activated carbon is preferred, or a combination of activated carbon and diatomaceous earth is used. More preferably, the amount of porous adsorbent material added is 0.08–0.20% (by mass).

[0050] After processing, the reaction solution is sequentially passed through a pre-filtration unit with a pore size of 10–20 μm and a precision filtration unit with a pore size of 1–10 μm. This step removes trace insoluble components, catalyst residues, trace particles generated after enzyme treatment, and substances that may affect the color and odor of the product.

[0051] S7, Product Adjustment

[0052] After filtration, the pH of the resulting filtrate is adjusted to 6.8–7.8, preferably 7.0–7.5, and deionized water is added according to the active ingredient content of the target product; preferably, the free tertiary amine content in the obtained dodecyl polyoxyethylene (5) amine oxide product is not higher than 0.10% by mass, more preferably not higher than 0.08% by mass, more preferably not higher than 0.06% by mass, preferably the residual hydrogen peroxide content is not higher than 0.05% by mass, more preferably not higher than 0.03% by mass; preferably the APHA color is not higher than 50, more preferably not higher than 30.

[0053] Compared with conventional direct oxidation processes, this invention achieves a higher conversion rate of polyether tertiary amines at a lower hydrogen peroxide excess coefficient through a combination of pre-hydration, three-component site-specific catalysis, segmented gradient oxidation, and terminal reactivation deep oxidation. The free tertiary amine content of the resulting product can be controlled below 0.10% by mass, preferably not exceeding 0.06% by mass, and the residual hydrogen peroxide content can be controlled below 0.05% by mass. Furthermore, no sulfite reducing agent needs to be added during post-treatment.

[0054] Furthermore, the hydration characteristics of the polyoxyethylene segments and the low content of residual tertiary amines, inorganic salts, and byproducts are beneficial for the product in the Ca content range. 2+ Mg 2+ The transparency, foam retention, and thickening stability of the medium make the resulting product suitable for washing and personal care formulations under high hardness water conditions. Detailed Implementation

[0055] The following further explains the relationship between the raw materials, process conditions, parameter ranges, and various technical features involved in this invention. It should be understood that the following content is a further explanation of the technical solution of this invention, and not a limitation on the scope of protection of this invention. Without departing from the technical concept of this invention, those skilled in the art can adjust the specific feed amount accordingly based on the production scale, the content of active ingredients in the raw materials, and the concentration of the target product.

[0056] Dodecyl polyoxyethylene (5) tertiary amine

[0057] The dodecyl polyoxyethylene (5) tertiary amine described in this invention refers to a tertiary amine compound containing a dodecyl hydrophobic chain, an average of about 5 oxyethylene structural units, and a structure that can be formed by hydrogen peroxide to form an amine oxide structure.

[0058] The term "polyoxyethylene (5)" does not require that each molecule strictly contains 5 oxyethylene structural units, but rather refers to the fact that the average EO addition number of the raw material is in a distribution range centered on 5; the present invention preferably has an average EO addition number of 4.5 to 5.5, more preferably 4.8 to 5.2, and most preferably about 5.0.

[0059] When the EO addition number is too low, the hydrophilic chain length of the resulting amine oxide is insufficient, which can lead to problems at low temperatures or higher Ca2+ levels. 2+ Mg 2+ Under certain concentration conditions, its hydration capacity decreases; while an excessively high EO addition number can further improve hydrophilicity, it reduces the proportion of hydrophobic chains and amine oxide functional groups per unit mass of product, affecting the thickening and interfacial adsorption properties of the compound. Therefore, this invention selects an average EO addition number of 4.5–5.5 as the preferred structural range.

[0060] The raw material, dodecyl polyoxyethylene (5) tertiary amine, preferably has a low initial color and low content of metal impurities to reduce the possibility of non-selective decomposition of hydrogen peroxide by trace metals during subsequent oxidation.

[0061] Prehydrated tertiary amine solution

[0062] The "pre-hydrated tertiary amine solution" referred to in this invention is a liquid obtained by pre-contacting dodecyl polyoxyethylene (5) tertiary amine with water under specified water content, temperature, and pH conditions before adding the main oxidant. Preferably, 100 parts by weight of dodecyl polyoxyethylene (5) tertiary amine are mixed with 45-80 parts by weight of deionized water and treated at 50-55°C for 30-45 minutes.

