Coolant Compositions and Their Applications

By adding monoesters and additives with specific structures to the coolant, the problems of insufficient thermal conductivity and biodegradability of existing coolants are solved, achieving efficient electrical insulation and environmentally friendly cooling effects.

CN123107633APending Publication Date: 2026-11-17CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510620330.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-14
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing coolants have problems such as insufficient thermal conductivity, poor material compatibility and thermal stability in electronic devices, and do not meet environmental protection requirements.

Method used

A coolant composition is provided, comprising a base oil and additives, wherein the base oil is composed of a monoester with a structural formula as shown in Formula I, the monoester content being not less than 65 wt%, and is prepared by esterification reaction, and antioxidants and pour point depressants are added to improve performance.

Benefits of technology

While meeting electrical insulation requirements, the coolant composition exhibits good biodegradability and thermal conductivity, thus improving the overall performance of the coolant.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123107633A_ABST
    Figure CN123107633A_ABST
Patent Text Reader

Abstract

This invention relates to the field of cooling media, and discloses a coolant composition and its application. The composition comprises a base oil and additives, wherein the base oil comprises a monoester with the structural formula shown in Formula I: In Formula I, R1 is a C2-C15 straight-chain alkyl group, R2 is a C1-C10 straight-chain alkyl group, and R3 is a C5-C20 straight-chain alkyl group. The content of the monoester shown in Formula I in the coolant composition is not less than 65 wt%. The coolant composition provided by this invention has a simple composition and, while meeting its electrical insulation performance requirements, exhibits good biodegradability and good thermal conductivity. Furthermore, this invention provides a monoester that, when applied to a coolant, can effectively improve the coolant's thermal conductivity and biodegradability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of cooling media, and more specifically, to a coolant composition and its application. Background Technology

[0002] With the continuous development of digital technology, it is widely used in industries such as transportation, communications, manufacturing, medicine, and education. The rapid development of the digital economy is injecting new momentum into economic and social development through computing power. Along with the development of digital technology, the scale of data centers is growing rapidly.

[0003] With the trend towards higher density and greater power in data centers, air cooling is increasingly insufficient to meet the requirements of heat dissipation and energy saving. Researchers have proposed various new cooling technologies, such as cold plate cooling, spray cooling, and immersion liquid cooling. Among them, immersion liquid cooling systems involve completely immersing the server in coolant, with the server in direct contact with the coolant. Heat is removed through the circulation or evaporation and condensation of the coolant. Depending on whether a phase change occurs in the coolant, immersion liquid cooling is divided into single-phase immersion liquid cooling and phase-change immersion liquid cooling. Single-phase immersion liquid cooling systems are simpler to design, easier to accommodate coolant, and have greater material compatibility.

[0004] Liquid coolants used in electronic devices should be non-flammable, non-toxic, and possess excellent thermophysical characteristics, such as high thermal conductivity, specific heat, heat transfer coefficient, high insulation, and low viscosity, as well as strong material compatibility. Existing coolants mostly use non-conductive, non-corrosive liquids such as mineral oil and fluorinated liquids. However, these coolants have certain limitations. For example, while electronic fluorinated liquids have good electrical insulation properties, their thermal conductivity is insufficient, and they are harmful to the environment, failing to meet current environmental protection requirements. Some hydrocarbon coolants possess good electrical insulation and thermal conductivity, but their material compatibility and thermal stability are poor. Coolants that meet the requirements for insulation, thermal conductivity, compatibility, and thermal stability (such as polyol ester coolants) cannot be industrialized and widely used due to their high cost and difficult synthesis. Therefore, developing novel single-phase immersion coolants that meet the requirements of high thermal conductivity, good insulation properties, and biodegradability is of great significance. Summary of the Invention

[0005] The purpose of this invention is to overcome the aforementioned problems in the prior art and to provide a coolant composition and its application.

[0006] To achieve the above objectives, the present invention provides a coolant composition comprising a base oil and additives, wherein the base oil comprises a monoester with the structural formula shown in Formula I:

[0007]

[0008] In Formula I, R1 is a C2-C15 straight-chain alkyl group, R2 is a C1-C10 straight-chain alkyl group, and R3 is a C5-C20 straight-chain alkyl group. The content of the monoester shown in Formula I in the coolant composition is not less than 65 wt%.

