A high-temperature resistant thermal insulation coating composed of aerogel and PBI and its preparation method
By combining modified silica aerogel with polybenzimidazole resin and using a gradient curing process, the problems of poor thermal insulation of pure PBI coating and easy peeling of aerogel coating were solved, and a high-strength, high-thermal-insulation, and high-temperature-resistant composite coating was prepared, which is suitable for high-temperature industrial protection.
Patent Information
- Application Number
- CN202611540861.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-30
- Publication Date
- 2026-11-17
AI Technical Summary
Existing pure PBI coatings have poor thermal insulation and insufficient ablation resistance, pure aerogel coatings have poor mechanical properties and are prone to peeling off, and conventional compound coatings have poor compatibility and unstable performance, which cannot meet the high-temperature industrial protection requirements.
By combining modified silica aerogel with high molecular weight polybenzimidazole resin and employing precise formulation and gradient curing process, a nanoporous thermal insulation network is constructed to improve the coating's high temperature resistance, thermal insulation, adhesion, and stability.
It achieves high strength, high heat insulation, high temperature resistance, and ablation resistance coating performance, suitable for high temperature environments of 600~1100℃, with low thermal conductivity, strong adhesion, extended service life, and suitable for a variety of substrates.
Smart Images

Figure FT_1 
Figure FT_2 
Figure FT_3
Abstract
Description
Technical Field
[0001] This invention relates to the fields of high-temperature protective coating materials and polymer composite thermal insulation materials, specifically to a high-temperature resistant thermal insulation coating composed of aerogel and PBI and its preparation method. Background Technology
[0002] Polybenzimidazole (PBI) is an ultra-high performance, high-temperature resistant polymer material with extremely high thermal stability, excellent mechanical strength, radiation resistance, and chemical corrosion resistance. Its thermal decomposition temperature exceeds 550℃, making it one of the core matrix materials for high-end high-temperature coatings. Pure PBI coatings exhibit good film-forming properties, strong adhesion, are not easily peeled off, and possess excellent mechanical properties, making them widely used in high-end high-temperature protection applications. However, existing pure PBI coatings have obvious technical defects: the PBI matrix structure is dense and lacks a porous thermal insulation structure. At high temperatures, the heat conduction rate is fast, and the thermal insulation performance is extremely poor, which cannot meet the thermal insulation and cooling requirements of medium and high temperature scenarios. At the same time, under long-term high-temperature service environment, pure PBI coatings are prone to thermal stress concentration, generating micro cracks, with limited ablation resistance and insufficient long-term high-temperature protection capability. Silica aerogel is currently known as the solid material with the best thermal insulation performance. It has the characteristics of nanoporous network structure, high porosity, extremely low thermal conductivity, and high temperature resistance, making it an ideal high-temperature thermal insulation filler. Pure aerogel coatings have excellent thermal insulation effects, but they have fatal shortcomings: extremely poor film-forming properties, low mechanical strength, loose texture, and weak adhesion to the substrate. After construction, it is very prone to powdering, peeling, flaking, and cracking, making it unsuitable for long-term use as a protective coating and having very low industrial practicality. Currently, some studies have attempted to prepare high-temperature coatings by simply compounding aerogels with polymer resins, but these methods generally suffer from several technical drawbacks: First, the aerogels are not modified, resulting in poor compatibility with the PBI resin matrix, easy aggregation and sedimentation, uneven internal structure of the coating, and defects such as pores and pinholes, significantly reducing high-temperature resistance and thermal insulation performance. Second, the formulation ratios are crude, lacking precise component control, making it impossible to balance the mechanical and thermal insulation properties of the coating. Third, the curing process is simplistic; one-time high-temperature curing easily leads to uneven shrinkage inside and outside the coating, causing cracks and decreased adhesion. In summary, existing technologies lack a PBI / aerogel composite high-temperature coating that combines high-strength adhesion, high temperature resistance, excellent thermal insulation, ablation resistance, and resistance to cracking and peeling, becoming a technical bottleneck for industrial application in this field. Therefore, this invention develops an aerogel-PBI composite high-temperature resistant and thermally insulating coating and its precise preparation process, addressing the core pain points of existing technologies. Summary of the Invention
[0003] Purpose of the invention The purpose of this invention is to overcome the shortcomings of existing technologies, such as poor thermal insulation and insufficient ablation resistance of pure PBI coatings, poor mechanical properties and easy peeling of pure aerogel coatings, and poor compatibility and unstable performance of conventional composite coatings. This invention provides a high-temperature resistant thermal insulation coating composed of aerogel and PBI and its preparation method. Through material modification, precise formulation and gradient curing process, the coating achieves an integrated breakthrough in high temperature resistance, high thermal insulation, high strength and high stability, making it suitable for various high-temperature industrial protection scenarios.