[0063] For example, 100 parts by weight of tertiary amine can be mixed with 45 parts by weight, 50 parts by weight, 55 parts by weight, 60 parts by weight, 65 parts by weight, 70 parts by weight, or 80 parts by weight of deionized water. As the most preferred method of the present invention, 50 parts by weight of deionized water are first added to every 100 parts by weight of dodecyl polyoxyethylene (5) tertiary amine, and the mixture is stirred at 53°C at a speed that allows the system to flow uniformly without producing obvious air entrapment for 40 min. Then, the pH is adjusted to about 7.3 with a citric acid aqueous solution and the treatment is continued for 20 min.

[0064] This step differs from directly adding all process water, tertiary amine, and catalyst to the reactor simultaneously. In this invention, the polyether tertiary amine first completes its independent hydration equilibrium before contacting the catalytic components, resulting in a more stable initial state for the subsequent catalytic oxidation process.

[0065] Coordination catalyst

[0066] The present invention preferably uses sodium tungstate, phosphoric acid and gluconic acid as three partitioning catalyst components.

[0067] Based on 1 part sodium tungstate, the amount of phosphoric acid can be 0.20 parts, 0.30 parts, 0.40 parts, 0.50 parts, 0.60 parts or 0.80 parts; the amount of gluconic acid can be 0.10 parts, 0.20 parts, 0.27 parts, 0.30 parts, 0.40 parts or 0.60 parts.

[0068] The most preferred mass ratio is: sodium tungstate: phosphoric acid: gluconic acid = 1:0.40:0.27. During preparation, it is not preferred to add the three components directly to the tertiary amine reaction solution, but rather to add an appropriate amount of deionized water first and premix at 40-55℃ for 10-30 min.

[0069] In one specific method, 0.45 parts by weight of sodium tungstate, 0.18 parts by weight of 85% phosphoric acid, and 0.12 parts by weight of gluconic acid are added to 15 parts by weight of deionized water, stirred at 48°C for 20 min, and then the pre-hydrated tertiary amine solution is added.

[0070] Hydrogen peroxide added in stages

[0071] The present invention preferably uses an aqueous solution of hydrogen peroxide with a mass concentration of 30-50%, and more preferably a 50% (w / w) aqueous solution of hydrogen peroxide.

[0072] The ratio of the total effective molar amount of hydrogen peroxide to the molar amount of tertiary amine groups is preferably 1.01 to 1.08:1; for example, it can be 1.01:1, 1.02:1, 1.03:1, 1.04:1, 1.045:1, 1.05:1, 1.06:1 or 1.08:1; the most preferred ratio is 1.045:1.

[0073] This invention does not preferentially use a large hydrogen peroxide excess coefficient to obtain low free amine, but instead utilizes segmented supply and end reactivation to improve the effective utilization rate.

[0074] Preferably, the effective hydrogen peroxide is divided into three parts in a ratio of 20:68:12; the first part is added within about 30 minutes to allow the system to smoothly enter the oxidation reaction state; the second part is added within about 90 minutes, which is the main oxidation stage; after the second part is added, the temperature is maintained at about 74°C for about 60 minutes to make the tertiary amine conversion rate reach more than 98.5%; then the final deep oxidation step of the present invention is carried out.

[0075] Terminal residual amine reactivation treatment

[0076] After the main oxidation is complete, it is preferable to first detect the free tertiary amine or calculate the tertiary amine conversion rate. When the tertiary amine conversion rate reaches 98.5%–99.5%, the temperature is adjusted to 62–70°C, preferably 65–68°C; a reactivation conditioning solution is prepared using citric acid and gluconic acid; preferably, the mass ratio of the two is 1:1, and it is prepared as a 10–30% by mass aqueous solution, preferably a 20% by mass aqueous solution; based on 100 parts by mass of initial tertiary amine, the reactivation conditioning solution is preferably added at 0.05–0.15 parts by mass; after addition, the pH of the reaction system is adjusted to 6.2–7.0, most preferably about 6.6. Then, the third part of hydrogen peroxide is added.

[0077] In particular, the hydrogen peroxide in the third part of the present invention is not added at the rate of the main oxidation stage, but the average feeding rate is reduced to 20 to 50% of the average feeding rate of the second part; for example, it can be 20%, 25%, 30%, 35%, 40%, 45% or 50%, and most preferably 35%.

[0078] By using the above method, the local accumulation of hydrogen peroxide can be reduced when only a small amount of tertiary amine remains in the reaction system, so that the oxidant supply rate matches the reaction rate of the residual tertiary amine.