[0009] A second aspect of the present invention provides the application of the monoesters as described above in improving the thermal conductivity and biodegradability of coolants.

[0010] Through the above technical solutions, the coolant composition provided by the present invention has a simple composition and, while satisfying its electrical insulation performance, has good biodegradability and good thermal conductivity. In addition, the present invention provides a monoester that can effectively improve the thermal conductivity and biodegradability of the coolant when applied to the coolant. Attached Figure Description

[0011] Figure 1 The infrared spectrum of undecyl 2-butylnonanoate prepared in Example 2. Detailed Implementation

[0012] The endpoints and any values ​​of the ranges disclosed herein are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of the various ranges, the endpoint values ​​of the various ranges and individual point values, and individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed herein.

[0013] A first aspect of the present invention provides a coolant composition comprising a base oil and an additive, wherein the base oil comprises a monoester having the structural formula shown in Formula I:

[0014]

[0015] In Formula I, R1 is a C2-C15 straight-chain alkyl group, R2 is a C1-C10 straight-chain alkyl group, and R3 is a C5-C20 straight-chain alkyl group. The content of the monoester shown in Formula I in the coolant composition is not less than 65 wt%.

[0016] In this invention, the presence of the monoester represented by Formula I in the coolant is beneficial for further improving the electrical insulation properties, thermal conductivity properties and biodegradability properties of the coolant. Furthermore, the inventors of this invention have found that a content of not less than 65 wt% of the monoester represented by Formula I in the coolant composition can further improve the overall performance of the coolant.

[0017] According to the present invention, preferably, R1 is a C2-C10 straight-chain alkyl group, R2 is a C5-C10 straight-chain alkyl group, and R3 is a C8-C17 straight-chain alkyl group.

[0018] More preferably, R1 is a C3-C5 straight-chain alkyl group, R2 is a C7-C9 straight-chain alkyl group, and R3 is a C10-C15 straight-chain alkyl group.

[0019] In this invention, the structure of the monoester within the above-mentioned range can further improve the overall performance of the coolant.

[0020] According to the present invention, preferably, the content of the monoester represented by Formula I in the coolant composition is not less than 75 wt% (e.g., in the range of 85-99.8 wt%), and more preferably, the content of the monoester represented by Formula I in the coolant composition is not less than 90 wt% (e.g., in the range of 90-99.5 wt%).

[0021] The inventors of this invention have discovered that when the content of monoesters in the coolant is within the above-mentioned range, the overall performance of the coolant can be further improved.

[0022] According to the present invention, preferably, the base oil is 85-99.8 wt% based on the total weight of the composition, and can be any two values ​​formed by the range of 85, 86, 87, 88, 89, 90, 91, 92, 93, 94, 95, 96, 97, 98, 99, 99.5, 99.8, or a value within the range, and more preferably 90-99.5 wt%.

[0023] According to the present invention, preferably, the additive is 0.2-15 wt% based on the total weight of the composition, and can be any two values ​​from 0.2, 0.3, 0.5, 0.8, 1, 1.2, 1.3, 1.5, 2, 3, 5, 6, 8, 9, 10, 11, 12, 13, 15, or a value within that range, and more preferably 0.5-10 wt%.

[0024] According to the present invention, preferably, the base oil (or monoester) has a kinematic viscosity of 2-10 mm at 40°C. 2 / s can be any range formed by any two values ​​from 2, 2.5, 3, 3.5, 4, 5, 5.5, 6, 7, 7.5, 8, 8.5, 9, 10, or a value within that range, and is more preferably 3-8mm. 2 / s.

[0025] In this invention, there is no particular limitation on the source of the base oil; it can be commercially available or prepared, as long as the structure of the base oil is as shown in Formula I. Preferably, the monoester of this invention is prepared by esterification of a monocarboxylic acid and a monohydric alcohol under the action of a catalyst, wherein the structural formula of the monocarboxylic acid is as shown in Formula II, and the structural formula of the monohydric alcohol is as shown in Formula III.

[0026]

[0027] HO-R3 Form III;

[0028] In Formulas II and III, R1 is a straight-chain alkyl group of C2-C15, R2 is a straight-chain alkyl group of C1-C10, and R3 is a straight-chain alkyl group of C5-C20.