[0004] Technical solution To achieve the above objectives, the present invention adopts the following technical solution: The present invention provides an aerogel and PBI composite high-temperature resistant heat insulation coating, which, by mass parts, comprises the following raw material components: 25-40 parts of polybenzimidazole resin, 15-30 parts of modified silica aerogel, 3-8 parts of high-temperature resistant crosslinking agent, 8-15 parts of inorganic high-temperature resistant filler, 1-3 parts of dispersant, 0.5-2 parts of leveling agent, 0.3-1 part of defoamer, and 30-50 parts of polar organic solvent. Furthermore, the modified silica aerogel is a silane coupling agent surface-modified hydrophobic silica aerogel with a particle size of 20-80 nm, a porosity of ≥90%, a specific surface area of 800-1200 m² / g, and a hydrophobic angle of ≥135°, which solves the problems of hydrophilicity, aggregation, and poor compatibility with the matrix of the original aerogel. Furthermore, the polybenzimidazole resin is a high molecular weight linear polybenzimidazole with a weight average molecular weight of 30,000 to 50,000, a thermal decomposition temperature of ≥550℃, and a solid content of ≥98%, ensuring film strength and high-temperature stability. Furthermore, the high-temperature resistant crosslinking agent is a melamine-formaldehyde crosslinking agent or an organoboron crosslinking agent; the inorganic high-temperature resistant filler is one or more of nano-alumina, nano-zirconia, and talc, with a particle size of 50–200 nm. The polar organic solvent is one or more of N,N-dimethylformamide, N-methylpyrrolidone, and dimethyl sulfoxide. The present invention also provides a method for preparing the above-mentioned composite coating, comprising the following steps: (1) Aerogel modification pretreatment: The original silica aerogel was placed in a vacuum drying oven and dried at 120-150℃ for 2-4 hours to remove adsorbed moisture and impurities; then the dried aerogel was dispersed in anhydrous ethanol, a silane coupling agent was added, ultrasonically dispersed for 30-60 minutes, and stirred at a constant temperature for 2-3 hours. After filtration, washing, and vacuum drying, modified silica aerogel was obtained for later use. (2) Matrix preparation: Add polybenzimidazole resin to a polar organic solvent, stir at room temperature for 20-40 min, heat to 60-80℃ and stir for 1-2 h until the resin is completely dissolved to form a uniform and transparent PBI resin base liquid. (3) Coating compounding: Add dispersant, defoamer and leveling agent to PBI resin base liquid in sequence, stir at low speed for 10-20 min; then add modified silica aerogel and inorganic high temperature resistant filler, disperse at high speed for 30-50 min, finally add high temperature resistant crosslinking agent, stir at low speed until uniform, filter to remove impurities, and obtain composite high temperature resistant coating. (4) Substrate pretreatment: The substrate to be coated is sandblasted to remove rust, oil and dust, and the surface cleanliness of the substrate is Sa2.5 or above. It is then dried for later use. (5) Spraying and curing: The composite coating is sprayed onto the substrate surface in layers using a high-pressure airless spraying method. The thickness of each layer is 20-40 μm, and the next layer is sprayed after 5-10 min intervals, with a total coating thickness of 80-150 μm. After spraying, the coating is allowed to stand at room temperature for 30-60 min for pre-curing, and then cured using a gradient temperature rise process: 80℃ for 1 h, 150℃ for 1 h, 220℃ for 2 h, and 300℃ for 1 h. The coating is then allowed to cool naturally to room temperature to obtain a high-temperature heat-insulating coating of aerogel and PBI composite. Preferably, in step (1), the silane coupling agent is one of KH-550 and KH-560, and the amount added is 3% to 6% of the mass of the aerogel. In step (3), the high-speed shear dispersion speed is 2500 to 3500 r / min, and the filter is a 200 to 300 mesh filter. In step (5), the spraying environment temperature is 20 to 30℃, the relative humidity is 40% to 60%, and there is no dust or convection wind.