[0079] Catalase post-treatment

[0080] After oxidation is complete, reducing inorganic salts are not added immediately; instead, the temperature is lowered first. When the temperature drops to 38–48°C, catalase is added. The preferred treatment temperature is 42–45°C, and the most preferred temperature is 43°C. The amount of catalase used can be 20 U / g, 40 U / g, 50 U / g, 60 U / g, 80 U / g, 100 U / g, 120 U / g, 150 U / g, or 200 U / g of the reaction solution, with 80 U / g of the reaction solution being the most preferred. After treatment at 43°C for about 40 min, the residual amount of H2O2 is preferably reduced to below 0.05% by mass, and more preferably below 0.03% by mass.

[0081] Since this process mainly generates water and oxygen without introducing additional inorganic anions such as sulfite, it is particularly suitable for the low-salt, high-hardness water adaptability products required by this invention.

[0082] Adsorption and precision filtration

[0083] After enzyme treatment, 0.05–0.30% by mass of porous adsorbent material can be added.

[0084] In personal care products requiring low color intensity, it is preferable to add 0.08–0.15% by mass of powdered activated carbon and adsorb at 40–45°C for 20–40 min; as the optimal point, add 0.12% by mass of powdered activated carbon and stir at 42°C for 30 min. In another embodiment, a combination of activated carbon and diatomaceous earth can be used, where activated carbon is mainly used to adsorb trace colored substances and organic impurities, and diatomaceous earth is used to improve solid-liquid separation performance. After adsorption, it is preferable to use a precision filter of about 5 μm for filtration.

[0085] Final product

[0086] After the above treatment, the pH of the filtrate is adjusted to 6.8–7.8, preferably 7.0–7.5; depending on different usage requirements, the active ingredient content can be adjusted to 25–50% by mass. When used as a raw material for shampoos, bath products, and high-grade detergents, it is preferably adjusted to 30–35% by mass; when used as a high-concentration industrial raw material, it can be adjusted to 40–50% by mass.

[0087] The dodecyl polyoxyethylene (5) amine oxide prepared under the preferred conditions of this invention has the following free tertiary amine content: preferably ≤0.08% by mass, more preferably ≤0.06% by mass; residual H2O2: preferably ≤0.05% by mass, more preferably ≤0.03% by mass; APHA: preferably ≤50, more preferably ≤30. The particularly preferred product, after being prepared into a 5% by mass solution in artificial hard water with a concentration of 600 mg / L (calculated as CaCO3) and allowed to stand at 25°C for 24 h, still maintains high light transmittance and can maintain good foam stability and thickening properties when compounded with AES and CAPB.

[0088] IX. Optimal Specific Preparation Scheme

[0089] As a particularly preferred embodiment of the present invention, 250.00 g of dodecyl polyoxyethylene (5) tertiary amine was weighed, wherein the average EO addition number of the tertiary amine was 5.0; 125.00 g of deionized water was added, and the mixture was stirred at 53°C and 350 r / min for 40 min. The pH was adjusted to 7.3 with 10% citric acid aqueous solution, and the mixture was stirred for another 20 min to obtain a prehydrated tertiary amine solution.

[0090] Separately weigh 0.45 g of sodium tungstate, 0.18 g of 85% phosphoric acid and 0.12 g of gluconic acid, add 15.00 g of deionized water, and stir at 48℃ for 20 min to obtain a coordination catalyst solution; add the coordination catalyst solution to the prehydrated tertiary amine solution, stir evenly and heat to 69℃.

[0091] The total amount of 50% (w / w) hydrogen peroxide aqueous solution was determined according to the molar ratio of tertiary amine group:H2O2 = 1:1.045, and divided into first, second, and third oxidant portions according to the effective H2O2 molar ratio of 20:68:12. The first oxidant portion was added uniformly over 30 min, followed by the second oxidant portion over 90 min, with the reaction temperature controlled at 69–72 °C. After the second oxidant portion was added, the reaction solution was heated to 74 °C and held for 60 min; the conversion rate of the tertiary amine was measured; when the conversion rate of the tertiary amine reached approximately 98.9%, the reaction solution was cooled to 66 °C; 0.30 g of reactivation adjustment solution was added. The reactivation adjustment solution was a 20% (w / w) aqueous solution of citric acid and gluconic acid prepared in a 1:1 (w / w) mass ratio, adjusting the pH of the reaction solution to approximately 6.6, and then the third oxidant portion was added at an average feeding rate of 35% of the second oxidant portion.