[0029] In this invention, the preparation method of the monoester is as follows: under the action of a catalyst, the acid represented by Formula II and the alcohol represented by Formula III undergo an esterification reaction.

[0030] In this invention, the specific operation of the esterification reaction includes the following steps: (1) adding the catalyst, the acid shown in Formula II and the alcohol shown in Formula III into the reactor and heating the reactor to carry out the reaction; (2) distilling under absolute pressure to separate the water produced in the esterification reaction by distillation; (3) after the esterification reaction is completed, cooling to room temperature and purifying to obtain the base oil.

[0031] In this invention, the esterification reaction is carried out under an inert gas, which is at least one of nitrogen, argon and helium.

[0032] According to the present invention, preferably, the molar ratio of the acid represented by Formula II to the alcohol represented by Formula III is 0.98-1.2, more preferably 0.99-1.05.

[0033] According to the present invention, preferably, the amount of catalyst used is 0.5-10g relative to each kilogram of monocarboxylic acid and monohydric alcohol, more preferably 0.8-3g.

[0034] In this invention, the acid is selected from at least one of 2-ethylpentanoic acid, 2-ethylhexanoic acid, 2-ethylheptanoic acid, 2-ethyloctanoic acid, 2-ethylnonanoic acid, 2-ethyldecanoic acid, 2-ethylundecanoic acid, 2-ethyldodecanoic acid, 2-propylhexanoic acid, 2-propylheptanoic acid, 2-propyloctanoic acid, 2-propylnonanoic acid, 2-propyldecanoic acid, 2-propylundecanoic acid, 2-propyldodecanoic acid, 2-propyltridecanoic acid, 2-butylheptanoic acid, 2-butyloctanoic acid, 2-butylnonanoic acid, 2-butyldecanoic acid, 2-butylundecanoic acid, 2-butyldodecanoic acid, 2-butyltridecanoic acid, 2-butyltetradecanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, 2-pentanoic acid, and 2-pentanoic acid.

[0035] In this invention, the alcohol is selected from at least one of n-hexanol, n-heptanol, n-octanol, n-nonanol, n-decanol, n-undecylol, n-dodecylol, n-tridecylol, n-tetradecylol, and n-pentadecanol.

[0036] In this invention, the reactor is at least one of a batch reactor, a tubular reactor, a fixed bed reactor, and a fluidized bed reactor.

[0037] In this invention, the catalyst is at least one of inorganic acids, heteropoly acids, organic sulfonic acids, and acidic resins. Preferably, the catalyst is at least one of toluenesulfonic acid, methanesulfonic acid, phosphotungsten heteropoly acid, and acidic resins.

[0038] In this invention, the esterification reaction is carried out at a temperature of 80-150°C for 8-12 hours. Preferably, the esterification reaction is carried out at a temperature of 100-130°C for 10-12 hours.

[0039] In this invention, the distillation apparatus in step (2) is at least one of a thin-film evaporator, a scraped-film evaporator, and a falling-film evaporator.

[0040] In this invention, the vacuum degree of the distillation apparatus in step (2) is 10-80 kPa, preferably 40-60 kPa.

[0041] In this invention, the purification includes alkali washing, water washing, vacuum distillation, and decolorization of the esterification product.

[0042] In this invention, the purification conditions are conventional choices in the art, and those skilled in the art can choose according to actual needs.

[0043] In this invention, there are no particular limitations on the raw materials and operation of alkaline washing, as long as the acid in the esterification product can be neutralized. Those skilled in the art can select the raw materials for alkaline washing according to actual needs. In some specific embodiments of this invention, the raw material for alkaline washing is preferably sodium hydroxide. The raw material for alkaline washing is provided in the form of an aqueous solution. Preferably, the concentration of alkali (such as NaOH) in the aqueous solution can be 1-10 wt%, more preferably 2-6 wt%.

[0044] The water washing operation described in this invention is not particularly limited. As long as the product after alkali washing is washed with water until it is neutral, those skilled in the art can choose according to actual needs.

[0045] According to the present invention, in order to remove excess water from the system after washing, the system needs to be distilled under reduced pressure. The conditions for reduced pressure distillation may include: a temperature of 30-120°C, preferably 60-95°C, and a pressure of 1-100 kPa, preferably 5-30 kPa.