[0005] Beneficial effects Compared with the prior art, the present invention has the following significant inventive progress and beneficial effects: 1. Collaborative material innovation and complementary performance breakthroughs. This invention is the first to precisely composite a high-strength, high-temperature resistant PBI matrix with an ultra-low thermal insulation aerogel porous structure. The PBI resin provides excellent film-forming properties, adhesion, mechanical strength, and aging resistance, solving the problem of powdering and peeling of aerogel coatings. The modified aerogel is uniformly dispersed inside the matrix to construct a nanoporous thermal insulation network, significantly reducing the thermal conductivity of the coating and compensating for the thermal insulation shortcomings of pure PBI coatings, achieving a triple performance integration of high strength, high temperature resistance, and high thermal insulation. 2. Modification treatment improves compatibility and significantly enhances coating stability. Silica aerogel is hydrophobically modified with a silane coupling agent to eliminate hydrophilic groups on the aerogel surface, improving its interfacial bonding with organic PBI resin. This prevents filler agglomeration, sedimentation, and delamination, resulting in a uniform and dense internal structure of the coating, free of pores and pinholes. This significantly improves the coating's high-temperature resistance, damp-heat resistance, and aging resistance, greatly extending its service life. 3. Precise formulation and controllable performance. This invention limits the precise ratio of each component through extensive experiments, balancing the filler content and film-forming performance. This ensures sufficient aerogel insulation components while avoiding excessive filler that could lead to a decrease in the mechanical properties of the coating and film failure. Combined with high-temperature resistant inorganic fillers and crosslinking agents, the upper limit of the coating's temperature resistance, hardness, and ablation resistance are further improved. 4. Gradient curing process completely solves cracking defects. This invention abandons the traditional one-time high-temperature curing process and adopts a gradient temperature-increasing segmented curing method, which allows the solvent inside the coating to evaporate slowly and the resin to cross-link and cure gradually. The shrinkage rate inside and outside is consistent, which completely eliminates thermal stress concentration and prevents coating cracking, peeling and detachment problems, greatly improving the coating forming quality and service stability. 5. Excellent overall performance and wide applicability. The composite coating prepared by this invention can withstand high temperatures of 600-1100℃ for a long time, with a thermal conductivity of ≤0.035W / (m·K), significant heat insulation and cooling effect, and excellent adhesion (Grade 0), flexibility, impact resistance, wear resistance, ablation resistance, and resistance to high and low temperature cycle aging. Its overall performance is superior to existing similar products. 6. The process is simple and controllable, with high industrialization feasibility. The entire preparation process is characterized by mild conditions, simple operation, and controllable parameters. It requires no special high-end equipment, has good spray coating properties, and is compatible with various substrates such as metals, ceramics, and composite materials, enabling large-scale industrial production. Attached Figure Description Figure 1 This is a schematic diagram of the cross-sectional structure of the composite coating according to an embodiment of the present invention; Figure 2 This is a schematic diagram of the microstructure of the aerogel particles dispersed in the PBI resin matrix according to the present invention. Figure 3 This is a flowchart of the overall process of the preparation method of the present invention. In the figure, the markings are: 1-metal substrate; 2-primer coating; 3-topcoat coating; 4-PBI resin matrix phase; 5-modified silica aerogel particles; 6-inorganic high-temperature resistant filler particles. Detailed Implementation The present invention will be further described in detail below with reference to specific embodiments. These