[0092] After the third oxidant portion is completely added, continue to maintain the temperature at 67°C for 60 minutes.

[0093] After the reaction was completed, the reaction solution was cooled to 43°C, and catalase was added to make the amount of catalase 80 U / g of the reaction solution according to the enzyme activity. The mixture was stirred at 43°C for 40 min. Then, 0.12% of powdered activated carbon by mass of the reaction solution was added, and the mixture was adsorbed at 42°C for 30 min. Finally, the mixture was filtered through a 5 μm precision filter.

[0094] Finally, the pH of the filtrate was adjusted to 7.3 using sodium citrate aqueous solution, and the active ingredient content of the product was adjusted using deionized water to obtain dodecyl polyoxyethylene (5) amine oxide with low residual amine and high hard water resistance.

[0095] The following examples are provided to further illustrate the present invention, but do not constitute a limitation on the scope of protection. Unless otherwise stated, all percentages are mass percentages. The conversion rate of tertiary amines was calculated by acid-base titration combined with the free amine content; the H2O2 residue was determined by iodometric titration; the color was determined by platinum-cobalt colorimetry; and the hard water was prepared using CaCl2 and MgCl2.

[0096] Example 1

[0097] Weigh 250.00 g of dodecyl polyoxyethylene (5) tertiary amine, with an average EO addition number of 5.0. Add 125.00 g of deionized water and stir at 53℃ and 350 r / min for 40 min; add 10% citric acid aqueous solution to adjust the pH to 7.3 and continue stirring for 20 min to obtain the prehydrated tertiary amine solution.

[0098] Separately, 0.45 g of sodium tungstate, 0.18 g of 85% phosphoric acid, and 0.12 g of gluconic acid were added to 15.00 g of deionized water and stirred at 48 °C for 20 min to obtain a coordination catalyst solution; wherein the mass ratio of sodium tungstate, phosphoric acid, and gluconic acid was 1:0.40:0.27. The coordination catalyst solution was added to the prehydrated tertiary amine solution and heated to 69 °C.

[0099] A 50% (w / w) hydrogen peroxide solution was measured with a molar ratio of tertiary amine groups to H₂O₂ of 1:1.045. The hydrogen peroxide was divided into three portions with an effective H₂O₂ molar ratio of 20:68:12. The first portion was added over 30 min; subsequently, the second portion was added uniformly over 90 min, controlling the reaction temperature at 69–72 °C. After the second portion was added, the temperature was raised to 74 °C and maintained for 60 min.

[0100] After the conversion rate of the tertiary amine reached 98.9%, the reaction solution was cooled to 66°C. 0.30 g of reactivation conditioning solution was added; this conditioning solution was prepared as a 20% by mass aqueous solution of citric acid and gluconic acid in a 1:1 mass ratio, adjusting the pH of the system to 6.6. Hydrogen peroxide (the third part) was added at approximately 35% of the average addition rate of the second part, and the mixture was kept at 67°C for 60 min after the addition was complete.

[0101] After the reaction was complete, the temperature was lowered to 43°C, and catalase was added to achieve an enzyme activity of 80 U / g of the reaction solution. The mixture was stirred for 40 min. 0.12% (w / w) of powdered activated carbon was added, and adsorption was performed at 42°C for 30 min. The mixture was then filtered through a 5 μm filter. The pH was adjusted to 7.3 using a 10% (w / w) sodium citrate aqueous solution, and deionized water was added to bring the active ingredient content of the product to approximately 31%. The resulting product is referred to as Example 1.

[0102] Example 2

[0103] Except for the following conditions, it was prepared according to Example 1: 275.00 g of tertiary amine; pre-hydration temperature 50°C, time 30 min; sodium tungstate / phosphate / sorbitol mass ratio 1:0.30:0.35; molar ratio of H2O2 to tertiary amine groups 1.06:1; three-stage H2O2 molar ratio 18:70:12; final reactivation pH 6.8; third-stage feeding rate 40% of the average rate of the second stage; catalase dosage 100 U / g. The final active ingredient content was adjusted to approximately 40%.

[0104] Example 3

[0105] Except for the following conditions, it was prepared according to Example 1: the average EO addition number was 5.2; the prehydration temperature was 56°C and the time was 35 min; the mass ratio of sodium tungstate / sodium dihydrogen phosphate / sodium gluconate was 1:0.55:0.30; the molar ratio of H2O2 to tertiary amine groups was 1.03:1; the molar ratio of H2O2 in the three stages was 22:65:13; the final reactivation pH was 6.5; the feeding rate of the third stage was 30% of the average rate of the second stage; and adsorption filtration was performed using 0.08% by mass activated carbon and 0.08% by mass diatomaceous earth.