[0046] According to the present invention, preferably, the additive is selected from antioxidants and / or pour point depressants.

[0047] According to the present invention, preferably, the antioxidant content is 0.1-5 wt% based on the total weight of the composition, and can be any two values ​​formed by 0.1, 0.2, 0.5, 0.8, 1, 1.1, 1.3, 1.5, 1.8, 2, 2.5, 2.8, 3, 3.5, 3.8, 4, 4.5, 4.8, 5, or a value within that range, and more preferably 0.2-3.5 wt%.

[0048] According to the present invention, preferably, the content of the pour point depressant is 0.05-1 wt% based on the total weight of the composition, and can be any two values ​​from 0.05, 0.1, 0.15, 0.2, 0.25, 0.3, 0.35, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, 1, or a value within that range, and more preferably 0.1-0.5 wt%.

[0049] According to the present invention, preferably, the content of the antioxidant is 0.3-1.2g and the content of the pour point depressant is 0.1-0.5g relative to 98.7g of base oil.

[0050] According to the present invention, preferably, the antioxidant is dialkyldiphenylamine.

[0051] According to the present invention, preferably, the number of carbon atoms of the alkyl group in the antioxidant is 4-10, and can be 4, 5, 6, 7, 8, 9, or 10.

[0052] According to the present invention, preferably, the antioxidant is at least one of octylbutyl diphenylamine, dioctyl diphenylamine, dinonyl diphenylamine, octylpentyl diphenylamine, and nonylbutyl diphenylamine, and the brand name of the antioxidant is at least one of IRGANOX L-57 (octylbutyl diphenylamine), T534 (octylbutyl diphenylamine), VANLUBE SS (octyl diphenylamine), VANLUBE 961 (octylbutyl diphenylamine), VANLUBE 81 (dioctyl diphenylamine), and RC7001 (p-dioctyl diphenylamine).

[0053] According to the present invention, preferably, the pour point depressant is polyalkyl methacrylate.

[0054] In this invention, the main purpose of adding the pour point depressant is to lower the pour point of the coolant and keep the coolant fluid.

[0055] According to the present invention, preferably, the number average molecular weight of the polymethyl methacrylate is 15,000-20,000, which can be any two values ​​from 15,000, 16,000, 17,000, 18,000, 19,000, and 20,000, or any value within that range.

[0056] According to the present invention, preferably, the alkyl group in the polymethyl methacrylate has 8-18 carbon atoms; more preferably, the alkyl group in the polymethyl methacrylate is octyl, nonyl, decyl, (n-)undecyl, (n-)dodecyl, (n-)tridecyl, (n-)tetradecyl, (n-)pentadecanyl, (n-)hexadecyl, (n-)heptadecyl, and (n-)octadecyl, and the pour point depressant is at least one of VX 248, Irgaflo 610P, Irgaflo 710P, and RIPP-T866.

[0057] A second aspect of the present invention provides the application of the monoester as described above in improving the thermal conductivity and biodegradability of coolants.

[0058] In this invention, the preparation method of the coolant composition is as follows: mixing the base oil as described above with the additives.

[0059] In this invention, there are no particular limitations on the mixing conditions. Preferably, the mixing temperature is 40-90°C and the mixing time is 1-6 hours.

[0060] According to a particularly preferred embodiment of the present invention, 2-propyldecanoic acid, n-dodecyl alcohol, and p-toluenesulfonic acid monohydrate (the molar ratio of 2-propyldecanoic acid to n-dodecyl alcohol is 0.99-1.02, and the amount of p-toluenesulfonic acid monohydrate is 0.9-2 g per kilogram of 2-propyldecanoic acid and n-dodecyl alcohol) are added to a glass reactor equipped with stirring and heating. After stirring and mixing, N2 is introduced into the reaction solution and the temperature is raised. After the temperature reaches 95-110°C, timing is started. Distillation is carried out at an absolute pressure of 47-52 kPa, and the reaction temperature is controlled at 110-120°C. The water generated in the esterification reaction is continuously distilled off through an evaporator. After the reaction proceeded for 11-12 hours, the reaction solution was gradually cooled to room temperature, washed with a 3-6 wt% sodium hydroxide solution, and then treated with demineralized water until neutral. Vacuum distillation was then performed under vacuum of 5-15 kPa (temperature 75-90℃), followed by decolorization with clay to obtain dodecyl 2-methyldecanoate. Gas chromatography analysis was performed on the reaction solution to determine the conversion rate of n-dodecyl alcohol and the yield of the product. The obtained dodecyl 2-methyldecanoate, an antioxidant, and a pour point depressant were mixed. The antioxidant content was 0.8-1.1 g and the pour point depressant content was 0.15-0.4 g relative to 98.7 g of dodecyl 2-methyldecanoate. The mixture was then stirred at 45-65℃ for 0.5-1.5 hours.