embodiments are for illustrative purposes only and do not constitute a limitation on the scope of protection of the present invention. Example 1 A high-temperature resistant heat insulation coating composed of aerogel and PBI, comprising the following raw materials by mass: 32 parts of polybenzimidazole resin, 22 parts of modified silica aerogel, 5 parts of organoboron crosslinking agent, 12 parts of nano-alumina filler, 2 parts of dispersant, 1 part of leveling agent, 0.5 parts of defoamer, and 38 parts of N-methylpyrrolidone solvent. Preparation method: 1. Aerogel modification: Dry the original silica aerogel at 130℃ for 3h, add anhydrous ethanol for dispersion, add 4% KH-560 coupling agent by weight of aerogel, sonicate for 40min, stir at constant temperature for 2.5h, filter and dry to obtain modified aerogel; 2. Matrix preparation: Add N-methylpyrrolidone to PBI resin, stir at room temperature for 30min, stir at 70℃ for 1.5h until completely dissolved; 3. Coating compounding: Add the additives sequentially and stir at low speed for 15min, add the modified aerogel and nano alumina, shear at 3000r / min for 40min, add the crosslinking agent and stir evenly, filter through a 250 mesh filter; 4. Substrate sandblasting and degreasing pretreatment; 5. Layered spraying, total thickness 120μm, pre-curing at room temperature for 40min, gradient curing: 80℃ for 1h, 150℃ for 1h, 220℃ for 2h, 300℃ for 1h, cool to obtain the finished coating. Example 2 A high-temperature resistant thermal insulation coating composed of aerogel and PBI, comprising the following raw materials by weight: 28 parts polybenzimidazole resin, 28 parts modified silica aerogel, 6 parts melamine-formaldehyde crosslinking agent, 10 parts nano-zirconia filler, 1.5 parts dispersant, 0.8 parts leveling agent, 0.4 parts defoamer, and 42 parts mixed solvent (DMF+NMP). The preparation method is the same as in Example 1, and the total coating thickness is 100 μm. Comparative Example 1 (Pure PBI coating) Remove the aerogel filler; the remaining raw materials and processes are the same as in Example 1. Comparative Example 2 (Unmodified Aerogel Composite Coating) The original unmodified silica aerogel was used, and the other raw materials and processes were the same as in Example 1. Performance test results: Standard performance tests were performed on the coatings of each embodiment and comparative example, and the results are as follows: 1. Temperature resistance: Examples 1 and 2 can withstand high temperatures of 900-1100℃ for a long time without cracking or peeling; the pure PBI coating of Comparative Example 1 fails to provide heat insulation above 800℃; the coating of Comparative Example 2 shows local cracking and powdering at 800℃. 2. Thermal conductivity: The thermal conductivity of Examples 1 and 2 is ≤0.035W / (m·K); the thermal conductivity of Comparative Example 1 is 0.085W / (m·K), which is extremely poor in terms of thermal insulation performance; the thermal conductivity of Comparative Example 2 is 0.052W / (m·K), which is a significant decrease in thermal insulation effect. 3. Adhesion: Examples 1 and 2 have an adhesion rating of 0; Comparative Example 2 has an adhesion rating of 2, indicating a risk of localized detachment. 4. Aging resistance: After 100 cycles of high and low temperatures, the coating of the example showed no abnormalities; the thermal insulation performance of Comparative Example 1 decreased by 35%, and the thermal insulation performance of Comparative Example 2 showed micro-cracks. The test results demonstrate that the composite coating prepared by the present invention through precise compounding of modified aerogel and PBI and a proprietary process has comprehensive performance improvements compared to existing technologies, solves long-standing technical pain points in the industry, and has significant inventiveness and practicality.
Claims
1. A high-temperature resistant thermal insulation coating composed of aerogel and PBI, characterized in that, By weight, it includes the following raw material components: 25-40 parts of polybenzimidazole resin, 15-30 parts of modified silica aerogel, 3-8 parts of high-temperature crosslinking agent, 8-15 parts of inorganic high-temperature filler, 1-3 parts of dispersant, 0.5-2 parts of leveling agent, 0.3-1 part of defoamer, and 30-50 parts of polar organic solvent.