[0106] Comparative Example 1

[0107] The pre-hydration, coordination catalytic pre-activation, staged addition, and end-stage reactivation steps were omitted. 250.00 g of tertiary amine was mixed with water and heated to 70°C. 5% excess of 50% by mass hydrogen peroxide (theoretical amount) was added continuously over 2 hours, and the mixture was kept at 75°C for 4 hours. After the reaction was completed, the temperature was lowered directly without using catalase; only the pH was adjusted and the mixture was filtered.

[0108] Comparative Example 2

[0109] Except for the elimination of the prehydration process in step S1 and the direct mixing of the tertiary amine and all process water before entering the catalytic oxidation step, the other conditions are the same as in Example 1.

[0110] Comparative Example 3

[0111] Except for the coordination catalyst, which uses only sodium tungstate and phosphoric acid and omits gluconic acid, and the amounts of sodium tungstate and phosphoric acid are the same as in Example 1, the other conditions are the same as in Example 1.

[0112] Comparative Example 4

[0113] Except for the use of sodium tungstate and gluconic acid as catalysts and the absence of phosphoric acid, the other conditions were the same as in Example 1.

[0114] Comparative Example 5

[0115] The catalyst and prehydration conditions were the same as in Example 1, but all hydrogen peroxide was added continuously at a constant rate over 120 min, followed by holding at 74°C for 120 min, without setting a third stage of low-flux deep oxidation.

[0116] Comparative Example 6

[0117] The ratio of hydrogen peroxide in the three stages is the same as in Example 1, but after the second stage of oxidation is completed, no reactivation conditioning solution is added, and the third part of hydrogen peroxide is added directly.

[0118] Comparative Example 7

[0119] Except that the average feeding rate of hydrogen peroxide in the third part was adjusted to 100% of the average feeding rate in the second part, the other conditions were the same as in Example 1.

[0120] Comparative Example 8

[0121] The catalyst of Example 1 was used, but the molar ratio of H2O2 to tertiary amine groups was increased to 1.15:1, and it was added in two stages at the same rate; after the reaction was completed, enzyme treatment was carried out as in Example 1.

[0122] Comparative Example 9

[0123] The oxidation phase was the same as in Example 1, but catalase was not used after the reaction was completed. Instead, sodium bisulfite aqueous solution was used to treat the reaction until H2O2 was below 0.05%, followed by filtration and pH adjustment.

[0124] Comparative Example 10

[0125] The EO=5 raw material in Example 1 was replaced with a dodecyl polyoxyethylene ether tertiary amine with an average EO addition number of about 3.0, and the remaining steps were the same as in Example 1, in order to investigate the effect of polyether chain length on performance in low temperature and hard water applications.

[0126] Performance testing methods

[0127] 1. Free tertiary amine: Weigh a certain mass of sample, dissolve it in a mixed solvent of isopropanol / water, and perform potentiometric titration using a standard acid solution. The result is expressed as the mass fraction of free tertiary amine.

[0128] 2. H2O2 residue: Iodometric method was used, in which potassium iodide reacts with residual H2O2 under acidic conditions to release iodine, and then titrated with standard sodium thiosulfate solution.

[0129] 3. Color: APHA value was determined according to the platinum-cobalt colorimetric method.

[0130] 4. Low temperature stability: The transparency, turbidity and precipitation of the sample were observed after standing at 5±1℃ for 24 h and 72 h and before returning to room temperature.

[0131] 5. Hard water transparency stability: Prepare a 5% (w / w) aqueous solution of the sample, and prepare it with 300 mg / L and 600 mg / L hard water (calculated as CaCO3), respectively. Place it at 25℃ for 24 h, measure the transmittance at 600 nm and observe the precipitation.

[0132] 6. Hard water foam retention rate: 0.5% by mass of sample solution was prepared with deionized water and 600 mg / L hard water respectively. The initial foam height and 5-minute foam height were determined by the Ross-Miles method. The retention rate was calculated as 5-minute foam height of hard water / 5-minute foam height of deionized water × 100%.