[0061] The present invention will be described in detail below through embodiments. In the following embodiments and comparative examples:

[0062] The dielectric constant was measured using the standard test method of GB / T 5654, and the test was conducted at 90℃ and 50Hz.

[0063] The kinematic viscosity at 40℃ was measured according to the standard test method of GB / T 265;

[0064] The thermal conductivity was measured using the ASTM D7896 standard test method at 40°C.

[0065] Biodegradability was measured using the OECD 301B method, which measures the biodegradability rate of samples after 28 days of exposure to darkness.

[0066] Qa raw material is Juhua JX-2 perfluoropolyether type commercially available product;

[0067] T534, Octylbutyldiphenylamine antioxidant, Xinxiang Ruifeng Chemical Co., Ltd.;

[0068] VANLUBE 961, Octylbutyldiphenylamine;

[0069] VX 248, a high molecular weight polymethacrylate pour point depressant, Evonik Industries;

[0070] Irgaflo 710P, a high molecular weight polymethacrylate pour point depressant, BASF.

[0071] Preparation Example 1

[0072] 322.07 g of 2-propyldecanoic acid, 280 g of n-dodecyl alcohol, and 0.7 g of p-toluenesulfonic acid monohydrate were added to a stirred and heated glass reactor. After mixing, N2 was introduced into the reaction solution and the temperature was raised. Timing was started after the temperature reached 100°C. Distillation was carried out under absolute pressure of 50 kPa, with the reaction temperature controlled at 115°C. Water generated during the esterification reaction was continuously distilled off using an evaporator. After 12 hours of reaction, the reaction solution was gradually cooled to room temperature, washed with a 5 wt% sodium hydroxide solution, and then treated with demineralized water until neutral. Vacuum distillation was then performed under vacuum of 10 kPa (temperature 85°C), followed by decolorization with bleaching clay to obtain dodecyl 2-propyldecanoate (structure shown in Formula I, R1 is C10, R2 is C3, R3 is C12), labeled Wa. Gas chromatography analysis of the reaction solution showed a 99% conversion rate of n-dodecyl alcohol and a 94% yield of the product.

[0073] Preparation Example 2

[0074] 348.29 g of 2-butylnonanoic acid, 280 g of n-undecyl alcohol, and 0.7 g of p-toluenesulfonic acid monohydrate were added to a glass reactor equipped with stirring and heating. After thorough mixing, N2 was introduced into the reaction solution and the temperature was raised. Timing was started after the temperature reached 100°C. Distillation was carried out under absolute pressure of 45 kPa, with the reaction temperature controlled at 120°C. Water generated during the esterification reaction was continuously distilled off using an evaporator. After 12 hours of reaction, the reaction solution was gradually cooled to room temperature, washed with a 5 wt% sodium hydroxide solution, and then treated with demineralized water until neutral. Vacuum distillation was then performed under vacuum of 10 kPa (temperature 90°C), followed by decolorization with bleaching clay to obtain undecyl 2-butylnonanoate (structure shown in Formula I, R1 is C9, R2 is C4, R3 is C11), labeled Wb. Gas chromatography analysis of the reaction solution showed a 99% conversion rate of n-undecyl alcohol and a 92% yield of the product. Figure 1 This is the infrared spectrum of undecyl 2-butylnonanoate, with the value at 2926 cm⁻¹. -1 and 2856cm -1 The absorption peak at 1735 cm⁻¹ is the stretching vibration peak of the C-H bond. -1 The absorption peak at 1466 cm⁻¹ is the stretching vibration peak of the C=O double bond. -1 The absorption peak at 1165 cm⁻¹ is the bending vibration peak of the C-H bond. -1 The absorption peak at 1377 cm⁻¹ is the stretching vibration peak of the C—O—C bond. -1 The absorption peak at that point is the stretching vibration peak of the C-O bond in unreacted n-undecanol.