2. The aerogel and PBI composite high-temperature heat-insulating coating according to claim 1, characterized in that, The modified silica aerogel is a hydrophobic silica aerogel modified with a surface hydroxyl silane coupling agent, with a particle size of 20-80 nm, a porosity of ≥90%, a specific surface area of 800-1200 m² / g, and a hydrophobic angle of ≥135°.
3. The aerogel and PBI composite high-temperature heat-insulating coating according to claim 1, characterized in that, The polybenzimidazole resin is a high molecular weight linear polybenzimidazole with a weight average molecular weight of 30,000 to 50,000, a thermal decomposition temperature of ≥550℃, and a solid content of ≥98%.
4. The aerogel and PBI composite high-temperature heat-insulating coating according to claim 1, characterized in that, The high-temperature resistant crosslinking agent is a melamine-formaldehyde crosslinking agent or an organoboron crosslinking agent; the inorganic high-temperature resistant filler is one or more of nano-alumina, nano-zirconia, and talc powder, with a particle size of 50-200 nm.
5. The aerogel and PBI composite high-temperature heat-insulating coating according to claim 1, characterized in that, The polar organic solvent is one or more mixed solvents selected from N,N-dimethylformamide, N-methylpyrrolidone, and dimethyl sulfoxide.
6. A method for preparing a high-temperature resistant heat-insulating coating composed of aerogel and PBI as described in any one of claims 1 to 5, characterized in that, Includes the following steps: (1) Aerogel modification pretreatment: The original silica aerogel was placed in a vacuum drying oven and dried at 120-150℃ for 2-4 hours to remove adsorbed moisture and impurities; then the dried aerogel was dispersed in anhydrous ethanol, a silane coupling agent was added, ultrasonically dispersed for 30-60 minutes, and stirred at a constant temperature for 2-3 hours. After filtration, washing, and vacuum drying, modified silica aerogel was obtained for later use. (2) Matrix preparation: Add polybenzimidazole resin to a polar organic solvent, stir at room temperature for 20-40 min, heat to 60-80℃ and stir for 1-2 h until the resin is completely dissolved to form a uniform and transparent PBI resin base liquid. (3) Coating compounding: Add dispersant, defoamer and leveling agent to PBI resin base liquid in sequence, stir at low speed for 10-20 min; then add modified silica aerogel and inorganic high temperature resistant filler, disperse at high speed for 30-50 min, finally add high temperature resistant crosslinking agent, stir at low speed until uniform, filter to remove impurities, and obtain composite high temperature resistant coating. (4) Substrate pretreatment: The substrate to be coated is sandblasted to remove rust, oil and dust, and the surface cleanliness of the substrate is Sa2.5 or above. It is then dried for later use. (5) Spraying and curing: The composite coating is sprayed onto the substrate surface in layers using a high-pressure airless spraying method. The thickness of each layer is 20-40 μm, and the next layer is sprayed after 5-10 minutes. The total thickness of the coating is 80-150 μm. After spraying, allow to stand at room temperature for 30-60 minutes for pre-curing, then use a gradient temperature increase process for curing: keep at 80℃ for 1 hour, 150℃ for 1 hour, 220℃ for 2 hours, and 300℃ for 1 hour, and then cool naturally to room temperature to obtain a high-temperature heat-insulating coating of aerogel and PBI composite.
7. The preparation method according to claim 6, characterized in that, In step (1), the silane coupling agent is one of KH-550 and KH-560, and the amount of coupling agent added is 3% to 6% of the mass of the aerogel.
8. The preparation method according to claim 6, characterized in that, In step (3), the high-speed shear dispersion speed is 2500-3500 r / min, and the filter is a 200-300 mesh filter.
9. The preparation method according to claim 6, characterized in that, In step (5), the spraying environment temperature is 20-30℃, the relative humidity is 40%-60%, and there is no dust or convection wind.
10. The application of a high-temperature resistant heat-insulating coating composed of aerogel and PBI as described in any one of claims 1 to 5, characterized in that, The coating is applied to aerospace components, industrial high-temperature pipelines, metallurgical furnaces, power high-temperature equipment, and new energy high-temperature shells for heat insulation, high-temperature resistance, and ablation protection.