[0133] 7. Thickening retention rate of compound formulation: The compound surfactant was prepared by mixing this product with AES and CAPB at an active ingredient mass ratio of 1:4:2. The amount of NaCl added was fixed at 1.5% by mass. The formulation was prepared with deionized water and 600 mg / L hard water, respectively. After equilibration at 25℃ for 24 h, the viscosity was measured. The thickening retention rate was calculated as hard water viscosity / deionized water viscosity × 100%.

[0134] 8. Storage stability: After being stored at 45℃ for 30 days, the changes in free tertiary amine, H2O2, APHA and appearance before and after storage were measured.

[0135] Table 1 Performance Results

[0136]

[0137] The results above show that Examples 1-3 maintained superior levels in terms of free amine, residual H2O2, color, hard water transmittance, foam retention, and thickening retention. In particular, Example 1, compared to the single-factor missing schemes of Comparative Examples 2-7, demonstrates that pre-hydration, tri-component site catalysis, segmented supply, and end-of-pipe reactivation are not independent conventional optimizations: omitting any of these key steps resulted in increased residual amine or peroxides and reduced application performance under hard water conditions to varying degrees. Comparative Example 8 shows that simply increasing H2O2 cannot equivalently replace end-of-pipe microenvironment control; Comparative Example 9 shows that although sulfite can reduce H2O2, the increased ionic load is detrimental to transparency and thickening performance in high-hardness water; Comparative Example 10 illustrates a correlation between the EO chain length window and low-temperature / hard water performance.

[0138] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them; although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features; and these modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for preparing a dodecyl polyoxyethylene (5) amine oxide with low residual amine content and high hard water resistance, characterized in that, include: The dodecyl polyoxyethylene (5) tertiary amine was pre-hydrated with water at 45–60 °C. Tungstate, phosphoric acid-containing components, and polyhydroxy coordination components were pre-activated at a mass ratio of 1:(0.20-0.80):(0.10-0.60) to form a coordination catalyst solution. The coordination catalyst solution was added to a pre-hydrated tertiary amine solution, and hydrogen peroxide was added sequentially in three oxidant portions according to a molar ratio of (15-25):(60-75):(8-18). After the second oxidant portion reacted, when the tertiary amine conversion rate reached 98.5% or higher, the system was adjusted to 62-70°C and pH 6.2-7.0, a reactivation adjustment solution was added, and the third oxidant portion was added at a rate of 20-50% of the average feeding rate of the second oxidant portion for terminal deep oxidation. After the reaction was completed, residual hydrogen peroxide was decomposed by catalase at 38-48°C, and the solution was treated and filtered by porous adsorption material to obtain the dodecyl polyoxyethylene (5) amine oxide. The average EO addition number of the dodecyl polyoxyethylene (5) tertiary amine is 4.5 to 5.5; The mass fraction of tertiary amine in the prehydration treatment was 55-75%, and the prehydration time was 20-60 min.

2. The preparation method according to claim 1, characterized in that, The tungstate is sodium tungstate; the phosphoric acid component is phosphoric acid and / or dihydrogen phosphate; the polyhydroxy coordination component is at least one of gluconic acid, gluconate, sorbitol and glycerol.

3. The preparation method according to claim 1, characterized in that, Based on 1 mol of tertiary amine groups, the total amount of hydrogen peroxide added is 1.01–1.08 mol.

4. The preparation method according to claim 1, characterized in that, The first oxidant portion is added within 20–40 min, and the second oxidant portion is added within 60–120 min.

5. The preparation method according to claim 1, characterized in that, The reactivation conditioning solution contains citric acid and gluconic acid in a mass ratio of 1:(0.5-2.0).

6. The preparation method according to claim 1, characterized in that, After the third oxidant is added, keep it at 62-70℃ for 30-90 min.

7. The preparation method according to claim 1, characterized in that, The amount of catalase used is 20-200 U / g of reaction solution.

8. The preparation method according to claim 1, characterized in that, The porous adsorbent is selected from one or more of activated carbon, diatomaceous earth and cross-linked porous adsorbent resin, and its addition amount is 0.05 to 0.30% of the mass of the reaction solution.

9. A dodecyl polyoxyethylene (5) oxide amine, characterized in that, The amine oxide is prepared by the method described in any one of claims 1 to 8, wherein the content of free tertiary amine in the amine oxide is not higher than 0.10% by mass, and the residual hydrogen peroxide is not higher than 0.05% by mass.

10. The use of the dodecyl polyoxyethylene (5) amine oxide of claim 9 in detergents, shampoos, bath products or industrial cleaning agents.