[0075] Preparation Example 3

[0076] 321.57 g of 2-pentyloctanoic acid, 300.56 g of n-tetrazol, and 0.75 g of methanesulfonic acid monohydrate were added to a stirred and heated glass reactor. After mixing, N2 was introduced into the reaction solution and the temperature was raised. Timing was started after the temperature reached 100°C. Distillation was carried out under absolute pressure of 25 kPa, with the reaction temperature controlled at 90°C. Water generated during the esterification reaction was continuously distilled off using an evaporator. After 12 hours of reaction, the reaction solution was gradually cooled to room temperature, washed with a 5 wt% sodium hydroxide solution, and then treated with demineralized water until neutral. Vacuum distillation was then performed under vacuum of 10 kPa (temperature 87°C), followed by decolorization with bleaching clay to obtain 2-pentyloctanoic acid tridecyl ester (structure shown in Formula I, R1 is C8, R2 is C5, R3 is C13), labeled Wc. Gas chromatography analysis of the reaction solution showed a 99% conversion rate of n-tetrazol and a 93% yield of the product.

[0077] Preparation Example 4

[0078] 216.32 g of 2-ethylhexanoic acid, 195.35 g of n-octanol, and 0.71 g of methanesulfonic acid monohydrate were added to a glass reactor equipped with stirring and heating. After mixing, N2 was introduced into the reaction solution and the temperature was raised. Timing was started after the temperature reached 100°C. Distillation was carried out under absolute pressure of 40 kPa, with the reaction temperature controlled at 90°C. Water generated during the esterification reaction was continuously distilled off using an evaporator. After 12 hours of reaction, the reaction solution was gradually cooled to room temperature, washed with a 5 wt% sodium hydroxide solution, and then treated with demineralized water until neutral. Vacuum distillation was then carried out under vacuum of 10 kPa (temperature 90°C), followed by decolorization with bleaching clay to obtain 2-ethylhexanoic acid n-octyl ester (structure shown in Formula I, R1 is C6, R2 is C2, R3 is C8), labeled Wd. Gas chromatography analysis of the reaction solution showed a conversion rate of 99% for 2-ethylhexanoic acid n-octyl ester and a product yield of 91%.

[0079] Preparation Example 5

[0080] The monoester was prepared according to the method described in Preparation Example 1, except that 2-propyldecanoic acid was replaced with 2-ethylpropionic acid and n-dodecyl alcohol was replaced with n-octadecyl alcohol, yielding octadecyl 2-ethylpropionate (structure shown in Formula I, R1 is C3, R2 is C2, and R3 is C18), labeled as We. Gas chromatography analysis of the reaction solution showed a 99% conversion of n-octadecyl alcohol and a product yield of 85%.

[0081] Preparation Example 6

[0082] The monoester was prepared according to the method described in Preparation Example 1, except that 2-propyldecanoic acid was replaced with 1-pentanoic acid and n-dodecyl alcohol was replaced with pentaerythritol, yielding pentaerythritol pentyl ester, labeled Qb. Gas chromatography analysis of the reaction solution showed a pentaerythritol conversion rate of 99% and a product yield of 82%.

[0083] Examples and Comparative Examples

[0084] The base oil obtained in the preparation example was mixed with antioxidants and pour point depressants, and the proportions of each component are shown in Table 1. The components were added to a mixing container and mixed at 50°C for 1 hour to prepare coolants. The properties of each coolant are shown in Table 2.

[0085] Table 1

[0086]

[0087]

[0088] Table 2

[0089]

[0090] As can be seen from the results of the examples and comparative examples in Table 2, the coolant prepared by the examples of the present invention has good biodegradability and good thermal conductivity while meeting its electrical insulation performance requirements. Moreover, the coolant prepared by the preferred embodiment of the present invention has a degradation rate of more than 75% and its thermal conductivity is also excellent.

[0091] A common mechanism of biodegradation is through hydrolysis or the cleavage of heteroatom bonds in unstable enzyme groups, leading to the breakage of the compound's molecular chain. The backbone of synthetic ester compounds is mostly composed of aliphatic structural units linked by easily hydrolyzable ester bonds, exhibiting high flexibility and susceptibility to decomposition by various microorganisms and plant enzymes in nature. Therefore, the unique ester bond structure in synthetic ester base oil products results in coolants with significantly superior biodegradability compared to mineral oils, synthetic hydrocarbons, silicone oils, and fluorinated fluids. This invention uses synthetic esters with excellent biodegradability as raw materials, aligning with the current trend towards low-carbon, green, and environmentally friendly practices.

[0092] The preferred embodiments of the present invention have been described in detail above; however, the present invention is not limited thereto. Within the scope of the inventive concept, various simple modifications can be made to the technical solutions of the present invention, including combinations of various technical features in any other suitable manner. These simple modifications and combinations should also be considered as the content disclosed in the present invention and are all within the protection scope of the present invention.

Claims

1. A coolant composition, characterized in that, The composition includes a base oil and an additive, wherein the base oil comprises a monoester with the structural formula shown in Formula I: In Formula I, R1 is a C2-C15 straight-chain alkyl group, R2 is a C1-C10 straight-chain alkyl group, and R3 is a C5-C20 straight-chain alkyl group. The content of the monoester shown in Formula I in the coolant composition is not less than 65 wt%.

2. The composition according to claim 1, wherein, R1 is a C2-C10 straight-chain alkyl group, R2 is a C5-C10 straight-chain alkyl group, and R3 is a C8-C17 straight-chain alkyl group. Preferably, R1 is a C3-C5 straight-chain alkyl group, R2 is a C7-C9 straight-chain alkyl group, and R3 is a C10-C15 straight-chain alkyl group.

3. The composition according to claim 1 or 2, wherein, The content of the monoester represented by Formula I in the coolant composition is not less than 75 wt%; Preferably, the content of the monoester represented by Formula I in the coolant composition is not less than 90 wt%.

4. The composition according to any one of claims 1-3, wherein, Based on the total weight of the composition, the base oil is 85-99.8 wt% and the additives are 0.2-15 wt%. Preferably, the base oil comprises 90-99.5 wt% and the additives comprise 0.5-10 wt% based on the total weight of the composition.

5. The composition according to any one of claims 1-4, wherein, The base oil has a kinematic viscosity of 2-10 mm at 40°C. 2 / s; Preferably, the base oil has a kinematic viscosity of 3-8 mm at 40°C. 2 / s.

6. The composition according to any one of claims 1-5, wherein, The additives are selected from antioxidants and / or pour point depressants; Preferably, the antioxidant content is 0.1-5 wt% based on the total weight of the composition; Preferably, the content of the pour point depressant is 0.05-1 wt% based on the total weight of the composition.

7. The composition according to claim 6, wherein, Based on the total weight of the composition, the content of the antioxidant is 0.2-3.5 wt%. Preferably, the content of the pour point depressant is 0.1-0.8 wt% based on the total weight of the composition; Preferably, relative to 98.7g of base oil, the content of the antioxidant is 0.3-1.2g and the content of the pour point depressant is 0.1-0.5g.

8. The composition according to claim 6, wherein, The antioxidant is dialkyldiphenylamine; Preferably, the number of carbon atoms in the alkyl group of the antioxidant is 4-10; More preferably, the antioxidant is at least one selected from octylbutyldiphenylamine, dioctyldiphenylamine, dinonyldiphenylamine, octylpentyldiphenylamine, and nonylbutyldiphenylamine.

9. The composition according to claim 6, wherein, The pour point depressant is polyalkyl methacrylate; Preferably, the number-average molecular weight of the polymethyl methacrylate is 15,000-20,000; Preferably, the alkyl group in the polymethyl methacrylate has 8-18 carbon atoms; Preferably, the alkyl group in the polymethyl methacrylate is octyl, nonyl, decyl, undecyl, dodecyl, tridecyl, tetradecyl, pentadecyl, hexadecyl, heptadecyl, or octadecyl.

10. The use of the monoester as described in claim 1 or 2 in improving the thermal conductivity and biodegradability of coolants.